Injection mold for hold-down chain wheel of escalator hand strap
By designing a coaxial and angled runner structure in the elevator handrail belt compression sprocket injection mold, it ensures that the cooling and solidification raw materials do not enter the molding cavity directly, solving the problem of uneven structure in the existing technology and improving the sprocket Mechanical properties and production quality.
Patent Information
- Application Number
- CN202420782398.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-15
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-04-15
AI Technical Summary
After the mold is opened, the raw materials in the gate cool down and solidify the structure in the mold, which reduces the tensile strength, impact toughness and wear resistance of the sprocket.
An injection mold including a second unit mold and a first unit mold provided with a gate is designed, and a forming cavity is communicated through a main flow channel. The main flow channel includes a front runner, a rear runner and a branch runner, and a front runner Coaxial to the rear runner, the branch runner and the front runner are at an angle to ensure that the cooled and solidified raw materials enter the rear runner first, and the subsequent melted raw materials enter the molding cavity through the branch runner, reducing the solidified raw materials into molding chance of cavity.
It effectively improves the quality of the compression sprocket produced by injection molds, improves the mechanical properties of the sprocket, reduces the chance of cooling and solidification raw materials entering the molding cavity, and enhances the uniformity and performance of the sprocket.
Smart Images

Figure CN222096838U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of compression sprocket production, in particular to an injection mold for a compression sprocket of an elevator handrail. Background Art
[0002] The elevator handrail compression sprocket is a key component in the elevator equipment. Its main function is to tighten the chain on the elevator handrail to ensure that the handrail runs smoothly and stably.
[0003] Injection molds are required for the production of compression sprockets. After the injection mold is opened, part of the raw material in the gate comes into contact with the air to cool and solidify. When the mold is closed again for production, the partially solidified raw material is fed into the molding cavity, resulting in an uneven internal structure of the compression sprocket that is finally formed. This makes it easy for stress concentration to occur when it is subjected to force, thereby reducing the mechanical properties of the compression sprocket, such as tensile strength, impact toughness and wear resistance.
[0004] Therefore, it is necessary to improve the injection mold in the prior art. Utility Model Content
[0005] The utility model aims to overcome the defects in the prior art and provide an elevator handrail compression sprocket injection mold, thereby improving the quality of the compression sprocket injection-molded by the injection mold.
[0006] To achieve the above purpose, the specific technical scheme of the elevator handrail compression sprocket injection mold of the utility model is as follows:
[0007] An elevator handrail compression sprocket injection mold comprises a second unit mold and a first unit mold provided with a gate. In a mold closing state, the gate is connected to a molding cavity through a main flow channel. The main flow channel comprises a front section flow channel connected to the gate. The front section flow channel is connected to a rear section flow channel and a branch section flow channel connected to the molding cavity. The front section flow channel is coaxially arranged with the rear section flow channel, and the branch section flow channel is arranged at an angle to the front section flow channel.
[0008] Preferably, two inserts are relatively slidably arranged on the parting surface of the second unit mold, and the opposite sides of the two inserts are provided with unit cavities and unit flow channels; when the mold is in the closed state, the two unit flow channels are combined to form a main flow channel, and the two unit cavities are combined with the parting surface of the first unit mold and the second unit mold to form a molding cavity, and a core block is also arranged in the molding cavity.
[0009] Preferably, a recess communicating with the rear section flow channel is further provided on the parting surface of the second unit mold.
[0010] Preferably, the inner diameter of the recess gradually decreases from its opening toward the bottom.
[0011] Preferably, two inclined guide rods are symmetrically arranged on the parting surface of the first unit mold, and along the moving direction of the insert, the distance between one end of the two inclined guide rods adjacent to the second unit mold is greater than the distance between the other ends, and the two inserts are provided with guide holes that slide with the inclined guide rods.
[0012] Preferably, a groove is provided on the parting surface of the first unit mold, and in the mold closing state, the two inserts are plugged into and matched with the groove, and the back side surfaces of the two inserts are both inclined guide surfaces.
[0013] Preferably, the core block is slidably connected to the second unit mold along a moving direction of the first unit mold when the first unit mold is opened.
