Inductor component
The inductor component addresses bonding and cracking issues by incorporating a high-concentration phosphorus-containing portion along the coil, improving bondability and reducing linear expansion coefficient differences, thereby enhancing quality and yield.
Patent Information
- Application Number
- JP2023066542
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-14
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2043-04-14
AI Technical Summary
Conventional inductor components using glass-based insulating materials face issues with reduced strength due to impact and stress, leading to potential cracking and poor bonding between the element body and coil, especially when quartz fillers are used, which further deteriorate bondability.
An inductor component with an element body containing an amorphous material and a crystalline filler, featuring a high-concentration phosphorus-containing portion along the coil, where the phosphorus concentration is higher than the central portion, enhancing bonding and reducing linear expansion coefficient differences.
Improves the quality and yield of inductor components by ensuring close contact between the coil and element body, preventing peeling and cracking, while reducing dielectric loss and increasing Q at high frequencies.
Smart Images

Figure 2024152387000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to inductor components. [Background technology]
[0002] A conventional inductor component is described in JP 2018-131353 A (Patent Document 1). This inductor component includes an element body containing a glass-based insulating material and a coil disposed within the element body.
[0003] However, when an inductor component contains a glass-based insulating material, the strength of the inductor component is reduced, and cracks may occur in the element of the inductor component due to the impact during mounting or the stress caused by the bending of the board. To address this problem, for example, a crystalline filler is added to the glass-based insulating material. In Patent Document 1, the element part is a glass ceramic containing a glass-based insulating material and a crystalline filler. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2018-131353 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, in the above-mentioned conventional inductor components, the addition of a crystalline filler to the element body suppresses the softening of the glass-based material, which may cause poor bonding (peeling) between the element body and the coil, and may also increase the difference in linear expansion coefficient between the element body and the coil, which may cause cracks in the element body near the coil due to stress caused by the difference in linear expansion coefficient. In particular, when a quartz filler, which is effective in reducing the dielectric constant of glass-based insulating materials, is used, the softening of the glass-based material is further suppressed, which may further reduce the bonding strength between the element body and the coil.
[0006] Therefore, an object of the present disclosure is to provide an inductor component that can improve quality and increase yield. [Means for solving the problem]
[0007] In order to solve the above problems, an inductor component according to one aspect of the present disclosure comprises: An element body made of an insulating material; a coil disposed within the element body and wound helically along an axis; Equipped with The insulating material contains a base material made of an amorphous material containing B, Si, and O, and a crystalline filler; the element body includes a high-concentration phosphorus-containing portion located along the coil, The P concentration in the base material in the high-concentration phosphorus containing portion is higher than the P concentration in the base material in the central portion of the element body.
[0008] Here, the central part of the element body refers to a part within a radius of 10 μm from the center point of the element body in a cross section of the element body that includes the center point. For example, if the element body is approximately cubic, the center point is the point where the length, width, and height of the element body are all half. If the part within the radius of 10 μm is occupied by a coil and the concentration of P in the base material cannot be detected, the central part is expanded to a part within a radius of 20 μm from the center point. In addition, the P concentration in the base material is the proportion of P when the base material is used as the standard, and is the element concentration obtained by elemental analysis of SEM (scanning electron microscope) images of the base material part of the element body using EDX (energy dispersive X-ray spectroscopy). In addition, in this specification, when "B", "Si", "O", or "P" is written, it refers to the element represented by the corresponding symbol, and "containing the corresponding element" does not mean including the element as a simple substance, but including the corresponding element as a compound.
[0009] According to the above aspect, the element body includes a high-concentration phosphorus-containing portion at a position along the coil, and the concentration of P in the base material in the high-concentration phosphorus-containing portion is higher than the concentration of P in the base material in the center of the element body. As a result, the high-concentration phosphorus-containing portion (glass containing phosphorus) is easily softened, so that adhesion between the coil and the high-concentration phosphorus-containing portion along the coil can be ensured during firing, and the bonding between the element body and the coil can be improved, and peeling between the element body and the coil can be suppressed. In addition, since the high-concentration phosphorus-containing portion (glass containing phosphorus) has a large linear expansion coefficient, the difference in linear expansion coefficient between the coil and the high-concentration phosphorus-containing portion along the coil can be reduced, and the occurrence of cracks in the element body near the coil due to stress caused by the difference in linear expansion coefficient between the element body and the coil inside the product after firing can be suppressed. Therefore, the quality of the inductor component can be improved, and the yield of the inductor component can be improved.
[0010] Preferably, in one embodiment of the inductor component, the high concentration phosphorus-containing portion is present at a position within 10 μm from the surface of the coil.
[0011] According to the embodiment, the high concentration phosphorus containing portion can cover the coil in a film shape, and the volume of the high concentration phosphorus containing portion in the element body can be relatively small, thereby reducing the dielectric constant of the element body, reducing dielectric loss, and improving coil characteristics.
[0012] Preferably, in one embodiment of the inductor component, the concentration of P in the base material in the high concentration phosphorus containing portion is 1.5 times or more the concentration of P in the base material in a central portion of the element body.
[0013] According to the embodiment, the P concentration in the base material in the high-concentration phosphorus containing portion can be relatively high, the bond between the element body and the coil can be improved, and the difference in linear expansion coefficient between the element body and the coil can be reduced.
[0014] Preferably, in one embodiment of the inductor component, The coil has a first coil wiring and a second coil wiring stacked adjacent to each other in the axial direction, the high concentration phosphorus containing portion includes a first high concentration phosphorus containing portion covering at least a portion of a surface of the first coil wiring facing the second coil wiring, and a second high concentration phosphorus containing portion covering at least a portion of a surface of the second coil wiring facing the first coil wiring, The element body has an interlayer portion located between the first high concentration phosphorus containing portion and the second high concentration phosphorus containing portion, and a concentration of P in the base material in the interlayer portion is lower than a concentration of P in the base material in the first high concentration phosphorus containing portion and is also lower than a concentration of P in the base material in the second high concentration phosphorus containing portion.
[0015] According to the embodiment, the P concentration in the base material in the interlayer portion of the element body can be made relatively small, thereby decreasing the dielectric constant of the element body, reducing dielectric loss, and improving coil characteristics.
[0016] Preferably, in one embodiment of the inductor component, the coil partially contains an amorphous material containing B, Si, and O.
