Noise filter and electronic apparatus
By positioning resistance elements near a heat dissipation member within a ceramic-based noise filter, the instability caused by temperature rises in power amplifiers is mitigated, ensuring stable operation through enhanced heat dissipation.
Patent Information
- Application Number
- JP2024041001
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-17
- Filing Date
- 2024-03-15
- Publication Date
- 2024-10-01
Smart Images

Figure 2024133026000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a noise filter and an electronic device, and more particularly to a noise filter for a power amplifier and an electronic device having the same. [Background technology]
[0002] Electronic devices such as RF (Radio Frequency) power amplifiers may require a noise filter circuit that supports the broadband of the amplifier, in addition to semiconductor switching elements such as MOSFETs (Metal Oxide Semiconductor Field Effect Transistors) or IGBTs (Insulated Gate Bipolar Transistors) and heat dissipation members for promoting heat dissipation from the semiconductor switching elements. In recent years, for example, a broadband of about several hundred MHz is required for RF power amplifiers for frequencies on the order of several GHz.
[0003] JP2022-518866A (Patent Document 1) discloses an RF power amplifier having a heat sink and a power device welded onto the heat sink. The power device has a carrier flange. A transistor and a decoupling circuit module are attached to the carrier flange. The decoupling circuit module has a first capacitor, a second capacitor, and a damping resistor. The damping resistor is connected to the first capacitor and the second capacitor. The first capacitor, the second capacitor, and the damping resistor are made of a multilayer co-fired ceramic material stack.
[0004] Japanese Patent Laid-Open Publication No. 2002-246864 (Patent Document 2) discloses a bandpass filter with a variable center frequency band, in which first and second resistors for cutting DC are disposed on the upper surface of a laminate having multiple ceramic layers. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Special Publication No. 2022-518866 [Patent Document 2] JP 2002-246864 A Summary of the Invention [Problem to be solved by the invention]
[0006] According to the inventor's research, the operation of the power amplifier may become unstable due to a temperature rise caused by power consumption in a resistor element of a noise filter. This instability may be caused, for example, by the resistance value of the resistor element fluctuating beyond an allowable range due to the temperature rise, or by the characteristics of other elements of the noise filter, such as the capacitance or insulation resistance value of a capacitor, fluctuating beyond an allowable range.
[0007] The present invention has been made to solve the above-mentioned problems, and one object of the present invention is to provide a technique capable of suppressing instability in the operation of a power amplifier caused by a temperature rise accompanying power consumption in a resistive element of a noise filter. [Means for solving the problem]
[0008] A first aspect is a noise filter for a power amplifier, comprising: a ceramic member having a first surface and a second surface opposite to each other in a thickness direction and having electrical insulation; at least one ground internal electrode layer arranged in the ceramic member; at least one first internal electrode layer arranged in the ceramic member and facing the at least one ground internal electrode layer so as to form a first capacitance; a first electrode terminal arranged on the first surface of the ceramic member; at least one ground electrode terminal arranged on the second surface of the ceramic member and electrically connected to the at least one ground internal electrode layer; a resistor element arranged on the second surface of the ceramic member and having a first end electrically connected to the first electrode terminal and a second end electrically connected to the at least one first internal electrode layer, the resistor element having an electrical resistance between the first end and the second end; and an insulator covering the resistor element.
[0009] A second aspect of the present invention is the noise filter according to the first aspect, wherein the at least one ground electrode terminal is disposed directly on the second surface.
[0010] A third aspect of the present invention is the noise filter according to the second aspect, wherein the insulator is a glass film.
[0011] A fourth aspect of the present invention is the noise filter according to the first aspect, wherein the at least one ground electrode terminal is indirectly disposed on the second surface via the insulator.
[0012] A fifth aspect of the present invention is the noise filter according to the fourth aspect, wherein the insulator is a ceramic film.
[0013] A sixth aspect is a noise filter for a power amplifier, comprising: a ceramic member having a first surface and a second surface opposite to each other in a thickness direction and having electrical insulation; at least one ground internal electrode layer disposed in the ceramic member; at least one first internal electrode layer disposed in the ceramic member and facing the at least one ground internal electrode layer so as to form a first capacitance; a first electrode terminal disposed on the first surface of the ceramic member; at least one ground electrode terminal disposed on the second surface of the ceramic member and electrically connected to the at least one ground internal electrode layer; and a resistive element disposed between all internal electrode layers including the at least one first internal electrode layer and the at least one ground internal electrode layer in the thickness direction and the second surface of the ceramic member, the resistive element having a first end electrically connected to the first electrode terminal and a second end electrically connected to the at least one first internal electrode layer, and having an electrical resistance between the first end and the second end, the resistive element being at least partially embedded in the ceramic member.
[0014] A seventh aspect of the present invention is the noise filter according to the sixth aspect, wherein the resistive element is completely embedded in the ceramic member.
[0015] Aspect 8 is the noise filter according to aspect 6, wherein the resistive element is partially embedded in the ceramic member, and the noise filter further comprises an insulator that completely embeds the resistive element together with the ceramic member.
[0016] A ninth aspect is the noise filter of any one of the first to fifth and eighth aspects, further comprising a metal-containing layer on the insulator.
[0017] A tenth aspect of the present invention is the noise filter of the seventh aspect, further comprising a metal-containing layer on the ceramic member.
[0018] An eleventh aspect is a noise filter according to any one of aspects 1 to 10, further comprising a second electrode terminal disposed on the first surface of the ceramic member or on a side surface connecting the first surface and the second surface, and electrically connected to the at least one first internal electrode layer.
[0019] A twelfth aspect of the noise filter according to the eleventh aspect, wherein the second electrode terminal has a shape that is not congruent with the first electrode terminal.
[0020] A thirteenth aspect is a noise filter according to any one of aspects 1 to 12, wherein the at least one ground electrode terminal includes a first ground electrode terminal and a second ground electrode terminal, and the resistive element is disposed between the first ground electrode terminal and the second ground electrode terminal in a planar layout perpendicular to the thickness direction.
[0021] A fourteenth aspect is a noise filter according to any one of the first to thirteenth aspects, further comprising a ground via electrode group including a plurality of via electrodes that electrically connect the at least one ground electrode terminal and the at least one ground internal electrode layer to each other and are arranged in parallel with each other.
[0022] Aspect 15 is a noise filter described in any one of aspects 1 to 14, further comprising at least one second internal electrode layer disposed in the ceramic member, facing the at least one ground internal electrode layer so as to form a second capacitance, and electrically connected to the first electrode terminal.
[0023] Aspect 16 is a noise filter described in aspect 15, further comprising a via electrode group including a plurality of via electrodes electrically connecting the first electrode terminal and the at least one second internal electrode layer and arranged in parallel with each other.
[0024] A seventeenth aspect is a noise filter according to any one of aspects 1 to 16, wherein the at least one internal electrode layer is a plurality of first internal electrode layers, and the noise filter further comprises a via electrode group including a plurality of via electrodes electrically connecting the plurality of first internal electrode layers to each other and arranged in parallel with each other.
[0025] Aspect 18 is an electronic device comprising: a noise filter according to any one of aspects 1 to 17; a heat dissipation member facing the second surface of the ceramic member of the noise filter; and a conductive adhesive that bonds the at least one ground electrode terminal of the noise filter and the heat dissipation member to each other.
[0026] A nineteenth aspect is the electronic device according to the eighteenth aspect, wherein the conductive adhesive has a portion disposed between the heat dissipation component and the resistive element in the thickness direction.
[0027] Aspect 20 is an electronic device described in aspect 18 or 19, further comprising a semiconductor switching element mounted on the heat dissipation member and having a first main terminal electrically connected to the heat dissipation member, a second main terminal spaced from the first main terminal, and a control terminal for receiving a signal to control switching between the first main terminal and the second main terminal, a control lead electrically connected to the control terminal of the semiconductor switching element, and a main lead electrically connected to the second main terminal of the semiconductor switching element and the first electrode terminal of the noise filter.
