By coating the surface of the metal material with non-stoichiometric oxide, carbide or nitride coating, the problem of embrittlement of metal materials in hydrogen-containing fluid media is solved, and higher resistance to hydrogen embrittlement and corrosion resistance is achieved, ensuring the long-term stability and accuracy of the pressure sensor.
Patent Information
- Application Number
- JP2024533999
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-23
- Filing Date
- 2022-11-09
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2042-11-09
AI Technical Summary
In the prior art, metal materials are susceptible to hydrogen embrittlement when in contact with hydrogen-containing fluid media, resulting in material embrittlement and long-term stability of pressure sensors. Conventional protective measures such as the gold layer are easily damaged, which cannot effectively prevent hydrogen penetration.
Non-stoichiometric oxides, carbides or nitrides are used to coat the metal material as protective layers to form a non-stoichiometric oxide, carbide or nitride coating to reduce hydrogen permeability, and improve the anti-hydrogen embrittlement of the material through microstructure adjustment and interface treatment.
Effectively reduce hydrogen permeability, improve the hydrogen embrittlement resistance and corrosion resistance of metal materials, ensure long-term stability and accuracy of pressure sensors, and avoid the fragility and damage problems of traditional gold layers.
Smart Images

Figure 2024544379000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a diaphragm for use with a hydrogen-containing fluid medium, and to a transducer including the diaphragm. [Background technology]
[0002] The diaphragm separates the fluid medium in the first space from the second space. In the field of pressure measurement technology, transducers often comprise a diaphragm. The diaphragm separates the measuring device (e.g. the transducer element) from the fluid medium whose pressure is to be determined. The fluid medium is a gaseous medium and / or a liquid medium. For this purpose, the diaphragm usually comprises a surface having a first dimension and a second dimension, the first dimension and the second dimension extending substantially in a direction perpendicular to the longitudinal axis. In a third dimension extending parallel to the longitudinal axis, the diaphragm has a thickness, also called wall thickness.
[0003] In the following, fluid medium is understood to mean a hydrogen-containing fluid medium which contains at least 1% by volume of hydrogen.
[0004] Typically, the surface of the diaphragm comprises an area in contact with the fluid medium in the first space. In the case of a pressure transducer, the pressure of the fluid medium acting on the area of the diaphragm is transmitted to the pressure transducer element (transducer element for short) with as few losses as possible. The flexibility of the diaphragm area directly exposed to the fluid medium should be as high as possible or its stiffness as low as possible, so that the sensitivity of the measuring device including the transducer element is less affected by the diaphragm. However, the material of this low stiffness area should not be irreversibly deformed by the measuring pressure. When using materials with a yield strength of about 400 MPa (megapascals), the diaphragm must be of an appropriate thickness so that it is not irreversibly deformed. In addition, the diaphragm may comprise a thicker area, for example where the diaphragm is connected to the transducer housing. The thicker area also serves to improve the stability of the diaphragm.
[0005] The yield strength of metallic materials is determined by the standard DIN EN ISO 6892-1. It is P 0.2 Equivalent to the value.
[0006] The surface of the diaphragm may extend substantially along the first and second dimensions, but may be partially curved in the direction of the longitudinal axis.
[0007] A diaphragm can also separate the fluid medium from other types of transducer elements, for example in a temperature transducer, where the temperature transducer element is separated from the fluid medium by a diaphragm. In this case, the temperature of the fluid medium is transferred to the temperature transducer element through the diaphragm. Again, the walls of the diaphragm need to be as thin as possible to obtain the highest possible heat transfer coefficient.
[0008] Corrosion is generally understood to mean a measurable change in a substance. Corrosion can occur due to exposure to various substances. Thus, corrosion of metallic materials is well known in relation to various alkalis or acids, gases (e.g. hydrogen or oxygen), salt water, and many other substances.
[0009] However, hereinafter, unless otherwise stated, corrosion refers to corrosion caused by atomic and / or molecular hydrogen.
[0010] When the fluid medium contains hydrogen, the diaphragm must be both tight and resistant to atomic and / or molecular hydrogen. For this reason, commercially available hydrogen-resistant polycrystalline metals, such as austenitic steel 1.4404 (also known as 316L), with a yield strength of about 400 MPa at room temperature, or nickel-based alloy 2.4819 (also known as C-276), also with a yield strength of about 400 MPa at room temperature, are often used as materials for diaphragms that are also heat-resistant above 200°C. However, these materials are characterized by an average grain size of more than 20 μm. Coarse-grained polycrystalline metals are less suitable as materials for thin diaphragms with a thickness of less than 500 μm, since only a few grains are present in the thin-walled regions of the diaphragm, which may cause the material to not behave isotropically. Furthermore, the diffusion path of molecular and / or atomic hydrogen along the grain boundaries between the grains is relatively short through the coarse-grained regions. This is a disadvantage because the short path allows hydrogen to easily diffuse through the diaphragm.
[0011] The designation 1.4404 as well as the other material numbers listed below correspond to DIN EN 10027-2.
[0012] So-called hydrogen embrittlement occurs when molecular and / or atomic hydrogen penetrates into metallic materials, which then run the risk of causing brittle fracture when the material is subjected to stress.
[0013] Hydrogen embrittlement refers to the intrusion and subsequent incorporation of hydrogen into the lattice structure of a metal or alloy, altering its ductility and strength, potentially resulting in hydrogen-related cracking and limiting the use of susceptible materials in applications in contact with hydrogen.
[0014] It is well known that stronger metals or alloys are more susceptible to hydrogen embrittlement than weaker metals.
[0015] The materials steel 1.4404 (also known as 316L) and alloy 2.4819 (also known as C-276) are generally considered to be corrosion resistant. They have a low yield strength and therefore exhibit a higher plastic deformation capacity at lower forces than materials with a higher yield strength. To compensate for this drawback, diaphragms are often manufactured with thicknesses of more than 500 μm. However, this is a disadvantage, since thicker diaphragms have a higher inertial mass. In addition, thicker diaphragms are also more rigid.