[0017] Here, the coil partially encapsulating the amorphous material means that the amorphous material is not completely embedded in the coil, and part of the amorphous material is exposed from the outer circumferential surface of the coil.
[0018] According to the embodiment, the coil partially contains the amorphous material. Therefore, in the sintering step of the manufacturing method of the inductor component, liquid phase sintering is considered to have progressed to the extent that the amorphous material reaches the surface of the coil from the inside of the coil. This further improves the smoothness of the coil, and further enables a high Q at high frequencies.
[0019] Furthermore, high-frequency current flows preferentially on the surface of the coil due to the skin effect. Therefore, if the coil partially contains amorphous material, the surface area of the coil increases and the electrical resistance decreases, making it possible to further increase the Q factor at high frequencies.
[0020] Preferably, in one embodiment of the inductor component, the coil is completely encapsulated in an amorphous material comprising B, Si, and O.
[0021] Here, the coil completely encapsulating the amorphous material means that the amorphous material is completely embedded in the coil and is not exposed from the outer circumferential surface of the coil.
[0022] According to the embodiment, when the coil completely encapsulates the amorphous material, an interface between the coil and the amorphous material is formed within the coil. This increases the surface area of the coil, and reduces the electrical resistance due to the skin effect at high frequencies. Therefore, the inductor component according to the embodiment can further increase the Q factor at high frequencies.
[0023] Preferably, in one embodiment of the inductor component, the crystalline filler includes any of Al, Si, Ti, Zr, Ca, Mg, Fe and Mn.
[0024] According to the embodiment, the strength of the inductor component can be further improved.
[0025] Preferably, in one embodiment of the inductor component, said crystalline filler is quartz particles or crystalline silica particles.
[0026] According to the embodiment, the dielectric constant of the element body can be reduced, and the characteristics of the inductor component can be improved.
[0027] Preferably, in one embodiment of the inductor component, the content of the crystalline filler in the high concentration phosphorus containing portion is not less than 80% and not more than 120% of the content of the crystalline filler in a central portion of the element body.
[0028] According to the embodiment, the content of the crystalline filler does not decrease in the high concentration phosphorus containing portion, and thus the amount of the crystalline filler can be secured in the high concentration phosphorus containing portion, and the strength of the element body can be secured.
[0029] On the other hand, if the content of crystalline filler in the high concentration phosphorus containing portion becomes high, the softening of the high concentration phosphorus containing portion is suppressed, which may reduce the bonding strength between the element body and the coil, and the difference in linear expansion coefficient between the high concentration phosphorus containing portion (element body) and the coil becomes large, which may cause cracks to occur in the element body near the coil due to stress caused by the difference in linear expansion coefficient. However, since the concentration of P in the base material of the high concentration phosphorus containing portion is high, it is possible to promote the softening of the high concentration phosphorus containing portion and improve the bonding strength between the element body and the coil, while reducing the difference in linear expansion coefficient between the high concentration phosphorus containing portion (element body) and the coil and suppress cracks in the element body near the coil.
[0030] Therefore, it is possible to realize an inductor component with high yield while ensuring the strength of the element body.
[0031] Preferably, in one embodiment of the inductor component, The coil has a plurality of coil wires stacked along the axis, In a cross section including the axis, the P concentration distribution in the base material in the high concentration phosphorus containing portion covering at least a portion of the periphery of one coil wiring is different from the P concentration distribution in the base material in the high concentration phosphorus containing portion covering at least a portion of the periphery of the other coil wiring.
[0032] Here, different concentration distributions means, for example, that the thickness and concentration of a high-concentration phosphorus-containing portion on the inner diameter side, outer diameter side, or inter-wiring side of a certain coil wiring is different from the thickness and concentration of a high-concentration phosphorus-containing portion on the corresponding inner diameter side, outer diameter side, or inter-wiring side of another coil wiring. According to the embodiment, in a cross section including the axis, the P concentration distribution in the base material of the high-concentration phosphorus-containing portion becomes random and irregular due to different coil wirings, which improves the bonding between the element body and the coil uniformly throughout the inductor component, and reduces the difference in linear expansion coefficient between the element body and the coil. Effect of the Invention
[0033] According to an inductor component according to one aspect of the present disclosure, it is possible to improve quality and increase yield. [Brief description of the drawings]
[0034] [Figure 1] FIG. 1 is a transparent perspective view showing a first embodiment of an inductor component. [Diagram 2] FIG. 2 is an exploded perspective view of the inductor component. [Diagram 3] 3 is a plan view showing a layer including coil wiring in the bottom layer of FIG. 2. [Figure 4] FIG. 4 is a cross-sectional view taken along line IV-IV of FIG. [Diagram 5] FIG. 5 is a partially enlarged view of FIG. [Figure 6A] 1A to 1C are explanatory diagrams illustrating a manufacturing method of an inductor component. [Figure 6B] 1A to 1C are explanatory diagrams illustrating a manufacturing method of an inductor component. [Figure 6C] 1A to 1C are explanatory diagrams illustrating a manufacturing method of an inductor component. [Figure 7] 11 is a plan view of some layers illustrating a second embodiment of an inductor component. FIG.
[0035] Hereinafter, an inductor component according to one aspect of the present disclosure will be described in detail with reference to the illustrated embodiments. Note that the drawings include some schematic views and may not reflect actual dimensions or ratios.
[0036] First Embodiment (composition) Fig. 1 is a see-through perspective view showing a first embodiment of the inductor component. Fig. 2 is an exploded perspective view of the inductor component. Fig. 3 is a plan view showing a layer including the bottom coil wiring of Fig. 2. Fig. 4 is a cross-sectional view taken along line IV-IV of Fig. 1. Fig. 5 is an enlarged view of a portion of Fig. 4 (enlarged view of part A).
[0037] 1 and 2, the inductor component 1 includes an element body 10, a coil 20 disposed within the element body 10, and a first external electrode 30 and a second external electrode 40 electrically connected to the coil 20. In FIG. 1, the element body 10 is depicted as transparent so that the internal structure of the element body 10 can be easily understood. Also, in FIG. 1, a high-concentration phosphorus-containing portion 101 is not depicted so that the internal structure of the element body 10 can be easily understood.
