Method for analyzing crystal structure, crystal form, or crystal distribution of rubber material when extended
The use of a transmission electron microscope with nano-diffraction imaging addresses the challenge of observing localized crystal behavior in rubber materials, offering precise analysis and reduced damage, thereby enhancing understanding of crystal impact on cracks.
Patent Information
- Application Number
- JP2023071742
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-25
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2043-04-25
AI Technical Summary
Existing methods like X-ray diffraction struggle to observe the localized occurrence and effect of stretched crystals in rubber materials, particularly in localized parts, making it difficult to understand their impact on cracks.
Utilizing a transmission electron microscope with a focused electron beam of 100 nm or less for nano-diffraction imaging to analyze crystal structure, morphology, and distribution during stretching, allowing precise observation of localized areas.
Enables high-precision analysis of crystal structure, morphology, and distribution in localized parts of rubber materials during stretching, reducing electron beam damage and providing detailed insights into crystal behavior.
Smart Images

Figure 2024157396000002 
Figure 2024157396000003 
Figure 2024157396000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for analyzing the crystal structure, crystal morphology, or crystal distribution of a rubber material during stretching. [Background technology]
[0002] Conventionally, techniques such as wide-angle X-ray diffraction (WAXD) and other X-ray diffraction techniques have been used to observe the state of stretched crystals in the entire rubber material. Summary of the Invention [Problem to be solved by the invention]
[0003] Techniques such as X-ray diffraction can be powerful tools for understanding the state of elongated crystals throughout the entire sample, but it is necessary to observe them in real space to understand how elongated crystals occur locally and how they act on cracks.
[0004] The present invention aims to solve the above-mentioned problems and provide an analysis method capable of analyzing the crystal structure, crystal morphology, and crystal distribution of a rubber material during stretching, even in a localized portion of the rubber material. [Means for solving the problem]
[0005] The present invention relates to a method for analyzing the crystal structure, crystal morphology, or crystal distribution of a rubber material during stretching, using a transmission electron microscope to observe the stretching deformation behavior and / or the state of the rubber material during stretching, and using a nanodiffraction imaging method in which an electron diffraction pattern obtained by scanning an electron beam focused to a diameter of 100 nm or less on the surface of the rubber material is analyzed. Effect of the Invention
[0006] The present invention is a method for analyzing the crystal structure, crystal morphology, or crystal distribution of a rubber material during stretching by using a transmission electron microscope to observe the stretching deformation behavior and / or the state of the rubber material during stretching, and by using a nanodiffraction imaging method in which an electron diffraction pattern obtained by scanning an electron beam focused to a diameter of 100 nm or less on the surface of the rubber material is analyzed. Therefore, an analysis method can be provided that makes it possible to analyze the crystal structure, crystal morphology, and crystal distribution of a rubber material during stretching, even in a localized portion of the rubber material. [Brief description of the drawings]
[0007] [Figure 1] This figure shows the relationship between the nominal tensile strain (between the chucks) and the stress of the sample, and the relationship between the nominal strain (at the irradiated area) and the stress of the sample. [Diagram 2] Fig. 2(a) is a schematic diagram showing the stretching deformation mechanism when observing the state of a sample during stretching using a transmission electron microscope to obtain an observation image. Fig. 2(b) is a schematic diagram of an apparatus equipped with the annular dark-field method and nano-diffraction imaging method of scanning transmission electron microscopy, and the observation method. [Diagram 3] These are TEM images of the sample at various strains during the stretching process. [Figure 4] FIG. 4 is an enlarged view of a void (air gap) portion in the TEM image of FIG. 3 where strain is 0, 2.4, 3.9, and 6.1, and is a schematic diagram showing the state of void growth. [Diagram 5] This figure shows the state of crystals observed by nano-diffraction imaging using the annular dark-field method of scanning transmission electron microscopy for regions (1) and (2) of the 12-divided portion of the stretched TEM observation image of strain = 6.1 in Figure 3. [Figure 6] This is a diffraction pattern obtained by accumulating nine electron diffraction patterns (μ-ED patterns) obtained by irradiating a micron-sized electron beam locally on a sample as shown in Figure 5. [Figure 7] This is a diffraction pattern obtained by wide-angle X-ray diffraction at a position away from the void (air gap). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] The analytical method of the present invention is a method for analyzing the crystal structure, crystal morphology, or crystal distribution of a rubber material (sample) during stretching by using a transmission electron microscope to observe the stretching deformation behavior and / or the state of the rubber material (sample) during stretching, and by using a nanodiffraction imaging method to analyze an electron diffraction pattern obtained by scanning an electron beam focused to a diameter of 100 nm or less over the surface of the rubber material (sample surface).
