Heterojunction semiconductor device and method for fabricating a heterojunction semiconductor device

DE102016108911B4Inactive Publication Date: 2024-10-17DENSO CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102016108911
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-05-18
Filing Date
2016-05-13
Publication Date
2024-10-17
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A heterojunction semiconductor device comprising: a channel layer (14) comprising a first semiconductor; a barrier layer (16) provided on the channel layer (14) and comprising a semiconductor having a band gap larger than a band gap of the first semiconductor; a source electrode (24) and a drain electrode (26) provided on the barrier layer (16) and in ohmic contact with the barrier layer (16); and a p-type semiconductor layer (18) provided on the barrier layer (16), the p-type semiconductor layer (18) being provided in a region between the source electrode (24) and the drain electrode (26) on the barrier layer (16); characterized by an n-type semiconductor layer (20) provided on the p-type semiconductor layer (18);and a gate electrode (22) connected to the n-type semiconductor layer (20), wherein a connection surface between the p-type semiconductor layer (18) and the n-type semiconductor layer (20) has a concave-convex structure in which a concave portion (18a) of the p-type semiconductor layer (18) is embedded with a convex portion of the n-type semiconductor layer (20), and a concave portion of the n-type semiconductor layer (20) is embedded with a convex portion of the p-type semiconductor layer (18), wherein in a convex region of the p-type semiconductor layer (18) of the concave-convex structure, the p-type semiconductor layer (18) and the gate electrode (22) are connected to each other by an insulating layer (50);
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION1. Field of the InventionThe present invention relates to a heterojunction semiconductor device and a method for manufacturing a heterojunction semiconductor device.2. Description of Related ArtDisclosed is a nitride semiconductor device which is a heterojunction semiconductor element device in which a channel layer formed of gallium nitride (GaN) and a barrier layer formed of aluminum gallium nitride (AlGaN) are connected to each other. In this nitride semiconductor device, a p-type GaN layer, an n-type GaN layer, and a gate electrode are laminated on the barrier layer (see Japanese Patent Publication No. JP 2013-80 894 A).In the nitride semiconductor device according to the related art described above, the dopant concentration in the p-type GaN layer may be set to be high, so that the device is configured to be in an off state (normal off state) in a state where no voltage is applied to the gate electrode. In addition, the dopant concentration in the n-type GaN layer may be set to be high so that a contact resistance with the gate electrode is reduced.US 2005 / 0 189 559 A1 describes a semiconductor device having a first semiconductor layer, a second semiconductor layer having first conductivity or an undoped second semiconductor layer formed on the first semiconductor layer, a third semiconductor layer having second conductivity selectively formed on the second semiconductor layer, a gate electrode formed on the third semiconductor layer, a source electrode electrically connected to the second semiconductor layer, and a drain electrode electrically connected to the second semiconductor layer. The distance between the drain electrode and the third semiconductor layer is larger than the distance between the source electrode and the third semiconductor layer.The publication US 2012 / 0 193 637 A1 describes a further semiconductor structure.SUMMARY OF THE INVENTIONIn a case where the p-type GaN layer having a high dopant concentration and the n-type GaN layer having a high dopant concentration are connected to each other, a depletion region formed at an interface between the p-type GaN layer and the n-type GaN layer is narrowed. As a result, a leakage current flowing from the gate electrode to a source electrode may increase.It is an object of the invention to provide an improved heterojunction semiconductor device and a manufacturing method thereof. This object is achieved by a heterojunction semiconductor device according to claim 1 and a manufacturing method according to claim 6. Advantageous further developments are specified in the dependent claims.According to a first aspect, a heterojunction semiconductor device includes: a channel layer including a first semiconductor; a barrier layer provided on the channel layer and including a semiconductor having a band gap larger than a band gap of the first semiconductor; a source electrode and a drain electrode provided on the barrier layer and in ohmic contact with the barrier layer; a p-type semiconductor layer provided on the barrier layer, the p-type semiconductor layer being provided on the barrier layer in a region between the source electrode and the drain electrode; an n-type semiconductor layer provided on the p-type semiconductor layer; and a gate electrode connected to the n-type semiconductor layer. A connection surface between the p-type semiconductor layer and the n-type semiconductor layer has a concave-convex structure.In the first embodiment, the p-type semiconductor layer and the gate electrode are connected to each other through an insulating layer in a convex portion of the p-type semiconductor layer of the concave-convex structure.In the first embodiment, the gate electrode may be provided on an upper surface of the n-type semiconductor layer and a side surface of the n-type