[0038] The inductor component 1 is electrically connected to wiring on a circuit board (not shown) via the first and second external electrodes 30, 40. The inductor component 1 is used, for example, as an impedance matching coil (matching coil) for high-frequency circuits, and is used in electronic devices such as personal computers, DVD players, digital cameras, TVs, mobile phones, car electronics, and medical and industrial machinery. However, the uses of the inductor component 1 are not limited to this, and it can also be used, for example, in tuning circuits, filter circuits, rectifier circuits, and the like.
[0039] The element body 10 is formed in a substantially rectangular parallelepiped shape. The surface of the element body 10 has a first end face 15, a second end face 16 opposite the first end face 15, a bottom face 17 connected between the first end face 15 and the second end face 16, and a top face 18 opposite the bottom face 17. As shown in the figure, the X direction is a direction perpendicular to the first end face 15 and the second end face 16, the Y direction is a direction parallel to the first end face 15, the second end face 16, and the bottom face 17, and the Z direction is a direction perpendicular to the X direction and the Y direction and perpendicular to the bottom face 17. The shape of the inductor component 1 is not particularly limited, and may be a cylindrical shape, a polygonal columnar shape, a truncated cone shape, or a truncated polygonal pyramid shape.
[0040] The element body 10 is a laminated body in which a plurality of insulating layers 11 are stacked. The stacking direction of the insulating layers 11 is a direction (Y direction) parallel to the first and second end faces 15, 16 and the bottom face 17 of the element body 10. That is, the insulating layers 11 are in a layered form spreading on the XZ plane. In this specification, "parallel" is not limited to a strict parallel relationship, but also includes a substantial parallel relationship taking into account a realistic range of variation. Note that in the element body 10, the interfaces between the plurality of insulating layers 11 may not be clear due to sintering or the like.
[0041] The insulating layer 11 of the element body 10 is made of an insulating material. The insulating material contains a base material made of an amorphous material containing B, Si, and O, and a crystalline filler. When the element body 10 contains the crystalline filler, the element body 10 can suppress the occurrence of cracks due to impact during mounting or stress when the board is bent. In this case, the strength of the inductor component 1 according to this embodiment can be increased. The amorphous material containing B, Si, and O is, for example, borosilicate glass containing B, Si, and O. The amorphous material may include, in addition to borosilicate glass, glasses containing, for example, SiO2, B2O3, K2O, Li2O, CaO, ZnO, Bi2O3, P2O5, and / or Al2O3, such as SiO2-B2O3-K2O glass, SiO2-B2O3-Li2O-Ca glass, SiO2-B2O3-P2O5 glass, SiO2-B2O3-Li2O-CaO-ZnO glass, or Bi2O3-B2O3-SiO2-Al2O3 glass. Two or more of these glasses may be combined.
[0042] The crystalline filler preferably contains, for example, any one of Al, Si, Ti, Zr, Ca, Mg, Fe, and Mn. When the crystalline filler contains any one of the above elements, the strength of the inductor component 1 can be further improved. In addition, the crystalline filler is preferably, for example, quartz particles or crystalline silica particles. This can suppress the dielectric constant of the element body 10, and improve the characteristics of the inductor component 1.
[0043] The first external electrode 30 and the second external electrode 40 are made of a conductive material such as Ag or Cu. The first external electrode 30 is, for example, L-shaped and provided across the first end face 15 and the bottom face 17. The second external electrode 40 is, for example, L-shaped and provided across the second end face 16 and the bottom face 17.
[0044] The first external electrode 30 does not protrude from the first end face 15 and the bottom face 17, but may protrude from at least one of the first end face 15 and the bottom face 17. The second external electrode 40 does not protrude from the second end face 16 and the bottom face 17, but may protrude from at least one of the second end face 16 and the bottom face 17.
[0045] The first external electrode 30 may be provided only on the bottom surface 17 without being provided on the first end surface 15, and similarly, the second external electrode 40 may be provided only on the bottom surface 17 without being provided on the second end surface 16. In other words, it is sufficient that the first external electrode 30 and the second external electrode 40 are provided at least on the bottom surface 17.
[0046] The coil 20 is made of, for example, the same conductive material and amorphous material as the first and second external electrodes 30, 40. The coil 20 is wound in a spiral shape along the axis AX. A first end of the coil 20 is connected to the first external electrode 30, and a second end of the coil 20 is connected to the second external electrode 40. In this embodiment, the coil 20 and the first and second external electrodes 30, 40 are integrated and no clear boundary exists, but this is not limited thereto, and a boundary may exist by forming the coil 20 and the external electrodes using different materials or different construction methods.
[0047] The coil 20 is formed in a substantially elliptical shape when viewed from the direction of the axis AX, but is not limited to this shape. The shape of the coil 20 may be, for example, a circle, an ellipse, a rectangle, another polygon, or a combination of these. The axis AX of the coil 20 refers to the central axis of the spiral around which the coil 20 is wound. In the inductor component 1, the direction of the axis AX of the coil 20 and the lamination direction of the insulating layers 11 refer to the same direction. However, the direction of the axis AX of the coil 20 may be perpendicular to the lamination direction of the insulating layers 11.
[0048] The coil 20 has a winding portion 21a wound in a spiral shape, and an extraction portion 21b that electrically connects the winding portion 21a and the external electrodes 30, 40. The coil 20 includes a coil wiring 21 wound along a plane. The coil wiring 21 is stacked along the axis AX direction. The coil wiring 21 is formed by being wound on a main surface (XZ plane) of the insulating layer 11 perpendicular to the axis AX direction. The coil wiring 21 adjacent to each other in the stacking direction are electrically arranged in series through a via conductor 26 that penetrates the insulating layer 11 in the thickness direction (Y direction). In this way, the coil wirings 21 are electrically connected to each other in series to form a spiral. Specifically, the coil 20 has a configuration in which a plurality of coil wirings 21, each of which is electrically connected to each other and has less than one turn, are stacked, and the coil 20 has a helical shape. The coil wiring 21 is composed of one coil conductor layer 25. The coil wiring 21 has a winding portion 21a wound along a plane and an extraction portion 21b that electrically connects the winding portion 21a and the external electrodes 30, 40. The coil wiring 21 (coil conductor layer 25) is formed on the insulating layer 11.
