Semiconductor devices with germanium-rich active layers and doped junction layers

By integrating a δ-doped p-type semiconductor junction layer between Ge and silicon substrates, the etch selectivity of SiGe layers is enhanced, enabling precise scaling and formation of Ge-rich nanowires and nanoribbons in transistors, addressing the etching challenges and maintaining material performance.

DE112013005622B4Inactive Publication Date: 2024-11-07INTEL CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE112013005622
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2012-12-17
Filing Date
2013-06-14
Publication Date
2024-11-07
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The challenge in using germanium (Ge) in modern transistor designs is the difficulty in etching SiGe layers with sufficient selectivity versus Ge, which often leads to erosion of finely printed Ge features, diluting material-based performance gains in aggressively scaled transistors.

Method used

Incorporating a doped p-type semiconductor junction layer between the Ge-rich device layer and the silicon substrate to enhance etch selectivity, utilizing a δ-doped p-type buried layer that modulates galvanic processes and reduces Ge etching, thereby preserving fine Ge-rich nanowire geometries.

Benefits of technology

The solution provides improved etch selectivity and durability of Ge-rich device layers, allowing precise scaling and formation of fine Ge features in transistors, such as nanowires and nanoribbons, with minimal subchannel leakage and enhanced material performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Semiconductor component stack (100), comprising: a germanium(Ge)-rich component layer (108A;208A;308A) provided over a silicon(Si) substrate (104;304); a SiGe transition layer (107C;207C;307C) provided above the substrate (104;304) and below the component layer (108A;208A;308A); a δ-doped SiGe layer (107B;207C;307C) of the p-type provided above the substrate (104;304) and below the transition layer (107C;207C;307C); a SiGe layer (107A;207A;307A) of n-type provided above the substrate (104;304) and below the δ-doped SiGe layer (107B;207B;307B) of p-type; and one or more SiGe buffer layer(s) of n type provided above the substrate (104;304) and below the SiGe layer (107A;207A;307A) (106A; 106B;306A;306B).
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The embodiments of the invention belong to the field of semiconductor devices, and in particular to the field of semiconductor devices with germanium (Ge) active layers. BACKGROUND

[0002] For several decades, feature scaling in integrated circuits has enabled increased densities of functional units on a semiconductor chip. For example, reducing transistor size allows for the integration of a larger number of memory devices on a chip, leading to the production of products with increased capacity.

[0003] In the fabrication of field-effect transistors (FETs) for integrated circuit devices, crystalline semiconducting materials other than silicon can be advantageous. An example of such a material is Ge, which offers several potentially advantageous features compared to silicon, including, but not limited to, high charge carrier (hole) mobility, band gap offset, a different lattice constant, and the ability to alloy with silicon to form semiconducting binary alloys of SiGe.

[0004] One problem with the use of Ge in modern transistor designs is that the extremely fine features (e.g., 22 nm and below) now achieved for silicon FETs, which have been aggressively scaled over the years, are now difficult to achieve in Ge, often diluting potential material-based performance gains when implemented in less aggressively scaled forms. The difficulty in scaling is related to the material properties of Ge, and more specifically, the difficulty in etching SiGe, which is often used as an interlayer between a Ge active layer (e.g., transistor channel layer) and an underlying silicon substrate material, with sufficient selectivity to Ge to remove the SiGe without eroding a finely printed Ge active layer feature.

[0005] Material stacking architectures and etching techniques that selectively enable high SiGe:Ge etching are therefore advantageous. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] US 7 145 167 B1, KR 10 2011 0 025 075 A, US 2009 / 0 085 027 A1 and KR 10 1998 0 083 547 A concern printed documents on the relevant prior art. BRIEF DESCRIPTION OF THE DRAWINGS Fig. 1A illustrates a cross-sectional view of a semiconductor layer stack including a germanium device layer provided over a delta-doped p-type junction layer, in accordance with an embodiment of the present invention; Fig. 1B illustrates a graphical representation of the dopant concentration depth profile of a semiconductor layer stack including a delta-doped p-type transition layer in accordance with an embodiment of the present invention; Fig. 2A and Fig. 2B illustrate cross-sectional views of a local growth of the Fig. 2A in accordance with an embodiment of the present invention; Fig. 3A and Fig. 3B illustrate cross-sectional views in the fabrication of a planar semiconductor device using the semiconductor stack of Fig. 1A in accordance with another embodiment of the present invention; Fig. 4A - 4C illustrate oblique views showing various operations in a method for manufacturing non-planar semiconductor devices using the semiconductor stack of Fig. 1A in accordance with embodiments of the present invention; Fig. Figure 5A illustrates an isometric cross-sectional view of a nanowire or nanoribbon semiconductor device using the semiconductor stack of Fig. 1A in accordance with an embodiment of the present invention; Fig. Figure 5B illustrates a channel cross-sectional view of the nanowire-based semiconductor structure of Fig. 5A in accordance with an embodiment of the present invention; Fig. Figure 5C illustrates a cross-sectional view of the nanowire-based semiconductor structure of Fig. 5A in accordance with an embodiment of the present invention; Fig. 6A-6D illustrate isometric cross-sectional views representing various operations in a method of fabricating a nanowire semiconductor device having, at least at one point in the process, a germanium device layer provided over a p-doped junction layer in accordance with an embodiment of the present invention; and Fig. 7 illustrates a computer device in accordance with an implementation of the invention. DETAILED DESCRIPTION

[0007] Semiconductor devices having Ge-rich active layers provided over doped semiconductor junction layers are described. In the following description, numerous details are set forth. However, it will be apparent to one skilled in the art that the present invention may be practiced without these specific details. In some instances, well-known methods and devices are shown in block diagram form rather than in detail to avoid obscuring the present invention. Reference throughout the specification to "one embodiment" means that a particular feature, structure, function, or characteristic described in connection with the embodiment is included in at least one embodiment of the invention.Thus, the appearance of the phrase "in one embodiment" in various places throughout the specification does not necessarily refer to the same embodiment of the invention. Moreover, the particular features, structures, functions, or characteristics may be combined in any suitable manner in one or more embodiments. For example, a first embodiment may be combined with a second embodiment wherever the two embodiments are not mutually exclusive.

[0008] The terms "coupled" and "connected," along with their derivatives, may be used herein to describe structural relationships between components. It should be understood that these terms are not intended to be synonyms. Rather, in particular embodiments, "connected" may be used to indicate that two or more elements are in direct physical or electrical contact with each other. "Coupled" may be used to indicate that two or more elements are in direct or indirect (with other intervening elements) physical or electrical contact with each other, and / or that the two or more elements cooperate or interact with each other (e.g., as in a cause / effect relationship).