[0014] Preferably, the second unit mold is slidably connected to a moving seat along the moving direction of the core block, the core block is fixedly connected to the moving seat, and the second unit mold is provided with a limiting hole that slidably cooperates with the core block.
[0015] The elevator handrail compression sprocket injection mold of the utility model has the following advantages: in the process of raw materials entering the molding cavity through the gate and the main channel in sequence, part of the raw materials cooled and solidified in the gate are first squeezed into the rear section flow channel, and when the rear section flow channel is filled, the subsequent melted raw materials enter the molding cavity through the branch section flow channel, thereby reducing the probability of solidified raw materials entering the molding cavity and improving the quality of the compression sprocket produced by the injection mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a structural schematic diagram of the injection mold of the utility model;
[0017] Figure 2 It is a first cross-sectional view of the injection mold of the utility model;
[0018] Figure 3 It is a second cross-sectional view of the injection mold of the utility model;
[0019] Figure 4 It is a schematic diagram of the connection structure between the second unit mold and the insert block of the utility model;
[0020] Figure 5 It is a structural schematic diagram of the first unit mold of the utility model;
[0021] Figure 6 It is a structural schematic diagram of the second unit mold of the utility model;
[0022] Figure 7 It is a structural schematic diagram of the insert block of the utility model;
[0023] Markings in the figure are as follows: 1. first unit mold; 2. second unit mold; 3. movable seat; 4. insert block; 101. gate; 102. groove; 103. inclined guide rod; 201. notch; 202. limit hole; 203. slide groove; 301. core block; 41. guide hole; 42. molding cavity; 43. slider; 44. main flow channel; 441. front section flow channel; 442. rear section flow channel; 443. branch section flow channel. DETAILED DESCRIPTION
[0024] The following is a further description of the specific implementation of the present invention in conjunction with the accompanying drawings and embodiments. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the present invention.
[0025] The terms “top surface”, “bottom surface” and “underside” are based on the normal use state of the injection mold and are only used to facilitate the description of the present invention and simplify the description. They do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation. Therefore, they cannot be understood as a limitation on the present invention.
[0026] like Figure 1-7 As shown, an elevator handrail compression sprocket injection mold includes a second unit mold 2 and a first unit mold 1 provided with a gate 101. When the molds are in the closed state, the gate 101 is connected to the molding cavity 42 through the main channel 44. The main channel 44 includes a front section flow channel 441 connected to the gate 101, the front section flow channel 441 is connected to the rear section flow channel 442 and a branch section flow channel 443 connected to the molding cavity 42, the front section flow channel 441 and the rear section flow channel 442 are coaxially arranged, and the branch section flow channel 443 is arranged at an angle to the front section flow channel 441.
[0027] The above-mentioned injection mold is installed on an injection molding machine and is used for injection molding the compression sprocket of an elevator handrail. When in use, the injection molding machine controls the relative movement of the first unit mold 1 and the second unit mold 2 to realize the opening and closing of the injection mold. After the injection mold is closed, the injection molding machine injects the melted raw material through the gate 101, and then the raw material enters the molding cavity 42 through the main channel 44, and is cooled and molded in the molding cavity 42 to form a compression sprocket; then the injection mold is opened and the finished compression sprocket is taken out. During this process, part of the raw material located inside the gate 101 is cooled and solidified after contacting with the air. In the subsequent production process, the solidified raw material enters the molding cavity 42, which will affect the finished compression sprocket produced by the injection mold.
[0028] In order to solve the above problems, the main flow channel 44 is divided into a front section flow channel 441, a branch section flow channel 443 and a rear section flow channel 442. The number of molding cavities 42 in the injection mold can be adjusted according to actual needs. The number of branch section flow channels 443 is consistent with the number of molding cavities 42, and each branch section flow channel 443 is connected to a molding cavity 443; in this way, in the process of the raw material entering each molding cavity 42 through the main flow channel 44, since the front section flow channel 441 and the rear section flow channel 442 are coaxially arranged, the two are straight flow channels, and the branch section flow channel 443 and the front section flow channel 443 are connected. The runners 441 are distributed at right angles and are not directly connected to each other. Therefore, part of the raw material cooled and solidified inside the gate 101 first enters the rear runner 442. When the rear runner 442 is filled with raw material, the raw material in a molten state that enters subsequently can no longer enter the rear runner 442, and under the action of pressure, it will enter the molding cavity 42 through the branch runner 443. By holding the cooled and solidified raw material in the rear runner 442, the probability of the cooled and solidified raw material entering the molding cavity 42 can be reduced, thereby improving the quality of the injection mold production compression sprocket flattening.