[0049] 3, 4, and 5, the element body 10 includes a high concentration phosphorus containing portion 101 at a position along the coil 20. The high concentration phosphorus containing portion 101 covers at least a portion of each coil wiring 21 along each coil wiring 21. The high concentration phosphorus containing portion 101 contacts the coil wiring 21. Specifically, the high concentration phosphorus containing portion 101 has a first portion 101a that covers at least a portion of the coil wiring 21 along the coil wiring 21, a second portion 101b that covers at least a portion of the first external electrode 30 along the first external electrode 30, and a third portion 101c that covers at least a portion of the second external electrode 40 along the second external electrode 40.
[0050] The concentration of P in the base material in the high-concentration phosphorus containing portion 101 is higher than the concentration of P in the base material in a central portion 103 of the element body 10. In this embodiment, the reference center point of the central portion 103 is a point that is halfway between the bottom surface 17 in the X direction and the Y direction and halfway between the first end surface 15 in the Z direction.
[0051] The high concentration phosphorus containing portion 101 covers the entire periphery of the coil 20, but may cover the coil 20 partially. That is, the element body 10 may have the high concentration phosphorus containing portion 101 at a position along a part of the coil 20. More specifically, the high concentration phosphorus containing portion 101 may cover only the inner periphery side of the coil 20. That is, the element body 10 may have the high concentration phosphorus containing portion 101 at a position along the inner periphery of the coil 20. That is, the high concentration phosphorus containing portion 101 may contact the inner edge of the coil 20. Also, the high concentration phosphorus containing portion 101 may cover only the outer periphery side of the coil 20. That is, the element body 10 may have the high concentration phosphorus containing portion 101 at a position along the outer periphery of the coil 20. That is, the high concentration phosphorus containing portion 101 may contact the outer edge of the coil 20.
[0052] According to the above configuration, the element body 10 includes the high concentration phosphorus containing portion 101 at a position along the coil 20, and the concentration of P in the base material in the high concentration phosphorus containing portion 101 is higher than the concentration of P in the base material in the central portion 103 of the element body 10. As a result, the high concentration phosphorus containing portion 101 (glass containing phosphorus) is easily softened, so that adhesion between the coil 20 and the high concentration phosphorus containing portion 101 along the coil 20 can be ensured during firing, the bonding between the element body 10 and the coil 20 can be improved, and peeling between the element body 10 and the coil 20 can be suppressed. In addition, since the high concentration phosphorus containing portion 101 (glass containing phosphorus) has a large linear expansion coefficient, the difference in linear expansion coefficient between the coil 20 and the high concentration phosphorus containing portion 101 along the coil 20 can be reduced, and the occurrence of cracks in the element body 10 near the coil 20 due to stress caused by the difference in linear expansion coefficient between the element body 10 and the coil 20 inside the product after firing can be suppressed. Therefore, the quality of the inductor component 1 can be improved, and the yield of the inductor components can be increased.
[0053] In short, the inventors of the present application have noticed that glass containing phosphorus has a relatively low softening point (melting point) and a tendency for the linear expansion coefficient to be large, and have further found that there is an effect that the phosphorus element is likely to segregate (phase-separate) in the vicinity of the coil 20 when the glass containing phosphorus is fired at a high temperature for a long time. In other words, the inventors of the present application have found that the phosphorus element segregates in the vicinity of the coil 20 by adjusting the firing temperature and firing time of the glass containing phosphorus. For example, when borosilicate glass containing phosphorus is used as the glass material, it has been confirmed that when the firing temperature is set to 800°C to 900°C and the firing time is set to 30 minutes to 60 minutes, P in the glass, which is the base material of the element body 10, approaches the metal element of the coil 20, and P can be phase-separated in the vicinity of the coil 20. Based on these findings, the inventors of the present application have arrived at a configuration in which the high-concentration phosphorus-containing portion 101, which has a low softening point and a large linear expansion coefficient, is provided in a position along the coil 20.
[0054] Furthermore, since the element body 10 includes the high-concentration phosphorus-containing portion 101 located along the coil 20, the high-concentration phosphorus-containing portion 101 (glass containing phosphorus) has a low softening point, and the surface of the coil 20 can be smoothed by liquid phase sintering. This makes it possible to suppress loss of current flowing through the coil 20. In particular, because high-frequency current flows preferentially through the surface of the coil 20 due to the skin effect, current loss can be further suppressed. This makes it possible to achieve a high Q for the inductor component 1.
[0055] Preferably, the high concentration phosphorus containing portion 101 is present at a position within 10 μm from the surface of the coil 20. According to the above configuration, the high concentration phosphorus containing portion 101 can cover the coil 20 in a film-like shape, and the volume of the high concentration phosphorus containing portion 101 in the element body 10 can be relatively small. This can reduce the dielectric constant of the element body 10, reduce dielectric loss, and improve the coil characteristics.
[0056] Preferably, the P concentration in the base material in the high concentration phosphorus containing portion 101 is 1.5 times or more the P concentration in the base material in the central portion 103 of the element body 10. Here, as a method for measuring the P concentration in the base material, for example, the P concentration in the base material can be obtained from the concentration distribution in the cross section of the element body 10 using fluorescence spectroscopy, ICP, WDX, etc. Specifically, the average value of the P concentration in the base material is obtained from the cross-sectional image of the central portion 103 parallel to the XZ plane perpendicular to the stacking direction. In the same manner, the average value of the P concentration in the base material is obtained from the cross-sectional image of the high concentration phosphorus containing portion 101. Thereby, the average value of the P concentration in the base material in the high concentration phosphorus containing portion 101 and the average value of the P concentration in the base material in the central portion 103 of the element body 10 are compared.
[0057] According to the above configuration, the P concentration in the base material in the high-concentration phosphorus containing portion 101 can be made relatively high, the bond between the element body 10 and the coil 20 can be improved, and the difference in linear expansion coefficient between the element body 10 and the coil 20 can be made smaller.
[0058] 4, the coil 20 has first coil wiring 211 and second coil wiring 212 stacked adjacent to each other in the axial direction AX. In FIG. 4, the coil wiring in the second layer from the top is the first coil wiring 211, and the coil wiring in the third layer from the top is the second coil wiring 212. However, the other coil wirings may be the first coil wiring 211 and the second coil wiring 212.
[0059] The first coil wiring 211 has an opposing surface 211a opposing the second coil wiring 212. The second coil wiring 212 has an opposing surface 212a opposing the first coil wiring 211. The high concentration phosphorus containing portion 101 includes a first high concentration phosphorus containing portion 1011 covering at least a portion of the opposing surface 211a of the first coil wiring 211, and a second high concentration phosphorus containing portion 1012 covering at least a portion of the opposing surface 212a of the second coil wiring 212.