[0009] The terms "over," "under," "between," and "on," as used herein, refer to a relative position of one material layer or component with respect to other layers or components. For example, a layer provided over (above) or under another layer may be in direct contact with the other layer or may have one or more intervening layers. Furthermore, a layer provided between two layers may be in direct contact with the two layers or may have one or more intervening layers. In contrast, a first layer "on" a second layer is in direct contact with that second layer. Likewise, unless expressly stated otherwise, a feature provided between two features may be in direct contact with the adjacent features or may have one or more intervening features.

[0010] One or more embodiments described herein utilize germanium-on-silicon (Ge-on-Si) substrate device architectures that further utilize a transition layer disposed between a Ge-rich device layer and a Si substrate that is doped to improve the resistance of the Ge-rich device layer to etchants used to remove other semiconductor layers of a device stack composed of relatively less Ge than the device layer.

[0011] In some embodiments, a doped p-type semiconductor junction layer is provided between a Ge-rich device layer and a Si substrate. Such arrangements can be used in the formation of germanium-based transistors as planar devices, fin- or tri-gate-based devices, and gate-all-around devices (e.g., nanowire devices). More specifically, one or more embodiments are directed to performing delamination of rectangular-shaped Ge-containing nanowires or nanoribbons from Ge / SiGe, Ge / Si, SiGe / SiGe, or SiGe / Si multilayer stacks.

[0012] One or more embodiments described herein benefit from a δ-doped p-type buried semiconductor layer to increase the resistance of an overlying Ge-rich device layer to certain wet etchants useful for removing other materials from the semiconductor device stack, such as one or more SiGe (or pure Si) layers with a relatively lower Ge content (i.e., richer in Si than the device layer), thereby improving etch process selectivity to a device layer of either pure Ge or a more Ge-rich SiGe. In some embodiments, the presence of the doped p-type buried layer has been found to increase the resistance of a Ge-rich device layer to wet SiGe etchants used during undercutting of the Ge device layer and / or stripping processes (e.g.,for gate-all-around or nanowire / nanoribbon devices), thereby preserving fine Ge-rich nanowire geometries.

[0013] The inventors discovered that for certain wet etchants sensitive to the oxidation state of surface atoms in an exposed Ge layer (or SiGe layer, which is relatively richer in Ge), Ge dissolution can be dramatically reduced with the introduction of a buried p-type doped semiconductor layer into a semiconductor film stack. While not bound by theory, the improved etch resistance of the Ge-rich device layer(s) is currently attributed, at least in part, to galvanic coupling between the Ge-rich device layer and the buried p-type doped layer, whereby the charges and electronic states within the Ge-rich device layer are modulated by those in the doped p-type buried layer, thereby altering galvanic processes that affect Ge dissolution.Where the material layers between the Ge-rich device layer exposed to the etchant and the buried p-type doped layer are undoped (i.e., the intrinsically doping concentration), the p-type doped layer can be recessed below the device layers (e.g., 50-100 nm or more) and still suppress etching of the overlying Ge-rich semiconductor device layer when exposed to, for example, a wet SiGe etchant.

[0014] In one or more embodiments, the δ-doped p-type buried layer is provided above an n-type subchannel leakage suppression layer of the semiconductor device stack, which may also be a δ-doped layer. Where the p-type doped layer is provided above a doped n-type leakage suppression layer, the plates of doped material may form a doping dipole. Rectifying characteristics associated with conduction band discontinuities resulting from the doping dipole may also play a role in the observed Ge etch suppression. With the material layers between the Ge-rich device layer and the buried doped p-type layer being undoped (e.g.,Intrinsic), Ge etch suppression can also be achieved with a δ-doped p-type doped layer having a dopant concentration that ensures that mobile charge is fully consumed by the underlying n-type doped leakage suppression layer, so that the presence of the p-type doped layer does not detrimentally increase subchannel leakage between a source and drain of a FET device. In some embodiments, a δ-doped p-type buried layer can undergo migration / diffusion and expand to more than 15 nm during thermal processing (e.g., following a selective etch of SiGe over Ge), but still not completely compensate for n-type dopants in the leakage suppression layer, enabling both Ge etch suppression during fabrication and leakage suppression in the completed FET device.

[0015] Fig. 1A illustrates a cross-sectional view of a semiconductor layer stack 100 including a Ge device layer provided over a delta-doped junction layer, in accordance with an embodiment of the present invention. As shown, the semiconductor device stack 100 includes a germanium (Ge)-based device layer stack 108 (such as a compressively strained germanium layer) grown over a silicon (Si) substrate 104 (e.g., as part of a silicon wafer).

[0016] The substrate 104 may be constructed of any semiconductor material that can withstand fabrication and serve as a seed layer for the crystalline growth of the semiconductor layers in the stack 100. In one embodiment, the substrate 104 is a bulk substrate, such as a P-type silicon substrate commonly used in the semiconductor industry. In one embodiment, the substrate 104 is constructed of a crystalline silicon, silicon / germanium, or germanium layer doped with a charge carrier, such as, but not limited to, phosphorus, arsenic, boron, or a combination thereof. In one embodiment, the concentration of silicon atoms in the substrate 104 is greater than 97%, or alternatively, the concentration of dopant atoms is less than 1%. In another embodiment, the substrate 104 is constructed of an epitaxial layer grown on top of a standalone crystalline substrate, e.g.,an epitaxial silicon layer grown on top of a boron-doped monocrystalline bulk silicon substrate. The substrate 104 may also include an insulating layer provided between a bulk crystal substrate and an epitaxial layer, for example, to form a silicon-on-insulator substrate. In one embodiment, the insulating layer is composed of a material such as, but not limited to, silicon dioxide, silicon nitride, silicon oxynitride, or a high-k dielectric layer. The substrate 104 may alternatively be composed of a Group III-V material. In one embodiment, the substrate 104 is composed of a III-V material such as, but not limited to, gallium nitride, gallium phosphide, gallium arsenide, indium phosphide, indium antimonide, indium gallium arsenide, aluminum gallium arsenide, indium gallium phosphide, or a combination thereof.In another embodiment, the substrate 104 is constructed of a III-V material and charge carrier dopant impurity atoms such as, but not limited to, carbon, silicon, germanium, oxygen, sulfur, selenium, or tellurium.

