Method for polishing silicon wafers

DE112018001605B4Active Publication Date: 2024-10-17SHIN ETSU HANDOTAI CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
DE112018001605
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2017-04-24
Filing Date
2018-03-16
Publication Date
2024-10-17
Estimated Expiration
2038-03-16

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A method for polishing a silicon wafer (W), comprising: a first polishing step for polishing a surface of the silicon wafer (W) by bringing the silicon wafer (W) held by a polishing head (3) into abrasive contact with a polishing cloth (1) attached to a rotary table (2) while an aqueous alkaline solution containing an abrasive grain is applied to the polishing cloth (1); and a second polishing step for polishing a surface of the silicon wafer (W) by bringing the silicon wafer (W) into abrasive contact with the polishing cloth (1) while an aqueous alkaline solution containing a polymer without an abrasive grain is applied to the polishing cloth (1), wherein the polishing cloth (1) is controlled to have a surface temperature ofso that the surface temperature of the polishing cloth (1) in the second polishing step is 2 °C or more higher than the surface temperature of the polishing cloth (1) in the first polishing step in order to polish the silicon wafer (W).
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD The present invention relates to a method for polishing a silicon wafer. STATE OF THE ART In recent years, semiconductor devices have made remarkable progress toward miniaturization, weight reduction, and higher integration. Accordingly, wafers used to form the matrix have been advanced to higher quality and larger diameters, with some exceeding 300 mm in diameter. Requirements for improving wafer flatness and surface roughness are becoming increasingly stringent. Previous polishing has mainly been performed by a method using a polishing apparatus equipped with a turntable with a polishing cloth attached thereto, a polishing head for holding a wafer from its back side, and a nozzle for applying a slurry, in which method the wafer surface is brought into grinding contact with the polishing cloth using the polishing head while rotating the turntable and the polishing head, and a slurry is applied to the polishing cloth (see Patent Document 1). Previously, polishing was performed that included a first step of precisely processing a wafer for flatness by applying a slurry containing abrasive grains, and a second step of precisely processing the wafer for surface conditions (roughness, scratches, particles, etc.) by applying a slurry containing a polymer but without abrasive grains. In these multi-step polishing embodiments, the polishing conditions, such as the rotational speed of the turntable, etc., were always constant. LITERATURE LIST PATENT LITERATURE Patent Document 1: JP 2001 - 334 454 APatent Document 2: JP 2011 - 42 536 A , which describes a method for producing an epitaxial silicon wafer. SUMMARY OF THE INVENTION TECHNICAL TASK The present inventors conducted research on polishing including the first and second stages described above to find that ΔESFQRmax between before and after polishing has a trade-off relationship with surface roughness with respect to the rotational speed of a turntable (Fig. 3). Incidentally, Fig. 3 is a graph showing the relative value of surface roughness (left axis) and the relative value of ΔESFQRmax (edge flatness, right axis), which are normalized based on values when the rotational speed of the turntable is tripled. Even in such a relationship, polishing technology is required to improve both properties. The present invention was achieved with the above-described objectives in mind. It is an object of the present invention to provide a method for polishing a silicon wafer that enables both flatness and surface roughness to be improved. SOLUTION TO THE TASK To achieve the above-described objectives, the present invention provides a method for polishing a silicon wafer, the method comprising: a first polishing step of polishing a surface of the silicon wafer by bringing the silicon wafer held by a polishing head into grinding contact with a polishing cloth attached to a turntable while applying an aqueous alkaline solution containing an abrasive grain to the polishing cloth; and a second polishing step of polishing a surface of the silicon wafer by bringing the silicon wafer into grinding contact with the polishing cloth while applying an aqueous alkaline solution containing a polymer without containing an abrasive grain to the polishing cloth; wherein the polishing cloth is controlled to have a surface temperature,so that the surface temperature of the polishing cloth in the second polishing step is 2 °C or more higher than the surface temperature of the polishing cloth in the first polishing step to polish the silicon wafer. It becomes possible to obtain a silicon wafer in which both higher flatness and a reduction in surface roughness are achieved by polishing, wherein the surface temperature of the polishing cloth is set 2 °C or more higher in the second polishing step than in the first polishing step as described above. Preferably, the surface temperature of the polishing cloth is controlled while the surface temperature of the polishing cloth is measured with an infrared beam. This makes it possible to control the surface temperature of the polishing cloth more precisely. In this case, it is preferable that the surface temperature of the polishing cloth is controlled by adjusting at least one of a rotational speed of the turntable and a flow rate and a temperature of an aqueous coolant flowing into the turntable. When the surface temperature of the polishing cloth is controlled in this way, it is possible to easily control the surface temperature to make the surface temperature of the polishing cloth in the second polishing step 2 °C or more higher than that of the polishing cloth in the first polishing step. ADVANTAGEOUS EFFECT OF THE INVENTION The inventive method for polishing a