[0060] The element body 10 has an interlayer portion 100 located between a first high concentration phosphorus containing portion 1011 and a second high concentration phosphorus containing portion 1012. The concentration of P in the base material in the interlayer portion 100 is lower than the concentration of P in the base material in the first high concentration phosphorus containing portion 1011, and is also lower than the concentration of P in the base material in the second high concentration phosphorus containing portion 1012.
[0061] With this configuration, it is possible to relatively reduce the P concentration in the base material in the interlayer portion 100 of the element body 10. This reduces the dielectric constant of the element body 10, reduces dielectric loss, and improves coil characteristics.
[0062] As shown in FIG. 4, the coil 20 has a substantially square cross-sectional shape, but is not limited to this shape. The cross-sectional shape of the coil 20 may be, for example, a circle, an ellipse, a rectangle, another polygon, or a combination of these. If the cross-sectional shape of the coil 20 is a substantially rectangle with a high aspect ratio, the cross-sectional area of the coil 20 increases and the resistance to high-frequency current is reduced, making it possible to further increase the Q. The aspect ratio is (thickness t of the coil wiring 21) / (width w of the coil wiring 21). The width w of the coil wiring 21 indicates the width in the direction perpendicular to the axis AX of the coil 20 in a cross section perpendicular to the extension direction of the coil wiring 21. The thickness t of the coil wiring 21 indicates the thickness of the coil 20 in the axis AX direction in a cross section perpendicular to the extension direction of the coil wiring 21.
[0063] 5, coil 20 preferably partially contains an amorphous material (hereinafter, referred to as exposed glass 107). The amorphous material contains B, Si, and O, and is made of, for example, the same material as the amorphous material contained in element 10. Here, "coil 20 partially contains amorphous material" refers to a state in which the amorphous material is not completely embedded in coil 20, and part of the amorphous material is exposed from the outer circumferential surface of coil 20.
[0064] According to the above configuration, it is believed that in the sintering step of the manufacturing method of the inductor component 1, liquid layer sintering has progressed to an extent that the amorphous material reaches the surface from the inside of the coil 20. This further improves the smoothness of the coil 20, making it possible to further increase the Q factor at high frequencies.
[0065] Furthermore, the high-frequency current flows preferentially on the surface of the coil 20 due to the skin effect. Therefore, when the coil 20 partially contains the exposed glass 107, a recess is formed on the surface of the coil 20, and the surface area of the coil 20 increases. This reduces the electrical resistance. Therefore, it becomes possible to further increase the Q factor at high frequencies.
[0066] 5, coil 20 preferably completely encapsulates amorphous material (hereinafter, referred to as encapsulated glass 105). Here, "coil 20 completely encapsulates amorphous material" refers to a state in which the amorphous material is completely embedded in coil 20 and is not exposed from the outer circumferential surface of coil 20.
[0067] According to the above configuration, when coil 20 completely encapsulates encapsulated glass 105, an interface between coil 20 and encapsulated glass 105 is formed within coil 20. This increases the surface area of coil 20, and reduces electrical resistance due to the skin effect at high frequencies. This further enables a high Q at high frequencies.
[0068] As shown in FIG. 5, the content of the crystalline filler in the high concentration phosphorus containing portion 101 is preferably 80% or more and 120% or less of the content of the crystalline filler in the central portion 103 of the element body 10.
[0069] Here, the content of the crystalline filler is calculated, for example, from the area of the crystalline filler per unit area in the cross section of the element body 10. Specifically, the ratio of the area of the crystalline filler per unit area is obtained from a cross-sectional image (SEM image) of the central portion 103 parallel to the XZ plane perpendicular to the stacking direction. This ratio corresponds to the content of the crystalline filler in the central portion 103 of the element body 10. Similarly, the ratio of the area of the crystalline filler per unit area is obtained from the cross-sectional image of the high concentration phosphorus containing portion 101. This ratio corresponds to the content of the crystalline filler in the high concentration phosphorus containing portion 101.
[0070] According to the above configuration, the content of the crystalline filler does not decrease in the high concentration phosphorus containing portion 101. In this manner, the amount of the crystalline filler can be secured in the high concentration phosphorus containing portion 101, and the strength of the element body 10 can be secured.
[0071] On the other hand, if the content of crystalline filler in the high concentration phosphorus containing portion 101 becomes high, the softening of the high concentration phosphorus containing portion 101 is suppressed, which may reduce the bonding strength between the element body 10 and the coil 20. Also, the difference in linear expansion coefficient between the high concentration phosphorus containing portion 101 (element body 10) and the coil 20 increases, which may cause cracks to occur in the element body 10 near the coil due to stress caused by the difference in linear expansion coefficient. However, since the concentration of P in the base material of the high concentration phosphorus containing portion 101 is high, it is possible to promote the softening of the high concentration phosphorus containing portion 101 and improve the bonding strength between the element body 10 and the coil 20, while reducing the difference in linear expansion coefficient between the high concentration phosphorus containing portion 101 (element body 10) and the coil 20 and suppress cracks in the element body 10 near the coil.
[0072] Therefore, the strength of element body 10 can be ensured, and inductor component 1 can be realized with high yield.
[0073] As shown in FIG. 4, preferably, the multiple coil wirings 21 include one coil wiring 21 and another coil wiring 21, and in a cross section including the axis AX, the concentration distribution of P in the base material in the high concentration phosphorus containing portion 101 covering at least a part of the periphery of the one coil wiring 21 is different from the concentration distribution of P in the base material in the high concentration phosphorus containing portion 101 covering at least a part of the periphery of the other coil wiring 21. For example, in the high concentration phosphorus containing portion 101 covering the one coil wiring 21, the concentration of P in the base material is highest on the outer periphery side of the one coil wiring 21, and in the high concentration phosphorus containing portion 101 covering the other coil wiring 21, the concentration of P in the base material is highest on the inner periphery side of the other coil wiring 21. Note that the positions where the high concentration phosphorus containing portions are thickest may be different, instead of the positions of the high concentration portions. In FIG. 4, any one of the five layers of coil wirings 21 is referred to as the one coil wiring 21, and the other coil wirings 21 of the five layers of coil wirings 21 are referred to as the other coil wirings 21.