[0017] The Ge-rich device layer stack 108 may include one or more Ge device layers, with only a first Ge-rich device layer 108A formed in Fig. 1A. In an exemplary embodiment, the thickness of the Ge-rich device layer 108A is in the range of 5 - 15 nm and is composed essentially of pure Ge (i.e., some impurities at the intrinsic level may be present). A silicon-germanium (SiGe) buffer layer stack 106 is provided between a Si substrate 104 and the Ge-rich device layer stack 108 (e.g., further comprising a first layer 106A of approximately 0.5 - 1 µm Si 0,7 Ge 0,3and a second layer 106B consisting of approximately 0.3 - 1 µm Si 0,3 Ge 0,7 constructed) to account for thermal and / or lattice mismatch between Ge and Si. Alternatively, the buffer layer stack 106 may comprise SiGe with a graded Ge composition (e.g., from 30% to 70%), or multiple layers of SiGe with a varying Ge concentration, or any combination of these different types of buffer layer structures. In the exemplary embodiment, the buffer layer stack 106 is provided immediately above or directly on the Si substrate 204 with a transition layer stack 107 further provided immediately above or on the buffer layer stack 106 and also between the Si substrate 104 and the device layer stack 108.

[0018] The transition layer stack 107 includes an n-type doped SiGe layer 107A (e.g., a layer of relaxed phosphorus doped Si0,3 Ge 0,7 ). In the exemplary embodiment, the n-type doped SiGe layer 107A has a thickness of 5 - 20 nm with a dopant concentration in the range of 1e17 - 1e19 atoms / cm 3 and advantageously at least 1e18 cm -3 Because phosphorus and other n-type dopants, such as arsenic, diffuse rapidly in both SiGe and Ge, the n-type doped SiGe layer 107A is recessed from the Ge device layer stack 108 to reduce the entry of n-type dopants into the Ge device layer stack 108. For example, the n-type doped SiGe layer 107A may be located 25-100 nm below the Ge device layer 108, for example, separated by a semiconductor layer 107C composed of relaxed intrinsic Si 0,3 Ge 0,7Alternatively, to further improve short-channel effects and / or leakage while the device layer 108 is in an “off” or non-conducting state, the semiconductor layer 107C may be an undoped Si or SiGe layer of relatively low concentration germanium (e.g., <7% Ge) as a reinforced diffusion barrier (or further in addition to a thickness of intrinsic Si 0,3 Ge 0,7 ). The total thickness of the semiconductor layer 107A can therefore vary considerably.

[0019] The transition layer stack 107 further includes a doped p-type SiGe layer 107B (e.g., a layer of relaxed Si 0,3 Ge 0,7). In the exemplary embodiment, the p-type doped SiGe layer 107B is a δ-doped layer that approximates a 2-D plate of layer charge. In such embodiments, the p-type doped SiGe layer 107B has a thickness of 5-15 nm, which is achievable by in-situ doping during the epitaxial growth of the junction layer stack 107. Larger thicknesses may also be possible, but with limitations so that the n-type doped layer 107A is not fully compensated. In the exemplary embodiment, the p-type doped SiGe layer 107B has a doping between 5e17 and 1e19 cm -3 , advantageously of at least 1e18cm -3 The p-type dopant species is boron in the exemplary embodiment, although other p-type dopant species can be expected to perform similarly.

[0020] Fig. 1B illustrates a graphical representation of the dopant concentration depth profile of a semiconductor layer stack including a δ-doped p-type SiGe transition layer, such as layer 107B, provided over a doped n-type leakage suppression layer, such as SiGe layer 107A, in accordance with an embodiment of the present invention. The illustrated dopant concentration depth profile represents an "as-grown" state of the semiconductor stack as opposed to an "as-annealed" state. As shown in Fig. As shown in Figure 1B, a boron-doped SiGe transition layer has a boron concentration of 2e18cm -3 and has a δ-doping of at least 1e18cm -3 over a depth range of approximately 15 nm, demarcated as “107B”. A phosphorus doping of approximately 1e18cm -3and spans the depths marked with “107A”, corresponds to the doped leakage suppression layer of the n-type SiGe junction layer. As shown in Fig. As shown in Figure 1B, the phosphorus-doped layer 107A has a greater thickness than the boron-doped layer 107B and is more graded than the boron-doped layer 107B (i.e., non-δ-doped).

[0021] In some embodiments, a p-type SiGe transition layer is spaced from an underlying n-type SiGe transition layer by a non-intentionally doped (e.g., intrinsically doped) SiGe layer. Such a spacer layer is denoted by 107A' in Fig. 1A and has a minimum thickness (e.g., 2-5 nm) depending on the growth rate kinetics and the speed with which a growth chamber switches between an n-type and p-type dopant. The spacer layer 107A' is SiGe (e.g., Si 0,3 Ge 0,7), which is grown after the termination of the n-type dopant and before the introduction of the p-type dopant. The effective doping of the spacer layer 107A' is for an embodiment in Fig. Figure 1B illustrates where both the boron and phosphorus doping amounts are below 5e17 cm -3 In certain embodiments, the spacer layer 107A' has a thickness of 2-5 nm. For embodiments at the upper end of this range, the layer 107A, 107A', and 107B can be characterized as a p-in δ-doped structure in which at least the p-type layer is a δ-doped layer.

[0022] Depending on the embodiment, the semiconductor stack 100 may be either a “global” film stack provided over an entire surface of a substrate (e.g., the substrate 104 is Fig. 1A for an entire wafer), or a “local” film stack that is provided only over certain areas of a substrate (e.g., the substrate 104 is in Fig. 1A for a small area of ​​a wafer). In both embodiments, the semiconductor stack 100 can be formed using any epitaxial technique known to be suitable for SiGe materials, such as, but not limited to, CVD and molecular beam epitaxy (MBE). As used herein, an "epitaxial" layer is aligned with the seed surface (e.g., having a preferred crystal orientation as a result of the crystallinity of the seed surface). Fig. 2A and Fig. 2B illustrate cross-sectional views of a local growth embodiment in which the Fig. 1A is grown with the advantage of aspect ratio trapping (ART).

[0023] As in Fig. 2A, an insulating dielectric has sidewalls 250 that define a trench 260 with a semiconductor seed surface exposed at the trench bottom. As shown in Fig. As shown in Figure 2B, the local and selective epitaxial growth of crystalline semiconductor forms a SiGe buffer layer 206B (e.g., having properties as described for layer 106A) over a SiGe buffer layer 206A (e.g., having properties as described for layer 106A) provided on a substrate 204 (e.g., having properties as described for substrate 104). Also provided in trench 260 are transition layers 207A, 207B, and 207C (e.g., having properties as described for layers 107A, 207B, and 107C, respectively) and device layers 208A and 208B with sacrificial layers 209A and 209B therebetween. In the exemplary embodiment, the sacrificial layers 209A and 209B are each SiGe layers and may each have the same composition. In advantageous embodiments, the Ge concentration in the sacrificial layers 209A, 209B is lower than in the transition layers (e.g., <70% Ge) in order to maintain a certain degree of stress (e.g.,1-1.5%) relative to the transition layer 207C. In one embodiment, the device layers 208A and 208B are each substantially pure Ge. In another embodiment, the device layers 208A and 208B each have a SiGe composition that is richer in Ge than the sacrificial layers 209A, 209B, which may be either a SiGe alloy or silicon.