[0016] In one known embodiment, the pressure transducer comprises a space behind the diaphragm, which is filled with a fluid pressure transmission medium. In this embodiment, the risk of the diaphragm undergoing irreversible plastic deformation is low, since the fluid pressure transmission medium opposes the deformation of the diaphragm. The fluid pressure transmission medium (e.g. oil with low compressibility) transmits the pressure acting on the diaphragm to a measuring element located away from the diaphragm. Furthermore, the diaphragm is required to transmit the pressure with as few losses as possible, i.e. it is advantageous for the diaphragm to be made thin. If the fluid medium to be measured contains hydrogen, over time hydrogen accumulates in the fluid pressure transmission medium, increasing its volume and causing the diaphragm to bulge outwards. The diaphragm expands due to hydrogen diffused through it. This can on the one hand damage the diaphragm and on the other hand change the pressure conditions near the measuring element. The diffusion of molecular and / or atomic hydrogen through the diaphragm has a negative effect on the long-term stability of the transducer.
[0017] US Pat. No. 5,399,366 describes a transducer with a diaphragm made of alloy 2.4819 (also known as C-276). The material itself is considered to be corrosion resistant, but due to the low thickness of the diaphragm, it is not impermeable to hydrogen. By depositing a soft gold layer on the diaphragm, the diffusion of molecular and / or atomic hydrogen is prevented. The gold layer is substantially chemically inert, which reduces the dissociation of molecular components from the fluid medium in contact with the diaphragm. Dissociation of molecular components of the fluid medium or other chemical reactions at and with the surface can lead to corrosion of the surface. However, due to the low strength of gold, the soft gold layer is not scratch resistant and can therefore be damaged during use and subsequently fail to function as a diffusion barrier to hydrogen. [Prior art documents] [Patent documents]
[0018] [Patent Document 1] US Patent Application Publication No. 2005 / 0109114 Summary of the Invention [Problem to be solved by the invention]
[0019] It is an object of the present invention to provide an improved diaphragm to alleviate the above-mentioned drawbacks.It is a further object of the present invention to improve the corrosion resistance of the diaphragm to atomic and / or molecular hydrogen. [Means for solving the problem]
[0020] This object is achieved by the features of the independent claims.
[0021] The present invention relates to a diaphragm for hermetically separating a first space containing a hydrogen-containing fluid medium from a second space. The diaphragm comprises a metallic material. The diaphragm comprises a coating for reducing the permeability of molecular and / or atomic hydrogen, the coating being deposited between the metallic material of the diaphragm and the fluid medium, at least in the area that contacts the fluid medium during use. The coating comprises an oxide, carbide or nitride, such as aluminum oxide, aluminum carbide, aluminum nitride, chromium oxide, chromium nitride, silicon oxide, silicon carbide, silicon nitride, titanium oxide, titanium carbide, titanium nitride, zirconium oxide, rare earth carbide or nitride, or rare earth oxide.
[0022] According to the present invention, the coating comprises at least one non-stoichiometric oxide, carbide, or nitride.
[0023] Preferably, the coating comprises a non-stoichiometric mixture.
[0024] For example, the diaphragm is a diaphragm for a transducer for determining the pressure of a fluid medium.
[0025] Preferably, the metallic material is an alloy comprising at least one chemical element including a metal and at least one other chemical element.
[0026] The diaphragm is intended to separate a space containing a hydrogen-containing fluid medium from another space. The hydrogen-containing fluid medium contains at least 1% by volume of hydrogen and is also referred to in the following text as corrosive agent or corrosive fluid medium.
[0027] The metallic material of the diaphragm is composed of a metal or alloy, such as, for example, a nickel-based alloy (e.g., electroformed nickel, nickel 270, nickel 301, K-Monel), or a titanium-based alloy (e.g., pure titanium, Ti-6Al-4V, Ti-5Al-2.5Sn, Ti-11.5Mo-6Zr-4.5Sn, alpha-2TiAl alloy, gamma-TiAl alloy), or a copper-based alloy (e.g., OFHC copper, aluminum, bronze, Be-Cu alloys, GRCop-84 (Cu-8Cr-4Nb), NARloy-Z (Cu-3Ag-0.5Zr), 70-30 brass), or aluminum-based alloys (e.g., 1100-T0, 2011, 2024, 5086, 6061-T6, 6063, 7039, 7075-T73), or austenitic steels (e.g., CG-27, Tenelon, A302B, A286, 216, 304L, 304N, 304LN, 305, 308L, 309S, 310, 316, 321, 347, 18-2-12 (Nitronic 32), 21-6-9 (Nitronic 40), 22-13-5 (Nitronic 50), 18-18Plus, 18-2-Mn, 18-3-Mn), or ferritic steels (e.g., A106-Gr.B, A212-61T, A 372, A515-Gr.70, A516, A517-F(T-1), A533B, HY-80, HY-100, Iron (Armco), X42, X52, X60, X65, X70, X100, 430F, 1020, 1080, C1025, 1042, 4140, 4340), or martensitic steels (e.g., AerMet100, D6AC, H-11, Fe-9Ni-4Co-0.20C, 410, 440A, 440C, 17-4PH, 18Ni-250), or nickel-based superalloys (superalloys) (e.g., AF-115, AF-56, Astroloy, CM SX-2, CM SX-3, CM SX-4C, CM SX-4D, CM-SX5, Hastelloy, Haynes 230, Haynes 242, IN100, Inconel 625, Inconel 700, Inconel 706, Inconel 713LC, Inconel 718, Inconel X-750, Inco 4005, MAR-M200, MAR-M246, MA 6000, MA 754, MERL 76, NASA-HR1, PWA 1480, PWA 1480E, Rene 41, Rene N-4, Rene 95, RR 2000, Udimet 720, Udimet 700, Waspaloy), or iron-based superalloys (e.g., A286, Incoloy 802, Incoloy 901, Incoloy 903, Incoloy 907, Incoloy 909, JBK-75, MA 956, Ni-SPAN-C,) or cobalt-based superalloys (e.g., Haynes 188, MP35N, MP159, MP98T, X-45). These alloys are described in more detail in JALee, Hydrogen Embrittlement, NASA / TM-2016-218602, Alabama, USA (2016), Tables 2, 3, 4. In principle, the alloys are suitable for use as metallic materials for manufacturing diaphragms, with the various dimensions of the diaphragm being selected depending on the material properties. However, some alloys are only partially suitable for direct exposure to hydrogen-containing fluid media. Coating the metallic material allows the expert to select the metallic material of the diaphragm according to the appropriate physical properties, such as stiffness, thermal conductivity, coefficient of thermal expansion, or yield strength. The coating protects the metallic material from hydrogen-related corrosion. Hydrogen resistance of the metallic material is an advantage, but not essential.
