Nitride semiconductor device and method of manufacturing the same

The nitride semiconductor device addresses high parasitic capacitance issues by using a conductive substrate with a semi-insulating layer and insulator-filled groove, improving high-frequency performance.

JP2024142244AInactive Publication Date: 2024-10-10ROHM CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023054353
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

High-cost substrates such as semi-insulating SiC and high-resistance Si substrates are used for nitride semiconductor HEMTs, leading to high parasitic capacitance and inadequate high-frequency characteristics due to capacitive coupling with conductive substrates.

Method used

A nitride semiconductor device is designed with a conductive substrate having a semi-insulating layer and a nitride semiconductor layer, where a groove is etched in the substrate and filled with a buried electrode, and an insulator is placed inside the groove to reduce parasitic capacitance.

Benefits of technology

The device structure effectively reduces parasitic capacitance between the electrode and the conductive substrate, enhancing high-frequency characteristics and reducing the impact on high-frequency operations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide a nitride semiconductor device having a device structure in which a nitride semiconductor layer is formed on a conductive substrate and capable of reducing a parasitic capacitance formed between an electrode and the conductive substrate, and a method of manufacturing the nitride semiconductor device.SOLUTION: A nitride semiconductor device 1 includes: a conductive substrate 101 with both sides defined by a first surface 2a and a second surface 2b opposite each other; a base substance 10 provided on the first surface 2a of the conductive substrate 101, and including a nitride semiconductor layer 12 in which a semiconductor element is formed; an embedded electrode provided in the base substance 10 and electrically connected to the semiconductor element; and an insulator 180 disposed inside a groove formed in the conductive substrate 101, in a region facing the embedded electrode.SELECTED DRAWING: Figure 2B
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a nitride semiconductor device and a method for manufacturing the same. [Background technology]

[0002] High electron mobility transistors (HEMTs) are widely used as high-speed switching devices and high-frequency amplification devices. By using nitride semiconductors with a large band gap in the HEMT structure, high-speed operation and high voltage resistance can be achieved. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-077865 A Summary of the Invention [Problem to be solved by the invention]

[0004] Materials such as AlGaN and InAlGaN are used for the electron supply layer of nitride semiconductor HEMT. Semi-insulating SiC substrates and high-resistance Si substrates with high resistivity are generally used as substrates for nitride semiconductors, but these substrates generally have high selling prices and are expensive. On the other hand, a method has been proposed in which a high-resistance layer is formed on a conductive substrate, and a nitride semiconductor layer is formed on the high-resistance layer, thereby reducing losses due to capacitive coupling of the conductive substrate while using a relatively low-cost conductive substrate. However, the above structure alone cannot sufficiently reduce the parasitic capacitance generated between the electrode formed on the nitride semiconductor layer and the conductive substrate, and the desired high-frequency characteristics are not obtained.

[0005] An object of the present disclosure is to provide a nitride semiconductor device having a device structure in which a nitride semiconductor layer is formed on a conductive substrate, and capable of reducing the parasitic capacitance formed between an electrode and the conductive substrate, and a method for manufacturing the same. [Means for solving the problem]

[0006] In order to solve the above-mentioned problems, one aspect of the present disclosure is a nitride semiconductor device comprising: a conductive substrate having both sides defined by a first surface and a second surface opposing each other; a base provided on the first surface of the conductive substrate and including a nitride semiconductor layer on which a semiconductor element is formed; an electrode provided on the base and electrically connected to the semiconductor element; and an insulator disposed inside a groove formed in the conductive substrate in a region opposing the electrode.

[0007] Another aspect of the present disclosure is a method for manufacturing a nitride semiconductor device, comprising: forming a semi-insulating layer on a first surface of a conductive substrate, both surfaces of which are defined by opposing first and second surfaces; forming a nitride semiconductor layer on the semi-insulating layer; etching the nitride semiconductor layer to form an opening region; filling the opening region with a buried electrode; selectively etching a portion of the conductive substrate from the second surface to form a groove reaching the buried electrode; and forming an insulator inside the groove. Effect of the Invention

[0008] According to one aspect and another aspect of the present disclosure, it is possible to provide a nitride semiconductor device and a method for manufacturing the same, which have a device structure in which a nitride semiconductor layer is formed on a conductive substrate and can reduce parasitic capacitance formed between an electrode and the conductive substrate. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a plan view of a nitride semiconductor device according to an embodiment. [Figure 2A] FIG. 2A is a cross-sectional view taken along line II in FIG. [Figure 2B] FIG. 2B is a cross-sectional view taken along line II-II in FIG. [Figure 2C] FIG. 2C is a cross-sectional view taken along line III-III in FIG. [Figure 2D] FIG. 2D is a cross-sectional view of a laminated structure of a base body including a conductive substrate and a nitride semiconductor layer. [Figure 3A] FIG. 3A is a cross-sectional view of a nitride semiconductor device according to a modified example of the embodiment taken along line II in FIG. [Figure 3B] FIG. 3B is a cross-sectional view of the nitride semiconductor device according to the modified example of the embodiment taken along line II-II in FIG. [Figure 3C] FIG. 3C is a cross-sectional view of a nitride semiconductor device according to a comparative example taken along line II in FIG. [Figure 3D] FIG. 3D is a cross-sectional view of a nitride semiconductor device according to a comparative example taken along line II-II in FIG. [Figure 4A] FIG. 4A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 4B] FIG. 4B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 5A] FIG. 5A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 5B] FIG. 5B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 6A] FIG. 6A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 6B] FIG. 6B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 7A] FIG. 7A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 7B] FIG. 7B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 8A] FIG. 8A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 8B]FIG. 8B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 9A] FIG. 9A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 9B] FIG. 9B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 10A] FIG. 10A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 10B] FIG. 10B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 11A] FIG. 11A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 11B] FIG. 11B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing the nitride semiconductor device according to the embodiment. [Figure 12A] FIG. 12A is a cross-sectional view taken along line II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. [Figure 12B] FIG. 12B is a cross-sectional view taken along line II-II in FIG. 1, showing a step of the method for manufacturing a nitride semiconductor device according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, embodiments of the nitride semiconductor device of the present disclosure will be described with reference to the accompanying drawings. Note that, for simplicity and clarity of description, components shown in the drawings are not necessarily drawn to scale. Also, hatching lines may be omitted in cross-sectional views to facilitate understanding. The accompanying drawings are merely illustrative of embodiments of the present disclosure and should not be considered as limiting the present disclosure.