[0024] Fig. 3A and Fig. 3B illustrate cross-sectional views of embodiments of a planar semiconductor device using the semiconductor stack 100. Referring first to Fig. 3B, a semiconductor device 300 includes a gate stack 305 disposed over a substrate 304. A Ge-rich device layer 308A is provided over the substrate 304, below the gate stack 305. In general, the semiconductor device 300 may be any semiconductor device including a gate, a channel region, and a pair of source / drain regions, such as, but not limited to, a MOS-FET. In the exemplary embodiment, the device 300 is a PMOS-FET, which serves as one of complementary transistor types within a CMOS integrated circuit.

[0025] In the exemplary embodiment, the Ge-rich device layer 308A is essentially pure Ge that has been strained by 1-2% under pressure. A SiGe transition layer 307C is provided over the substrate 304 beneath the germanium active layer 308A. An n-type junction leakage suppression layer 307A is provided over the substrate 304, with the p-type Ge etch suppression layer 307B provided between the transition layer 307C and the leakage suppression layer 307A, as described in the context of the stack 100. In the exemplary PMOS embodiment, the raised source and drain regions 322 are deposited or grown, heavily doped as p-type (e.g., boron), and provided over the junction leakage suppression layer 307A on both sides of the gate stack 305. The source-drain regions 322 may or may not form p+ / n junctions with the n-type leakage suppression layer 307A (e.g.,Source / drain regions 322 provided on an upper portion of the junction layer 307C).

[0026] In the Fig. 3A, the gate stack 305 is provided directly on the Ge active layer 308A, the germanium device layer 308A is provided directly on the undoped SiGe junction layer 307C, the junction layer 307C is provided directly on the p-type junction layer 307B, the p-type junction layer 307B is provided directly on the junction leakage suppression layer 307A (with only one SiGe spacer, such as 107A', in between).

[0027] The gate stack 305 may include a gate electrode 305B provided directly on a gate dielectric layer 305A, as shown in Fig. 3A. In one embodiment, the gate electrode 305B is constructed from a metal gate, and the gate dielectric layer 305A is constructed from a high-K material. For example, in one embodiment, the gate dielectric layer 305A is constructed from a material such as, but not limited to, hafnium oxide, hafnium oxynitride, hafnium silicate, lanthanum oxide, zirconium oxide, zirconium silicate, tantalum oxide, barium strontium titanate, barium titanate, strontium titanate, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, lead zinc niobate, or a combination thereof. Furthermore, a portion of the gate dielectric layer 305A may include a layer of native oxide formed from the top few layers of the Ge-rich device layer 308A.In one embodiment, gate dielectric layer 305A is comprised of a high-k upper region and a lower region comprised of an oxide of a semiconductor material. In one embodiment, gate dielectric layer 305A is comprised of a hafnium oxide upper region and a silicon dioxide or silicon oxynitride lower region.

[0028] In one embodiment, the gate electrode 305B is composed of a metal layer, such as, but not limited to, metal nitrides, metal carbides, metal silicides, metal aluminides, hafnium, zirconium, titanium, tantalum, aluminum, ruthenium, palladium, platinum, cobalt, nickel, or conductive metal oxides. In a specific embodiment, the gate electrode 305B is constructed of a non-functional ambient fill material formed over a functional metal ambient layer. In one embodiment, the gate electrode 305B is constructed of a P-type material. The gate stack 305 may also include dielectric spacers 318, as shown in Fig. 3A.

[0029] As in Fig. 3B, the source and drain regions 322 are “embedded” or “raised” replacement source and drain regions. Fig. 3A further illustrates a cross-sectional view during fabrication of the device 300. Referring to Fig. 3A, portions of the Ge-rich device layer 308A and, in the exemplary embodiment, portions of the upper junction layer 307C, and even portions of the p-type junction layer 307B are removed to provide recessed regions 320 on both sides of the gate stack 305. Recessed regions 320 may be formed by any suitable technique that removes portions of the device layer 308A, such as a dry etch or a wet etch process. In one embodiment, at least a portion of the recessed regions 320 are formed by a wet etch that is sensitive to the oxidation state of the Ge-rich device layer 308A, such as, but not limited to, aqueous hydroxide chemistries such as ammonium hydroxide (NH4OH), potassium hydroxide (KOH), tetramethylammonium hydroxide (TMAH), or other tetraalkylammonium hydroxides.In one embodiment, a first recess of regions 320 involves a plasma dry etch to define Ge-rich device layer 308A using NF3, HBr, SF6, or Cl2, while a second recess of regions 320 involves a wet etch of SiGe transition layer 307C using an aqueous hydroxide chemistry. The presence of p-type transition layer 307B is advantageous in the formation of recessed regions 320 because it allows, for example, a first etch of Ge-rich device layer 308A followed by a SiGe etch of the upper transition layer 307C, which is highly selective (almost infinitely) to Ge-rich device layer 308A (which is, for example, pure Ge). As such, tips of the source and drain regions located in close proximity to the ends of the device channel can be formed with great precision, allowing scaling of the FET gate length (L. g). In one embodiment, the gate stack 305 directs the formation of recessed regions 320 (i.e., self-aligned recessed regions 320). In one embodiment, recessed regions 320 are formed with rounded edges, as shown in Fig. 3B. In another embodiment, however, recessed regions 320 are formed with faceted corners. In one embodiment, the n-type leakage suppression layer 307A serves as an etch stop during the formation of the recessed regions 320. Referring again to Fig. 3B, a pair of embedded source and drain regions 322 are epitaxially formed in the recessed regions 320, or not. In one embodiment, the source and drain regions 322 uniaxially exert compressive stress on the Ge-rich device layer 308 and are constructed of a material with a lattice constant greater than that of germanium, such as III-V materials with a lattice constant greater than that of germanium.

[0030] As mentioned above, embodiments of the present invention can be applied to non-planar MOSFETs. For example, devices with a three-dimensional architecture, such as tri-gate devices, can benefit from the semiconductor device stack including a buried p-type junction layer. Fig. 4A - 4C illustrate tilted views illustrating various operations in a method for fabricating non-planar semiconductor devices using the semiconductor stack of Fig. 1A in accordance with embodiments of the present invention.

[0031] In general, non-planar FET embodiments can benefit from a buried p-type Ge etch suppression layer by enabling the formation of a fin in the Ge-rich device layer with a very fine lateral dimension (e.g., < 22 nm). Following the formation of the Ge-rich fin surrounding and / or underlying regions of SiGe, it can be etched with essentially unlimited selectivity to the Ge-rich fin structure, allowing for well-controlled channel lengths and / or source / drain tips and / or subchannel feature dimensions with chemically sharp interfaces formed along the Ge-rich structures.