[0028] As mentioned at the beginning, some of the above-mentioned metallic materials have a coarse-grained polycrystalline structure, which makes them less suitable for use as materials for thin diaphragms with a thickness of less than 500 μm that are in direct contact with hydrogen-containing fluid media. However, coating the diaphragm eliminates this drawback, thus providing a relatively wide range of materials to choose from as metallic materials for the diaphragm.
[0029] Preferably, the diaphragm has a thickness of less than 500 μm, at least in certain areas. This is advantageous in terms of transmitting the pressure of the fluid medium from the first space to the measuring device arranged in the second space with as few losses as possible. Furthermore, a diaphragm with a thickness of less than 500 μm exhibits a lower inertia than a diaphragm with a larger thickness. This is advantageous because when the transducer is accelerated, the inert mass of the diaphragm exerts only a very small force on the measuring device, so that the pressure measurement is not or only slightly affected by the acceleration.
[0030] Particularly preferably, the metallic materials are fine-grained steels with a structure of martensite, bainite, needle ferrite, Widmanstätten ferrite or a mixture of these structures. Generally, these are not considered to be hydrogen resistant, but surprisingly, due to their relatively fine-grained structure, they have a low tendency to hydrogen embrittlement. The fine-grained structure increases the diffusion path, which is why hydrogen cannot diffuse over short distances through these materials. Thus, the metallic materials have a certain resistance to hydrogen. Bainite, needle ferrite and Widmanstätten ferrite are also known as intermediate structures. Intermediate structures include structures between martensite and pearlite. Needle ferrite is intended to mean the material called acicular ferrite in English.
[0031] The structures of martensite, bainite, Widmanstätten ferrite, needle ferrite or mixtures of these structures are characterized by an average grain size of less than 20 μm and are therefore particularly suitable for the production of thin-walled diaphragms with a thickness of less than 500 μm. Due to the small average grain size, the components exhibit isotropic physical properties, which is advantageous when using the diaphragms.
[0032] Particularly preferably, the structure comprises martensite with partially coherent or incoherent precipitates, preferably at the grain boundaries within the material, as described in Metallkunde, E. Hornbogen and H. Warlimont, 4th edition, Springer Verlag 2001. Partially coherent or incoherent precipitates in the sense of this description are described in Werkstoffkunde-Stahl-Vol. 1, Verein Deutscher Eisenhuttenleute (ed.), Springer Verlag 1984, or in Pirlog, Madalina, and PK Pranzas. “CHARACTERIZATION OF COPPER PRECIPITATES IN FE-CU ALLOYS WITH SMALL-ANGLE NEUTRON SCATTERING”.
[0033] Incoherent and partially coherent precipitates act as hydrogen sinks. Hydrogen accumulates in the hydrogen sinks, which prevents the accumulated hydrogen from penetrating further into the material. Coherent precipitates are located within grains, which reduces hydrogen mobility compared to materials containing coherent precipitates, but hydrogen still migrates preferably along grain boundaries within the material.
[0034] The coating is part of the diaphragm. According to the invention, the metallic material of the diaphragm includes a coating. The coating is disposed on the side of the metallic material of the diaphragm that faces the fluid medium.
[0035] According to the invention, the diaphragm is provided with a coating. The coating serves to reduce the permeability of the diaphragm to atomic or molecular components of the fluid medium, in particular molecular and / or atomic hydrogen. The coating is arranged between the metallic material of the diaphragm and the fluid medium, at least in the area that is in contact with the fluid medium during use. The coating comprises an oxide, carbide or nitride. The oxide, carbide or nitride is, for example, aluminum oxide, aluminum carbide, aluminum nitride, chromium oxide, chromium nitride, silicon oxide, silicon carbide, silicon nitride, titanium oxide, titanium carbide, titanium nitride, zirconium oxide or rare earth oxide. The coating prevents direct contact between the metallic material of the diaphragm and the fluid medium. The coating prevents direct adsorption of molecular and / or atomic components from the fluid medium onto the metallic material of the diaphragm. The aforementioned oxides, nitrides and carbides are substantially chemically inert compared to the steels, alloys and metallic materials mentioned at the outset, so that the coating of metallic materials reduces chemical reactions or dissociation of components at the surface of the diaphragm thus coated, further improving the corrosion resistance of the diaphragm compared to an uncoated diaphragm.
[0036] The coating is thinner than the thickness of the metal material. Preferably, the thickness of the coating is at most 10% of the total thickness of the membrane. The typical thickness of the coating is 1 μm to 5 μm. Therefore, the stiffness and yield strength of the membrane are mainly determined by the metal material.
[0037] Generally, the thermal expansion coefficient of metal materials is 5 to 10 in the temperature range of 20°C to 100°C. -6 K -1 ~15·10 6 K -1 The mismatch between the metal material and the coating is compensated to some extent by the epitaxial effect. When the coating is applied using an epitaxial process, the epitaxial effect promotes adhesion of the coating to the metal material.
[0038] The coating also has a coefficient of thermal expansion. Preferably, the coefficient of thermal expansion of the coating does not differ by more than 50% from that of the metallic material. This prevents the coating from peeling and cracking under thermal stress.
[0039] Thermal stress or temperature change occurs when the temperature of at least some area of the diaphragm increases or decreases by more than 10°C compared to the temperature at any previous time for any period of time, which may be up to several days.
