Electrical connecting sheet
A steel-based electrical connecting piece with a nickel-plated and zinc-plated structure addresses the cost and reliability issues of nickel connectors by enhancing elasticity and welding stability, resulting in lower production costs and higher yield rates.
Patent Information
- Application Number
- CN202420635462.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-29
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-03-29
AI Technical Summary
Existing connectors for connecting battery management systems and battery packs, typically made of tinned nickel sheets, are costly due to high nickel prices, have poor elasticity, and are prone to welding failures during the SMT process.
An electrical connecting piece made of steel, featuring a nickel-plated and zinc-plated steel body with bent sections, including a bending groove and through holes, enhances elasticity and welding stability while reducing nickel usage.
The steel-based connector achieves lower production costs, improved welding reliability, and higher yield rates by utilizing the elasticity of steel to fit the welding surface, ensuring stable connections and reduced defects.
Smart Images

Figure CN222107033U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to an electrical connecting piece and belongs to the technical field of batteries. Background Art
[0002] The description in this section merely provides background information related to the disclosure of the present utility model and does not constitute prior art.
[0003] In the field of battery processing, the connection between BMS (battery management system) and battery pack is an indispensable link in the battery field, which is directly related to the safety of battery operation. The purpose is to enable the battery management system to effectively monitor and manage the battery pack, and provide necessary protection measures to prevent overcharging and over-discharging of the battery, extend the service life of the battery, and ensure the safety and stability of the entire power system.
[0004] The existing connectors used for connecting battery management systems and battery packs on the market are generally tinned nickel sheets, and the connectors are welded to circuit boards and other locations through the SMT process (surface mount technology). However, the price of nickel sheets is generally high, making it difficult to control the production cost of the connectors. At the same time, the elasticity of nickel connectors is poor, and when laser welding the connectors, it is easy to cause welding failures due to poor contact.
[0005] There is no electrical connecting piece that can solve the above problems at present. Utility Model Content
[0006] The utility model aims to provide an electrical connecting piece which can achieve good elasticity through a steel body to enhance welding effect, use less nickel and achieve lower cost.
[0007] In order to achieve the above-mentioned object, the utility model discloses the following electrical connecting piece, which includes:
[0008] The main body comprises at least two bent sections, at least one of the bent sections is provided with a nickel-plated layer and a zinc-plated layer covering the outside of the nickel-plated layer and used for welding, wherein the material of the main body is steel.
[0009] Furthermore, the bent section provided with the galvanized layer is located at one end of the edge of the body.
[0010] Furthermore, one of the bending sections includes a connecting section, and the connecting section is located at the other end of the edge of the body.
[0011] Furthermore, the bending section provided with the galvanized layer includes a through hole.
[0012] Furthermore, the main body also includes a bending groove, which is composed of at least two adjacent bending sections. The bending groove is arranged adjacent to the bending section where the galvanized layer is arranged. The bending groove protrudes toward the side of the surface to be welded, and the bending groove matches the edge of the surface to be welded.
[0013] Furthermore, the protruding thickness of the bending groove is 1.75 mm, and the width of the bending groove is 6 mm.
[0014] Furthermore, the steel thickness of the main body is 0.15 mm, and the specific material is 304 stainless steel.
[0015] Furthermore, the thickness of the zinc coating is 2-5 um.
[0016] Furthermore, a nickel plating layer is provided on all the bending segments.
[0017] By means of the above technical solution, the beneficial effects of the utility model are as follows:
[0018] 1. The electrical connector of the utility model can complete the normal connection between the battery management system and the battery pack through the steel body, replacing the original nickel body, achieving lower costs. At the same time, because the steel product has better elasticity, the body has a better contact effect with the surface to be welded during the laser welding process, which can significantly reduce the welding defect rate.
[0019] 2. The main body of the electrical connecting piece of the utility model is bent into multiple sections, wherein a bending groove is provided to match the surface to be welded, so as to further fit the surface to be welded, and further utilize the elasticity of the steel material to realize the release of the corresponding stress during the welding process, so that the main body has a better stability effect after welding. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the embodiments of this specification or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in this specification. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0021] Figure 1 is a front view of an electrical connecting sheet provided in an embodiment of this specification;
[0022] Figure 2 is a side view of an electrical connecting sheet provided in an embodiment of this specification;
[0023] In the figure: 1, main body; 11, bending section; 111, connecting section; 112, through hole; 12, bending groove; 2, galvanized layer. DETAILED DESCRIPTION
[0024] In order to enable those skilled in the art to better understand the technical solutions in this specification, the technical solutions in the embodiments of this specification will be clearly and completely described below in conjunction with the drawings in the embodiments of this specification. Obviously, the described embodiments are only part of the embodiments of this specification, not all of the embodiments. Based on the embodiments in this specification, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of this specification.