[0009] Using techniques such as X-ray diffraction (WAXD), it is difficult to grasp the crystalline state of a rubber material during stretching, especially the crystalline state in localized portions of the rubber material during stretching. On the other hand, the present invention uses a nanodiffraction imaging method in which, for example, a transmission electron microscope is used to observe the state of a rubber material during stretching, and a scanning transmission electron microscope method with atomic resolution is used for a local portion of the electron microscope image obtained thereby, and an electron diffraction pattern obtained while scanning an electron beam focused to a diameter of nm on the surface of the rubber material is analyzed, thereby making it possible to accurately observe the crystalline state even in a local portion of the rubber material during stretching. Stretched crystals are very sensitive to electron beam damage, and when a specified amount of electron beam is irradiated, the diffraction peaks of the stretched crystals disappear, so it is important to observe without irradiating the electron beam as much as possible. If the procedure is performed in the order of stretched TEM → field of view search → diffraction, diffraction peaks will not be obtained due to unintended electron beam damage that is thought to be caused by image observation (field of view search). On the other hand, in the present invention, field of view search is not performed, and a diffraction pattern is obtained while comprehensively scanning with the electron beam, and then the procedure is performed by selecting the image. This simplifies the procedure of searching for the observation field of view and allows a large measurement field of view, and a detailed analysis field of view can be selected when analyzing the diffraction pattern. This makes it possible to accurately observe the crystal state, specifically the crystal structure, crystal morphology, and crystal distribution of the rubber material, even in localized parts of the rubber material during stretching.
[0010] Examples of rubber materials (samples) applicable to the above analysis method include samples of a rubber component alone and samples of a rubber composition containing a rubber component and other components.
[0011] The rubber component is not particularly limited, and for example, diene rubber can be used. Examples of diene rubber include isoprene rubber, butadiene rubber (BR), styrene butadiene rubber (SBR), styrene isoprene butadiene rubber (SIBR), ethylene propylene diene rubber (EPDM), chloroprene rubber (CR), and acrylonitrile butadiene rubber (NBR). Other examples include butyl rubber and fluororubber. These may be used alone or in combination of two or more.
[0012] The rubber material (sample) may contain a filler. Examples of the filler include silica, carbon black, calcium carbonate, talc, alumina, clay, aluminum hydroxide, aluminum oxide, mica, etc. For example, the above method can be suitably applied to a sample of a rubber composition containing silica and / or carbon black.
[0013] The rubber material (sample) may contain other components in addition to the rubber component and the filler. For example, the above method can be suitably applied to a sample of a rubber composition containing at least one compounding agent commonly used in the tire industry, such as a plasticizer, an antioxidant, stearic acid, wax, zinc oxide, sulfur, and a vulcanization accelerator. In particular, from the viewpoint of measuring the elongation rate of the sample, a sample of a rubber composition containing zinc oxide can be suitably applied. When zinc oxide is contained, the elongation rate in the observation field of the transmission electron microscope image during elongation can be calculated from the distance between the zinc oxide particles.
[0014] The rubber material (sample) is produced by a general method, for example, by kneading the ingredients in a kneading machine such as a Banbury mixer or an open roll, and then vulcanizing the ingredients as necessary.
[0015] In the above analysis method, the type of transmission electron microscope (TEM) that can be used is not particularly limited, but from the viewpoint of improving measurement accuracy, it is preferable to use a scanning transmission electron microscope (STEM). In the above method, the use of a transmission electron microscope allows the state of a rubber material (sample) during stretching to be observed directly with high accuracy. In particular, it is preferable to obtain TEM images (images obtained by in situ tensile 3D TEM observation of the rubber material) at various strains (during stretching) during the stretching process of the rubber material (sample) and directly observe the state of the rubber material (sample) during various stretching.
[0016] In the above-mentioned analysis method, a transmission electron microscope is used to directly observe the stretching deformation behavior and / or state of a rubber material (sample) during stretching to obtain an observation image (electron microscope image), and the observation image is analyzed using a nanodiffraction imaging method (NDI method) in which an electron beam focused to a diameter of nm is scanned over the surface of the rubber material (sample surface) to obtain an electron diffraction pattern for a local portion of the electron microscope image. This makes it possible to accurately observe the crystalline state even in a local portion of the rubber material during stretching.
[0017] When directly observing the stretching deformation behavior and / or the state of a rubber material (sample) during stretching using a transmission electron microscope, the local strain (ε) within the observation field of the transmission electron microscope image is preferably 1 or more, more preferably 2 or more, and is preferably 40 or less, more preferably 20 or less.