[0040] Advantageously, the diaphragm comprises an adhesion promoter layer. The adhesion promoter layer serves to prevent the delamination of the coating from the metallic material. The mechanical stresses occurring during temperature changes are therefore advantageously distributed between the interface between the metallic material and the adhesion promoter layer and the other interface between the adhesion promoter layer and the coating. This reduces local mechanical stresses and prevents the occurrence of cracks under mechanical or thermal stresses. Advantageously, the adhesion promoter layer is a metal with a strong oxygen affinity, for example a refractory metal, aluminum or a rare earth metal. The refractory metal is titanium, vanadium, chromium, zirconium, niobium, hafnium, tantalum, molybdenum or tungsten. The purity of the adhesion promoter layer is at least 75% by weight. A purity of at least 75% by weight means that 75% by weight of the adhesion promoter layer consists of a metal.
[0041] Preferably, the adhesion promoter layer comprises at least 90% by weight of zirconium or tungsten, which are easily applied in the form of a layer.
[0042] In an embodiment according to the invention, the diaphragm comprises a coating made of a non-stoichiometric oxide, a non-stoichiometric nitride, or a non-stoichiometric carbide.
[0043] An oxide, nitride, or carbide is non-stoichiometric when the chemical elements are not present in the respective mixture in an optimal ratio. Usually, for a stoichiometric oxide, nitride, or carbide, the optimal ratio is the most stable compound.
[0044] Stoichiometric carbides are, for example, SiC (silicon carbide), Al4C3 (aluminum carbide), or TiC (titanium carbide).
[0045] The nonstoichiometric carbides are the mixture (1-y)M-yMC x (0 <x<x M,C And 0 <y≦1、ただし、M=Siでx Si,C =1, or M=Al and x Al,C =3 / 4, or M=Ti and x Ti,C = 1). The constant x M,C depends on the element M of the carbide C. x M,C In this way, the stoichiometric ratio of each element M in combination with carbon C is reached. Other elements can also be used for M. The stoichiometric ratios of carbides can be obtained from the technical literature.
[0046] Stoichiometric nitrides are, for example, AlN (aluminum nitride), CrN (chromium nitride), Si3N4 (silicon nitride), TiN (titanium nitride).
[0047] Non-stoichiometric nitrides are mixtures (1-y)M-yMN x (0 <x<x M,N And 0 <y≦1、ただし、M=Alでx Al,N =1, or M=Cr and x Cr,N =1, or M=Si and x Si,N = 4 / 3, or M = Ti and x Ti,N = 1). The constant x M,N depends on the element M of the nitride N. x M,N Thus, the stoichiometric ratio of each element M in combination with nitrogen N is reached. Other elements can also be used for M. The stoichiometric ratios of nitrides can be obtained from the technical literature.
[0048] Stoichiometric oxides are, for example, Al2O3 (aluminum oxide), SiO2 (silicon oxide), TiO2 (titanium oxide), ZrO2 (zirconium oxide), Cr2O3 (chromium oxide), or in the case of rare earth oxides, Sc2O3, Y2O3, La2O3, CeO2, Pr2O3, Nd2O3, Pm2O3, Sm2O3, EuO, Gd2O3, Tb2O3, Dy2O3, Ho2O3, Er2O3, Tm2O3, Yb2O3, Lu2O3.
[0049] The rare earth elements are Sc (scandium), Y (yttrium), La (lanthanum), Ce (cerium), Pr (praseodymium), Nd (neodymium), Pm (promethium), Sm (samarium), Eu (europium), Gd (gadolinium), Tb (terbium), Dy (dysprosium), Ho (holmium), Er (erbium), Tm (thulium), Yb (ytterbium), and Lu (lutetium).
[0050] Nonstoichiometric oxides are mixtures (1-y)M-yMO x (0 <x<x M,O And 0 <y≦1、ただし、M=Alでx Al、O =1.5, or M=Cr and x Cr、O = 1.5, or M = Si and x Si、O =2, or M=Ti and x Ti、O =2, or M=Zr and x Zr、O = 2, or M = rare earth element x 希土類元素、O =1~2). Constant x M,O depends on the element M relative to the oxide O. x M,O In this way, the stoichiometric ratios of each element M in combination with oxygen O are reached. Other elements can also be used for M. Oxide stoichiometric ratios are available for other elements M in the technical literature.
[0051] Coatings made of non-stoichiometric oxides, non-stoichiometric nitrides, or non-stoichiometric carbides are advantageous because the thermal expansion coefficient of the non-stoichiometric oxide, nitride, or carbide can be adjusted. Preferably, the thermal expansion coefficient of the coating does not differ from that of the metallic material by more than 50%. This prevents the coating from peeling and crack formation under thermal stress. In this embodiment, the adhesion promoter layer can be omitted.
[0052] The word "or" with respect to carbides, nitrides, and oxides should not be understood as exclusive "or". Thus, a coating containing carbides may also contain nitrides. So-called carbonitrides are expressly disclosed as being included in both carbide-containing and nitride-containing coatings. Examples include mixtures of titanium carbide and titanium nitride (titanium carbonitride), zirconium carbide and zirconium nitride (zirconium carbonitride), or chromium carbide and chromium nitride (chromium carbonitride). Gold, another substantially chemically inert material, has a Vickers hardness of less than 100 HV10, whereas exemplary oxides, nitrides, and carbides have a Vickers hardness of more than 100 HV. Thus, the mechanical resistance of the coating to metallic materials is improved compared to gold coatings known in the prior art.
[0053] Vickers hardness refers to the Vickers hardness under a test force of 10 kilopounds or 10 kgf (kilogram force), so-called HV10. The Vickers hardness test is described in the standard DIN EN ISO 6507-1:2018~-4:2018.
[0054] Preferably, the coating contains non-stoichiometric aluminum oxide or non-stoichiometric titanium carbide. Aluminum oxide is known in the industry as a chemically inert material. Also, aluminum oxide is relatively inexpensive compared to rare earth elements or zirconium. Titanium carbide is also widely used in the industry, is cost-effective, and is known as a substantially chemically inert material. The Vickers hardness of another substantially chemically inert material, gold, is less than 100 HV10, but the Vickers hardness of aluminum oxide exceeds 1500 HV10. Therefore, when used as a coating for a metallic material, the mechanical resistance is improved compared to a coating made of gold. The Vickers hardness of titanium carbide exceeds 2500 HV10, and when used as a coating for a metallic material, the mechanical resistance is improved compared to a coating made of gold.