[0074] According to the above configuration, in a cross section including the axis AX, the concentration distribution of P in the base material of the high-concentration phosphorus containing portion 101 becomes random and irregular due to the different coil wirings 21. This makes it possible to improve the bonding between the element body 10 and the coil 20 uniformly throughout the inductor component 1, and to reduce the difference in linear expansion coefficient between the element body 10 and the coil 20.
[0075] (Manufacturing method for inductor components) An example of a method for manufacturing an inductor component will now be described with reference to Fig. 2. The method for manufacturing an inductor component includes a mother laminate forming step of forming a mother laminate, a cutting step of cutting the mother laminate to form laminates, a sintering step of sintering the laminate, and a polishing step of polishing the sintered laminate.
[0076] [Mother laminate formation process] The mother laminate is an assembly of a plurality of laminates formed together. In the following description, the members in the assembled state will be given the same names and symbols as the members after separation.
[0077] In the mother laminate formation step, an insulating layer 11 is formed, and a conductor layer is formed on the insulating layer 11. This step is repeated to stack a plurality of insulating layers 11 each having a conductor layer. In this way, a mother laminate is formed. The mother laminate formation step using the screen printing method will be described below.
[0078] (1. Preparation of paste) An insulating paste, a conductive paste, and a conductive paste for external electrodes are prepared. The insulating paste contains a filler material (an example of a crystalline filler), a glass material (an example of a base material; more specifically, glass powder) made of an amorphous material, and a solvent. The amorphous material is, for example, borosilicate glass. The glass material contains phosphorus. The crystalline filler is, for example, ceramics. The insulating paste may further contain an organic material or a composite material, and among these, a material with a small dielectric constant or dielectric loss is preferable. The organic material is, for example, a polymer (more specifically, an epoxy resin, an acrylic resin, a fluororesin, etc.). The composite material is, for example, a glass epoxy resin.
[0079] The conductive paste includes a glass material made of an amorphous material, a conductive material (more specifically, a metal powder), and a solvent. The conductive material is preferably a material with good conductivity, such as Ag, Cu, and Au. The conductive paste for external electrodes includes a conductive material and a solvent, but does not include a glass material made of an amorphous material.
[0080] (2. Formation of outer insulating layer) The outer insulating layer (insulating paste layer) 11 corresponds to the first insulating layer 11 from the bottom in Fig. 2. The insulating paste is applied onto a base material such as a carrier film (not shown) using a screen printing method. This process is repeated to form the outer insulating layer 11 having a predetermined thickness.
[0081] (3. Formation of an insulating layer (first layer) having a conductor layer) An insulating paste is applied onto the outer insulating layer 11 by using a screen printing method to form the insulating layer 11. The insulating layer 11 corresponds to the second insulating layer 11 from the bottom in FIG.
[0082] Next, a conductive paste is pattern-printed into a predetermined shape on the insulating layer 11 using a screen printing method to form a conductor layer. As a method for forming the conductor layer, a photolithography method using a photosensitive conductive paste may be used in addition to the screen printing method. Specifically, the photosensitive conductive paste layer is exposed to active energy rays (more specifically, ultraviolet rays, etc.) through a photomask along a desired coil pattern. After exposure, the layer is developed with a developer (more specifically, an alkaline solution, etc.). This forms a coil conductor layer 25 having a desired coil pattern. Similarly, an external conductive layer having a desired pattern is formed using a conductive paste for external electrodes. As a result, an insulating layer 11 including the coil conductor layer 25 and the external conductor layer is formed.
[0083] (4. Formation of insulating layer (second layer) with conductor layer) A second insulating layer 11 having a conductor layer is formed. This insulating layer 11 corresponds to the third insulating layer 11 from the bottom in Fig. 2. The second insulating layer 11 differs from the first insulating layer 11 in that it has an opening and a via hole, but does not have a coil conductor layer 25.
[0084] An insulating paste is applied onto the first insulating layer 11 to form an insulating paste layer. A laser beam is irradiated onto predetermined locations of the insulating paste layer to form an insulating layer 11 having openings and via holes. A conductive layer is formed in the openings and via holes using a screen printing method. This forms an insulating layer 11 having a conductor layer and via conductors 26.
[0085] (5. Formation of insulating layer (third layer) with conductive layer) A third insulating layer 11 having a conductor layer is formed. This insulating layer 11 corresponds to the fourth insulating layer 11 from the bottom in Fig. 2. The third insulating layer 11 differs from the second insulating layer 11 in that it has a coil conductor layer 25.
[0086] By irradiating predetermined locations of the insulating paste layer with laser light, an insulating layer having openings and via holes is formed on the second insulating layer 11. The conductive paste is pattern-printed into a desired shape to form a conductor layer. As a result, a coil conductor layer 25 is formed in the via holes and on the insulating layer 11, and an external conductor layer is formed in the openings. A third insulating layer 11 is formed.
[0087] (6. Lamination) The process of forming the second and third insulating layers 11 is repeated to form the fourth and subsequent insulating layers 11. The fourth and subsequent insulating layers 11 correspond to the fifth to tenth insulating layers 11 from the bottom in FIG. 2. Then, an outer insulating layer 11 is formed. The outer insulating layer 11 corresponds to the eleventh insulating layer 11 from the bottom in FIG. 2. In this manner, a mother laminate is manufactured.
[0088] A mark layer may be formed before or after forming the outer insulating layer 11. The mark layer is, for example, a colored insulating paste mixed with a filler.
[0089] Moreover, a spin coating method or a spray coating method may be used instead of the screen printing method.
[0090] Furthermore, the mother laminate may include, as the bottom layer, an insulating layer 11 that does not have a conductor layer.
[0091] The openings and via holes may also be formed by pressing, spin coating, or spray coating of an insulating material sheet, followed by laser or drill processing, or photolithography using a photosensitive insulating paste.
[0092] In forming the conductor layer, a plurality of conductor layers may be formed and stacked to form a conductor layer having a cross-sectional shape (rectangle) with a high aspect ratio. The formation of the plurality of conductor layers may be performed by repeating the above-mentioned screen printing method and photolithography method multiple times, or may be performed in combination with other methods.
[0093] Instead of the conductive paste layer, the conductor layer may be formed by a sputtering method, a vapor deposition method, a foil pressure bonding method, or the like. The patterning of the conductor layer is not limited to the above-mentioned screen printing method, and a subtractive method (more specifically, a photolithography method, or the like) or an additive method (more specifically, a semi-additive method, or the like) may be used. The semi-additive method is, for example, a method in which a negative pattern is formed, a plating film is formed, and unnecessary parts are removed.