[0028] Behavior 21 is an electronic device as described in behavior 20, further comprising a frame body provided on the heat dissipation member, surrounding the noise filter and the semiconductor switching element on the heat dissipation member and supporting the control lead and the main lead, and a cover body attached to the frame body so as to seal the space surrounded by the frame body on the heat dissipation member. Effect of the Invention
[0029] According to the above aspect, at least one ground electrode terminal and the resistive element are both disposed on the second surface of the ceramic member. As a result, in an electronic device in which the ground electrode terminal of the noise filter is joined to the heat dissipation member, the resistive element faces the heat dissipation member. This allows the resistive element to be disposed close to the heat dissipation member. This increases the efficiency of heat dissipation from the resistive element. This makes it possible to suppress instability in the operation of the power amplifier caused by a temperature rise accompanying power consumption in the resistive element of the noise filter.
[0030] The objects, features, aspects and advantages of the present invention will become more apparent from the following detailed description and the accompanying drawings. [Brief description of the drawings]
[0031] [Figure 1] 2 is a diagram illustrating an equivalent circuit of the electronic device according to the first embodiment. FIG. [Diagram 2] 1 is a plan view illustrating a schematic configuration of an electronic device in accordance with a first embodiment, with a lid not shown. [Diagram 3] FIG. 2 is a schematic cross-sectional view taken along line III-III in FIG. [Figure 4] 4 is a schematic partial cross-sectional view corresponding to region III in FIG. 3. [Diagram 5] 1 is a cross-sectional view illustrating a schematic configuration of a noise filter according to a first embodiment. [Figure 6] 1 is a top view illustrating a schematic configuration of a noise filter according to a first embodiment. [Figure 7] 2 is a bottom view illustrating a schematic configuration of the noise filter according to the first embodiment. FIG. [Figure 8] 5 is a partial cross-sectional view showing the configuration of an electronic device of a comparative example in the same field of view as that of FIG. 4. [Figure 9] 11 is a graph showing the relationship between the power consumption of a resistive element and the surface temperatures of a heat dissipation member and a noise filter in an electronic device of a comparative example. FIG. [Figure 10]10 is a graph showing the relationship between the power consumption of a resistive element and the surface temperatures of a heat dissipation member and a noise filter in the electronic device of the example. FIG. [Figure 11] 11 is a cross-sectional view illustrating a schematic configuration of a noise filter according to a second embodiment. FIG. [Figure 12] FIG. 11 is a cross-sectional view illustrating a schematic configuration of a noise filter according to a third embodiment. [Figure 13] FIG. 11 is a cross-sectional view illustrating a schematic configuration of a noise filter according to a fourth embodiment. [Figure 14] FIG. 13 is a diagram illustrating an equivalent circuit of a noise filter according to a fifth embodiment. [Figure 15] FIG. 13 is a cross-sectional view illustrating a schematic configuration of a noise filter according to a fifth embodiment. [Figure 16] FIG. 13 is a cross-sectional view illustrating a schematic configuration of a noise filter according to a sixth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0032] <Embodiment 1> Fig. 1 is a diagram that shows a schematic equivalent circuit of electronic device 200 in embodiment 1. Fig. 2 is a plan view that shows a schematic configuration of electronic device 200 while omitting illustration of cover 295 (Fig. 3). Fig. 3 is a schematic cross-sectional view along line III-III in Fig. 2. Fig. 4 is a schematic partial cross-sectional view corresponding to region IV in Fig. 3.
[0033] In this embodiment, the electronic device 200 is an RF power amplifier, and has a noise filter 101 for the power amplifier. For example, the RF may be 1 GHz or more and 10 GHz or less, and the bandwidth may be 100 MHz or more and 1 GHz or less. The noise filter 101 is for removing noise below a frequency corresponding to the bandwidth required for the RF power amplifier, and for that purpose, has a resistance R, a capacitance C1 (second capacitance), and a capacitance C2 (first capacitance) so as to configure the equivalent circuit shown in FIG. 1. The resistance R is, for example, 0.5Ω or more and 10Ω or less. The capacitance C1 may be smaller than the capacitance C2, but is not necessarily limited to this.
[0034] The electronic device 200 includes, in addition to the noise filter 101, at least one electrical element 270 including a semiconductor switching element 271, a control lead 292 and a main lead 291 electrically connected to the semiconductor switching element 271, a heat dissipation member 251, and a conductive adhesive 252 for mounting the noise filter 101 on the heat dissipation member 251.
[0035] The semiconductor switching element 271 is mounted on the heat dissipation member 251. The semiconductor switching element 271 may be an element using a wide band gap semiconductor (particularly, gallium nitride (GaN)) suitable for high frequency operation, for example, a MOSFET or an IGBT. The semiconductor switching element 271 has a first main terminal electrically connected to the heat dissipation member 251, a second main terminal separated from the first main terminal, and a control terminal for receiving a signal for controlling switching between the first main terminal and the second main terminal. When the semiconductor switching element 271 is a MOSFET, the control terminal is a gate terminal G (FIG. 1), and the first main terminal and the second main terminal may be a source terminal S (FIG. 1) and a drain terminal D (FIG. 1), respectively, and the specific description below will be given for this case. In this embodiment, the at least one electric element 270 includes another electric element 272 (not shown in the equivalent circuit of FIG. 1), and the electric element 272 may include, for example, a capacitor.
[0036] The main lead 291 (FIG. 2) is electrically connected to the drain terminal D (FIG. 1) of the semiconductor switching element 271 and the external electrode terminal 31 (first electrode terminal) of the noise filter 101 (FIG. 4). The electrical connection between the main lead 291 and the external electrode terminal 31 of the noise filter 101 may be made by a bonding wire 261 and a metallized layer 281 as shown in FIG. 2, or the main lead 291 and the external electrode terminal 31 may be directly connected to each other by a bonding wire. The bonding wire 261 of the noise filter 101 connects the external electrode terminal 31 (FIG. 4) and the metallized layer 281 in contact with the main lead 291 to each other. The wiring 262 for electrically connecting the main lead 291 and the semiconductor switching element 271 is configured by a series connection of a bonding wire 262a and a bonding wire 262b in the example shown in FIG. 2. The bonding wire 262a connects the main lead 291 and the electrical element 272 to each other. The bonding wire 262b connects the electrical element 272 and the semiconductor switching element 271 to each other. The bonding wire 262a and the bonding wire 262b are connected to each other in series by the electrical element 272, and this series connection is typically obtained by connecting the bonding wire 262a and the bonding wire 262b to a common electrode of the electrical element 272.
[0037] The control lead 292 is electrically connected to the gate terminal G of the semiconductor switching element 271. This electrical connection may be made, for example, by bond wire 265 (FIG. 2).
[0038] The heat dissipation member 251 has a function of removing heat from a member arranged thereon. In other words, the heat dissipation member 251 is a heat sink. Therefore, the heat dissipation member 251 preferably has high thermal conductivity, and from this viewpoint, it is typically formed of a metal. The metal is, for example, copper (Cu), a copper alloy, or a laminate material thereof. The copper alloy is, for example, a copper molybdenum alloy (Cu-Mo). As a laminate material, for example, a laminate material having a three-layer structure (Cu / Cu-Mo / Cu) of copper (Cu), a copper molybdenum alloy (Cu-Mo), and copper (Cu) is well known in the art as a material having high thermal conductivity and a linear expansion coefficient in an in-plane direction that is easily compatible with typical ceramic materials. Note that the alloy here refers to a mixture that is not solid-solutioned and an intermetallic compound in addition to a solid solution made of a plurality of metal components. The heat dissipation member 251 may have a plate-like shape. In other words, the heat dissipation member 251 may be a heat dissipation plate.