[0055] In a preferred embodiment, the diaphragm comprises a coating of non-stoichiometric aluminum oxide (1-y)Al-yAlO x (0 < x < 1.5 and 0 < y ≤ 1). The ability to adjust the thermal expansion coefficient of non-stoichiometric aluminum oxide is an advantage. Preferably, the thermal expansion coefficient of the coating does not differ by more than 50% from the thermal expansion coefficient of the metallic material. This prevents peeling of the coating and formation of cracks under thermal stress. In this embodiment, the adhesion promoter layer can be omitted.
[0056] In one embodiment, the diaphragm comprises a coating of non-stoichiometric carbide (1-y)M-yMC x (0 < x < x M,C and 0 < y ≤ 1) having an inclination within the coating, or a coating of non-stoichiometric nitride (1-y)M-yMN x (0 < x < x M,N and 0 < y ≤ 1) having an inclination within the coating, or a coating of non-stoichiometric oxide (1-y)M-yMO x (0 < x < x M,O and 0 < y ≤ 1) having an inclination within the coating. As already explained, the constants x M,C , x M,N , xM,O depends on the element M of carbide C, nitride N, oxide O, and corresponds to the stoichiometric ratio of the respective element M in relation to carbon C, nitrogen N, or oxygen O. In the coating, the proportion y increases gradually as the distance from the metallic material increases. Alternatively, in the coating, the proportion x increases gradually as the distance from the metallic material increases. However, in the coating, the proportions x and y may also increase gradually as the distance from the metallic material increases. This has the advantage that by appropriately selecting the ratios x and y, it is possible to specifically match the coating to the metallic material at the interface between the coating and the metallic material. This matching can minimize stresses at the interface and / or result in an adjusted thermal expansion coefficient. Creating a gradient in the coating is advantageous because the physical properties in the coating also change gradually. This prevents stresses or the formation of cracks from occurring in the coating. At the surfaces in contact with the fluid medium, the properties may be matched to the fluid medium. Thus, the coating may be exposed to other substances in the fluid medium besides hydrogen, and by appropriate selection of the ratios x and y, it may be possible to increase the resistance to other substances, such as alkaline or acidic gases or liquids.
[0057] Advantageously, the non-stoichiometric oxide (1-y)M-yMO with a gradient in the coating at the interface between the metallic material and the coating. x , non-stoichiometric nitride (1-y)M-yMN x , or non-stoichiometric carbides (1-y)M-yMC x The thermal expansion coefficient of the coating differs from that of the metallic material by no more than 50%.
[0058] Particularly preferred is non-stoichiometric aluminum oxide (1-y)Al-yAlO xThe coating in (0 < x < 1.5 and 0 < y ≤ 1) includes an inclination within the coating. As the distance from the metallic material increases within the coating, the ratio y gradually increases. Alternatively, as the distance from the metallic material increases within the coating, the ratio x gradually increases. However, as the distance from the metallic material increases within the coating, both the ratio x and the ratio y can gradually increase. The coefficient of thermal expansion of the coating at the interface between the metallic material and the coating does not differ from that of the metallic material by more than 50%.
[0059] In both cases where there is and is not an inclination within the coating, the non-stoichiometric oxide (1 - y)M - yMO x (0 < x < x M,O and 0 < y ≤ 1) or the non-stoichiometric nitride (1 - y)M - yMN x (0 < x < x M,N and 0 < y ≤ 1) or the non-stoichiometric carbide (1 - y)M - yMC x (0 < x < x M,CIn one embodiment of a diaphragm having a coating made from 0 < x ≦ 1 and 0 < y ≦ 1), the diaphragm comprises at least one other coating. The other coating is disposed on the side opposite to the metallic material of the coating. The other coating comprises a stoichiometric oxide, a stoichiometric carbide, or a stoichiometric nitride. Advantageously, the coefficient of thermal expansion of the coating is intermediate between the coefficient of thermal expansion of the metallic material and the coefficient of thermal expansion of the other coating. In this case, the coating functions partly as an adhesion promoter layer but still serves to reduce the permeability of the diaphragm to molecular hydrogen and / or atomic hydrogen. The other coating further reduces the permeability of the diaphragm to molecular hydrogen and / or atomic hydrogen. The chemical resistance of stoichiometric oxides, stoichiometric nitrides, and stoichiometric carbides is higher than that of non-stoichiometric oxides, non-stoichiometric nitrides, and non-stoichiometric carbides and is particularly chemically inert. The gradient within the coating is advantageous because the physical properties within the coating change gradually. This prevents the formation of stress or cracks in the coating. At the surface in contact with the other coating, the ratio of x to y can be selected to minimize strain even under thermal stress. The other coating has a particularly chemically inert stoichiometric composition.
[0060] Also, an adhesion promoter layer as described above can be provided between the coating and the metallic material.
[0061] In a special variant of a diaphragm having a coating of a non-stoichiometric oxide, nitride, or carbide with a gradient, at a certain distance from the interface between the coating and the metallic material, the coating transitions to a stoichiometric oxide, nitride, or carbide.
[0062] In another special variant of a diaphragm having a coating of a non-stoichiometric oxide, nitride, or carbide with a gradient, at a certain distance from the interface between the coating and the metallic material, the coating transitions to the respective stoichiometric oxide, nitride, or carbide.
[0063] In a further embodiment, a further stoichiometric coating is applied onto the non-stoichiometric coating, the thermal expansion coefficient of the coating being advantageously between that of the metallic material and that of the further coating.