semiconductor layer.In the first configuration, a corner of the concave-convex structure may have a curved surface.In the first embodiment, the channel layer may be composed of GaN. The barrier layer may be composed of AlGaN. The p-type semiconductor layer may be composed of p-type GaN. The n-type semiconductor layer may be composed of n-type GaN.In the first aspect, a width of a groove in the concave-convex structure may be set such that a barrier layer spreads over an entire convex portion of the p-type semiconductor layer and an entire convex portion of the n-type semiconductor layer.A second aspect provides a method of manufacturing a heterojunction semiconductor device. The second aspect includes: a) forming a barrier layer on a channel layer, the channel layer including a first semiconductor, the barrier layer including a semiconductor having a band gap larger than a band gap of the first semiconductor; b) forming a source electrode and a drain electrode in ohmic contact with the barrier layer, the source electrode and the drain electrode being formed on the barrier layer; c) forming a p-type semiconductor layer on the barrier layer, the p-type semiconductor layer being provided between the source electrode and the drain electrode; d) processing a surface of the p-type semiconductor layer to form a concave-convex structure, the surface of the p-type semiconductor layer being opposite to a surface of the p-type semiconductor layer opposing the barrier layer; e) forming an n-type semiconductor layer on the p-type semiconductor layer, a connection surface of the n-type semiconductor layer with the p-type semiconductor layer having a concave-convex structure; and f) forming a gate electrode on the n-type semiconductor layer.The second aspect further includes g) forming an insulating layer on the p-type semiconductor layer during a period between the step c) and the step d).In the second aspect, the above-mentioned step d) includes processing the insulating layer and the p-type semiconductor layer so that the insulating layer and the p-type semiconductor layer form a concave-convex structure, the insulating layer covering a tip of a convex portion of the concave-convex portion.In the second aspect, the above step f) may include forming the gate electrode on an upper surface and a side surface of the n-type semiconductor layer.In the second aspect, the above-mentioned step d) may include processing a corner of the concavo-convex structure to have a curved surface.In the second embodiment, in the above-mentioned step d), a groove in the concave-convex structure may be processed to have a width in which a barrier layer spreads over an entire convex portion of the p-type semiconductor layer and an entire convex portion of the n-type semiconductor layer.According to the first and second aspects, a device having a normal-off property and a reduced leakage current can be provided.BRIEF DESCRIPTION OF THE DRAWINGSFeatures, advantages, and technical and industrial significance of an exemplary embodiment of the invention will be described below with reference to the accompanying drawings, in which like reference numerals denote like elements. The following are shown: FIG. 1 is a sectional view schematically showing a configuration of a heterojunction semiconductor device according to an example contributing to understanding of the invention; FIG. 2A is a diagram showing spreading of a depletion region at a gate of a heterojunction semiconductor device in a case where a concave-convex structure is not provided at a connection surface between a p-type semiconductor layer and an n-type semiconductor layer; FIG. 2B is a diagram showing the spreading of the depletion region at the gate of the heterojunction semiconductor device in a case where the concave-convex structure is not provided at the junction surface between the p-type semiconductor layer and the n-type semiconductor layer; FIG. 2C is a diagram showing the spreading of the depletion region at the gate of the heterojunction semiconductor device in a case where the concave-convex structure is not provided at the junction surface between the p-type semiconductor layer and the n-type semiconductor layer; FIG. 3A is a diagram showing the spreading of the depletion region at a gate of the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 3B is a diagram showing the spreading of the depletion region at the gate of the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 3C is a diagram showing the spreading of the depletion region at the gate of the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4A is a diagram showing a method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4B is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4C is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4D is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4E is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4F is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4G is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4H is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 4I is a diagram showing the method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 5 is a sectional view schematically showing a configuration of a heterojunction semiconductor device according to an embodiment; FIG. 6 is a diagram showing a method of manufacturing the heterojunction semiconductor device according to the embodiment; FIG. 7 is a sectional view schematically showing a configuration of a heterojunction semiconductor device according to an example contributing to understanding of the invention; FIG. 8 is a diagram showing a method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention; FIG. 