[0039] The heat dissipation member 251 faces each of the source terminal S (FIG. 1) of the semiconductor switching element 271 and the lower surface SF2 (second surface) (FIG. 4) of the ceramic member 10 of the noise filter 101. A conductive adhesive (not shown) bonds the heat dissipation member 251 and the source terminal S of the semiconductor switching element 271 to each other. A conductive adhesive 252 bonds the heat dissipation member 251 and at least one ground electrode terminal 30a, 30b (FIG. 4) of the noise filter 101 to each other. The conductive adhesive 252 connects the heat dissipation member 251 and the insulating film 90 (insulator) (FIG. 4) of the noise filter 101 to each other in the thickness direction (vertical direction in FIG. 4). The conductive adhesive 252 contains a metal, such as silver (Ag). The conductive adhesive 252 may be, for example, solder. Therefore, the conductive adhesive 252 has not only a current carrying function but also a heat conducting function. The material of the conductive adhesive for the semiconductor switching element 271 and the material of the conductive adhesive 252 for the noise filter 101 may be the same as or different from each other.
[0040] The electronic device 200 may further include a frame 280 (FIGS. 2 and 3) and a lid 295 (FIG. 3). The frame 280 is provided on the heat dissipation member 251, and surrounds the noise filter 101 and the semiconductor switching element 271 on the heat dissipation member 251. The frame 280 supports a main lead 291 and a control lead 292. A metallized layer 281 and a metallized layer 282 to which the main lead 291 and the control lead 292 are respectively bonded may be provided on the frame 280. The lid 295 is attached to the frame 280 so as to seal a space CV (FIG. 3) surrounded by the frame 280 on the heat dissipation member 251.
[0041] 5 to 7 are a cross-sectional view, a top view, and a bottom view, respectively, that show a schematic configuration of noise filter 101 in this embodiment. Note that the terms "top surface" and "bottom surface" are used in this specification with the intention of distinguishing between opposite surfaces, and do not imply any limitation related to the direction of gravity.
[0042] The noise filter 101 has a ceramic member 10, at least one ground internal electrode layer 20, at least one second internal electrode layer 21, and at least one first internal electrode layer 22. When a plurality of ground internal electrode layers 20 are used, they are electrically connected to each other. In other words, the plurality of ground internal electrode layers 20 are electrically connected to each other. When a plurality of second internal electrode layers 21 are used, they are electrically connected to each other. In other words, the plurality of second internal electrode layers 21 are electrically connected to each other. When a plurality of first internal electrode layers 22 are used, they are electrically connected to each other. In other words, the plurality of first internal electrode layers 22 are electrically connected to each other. These electrical connections may be made using via electrodes arranged in the ceramic member 10, as described later. In the following, a detailed description will be given of a case in which a plurality of ground internal electrode layers 20, one second internal electrode layer 21, and a plurality of first internal electrode layers 22 are used.
[0043] The ceramic member 10 has an upper surface SF1 (first surface) and a lower surface SF2 (second surface) that are opposite to each other in the thickness direction. The upper surface SF1 may be a flat surface. The lower surface SF2 may be a flat surface. The ceramic member 10 has electrical insulation properties. The ceramic member 10 may be made of low temperature co-fired ceramics (LTCC) to enable simultaneous firing with the ground internal electrode layer 20, the second internal electrode layer 21, and the first internal electrode layer 22. The relative dielectric constant of the ceramic member 10 may be 20 or more to easily form the capacitance C1 and the capacitance C2. The relative dielectric constant of the ceramic member 10 may be 300 or less, for example, in order to optimize other characteristics other than the dielectric constant characteristic.
[0044] The ground internal electrode layer 20, the second internal electrode layer 21, and the first internal electrode layer 22 are disposed in the ceramic member 10. The ground internal electrode layer 20 and the non-ground internal electrode layers including the second internal electrode layer 21 and the first internal electrode layer 22 may be disposed alternately in the thickness direction in the ceramic member 10. The second internal electrode layer 21 faces at least one ground internal electrode layer 20 so as to form a capacitance C1, and faces the upper ground internal electrode layer 20 and the lower ground internal electrode layer in the thickness direction in FIG. 5. The first internal electrode layer 22 faces at least one ground internal electrode layer 20 so as to form a capacitance C2, and faces the upper ground internal electrode layer 20 and the lower ground internal electrode layer in the thickness direction in FIG. 5.
[0045] 5, the first internal electrode layer 22 is formed inside the ground via electrodes 40a and 40b in the direction perpendicular to the thickness direction (horizontal direction in the figure), but at least a part of the first internal electrode layer 22 may be formed outside the ground via electrodes 40a and 40b. The same applies to the second internal electrode layer 21.
[0046] 5, the second internal electrode layer 21 may be disposed in the thickness direction between the first internal electrode layer 22 and the upper surface SF1 of the ceramic component 10. According to the present inventor's simulation, this makes it easier to suppress electrical loss caused by the noise filter 101.
[0047] 5, the electrode layer closest to the upper surface SF1 is the ground internal electrode layer 20, but as a modified example, it may be the second internal electrode layer 21 or the first internal electrode layer 22. Similarly, the electrode layer closest to the lower surface SF2 is the ground internal electrode layer 20 in FIG. 5, but as a modified example, it may be the second internal electrode layer 21 or the first internal electrode layer 22.
[0048] The noise filter 101 has at least one via electrode 41 connected to the second internal electrode layer 21 and at least one via electrode 42 connected to the first internal electrode layer 22. Figs. 6 and 7 show an example in which a plurality of via electrodes 41 arranged in parallel with each other and a plurality of via electrodes 42 arranged in parallel with each other are provided. In other words, a plurality of via electrodes 42 are provided in at least one ceramic layer located between the first internal electrode layers adjacent to each other in the thickness direction of the ceramic member 10. Also, a plurality of via electrodes 41 are provided in at least one ceramic layer located between the second internal electrode layers adjacent to each other in the thickness direction of the ceramic member 10.
[0049] When a plurality of first internal electrode layers 22 are provided, each via electrode 42 may extend along the thickness direction (vertical direction in FIG. 5) so as to be in contact with all of the plurality of first internal electrode layers 22, or may extend in the thickness direction so as to be in contact with only a portion of the first internal electrode layers 22 among the plurality of first internal electrode layers 22. Similarly, when a plurality of second internal electrode layers 21 are provided, each via electrode 41 may extend along the thickness direction (vertical direction in FIG. 5) so as to be in contact with all of the plurality of second internal electrode layers 21, or may extend in the thickness direction so as to be in contact with only a portion of the second internal electrode layers 21 among the plurality of second internal electrode layers 21.
[0050] The number and arrangement of the via electrodes 42 may be common to each ceramic layer or may differ from each other. Similarly, the number and arrangement of the via electrodes 41 may be common to each ceramic layer or may differ from each other.
[0051] The multiple via electrodes 41 are also referred to as a first via electrode group 41P, and the multiple via electrodes 42 are also referred to as a second via electrode group 42P.
[0052] The noise filter 101 further has at least one ground electrode terminal on the lower surface SF2 of the ceramic member 10. In this embodiment, the at least one ground electrode terminal is directly disposed on the lower surface SF2. In the following, a case where a plurality of ground electrode terminals, specifically, a ground electrode terminal 30a (first ground electrode terminal) and a ground electrode terminal 30b (second ground electrode terminal), are used will be described in detail. The ground electrode terminals 30a and 30b may be collectively referred to as the ground electrode terminals 30. The ground electrode terminals 30 are electrically connected to the ground internal electrode layer 20.