silicon wafer makes it possible to obtain a silicon wafer in which both a higher flatness and a reduction in surface roughness have been achieved. BRIEF DESCRIPTION OF THE ILLUSTRATIONS Fig. 1 is a graph showing the change in the surface temperature of the polishing cloth in Examples 1 and 2; Fig. 2 is a schematic diagram showing an example of a single-side polishing apparatus that can be used in the inventive method for polishing a silicon wafer; Fig. 3 is a graph showing the trade-off relationship between ΔESFQRmax and surface roughness. DESCRIPTION OF EMBODIMENTS As described above, a method for polishing a silicon wafer that can achieve both higher flatness and a reduction in surface roughness was required. The present inventors further investigated and found that flatness is predominantly influenced by the polishing temperature in the first polishing step (the surface temperature of the polishing cloth in the first polishing step) where an alkaline aqueous solution containing only an abrasive grain is applied, and surface roughness is predominantly influenced by the polishing temperature in the second polishing step (the surface temperature of the polishing cloth in the second polishing step) where an alkaline aqueous solution containing only a polymer is applied. Accordingly, polishing conditions for achieving both flatness and improving surface roughness by polishing are determined, and the surface temperature of the polishing cloth is monitored by an infrared ray to set the surface temperature of the polishing cloth for polishing in the second polishing step higher than the surface temperature of the polishing cloth in the first polishing step. Then, the present inventors found that both higher flatness and reduction in surface roughness can be achieved by controlling the surface temperature of the polishing cloth in the second polishing step to be 2 °C or more higher than the surface temperature of the polishing cloth in the first polishing step; thereby achieving the present invention. That is, the present invention provides a method for polishing a silicon wafer, the method comprising: a first polishing step of polishing a surface of the silicon wafer by bringing the silicon wafer held by a polishing head into grinding contact with a polishing cloth attached to a turntable while applying an aqueous alkaline solution containing an abrasive grain to the polishing cloth; and a second polishing step of polishing a surface of the silicon wafer by bringing the silicon wafer into grinding contact with the polishing cloth while applying an aqueous alkaline solution containing a polymer without containing an abrasive grain to the polishing cloth; wherein the surface temperature of the polishing cloth is controlled so that the surface temperature of the polishing cloth in the second polishing step is 2°C or more higher than the surface temperature of the polishing cloth in the first polishing step.to polish the silicon wafer. The following describes in detail the process for polishing a silicon wafer. In the present invention, a single-side polishing apparatus 10 may be used as shown in Fig. 2, which is equipped with a turntable 2 having a polishing cloth 1 attached thereto and a polishing head 3 for holding a wafer W. This single-side polishing apparatus 10 is configured to polish the surface of the wafer W by bringing the wafer W held by the polishing head 3 into grinding contact with the polishing cloth 1 and simultaneously applying a polishing agent (slurry) from the nozzle 4 onto the polishing cloth 1. It should be noted that the polishing apparatus used in the present invention is not limited to that shown in Fig. 2, which illustrates an embodiment with two polishing heads 3 mounted above a turntable. For example, one, three, or more polishing heads may be mounted above a turntable. The number of turntables is also not particularly limited, and a plurality of turntables may be mounted. A foamed urethane cloth or a nonwoven fabric is preferably used as the polishing cloth 1. In the present invention, first, the first polishing step is performed using such a single-side polishing apparatus 10 to polish the surface of the silicon wafer W by bringing the silicon wafer W held by the polishing head 3 into grinding contact with the polishing cloth 1 attached to the turntable 2 while applying an aqueous alkaline solution containing an abrasive grain to the polishing cloth from the nozzle 4. An alkaline aqueous solution containing an abrasive grain is used as the polishing agent (slurry) in the first polishing step. A typical example of the alkaline aqueous solution is an aqueous KOH solution. The abrasive grain is preferably colloidal silica. However, any alkaline aqueous solution containing an abrasive grain can be used, and the types of abrasive grain and alkaline aqueous solution are not limited to this. Subsequently, the second polishing step is performed to polish the surface of the silicon wafer W by bringing the silicon wafer W into abrasive contact with the polishing cloth 1 while applying an aqueous alkaline solution containing a polymer without containing an abrasive grain to the polishing cloth 1. The present invention is characterized in that the surface temperature of the polishing cloth for polishing a silicon wafer is controlled so that the surface temperature of the polishing cloth in the second polishing step is 2 °C or more higher than the surface temperature of the polishing cloth in the first polishing step (ie, ΔT ≥ 2 °C in Fig. 1 ). By controlling the surface temperature of the polishing cloth in this way, it is possible to achieve both higher flatness and a reduction in surface roughness. The polishing agent used in the second polishing step is an aqueous alkaline solution containing a polymer without abrasive grain (e.g., colloidal silica). Illustrative examples of the polymer include a polymer absorbed onto a wafer, such as hydroxyethyl cellulose. Aqueous ammonia can be exemplified as the aqueous alkaline solution. However, the types of the polymer and the aqueous alkaline solution