[0025] In the description of the present utility model, it should be noted that the terms "upper", "middle", "lower", "inner", "outer", "front", "back" and the like indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present utility model and simplifying the description, rather than indicating or implying that the device or component referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present utility model. The terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance. For those of ordinary skill in the art, the specific meanings of the above terms in the present utility model can be understood according to specific circumstances. The following describes the implementation method of the present utility model based on its overall structure.
[0026] See also Figure 1-2 , is an electrical connecting sheet of this embodiment, comprising:
[0027] The main body 1 includes at least two bent sections 11 formed by bending, at least one of the bent sections 11 is provided with a nickel-plated layer (not shown in the figure) and a zinc-plated layer 2 covering the outside of the nickel-plated layer and used for welding, wherein the material of the main body 1 is steel.
[0028] A bent section 11 with a zinc coating 2 is provided.
[0029] Through the above structure, when in use, the staff can directly point the bending section 11 with the galvanized layer 2 at one end of the main body 1 toward the surface to be welded, and at the same time, point the side of the bending section 11 with the galvanized layer 2 with the galvanized layer 2 toward the surface to be welded, so that the galvanized layer 2 directly contacts the surface of the surface to be welded, and perform the welding operation through external equipment. After the welding is completed, the solder paste on one side of the galvanized layer 2 melts and forms a solder joint, which is tightly fixed on the surface to be welded, so that the main body 1 is directly fixed to the surface to be welded. At this time, due to the bending structure of the main body 1, the connecting section 111 at the other end of the main body protrudes and tilts on the surface to be welded according to a preset height, and can be docked with the connection interface on the external battery pack. In this embodiment, the connection interface is the aluminum bar sheet on one side of the battery pack. The position of the bending section 11 can be adjusted according to preset requirements to achieve a more stable connection of the aluminum bar sheet.
[0030] In the above process, since the body 1 is made of steel, the steel material has better elasticity than the traditional nickel material. Therefore, in the process of laser welding of the SMT process, the steel body 1 can better fit the surface to be welded by deformation under slight pressure, making the welding process more stable. The cost of steel is also lower, which also makes the cost of the electrical connection sheet of this embodiment lower and the welding yield rate high, further achieving a lower battery production cost. At the same time, the steel material not only has better weldability, but also has higher metal strength, with considerable tensile, compressive, bending and shear strength. Through the results of multiple embodiments, it can be found that the electrical connection sheet in the utility model is based on mass production. In five randomly selected samples, under the condition that the steel thickness of the body 1 is 0.15mm, the peeling force of the body 1 is as low as 61.9N and as high as 88.2N, and the shear force of the body 1 is as low as 745.5N and as high as 803.9N, which is significantly better than the nickel sheet electrical connection sheet of the same thickness.
[0031] It is worth noting that, under the condition of meeting the preset quality requirements, compared with the electrical connector made of traditional nickel sheets, the utility model has a significantly improved yield rate on the basis of mass production. In the same randomly selected five samples, under the condition that the steel thickness of the body 1 is 0.15mm, the bubble rate is monitored by X-ray with a minimum of 2.3% and a maximum of 7.3%, which fully meets the use requirements.
[0032] Furthermore, the steel material of the main body 1 selected in the present embodiment is 304 stainless steel, and the specific thickness of the main body 1 is 0.15mmm. The conductivity of nickel is 6.97×10^7S / m, and the conductivity of the steel selected in the present embodiment is between 6×10^6 and 8×10^6S / m, which is slightly lower than the conductivity of nickel, but fully meets the use requirements of the connection between the battery management system and the battery pack. It is estimated that in 2024, the price range of nickel will be between US$11,000 and US$15,000 / ton, while the price range of stainless steel will be between US$1,500 and US$1,900 / ton. The price difference has been more than 7 times for a long time. That is to say, the main body 1 of the present embodiment is mainly made of steel, and the steel main body 1 can achieve significant cost reduction.
[0033] For further information, see Figure 1 , a bending section 11 provided with a galvanized layer 2 is located at one end of the edge of the body 1, and one section of the bending section 11 includes a connecting section 111, and the connecting section 111 is located at the other end of the edge of the body. Specifically, the bending section 11 provided with a galvanized layer 2 of this embodiment is used to connect with the surface to be welded, and the surface to be welded is connected at the battery management system, and the connecting section 111 is used to electrically connect with other connecting parts, and the other connecting parts are located at the battery pack, which can be the aluminum bar of the battery pack in this embodiment, so that the surface to be welded and the other connecting parts are electrically connected with the help of the body 1, and the battery management system and the battery pack are electrically connected. At the same time, since the body 1 is configured to be bent in the shape of multiple sections of the bending section 11, the specific number of sections or the direction and distance of the bending of the body 1 can be set according to preset needs, so that a certain space design can be formed between the surface to be welded and the other connecting parts through the bending dislocation of the body 1, and the stability of the electrical connection between the surface to be welded and the other connecting parts is also given through the elastic deformation of the body 1. Preferably, in this embodiment, the width of the connecting section 111 is slightly larger than the width of the bending section 11 provided with the galvanized layer 2, the width of the connecting section 111 is above 7 mm, and the connecting section 111 occupies approximately one-half of the length of the main body, while the bending section 11 fixedly provided with the galvanized layer 2 is narrower in width, and the bending section 11 provided with the galvanized layer 2 occupies a smaller length of the main body, approximately one-quarter.