9 is a sectional view schematically showing a configuration of a heterojunction semiconductor device according to another example contributing to understanding of the invention; and FIG. 10 is a diagram showing a method of manufacturing the heterojunction semiconductor device according to the other example contributing to understanding of the invention.DETAILED DESCRIPTION OF THE EMBODIMENT<Example contributing to understanding of the invention>As shown in FIG. 1, a heterojunction semiconductor device according to an example contributing to understanding the invention includes a substrate 10, a buffer layer 12, a channel layer 14, a barrier layer 16, a p-type semiconductor layer 18, an n-type semiconductor layer 20, a gate electrode 22, a source electrode 24, a drain electrode 26, and a protection layer 28.The channel layer 14 is a semiconductor layer that forms a heterojunction at an intersection with the barrier layer 16 described below. The channel layer 14 is formed of a semiconductor material having a high lattice match with the barrier layer 16. The thickness of the channel layer 14 is not specifically limited, and is preferably about several hundred nanometers.The channel layer 14 is formed on the substrate 10. The substrate 10 is formed of a material having a lattice constant and a thermal expansion coefficient similar to those of the channel layer 14, for example, silicon carbide, sapphire, aluminum nitride, aluminum gallium nitride, gallium nitride, or silicon. In addition, the buffer layer 12 may optionally be formed between the substrate 10 and the channel layer 14. The buffer layer 12 is provided to relax lattice mismatch between the substrate 10 and the channel layer 14. It is preferable that the buffer layer 12 is formed of a material having an average lattice constant between a lattice constant of the substrate 10 and a lattice constant of the channel layer 14. The buffer layer 12 may be formed as a single layer or a composite layer formed of, for example, gallium nitride (GaN), aluminum gallium nitride (AlGaN), aluminum nitride (AlN), indium gallium nitride (InGaN), or indium aluminum gallium nitride (InAlGaN).The barrier layer 16 is a semiconductor layer that is laminated on the channel layer 14 and forms a heterojunction at an intersection with the channel layer 14. The barrier layer 16 is formed of a semiconductor material having a band gap larger than a band gap of the channel layer 14 and having a high lattice matching with the channel layer 14. As a result, spontaneous polarization or piezoelectric polarization occurs at an intersection between the channel layer 14 and the barrier layer 16. Due to this polarization effect, a two-dimensional electron gas (2DEG) having a high carrier density (electron density) is generated at the interface between the channel layer 14 and the barrier layer 16.In addition, a two-dimensional electron gas (2DEG) may be generated by adding a dopant to the interface region between the channel layer 14 and the barrier layer 16 to perform δ-doping of the interface region. For example, in a case where the barrier layer 16 is formed of AlGaN, at least one of silicon (Si), germanium (Ge), and oxygen (O) may be used as an n-type dopant for δ doping.A combination of the channel layer 14 and the barrier layer 16 is not specifically limited as long as a hetero cut surface having high crystallinity is formed. For example, a Group III-V semiconductor composition including one or more Group III elements and one or more Group V elements, a Group II-VI semiconductor composition including one or more Group II elements and one or more Group VI elements, and a Group IV semiconductor including one or more Group IV elements may be appropriately selected and combined with each other. Examples of the combination of the barrier layer 16 and the channel layer 14 include AlGaN / GaN, AlGaAs / GaAs, AlN / GaN, InAlN / GaN, AlGaNP / GaNP, InAlGaAsP / InGaP, AlN / InN, and GaP / Si. For example, the channel layer 14 may be formed of i-type GaN, and the barrier layer 16 may be formed of i-type Al x Ga 1-x N. A stoichiometric composition ratio x of Al and Ga of the barrier layer 16 is not specifically limited. For example, in a high-power heterojunction semiconductor device, it is preferable that an average composition ratio x of the entire barrier layer 16 is 0.1 to 0.3.The p-type semiconductor layer 18 is provided on the barrier layer 16 in a region between the source electrode 24 and the drain electrode 26. The p-type semiconductor layer 18 is a semiconductor layer to which a p-type dopant is added. The thickness of the p-type semiconductor layer 18 is not specifically limited, but is preferably 50 nm to 300 nm (for example, 150 nm).For example, in a case where the p-type semiconductor layer 18 is formed of a group III-V semiconductor composition, examples of the group III-V semiconductor composition include a material obtained by adding a p-type dopant to gallium nitride (GaN), aluminum gallium nitride (AlGaN), aluminum nitride (AlN), indium gallium nitride (InGaN), indium aluminum gallium nitride (InAlGaN), or the like. Examples of the p-type dopant include magnesium (Mg). It is preferable that the dopant concentration in the p-type semiconductor layer 18 is higher than the dopant concentration in the channel layer 14.In the heterojunction semiconductor device according to the example, the p-type semiconductor layer 18 has a trench structure (concave-convex structure) in which a groove 18 ais formed in a depth direction. The width of the groove 18 ais not specifically limited, but is preferably 0.1 μm to 1 μm (for example, 0.5 μm). It is preferable that the