are not limited to this. The surface temperature of the polishing cloth is not particularly limited in the first and second polishing steps, as long as it is controlled so that the surface temperature of the polishing cloth in the second polishing step is 2°C or more higher than the surface temperature of the polishing cloth in the first polishing step. For example, they can have a predetermined temperature in the range of 25 to 35°C. Each polishing time can be set from 2 to 8 minutes. Preferably, the surface temperature of the polishing cloth is controlled while the surface temperature of the polishing cloth is measured with an infrared beam. This makes it possible to control the surface temperature of the polishing cloth more precisely. The method is not particularly limited to setting the surface temperature of the polishing cloth in the second polishing step to be 2°C or more higher than the surface temperature of the polishing cloth in the first polishing step. Specifically, the surface temperature of the polishing cloth can be controlled by adjusting at least one of the rotational speed of the turntable and the flow rate and temperature of an aqueous coolant flowing into the turntable, while measuring the surface temperature of the polishing cloth with an infrared ray. For example, the surface temperature of the polishing cloth after completion of the first polishing step can be raised by 2°C or more by increasing the rotational speed of the turntable to increase frictional heat, increasing the temperature of the aqueous coolant, or decreasing the flow rate of the aqueous coolant flowing into the turntable.The transition time (for increasing the temperature) from the first polishing step to the second polishing step may be, for example, 15 to 30 seconds. As a method for adjusting the surface temperature of the polishing cloth in the second polishing step to be 2°C or more higher than the surface temperature of the polishing cloth in the first polishing step, it is also possible to adjust the flow rate or temperature of the applied polishing agent, the rotational speed of the polishing head, or the flow rate or temperature of the aqueous coolant flowing into the polishing head. However, the surface temperature of the polishing cloth can be more easily controlled by adjusting the rotational speed of the turntable to which the polishing cloth is attached or the aqueous coolant flowing into the turntable. If the surface temperature of the polishing cloth in the second polishing step is lower than the surface temperature of the polishing cloth in the first polishing step, or if the difference between the surface temperature of the polishing cloth in the second polishing step and the surface temperature of the polishing cloth in the first polishing step is less than 2 °C, it becomes impossible to achieve both higher flatness and a reduction in surface roughness. EXAMPLES In the following, the present invention will be described in more detail by presenting examples and comparative examples, but the present invention is not limited to these examples. (Examples 1 to 2, Comparative Examples 1 to 3) The single-side polishing apparatus 10, as shown in Fig. 2, was used to polish the surface of the wafer W by bringing the wafer held by the polishing head 3 into grinding contact with the polishing cloth 1 attached to the turntable 2, while applying a slurry from the nozzle 4 onto the polishing cloth 1. A nonwoven fabric was used as the polishing cloth 1. An aqueous KOH solution containing colloidal silica was used as the polishing slurry in the first polishing step, and an aqueous ammonia solution containing hydroxyethylcellulose (HEC) with a molecular weight of 1,000,000,000 was used in the second polishing step. As shown in Fig. 1, a silicon wafer was polished while applying an aqueous KOH solution containing colloidal silica (the first polishing step); then, the coolant flow to the turntable was stopped, while simultaneously applying an aqueous ammonia solution containing HEC with a molecular weight of 1,000,000,000 was started, while increasing the rotation speed of the turntable for 15 seconds (temperature increase period); and the second polishing step was performed at a rotation speed that is a value relative to the rotation speed of the turntable in the first polishing step, as shown in Table 1. The surface temperature of the polishing cloth was measured with an infrared ray during the polishing process. Table 1 shows the difference between the average temperatures (ΔT) in the first polishing step and the second polishing step. Table 1 shows the temperature difference between the first and second polishing steps, as well as the corresponding ΔESFQRmax and surface roughness, measured using a TMS-3000W (manufacturer: Schmitt Industries Inc.). Edge flatness was measured using a Wafer Sight from KLA Tencor Corporation. When calculating the ESFQRmax, zones (also known as polar spots) were set to M49 mode with a total sector number of 72 and a sector length of 30 mm (2 mm EE (outer peripheral exclusion area)). ΔESFQRmax represents the difference between before and after polishing. [Table 1] [Table 1] Difference in mean temperature 0.3 °C 1.4 °C 1.8 °C 2.0 °C 2.6 °C Surface roughness *11,671,271,080,930,79 Flatness *1 (ΔES-FQRmax)0.730,780,830,880.83 Speed of the turntable during the second polishing step *21,01,62,22,83,5 Successful atOnly flatnessOnly flatnessOnly flatnessBothBoth *1 Relative value when the standard value is set to 1 *2 Relative value when the speed of the turntable in the first polishing step is set to 1 As shown in Table 1, Examples 1 and 2, in which the surface temperature of the polishing cloth in the second polishing step was controlled to be 2 °C or more higher than the surface temperature of the polishing cloth in the first polishing step, succeeded in achieving the standards in terms of both flatness and surface roughness. On the other hand, Comparative Examples 1 to 3 failed to achieve the surface roughness standard, thus failing both the flatness and surface roughness requirements.