[0053] In the case where the ground electrode terminal 30a and the ground electrode terminal 30b are provided as at least one ground electrode terminal as described above, the noise filter 101 has at least one ground via electrode 40a connected to the ground electrode terminal 30a and at least one ground via electrode 40b connected to the ground electrode terminal 30b. FIG. 7 shows an example in which a plurality of ground via electrodes 40a arranged in parallel with each other and a plurality of ground via electrodes 40b arranged in parallel with each other are provided. In other words, a plurality of ground via electrodes 40a and a plurality of ground via electrodes 40b are provided in at least one ceramic layer located between the ground internal electrode layers 20 adjacent to each other in the thickness direction of the ceramic member 10. Each ground via electrode may extend along the thickness direction (the vertical direction in FIG. 5) so as to contact all of the ground internal electrode layers 20, or may extend along the thickness direction so as to contact only some of the ground internal electrode layers 20 among the ground internal electrode layers 20. The number and arrangement of these ground via electrodes may be common to each ceramic layer or may be different. The ground via electrodes 40a are also referred to as a ground via electrode group 40aP, and the ground via electrodes 40b are also referred to as a ground via electrode group 40bP. The ground via electrodes 40a electrically connect the ground internal electrode layers 20 to each other. The ground via electrodes 40b also electrically connect the ground internal electrode layers 20 to each other.
[0054] The noise filter 101 further has an external electrode terminal 31 on the upper surface SF1 of the ceramic member 10. The external electrode terminal 31 is connected to the via electrode 41, and thereby electrically connected to the second internal electrode layer 21.
[0055] The noise filter 101 may further include a test electrode terminal 32 (second electrode terminal) on the upper surface SF1 of the ceramic member 10. The test electrode terminal 32 is electrically connected to the first internal electrode layer 22 by being connected to the via electrode 42. In a planar layout perpendicular to the thickness direction, the shape of the test electrode terminal 32 does not have to be congruent with the shape of the external electrode terminal 31. Specifically, the area of the test electrode terminal 32 may be smaller than the area of the external electrode terminal 31, and instead of or in addition to this, the shape of the test electrode terminal 32 may be different from the shape of the external electrode terminal 31. Note that the test electrode terminal 32 may be disposed on a side surface connecting the upper surface SF1 and the lower surface SF2 instead of on the upper surface SF1 of the ceramic member 10. In this case, at least one of the first internal electrode layers 22 may extend to have an end portion that reaches the side surface of the ceramic member 10, and the test electrode terminal 32 may be disposed on the side surface of the ceramic member 10 so as to contact the end portion. Furthermore, the test electrode terminal 32 may be omitted if it is unnecessary.
[0056] The noise filter 101 further has a resistive element 80 on the lower surface SF2 of the ceramic member 10. The resistive element 80 may be disposed between the ground electrode terminal 30a and the ground electrode terminal 30b in a planar layout perpendicular to the thickness direction. Specifically, in the present embodiment, the resistive element 80 may be disposed between the ground electrode terminal 30a and the ground electrode terminal 30b on the lower surface SF2. The resistive element 80 has a first end 81 electrically connected to the second internal electrode layer 21 and a second end 82 electrically connected to the first internal electrode layer 22. Here, since the second internal electrode layer 21 is electrically connected to the external electrode terminal 31, the first end 81 of the resistive element 80 is also electrically connected to the external electrode terminal 31. Moreover, since the first internal electrode layer 22 is electrically connected to the test electrode terminal 32, the second end 82 of the resistive element 80 is also electrically connected to the test electrode terminal 32. The resistive element 80 has an electrical resistance corresponding to the resistance R (FIG. 1) between a first end 81 and a second end 82. The resistive element 80 may be made of a resistive material having a lower electrical conductivity than the electrode material. A known thick-film resistor may be used as the resistive element 80. For example, a thick-film resistor containing Pd and Ag (Pd-Ag thick-film resistor) is well known.
[0057] The noise filter 101 may further have a first resistor electrode terminal 71 and a second resistor electrode terminal 72 on the lower surface SF2 of the ceramic member 10 in order to reliably and stably obtain electrical connection to the resistor element 80. The first resistor electrode terminal 71 and the second resistor electrode terminal 72 are in contact with the first end 81 and the second end 82 of the resistor element 80, respectively. Furthermore, the first resistor electrode terminal 71 and the second resistor electrode terminal 72 are in contact with the via electrode 41 and the via electrode 42, respectively. Thus, the first end 81 of the resistor element 80 is electrically connected to the external electrode terminal 31 through the first resistor electrode terminal 71 and the via electrode 41. Furthermore, the second end 82 of the resistor element 80 is electrically connected to the test electrode terminal 32 through the second resistor electrode terminal 72 and the via electrode 42. As a modified example, the first resistive electrode terminal 71 and the second resistive electrode terminal 72 may be omitted by directly contacting the via electrode 41 and the via electrode 42 to the first end 81 and the second end 82 of the resistive element 80, respectively. However, the following describes the case where the first resistive electrode terminal 71 and the second resistive electrode terminal 72 are used.
[0058] The noise filter 101 further includes an insulating film 90 (insulator). The insulating film 90 covers the resistor element 80. As a result, the insulating film 90 electrically insulates the conductive adhesive 252 from the resistor element 80. The insulating film 90 also covers the first resistor electrode terminal 71 and the second resistor electrode terminal 72. As a result, the insulating film 90 electrically insulates the conductive adhesive 252 from each of the first resistor electrode terminal 71 and the second resistor electrode terminal 72. The insulating film 90 preferably has high electrical insulation. In addition, it is assumed that the electronic device 200 will be mounted on another member (typically a substrate (not shown)) not shown, and this mounting is often performed by a process involving high-temperature heating such as a solder reflow process. Therefore, it is preferable that the insulating film 90 has high heat resistance of a typical reflow temperature (for example, about 250° C.) or higher. From this viewpoint, the insulating film 90 is preferably an inorganic insulating film, for example, a glass film. However, the insulating film 90 may be a resin film as long as it has sufficient heat resistance. The insulating film 90 has a thickness of, for example, 20 μm or more from the viewpoint of electrical insulation, and has a thickness of, for example, 40 μm or less from the viewpoint of not excessively inhibiting heat dissipation from the resistance element 80.
[0059] Next, a manufacturing method of the noise filter 101 will be briefly described below.
[0060] First, a fired body is formed having the ceramic member 10, the ground internal electrode layer 20, the second internal electrode layer 21, the first internal electrode layer 22, the ground via electrode 40a, the ground via electrode 40b, the via electrode 41, and the via electrode 42. The fired body may be formed using a known multilayer ceramic technique. For example, the following steps are performed in order: forming a ceramic green sheet, forming a via hole corresponding to the via electrode design, filling the via hole with an electrode paste (e.g., AgPd paste), printing the electrode paste (e.g., AgPd paste) corresponding to the electrode layer design, laminating the ceramic green sheets to form a laminate, and firing the laminate to form a fired body. The thicknesses of the ceramic green sheets constituting the laminate may be the same or different from each other.
[0061] Next, on the upper surface SF1 of the sintered body obtained by the above process, an electrode paste (for example, Au paste) that will become the external electrode terminal 31 and the test electrode terminal 32 is printed. Also, on the lower surface SF2 of the sintered body, a resistor paste (for example, paste for Pd-Ag thick film resistor) that will become the resistor element 80, an electrode paste (for example, AgPt paste) that will become the first resistor electrode terminal 71, the second resistor electrode terminal 72, the ground electrode terminal 30a, and the ground electrode terminal 30b, and a glass paste that will become the insulating film 90 are printed. Then, the above-mentioned paste bodies on the upper surface SF1 and the lower surface SF2 are fired. Note that the firing of these paste bodies does not necessarily need to be performed after all of the above paste bodies on the upper surface SF1 and the lower surface SF2 of the sintered body are applied, and after applying and firing a part of the paste body, applying and firing another paste body may be performed. For example, as a modification of the manufacturing method in the above-mentioned embodiment, the manufacturing methods of the first to third modifications described later may be performed.