[0094] In addition, in the mother laminate formation step, the mother laminate may be manufactured by forming the second, fourth, sixth, eighth, and tenth insulating layers 11 from the bottom and the outer insulating layer 11 shown in Fig. 2. The inductor component 1 manufactured by this method has a structure in which insulating layers having coil conductor layers are directly laminated.
[0095] [Cutting process] In the cutting step, the mother laminate is cut to form laminates. For example, the mother laminate is cut by dicing or the like to form a plurality of unsintered laminates so that the outer conductor layers are exposed from the cut surfaces.
[0096] [Sintering process] In the sintering step, the laminate is sintered. At this time, since the material of the insulating layer 11 (insulating paste) contains phosphorus, the laminate is fired at a high temperature of at least a certain temperature (800°C or higher), whereby the phosphorus element segregates in the vicinity of the coil wiring 21, and the high-concentration phosphorus-containing portion 101 can be formed along the coil wiring 21. The segregation of the high-concentration phosphorus-containing portion 101 is controlled by the temperature and time during firing. Note that, as long as the phosphorus element segregates in the vicinity of the coil wiring 21, the firing temperature may be 800°C or lower. Note that, as another method for segregating the phosphorus element, glass containing phosphorus may be used as the material of the coil wiring 21 (conductive paste). In this way, by firing the laminate, the glass containing phosphorus is allowed to seep out around the coil wiring 21 as a sintered body of the conductive paste, and phosphorus can be segregated in the vicinity of the coil wiring 21.
[0097] In this manner, the high concentration phosphorus containing portion 101 can be formed at a position along the coil 20. The high concentration phosphorus containing portion 101 does not need to completely cover the coil 20, and it is sufficient that it is located along the coil 20. In other words, as long as the high concentration phosphorus containing portion 101 is in contact with the coil 20, it may be located partially, for example, only on the inner circumferential side or only on the outer circumferential side of the coil 20. The high concentration phosphorus containing portion 101 may be located along the outer edge and inner edge of the coil 20.
[0098] 6A to 6C, the formation of the coil conductor layer 25 in the sintering process will be described. Fig. 6A to 6C are cross-sectional views showing the change in the coil conductor layer 25 in the sintering process. As shown in Fig. 6A, the coil conductor layer 25 before sintering is a conductor paste in which metal powder 111 and glass powder 113 are dispersed in varnish 19.
[0099] When sintering is started in this state, as shown in Fig. 6B, the solvent burns off and disperses, and adjacent metal powder particles 111 undergo localized shrinkage (necking) and are sintered to become metal parts 115. At this time, the glass powder particles 113 soften and flow between the metal parts 115 to become glass parts 117.
[0100] At this time, as shown in FIG. 6C, the softened glass portion 117 is pushed outward by the contraction of the metal powder 111 and moves to the outer periphery of the coil conductor layer 25. As a result, the surface of the coil conductor layer 25 is sintered in the extruded softened glass (glass portion 117), i.e., in the liquid phase, which further promotes sintering, and the surface is smoothed and crystal growth is likely to occur. This reduces the number of crystal grain boundaries that hinder the flow of current, and reduces the electrical resistance that leads to loss. As a result, the inductor component 1 can have a higher Q. At this time, the encapsulated glass 105 and the exposed glass 107 are formed as the glass portion 117. The encapsulated glass 105 is formed as a result of the glass portion 117 that was located farther from the outer periphery of the coil conductor layer 25 remaining in the coil conductor layer 25 without being pushed out. The exposed glass 107 is formed as a result of the glass portion 117 that was located relatively close to the outer periphery of the coil conductor layer 25 not being completely pushed out and remaining near the surface of the coil conductor layer 25. Therefore, the formed coil conductor layer 25 includes a metal portion 115 and a glass portion 117, and the glass portion 117 includes the encapsulated glass 105 and the exposed glass 107, as shown in FIG.
[0101] In addition, the ratio of encapsulated glass 105 in glass portion 117 depends on the amount of exposed glass 107 extruded, and therefore it is possible to control it using as an index the progress of sintering, more specifically, the degree of contraction based on the volume of metal powder 111. The degree of contraction of metal powder 111 is controlled by, for example, the temperature and time during firing.
[0102] [Polishing process] In the polishing step, the sintered laminate is polished by, for example, barrel processing.
[0103] [Other processes] The manufacturing method of the inductor component 1 may further include a plating step. The plating step is carried out after the polishing step, and plating is performed on the external conductor layer exposed on the outer surface of the laminate. In addition, after the polishing step and before the plating step, a further conductor layer may be provided on the external conductor layer of the laminate by a dipping method or a sputtering method using a conductive paste.
[0104] <Second embodiment> 7 is a plan view showing a second embodiment of the inductor component 1A and corresponds to FIG. 3. The second embodiment differs from the first embodiment in the configuration of the high-concentration phosphorus-containing portion. This different configuration will be described below. Note that in the second embodiment, the same reference numerals as those in the first embodiment denote the same configuration as in the first embodiment, and therefore the description thereof will be omitted.
[0105] 7, in the inductor component 1A of the second embodiment, the high concentration phosphorus containing portion 101A has only a first portion 101a that runs along the coil wiring 21 and covers at least a part of the coil wiring 21. In other words, the high concentration phosphorus containing portion 101A does not have the second portion 101b and the third portion 101c of the first embodiment. According to the above configuration, since the high concentration phosphorus containing portion 101A covers only the coil wiring 21, the volume of the high concentration phosphorus containing portion 101A in the element body 10 can be relatively small. Therefore, the dielectric constant of the element body 10 can be reduced, the dielectric loss can be reduced, and the coil characteristics can be improved.
[0106] The present disclosure is not limited to the above-described embodiments, and design modifications are possible without departing from the scope of the present disclosure. For example, the features of the first and second embodiments may be combined in various ways.
[0107] In the above embodiment, the high concentration phosphorus containing portion is provided along all of the coil wirings, but it is sufficient that the high concentration phosphorus containing portion is provided along at least one of the coil wirings.
[0108] In the above embodiment, the coil partially contains the exposed glass, but the coil does not necessarily have to contain the exposed glass.