[0011] The following detailed description includes apparatus and methods embodying exemplary embodiments of the present disclosure. This detailed description is merely explanatory in nature and is not intended to limit the embodiments of the present disclosure or the application and uses of such embodiments.

[0012] In the following description, the direction perpendicular to the substrate extending on the XY plane is referred to as the Z direction, the direction in which the electrodes extend perpendicular to the Z direction is referred to as the Y direction, and the direction in which the electrodes are arranged perpendicular to the Z direction and the Y direction is referred to as the X direction.

[0013] (Embodiment) (Plane layout of nitride semiconductor device) Fig. 1 is a plan view of a nitride semiconductor device according to an embodiment. The nitride semiconductor device 1 may include an insulating layer 14, and a source electrode 18 and a drain electrode 20 formed on the insulating layer 14. The Z-axis direction of the mutually orthogonal XYZ axes shown in Fig. 1 is a direction orthogonal to a first surface 2a (see Figs. 2A to 2C) of a conductive substrate 101 described later. The term "plan view" used in this specification means viewing the nitride semiconductor device 1 from above along the Z direction, unless otherwise explicitly stated.

[0014] Insulating layer 14 can be composed of any insulator material capable of insulating source electrode 18 from drain electrode 20. For example, insulating layer 14 can include SiO2, SiN, SiON, Al2O3, AlN, AlON, HfO, HfN, HfON, HfSiON, AlON, or any combination thereof.

[0015] The source electrode 18 and the drain electrode 20 can be composed of one or more conductive materials. For example, the source electrode 18 and the drain electrode 20 can each include Au, Ti, TiN, Pt, Cu, Al, AlSiCu, AlCu, or any combination thereof.

[0016] As shown in FIG. 1, a plurality of source electrodes 18 may be arranged. In the illustrated example, the source electrodes 18 extend in the Y direction, and the plurality of source electrodes 18 are arranged in the X direction. Similarly, the drain electrode 20 may include a base portion 20A and a plurality of drain fingers 20B connected to the base portion 20A. In the illustrated example, the base portion 20A extends in the X direction, and the plurality of drain fingers 20B extend in the Y direction. In this disclosure, the X direction and the Y direction are also referred to as the "first direction" and the "second direction", respectively. The plurality of source electrodes 18 and the plurality of drain fingers 20B may be arranged alternately and spaced apart from each other. In the illustrated example, the plurality of source electrodes 18 and the plurality of drain fingers 20B are arranged alternately in the X direction.

[0017] The nitride semiconductor device 1 may further include a gate wiring 19A and a plurality of gate electrodes 19 connected to the gate wiring 19A. In the illustrated example, the gate wiring 19A extends in the X direction, and the plurality of gate electrodes 19 extend in the Y direction. Each gate electrode 19 may be disposed between one of the plurality of source electrodes 18 and one of the plurality of drain fingers 20B in a planar view. In the illustrated example, each gate electrode 19 is disposed between the source electrode 18 and the drain finger 20B that face each other in the X direction in a planar view. The gate wiring 19A may extend between the plurality of source electrodes 18 and the plurality of drain fingers 20B in a planar view. Further details of the gate electrodes 19 will be described later with reference to FIG. 2A.

[0018] The nitride semiconductor device 1 includes, in a plan view, an active region 300 including a two-dimensional electron gas layer and an inactive region 200 not including a two-dimensional electron gas layer. In Fig. 1, the active region 300 is indicated by being surrounded by a dashed line.

[0019] (Cross-sectional structure of a nitride semiconductor device) Fig. 2A is a cross-sectional view taken along line II in Fig. 1. Fig. 2B is a cross-sectional view taken along line II-II in Fig. 1. Fig. 2C is a cross-sectional view taken along line III-III in Fig. 1. Fig. 2D is a cross-sectional view of a laminated structure of a conductive substrate 101 and a base 10 including a nitride semiconductor layer 12.

[0020] The nitride semiconductor device 1 includes a conductive substrate 101 having both sides defined by a first surface 2a and a second surface 2b opposed to each other, and a base 10 formed on the first surface 2a of the conductive substrate 101. The conductive substrate 101 is, for example, a hexagonal silicon carbide substrate (SiC substrate). The first surface 2a and the second surface 2b are main surfaces of the conductive substrate 101, and the first surface 2a is also referred to as the front surface of the conductive substrate 101, and the second surface 2b is also referred to as the back surface of the conductive substrate 101. The first surface 2a is parallel to a first direction (X direction) and a second direction (Y direction) perpendicular to the first direction in a plan view.

[0021] The conductive substrate 101 is, for example, a SiC substrate having an off angle θoff. The first surface 2a is inclined at the off angle θoff in a specific crystal direction with respect to the c-plane. The off angle θoff may be 2° or more and 6° or less. More preferably, the off angle θoff may be 3° or more and 5° or less, and further preferably, 3.5° or more and 4.5° or less. In this disclosure, the term "c-plane" is used to refer to the (0001) plane of a hexagonal SiC crystal.

[0022] In this embodiment, the specific crystal direction may be the [11-20] direction. That is, the first face 2a may be inclined at an off angle θoff of 2° to 6° in the [11-20] direction with respect to the c-plane. In addition, in the indexes representing crystal directions and faces in the present disclosure, a number preceded by a minus sign (for example, "2" in the case of the [11-20] direction) means the number with a bar above it.

[0023] The conductive substrate 101 may be a 4H-SiC substrate having a 4H-SiC crystal structure. Here, "4H" represents the polytype of SiC crystal. In the following, a case where the conductive substrate 101 is a 4H-SiC substrate will be described as an example. The resistivity of the conductive substrate 101 may be, for example, 0.01 Ω·cm or more and 0.03 Ω·cm or less. In this embodiment, the resistivity of the conductive substrate 101 may be about 0.02 Ω·cm. In addition, the thickness of the conductive substrate 101 may be, for example, 30 μm or more and 300 μm or less. In this embodiment, the conductive substrate 101 may have a thickness of 150 μm. In addition to the 4H-SiC substrate, the conductive substrate 101 may be a SiC substrate having a 6H-SiC crystal structure. In addition to silicon carbide (SiC), a semiconductor material such as silicon (Si) or sapphire (Al2O3) may be used as the conductive substrate 101.