[0034] Furthermore, the bending section 11 provided with the zinc-plated layer 2 includes a through hole 112. Specifically, the through hole 112 can be provided to enhance the strength of the connection between components during the soldering process of surface mounting. During the flow soldering process, the solder will melt and fill the through hole 112, thereby forming a stable electrical connection and good mechanical fixation. Compared with direct mounting without through holes, the through hole 112 can form a higher strength welding effect between the body 1 and the surface to be welded, and can save the material consumption of the body 1, and can further enhance the stability of the connection.
[0035] Furthermore, if Figure 1-2 As shown, the body 1 also includes a bending groove 12, which is arranged near the bending section 11 provided with the galvanized layer 2, and the bending groove 12 protrudes toward the side of the surface to be welded, and the bending groove 12 matches the edge of the surface to be welded. At the same time, the protruding thickness of the bending groove 12 is 1.75mm, and the width of the bending groove 12 is 6mm. Specifically, the bending groove 12 is composed of three sections of the surface bent by the body 1, wherein a section of the surface close to the surface to be welded can match the edge position of the surface to be welded, so as to achieve a better abutment combination between the body 1 and the surface to be welded before and after welding. By the 1.75mm thickness of the section of the surface close to the surface to be welded relative to the surface to be welded, when welding is achieved, one side of the surface to be welded of the battery management system is abutted against the bending section 11 provided with the galvanized layer 2 and the bending groove 12, and the stress on the welding point is reduced by the absorption of vibration by the bending groove 12 during welding, thereby achieving a better welding effect and improving the production yield rate of the utility model.
[0036] Furthermore, the thickness of the zinc-plated layer 2 is 2-5um, and the thickness of the zinc-plated layer matches the steel thickness of 0.15mm, which can achieve sufficient welding quality and anti-corrosion performance and increase the welding bonding strength on the basis of good cost control. At the same time, the nickel-plated layer on the outer surface of the bending section 11 of the body 1 is an integral nickel-plated layer, and the thickness of the nickel-plated layer (not shown in the figure) is 0.5-2um, and the nickel-plated layer completely covers all the bending sections 11. The overall nickel plating can improve the corrosion resistance of the steel and facilitate the combination with the zinc-plated layer 2 to achieve a better welding effect. At the same time, the nickel content of the thinner nickel-plated layer is relatively lower than that of the traditional entire body 1 made entirely of nickel material, which significantly reduces the nickel cost.
[0037] Although different specific embodiments are mentioned in the content of this application, this application is not limited to the situations described in the industry standards or embodiments, etc. Some industry standards or slightly modified implementation plans based on the implementation of the custom methods or embodiments can also achieve the same, equivalent or similar, or predictable implementation effects after deformation of the above embodiments. The embodiments of data acquisition, processing, output, judgment methods, etc. after these modifications or deformations can still fall within the scope of the optional implementation plans of this application.
[0038] Although the present application has been described through embodiments, those skilled in the art will appreciate that there are many modifications and changes to the present application without departing from the spirit of the present application. It is intended that the attached embodiments include these modifications and changes without departing from the present application.
Claims
1. An electrical connecting sheet, characterized in that: include: The main body comprises at least two bent sections, at least one of the bent sections is provided with a nickel-plated layer and a zinc-plated layer covering the outside of the nickel-plated layer and used for welding, wherein the material of the main body is steel.
2. The electrical connecting sheet according to claim 1, characterized in that: The bent section provided with the galvanized layer is located at one end of the edge of the body.
3. The electrical connecting sheet according to claim 2, characterized in that: One of the bent sections includes a connecting section, and the connecting section is located at the other end of the edge of the body.
4. The electrical connecting sheet according to claim 1, characterized in that: The bending section provided with the galvanized layer includes a through hole.
5. The electrical connecting sheet according to claim 1, characterized in that: The main body also includes a bending groove, which is composed of at least two adjacent bending sections. The bending groove is arranged adjacent to the bending section where the galvanized layer is arranged. The bending groove protrudes toward the side of the surface to be welded, and the bending groove matches the edge of the surface to be welded.
6. The electrical connecting sheet according to claim 5, characterized in that: The protruding thickness of the bending groove is 1.75 mm, and the width of the bending groove is 6 mm.
7. The electrical connecting sheet according to claim 1, characterized in that: The steel thickness of the main body is 0.15 mm, and the specific material is 304 stainless steel.
8. The electrical connecting sheet according to claim 1, characterized in that: The thickness of the zinc coating is 2-5 um.
9. The electrical connecting sheet according to claim 1, characterized in that: All the bending sections are provided with a nickel-plated layer.