depth of the groove 18a is set according to the thickness of the p-type semiconductor layer 18. The depth of the groove 18 ais not specifically limited, but is preferably 50 nm to 250 nm (for example, 100 nm).The width of the groove 18a may be adjusted such that a depletion region 30 spreads over the entire convex portion of the p-type semiconductor layer 18 and the entire convex portion of the n-type semiconductor layer 20. The width is determined in consideration of the semiconductor materials used, the dopant concentrations in the semiconductor material, and the depth of the trench. When the depletion layer 30 spreads over the entire convex portion of the p-type semiconductor layer 18 and the entire convex portion of the n-type semiconductor layer 20, the area of the depletion layer 30 corresponding to at least the depth of the groove 18 ain the concave-convex structure can be secured.The n-type semiconductor layer 20 is formed on the p-type semiconductor layer 18. In the heterojunction semiconductor device according to the example, the n-type semiconductor layer 20 is embedded in the groove 18a provided in the p-type semiconductor layer 18. That is, a connection surface between the p-type semiconductor layer 18 and the n-type semiconductor layer 20 has a concave-convex structure. More specifically, in the connection surface between the p-type semiconductor layer 18 and the n-type semiconductor layer 20, a concave portion (groove 18 a) of the p-type semiconductor layer 18 is embedded with a convex portion of the n-type semiconductor layer 20, and a concave portion of the n-type semiconductor layer 20 is embedded with a convex portion of the p-type semiconductor layer 18. The sum of the thickness of the n-type semiconductor layer 20 and the thickness of the p-type semiconductor layer 18 is preferably 50 nm to 300 nm (for example, 150 nm).For example, in a case where the n-type semiconductor layer 20 is formed of a group III-V semiconductor composition, examples of the group III-V semiconductor composition include a material obtained by adding a p-type dopant to gallium nitride (GaN), aluminum gallium nitride (AlGaN), aluminum nitride (AlN), indium gallium nitride (InGaN), indium aluminum gallium nitride (InAlGaN), or the like. Examples of the n-type dopant include selenium (Se), silicon (Si), germanium (Ge), and oxygen (O). It is preferable that the dopant concentration in the n-type semiconductor layer 20 is higher than the dopant concentration in the channel layer 14.The gate electrode 22 is formed on the n-type semiconductor layer 20. It is preferable that the gate electrode 22 is formed of metal, metal silicide and an alloy thereof. For example, although not limited thereto, it is preferable that the gate electrode 22 includes at least one element selected from a group consisting of aluminum (Al), molybdenum (Mo), gold (Au), nickel (Ni), platinum (Pt), titanium (Ti), palladium (Pd), iridium (Ir), rhodium (Rh), cobalt (Co), tungsten (W), tantalum (Ta), copper (Cu), and zinc (Zn). The gate electrode 22 may be formed on the n-type semiconductor layer 20 by sputtering, vacuum-based vapor deposition, or the like using a well-known mask technique such as photolithography.The source electrode 24 and the drain electrode 26 are electrodes for supplying a current to the heterojunction semiconductor device. The source electrode 24 and the drain electrode 26 are provided on the barrier layer 16 to form an ohmic connection with the barrier layer 16. It is preferable that the source electrode 24 and the drain electrode 26 are formed of metal, metal silicide and an alloy thereof. For example, although not limited thereto, it is preferable that the source electrode 24 and the drain electrode 26 include at least one selected from a group consisting of aluminum (Al), molybdenum (Mo), gold (Au), nickel (Ni), platinum (Pt), titanium (Ti), palladium (Pd), iridium (Ir), rhodium (Rh), cobalt (Co), tungsten (W), tantalum (Ta), copper (Cu), and zinc (Zn). For example, the source electrode 24 and the drain electrode 26 may have a layered structure of titanium (Ti) / aluminum (Al) / nickel (Ni) or a layered structure of titanium (Ti) / aluminum-copper (AlCu). In a case where the barrier layer 16 is formed of another semiconductor material, the source electrode 24 and the drain electrode 26 may be formed of a material selected from materials capable of forming ohmic connection with the semiconductor material. The source electrode 24 and the drain electrode 26 may be formed on appropriate regions on the barrier layer 16 by sputtering, vacuum-based vapor deposition, or the like using a well-known mask technique such as photolithography.The protection layer 28 is provided to protect a surface of the barrier layer 16. The protection layer 28 is provided in a region of the surface of the barrier layer 16 in which the gate electrode 22, the source electrode 24, and the drain electrode 26 are not provided. For example, in a case where the barrier layer 16 is formed of AlGaN, the protection layer 28 may be formed of a material selected from silicon oxide (SiO 2), silicon nitride (SiN), aluminum oxide (Al 2 O 3) and the like. In a case where the barrier layer 16 is formed of another semiconductor material, the protective layer 28 may be formed of a material having a greater chemical and mechanical stability than the barrier layer 16. By forming the protective layer 28, the surface of the barrier layer 16 can be chemically and mechanically protected, and the interface state density at an interface with the barrier layer 16 can be reduced.By applying a voltage between the source electrode 24 and the drain electrode 26 and applying a voltage