[0024] In this embodiment, as shown in FIG. 2D , the base 10 includes a semi-insulating layer 102 formed on the first surface 2a of a conductive substrate 101, and a nitride semiconductor layer 12 laminated on the semi-insulating layer 102. The semi-insulating layer 102 may be a GaN layer doped with an impurity. The impurity doped into the semi-insulating layer 102 may be, for example, carbon (C) or iron (Fe). Alternatively, the impurity may be both C and Fe. The impurity is such that the difference (Na−Nd) between the acceptor concentration Na and the donor concentration Nd is 1×10 17 cm -3 The GaN layer may be doped to about 1 μm. The thickness of the semi-insulating layer 102 may be 1 μm or more and 10 μm or less. In this embodiment, the semi-insulating layer 102 may have a thickness of 2 μm. By disposing the semi-insulating layer 102 between the conductive substrate 101 and the nitride semiconductor layer 12, the conductive substrate 101 and the semiconductor element formed on the nitride semiconductor layer 12 can be electrically insulated from each other. For example, the semi-insulating layer 102 can suppress leakage current. Note that, when the nitride semiconductor layer 12 can be directly disposed on the first surface 2a of the conductive substrate 101, the semi-insulating layer 102 does not need to be disposed between the conductive substrate 101 and the nitride semiconductor layer 12.

[0025] In this embodiment, the resistivity of the conductive substrate 101 is 1 Ω·cm or less, and the resistivity of the semi-insulating layer 102 may be 1×10 3 Ω·cm or more. In this embodiment, the resistivity of the semi-insulating layer 102 may be 1×10 5 Ω·cm or more. In this embodiment, the semi-insulating layer 102 may have a thickness of 5 μm or more. In this embodiment, the semi-insulating layer 102 may have a 4H-SiC crystal structure. Further, the semi-insulating layer 102 may have a 6H-SiC crystal structure or a 3C-SiC crystal structure.

[0026] The nitride semiconductor layer 12 includes an electron traveling layer 120 and an electron supply layer 122 laminated on the electron traveling layer 120. The electron traveling layer 120 may be formed on the semi-insulating layer 102. The electron traveling layer 120 is composed of a nitride semiconductor. The electron traveling layer 120 can be composed of GaN. In this embodiment, the electron traveling layer 120 may be an n-type GaN layer doped with donor-type impurities. In another example, the electron traveling layer 120 may be an undoped GaN layer. The thickness of the electron traveling layer 120 may be 0.05 μm or more and 1 μm or less. In this embodiment, the electron traveling layer 120 may have a thickness of about 0.2 μm.

[0027] The electron supply layer 122 is composed of a nitride semiconductor having a larger bandgap than the electron traveling layer 120. Materials such as AlGaN and InAlGaN are used for the electron supply layer 122. In this embodiment, the electron supply layer 122 may be composed of Al x Ga 1-x N, where 0 < X ≦ 1, and more preferably, 0.1 < X < 0.3. Note that the larger the Al composition ratio, the larger the bandgap of AlGaN. In this embodiment, X = 0.2 may be used. The thickness of the electron supply layer 122 may be 1 nm or more and 100 nm or less. In this embodiment, the electron supply layer 122 may have a thickness of about 20 nm.

[0028] The electron transit layer 120 and the electron supply layer 122 are made of nitride semiconductors having different lattice constants. Therefore, the nitride semiconductor (e.g., GaN) constituting the electron transit layer 120 and the nitride semiconductor (e.g., AlGaN) constituting the electron supply layer 122 form a lattice-mismatched heterojunction. The energy level of the conduction band of the electron transit layer 120 near the heterojunction interface becomes lower than the Fermi level due to spontaneous polarization of the electron transit layer 120 and the electron supply layer 122 and piezoelectric polarization caused by crystal distortion near the heterojunction interface. As a result, a two-dimensional electron gas layer 121 is formed in the electron transit layer 120 at a position close to the heterojunction interface between the electron transit layer 120 and the electron supply layer 122 (for example, within a range of about several nm from the interface). The two-dimensional electron gas layer 121 is also referred to as "2DEG" (Two Dimensional Electron Gas). The two-dimensional electron gas layer 121 in the electron transit layer 120 functions as a channel of the nitride semiconductor device 1. The sheet carrier density of the two-dimensional electron gas layer 121 generated in the electron transit layer 120 can be increased by increasing at least one of the Al composition ratio and the thickness of the electron supply layer 122.

[0029] As described above, a HEMT is formed as a semiconductor element in the active region 300 of the nitride semiconductor layer 12. As described later, for example, an ion-implanted layer 13 is formed by selectively implanting ions into a part of the nitride semiconductor layer 12, and the region where the ion-implanted layer 13 is formed is defined as an inactive region 200.

[0030] The nitride semiconductor device 1 may further include an insulating layer 14 formed on the electron supply layer 122. A source contact opening 14S, a drain contact opening 14D, and a gate contact opening 14G are formed in the insulating layer 14, exposing the surface of the electron supply layer 122. The source contact opening 14S and the drain contact opening 14D are spaced apart in the X direction. The gate contact opening 14G is located between the source contact opening 14S and the drain contact opening 14D, which are spaced apart in the X direction. In this embodiment, the insulating layer 14 may be SiN. The thickness of the insulating layer 14 may be, for example, not less than 10 nm and not more than 200 nm. In this embodiment, the insulating layer 14 may have a thickness of about 100 nm.

[0031] The nitride semiconductor device 1 includes a gate electrode 19, a source electrode 18, and a drain electrode 20 arranged on a nitride semiconductor layer 12. The source electrode 18 and the drain electrode 20 are spaced apart in a first direction (X direction). The gate electrode 19 is arranged between the source electrode 18 and the drain electrode 20 that are spaced apart in the first direction. The source electrode 18, the drain electrode 20, and the gate electrode 19 are arranged so as to enable electrons to travel in the first direction through a two-dimensional electron gas layer 121. The source electrode 18 is in contact with the electron supply layer 122 through a source contact opening 14S. The drain electrode 20 is in contact with the electron supply layer 122 through a drain contact opening 14D. The gate electrode 19 is in contact with the electron supply layer 122 through a gate contact opening 14G.