[0018] From the viewpoint of measurement accuracy, it is desirable to use a nano-diffraction imaging method for the above analysis method, which uses a STEM with atomic resolution and analyzes the electron diffraction (ED) pattern acquired by scanning the surface of the rubber material with a focused electron beam converged to a nanometer diameter. The STEM-based NDI method can visualize the distribution of crystal structure on the nm scale by scanning an electron beam with a diameter of several nanometers on the nm order and acquiring an electron diffraction pattern (ED diagram) from each point.
[0019] From the viewpoint of measurement accuracy, the spatial resolution of the scanning transmission electron microscope is preferably less than 0.2 nm, more preferably less than 0.1 nm. There is no particular lower limit, and the smaller the spatial resolution, the more desirable it is.
[0020] For example, when observing the state of crystals by the NDI method using a STEM, it is desirable to obtain an ED pattern while scanning an electron beam narrowed to nm size on a sample in nm steps. From the viewpoints of measurement accuracy and minimizing damage to the sample, it is preferable to scan in nm steps of 20 nm x 20 nm, and more preferably in nm steps of 5 nm x 5 nm.
[0021] Regarding the NDI measurement conditions, for example, from the viewpoint of spatial resolution, the probe size is preferably φ1 to φ150 nm, more preferably φ1 to φ20 nm. From the viewpoints of measurement error, analysis accuracy, and suppression of damage to the sample, the total dose is 1.0×10 -6 ~1.0×10 3 e - / Å 2 is preferred, and 1.0×10 -3 ~1.0×10 3 e - / Å 2 Here, the total dose is a value expressed by dose rate × dwell time.
[0022] An example of the analysis method of the present invention will be described below, but the method is not limited to the following method.
[0023] As a sample (rubber material), for example, a rubber composition (vulcanized rubber composition) of Blend 1 shown in Table 1 is prepared. [Table 1]
[0024] Figure 1 shows the relationship between nominal tensile strain (between chucks) and stress, and the relationship between nominal strain (at the irradiated area) and stress for the sample of formulation 1. Here, crystallization begins before the sudden increase in stress in the sample.
[0025] The upper diagram in Figure 2 (Figure 2(a)) is a schematic diagram showing the mechanism of deformation due to stretching when a transmission electron microscope is used to observe the state of a sample (rubber material) during stretching and obtain an observation image. The tensile 3D TEM holder 11 (sample cartridge) achieves two-way pulling (pulling the observation sample in opposite directions at the same time) of the observation sample (rubber material) 12. As a result, the sample is stretched by two-way pulling, making it possible to perform TEM observation without any misalignment of the field of view even during stretching.
[0026] From the sample of Formulation 1, a thin section is prepared with a diamond knife using a cryo-ultramicrotome and fixed to a sample cartridge. The fixed thin section is observed under various stretching (distortion) conditions using a TEM. An example of the preparation conditions for the thin section (observation sample) is as follows, but can be changed as appropriate.
[0027] (Production conditions) Cryo-ultramicrotome: cutting temperature -160℃ Film thickness before stretching: 400nm
[0028] FIG. 3 shows TEM images of the sample at various strains (ε) during the stretching process (ε = 0, 2.4, 3.9, 6.1). The dark areas in the figure are zinc oxide, etc., and the light areas are the rubber matrix. The sample is stretched in the vertical direction relative to the observation field. By measuring the distance between the zinc oxide aggregates in each TEM image, the strain and stretch rate at each stretching stage can be calculated. Since it is possible to observe the increase in the distance between the zinc oxide aggregates in synchronization with the operation of the tensile 3D TEM holder 11, there is no misalignment of the field during stretching, and in situ observation (observation at the relevant point of the stretching location) at various strains during the sample stretching process is possible. For microscopic deformations, such as the generation of nanovoids and deformation of zinc oxide particle aggregates, in situ same-field observation using the tensile 3D TEM holder 11 is very effective. An example of the observation conditions for the stretching TEM is as follows, but can be changed as appropriate.
[0029] (Stretched TEM observation conditions) Resolution: 7.14nm Dose: 6.2×10 -4 e - / (Å 2 (1 piece)
[0030] Figure 4 shows an enlarged view of the voids (air gaps) in the TEM images of Figure 3 with strains (ε) = 0, 2.4, 3.9, and 6.1, as well as a schematic diagram showing the state of void growth. The enlarged view of the voids shows that when the sample is stretched to ε = 6.1, voids are generated and grow near the zinc oxide. The schematic diagram of void growth also shows that in the case of low strain, voids grow along the rubber / zinc oxide interface, and when the stretching strain is a certain level or higher (e.g., ε > 2.0), the growth of voids increases rapidly, suggesting that the voids show a two-stage growth process near the zinc oxide.