[0032] Referring to Fig. 4A, a semiconductor device 400 includes a gate stack 405 provided over a substrate 404. A three-dimensional Ge-rich device body 408A is provided over the substrate 404 and under the gate stack 405. An isolation region 420 is provided over the substrate 404 with the three-dimensional device body 408A extending therefrom (device bodies planar with the isolation region 420 are also possible). An upper transition layer 407C is provided over the substrate 404 under the three-dimensional germanium-rich device body 408A. A Ge etch suppression layer 407B is provided under the upper transition layer 407C and has at least some properties described elsewhere herein in the context of layer 107B of the device stack 100 ( Fig. 1). Layer 407B is provided over a junction leakage suppression layer 407C, which is provided over buffer 406 and substrate 404. The material compositions and dimensions of all semiconductor layers in device 400 are identical or similar to those described for semiconductor device 300, since both device embodiments utilize semiconductor stack 100.

[0033] In one embodiment, at least a portion of the isolation region 420 and / or the non-planar semiconductor device stack surrounded by the isolation region 420 is formed by a wet etch sensitive to the oxidation state of the Ge-rich device layer 408A, such as, but not limited to, the aqueous hydroxide chemistries described elsewhere herein (TMAH, etc.). In one embodiment, a first etch of a semiconductor device stack (e.g., stack 100) to form the isolation region 420 involves a plasma dry etch, such as, but not limited to, NF3, HBr, SF6, or Cl2. A second etch, for example, of the dry etch sidewall of the semiconductor stack exposed by the dry etch, involves a wet etch of the SiGe transition layer 307C using aqueous hydroxide chemistries.Alternatively, or additionally, deepening the isolation region 420 relative to the non-planar semiconductor body may involve a wet etch sensitive to the oxidation state of the Ge-rich device layer 408A, such as, but not limited to, the aqueous hydroxide chemistries described elsewhere herein (TMAH, etc.). In either situation, the presence of the p-type transition layer 307B enables a SiGe etch of the upper transition layer 307C, which is highly selective (almost infinitely selective) to the Ge-rich device layer 308A (which is, for example, pure Ge).

[0034] Regions of the device body 408A not provided beneath the gate stack 405 (and surrounding dielectric spacer 418) are doped source and drain regions. In accordance with one embodiment of the present invention, the isolation region 420 extends to the interface of the three-dimensional Ge-rich (e.g., pure Ge) device body 408A and the upper transition layer 407C (e.g., Si 0,3 Ge 0,7 ) deepened, as in Fig. 4A. However, other embodiments may include adjusting the height of the isolation regions 420 above or below this particular interface.

[0035] In one embodiment, the source and drain regions are formed by doping (e.g., p-type) regions of the three-dimensional germanium active body 406 not covered by the gate stack 405. Regions of the transition layer 407C may also be p-type doped in the source and drain regions with p-type dopants extending continuously into the p-type layer 407B to form p+ / n diodes with the n-type leakage suppression layer 407A at opposite ends of the non-planar device body. In contrast, in another embodiment, the source and drain regions are embedded source and drain regions. For example, Fig. 4B and Fig. 4C Cross-sectional views of the fabrication of another semiconductor device having a Ge-rich device layer with an underlying diffusion barrier layer in accordance with another embodiment of the present invention.

[0036] Referring to Fig. 4B, portions of the three-dimensional Ge-rich body 408A and possibly portions of the p-type transition layer 407C and the p-type transition layer 407B are removed to provide recessed regions 422 on both sides of the gate stack 405. Recessed regions 422 may be formed by any suitable technique that removes portions of the three-dimensional Ge-rich device body 408A, etc., such as a dry etch or a wet etch process. In one embodiment, at least a portion of the recessed regions 422 are formed by a wet etch that is sensitive to the oxidation state of the Ge-rich device layer 408A, the aqueous hydroxide chemistries (TMAH, etc.) described elsewhere herein.In one embodiment, a first recess of the regions 422 entails a plasma dry etch to define the Ge-rich device layer 408A using NF3, HBr, SF6, or Cl2, while a second recess of the regions 422 entails the wet etch using NH4OH or TMAH or the like. The presence of the p-type junction layer 407B is advantageous in the formation of the recessed regions 422, allowing, for example, a first etch of the Ge-rich device layer 408A followed by a SiGe etch of the junction layer 407C, which is highly selective (almost infinitely) to the Ge-rich device layer 408A (which is, for example, pure Ge). As such, tips of the source and drain regions can be formed with great precision, allowing scaling of the gate length of the FET (L). g). In one embodiment, the gate stack 405 directs the formation of recessed regions 422, forming self-aligned recessed regions 422. In one embodiment, the n-type leakage suppression layer 407A serves as an etch stop during the formation of the recessed regions 422.

[0037] Referring to Fig. 4C, a pair of raised source and drain regions 424 are epitaxially formed in the recessed regions 422, or not. In one embodiment, the source and drain regions 424 uniaxially exert compressive stress on the Ge-rich device layer 408A and are constructed of a material with a lattice constant greater than germanium, such as III-V materials with a lattice constant greater than germanium.

[0038] Fig. Figure 5A illustrates an isometric cross-sectional view of a nanowire or nanoribbon semiconductor device using the semiconductor stack of Fig. 1A in accordance with an embodiment of the present invention. Fig. Figure 5B illustrates a channel cross-sectional layer of the nanowire-based semiconductor structure of Fig. 5A in accordance with an embodiment of the present invention. Fig. Figure 5C illustrates a cross-sectional view of the nanowire-based semiconductor structure of Fig. 5A in accordance with an embodiment of the present invention.

[0039] Referring first to Fig. 5A, a semiconductor device 500 includes one or more vertically aligned or stacked germanium nanowires (508 set) provided above a substrate 504. Embodiments herein include either single-wire devices or multi-wire devices. As an example, a device based on two nanowires with nanowires 508A, 508B is shown for illustrative purposes. For ease of description, nanowire 508A is used as an example, in which the description focuses on only one of the nanowires in set 508. It should be understood that where attributes of one nanowire are described, embodiments based on a plurality of nanowires may have the same attributes for each of the nanowires.