[0032] The source electrode 18 and the drain electrode 20 may be made of any material capable of forming an ohmic contact with the nitride semiconductor layer 12. In this embodiment, the source electrode 18 and the drain electrode 20 may include a Ti layer and an Al layer. In this case, the Ti layer may be located between the nitride semiconductor layer 12 and the Al layer. In one example, the Ti layer may have a thickness of about 20 nm, and the Al layer may have a thickness of about 300 nm. In another example, the source electrode 18 and the drain electrode 20 may include a Ta layer and an Al layer. In yet another example, the source electrode 18 and the drain electrode 20 may include a Ti layer, an Al layer, a Ni layer, and an Au layer, in this order from the bottom.

[0033] The gate electrode 19 may be made of any material that forms a Schottky contact with the nitride semiconductor layer 12. In this embodiment, the gate electrode 19 may include a Ni layer and an Au layer. In this case, the Ni layer may be located between the nitride semiconductor layer 12 and the Au layer. In one example, the Ni layer may have a thickness of 10 nm, and the Au layer may have a thickness of 600 nm.

[0034] The gate electrode 19 is disposed between the source electrode 18 and the drain electrode 20 that are spaced apart in the first direction (X direction) and extends in the second direction (Y direction) (see FIG. 1). The source electrode 18 and the drain electrode 20 also extend in the second direction (Y direction). That is, the source electrode 18, the gate electrode 19, and the drain electrode 20 that extend in the second direction (Y direction) are arranged in this order in the first direction (X direction). Therefore, between the source electrode 18 and the drain electrode 20, electrons can travel in the first direction (X direction) through the two-dimensional electron gas layer 121 of the electron travel layer 120. The source electrode 18, the gate electrode 19, and the drain electrode 20 are disposed so that the first direction (X direction) (i.e., the electron travel direction) satisfies a predetermined relationship with a specific crystal direction (e.g., [11-20]) of the conductive substrate 101.

[0035] Although the above description with reference to FIGS. 2A to 2C focuses on one source electrode 18, one drain electrode 20, and the gate electrode 19 disposed therebetween, the nitride semiconductor device 1 may include a plurality of gate electrodes 19, a plurality of source electrodes 18, and a plurality of drain electrodes 20 disposed on the nitride semiconductor layer 12. Each of the plurality of source electrodes 18 may be commonly connected. Similarly, each of the plurality of drain electrodes 20 may be connected to one of the plurality of drain fingers 20B (see FIG. 1). The plurality of source electrodes 18 and the plurality of drain electrodes 20 may be alternately disposed in the first direction (X direction). Also, each of the plurality of gate electrodes 19 may be disposed between one of the plurality of source electrodes 18 and one of the plurality of drain electrodes 20.

[0036] Hereinafter, an electrode disposed on the first surface 2a side of the conductive substrate 101 will be referred to as a "surface electrode" or simply as an "electrode." For example, the source electrode 18, the drain electrode 20 including the base portion 20A and the drain finger 20B, the gate electrode 19, and the gate wiring 19A are surface electrodes.

[0037] In the active region 300 of the nitride semiconductor device 1, the nitride semiconductor layer 12 includes an electron transit layer 120 and an electron supply layer 122 that forms a heterojunction with the electron transit layer 120, as shown in FIG. 2A. That is, in the active region 300, the electron transit layer 120 includes a two-dimensional electron gas layer 121 at the interface with the electron supply layer 122. In other words, the active region 300 is a region that includes the two-dimensional electron gas layer 121 in a planar view. On the other hand, the inactive region 200 is a region that does not include the two-dimensional electron gas layer 121 in a planar view. In other words, the inactive region 200 is a region through which no main current of the nitride semiconductor device 1 flows.

[0038] As described above, the nitride semiconductor device 1 according to the embodiment includes a conductive substrate 101 having both sides defined by a first surface 2a and a second surface 2b opposed to each other, and a base 10 provided on the first surface 2a of the conductive substrate 101 and including a nitride semiconductor layer 12 on which a semiconductor element is formed. The nitride semiconductor device 1 further includes a surface electrode provided on the base 10 and electrically connected to the semiconductor element formed in the nitride semiconductor layer 12. The nitride semiconductor device 1 further includes a first embedded electrode 22A shown in FIG. 2A, a second embedded electrode 22B shown in FIG. 2B, and a third embedded electrode 22C shown in FIG. 2C.

[0039] As shown in FIG. 2A, the source electrode 18 is electrically connected to a through electrode 24E that penetrates the conductive substrate 101 in a region facing the source electrode 18 through a first embedded electrode 22A that is disposed in an opening formed in the insulating layer 14 and the nitride semiconductor layer 12. The first embedded electrode 22A is electrically connected to a back surface electrode 24B that is disposed on the second surface 2b of the conductive substrate 101 through the through electrode 24E. The back surface electrode 24B is, for example, a ground electrode of the nitride semiconductor device 1. The source electrode 18 is connected to a ground electrode formed on the second surface 2b of the conductive substrate 101 through the first embedded electrode 22A that is a conductive member that penetrates the conductive substrate 101.

[0040] 2B, the base portion 20A of the drain electrode 20 is disposed on the second buried electrode 22B. The second buried electrode 22B is disposed in an opening formed in the insulating layer 14 and the nitride semiconductor layer 12. The second buried electrode 22B is a surface electrode electrically connected to the drain electrode 20. The drain electrode 20 including the base portion 20A and the drain finger 20B and the second buried electrode 22B form a drain electrode.

[0041] 2C, the gate wiring 19A connected to the gate electrode 19 is disposed on the third embedded electrode 22C. The third embedded electrode 22C is disposed in an opening formed in the insulating layer 14 and the nitride semiconductor layer 12. The third embedded electrode 22C is a surface electrode electrically connected to the gate electrode 19. The gate electrode 19, the gate wiring 19A, and the third embedded electrode 22C form a gate electrode.

[0042] As shown in FIG. 2B and FIG. 2C, the nitride semiconductor device 1 includes an insulator 180 disposed inside a groove formed in the conductive substrate 101 in a region facing the second embedded electrode 22B and the third embedded electrode 22C. In other words, the nitride semiconductor device 1 includes an insulator 180 disposed inside a groove formed in the conductive substrate 101 in a region facing the front electrode. As shown in FIG. 2B and FIG. 2C, the insulator 180 may completely fill the inside of the groove penetrating the conductive substrate 101. In this embodiment, as shown in FIG. 2B and FIG. 2C, the insulator 180 fills the inside of an opening that is connected to the groove formed in the conductive substrate 101 and is formed penetrating the semi-insulating layer 102.