[0062] As described above, in the present embodiment, the first resistive electrode terminal 71, the second resistive electrode terminal 72, the resistive element 80, and the insulating film 90 may be formed after firing the ceramic member 10. Therefore, it is not necessary to select the materials of the first resistive electrode terminal 71, the second resistive electrode terminal 72, the resistive element 80, and the insulating film 90 so that they can be fired simultaneously with the ceramic member 10.
[0063] In the first modified example, the sintered body is first formed. Next, an electrode paste (e.g., Au paste) that will become the external electrode terminal 31 and the test electrode terminal 32 is printed on the upper surface SF1 of the sintered body, and an electrode paste (e.g., AgPt paste) that will become the first resistor electrode terminal 71, the second resistor electrode terminal 72, the ground electrode terminal 30a, and the ground electrode terminal 30b is printed on the lower surface SF2 of the sintered body. Then, the above-mentioned paste bodies on the upper surface SF1 and the lower surface SF2 are fired. Next, a resistor paste (e.g., paste for a Pd-Ag thick film resistor) that will become the resistor element 80 is printed on the lower surface SF2 of the sintered body, and this paste body is fired. Next, a glass paste that will become the insulating film 90 is printed on the lower surface SF2 of the sintered body, and this paste body is fired.
[0064] In the second modification, an electrode paste (e.g., Au paste) that will become the external electrode terminal 31 and the test electrode terminal 32 is printed on the upper surface SF1 of the laminate, and an electrode paste (e.g., AgPt paste) that will become the first resistor electrode terminal 71, the second resistor electrode terminal 72, the ground electrode terminal 30a, and the ground electrode terminal 30b is printed on the lower surface SF2 of the laminate. Then, the laminate and the above-mentioned paste bodies on the upper surface SF1 and the lower surface SF2 are fired simultaneously. Next, a resistor paste (e.g., paste for a Pd-Ag thick film resistor) that will become the resistor element 80 is printed on the lower surface SF2 of the sintered body obtained by the firing, and this paste body is fired. Next, a glass paste that will become the insulating film 90 is printed on the lower surface SF2 of the sintered body, and this paste body is fired.
[0065] In the third modified example, an electrode paste (e.g., Au paste) that will become the external electrode terminal 31 and the test electrode terminal 32 is printed on the upper surface SF1 of the laminate, and an electrode paste (e.g., AgPt paste) that will become the first resistor electrode terminal 71, the second resistor electrode terminal 72, the ground electrode terminal 30a, and the ground electrode terminal 30b, and a resistor paste (e.g., paste for a Pd-Ag thick film resistor) that will become the resistor element 80 are printed on the lower surface SF2 of the laminate. Then, the laminate and the above-mentioned paste bodies on the upper surface SF1 and the lower surface SF2 are fired at the same time. Next, a glass paste that will become the insulating film 90 is printed on the lower surface SF2 of the sintered body, and this paste body is fired.
[0066] In any of the manufacturing method of the present embodiment and its first to third modified examples, the laminate is fired to form a fired body, and then the insulating film 90 is formed by firing the glass paste. Therefore, when the laminate is fired, the glass paste is not applied to the laminate. This prevents the conductive components in the laminate from diffusing into the glass during firing of the laminate. This makes it possible to suppress the amount of conductive components diffusing into the insulating film 90.
[0067] As a conventional technique for mass production, after a single block as a semi-finished product including portions that will become multiple noise filters 101 is formed by the above-described manufacturing method, the semi-finished product may be diced to cut out multiple noise filters 101.
[0068] Fig. 8 is a partial cross-sectional view showing the configuration of an electronic device 200C of a comparative example in the same field of view as that of Fig. 4. The electronic device 200C has a noise filter 101C of a comparative example. In the noise filter 101C, a resistive element 80 is disposed on an upper surface SF1, not on a lower surface SF2.
[0069] FIG. 9 is a graph showing the relationship between the power consumption of the resistive element 80 and the surface temperatures of the heat dissipation member 251 and the noise filter 101C in the electronic device 200C of the comparative example. FIG. 10 is a graph showing the relationship between the power consumption of the resistive element 80 and the surface temperatures of the heat dissipation member 251 and the noise filter 101 in the electronic device 200 of the example corresponding to the present embodiment. In common with both, a heat sink having a three-layer structure (Cu / Cu-Mo / Cu) was used as the heat dissipation member 251. The dimensions of the noise filter were length 3 mm x width 1 mm x thickness 0.5 mm. The capacitance C1 was 0.15 nF, the capacitance C2 was 1.1 nF, and the resistance R was 2 Ω. The plots in each graph indicate the measurement points. The numerical values of the surface temperatures for the representative values of the power consumption obtained from linear approximation for these measurement points are shown in Table 1 below.
[0070] [Table 1]
[0071] When comparing at a power consumption of 3 W, the surface temperature of the noise filter 101C of the comparative example was about 160° C., whereas the surface temperature of the noise filter 101 of the embodiment was 90° C. The temperature range in which the characteristics of the ceramic material constituting the ceramic member 10 are guaranteed is, for example, −55° C. to +125° C., and the temperature range in which the characteristics of the resistor material constituting the resistance element 80 are guaranteed is, for example, 25° C. to 150° C. In the comparative example, therefore, there is concern that the characteristics of the ceramic member 10 and the resistance element 80 may vary excessively due to the excessively high surface temperature of the noise filter 101C. This excessive variation may lead to excessive variation of at least one of the resistance R, the capacitance C1, and the capacitance C2, and as a result, the operation of the electronic device 200C as a power amplifier may become unstable. In contrast, in the embodiment, the surface temperature of the noise filter 101 is sufficiently low, and therefore it is considered that the desired characteristics of the ceramic member 10 and the resistance element 80 are sufficiently maintained. In the embodiment, even when the power consumption was further increased to 4 W, the surface temperature was sufficiently suppressed.
[0072] The reason why the surface temperature of noise filter 101C of the comparative example was high as described above is believed to be that the efficiency of heat dissipation from resistance element 80 in electronic device 200C of the comparative example is low. Specifically, in electronic device 200C, heat generated from resistance element 80 is removed by dissipation into the atmosphere above upper surface SF1 and by dissipation to heat dissipation member 251 via ceramic member 10, but the former atmospheric cooling action is generally less efficient than the cooling action using a heat dissipation member, and the latter heat dissipation action is also considered to be less efficient because the thermal conductivity of the ceramic material constituting ceramic member 10 is generally low.
[0073] 4, the ground electrode terminal 30 and the resistive element 80 are both disposed on the lower surface SF2 of the ceramic member 10. As a result, in the electronic device 200 in which the ground electrode terminal 30 of the noise filter 101 is joined to the heat dissipation member 251, the resistive element 80 faces the heat dissipation member 251. This allows the resistive element 80 to be disposed close to the heat dissipation member 251. This increases the efficiency of heat dissipation from the resistive element 80. This makes it possible to suppress instability in the operation of the power amplifier caused by a temperature rise accompanying power consumption in the resistive element 80 of the noise filter 101.
[0074] The noise filter 101 may have a test electrode terminal 32. As a result, the first end 81 and the second end 82 of the resistive element 80 are electrically connected to the external electrode terminal 31 and the test electrode terminal 32, respectively. Therefore, the resistance value of the resistive element 80 can be inspected by measuring the resistance value between the external electrode terminal 31 and the test electrode terminal 32. Note that the connection of a measuring device for this inspection can be performed, for example, by contacting a probe electrode with the external electrode terminal 31 and the test electrode terminal 32. After this inspection, a bonding wire 261 (FIG. 2) is connected to the external electrode terminal 31 as an electrical wiring, but it is optional whether or not an electrical wiring is connected to the test electrode terminal 32, and usually it is not necessary to connect it.
