Powder injection molding process for a turbomachine blade
The method of using multiple injection heads with varying metal particle sizes in separate mold cavities addresses the limitation of single composition in powder injection molding, enabling blades with tailored mechanical properties through controlled injection.
Patent Information
- Application Number
- FR2019005158
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-05-16
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2039-05-16
AI Technical Summary
Existing powder injection molding processes for turbomachine blades can only produce parts with a single metal composition, limiting the ability to achieve different mechanical properties in various areas of the part.
A method involving multiple injection heads to introduce mixtures with different metal particle sizes into separate mold cavities, allowing for the creation of zones with distinct mechanical properties through controlled injection parameters.
Enables the production of turbomachine blades with differentiated mechanical properties by ensuring adequate junction interfaces and optimized mechanical performance in specific areas.
Smart Images

Figure 00000007_0000 
Figure 00000007_0001 
Figure 00000008_0000
Abstract
Description
Title of the invention: Method for injection molding a powder of a turbomachine blade Technical field of the invention
[0001] The present disclosure relates to the field of methods for manufacturing metal parts, such as a turbomachine blade, by powder injection molding. State of the prior art
[0002] The powder injection manufacturing process consists of producing a mixture using a metal powder, a first binder powder and a second binder powder. As shown in [Fig.l], the granules of said mixture are injected using an injector 2 into a mold 4 to obtain a part, such as a blade 6, called a green part which then undergoes a debinding operation aimed at removing the first binder and at the end of which a so-called brown part is obtained. The last step of the process consists of carrying out a sintering operation making it possible to remove the second binder to obtain the final part 6. It can be seen that the injector is used to inject the mixture into the cavity of the mold whose imprint corresponds to the external shape of the blade.
[0003] This known method makes it possible to obtain a part whose internal structure is formed from a single metal powder which may comprise one or more different types of metal particles. However, a metal part may need to have different metal compositions depending on the areas or parts of it to have different mechanical properties. However, the current technique's powder injection manufacturing method only allows the injection of a single mixture into the mold. Summary of the invention
[0004] The present document thus relates to a method of manufacturing a metal part, such as a turbomachine blade, by powder injection molding, comprising the following steps: a. Providing a first mixture comprising first metal particles having on average a first diameter; b. Providing a second mixture comprising second metal particles having on average a second diameter, the first diameter being different from the second diameter; c. Providing a mold comprising a first cavity and a second cavity connected to each other; d. Inject the first mixture into the first cavity and inject the second mixture into the second cavity.
[0005] The proposed method makes it possible to obtain, after sintering, a metal part having two zones having different mechanical properties since a first zone results from the injection of the first mixture into the first cavity of the mold and a second zone results from the injection of the second mixture into the second cavity. In order to be able to carry out the differentiated injection proposed in step d), it is necessary to adapt the device to include a first injection head for the first mixture into the first cavity of the mold and a second injection head for the second mixture into the second cavity of the mold. The method is not limited to the supply of a first mixture and a second mixture and could, of course, include the supply of one or more other mixtures.
[0006] A time delay may be applied between the first injection head and the second injection head to fill the first cavity and the second cavity adequately and create an adequate junction interface between the first mixture and the second mixture. To this end, a numerical simulation may be carried out, prior to injection, to determine the injection parameters of the first mixture and the second mixture, said parameters comprising the flow rate, the pressure, the initial injection time and the injection duration.
[0007] Said metal part may be a blade, said first cavity of the mold being for example shaped to form a root of the blade and said second cavity of the mold being shaped for example to form a part of the blade.
[0008] Said first average diameter may be smaller than the second average diameter. Thus in the case of a blade as indicated in the previous paragraph, the smaller grain size in the first zone forming the root will give smaller metal grains than in the second zone forming the blade. The first zone will thus have better fatigue properties than in the second zone which will in turn have better finishing properties than in the first zone. It is thus possible to differentiate the mechanical properties of the blade depending on the zone of the blade considered.
[0009] Said first average diameter may be less than 25 pm. Said second average diameter may be less than 65 pm.
[0010] Each of the first mixture and the second mixture may have at least 35% metal particles by volume.
[0011] The first metal particles may be made from a first metal base and the second metal particles may be made from a second metal base, the first metal base being close to the second metal base.
[0012] The first metal particles and the second metal particles can be made from the same chemical material. Brief description of the figures
[0013] [Fig-1] already described previously, is a schematic view of a device injection of a known type;
[0014] [Fig.2] is a schematic view of an injection device of a device for use with an injection method according to the present disclosure;
[0015] [Fig.3] is a schematic view of a turbomachine blade obtainable with the method of the present disclosure. Detailed description of the invention
[0016] Reference is now made to Figures 2 and 3 which schematically represent an installation 10 for powder injection molding of a turbomachine blade 11, such as a low-pressure turbine blade. According to the method of the present disclosure, the mold 12 comprises at least two cavities and comprises, in this case, three cavities, namely a first cavity 12a as well as a second cavity 12b and a third cavity 12c. The mold 12 has a longitudinal dimension L. The first cavity 12a and the third cavity 12c communicate with the second cavity 12a and are formed in longitudinal end portions of the mold in order to form the blade in a single piece after molding.The first cavity 12a of the mold 12 is intended to form the radially internal part of the blade 11 comprising the root 14 of the blade 11 called first part 11a, the second cavity 12a of the mold 12 is intended to form the blade of the blade 11 called second part 11b and the third cavity 12c of the mold 12 is intended to form the radially external part of the blade 11 comprising a platform sector 16 carrying radial wipers 18 and called third part 11c.