to the gate electrode 22 in the heterojunction semiconductor device according to the example, a current flows between the source electrode 24 and the drain electrode 26. By changing the voltage applied to the gate electrode 22, the current flowing between the source electrode 24 and the gate electrode 26 can be controlled.Here, by providing the p-type semiconductor layer 18 and the n-type semiconductor layer 20 under the gate electrode 22, a current can be controlled not to flow between the source electrode 24 and the drain electrode 26 in a state where no voltage is applied to the gate electrode 22. That is, the heterojunction semiconductor device according to the example serves as a normal-off heterojunction semiconductor device.Here, as shown in FIG. 2A, in a case where it is assumed that the p-type semiconductor layer 18 does not have a trench structure, the spreading of the depletion region at the intersection between the p-type semiconductor layer 18 and the n-type semiconductor layer 20 during the application of a voltage to the gate electrode 22 will be discussed. As the voltage applied to the gate electrode 22 increases, the depletion region 30 spreads at the intersection between the p-type semiconductor layer 18 and the n-type semiconductor layer 20, as shown in FIGS. 2B and 2C. At this time, in a case where the dopant concentration in the p-type semiconductor layer 18 is set to be high to realize the normal off state and where the dopant concentration in the n-type semiconductor layer 20 is set to be high to reduce contact resistance with the gate electrode 22, the width of the depletion region 30 at the intersection between the p-type semiconductor layer 18 and the n-type semiconductor layer 20 is narrowed, and the amount of leakage current between the gate electrode 22 and the source electrode 24 increases.Here, as shown in FIG. 3A, in a case where it is assumed that the p-type semiconductor layer 18 has a trench structure, the spreading of the depletion region at the intersection between the p-type semiconductor layer 18 and the n-type semiconductor layer 20 during the application of a voltage to the gate electrode 22 will be discussed. As the voltage applied to the gate electrode 22 increases, the depletion region 30 spreads at the intersection between the p-type semiconductor layer 18 and the n-type semiconductor layer 20, as shown in FIGS. 3B and 3C. At this time, even if the impurity concentrations in the p-type semiconductor layer 18 and the n-type semiconductor layer 20 are set to be high, the amount of leakage current between the gate electrode 22 and the source electrode 24 can be reduced. This is because since the connection area of the intersection between the p-type semiconductor layer 18 and the n-type semiconductor layer 20 is large, the width of the depletion region 30 is wider than in the structure shown in FIGS. 2A to 2C in which no concavo-convex structure is provided.(Production Method)A method of manufacturing the heterojunction semiconductor device according to the example contributing to understanding of the invention will be described below with reference to Figs. 4A to 4I.In step S 10, as shown in FIG. 4A, the buffer layer 12, the channel layer 14, and the barrier layer 16 are formed on the substrate 10. The buffer layer 12, the channel layer 14, and the barrier layer 16 may be formed using a well-known method such as metal organic chemical vapor deposition (MOCVD) or molecular beam epitaxy (MBE). Raw materials (raw material gases) and film forming conditions used in the MOCVD or the MBE may be appropriately selected according to the semiconductor materials constituting the buffer layer 12, the channel layer 14, and the barrier layer 16.For example, in order to form the channel layer 14 using GaN and form the barrier layer 16 using AlGaN, the channel layer 14 and the barrier layer 16 may be formed by the MOCVD using ammonia gas, trimethylaluminium (TMA), and trimethylgallium (TMG). In order to change the composition ratio x of the channel layer 14 and the barrier layer 16, a ratio of the supply flow rates of ammonia gas, TMA, and TMG may be changed appropriately in consideration of a relationship to the substrate temperature, the raw material supply pressure, and the film formation time, so that the channel layer 14 and the barrier layer 16 have a desired composition ratio x. When the buffer layer 12, the channel layer 14, and the barrier layer 16 are formed of other semiconductor materials, a well-known film forming method may be used to form the layers.In step S 12, as shown in FIG. 4B, the p-type semiconductor layer 18 is formed on the barrier layer 16. In the following description for the steps, the substrate 10, the buffer layer 12, and the channel layer 14 are not shown in the drawing. To form the p-type semiconductor layer 18 using GaN, the p-type semiconductor layer 18 may be formed by the MOCVD using ammonia gas and trimethylgallium (TMG) while adding magnesium (Mg) as a dopant. The p-type semiconductor layer 18 may be formed on the entire surface of the barrier layer 16.In step S 14, as shown in FIG. 4C, the p-type semiconductor layer 18 is etched such that the p-type semiconductor layer 18 remains on the barrier layer 16 only in a gate region. Using a photolithography technique, a resist 32 is formed only in a gate forming region, and the p-type semiconductor layer 18 is etched over the resist 32 as a mask. For the etching of the p-type semiconductor layer 18, either dry etching or wet etching may be used. For example, the p-type semiconductor layer 18 may be etched using reactive ion etching using a chlorine gas plasma. After the etching is completed, the