[0075] As shown in FIG. 6, the shape of the test electrode terminal 32 does not have to be the same as the shape of the external electrode terminal 31. This makes it easy to distinguish the test electrode terminal 32 from the external electrode terminal 31 based on their appearances. In particular, as shown in FIG. 6, when the area of the test electrode terminal 32 is smaller than that of the external electrode terminal 31, the material cost of the test electrode terminal 32 can be reduced compared to when the area of the test electrode terminal 32 is equal to or larger than that of the external electrode terminal 31. This effect is large when the test electrode terminal 32 contains a precious metal that requires high material costs, and is particularly large when it contains gold (Au). It is assumed that the external electrode terminal 31 handles the main current of the semiconductor switching element 271, while the test electrode terminal 32 handles a small current for inspecting the resistance value of the resistor element 80. Therefore, the test electrode terminal 32 does not need to be large enough to handle the main current, and therefore its function can be sufficiently ensured even if it has an area smaller than that of the external electrode terminal 31. From this viewpoint, the area of the test electrode terminal 32 is preferably 80% or less, and more preferably 60% or less, of the external electrode terminal 31. If the area of the test electrode terminal 32 is excessively small, it becomes difficult to make electrical connection for testing purposes. From this viewpoint, the area of the test electrode terminal 32 is, for example, preferably 10% or more, and more preferably 20% or more, of the external electrode terminal 31.
[0076] When the area of the test electrode terminal 32 is made larger than that of the external electrode terminal 31 in order to distinguish between the test electrode terminal 32 and the external electrode terminal 31, the area of the test electrode terminal 32 is preferably 110% or more, and more preferably 120% or more, of the external electrode terminal 31 in order to make it easy to distinguish the sizes by visual inspection. However, in terms of reducing costs, the area of the test electrode terminal 32 is preferably 180% or less, and more preferably 160% or less, of the area of the external electrode terminal 31. The shape of the test electrode terminal 32 and the shape of the external electrode terminal 31 may be different from each other. In this case, as in the above, there is an advantage that it is easy to distinguish between the test electrode terminal 32 and the external electrode terminal 31.
[0077] As shown in Fig. 4, the ground electrode terminal 30 may include a ground electrode terminal 30a and a ground electrode terminal 30b. The resistive element 80 is disposed between the first ground electrode terminal 30a and the second ground electrode terminal 30b in a planar layout perpendicular to the thickness direction. This arrangement allows the ground electrode terminal 30a and the ground electrode terminal 30b to be disposed on one side and the other side of the resistive element 80 in the length direction (the horizontal direction in Fig. 4) in a well-balanced manner in the planar layout. This makes it possible to suppress, for example, the inclination of the noise filter 101 when it is mounted on the heat dissipation member 251.
[0078] The noise filter 101 may have a single ground via electrode 40a, or may have multiple ground via electrodes 40a (ground via electrode group 40aP) as shown in Fig. 7. In the latter case, even if one ground via electrode 40a is disconnected for some reason, the wiring function of the ground via electrode group 40aP can be roughly maintained. The noise filter 101 may have a single ground via electrode 40b, or may have multiple ground via electrodes 40b (ground via electrode group 40bP) as shown in Fig. 7. In the latter case, even if one ground via electrode 40b is disconnected for some reason, the wiring function of the ground via electrode group 40bP can be roughly maintained.
[0079] The noise filter 101 may have a single via electrode 41, or may have a plurality of via electrodes 41 (first via electrode group 41P) as shown in FIG. 6 and FIG. 7. In the latter case, even if one via electrode 41 is disconnected for some reason, the wiring function of the first via electrode group 41P can be roughly maintained. The noise filter 101 may have a single via electrode 42, or may have a plurality of via electrodes 42 (second via electrode group 42P) as shown in FIG. 6 and FIG. 7. In the latter case, even if a part of the second via electrode group 42P is disconnected for some reason, the wiring function of the second via electrode group 42P can be roughly maintained. However, the larger the total area in the planar layout of the via electrode 41 located between a pair of second internal electrode layers adjacent to each other in the thickness direction of the ceramic member 10 and the via electrode 42 located between a pair of first internal electrode layers adjacent to each other in the thickness direction, the smaller the capacitance becomes. Therefore, if the via electrodes have a total area CS between a pair of internal electrode layers (preferably between each pair), the total area CS is preferably 10% or less, more preferably 5% or less, of the area where the pair of internal electrode layers overlap in a planar layout. Each via electrode 42 may extend along the thickness direction (vertical direction in FIG. 5) so as to contact all of the first internal electrode layers 22, or may extend along the thickness direction so as to contact only some of the first internal electrode layers 22 among the first internal electrode layers 22. The number and arrangement of the via electrodes 42 may be the same or different for each layer. The number and arrangement of the via electrodes 41 may also be the same or different for each layer.
[0080] 5, the second internal electrode layer 21 and the first internal electrode layer 22 are formed inside the ground via electrodes 40a and 40b in the direction perpendicular to the thickness direction (horizontal direction in the figure), but when at least a part of the second internal electrode layer 21 and the first internal electrode layer 22 is formed outside the ground via electrodes 40a and 40b, the larger the total area of the ground via electrodes 40a and 40b in the planar layout, the more difficult it is to ensure a large capacitance. Therefore, if the ground via electrodes 40a and 40b have a total area CG between a pair of ground internal electrode layers 20 adjacent to each other in the thickness direction (preferably between each pair), the total area CG is preferably 10% or less, more preferably 5% or less, of the area where the pair of ground internal electrode layers 20 overlap each other in the planar layout.
[0081] 4, the conductive adhesive 252 may have a portion disposed between the heat dissipation member 251 and the resistance element 80 in the thickness direction. Specifically, the conductive adhesive 252 may connect the heat dissipation member 251 and the insulating film 90 to each other in the thickness direction. Since the conductive adhesive 252 also has excellent thermal conductivity, the thermal conductivity between the heat dissipation member 251 and the insulating film 90 is thereby increased. Therefore, the efficiency of heat dissipation from the resistance element 80 covered with the insulating film 90 can be improved.
[0082] Unlike a noise filter 105 (FIGS. 14 and 15) described later, the provision of the second internal electrode layer 21 allows a capacitance C1 to be formed within the ceramic member 10. In particular, in the configuration shown in FIG. 5, the ground internal electrode layer 20 between the first internal electrode layer 22 and the second internal electrode layer 21 can be utilized for both the capacitance C1 and the capacitance C2.
[0083] <Embodiment 2> 11 is a cross-sectional view showing a schematic configuration of a noise filter 102 according to the present embodiment. The noise filter 102 according to the present embodiment has an electrically insulating ceramic film 91 (insulating film in the second embodiment) instead of the insulating film 90 in the noise filter 101 (FIG. 5: the first embodiment). The ground electrode terminal 30a and the ground electrode terminal 30b are directly disposed on the lower surface SF2 in the noise filter 101 (FIG. 5: the above-mentioned first embodiment), but in the noise filter 102 (FIG. 11: the second embodiment), they are indirectly disposed on the lower surface SF2 via the ceramic film 91. The ceramic film 91 has a portion covering the lower surface of the resistance element 80, and the thickness of the thinnest portion of the portion is desirably 10 μm or more from the viewpoint of ensuring electrical insulation, and desirably 40 μm or less from the viewpoint of sufficiently suppressing thermal resistance.
[0084] In the manufacturing method of the noise filter 102, unlike the manufacturing method of the first embodiment described above, the ceramic film 91, the resistor element 80, the first resistor electrode terminal 71, and the second resistor electrode terminal 72 are fired simultaneously with the firing of the ceramic member 10. This reduces the number of steps, thereby enabling the manufacturing cost to be reduced. As a result of this firing, the ceramic member 10 and the ceramic film 91 are sintered together, and they form one ceramic body RC. The material of the ceramic film 91 may be the same as the material of the ceramic member 10, or may be different. In the former case, the sintering shrinkage of the ceramic member 10 and the sintering shrinkage of the ceramic film 91 during firing are the same, so that the occurrence of delamination between them during firing is suppressed.