[0064] In a further embodiment, the diaphragm comprises at least one other coating, a first other coating being arranged on the side of the coating facing the fluid medium, and each additional other coating being arranged on the side of the previous other coating facing the fluid medium. The at least one other coating comprises a non-stoichiometric carbide, nitride or oxide, as in the previous coating. However, the chemical composition of the other coating is different from the chemical composition of the coating. For example, if the coating is titanium oxide, titanium nitride or titanium carbide, the other coating can be aluminum nitride, aluminum oxide or aluminum carbide. Thus, the adjacent additional coatings also have different chemical compositions. This has the advantage that the other coating in contact with the fluid medium can be adapted to the fluid medium and provide resistance to other substances contained in the fluid medium, for example. The coating can also be tailored to the metallic material.
[0065] Non-stoichiometric aluminum oxide (1-y)Al-yAlO with or without gradient in the coating xIn a particular embodiment of a diaphragm having a coating of (0 < x < 1.5 and 0 < y ≤ 1), the diaphragm comprises at least one other coating. The other coating is disposed on the side opposite to the metallic material of the coating. The additional coating comprises stoichiometric aluminum oxide Al2O3. The coefficient of thermal expansion of the coating is between the coefficient of thermal expansion of the metallic material and the coefficient of thermal expansion of the other coating. In this case, the coating functions partly as an adhesion promoter layer but still serves to reduce the permeability of the diaphragm to molecular hydrogen and / or atomic hydrogen. The other coating further reduces the permeability of the diaphragm to molecular hydrogen and / or atomic hydrogen.
[0066] Non-stoichiometric aluminum oxide (1 - y)Al - yAlO with an inclination x In a special variant of a diaphragm having a coating of (0 < x < 1.5 and 0 < y ≤ 1), at a certain distance from the interface between the coating and the metallic material, the coating transitions to stoichiometric Al2O3.
[0067] In one embodiment, the diaphragm comprises an internal coating for reducing the permeability to molecular hydrogen and / or atomic hydrogen. The internal coating is disposed on the side opposite to the fluid medium in the second space of the metallic material of the diaphragm. In this embodiment, the internal coating comprises non-stoichiometric oxides, nitrides, or carbides. The same oxides, carbides, or nitrides as already described with respect to the coating are advantageous for this purpose. This means that the deposition can be carried out in the same way as in the case of the coating. The internal coating is particularly advantageous when the second space separated from the first space containing the fluid medium by the diaphragm is a closed volume. The closed volume can be, for example, inside the housing of a transducer. The additional internal coating further reduces the diffusion of molecular hydrogen or atomic hydrogen through the diaphragm, and thus reduces the accumulation of hydrogen in the second space. This avoids the above-mentioned adverse effects, such as the diaphragm expanding when the pressure transmission medium is disposed in the closed volume.
[0068] In one embodiment, the inner coating may not have the same chemical composition as the coating. A different coating may be selected because the coating contacts the fluid medium and the inner coating does not. For example, the inner coating or coatings may be electrically insulating. The coating may also be resistant to other substances that are not required for the inner coating.
[0069] As with the coating, an adhesion promoter may optionally be disposed between the inner coating and the metallic material of the diaphragm.
[0070] The invention also encompasses a transducer for determining the pressure of a fluid medium. The transducer comprises a pressure-exposed end facing the fluid medium. The transducer comprises a housing. The transducer comprises a measurement device. The measurement device is disposed inside the housing. The transducer comprises a diaphragm according to any of the above embodiments. The second space corresponds to a volume inside the housing.
[0071] The measuring device for determining the pressure of the fluid medium is, for example, at least one piezoelectric crystal which generates a piezoelectric charge as a function of the pressure acting on the diaphragm. In one embodiment, the piezoelectric crystal is arranged in a prestressing sleeve which prestresses the piezoelectric crystal. Thus, both negative and positive pressure changes can be detected. Alternatively, the measuring device may also include a capacitance measuring element which detects mechanical deformations in the form of a change in capacitance.
[0072] Alternatively, the measurement device may include a piezoresistive measuring element or a strain gauge (also called a strain gauge) that detects mechanical deformation in the form of a change in electrical resistance. Those skilled in the art will recognize other measurement devices that may be used in a transducer to determine the pressure of a fluid medium.
[0073] The diaphragm is disposed at the pressure-exposed end of the housing and hermetically separates the measuring device from the fluid medium. The housing and the diaphragm are connected by a material bond. The material bond may be, for example, a welded or soldered connection. An adhesive material bond is also conceivable.
[0074] The diaphragm comprises a first region that is in contact with the fluid medium during use. The diaphragm comprises a second region that is not in contact with the fluid medium during use. The inter-material bond is in the second region. Inter-material bonds made as soldered or welded connections usually develop more cracks or pores. Even in the case of adhesive inter-material bonds, the adhesive may be damaged by the liquid medium. Therefore, it is preferred that the inter-material bond is located in the second region that is not exposed to the fluid medium.
[0075] In the case of a diaphragm including a coating, the coating is disposed over at least the first region, but may also extend at least partially over the second region.
[0076] A second region is not in contact with a fluid medium within the meaning of this specification if the concentration of the corrosive component of the fluid medium in the second region is at most 1% of the concentration of the corrosive component in the first region.
[0077] The first and second regions may be separated from each other, for example, by a sealing element. Depending on the application in which the transducer is used in terms of temperature and pressure ranges, metal gaskets may be used, such as copper gaskets, gaskets made of 1.4404 or 1.4301 steel, alloy sealing elements, or metal-coated alloy gaskets. Plastic seals are also known for certain temperature and pressure ranges, for example seals made of polytetrafluoroethylene, fluoroelastomers, or nitrile compounds. Other materials can also be used for the sealing elements.
[0078] Preferably, the transducer is used to determine the pressure of a fluid medium when the fluid medium is corrosive and conventional transducers cannot be used.
[0079] Particularly preferably, the transducer is used to determine the pressure of a fluid medium containing at least a certain amount of molecular and / or atomic hydrogen. Hydrogen is known to cause so-called hydrogen embrittlement in many metallic materials, which, when subjected to thermal and / or mechanical stresses, leads to hydrogen embrittlement and a reduction in yield strength. The above-mentioned transducer significantly reduces these disadvantages.