[0043] As described above, in the nitride semiconductor device 1, in the inactive region 200, the insulator 180 is provided between the second buried electrode 22B electrically connected to the drain electrode 20 and the back electrode 24B. Also, the insulator 180 is provided between the third buried electrode 22C electrically connected to the gate electrode 19 and the back electrode 24B. That is, in the nitride semiconductor device 1, the conductive substrate 101 directly below a part of the front electrode is removed and the insulator 180 is provided. Since the conductive substrate 101 directly below the front electrode is removed, the parasitic capacitance formed between the front electrode and the conductive substrate 101 is reduced. Furthermore, the insulator 180 reduces the parasitic capacitance between the front electrode and the back electrode 24B.

[0044] In the above, an example in which the insulator 180 is disposed opposite both the second embedded electrode 22B and the third embedded electrode 22C has been shown. However, the insulator 180 may be disposed opposite the second embedded electrode 22B, and the insulator 180 may not be disposed opposite the third embedded electrode 22C. Alternatively, the insulator 180 may not be disposed opposite the second embedded electrode 22B, and may be disposed opposite the third embedded electrode 22C. Even when the insulator 180 is disposed opposite either the second embedded electrode 22B or the third embedded electrode 22C, the parasitic capacitance between the surface electrode and the conductive substrate 101 can be reduced.

[0045] As described above, in the nitride semiconductor device 1, the insulator 180 is disposed inside a groove formed in the conductive substrate 101, facing either a part of the drain electrode or a part of the gate electrode, or both a part of the drain electrode and the gate electrode, provided on the base 10. This reduces the parasitic capacitance formed between the surface electrode and the conductive substrate 101. As a result, for example, degradation of the high-frequency characteristics of the nitride semiconductor device 1 is suppressed.

[0046] In the active region 300, since the two-dimensional electron gas layer 121 is formed between the surface electrode and the conductive substrate 101, the influence of the parasitic capacitance between the surface electrode and the conductive substrate 101 on the nitride semiconductor device 1 is small. On the other hand, in the inactive region 200, the influence of the parasitic capacitance between the gate wiring 19A and the base portion 20A and the conductive substrate 101 on the nitride semiconductor device 1 is large. Therefore, by arranging the second embedded electrode 22B and the third embedded electrode 22C in the inactive region 200, the effect of reducing the influence of the parasitic capacitance on the nitride semiconductor device 1 is large.

[0047] The insulator 180 may include an insulator material including a paste agent. The insulator 180 may also include an insulator material including diamond-like carbon. The insulator 180 including a paste agent and diamond-like carbon can easily form the insulator 180 to a thickness required to fill the groove 25E, compared to forming the insulator 180 by growing, for example, a silicon oxide film.

[0048] (Modification) Fig. 3A is a cross-sectional view taken along line II in Fig. 1 of a nitride semiconductor device according to a modified example of the embodiment. Fig. 3B is a cross-sectional view taken along line II-II in Fig. 1 of a nitride semiconductor device according to a modified example of the embodiment. As shown in Fig. 3B, in the nitride semiconductor device according to the modified example, an insulator 180 disposed below a base portion 20A connected to a drain electrode 20 is formed so as to cover a wall surface of a groove formed in a conductive substrate 101 without completely filling the inside of the groove. The other configurations are similar to those of the above embodiment.

[0049] In the nitride semiconductor device 1 according to the modified embodiment, the parasitic capacitance of the nitride semiconductor device 1 can also be reduced by removing a portion of the conductive substrate 101 below the surface electrode and arranging an insulator 180 therein.

[0050] (Comparative Example) Fig. 3C is a cross-sectional view of the nitride semiconductor device according to the comparative example taken along line II in Fig. 1. Fig. 3D is a cross-sectional view of the nitride semiconductor device according to the comparative example taken along line II-II in Fig. 1.

[0051] In the nitride semiconductor device according to the comparative example, as shown in Fig. 3D, a conductive substrate 101, a semi-insulating layer 102, a nitride semiconductor layer 12, an ion-implanted layer 13, and an insulating layer 14 are disposed between a base portion 20A and a back electrode 24B. In the nitride semiconductor device according to the comparative example, a parasitic capacitance is formed between the drain electrode 20 and the conductive substrate 101 in the inactive region 200, which causes degradation of high-frequency operation. Although not shown, a parasitic capacitance is also formed between the gate electrode 19 and the conductive substrate 101, which causes degradation of high-frequency operation.

[0052] (Method of Manufacturing a Nitride Semiconductor Device According to an Embodiment) Figures 4A to 12A are cross-sectional views taken along line II in Figure 1, illustrating a step of a method for manufacturing a nitride semiconductor device according to an embodiment. Figures 4B to 12B are cross-sectional views taken along line II-II in Figure 1, illustrating a step of a method for manufacturing a nitride semiconductor device according to an embodiment.

[0053] The manufacturing method of the nitride semiconductor device 1 according to the embodiment includes the following manufacturing steps. A semi-insulating layer 102 is formed on the first surface 2a of the conductive substrate 101. A nitride semiconductor layer 12 is formed on the semi-insulating layer 102, and the nitride semiconductor layer 12 is etched to form an opening region. The opening region is filled with the second buried electrode 22B and the third buried electrode 22C made of a material having a high etching selectivity ratio with respect to the conductive substrate 101. An insulating layer 14 is formed on the nitride semiconductor layer 12. The insulating layer 14 is opened by etching to form a drain electrode 20 and a source electrode 18 in ohmic contact with the nitride semiconductor layer 12, and a gate electrode 19 in Schottky contact with the nitride semiconductor layer 12 is formed. A part of the conductive substrate 101 is selectively etched from the second surface 2b of the conductive substrate 101 to form a groove reaching the second buried electrode 22B and the third buried electrode 22C, and an insulator 180 is formed inside the groove. Hereinafter, the manufacturing method of the nitride semiconductor device according to the embodiment will be described in detail with reference to the drawings.

[0054] 4A and 4B, a conductive substrate 101 is prepared, both sides of which are defined by a first surface 2a and a second surface 2b that face each other. As the conductive substrate 101, for example, a conductive SiC substrate with a resistivity of about 0.02 Ω cm is used.