[0085] In this embodiment, the resistor element 80, the first resistor electrode terminal 71, and the second resistor electrode terminal 72 are disposed in the ceramic body RC. The ceramic body RC shares an upper surface SF1 with the ceramic member 10, and has an opposite lower surface SF3. The ground electrode terminals 30a and 30b are disposed on the lower surface SF3. The ground electrode terminals 30a and 30b may be connected to the ground internal electrode layer 20 through the ceramic film 91.
[0086] The noise filter 102 (FIG. 11: this embodiment) can be used in the electronic device 200 (FIG. 4) in place of the noise filter 101 (FIG. 5: the above-described embodiment 1). In either embodiment, the ground electrode terminal 30a and the ground electrode terminal 30b are bonded to the heat dissipation member 251 with a conductive adhesive 252. Since the lower surface of the noise filter 102 as the bonded surface is formed by the lower surface SF3 of the ceramic film 91 as in this embodiment, the flatness of the bonded surface of the noise filter 102 can be more easily ensured. This makes it easier to balance the noise filter 102 when bonding it to the heat dissipation member 251 (FIG. 4), and therefore makes it possible to perform more stable bonding.
[0087] Since the configuration other than the above is substantially the same as that of the first embodiment, the same or corresponding elements are given the same reference numerals and the description thereof will not be repeated.
[0088] <Embodiment 3> FIG. 12 is a cross-sectional view that shows a schematic configuration of a noise filter 103 according to the present embodiment. In the noise filter 103 according to the present embodiment, unlike the noise filter 101 (FIG. 5: embodiment 1), the resistive element 80 is completely embedded in the ceramic member 10. In other words, the resistive element 80 is disposed between the upper surface SF1 and the lower surface SF2 of the ceramic member 10 in the thickness direction. Specifically, the resistive element 80 is disposed between all the internal electrode layers, including the first internal electrode layer 22 and the ground internal electrode layer 20, and the second surface SF2 of the ceramic member in the thickness direction. In the example shown in FIG. 12, all the internal electrode layers also include the second internal electrode layer 21. The first resistive electrode terminal 71 and the second resistive electrode terminal 72 may also be completely embedded in the ceramic member 10.
[0089] In the manufacturing method of the noise filter 103, unlike the manufacturing method of the first embodiment described above, the firing of the resistive element 80, the first resistive electrode terminal 71, and the second resistive electrode terminal 72 is performed simultaneously with the firing of the ceramic member 10. This reduces the number of steps, thereby enabling the manufacturing cost to be reduced.
[0090] Noise filter 103 (FIG. 12: this embodiment) can be used in electronic device 200 (FIG. 4) in place of noise filter 101 (FIG. 5: the above-described first embodiment). In either embodiment, ground electrode terminal 30a and ground electrode terminal 30b are bonded to heat dissipation member 251 with conductive adhesive 252. Since resistor element 80 is completely embedded in ceramic member 10 as in this embodiment, resistor element 80 can be electrically insulated from conductive adhesive 252 (see FIG. 4) without insulating film 90 (FIG. 5: first embodiment).
[0091] Moreover, according to the noise filter 103 (FIG. 12: this embodiment), the portion of the lower surface of the noise filter 101 (FIG. 5) that was constituted by the insulating film 90 can be constituted by the ceramic member 10. This makes it easier to ensure the flatness of the lower surface of the noise filter 103 as the adherend surface. This makes it easier to balance the noise filter 103 when adhering it to the heat dissipation member 251 (FIG. 4) using the conductive adhesive 252, thereby enabling more stable adhesion.
[0092] Since the configuration other than the above is substantially the same as that of the first embodiment, the same or corresponding elements are given the same reference numerals and the description thereof will not be repeated.
[0093] <Fourth embodiment> FIG. 13 is a cross-sectional view that illustrates a schematic configuration of noise filter 104 in the present embodiment.
[0094] The resistive element 80 is only partially embedded in the ceramic member 10. Specifically, in this embodiment, the lower surface SF2 of the ceramic member 10 is not a flat surface but has a recessed portion (the central portion in FIG. 13). The resistive element 80 is disposed in this recessed portion. Thus, in the noise filter 104, unlike the noise filter 103 (FIG. 12: embodiment 3), the resistive element 80 is not disposed between the upper surface SF1 and the lower surface SF2 of the ceramic member 10 in the thickness direction. Also, as shown in FIG. 13, the resistive element 80 may have a portion protruding from the recessed portion.
[0095] The noise filter 104 has an insulating film 90 (insulator) that completely buries the resistive element 80 together with the ceramic member 10. This makes it possible to electrically insulate the resistive element 80 from the conductive adhesive 252 (see FIG. 4) in an electronic device 200 (see FIG. 4) having a configuration in which the noise filter 104 is bonded to a heat dissipation member 251 instead of the noise filter 101.
[0096] In the manufacturing method of the noise filter 104, the first resistive electrode terminal 71 and the second resistive electrode terminal 72 may be fired simultaneously with the firing of the ceramic member 10. The firing for forming the ground electrode terminal 30a and the ground electrode terminal 30b may also be performed simultaneously. The firing of the resistive element 80 may be performed simultaneously with this firing, or may be performed after this firing. On the other hand, the printing and firing of the glass paste for forming the insulating film 90 are performed after the firing of the ceramic member 10. This suppresses the conductive components in the ceramic member 10 from diffusing into the glass. Therefore, the amount of the conductive components diffusing into the insulating film 90 can be suppressed. When the resistive element 80 is fired after the firing of the ceramic member 10, the printing and firing of the glass paste for forming the insulating film 90 may be performed after the firing of the resistive element 80, and this also suppresses the conductive components in the resistive element 80 from diffusing into the glass.
[0097] According to this embodiment, the resistor element 80 is partially embedded in the ceramic member 10. As a result, in this embodiment (FIG. 13), even if the insulating film 90 is thinner, the resistor element 80 can be sufficiently electrically insulated from the conductive adhesive 252 (FIG. 5) compared to the above-described first embodiment (FIG. 5). Note that, for the noise filter 101 (FIG. 5) in the above-described first embodiment and the noise filter 104 (FIG. 13) in this fourth embodiment, it is more preferable that the lower surface of the ground electrode terminal 30a, the lower surface of the insulating film 90, and the lower surface of the ground electrode terminal 30b are on the same plane. As a result, when the noise filter 101 (or the noise filter 104) is bonded to the heat dissipation member 251 (FIG. 4), the noise filter 101 (or the noise filter 104) is more easily balanced, and therefore stable bonding can be achieved. In particular, the noise filter 104 (FIG. 13) in this fourth embodiment has the advantage that even if the resistive element 80 and the insulating film 90 are thicker than the ground electrode terminals 30a, 30b, the lower surface of the ground electrode terminal 30a, the lower surface of the insulating film 90, and the lower surface of the ground electrode terminal 30b can be easily arranged on the same plane.
[0098] Since the configuration other than the above is substantially the same as that of the first embodiment, the same or corresponding elements are given the same reference numerals and the description thereof will not be repeated.
[0099] <Embodiment 5> 14 and 15 are cross-sectional views each showing a schematic equivalent circuit and configuration of the noise filter 105 in the present embodiment 5. The noise filter 105 (FIG. 14) does not have a capacitance C1, unlike the noise filter 101 (FIG. 1: embodiment 1). Correspondingly, the noise filter 105 (FIG. 15) does not have a second internal electrode layer 21 (FIG. 5: embodiment 1) for forming the capacitance C1. The present embodiment 5 also provides substantially the same effects as those described in the embodiment 1, except for the effects related to the capacitance C1.