resist 32 is removed.In step S16, as shown in FIG. 4D, the groove 18a of the concavo-convex structure, which is the trench, is formed at the p-type semiconductor layer 18. Using a photolithography technique, a resist 34 is formed in a region of the p-type semiconductor layer 18 excluding a region for forming the groove 18a, and the p-type semiconductor layer 18 is etched over the resist 34 as a mask. For the etching of the p-type semiconductor layer 18, either dry etching or wet etching may be used as in the case of step S 14. After the etching is completed, the resist 34 is removed.In step S 18, as shown in FIG. 4E, the n-type semiconductor layer 20 is formed. To form the n-type semiconductor layer 20 using GaN, the n-type semiconductor layer 20 may be formed by the MOCVD using ammonia gas and trimethylgallium (TMG) while adding selenium (Se) as a dopant. The n-type semiconductor layer 20 may be formed on the entire surface of the barrier layer 16 and the p-type semiconductor layer 18. As a result, the n-type semiconductor layer 20 is embedded in the groove 18a of the trench structure formed on the p-type semiconductor layer 18.In step S 20, as shown in FIG. 4F, the n-type semiconductor layer 20 is etched such that the n-type semiconductor layer 20 remains only in the gate region. Using a photolithography technique, a resist 36 is formed only in the gate region, and the n-type semiconductor layer 20 is etched over the resist 36 as a mask. For the etching of the n-type semiconductor layer 20, either dry etching or wet etching may be used as in the case of step S 14. After the etching is completed, the resist 36 is removed.In step S22, as shown in FIG. 4G, the gate electrode 22 is formed. Using a photolithography technique, a resist 38 is formed in a region excluding the gate region, and the gate electrode 22 is etched over the resist 38 as a mask. The gate electrode 22 may be formed by sputtering or vacuum-based vapor deposition using a metal, a metal silicide, or an alloy thereof as a target or a vapor deposition source. After completion of the formation of the gate electrode 22, the resist 38 is removed.In step S 24, as shown in FIG. 4H, the source electrode 24 and the drain electrode 26 are formed. Using a photolithography technique, a resist 40 is formed in a region excluding the region of the source electrode 24 and the drain electrode 26, and the source electrode 24 and the drain electrode 26 are formed over the resist 40 as a mask. The source electrode 24 and the drain electrode 26 may be formed by sputtering or vacuum-based vapor deposition using metal, a metal silicide, or an alloy thereof as a target or a vapor deposition source. After completion of the formation of the source electrode 24 and the drain electrode 26, the resist 40 is removed.In step S 26, as shown in FIG. 4I, the protection layer 28 is formed in a region excluding the gate electrode 22, the source electrode 24, and the drain electrode 26. The protective layer 28 may be formed by sputtering using a material such as silicon oxide (SiO 2), silicon nitride (SiN), or aluminum oxide (Al 2 O 3), for example.By the steps described above, the heterojunction semiconductor device according to the example contributing to understanding of the invention can be manufactured.<>As shown in FIG. 5, a heterojunction semiconductor device according to an embodiment includes an insulating layer 50 formed on the p-type semiconductor layer 18 of the heterojunction semiconductor device according to the example contributing to understanding of the invention. Configurations different from the insulating layer 50 are the same as those of the heterojunction semiconductor device according to the example contributing to understanding of the invention. Accordingly, the components are represented by the same reference numerals as in the first example contributing to understanding of the invention, and description thereof will not be repeated.The insulating layer 50 is provided between a tip end of the convex portion of the trench structure of the p-type semiconductor layer 18 and the gate electrode 22. The convex portion has a shorter distance from the gate electrode 22 than the concave portion, and has a surface where the gate electrode 22 and the p-type semiconductor layer 18 are opposed to each other. In the convex region, for example, the distance between the gate electrode 22 and the p-type semiconductor layer 18 is 50 nm or less. Although not limited thereto, the insulating layer 50 may be formed of a material such as silicon oxide (SiO 2), silicon nitride (SiN), or aluminum oxide (Al 2 O 3), for example. The thickness of the insulating layer 50 is not specifically limited, but is preferably 10 nm to 100 nm.As shown in FIG. 6, the insulating layer 50 may be formed only on the tip end portion of the trench structure of the p-type semiconductor layer 18 using a method including: providing a step S 13 of forming the insulating layer 50 on the p-type semiconductor layer 18 during a period between the steps S 12 and S 14; and etching the insulating layer 50 using the same method as for the p-type semiconductor layer 18 in the steps S 14 and S 16.In a heterojunction semiconductor device according to a related art technique, in a case where a high voltage of static electricity or the like is directly applied to the gate electrode 22, the depletion region can reach the gate electrode 22 after spreading between the gate electrode 22 and the tip end portion of the trench structure of the p-type semiconductor layer 18, in other words, to the surface where the gate electrode 22 and the p-type semiconductor layer 18 oppose each other in the convex region of the p-type semiconductor layer 18. In such a case, a high current may flow through the gate portion and destroy the device. In the heterojunction semiconductor device according to the embodiment, the insulating layer 50 is provided between the gate electrode 22 and the tip end portion of the trench structure of the p-type semiconductor layer 18. Consequently, the spreading of the depletion zone is prevented in this region. Accordingly, the destruction of the gate caused by the application of a high voltage of static electricity or the like can be reduced.The junction area between the gate electrode 22 and the n-type semiconductor layer 20 is reduced, and a leakage current flowing through the gate electrode 22 can be reduced.