[0080] All of the described transducer embodiments are possible with a pressure transmission medium disposed in the second space, however, all of the described embodiments can also be implemented without a pressure transmission medium disposed in the second space.
[0081] The invention also encompasses a transducer for determining a temperature of a fluid medium. The transducer comprises a pressure exposed end facing the fluid medium. The transducer comprises a housing. The transducer comprises a measurement device for determining the temperature of the fluid medium. The measurement device is disposed within the housing. The transducer comprises a diaphragm according to any of the above embodiments.
[0082] The invention will now be explained in more detail and by way of example with reference to the drawings, in which: [Brief description of the drawings]
[0083] [Figure 1] 1 shows a schematic cross-sectional view of an embodiment of a transducer with an embodiment of a diaphragm according to the present invention, with optional coatings shown in dashed lines. [Diagram 2] 1 shows a schematic cross-sectional view of one embodiment of a diaphragm. [Diagram 3] 1 shows a schematic cross-sectional view of a further embodiment of a diaphragm. [Figure 4]1 shows a schematic cross-sectional view of a further embodiment of a diaphragm. [Diagram 5] 4 is a schematic cross-sectional view of a portion of a transducer with a diaphragm according to FIG. 3 and arranged in a wall; [Figure 6] 3 shows a schematic cross-sectional view of a part of a transducer with a diaphragm according to FIG. 2 and arranged in a wall; [Figure 7] 1 shows a schematic cross-sectional view of a further embodiment of a diaphragm. [Figure 8] 1 shows a schematic cross-sectional view of a further embodiment of a diaphragm. [Figure 9] 1 shows a schematic cross-sectional view of a further embodiment of a diaphragm. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0084] FIG. 1 shows a schematic cross-sectional view of an embodiment of a transducer 1 comprising an embodiment of a diaphragm 2 according to the present invention, with an optional coating 4 shown in dashed lines.
[0085] In the illustration of Figure 1, which is not drawn to scale, an optional coating 4 of metallic material 3 is shown in dashed lines. Figures 2 to 6 show the following coatings of diaphragm 2 which differ from the illustration shown in Figure 1:
[0086] In further embodiments of Figures 2-9, reference numbers are used consistently for like or equivalent elements.
[0087] Figures 2 to 4 show further embodiments of the diaphragm 2. The thickness of the diaphragm 2 and the thickness of the coating 4 are not drawn to scale for clarity.
[0088] Figures 5 to 6 show a further embodiment of a transducer 1 with a diaphragm 2. The thickness of the diaphragm 2 and the thickness of the coating 4 are not drawn to scale for clarity.
[0089] The diaphragm 2 of Figures 1 to 6 comprises a metallic material 3 and hermetically separates a first space 14 from a second space 15. At least one physical variable can be determined for a fluid medium 13 present in the first space 14. The physical variable is for example pressure and / or temperature.
[0090] The surface 6 of the diaphragm 2 faces the fluid medium 13. The diaphragm 2 has a first region 9 that contacts the fluid medium 13 when the diaphragm 2 is in use. The diaphragm 2 has a second region 10 that does not contact the fluid medium 13 in use, as shown in Figures 1 to 6.
[0091] Advantageously, the diaphragm 2 comprises a thin-walled region 21. The thin-walled region 21 preferably has a thickness of less than 500 μm in order to transmit the pressure of the fluid medium 13 from the first space 14 to the second space 15 with as few losses as possible.
[0092] In the embodiment shown in Figures 1-6, the diaphragm 2 is provided with a coating 4 for reducing the permeability to molecular or atomic hydrogen, the coating 4 being disposed between the metallic material 3 of the diaphragm 2 and the fluid medium 13, at least in the areas that will come into contact with the fluid medium 13 during use. The dashed and dotted lines representing the coating in Figure 1 indicate that the coating is optional.
[0093] In the embodiment shown in FIGS. 3 and 5, the diaphragm 2 is provided with an adhesion promoter layer 5 to prevent peeling of the coating 4 from the metal material 3 of the diaphragm 2 .
[0094] In the embodiment according to FIG. 4, the diaphragm 2 comprises a further coating 4 ′ arranged on the side of the coating 4 opposite the metallic material 3 .
[0095] In the embodiment according to Fig. 9, the diaphragm 2 comprises at least one further coating 4', 4'', 4''', ... arranged on the opposite side of the coating 4 to the metallic material 3. The further coating 4', 4'', 4''', ... comprises a non-stoichiometric carbide, nitride or oxide similar to the coating 4 described above.
[0096] In the embodiment according to Fig. 7, the diaphragm 2 comprises, for example, in addition to the coating 4 on the side of the metallic material 3 facing the fluid medium 13, an internal coating 22. The internal coating 22 is arranged in the second space 15 on the side of the metallic material 3 of the diaphragm 2 facing away from the fluid medium 13. Although not shown in the figures, an internal coating 22 may also be provided in other embodiments.
[0097] In the embodiment according to figure 8, the diaphragm 2 comprises a coating 4 and an adhesion promoter layer 5 on the side of the diaphragm 2 facing the fluid medium 13 of the metallic material 3. This embodiment of the diaphragm 2 further comprises an adhesion promoter layer 5 deposited on the side of the metallic material 3 opposite the fluid medium 13, which adhesion promoter layer 5 bonds the inner coating 22 to the metallic material 3.
[0098] Figures 1 and 5-6 each show an embodiment of a diaphragm 2 implemented in a transducer 1 for determining the pressure of a fluid medium 13. The transducer 1 comprises a pressure-exposed end 11 facing the fluid medium 13. The transducer 1 comprises a housing 7. A measuring device 16 is arranged in the housing 7. Each embodiment of the transducer 1 according to Figure 1, 5 or 6 represents a diaphragm 2 according to the invention.
[0099] The diaphragm 2 is disposed at the pressure-exposed end 11 of the transducer 1 and hermetically separates the measuring device 16 from the fluid medium 13. The housing 7 and the diaphragm 2 are joined to one another by an inter-material bond 8. The diaphragm 2 comprises a first region 9 that is in contact with the fluid medium 13 when the diaphragm 2 is in use. The diaphragm 2 comprises a second region 10 that is not in contact with the fluid medium 13 when in use. The first region 9 and the second region 10 are separated from one another by a sealing element 12 when the transducer 1 is in use. In each of the illustrated embodiments, the inter-material bond 8 is disposed in the second region 10.