[0100] <Sixth embodiment> FIG. 16 is a cross-sectional view that shows a schematic configuration of a noise filter 106 according to the sixth embodiment. In addition to the configuration of the noise filter 101 (FIG. 5: first embodiment), the noise filter 106 has a metal-containing layer 95 on an insulating film 90 (insulator), specifically, on the lower surface of the insulating film 90 in FIG. 16. The metal-containing layer 95 is a layer that contains metal. Specifically, the metal-containing layer 95 includes a portion made of metal at least on its surface (the lower surface in FIG. 16). Specifically, the metal-containing layer 95 may be substantially made of metal, or may be made of metal and ceramic dispersed in the metal. For example, when the insulating film 90 is formed by printing a glass film and then firing it, the metal-containing layer 95 may be formed by printing a silver paste or the like and then firing it after the firing.
[0101] The noise filter 106 has the metal-containing layer 95 on the insulating film 90, which can improve the adhesion between the noise filter 106 and the conductive adhesive material 252 (see FIG. 4). Also, the thermal resistance can be reduced.
[0102] As a modification, the metal-containing layer 95 may be applied to a modification of the first embodiment or to another embodiment other than the first embodiment, instead of the first embodiment. For example, the metal-containing layer 95 may be formed on the ceramic film 91 (insulator) of the noise filter 102 in the second embodiment. In this case, the metal-containing layer 95 may be formed by co-firing with the ceramic film 91. Also, the metal-containing layer 95 may be formed on the lower surface SF2 of the ceramic member 10 of the noise filter 103 in the third embodiment (in other words, the lower side of the ceramic member 10 in FIG. 12). In this case, the metal-containing layer 95 may be formed by co-firing with the ceramic member 10.
[0103] The above-mentioned first to sixth embodiments and their modifications may be freely combined with each other. Although the present invention has been described in detail, the above description is merely an example in all respects, and the present invention is not limited thereto. It is understood that countless modifications not illustrated can be envisioned without departing from the scope of the present invention. [Explanation of symbols]
[0104] 10: Ceramic components 20: Ground internal electrode layer 21: Second internal electrode layer 22: First internal electrode layer 30: Ground electrode terminal 30a: First ground electrode terminal 30b: second ground electrode terminal 31: External electrode terminal (first electrode terminal) 32: Test electrode terminal (second electrode terminal) 40a, 40b: Ground via electrodes 40aP, 40bP: Ground via electrode group 41, 42: Via electrodes 41P: First via electrode group 42P: Second via electrode group 80: Resistance element 81: First end 82: Second end 90: Insulating film (insulator) 91: Ceramic film (insulating film) 95: Metal-containing layer 101~106: Noise filters 200:Electronic equipment 251: Heat dissipation materials 252: Conductive adhesive 271: Semiconductor switching elements 280: Frame 291: Main lead 292: Control lead 295: Lid SF1: Top surface (first surface) SF2: Bottom surface (second surface)
Claims
1. A noise filter for a power amplifier, a ceramic member having a first surface and a second surface opposite to each other in a thickness direction and having electrical insulation properties; at least one ground internal electrode layer disposed within the ceramic member; at least one first internal electrode layer disposed in the ceramic member and facing the at least one ground internal electrode layer so as to form a first capacitance; a first electrode terminal disposed on the first surface of the ceramic member; at least one ground electrode terminal disposed on the second surface of the ceramic member and electrically connected to the at least one ground internal electrode layer; a resistive element disposed on the second surface of the ceramic member, the resistive element having a first end electrically connected to the first electrode terminal and a second end electrically connected to the at least one first internal electrode layer, the resistive element having an electrical resistance between the first end and the second end; an insulator covering the resistor element; A noise filter comprising:
2. 2. The noise filter according to claim 1, wherein the at least one ground electrode terminal is disposed directly on the second surface.
3. 3. The noise filter according to claim 2, wherein the insulator is a glass film.
4. 2. The noise filter according to claim 1, wherein the at least one ground electrode terminal is indirectly disposed on the second surface via the insulator.
5. 5. The noise filter according to claim 4, wherein the insulator is a ceramic film.
6. A noise filter for a power amplifier, a ceramic member having a first surface and a second surface opposite to each other in a thickness direction and having electrical insulation properties; at least one ground internal electrode layer disposed within the ceramic member; at least one first internal electrode layer disposed in the ceramic member and facing the at least one ground internal electrode layer so as to form a first capacitance; a first electrode terminal disposed on the first surface of the ceramic member; at least one ground electrode terminal disposed on the second surface of the ceramic member and electrically connected to the at least one ground internal electrode layer; a resistor element disposed between all the internal electrode layers including the at least one first internal electrode layer and the at least one ground internal electrode layer in the thickness direction and the second surface of the ceramic member, the resistor element having a first end electrically connected to the first electrode terminal and a second end electrically connected to the at least one first internal electrode layer, and having an electrical resistance between the first end and the second end; Equipped with The resistor element is at least partially embedded in the ceramic member.
7. 7. The noise filter according to claim 6, wherein the resistive element is completely embedded in the ceramic member.
8. 7. The noise filter according to claim 6, the resistive element is partially embedded in the ceramic member; The noise filter further includes an insulator that completely embeds the resistor element together with the ceramic member. Noise filter.
9. 9. The noise filter of claim 1, further comprising a metal-containing layer on the insulator.
10. 8. The noise filter of claim 7, further comprising a metal-containing layer on the ceramic member.
11. 9. The noise filter according to claim 1, further comprising a second electrode terminal disposed on the first surface of the ceramic member or on a side surface connecting the first surface and the second surface, and electrically connected to the at least one first internal electrode layer.
12. 12. The noise filter according to claim 11, wherein a shape of the second electrode terminal is not congruent with a shape of the first electrode terminal.
13. 9. The noise filter according to claim 1, wherein the at least one ground electrode terminal includes a first ground electrode terminal and a second ground electrode terminal, and the resistive element is disposed between the first ground electrode terminal and the second ground electrode terminal in a planar layout perpendicular to the thickness direction.
14. 9. The noise filter according to claim 1, the at least one ground electrode terminal and the at least one ground internal electrode layer are electrically connected to each other, and the at least one ground via electrode group includes a plurality of via electrodes arranged in parallel with each other.
15. 9. The noise filter according to claim 1, further comprising at least one second internal electrode layer disposed in the ceramic member, facing the at least one ground internal electrode layer so as to form a second capacitance, and electrically connected to the first electrode terminal.
16. 16. The noise filter according to claim 15, the noise filter further comprising a via electrode group including a plurality of via electrodes electrically connecting the first electrode terminal and the at least one second internal electrode layer and arranged in parallel with each other.
17. 9. The noise filter according to claim 1, the at least one internal electrode layer is a plurality of first internal electrode layers; the noise filter further comprising a via electrode group including a plurality of via electrodes electrically connecting the plurality of first internal electrode layers to each other and arranged in parallel to each other.
18. A noise filter according to any one of claims 1 to 8, a heat dissipation member facing the second surface of the ceramic member of the noise filter; a conductive adhesive material that bonds the at least one ground electrode terminal of the noise filter and the heat dissipation member to each other; An electronic device comprising:
19. 20. The electronic device according to claim 18, wherein the conductive adhesive has a portion disposed between the heat dissipation member and the resistive element in the thickness direction.
20. 20. The electronic device according to claim 18, a semiconductor switching element mounted on the heat dissipation member and having a first main terminal electrically connected to the heat dissipation member, a second main terminal spaced from the first main terminal, and a control terminal for receiving a signal for controlling switching between the first main terminal and the second main terminal; a control lead electrically connected to the control terminal of the semiconductor switching element; a main lead electrically connected to the second main terminal of the semiconductor switching element and the first electrode terminal of the noise filter; The electronic device further comprises:
21. 21. The electronic device according to claim 20, a frame provided on the heat dissipation member, surrounding the noise filter and the semiconductor switching element on the heat dissipation member and supporting the control lead and the main lead; a cover attached to the frame so as to seal a space surrounded by the frame on the heat dissipation member; and The electronic device further comprises:
Citation Information
Patent Citations
Center frequency band variable type band pass filter
JP2002246864A
Wide video bandwidth RF power amplifier
JP2022518866A