[0040] Each of the Ge-rich (e.g., pure Ge) nanowires 508 includes a channel region 506 provided within the nanowire. The channel region 506 has a length (L). Referring to Fig. 5B, the channel region also has a perimeter that is orthogonal to the length (L). Referring to the two Fig. 5A and Fig. 5B, a gate stack 505 surrounds the entire perimeter of each of the channel regions 506. The gate stack 505 includes a gate electrode along with a gate dielectric layer provided between the channel region 506 and the gate electrode (not shown individually). The channel region 506 is discrete in that it is completely surrounded by the gate stack 505, without any intervening material, such as an underlying substrate material (such as the transition layer 107C with respect to the stack 100) or other channel fabrication sacrificial materials separating the Ge-rich nanowires 508 from each other. Accordingly, in the embodiments with a plurality of nanowires 508, the channel regions 506 of the nanowires are also discrete relative to each other, as shown in Fig. 5B. A junction leakage suppression layer 507A is provided above the substrate 504 and below the one or more germanium nanowires 508. The gate stack 505 is provided above the n-type leakage suppression layer 507A and may be located on the SiGe junction layer 507C, as illustrated. Although not illustrated, in one embodiment, a buffer may be provided directly between the substrate 504 and the junction leakage suppression layer 507A, substantially as described in the context of the device stack 100.

[0041] Referring again to Fig. 5A, each of the nanowires 508 also includes source and drain regions 510 and 512 provided in the nanowire on either side of the channel region 506. The source and drain regions 510 / 512 are provided on the SiGe junction layer 507C, as illustrated. In one embodiment, the source and drain regions 510 / 512 are replaced source and drain regions, e.g., at least a portion of the nanowires is removed and replaced with a source / drain material region. In another embodiment, the source and drain regions 510 / 512 are composed of portions of the one or more germanium nanowires 508 that are merely doped (e.g., by a boron implant, etc.).

[0042] A contact pair 514 (shown dashed in Fig. 5A) is provided over the source / drain regions 510 / 512. In one embodiment, the semiconductor device 500 further includes a spacer pair 516 (shown in dashed lines in Fig. 5A). The spacers 516 are provided between the gate stack 505 and the contact pair 514. As described above, the channel regions and the source / drain regions are discrete in at least several embodiments. However, not all regions of the nanowires 508 need to be discrete. For example, referring to Fig. 5C, the nanowires 508A-508B are not discrete at the location beneath the spacers 516. In one embodiment, the stack of nanowires 508A-508B includes semiconductor sacrificial material between them (509B) and underlying (509A), which may be SiGe (e.g., of a lower Ge concentration than that of the transition layer 107C) or silicon. In one embodiment, the bottom nanowire 508A is still in contact with a portion of the transition layer 507C, which is used, for example, in manufacturing, as described further below.

[0043] In one embodiment, the one or more Ge-rich nanowires 508 are substantially composed of germanium, the transition layer 507C is the p-type Ge etch suppression layer 507B is doped Si 0,3 Ge 0,7 p-type and the junction leakage suppression layer 507A is doped Si 0,3 Ge 0,7 n-type, as described elsewhere herein for device stack 100. In one embodiment, the one or more germanium nanowires 508 are compressively strained (e.g., by 1-2% relative to the junction layer 507C).

[0044] Although the device 500 described above serves as a single device, e.g., a PMOS device, a CMOS architecture can also be formed to include both NMOS and PMOS nanowire-based devices provided on or over the same substrate. In one embodiment, the nanowires 508 can be sized as wires with z- and y-dimensions that are substantially identical, or as ribbons, where one of the z- and y-dimensions is larger than the other. The nanowires 508 can be square, rounded, or faceted (e.g., at some angle non-orthogonal to the z- and y-axes). The material compositions and dimensions can be the same as or similar to those described for the semiconductor stack 100 and the device 300 or 400.

[0045] In another aspect, methods for fabricating a nanowire semiconductor structure are provided. For example, Fig. 6A-6D are three-dimensional cross-sectional views representing various operations in a method of fabricating a nanowire semiconductor device having, at least at one point in the process, a Ge-rich device layer with an underlying SiGe transition layer and a doped p-type Ge etch suppression layer, in accordance with an embodiment of the present invention.

[0046] Referring to Fig. 6A, a ridge-type structure 612 is formed over a substrate 604. The ridge includes Ge-rich device layers 608A' and 608B' and two intermediate layers of silicon-rich material 609A' and 609B', such as silicon or silicon-germanium layers of higher Si content than device layers 608A' and 608B'. The ridge stops on transition layer 607C, although in other embodiments, ridge-type structure 612 may extend downward and include a patterned region of transition layer 607C. Although not shown, in one embodiment, a buffer is provided directly between substrate 604 and transition leakage suppression layer 607C.

[0047] Fig. 6B illustrates the fin-type structure 612 with the three sacrificial gate structures 614A, 614B, and 614C provided thereon. In such an embodiment, the three sacrificial gates 614A, 614B, and 614C are constructed from a sacrificial gate oxide layer 616 and a sacrificial polysilicon gate layer 618, which are deposited and patterned over the entire area, for example, using a plasma etching process common in the art.

[0048] After the patterning process for forming the three sacrificial gates 614A, 614B and 614C, spacers may be formed on the sidewalls of the three sacrificial gates 614A, 614B and 614C, and doping may be performed in the regions 620 of the ridge-type structure 612 formed in Fig. 6B (e.g., tip and / or source and drain type doping), and a dielectric interlayer may be formed to cover and subsequently expose the three sacrificial gates 614A, 614B, and 614C. The dielectric interlayer may then be polished to expose the three sacrificial gates 614A, 614B, and 614C for a replacement gate or gate-last process. Referring to Fig. 6C, the three sacrificial gates 614A, 614B and 614C are exposed together with the spacers 622 and the dielectric interlayer 624.

[0049] The sacrificial gates 614A, 614B, and 614C are then removed, for example, in a replacement gate or gate-last process flow convention in the field for the selected materials to expose channel regions of the fin-type structure 612. Referring to Fig. 6D, sacrificial gates 614A, 614B, and 614C are removed to provide trenches 626, thus exposing channel regions of the nanowires. Portions of the intermediate sacrificial layers exposed by trenches 626 are removed to leave discrete portions of Ge-rich device layers 608A' and 608B' for forming nanowires 608A and 608B. In Fig. 6D, sacrificial material 609A is illustrated for clarity, but would typically be removed simultaneously with a sacrificial layer provided between 608A and 608B.

[0050] In one embodiment, the silicon-rich sacrificial layers 609A and 609B are selectively etched using a wet etch that does not etch the Ge-rich device layers 608A' and 608B' to strip or undermine lengths of the device layers 608A' and 608B' that are not anchored by other structures (e.g., spacers 622). In one embodiment, the wet etch is sensitive to the oxidation state of the Ge-rich device layers 608A' and 608B'. Etch chemistries, such as, but not limited to, aqueous hydroxide chemistries including NH4OH, KOH, and TMAH, for example, may be utilized to selectively etch the sacrificial layers 609A and 609B. The presence of the p-type transition layer 607B is advantageous in improving the selectivity of a SiGe etch with respect to the Ge-rich device layers 608A' and 608B'.For example, in embodiments where device layers 608A' and 608B' are pure Ge, the etch selectivity with respect to the nanowires is nearly unlimited, so that sacrificial layers 609A and 609B can be removed along a chemically sharp interface with device layers 608A' and 608B' (i.e., no portion of the device layers is etched).