[0055] (B) Next, as shown in Figures 5A and 5B, a semi-insulating layer 102 is formed on the first surface 2a of the conductive substrate 101. The semi-insulating layer 102 is formed by, for example, chemical vapor deposition (CVD) to a carrier concentration of 2 x 10 15 cm -3 After forming a SiC layer adjusted to the above, the SiC layer is irradiated with an electron beam accelerated to an acceleration energy of about 500 keV. The irradiation fluence of the electron beam is, for example, 1×10 17 cm -2 The acceleration energy of the electron beam is preferably about 300 to 800 keV.

[0056] 6A and 6B, a nitride semiconductor layer 12 is formed on the semi-insulating layer 102. For example, a semiconductor element having a HEMT structure in which an electron transit layer 120 and an electron supply layer 122 are stacked is formed on the nitride semiconductor layer 12.

[0057] (D) Next, as shown in FIG. 7A and FIG. 7B, an inactive region 200 is formed in a part of the nitride semiconductor layer 12 by using an ion implantation technique. For example, the inactive region 200 may be defined by selectively ion-implanting argon (Ar) into a part of the surface of the nitride semiconductor layer 12 and forming the ion-implanted layer 13 as a modified layer. In addition to argon (Ar), for example, ion implantation of nitrogen or oxygen may be performed. Alternatively, a part of the nitride semiconductor layer 12 may be removed by dry etching such as reactive ion etching (RIE) to form a mesa structure as the active region 300. That is, the inactive region 200 is formed by removing the region where the two-dimensional electron gas layer 121 is formed by a method such as dry etching, and the inactive region 200 and the active region 300 can be formed separately.

[0058] 8A and 8B, a portion of the nitride semiconductor layer 12 is etched away using an inductively coupled plasma (ICP) etching technique to form an opening region exposing the surface 2c of the semi-insulating layer 102. As the etching gas, for example, a chlorine-based gas such as Cl2 or BCl3 can be used.

[0059] (F) Furthermore, the first buried electrode 22A, the second buried electrode 22B, and the third buried electrode 22C are formed on the surface 2c of the semi-insulating layer 102 exposed in the inactive region 200 and the active region 300. The first buried electrode 22A, the second buried electrode 22B, and the third buried electrode 22C may be formed simultaneously. In the following, the first buried electrode 22A, the second buried electrode 22B, and the third buried electrode 22C are also referred to as "buried electrodes" when not limited to each other. The material of the buried electrodes may be any material that has a high etching selectivity with respect to the conductive substrate 101. For example, Ni, Al, Cu, ITO, and the like can be used as the material of the buried electrodes. The thickness of the buried electrodes is, for example, about 0.3 μm to 3 μm. In forming the buried electrodes, techniques such as sputtering, vacuum deposition, and plating can be applied. The reason for using a material having a high etching selectivity with respect to the conductive substrate 101 is that it serves as an etching stop layer for protecting the nitride semiconductor layer 12 in a process to be described later.

[0060] (G) Next, as shown in FIG. 9A and FIG. 9B, an insulating layer 14 is formed on the nitride semiconductor layer 12 by, for example, plasma-enhanced chemical vapor deposition (PECVD). For example, a SiN layer is used as the insulating layer 14. The thickness of the SiN layer is about 100 nm. Other materials for the insulating layer 14 may be, for example, SiON, SiO2, Al2O3, AlN, AlON, HfO, HfN, HfON, HfSiON, or the like. Other methods for forming the insulating layer 14 may include, for example, a low pressure chemical vapor deposition (LPCVD) method, a sputtering method, an atomic layer deposition (ALD) method, and a molecular beam epitaxial growth (MBE) method. Note that, as shown in FIG. 9A, the insulating layer 14 is also formed on the first buried electrodes 22A in the active region 300. Furthermore, the insulating layer 14 is formed on the second embedded electrodes 22B and the ion-implanted layer 13 in the inactive region 200, as shown in FIG. 9B.

[0061] (H) Next, as shown in FIG. 10A and FIG. 10B, a window is opened in the insulating layer 14 by RIE or the like, and a drain electrode 20 and a source electrode 18 are formed in ohmic contact with the nitride semiconductor layer 12 in the opened region of the insulating layer 14. The source electrode 18 also extends onto the first buried electrode 22A formed in the active region 300, and the first buried electrode 22A and the source electrode 18 formed in the active region 300 are electrically connected. The base portion 20A connected to the drain electrode 20 also extends onto the second buried electrode 22B formed in the inactive region 200, as shown in FIG. 10B, and the second buried electrode 22B and the drain electrode 20 formed in the active region 300 are electrically connected. The ohmic contact of the drain electrode 20 and the source electrode 18 can be realized by forming Ti / Al on the nitride semiconductor layer 12 by electron beam (EB) deposition and holding it at a temperature of about 500 to 550°C. In this embodiment, the thickness of the Ti layer is about 20 nm, and the thickness of the Al layer is about 300 nm. The drain electrode 20 and the source electrode 18 may be made of, for example, Ta / Al. Also, a sputtering or MBE device may be used as a film forming device.

[0062] (I) Next, as shown in Figures 11A and 11B, a window is opened in the insulating layer 14 by RIE or the like, and a gate electrode 19 is formed in the opened region of the insulating layer 14. As shown in Figure 2C, the gate electrode 19 also extends onto the third embedded electrode 22C formed in the inactive region 200, and the third embedded electrode 22C and the gate electrode 19 formed in the active region 300 are electrically connected. The gate electrode 19 may be one that is in Schottky contact with the nitride semiconductor layer 12, and here a Ni / Au laminated structure is used. The Ni layer is about 10 nm thick, and the Au layer is about 600 nm thick.

[0063] (J) Next, as shown in FIG. 12A and FIG. 12B, the conductive substrate 101 is etched from the second surface 2b side by dry etching such as RIE to form a groove 25E penetrating the conductive substrate 101 in the inactive region 200. At the same time, a groove 25A penetrating the conductive substrate 101 is formed in the active region 300. A mixed gas of SF6 / O2 is used as the etching gas. CF4 or CHF3 may be used as the etching gas instead of SF6. When etching the conductive substrate 101 from the second surface 2b side, the etching may be performed with the drain electrode 20, the gate electrode 19, and the source electrode 18 attached to a dummy substrate or the like, with the second surface 2b facing upward. By forming a buried electrode as an etching stop layer, it is possible to prevent the nitride semiconductor layer 12 from being etched from the side or the dummy substrate from being etched. A material having an etching rate lower than that of the conductive substrate 101 is selected for the buried electrode.