<Example contributing to understanding of the invention>In a heterojunction semiconductor device according to an example contributing to understanding of the invention, as shown in FIG. 7, the gate electrode 22 is provided on an upper surface and a side surface of the n-type semiconductor layer 20 of the heterojunction semiconductor device according to the example contributing to understanding of the invention. Configurations different from the formation region of the gate electrode 22 are the same as those of the heterojunction semiconductor device according to the example contributing to understanding of the invention. Accordingly, the components are represented by the same reference numerals as in the example contributing to understanding of the invention, and description thereof will not be repeated.As shown in FIG. 8, the gate electrode 22 may be formed using a method including: forming the photoresist 38 as an opening in a portion of the upper surface and the side surface of the n-type semiconductor layer 20 in a step S 22; and forming the gate electrode 22 over the photoresist 38 as a mask by sputtering or vacuum-based vapor deposition using metal, metal silicide, or an alloy thereof. At this time, in order to form the gate electrode 22 having a sufficient thickness at the side surface of the n-type semiconductor layer 20, it is preferable that sputtering or vacuum-based vapor deposition may be applied while the substrate 10 is rotated in a state of being inclined with respect to a target or a vapor deposition source.In the heterojunction semiconductor device according to the example contributing to understanding of the invention, the gate electrode 22 is provided up to the side surface of the n-type semiconductor layer 20, and thus the junction area between the gate electrode 22 and the n-type semiconductor layer 20 can be widened. Accordingly, heat dissipation in the gate electrode 22 is improved. As a result, even in a case where a high voltage of static electricity or the like is applied to the gate electrode 22 and a high current flows through the gate electrode 22, the destruction of the device caused by the melting of the gate electrode 22 or the like can be suppressed.<Weiteres Example Contributing to Understanding of Invention>In a heterojunction semiconductor device according to another example contributing to understanding of the invention, as shown in FIG. 9, a corner 18b of the trench structure of the p-type semiconductor layer 18 has a curved surface. Configurations different from the shape of the p-type semiconductor layer 18 are the same as those of the heterojunction semiconductor device according to the example contributing to understanding of the invention. Accordingly, the components are represented by the same reference numerals as in the example contributing to understanding of the invention, and description thereof will not be repeated.As shown in FIG. 10, in the p-type semiconductor layer 18, the corner 18 bof the trench structure may be processed to be a curved surface using a method including: forming the groove 18 aof the trench structure in step S 16 to form the trench structure; and isotropically etching the groove 18 a.In the heterojunction semiconductor device according to the other example contributing to understanding of the invention, when a voltage is applied to the gate electrode 22, an electric field is not concentrated at the corner 18b of the trench structure of the p-type semiconductor layer 18. In addition, in a case where a high voltage is applied to the gate electrode 22, the destruction of the gate can be suppressed.A suitable combination of the configurations of the heterojunction semiconductor devices according to the embodiment and the examples contributing to understanding of the invention can be applied.The applicable range of the embodiment of the invention is not limited to a heterojunction field effect transistor (HJFET). The embodiment can be applied to any heterojunction semiconductor devices in which a current is controlled by a gate.A heterojunction semiconductor device comprising: a channel layer (14) comprising a first semiconductor; a barrier layer (16) provided on the channel layer (14) and comprising a semiconductor having a band gap larger than a band gap of the first semiconductor; a source electrode (24) and a drain electrode (26) provided on the barrier layer (16) and in ohmic contact with the barrier layer (16); a p-type semiconductor layer (18) provided on the barrier layer (16), the p-type semiconductor layer (18) being provided on the barrier layer (16) in a region between the source electrode (24) and the drain electrode (26); an n-type semiconductor layer (20) provided on the p-type semiconductor layer (18); and a gate electrode (22) connected to the n-type semiconductor layer (20). A connection surface between the p-type semiconductor layer (18) and the n-type semiconductor layer (20) has a concave-convex structure.