[0031] In the above analysis method, the crystallization state of the rubber material during stretching can be observed using, for example, the annular dark field method of scanning transmission electron microscopy (ADF-STEM) and the nano-diffraction imaging method (NDI) while observing the TEM observation of the sample at various strains (ε) during the stretching process. The lower diagram of Figure 2 (Figure 2(b)) is a schematic diagram showing the ADF-STEM and NDI equipped equipment and the observation method used in this case. Here, the crystal state inside the rubber material during stretching can be observed using the above-mentioned nano-diffraction imaging method while observing images using the annular dark field method of scanning transmission electron microscopy. ADF-STEM is a method in which a finely focused electron beam is irradiated while scanning the sample, and the transmitted electrons scattered at high angles are detected by an annular detector, and the integrated intensity of the detected electrons is displayed.
[0032] In FIG. 2(b), the scanning transmission electron microscope (STEM) may include, for example, an electron source that outputs an electron beam, a converging lens that converges the electron beam output by the electron source, and an objective lens that focuses the electron beam output from the electron source on the position of a sample. The converging lens can, for example, converge the electron beam to a nanometer level or less. The scanning transmission electron microscope may include, for example, a scanning coil that is disposed between the electron source and the objective lens and causes the electron beam to scan the surface of the sample, and an imaging lens that images the electron beam that has passed through the sample on an imaging plane.
[0033] The apparatus in Fig. 2(b) includes an annular dark field (ADF) detector 13 arranged at the imaging plane where the dark field image is formed, and also includes a pixel detector 14. Fig. 2(b) further illustrates that electron diffraction (ED) measurements are also performed, and more specifically, that a micro-electron diffraction (μ-ED) image is acquired.
[0034] When observing the state of crystallization using ADF-STEM and NDI, an electron microscope technique (nanodiffraction imaging, NDI) can be used in which a nanometer-scale structural parameter such as the crystallization rate is mapped by analyzing a large number of electron diffraction patterns obtained by scanning a sample in nm steps (20 nm x 20 nm in Figure 2(b)) with an electron beam narrowed to nm size. An example of NDI measurement conditions is as follows, but these can be changed as appropriate.
[0035] (NDI measurement conditions) Pixel size: 20×20nm 2 Probe size:φ20nm Dwell time:5.0×10 -3 s Total dose: 8.0e - / Å 2 Pixel detector: STELA camera Camera length: 400mm
[0036] Figure 5 shows the state of the crystals observed by nano-diffraction imaging (NDI) using annular dark-field scanning transmission electron microscopy (ADF-STEM) with atomic resolution for regions (1) and (2) of the 12-division (3 × 4) portion of the elongated TEM observation image of strain (ε) = 6.1 in Figure 3. Region (2) shows an ADF-STEM image of the area where voids have formed, and region (1) shows an ADF-STEM image of an area away from the voids.
[0037] The μ-ED patterns shown in FIG. 5 are composed of nine patterns (one set) for two locations (local) in region (1) and two locations (local) in region (2). Each pattern (each diffraction pattern) that composes the nine patterns has a pixel size of 20×20 nm. 2 A diffraction pattern obtained by integrating 5 × 5 (25) patterns (5 × 5 Bined, 100 2 nm 2 ).
[0038] When analyzing a diffraction pattern obtained by such electron diffraction, from the viewpoint of measurement accuracy, the integrated area of the diffraction pattern is 1×1 to 1000×1000 nm 2 The area is preferably 5×5 to 150×150 nm 2 In the case of FIG. 5, the integration area is preferably 100×100 nm 2 It is.
[0039] Then, one diffraction pattern (5×5 Bined, 100) is obtained by integrating the above 5×5 (25) patterns. 2 nm 2 ) is a set of nine μ-ED patterns (3×3, 300 2 nm 2 An example of the electron beam irradiation conditions for electron diffraction is as follows, but these can be changed as appropriate.
[0040] (Electron beam irradiation conditions) Dose rate: 2.9×10 -3 e - / Å 2 Exp. time:5.0s Total dose: 0.015e - / Å 2 Beam size: φ2.1μm
[0041] Figure 6 shows a set of nine μ-ED patterns (3×3, 300 2 nm 2 ) for each of the nine patterns, the diffraction pattern (3 × 3 binned, 300 2 nm 2 ) is shown. The degree of crystallinity Xc at each point can be calculated from the integrated diffraction pattern obtained by integrating these nine patterns, and it is 14%, 16%, 13%, and 20%, respectively. Figure 6 suggests that the degree of crystallinity is the same in the areas away from the voids, while the degree of crystallinity is higher in the vicinity of the voids.