[0109] In the above embodiment, the coil completely contains the encapsulated glass, but the coil does not have to contain the encapsulated glass.
[0110] The present disclosure includes the following aspects. <1> An element body made of an insulating material; a coil disposed within the element body and wound helically along an axis; Equipped with The insulating material contains a base material made of an amorphous material containing B, Si, and O, and a crystalline filler; the element body includes a high-concentration phosphorus-containing portion located along the coil, an inductor component, wherein the concentration of P in the base material in the high-concentration phosphorus containing portion is higher than the concentration of P in the base material in a central portion of the element body. <2> The high concentration phosphorus-containing portion is located within 10 μm from the surface of the coil. <1> 2. An inductor component according to claim 1 . <3> the concentration of P in the base material in the high concentration phosphorus containing portion is 1.5 times or more the concentration of P in the base material in the central portion of the element body; <1> or <2> 2. An inductor component according to claim 1 . <4> The coil has a first coil wiring and a second coil wiring stacked adjacent to each other in the axial direction, the high concentration phosphorus containing portion includes a first high concentration phosphorus containing portion covering at least a portion of a surface of the first coil wiring facing the second coil wiring, and a second high concentration phosphorus containing portion covering at least a portion of a surface of the second coil wiring facing the first coil wiring, the element body has an interlayer portion located between the first high concentration phosphorus containing portion and the second high concentration phosphorus containing portion, and a concentration of P in the base material in the interlayer portion is lower than a concentration of P in the base material in the first high concentration phosphorus containing portion and is lower than a concentration of P in the base material in the second high concentration phosphorus containing portion; <1> from <3> 13. An inductor component according to any one of the above. <5> The coil partially contains an amorphous material containing B, Si, and O. <1> from <4> 13. An inductor component according to any one of the above. <6> The coil completely encapsulates an amorphous material containing B, Si, and O. <1> from <5> 13. An inductor component according to any one of the above. <7> The crystalline filler includes any one of Al, Si, Ti, Zr, Ca, Mg, Fe, and Mn. <1> from <6> 13. An inductor component according to any one of the above. <8> The crystalline filler is quartz particles or crystalline silica particles; <1> from <7> 13. An inductor component according to any one of the above. <9> a content of the crystalline filler in the high concentration phosphorus containing portion is 80% or more and 120% or less of a content of the crystalline filler in a central portion of the element body; <1> from <8> 13. An inductor component according to any one of the above. <10> The coil has a plurality of coil wires stacked along the axis, In a cross section including the axis, a concentration distribution of P in the base material in the high concentration phosphorus containing portion covering at least a portion of a periphery of one coil wiring is different from a concentration distribution of P in the base material in the high concentration phosphorus containing portion covering at least a portion of a periphery of another coil wiring. <1> from <9> 13. An inductor component according to any one of the above. [Explanation of symbols]
[0111] 1,1A inductor components 10 Base 11 Insulating layer 20 Coil 21 Coil wiring 21a Winding section 21b Pull-out section 25 Coil conductor layer 26 Via conductor 30 1st external electrode 40 2nd external electrode 100 Interlayer part 101,101A High concentration phosphorus content 101a Part 1 101b Part 2 101c Part 3 103 Central part 105 Inclusion Glass 107 Exposed Glass 111 Metal powder 113 Glass Powder 115 Metal Part 117 Glass Department 211 First coil wiring 211a Opposite side 212 Second coil wiring 212a Opposite side 1011 1st high concentration phosphorus containing part 1012 2nd high concentration phosphorus containing part AX axis
Claims
1. An element body made of an insulating material; a coil disposed within the element body and wound helically along an axis; Equipped with The insulating material contains a base material made of an amorphous material containing B, Si, and O, and a crystalline filler, the element body includes a high-concentration phosphorus-containing portion located along the coil, an inductor component, wherein the concentration of P in the base material in the high concentration phosphorus containing portion is higher than the concentration of P in the base material in a central portion of the element body.
2. 2. The inductor component according to claim 1, wherein the high concentration phosphorus-containing portion is located within 10 μm from the surface of the coil.
3. 3. The inductor component according to claim 1, wherein the concentration of P in the base material in the high-concentration phosphorus-containing portion is at least 1.5 times the concentration of P in the base material in the central portion of the element body.
4. The coil has a first coil wiring and a second coil wiring stacked adjacent to each other in the axial direction, the high concentration phosphorus containing portion includes a first high concentration phosphorus containing portion covering at least a part of a surface of the first coil wiring facing the second coil wiring, and a second high concentration phosphorus containing portion covering at least a part of a surface of the second coil wiring facing the first coil wiring, 3. The inductor component according to claim 1, wherein the element body has an interlayer portion located between the first high concentration phosphorus containing portion and the second high concentration phosphorus containing portion, and a concentration of P in the base material in the interlayer portion is lower than a concentration of P in the base material in the first high concentration phosphorus containing portion and is lower than a concentration of P in the base material in the second high concentration phosphorus containing portion.
5. The inductor component according to claim 1 , wherein the coil partially contains an amorphous material containing B, Si, and O.
6. The inductor component of claim 1 or 2, wherein the coil is completely encapsulated in an amorphous material containing B, Si, and O.
7. 3. The inductor component according to claim 1, wherein the crystalline filler contains any one of Al, Si, Ti, Zr, Ca, Mg, Fe, and Mn.
8. The inductor component according to claim 1 , wherein the crystalline filler is quartz particles or crystalline silica particles.
9. 3. The inductor component according to claim 1, wherein a content of the crystalline filler in the high-concentration phosphorus containing portion is 80% or more and 120% or less of a content of the crystalline filler in a central portion of the element body.
10. The coil has a plurality of coil wires stacked along the axis, 3. The inductor component according to claim 1, wherein in a cross section including the axis, a concentration distribution of P in the base material in the high concentration phosphorus containing portion covering at least a portion of a periphery of one coil wiring is different from a concentration distribution of P in the base material in the high concentration phosphorus containing portion covering at least a portion of a periphery of another coil wiring.
Citation Information
Patent Citations
Dielectric porcelain composition and electronic parts
JP2007022820A
Lamination type inductor and method of manufacturing the same
JP2013098350A
Dielectric glass composition and laminate common mode choke coil including the same
JP2013135088A
Laminated inductor component and manufacturing method of the same
JP2019110170A
Inductor component
JP2021022611A