[0029] A further improvement is, Figure 1-4 As shown, two inserts 4 are relatively slidably arranged on the parting surface of the second unit mold 2, and the opposite sides of the two inserts 4 are provided with unit cavities and unit flow channels; when the mold is closed, the two unit flow channels are combined to form a main flow channel 44, and the two unit cavities are combined with the parting surfaces of the first unit mold 1 and the second unit mold 2 to form a molding cavity 42, and a core block 301 is also arranged in the molding cavity 42.
[0030] In the above-mentioned injection mold, the moving direction of the insert block 4 is perpendicular to the moving direction of the first unit mold 1, the parting surface of the second unit mold 2 is provided with two slide grooves 203, the insert block 4 is integrally formed with a slider 43, and the slide groove 203 and the slider 43 are slidably matched to realize the relative sliding of the two insert blocks 4; when the injection mold is closed, the two insert blocks 4 are first closed with each other, and then the first unit mold 1 and the second unit mold 2 are closed with each other. After closing, the molding cavity 42 is composed of the two unit cavities on the two insert blocks 4 and the parting surface of the first unit mold 1. , the parting surface of the second unit mold 2 and the core block 301 are combined, the molding cavity 42 is a cylindrical structure, and the main flow channel 44 is composed of two unit flow channels on the two insert blocks 4; after the injection molding is completed, the first unit mold 1 and the second unit mold 2 are opened, and the two insert blocks 4 are also opened, so that the finished product of the clamping sprocket is separated from the insert blocks 4, the first unit mold 1 and the second unit mold 2, so that the insert blocks 4 are easier to demold, and at the same time the main flow channel 44 will also be opened, which is convenient for taking out the sprue material inside the main flow channel 44, thereby improving the convenience of mold use.
[0031] A further improvement is, Figure 2 and 3As shown, a notch 201 connected to the rear runner 442 is also provided on the parting surface of the second unit mold 2. The notch 201 can be set according to the capacity inside the gate 101. When the space of the rear runner 442 cannot accommodate the raw material cooled and formed inside the gate 101, part of the raw material cooled and formed can directly enter the notch 201, thereby reducing the probability of the raw material cooled and formed entering the molding cavity 42, and improving the quality of the injection mold production clamping sprocket.
[0032] A further improvement is, Figure 2 and 3 As shown, the inner diameter of the recess 201 gradually decreases from the opening to the bottom. The recess 201 has a large opening and a small interior, which can facilitate the removal of the raw material inside the recess 201 after the injection mold is opened, and prevent the raw material from being stuck inside the recess 201, thereby improving the convenience of using the injection mold.
[0033] A further improvement is, Figure 2 and 5 As shown, two inclined guide rods 103 are symmetrically arranged on the parting surface of the first unit mold 1. Along the moving direction of the insert 4, the distance between the two ends of the two inclined guide rods 103 adjacent to the second unit mold 2 is greater than the distance between the other ends. Both inserts 4 are provided with guide holes 41 that are slidably matched with the inclined guide rods 103. When the injection mold is opened, the first unit mold 1 can move while the inclined guide rods 103 cooperate with the guide holes 41 to drive the two inserts 4 away from each other, thereby realizing the linkage between the first unit mold 1 and the insert 4. When the mold is closed, the first unit mold 1 drives the two inserts 4 to move closer to each other to complete the mold closing, thereby improving the convenience of mold use.
[0034] A further improvement is, Figure 5 As shown, the parting surface of the first unit mold 1 is provided with a groove 102. When the mold is closed, the two inserts 4 are plugged into the groove 102, and the back-facing sides of the two inserts 4 are inclined guide surfaces. In the injection mold, the guide surface of the same insert 4 and the inclined guide rod 103 connected to the insert are at the same angle, so that the linkage between the first unit film 1 and the insert 4 will not interfere with each other; when the mold is closed, the insert 4 is located inside the groove 102, and the insert 4 is locked by the groove 102, thereby improving the stability of the insert 4 and improving the quality of the injection mold production compression sprocket.