[0051] In alternative embodiments, although not shown, the transition layers 607C and 607B may also be removed, e.g., before, after, or at the same time as the removal of the sacrificial layers 609A and 609B. Also, the diffusion barrier layer may be completely removed or only partially removed, e.g., leaving residues under the spacers, or alternatively, it may be left intact. Subsequently, the device fabrication may be completed. In one embodiment, a surrounding gate electrode is formed around the germanium nanowires 604 and 608 and over the leakage suppression layer 507A, as described above in connection with Fig. 5A.

[0052] In the Fig. 6D, a channel design operation or tuning may be performed. For example, in one embodiment, the discrete regions of the Ge-rich device layers 608A and 608B may be thinned using oxidation and etching techniques, etc. Accordingly, the initial wires formed from the Ge-rich layers 608A' and 608B' may start thicker and are thinned to a size suitable for a channel region in a nanowire device, independent of the sizing of the device's source and drain regions.

[0053] After the formation of the discrete channel regions, as in Fig. 6D, the processing of the high-k gate dielectric and the metal gate can be performed, and source and drain contacts can be added. Contacts can be made at the location of the interlayer regions of the dielectric layer 624 shown in Fig. 6D remain. In addition, one or more thermal processes may anneal the semiconductor layers so that the p-type doped layer 607B and the n-type doped layer 607A can diffuse together, even to the point that the p-type and n-type dopants do not form separate peaks in a dopant profile, as in Fig. 1B. However, the n-type doped layer 607A is not completely compensated by the p-type doped layer 607A, and since annealing can be performed well after the selective etching of the SiGe sacrificial layers, the function of the p-type doped layer 607A can still be realized.

[0054] Fig. Figure 8 illustrates a computer device 700 in accordance with one implementation of the invention. The computer device 700 houses a circuit board 702. The circuit board 702 may include a number of components, including, but not limited to, a processor 704 and at least one communication chip 706. The processor 704 is physically and electrically connected to the circuit board 702. In some implementations, the at least one communication chip 706 is also physically and electrically connected to the circuit board 702. In other implementations, the communication chip 706 is part of the processor 704.

[0055] Depending on its applications, the computer device 700 may include other components that may or may not be physically and electrically connected to the circuit board 702. These other components include, but are not limited to, volatile memory (e.g., DRAM), non-volatile memory (e.g., ROM), flash memory, a graphics processor, a digital signal processor, a crypto processor, a chipset, an antenna, a display, a touchscreen display, a touchscreen controller, a battery, an audio codec, a video codec, a power amplifier, a global positioning system (GPS) device, a compass, an accelerometer, a gyroscope, a speaker, a camera, and a mass storage device (such as a hard disk drive, a compact disk (CD), a digital versatile disk (DVD), and so on).

[0056] The communication chip 706 enables wireless communications for the transfer of data to and from the computer component 700. The term "wireless" and its derivatives can be used to describe circuits, devices, systems, methods, techniques, communication channels, etc., that convey data through a non-solid medium using modulated electromagnetic radiation. The term does not imply that the associated devices do not contain any wires, although this could be the case in some embodiments. The communication chip 706 can implement any of a variety of wireless standards or protocols, including, but not limited to, Wi-Fi (IEEE 802.11 family), WiMAX (IEEE 802.16 family), IEEE 802.20, "Long Term Evolution" (LTE), Ev-DO, HSPA+, HSDPA+, HSUPA+, EDGE, GSM, GPRS, CDMA, TDMA, DECT, Bluetooth, derivatives thereof, and any other wireless protocols referred to as 3G, 4G, 5G, and beyond. The computer device 700 may include a plurality of communication chips 706. For example, a first communication chip 706 may be dedicated to shorter-range wireless communications, such as Wi-Fi and Bluetooth, and a second communication chip 706 may be dedicated to longer-range wireless communications, such as GPS, EDGE, GPRS, CDMA, WiMAX, LTE, Ev-DO, and others.

[0057] The processor 704 of the computer device 700 includes an integrated circuit die packaged within the processor 704. In some embodiments of the invention, the integrated circuit die of the processor includes one or more devices, such as MOSFETs, constructed in accordance with embodiments described elsewhere herein. The term "processor" may refer to any device or portion of a device that processes electronic data from registers and / or memory to convert that electronic data into other electronic data that can be stored in registers and / or memory.

[0058] The communication chip 706 also includes an integrated circuit form packaged within the communication chip 706. In accordance with another embodiment of the invention, the integrated circuit form of the communication chip includes one or more devices, such as MOSFETs, with features and / or fabricated in accordance with embodiments described elsewhere herein.

[0059] In further implementations, another component housed within the computer device 700 may include an integrated circuit form including one or more devices, such as MOS-FETs with features and / or fabricated in accordance with embodiments described elsewhere herein.

[0060] In certain embodiments, the computer device 700 may be a laptop, a netbook, a notebook, an ultrabook, a smartphone, a tablet, a personal digital assistant (PDA), an ultra-mobile PC, a cell phone, a desktop computer, a server, a printer, a scanner, a monitor, a set-top box, an entertainment controller, a digital camera, a portable music player, or a digital video recorder.