Claims

A heterojunction semiconductor device comprising: a channel layer (14) comprising a first semiconductor; a barrier layer (16) provided on the channel layer (14) and comprising a semiconductor having a band gap larger than a band gap of the first semiconductor; a source electrode (24) and a drain electrode (26) provided on the barrier layer (16) and in ohmic contact with the barrier layer (16); and a p-type semiconductor layer (18) provided on the barrier layer (16), wherein the p-type semiconductor layer (18) is provided on the barrier layer (16) in a region between the source electrode (24) and the drain electrode (26); characterized by an n-type semiconductor layer (20) provided on the p-type semiconductor layer (18); and a gate electrode (22) connected to the n-type semiconductor layer (20), wherein a connection surface between the p-type semiconductor layer (18) and the n-type semiconductor layer (20) has a concave-convex structure in which a concave portion (18a) of the p-type semiconductor layer (18) is embedded with a convex portion of the n-type semiconductor layer (20) and a concave portion of the n-type semiconductor layer (20) is embedded with a convex portion of the p-type semiconductor layer (18), wherein in a convex portion of the p-type semiconductor layer (18) of the concave-convex structure, the p-type semiconductor layer (18) and the gate electrode (22) are connected to each other by an insulating layer (50).The heterojunction semiconductor device according to claim 1, characterized in that the gate electrode (22) is provided on an upper surface of the n-type semiconductor layer (20) and a side surface of the n-type semiconductor layer (20).The heterojunction semiconductor device according to claim 1 or 2, characterized in that a corner (18b) of the concave-convex structure has a curved surface.The heterojunction semiconductor device according to any one of claims 1 to 3, characterized in that said channel layer (14) is composed of GaN, said barrier layer (16) is composed of AlGaN, said p-type semiconductor layer (18) is composed of p-type GaN, and said n-type semiconductor layer (20) is composed of n-type GaN.The heterojunction semiconductor device according to any one of claims 1 to 4, characterized in that a width of a groove (18a) in the concave-convex structure is set such that a barrier layer (30) spreads over an entire convex portion of the p-type semiconductor layer (18) and an entire convex portion of the n-type semiconductor layer (20).A method of manufacturing a heterojunction semiconductor device, comprising: a) forming a barrier layer (16) on a channel layer (14), the channel layer (14) comprising a first semiconductor, the barrier layer (16) comprising a semiconductor having a band gap larger than a band gap of the first semiconductor; b) forming a source electrode (24) and a drain electrode (26) in ohmic contact with the barrier layer (16), the source electrode (24) and the drain electrode (26) being formed on the barrier layer (16); c) forming a p-type semiconductor layer (18) on the barrier layer (16), the p-type semiconductor layer (18) being provided between the source electrode (24) and the drain electrode (26); d) processing a surface of the p-type semiconductor layer (18) to form a concave-convex structure, the surface of the p-type semiconductor layer (18) being opposite to a surface of the p-type semiconductor layer (18) opposite to the barrier layer (16); e) forming an n-type semiconductor layer (20) on the p-type semiconductor layer (18), a connection surface of the n-type semiconductor layer (20) with the p-type semiconductor layer (18) having a concave-convex structure; f) forming a gate electrode (22) on the n-type semiconductor layer (20); and g) forming an insulating layer (50) on the p-type semiconductor layer (18) during a period between step c) and step d).The method for manufacturing a heterojunction semiconductor device according to claim 6, characterized in that the step d) comprises processing the insulating layer (50) and the p-type semiconductor layer (18) so that the insulating layer (50) and the p-type semiconductor layer (18) form a concave-convex structure, the insulating layer (50) covering a tip of a convex portion of the concave-convex structure.The method for manufacturing a heterojunction semiconductor device according to claim 6 or 7, characterized in that the step f) comprises forming the gate electrode on an upper surface and a side surface of the n-type semiconductor layer.The method for manufacturing a heterojunction semiconductor device according to any one of claims 6 to 8, characterized in that the step d) comprises processing a corner (18b) of the concave-convex structure to have a curved surface.The method for manufacturing a heterojunction semiconductor device according to any one of claims 6 to 9, characterized in that in the step d), a groove (18a) in the concave-convex structure is processed to have a width in which a barrier layer (30) spreads over an entire convex portion of the p-type semiconductor layer (18) and an entire convex portion of the n-type semiconductor layer (20).

Citation Information

Patent Citations

  • Nitride semiconductor element and manufacturing method of the same

    JP2013080894A

  • Semiconductor device

    US20050189559A1

  • Low gate-leakage structure and method for gallium nitride enhancement mode transistor

    US20120193637A1

  • JP002013080894A