[0064] (K) Next, as shown in FIGS. 2A, 2B, and 2C, the grooves 25E formed in the conductive substrate 101 of the inactive region 200 are filled with an insulator 180. The resistivity of the insulator 180 is, for example, 10 Ω·cm or more. An insulating paste may be used for the insulator 180. When filling the grooves 25E formed in the conductive substrate 101 of the inactive region 200 with the insulator 180, it is not necessary to completely fill the grooves 25E as shown in FIG. 3B, and the insulator 180 may be formed to cover a portion of the grooves 25E.

[0065] (L) Next, as shown in Figures 2A, 2B, and 2C, the grooves 25A formed in the conductive substrate 101 of the active region 300 are filled with the through electrodes 24E. For example, a Ti / Cu laminate structure is formed by sputtering, and then gold plating is formed to form the through electrodes 24E. It is not necessary to completely fill the grooves 25A with the through electrodes 24E, and it is sufficient to only cover a part of the grooves 25A with the through electrodes 24E so that the first embedded electrode 22A, which serves as an etching stop layer, and the back electrode 24B are connected.

[0066] (M) After forming the through electrode 24E, the back electrode 24B is formed on the second surface 2b of the conductive substrate 101. For example, the back electrode 24B is formed on the entire surface of the second surface 2b by using a metal vapor deposition method. The source electrode 18 is set to the same potential as the back electrode 24B via the through electrode 24E and the first embedded electrode 22A.

[0067] (N) Although not shown in the figure, an insulating layer may be formed on the source electrode 18, the gate electrode 19, and the drain electrode 20, and windows may be opened in this insulating layer to form a laminated structure for pad electrodes on the source electrode 18, the gate electrode 19, and the drain electrode 20.

[0068] (Other embodiments) As described above, one embodiment has been described, but the descriptions and drawings forming a part of the disclosure are illustrative and should not be understood as limiting. From this disclosure, various alternative embodiments, examples and operating techniques will become apparent to those skilled in the art. Thus, the present embodiment includes various embodiments not described herein.

[0069] [Note] The technical ideas that can be understood from the present disclosure are described below. Note that, for the purpose of aiding understanding, not for the purpose of limitation, the components described in the appendices are given the reference symbols of the corresponding components in the embodiments. The reference symbols are shown as examples for the purpose of aiding understanding, and the components described in each appendix should not be limited to the components indicated by the reference symbols.

[0070] (Appendix 1) The nitride semiconductor device 1 includes a conductive substrate 101 having both sides defined by a first surface 2a and a second surface 2b opposed to each other, a base 10 provided on the first surface 2a of the conductive substrate 101 and including a nitride semiconductor layer 12 on which a semiconductor element is formed, an electrode provided on the base 10 and electrically connected to the semiconductor element, and an insulator 180 disposed inside a groove formed in the conductive substrate 101 in a region opposed to the electrode. According to the nitride semiconductor device 1 of Appendix 1, the parasitic capacitance formed between the electrode and the conductive substrate 101 can be reduced.

[0071] (Appendix 2) In the nitride semiconductor device described in Appendix 1, the base 10 includes a semi-insulating layer 102 disposed on the first surface 2a, and a nitride semiconductor layer 12 laminated on the semi-insulating layer 102. According to the nitride semiconductor device 1 of Appendix 1, by disposing the semi-insulating layer 102 between the conductive substrate 101 and the nitride semiconductor layer 12, the conductive substrate 101 and the semiconductor element formed on the nitride semiconductor layer 12 can be electrically insulated from each other.

[0072] (Appendix 3) In the nitride semiconductor device described in Supplementary Note 2, the insulator 180 is formed penetrating the semi-insulating layer 102 and fills the inside of the opening communicating with the trench.

[0073] (Appendix 4) In the nitride semiconductor device according to appendix 2 or 3, the resistivity of the conductive substrate 101 is 1 Ω·cm or less, and the resistivity of the semi-insulating layer 102 is 1×10 3 Ω·cm or more.

[0074] (Appendix 5) In the nitride semiconductor device according to claim 2 or 3, the resistivity of the semi-insulating layer 102 is 1×10 5 Ω·cm or more.

[0075] (Appendix 6) In the nitride semiconductor device according to Supplementary Note 2 or 3, the semi-insulating layer 102 has a thickness of 5 μm or more.

[0076] (Appendix 7) In the nitride semiconductor device according to Supplementary Note 2 or 3, the semi-insulating layer 102 has a 4H—SiC crystal structure.

[0077] (Appendix 8) In the nitride semiconductor device according to Supplementary Note 2 or 3, the semi-insulating layer 102 has a 6H—SiC crystal structure.

[0078] (Appendix 9) In the nitride semiconductor device according to Supplementary Note 2 or 3, the semi-insulating layer 102 has a 3C-SiC crystal structure.

[0079] (Appendix 10) In the nitride semiconductor device according to any one of Supplementary Notes 1 to 9, the nitride semiconductor layer 12 includes an electron transit layer 120 and an electron supply layer 122 forming a heterojunction with the electron transit layer 120. According to the nitride semiconductor device of Supplementary Note 10, in a nitride semiconductor device having a semiconductor element with a HEMT structure, it is possible to reduce parasitic capacitance formed between an electrode and a conductive substrate.

[0080] (Appendix 11) The nitride semiconductor device according to Supplementary Note 10 includes a drain electrode, a source electrode, and a gate electrode provided on a semiconductor element, and an insulator 180 is disposed facing either a part of the drain electrode or a part of the gate electrode, or both the part of the drain electrode and the gate electrode. According to the nitride semiconductor device according to Supplementary Note 11, it is possible to reduce parasitic capacitance formed between the drain electrode or the gate electrode, or both the drain electrode and the gate electrode, and the conductive substrate.

[0081] (Appendix 12) In the nitride semiconductor device described in Appendix 10 or 11, the source electrode is connected to a back surface electrode 24B serving as a ground electrode formed on the second surface 2b of the conductive substrate 101 via a conductive member penetrating the conductive substrate 101. According to the nitride semiconductor device described in Appendix 12, the source electrode can be electrically connected to the ground electrode from the second surface 2b, thereby making it possible to reduce the chip area.