Claims

[1] Semiconductor device stack (100), comprising: a germanium (Ge)-rich device layer (108A;208A;308A) provided over a silicon (Si) substrate (104;304); a SiGe transition layer (107C;207C;307C) provided above the substrate (104;304) and below the device layer (108A;208A;308A); a p-type δ-doped SiGe layer (107B;207C;307C) provided above the substrate (104;304) and below the transition layer (107C;207C;307C); an n-type SiGe layer (107A;207A;307A) provided above the substrate (104;304) and below the δ-doped p-type SiGe layer (107B;207B;307B); and one or more SiGe buffer layers (106A; 106B; 306A; 306B) provided above the substrate (104; 304) and below the n-type SiGe layer (107A; 207A; 307A). [2] The semiconductor device stack (100) according to claim 1, wherein the device layer (108A; 208A; 308A) is one of a plurality of device layers (108; 208; 308) separated by intermediate semiconductor sacrificial layers (209A; 209B) with a first device layer (108A; 208A; 308A) provided directly on a first sacrificial layer (209A), the first sacrificial layer (209A) being provided directly on the junction layer (107C; 207C; 307C), the junction layer (107C; 207C; 307C) being provided directly on the p-type δ-doped SiGe layer (107B; 207B; 307B), and the p-type δ-doped SiGe layer (107B; 207B; 307B) p-type is separated from the n-type SiGe layer (107A;207A;307A) by a SiGe spacer layer (107A'). [3] The semiconductor device stack (100) of claim 2, wherein the sacrificial layers (209A, 209B) have a lower concentration of Ge than the device layers (108; 208; 308); and wherein the transition layer (107C; 207C; 307C), the p-type δ-doped SiGe layer (107B; 207B; 307B), the SiGe spacer layer (107A'), and the n-type SiGe layer (107A; 207A; 307A) all have identical silicon and germanium contents. [4] The semiconductor device stack (100) of claim 3, wherein the transition layer (107C;207C;307C) is between 25 and 100 nm thick, the p-type δ-doped SiGe layer (107B;207B;307B) is between 5 and 15 nm thick, the SiGe spacer layer (107A') is between 2 and 5 nm thick, and the n-type SiGe layer (107A;207A;307A) is between 5 and 20 nm thick. [5] The semiconductor device stack (100) of claim 4, wherein the transition layer (107C; 207C; 307C) is intrinsic, wherein the p-type δ-doped SiGe layer (107B; 207B; 307B) has a boron dopant concentration of at least 1e18 cm -3 and wherein the n-type SiGe layer (107A; 207A; 307A) has a phosphorus dopant concentration of at least 1e18 cm -3 has. [6] The semiconductor device stack (100) of claim 4, wherein the device layers (108; 208; 308) consist essentially of germanium, are undoped, and each has a thickness between 5 and 15 nm, and wherein the semiconductor sacrificial layers (209A, 209B) are composed of SiGe and each has a thickness between 5 and 30 nm. [7] The semiconductor device stack (100) of claim 1, wherein at least the device layer (108A; 208A; 308A) and the transition layer (107C; 207C; 307C) are embedded within an adjacent isolation region (420) also provided on the substrate (104; 404). [8] Semiconductor device (300;400), comprising: a gate stack (305; 405) including a gate dielectric (305A) and a gate electrode (305B) provided over the semiconductor device stack (100) of claim 1, wherein the gate dielectric (305A) is in direct contact with the device layer (108A; 208A; 308A); and a source region (322) and a drain region (322) provided on opposite sides of the gate stack (305). [9] The semiconductor device (300; 400) of claim 8, wherein the device layer (108A; 208A; 308A) comprises a non-planar body having two opposite sidewalls extending from a dielectric isolation region (420) provided above the substrate (104; 304; 404) and adjacent to the device stack (100), and wherein the gate stack (305; 405) is provided on the sidewalls. [10] Semiconductor device (500) comprising: a plurality of germanium (Ge)-rich nanowires (508) aligned vertically across a silicon (Si) substrate (504); a SiGe transition layer (507C) provided between the plurality of nanowires (508) and the substrate (504); a p-type δ-doped SiGe layer (507B) provided under the SiGe junction layer (507C); an n-type SiGe layer (507A) provided between the p-type δ-doped SiGe layer (507B) and the substrate (504); a gate stack (505) provided over the plurality of nanowires (508) and completely surrounding a length of each of the plurality of nanowires (508); Spacers (516) provided adjacent to the gate stack (505); and Source / drain regions (510;512) provided adjacent to the spacers (516) on opposite sides of the gate stack (505) and in contact with the plurality of nanowires (508). [11] The semiconductor device (500) of claim 10, wherein the plurality of nanowires (508) are vertically separated by an intermediate semiconductor sacrificial layer (509A; 509B) along the lengths of the nanowires (508) covered by the spacers (516), wherein a first nanowire (508A) is provided directly on a first semiconductor sacrificial layer (509A), the first semiconductor sacrificial layer (509A) is provided directly on the transition layer (507C), the transition layer (507C) is provided directly on the p-type δ-doped SiGe layer (507B), and the p-type δ-doped SiGe layer (507A) is separated from the n-type SiGe layer (507A) by a SiGe spacer layer. [12] The semiconductor device (500) of claim 11, wherein the germanium (Ge)-rich nanowires (508) consist essentially of Ge, wherein the semiconductor sacrificial layer (509A; 509) contains silicon. [13] The semiconductor device (500) of claim 12, wherein the transition layer (507C) is between 25 and 100 nm thick, the p-type δ-doped SiGe layer (507B) is between 5 and 15 nm thick, the SiGe spacer layer (507A) is between 2 and 5 nm thick, and the n-type SiGe layer is between 5 and 20 nm thick. [14] The semiconductor device (500) of claim 13, wherein the transition layer (507C) is intrinsic, wherein the p-type δ-doped SiGe layer (507B) has a boron dopant concentration of at least 1e18 cm -3 and wherein the n-type SiGe layer (507A) has a phosphorus dopant concentration of at least 1e18cm -3 has. [15] The semiconductor device (500) of claim 13, wherein the nanowires (508) are undoped along the length surrounded by the gate stack (505) and each has a thickness between 5 and 15 nm, and wherein the sacrificial layers (509A; 509B) each have a thickness between 5 and 30 nm. [16] The semiconductor device (500) of claim 10, wherein the gate stack (505) is provided directly on the junction layer (507C). [17] A method of manufacturing a nanowire semiconductor device, the method comprising: Accommodating a semiconductor device stack (100) comprising: a germanium (Ge)-rich device layer provided on a semiconductor sacrificial layer (509A, 509B) comprising more silicon (Si) than present in the device layer; a p-type δ-doped SiGe layer (507B) buried beneath the semiconductor sacrificial layer (509A, 509B); selectively etching at least a partial thickness of the semiconductor sacrificial layer (509A, 509B) to the device layer with a wet etchant to undermine the device layer and form a discrete channel region of a nanowire (508); and Forming a gate stack (505) that completely surrounds the discrete channel region of the nanowire. [18] The method of claim 17, wherein the wet etchant is selected from the group consisting of: ammonium hydroxide, potassium hydroxide and tetramethylammonium hydroxide (TMAH). [19] The method of claim 17, wherein the wet etchant forms a chemically sharp interface between the device layer (108; 308A) and the semiconductor sacrificial layer (509A, 509B). [20] The method of claim 17, wherein the etching is performed without exposing the δ-doped p-type SiGe layer (507B) to the wet etchant.

Citation Information

Patent Citations

  • Configuration of MOS transistor

    KR1019980083547A

  • Accumulation type finfet, circuits and fabrication method thereof

    KR1020110025075A

  • Three dimensional strained quantum wells and three dimensional strained surface channels by ge confinement method

    US20090085027A1

  • High speed Ge channel heterostructures for field effect devices

    US7145167B1