[0017] The installation comprises two injection heads or injectors 18a, 18b of a mixture of metal powder and binders. The first injector 18a is intended to allow the injection of a first mixture into the first cavity 12a and the third cavity 12c while the second injector 18b is intended to allow the injection of a second mixture into the second cavity 12b. Although the first injector 18a aims to carry out the injection of a first mixture both into the first cavity 12a and into the third cavity 12c, the installation 10 could comprise more than two injectors and could for example comprise a third to carry out an injection of a differentiated mixture between the first cavity and the third cavity.
[0018] The method aims to: - provide a first mixture comprising first metal particles having on average a first diameter, - providing a second mixture comprising second metal particles having on average a second diameter, the first diameter being different from the second diameter; - inject the first mixture into the first cavity 12a and the third cavity 12c and inject the second mixture into the second cavity 12b.
[0019] In order to produce an adequate junction interface at the level of the first part 11a with the second part 11b and an adequate junction interface between the second part 11b and the third part 11c, it is possible to carry out, prior to the injection, a numerical simulation to determine the injection parameters of the first mixture and the second mixture, said parameters comprising the flow rate, the pressure, the initial injection time and the injection duration.
[0020] The first average diameter is chosen to be smaller than the second average diameter. Thus, the first part 11a and the third part 11c will have better fatigue properties than in the second part 11b which will have better finishing properties than in the first 11a and third 11c parts of the blade 11. It is thus possible to differentiate the mechanical properties of the blade 11 depending on the part or zone of the blade considered.
[0021] The first average diameter is preferably less than 25 pm and may be between 10 and 20 pm. The second average diameter is preferably less than 65 pm and may be between 20 and 35 pm. Each of the first mixture and the second mixture may have at least 35% metal particles by volume.
[0022] The binders used for one and the other (or others) of the mixtures may be identical. In an exemplary embodiment, the injection of the first mixture and the injection of the second mixture are carried out with the following parameters: injection pressure of 2080 bars, an injection temperature of 165°C, an injection speed of 30 mm / s, a pressure in the mold of 800 bars and a holding time of 4 s.
[0023] In order to allow sintering of the entire part in a furnace, the first metal particles must be made from a first metal base and the second metal particles are made from a second metal base, the first metal base being close to the second metal base.
[0024] The method described in this document makes it possible to simply and quickly produce a part having different internal structures in at least two parts or areas. Unlike additive manufacturing, it is not necessary to change the supply of the print head with the first mixture and the second mixture constantly, which is long and complex to achieve.
Claims
Claims
1. A method of manufacturing a metal turbomachine blade (11) by powder injection molding, comprising the following steps: a. Providing a first mixture comprising first metal particles having on average a first diameter; b. Providing a second mixture comprising second metal particles having on average a second diameter, the first diameter being different from the second diameter; c. Providing a mold (12) comprising a first cavity (12a), a second cavity (12b) and a third cavity (12c), the first cavity and the third cavity communicate with the second cavity, the first cavity and the second cavity are connected to each other, the first and third cavities are formed in longitudinal end portions of the mold; d.Injecting the first mixture into the first cavity (11a) and into the third cavity and injecting the second mixture into the second cavity (12b), wherein the first cavity (12a) of the mold (12) is shaped to form a radially internal portion of the blade (11) comprising a root (14) of the blade (11), the second cavity (12a) of the mold (12) being shaped to form the blade of the blade (11) and the third cavity (12c) of the mold (12) is shaped to form a radially external portion of the blade (11) comprising a platform sector (16) carrying radial wipers (18).
2. Method according to one of the preceding claims, in which said metal part is a blade (11), said first cavity (12a) of the mold (12) being shaped to form a root (14) of the blade (11) and said second cavity (12b) of the mold (12) being shaped to form a part of the blade (11).
3. Method according to one of the preceding claims, said first average diameter is less than the second average diameter.
4. Method according to one of the preceding claims, wherein said first average diameter is less than 25 pm.
5. A method according to any preceding claim, wherein said second average diameter is less than 65 pm.
6. A method according to any preceding claim, wherein each of the first mixture and the second mixture has at least 35% metal particles by volume.
7. A method according to any preceding claim, wherein the first metal particles are made from a first metal base and the second metal particles are made from a second metal base, the first metal base being close to the second metal base.
8. Method according to one of the preceding claims, in which the first metal particles and the second metal particles are made from the same chemical material.