Claims

A method for polishing a silicon wafer (W), the method comprising: a first polishing step for polishing a surface of the silicon wafer (W) by bringing the silicon wafer (W) held by a polishing head (3) into grinding contact with a polishing cloth (1) attached to a turntable (2) while applying an aqueous alkaline solution containing an abrasive grain to the polishing cloth (1); and a second polishing step for polishing a surface of the silicon wafer (W) by bringing the silicon wafer (W) into grinding contact with the polishing cloth (1) while applying an aqueous alkaline solution containing a polymer without containing an abrasive grain to the polishing cloth (1), wherein the polishing cloth (1) is controlled to have a surface temperature,so that the surface temperature of the polishing cloth (1) in the second polishing step is 2 °C or more higher than the surface temperature of the polishing cloth (1) in the first polishing step to polish the silicon wafer (W). A method for polishing a silicon wafer (W) according to claim 1, wherein the surface temperature of the polishing cloth (1) is controlled while the surface temperature of the polishing cloth (1) is measured by an infrared ray. A method for polishing a silicon wafer (W) according to claim 1 or claim 2, wherein the surface temperature of the polishing cloth (1) is controlled by adjusting at least one of a rotational speed of the turntable (2) and a flow rate and a temperature of an aqueous coolant flowing into the turntable (2).

Citation Information

Patent Citations

  • Work polishing method, work holding plate and work polishing device

    JP2001334454A

  • Method for manufacturing epitaxial silicon wafer

    JP2011042536A

  • JP002011042536A