[0082] (Appendix 13) In the nitride semiconductor device according to any one of Supplementary Notes 1 to 11, the insulator 180 includes an insulating material containing a paste agent. According to the nitride semiconductor device according to Supplementary Note 13, the time required for forming the insulator 180 can be shortened.

[0083] (Appendix 14) In the nitride semiconductor device according to any one of Supplementary Notes 1 to 11, the insulator 180 includes an insulating material containing diamond-like carbon. According to the nitride semiconductor device according to Supplementary Note 14, the time required to form the insulator 180 can be shortened. In particular, when the groove 25E is not completely filled with the insulator 180, the diamond-like carbon is suitably used to partially fill the groove 25E.

[0084] (Appendix 15) The method for manufacturing a nitride semiconductor device includes the following manufacturing steps. A semi-insulating layer 102 is formed on a first surface 2a of a conductive substrate 101, both surfaces of which are defined by a first surface 2a and a second surface 2b opposed to each other. A nitride semiconductor layer 12 is formed on the semi-insulating layer 102. An opening region is formed by etching the nitride semiconductor layer 12, and the opening region is filled with a second embedded electrode 22B and a third embedded electrode 22C. A part of the conductive substrate 101 is selectively etched from the second surface 2b to form a groove 25E reaching the second embedded electrode 22B and the third embedded electrode 22C, and an insulator 180 is formed inside the groove 25E. According to the method for manufacturing a nitride semiconductor device of Appendix 15, a nitride semiconductor device with reduced parasitic capacitance formed between an electrode and a conductive substrate can be manufactured.

[0085] (Appendix 16) In the nitride semiconductor device described in Appendix 15, the second embedded electrode 22B and the third embedded electrode 22C are made of a material having a high etching selectivity with respect to the conductive substrate 101. According to the manufacturing method for a nitride semiconductor device described in Appendix 16, in the step of etching the conductive substrate 101 from the second surface 2b, the second embedded electrode 22B and the third embedded electrode 22C can be used as an etching stop layer.

[0086] (Appendix 17) In the nitride semiconductor device according to Appendix 15 or 16, an insulating layer 14 is formed on the nitride semiconductor layer 12. Openings are formed in the insulating layer 14 by etching to form a drain electrode 20 and a source electrode 18 in ohmic contact with the nitride semiconductor layer 12. The insulating layer 14 is removed by etching to form a gate electrode 19 in Schottky contact with the nitride semiconductor layer 12. According to the method for manufacturing a nitride semiconductor device according to Appendix 17, it is possible to reduce parasitic capacitance formed between a conductive substrate and electrodes in a nitride semiconductor device having a source electrode, a drain electrode, and a gate electrode.

[0087] The above description is merely illustrative. Those skilled in the art may recognize that many more possible combinations and permutations are possible other than the components and methods (manufacturing processes) listed for the purpose of describing the technology of the present disclosure. The present disclosure is intended to embrace all alternatives, modifications, and alterations that fall within the scope of the present disclosure, including the scope of the claims. [Explanation of symbols]

[0088] 1...Nitride semiconductor device 2a…Side 1 2b…Second side 10...Base 12...Nitride semiconductor layer 13...Ion implantation layer 14…Insulating layer 18…Source electrode 19...Gate electrode 19A…Gate wiring 20...Drain electrode 20A…Base section 20B…Drain Finger 22A…First embedded electrode 22B...Second buried electrode 22C…Third embedded electrode 24B…Back electrode 24E…Through electrode 25A, 25E…Groove 101...Conductive substrate 102...Semi-insulating layer 120...Electron transport layer 121...2-dimensional electron gas layer 122...electron supply layer 180…Insulator 200…Inactive area 300...active area

Claims

1. a conductive substrate having opposing first and second surfaces defined thereon; a base body including a nitride semiconductor layer provided on the first surface of the conductive substrate and having a semiconductor element formed thereon; an electrode provided on the base and electrically connected to the semiconductor element; an insulator disposed within a groove formed in the conductive substrate in a region facing the electrode; A nitride semiconductor device comprising:

2. The substrate is a semi-insulating layer disposed on the first surface; the nitride semiconductor layer laminated on the semi-insulating layer; The nitride semiconductor device according to claim 1 ,

3. The nitride semiconductor device according to claim 2 , wherein said insulator is formed to penetrate said semi-insulating layer and fills an inside of an opening communicating with said trench.

4. The resistivity of the conductive substrate is 1 Ω cm or less, and the resistivity of the semi-insulating layer is 1×10 3 The nitride semiconductor device according to claim 2 , wherein the resistivity is Ω·cm or more.

5. The resistivity of the semi-insulating layer is 1×10 5 The nitride semiconductor device according to claim 2 , wherein the resistivity is Ω·cm or more.

6. The nitride semiconductor device according to claim 2 , wherein said semi-insulating layer has a thickness of 5 μm or more.

7. The nitride semiconductor device of claim 2 , wherein said semi-insulating layer has a 4H—SiC crystal structure.

8. The nitride semiconductor device of claim 2 , wherein said semi-insulating layer has a 6H—SiC crystal structure.

9. The nitride semiconductor device according to claim 2, wherein said semi-insulating layer has a 3C-SiC crystal structure.

10. The nitride semiconductor layer is An electron transport layer; an electron supply layer that forms a heterojunction with the electron transit layer; Equipped with The nitride semiconductor device according to claim 1 .

11. A drain electrode, a source electrode, and a gate electrode are provided on the semiconductor element, the insulator is disposed facing either a part of the drain electrode or a part of the gate electrode, or facing both a part of the drain electrode and the gate electrode; The nitride semiconductor device according to claim 10.

12. The nitride semiconductor device according to claim 11 , wherein the source electrode is connected to a ground electrode formed on the second surface of the conductive substrate via a conductive member penetrating the conductive substrate.

13. The nitride semiconductor device of claim 1 , wherein the insulator comprises an insulator material including a paste agent.

14. The nitride semiconductor device according to claim 1 , wherein the insulator includes an insulator material containing diamond-like carbon.

15. forming a base body including a nitride semiconductor layer having a semiconductor element formed on a first surface of a conductive substrate having opposing first and second surfaces; Etching the substrate to form an open area; filling the open region with a buried electrode; selectively etching a portion of the conductive substrate from the second surface to form a groove reaching the embedded electrode; Forming an insulator inside the groove A method for manufacturing a nitride semiconductor device comprising the steps of:

Citation Information

Patent Citations

  • Semiconductor device

    JP2020077865A