[0035] A further improvement is, Figure 3 and 6As shown, the core block 301 is slidably connected to the second unit mold 2 along the moving direction of the first unit mold 1 when the mold is opened, and the second unit mold 2 is slidably connected to the moving seat 3 along the moving direction of the core block 301. The core block 301 is fixedly connected to the moving seat 3, and the second unit mold 2 is provided with a limiting hole 202 that slidably cooperates with the core block 301. In the above-mentioned injection mold, the injection molding machine connected thereto is provided with a hydraulic cylinder for driving the moving seat 3 to move alone. When the injection mold is opened, the hydraulic cylinder pulls the moving seat 3 to move, thereby pulling the core block 301 to move inside the limiting hole 202, so that the core block 301 and the formed clamping sprocket are separated from each other, further improving the convenience of demoulding the finished clamping sprocket, and thus improving the convenience of using the injection mold.
[0036] It is understood that the present invention is described by some embodiments, and those skilled in the art are aware that various changes or equivalent substitutions may be made to these features and embodiments without departing from the spirit and scope of the present invention. In addition, under the teachings of the present invention, these features and embodiments may be modified to adapt to specific circumstances and materials without departing from the spirit and scope of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed herein, and all embodiments falling within the scope of the claims of this application are within the scope of protection of the present invention.
Claims
1. An elevator handrail compression sprocket injection mold, comprising a second unit mold (2) and a first unit mold (1) provided with a gate (101), characterized in that: When the mold is in a closed state, the gate (101) is connected to the molding cavity (42) through the main channel (44), the main channel (44) comprises a front section flow channel (441) connected to the gate (101), the front section flow channel (441) is connected to the rear section flow channel (442) and a branch section flow channel (443) connected to the molding cavity (42), the front section flow channel (441) and the rear section flow channel (442) are coaxially arranged, and the branch section flow channel (443) and the front section flow channel (441) are arranged at an angle.
2. The elevator handrail compression sprocket injection mold according to claim 1, characterized in that: Two inserts (4) are relatively slidably arranged on the parting surface of the second unit mold (2), and the opposite sides of the two inserts (4) are both provided with unit cavities and unit flow channels; In the mold closing state, the two unit flow channels are combined to form a main flow channel (44), and the two unit cavities are combined with the parting surfaces of the first unit mold (1) and the second unit mold (2) to form a molding cavity (42), and a core block (301) is also arranged in the molding cavity (42).
3. The elevator handrail compression sprocket injection mold according to claim 2, characterized in that: The parting surface of the second unit mold (2) is also provided with a recess (201) connected to the rear section flow channel (442).
4. The elevator handrail compression sprocket injection mold according to claim 3, characterized in that: The inner diameter of the notch (201) gradually decreases from its opening toward the bottom.
5. The elevator handrail compression sprocket injection mold according to claim 2, characterized in that: Two oblique guide rods (103) are symmetrically arranged on the parting surface of the first unit mold (1); along the moving direction of the insert block (4), the distance between one end of the two oblique guide rods (103) adjacent to the second unit mold (2) is greater than the distance between the other ends; and the two insert blocks (4) are each provided with a guide hole (41) that is slidably matched with the oblique guide rods (103).
6. The elevator handrail compression sprocket injection mold according to claim 5, characterized in that: The parting surface of the first unit mold (1) is provided with a groove (102). When the mold is in a closed state, the two inserts (4) are plugged into and matched with the groove (102), and the back-facing side surfaces of the two inserts (4) are both inclined guide surfaces.
7. The elevator handrail compression sprocket injection mold according to claim 2, characterized in that: The core block (301) is slidably connected to the second unit mold (2) along the moving direction of the first unit mold (1) when the first unit mold (1) is opened.
8. The elevator handrail compression sprocket injection mold according to claim 7, characterized in that: The second unit mold (2) is slidably connected to a movable seat (3) along the moving direction of the core block (301); the core block (301) is fixedly connected to the movable seat (3); and the second unit mold (2) is provided with a limiting hole (202) slidably matched with the core block (301).