[0042] FIG. 7 shows a diffraction pattern obtained by wide-angle X-ray diffraction (WAXD) at a position away from the void. The crystallinity of 11% obtained from the WAXD diffraction pattern is roughly consistent with the crystallinity of 13-16% obtained from μ-ED at a position away from the void in FIG. 6, confirming the validity of the μ-ED analysis described above. An example of the WAXD measurement conditions is as follows, but can be changed as appropriate.
[0043] (Measurement conditions) No. 7 dumbbell test piece Beam size: 350×0.400μm 2
[0044] As described above, the procedures for TEM image observation and diffraction measurement have been revised, and a transmission electron microscope is used to observe the state of the rubber material during stretching, while the nano-diffraction imaging method is used in which the electron diffraction pattern obtained by scanning a focused electron beam over the surface of the rubber material is analyzed. In other words, without searching for a field of view, a diffraction pattern is obtained by comprehensively scanning the electron beam, and then the image is selected. This reduces the damage caused by the electron beam to the sample, making it possible to detect the electron diffraction peaks of the elongation crystals and analyze the crystallization state of the rubber material during stretching.
[0045] In particular, by carrying out and analyzing simultaneous ADF-STEM and NDI measurements in addition to in-situ TEM observation of stretching, it is possible to obtain indications that, for example, in the case of elongation crystals in the high strain region (e.g., ε = 6.1), the degree of crystallinity is high near voids.
[0046] Therefore, it is believed that the analytical method of the present invention will lead to elucidation of the effect of local deformation behavior on the spatial / orientation distribution of elongated crystals.
[0047] The present invention (1) is a method for analyzing the crystal structure, crystal morphology, or crystal distribution of a rubber material during stretching, using a transmission electron microscope to observe the stretching deformation behavior and / or the state of the rubber material during stretching, and using a nanodiffraction imaging method in which an electron diffraction pattern obtained by scanning an electron beam focused to a diameter of 100 nm or less on the surface of the rubber material is analyzed.
[0048] The present invention (2) is the method according to the present invention (1), in which the nano-diffraction imaging method is carried out under the following measurement conditions: (Measurement conditions) Probe size: φ1~φ150nm Total dose: 1.0×10 -6 ~1.0×10 3 e - / Å 2
[0049] In the present invention (3), when analyzing a diffraction pattern obtained by performing electron diffraction, the integrated area of the diffraction pattern is 1×1 to 1000×1000 nm 2 The method according to the present invention (1) or (2) is in the above-mentioned range.
[0050] The present invention (4) is a method of any combination with any of the present inventions (1) to (3), in which the local distortion within the observation field of a transmission electron microscope image is 1 to 40. [Explanation of symbols]
[0051] 11 Tensile 3D TEM holder (sample cartridge) 12 Observation sample (rubber material) 13 Annular dark field detector 14 pixel detector
Claims
1. A method for analyzing the crystal structure, crystal morphology, or crystal distribution of a rubber material during stretching, using a transmission electron microscope to observe the stretching deformation behavior and / or the state of the rubber material during stretching, and using a nanodiffraction imaging method in which an electron diffraction pattern obtained by scanning an electron beam focused to a diameter of 100 nm or less on the surface of the rubber material is analyzed.
2. The method according to claim 1, wherein the nano-diffraction imaging method is carried out under the following measurement conditions: (Measurement conditions) Probe size: φ1~φ150nm Total dose: 1.0×10 -6 ~1.0 x 10 3 e - / Å 2
3. Furthermore, when analyzing the diffraction pattern obtained by performing electron diffraction, the integrated area of the diffraction pattern is 1×1 to 1000×1000 nm 2 The method of claim 1, in the region of
4. 2. The method according to claim 1, wherein the local distortion within the observation field of a transmission electron microscope image is 1 to 40.
Citation Information
Patent Citations
Analysis of composition structure for high molecule material surface
JP1983155331A
Method for forming transmitted electron beam intensity distribution image
JP2004004042A
Mesh and rubber segment observation method
JP2008096161A
Method and system for lattice distortion measurement
JP2009250943A
Methods for collecting and processing electron diffraction data
JP2014521106A
Cited By
Gaming machine
JP2026052642A
Gaming machine
JP2026052643A
Gaming machine
JP2026052644A
Gaming machine
JP2026052645A
Gaming machine
JP2026052646A