[0100] However, it is also conceivable for the bond between the materials 8 to be located in the areas 9, 10 which are in contact with the fluid medium 13. In this case, it is advantageous for the bond between the materials 8 to be completely covered by the coating 4.
[0101] Figures 5 and 6 show a transducer 1 used to determine the pressure of a fluid medium 13 inserted in a wall 17. For example, the wall 17 may be the wall 17 of a tank holding the fluid medium 13, a compressor, a heat pump, a refrigerator, a line transporting the fluid medium 13, the combustion chamber of an internal combustion engine, or a gas turbine.
[0102] Of course, the embodiments of the diaphragm 2 or transducer 1 disclosed herein may be combined with each other. Furthermore, embodiments including combinations of features of the embodiments described herein are also expressly encompassed herein. [Explanation of symbols]
[0103] 1 Transducer 2 Diaphragm 3 Metal materials 4. Coating 4' Coating 5 Adhesion promoter layer 6 surface 7. Housing 8. Bonding of Materials 9. First Area 10. The Second Region 11 Pressure Exposed Ends 12 Sealing elements 13 Fluid medium 14 The First Space 15 The Second Space 16 Measuring Equipment 17 Wall 19 Interface 21 Thin wall region 22 Internal Coating
Claims
1. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15), The diaphragm (2) includes a metal material (3), the diaphragm (2) is provided with a coating (4) that reduces the permeability to molecular and / or atomic hydrogen, The coating (4) is disposed between the metallic material (3) of the diaphragm (2) and the fluid medium (13), at least in the area that comes into contact with the fluid medium (13) during use, The coating (4) comprises at least one non-stoichiometric oxide, carbide, or nitride, such as aluminum oxide, aluminum carbide, aluminum nitride, chromium oxide, chromium nitride, silicon oxide, silicon carbide, silicon nitride, titanium oxide, titanium carbide, titanium nitride, zirconium oxide, or rare earth oxide.
2. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to claim 1, comprising: The coating (4) is a mixture of non-stoichiometric carbides (1-y)M-yMC x (0 < x < x M,C And 0<y≦1, where M=Si and x Si,C = 1, or M = Al and x Al,C = 3 / 4, or M = Ti and x Ti,C = 1), preferably non-stoichiometric titanium carbide (1-y) Ti-y TiC x (0<x<1 and 0<y≦1), or The coating (4) is a mixture of non-stoichiometric nitrides (1-y)M-yMN x (0 < x < x M,N And 0<y≦1, where M=Al and x Al,N = 1, or M = Cr and x Cr,N = 1, or M = Si and x Si,N = 4 / 3, or M = Ti and x Ti,N = 1) or The coating (4) is a non-stoichiometric mixture of oxides (1-y)M-yMO x (0 < x < x M,O And 0<y≦1, where M=Al and x Al、O = 1.5, or M = Cr and x Cr、O = 1.5, or M = Si and x Si、O = 2, or M = Ti and x Ti、O = 2, or M = Zr and x Zr、O = 2, or M = rare earth element and x 希土類元素、O = 1 to 2), preferably non-stoichiometric aluminum oxide (1-y)Al-yAlO x (0<x≦1.5 and 0≦y≦1).
3. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to claim 1 or 2, comprising: The coating (4) is a non-stoichiometric mixture (1-y)M-yMO having a gradient within the coating (4). x or (1-y)M-yMN x or (1-y)M-yMC x in which within said coating (3), the proportion y gradually increases with increasing distance from said metallic material (3), or The coating (4) is a non-stoichiometric mixture (1-y)M-yMO having a gradient within the coating (4). x or (1-y)M-yMN x or (1-y)M-yMC x in which within said coating (4) the proportion x gradually increases with increasing distance from said metallic material (3), or The coating (4) is a non-stoichiometric mixture (1-y)M-yMO having a gradient within the coating (4). x or (1-y)M-yMN x or (1-y)M-yMC xwherein within said coating (4), the proportions x and y gradually increase with increasing distance from said metallic material (3).
4. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 3, comprising: The coating (4) is a non-stoichiometric mixture (1-y)M-yMO having a gradient within the coating (4). x or (1-y)M-yMN x or (1-y)M-yMC x Including, A diaphragm, characterized in that the coating (4) gradually transitions to a stoichiometric mixture of carbides, nitrides, or oxides at a location away from an interface (19) between the coating (4) and the metallic material (3).
5. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 4, comprising: the coating (4) is thinner than the thickness of the metallic material (3), or A diaphragm, characterized in that the thickness of said coating (4) does not exceed 10% of the thickness of said diaphragm (2).
6. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15), comprising: The coating (4) has a thermal expansion coefficient, The metal material (3) has a thermal expansion coefficient, A diaphragm, characterized in that at the interface (19) between the metallic material (3) and the coating (4), the thermal expansion coefficient of the coating (4) does not differ from the thermal expansion coefficient of the metallic material (3) by more than 50%.
7. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 6, comprising: said diaphragm (2) being provided with at least one other coating (4', 4'', 4''', ...), said other coatings (4', 4'', 4''', ...) are arranged on the opposite side of said coating (4) to said metallic material (3); A diaphragm, characterized in that said other coatings (4', 4'', 4''', . . . ) comprise stoichiometric oxides, carbides or nitrides.
8. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 7, comprising: The coating (4) has a thermal expansion coefficient, said other coatings (4', 4'', 4''', ...) having a thermal expansion coefficient, The metal material (3) has a thermal expansion coefficient, A diaphragm, characterized in that the thermal expansion coefficient of the coating (4) has a value between the thermal expansion coefficient of the metal material (3) and the thermal expansion coefficient of the other coatings (4', 4'', 4''', ...).
9. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15), comprising: the diaphragm (2) is provided with an adhesion promoter layer (5) that prevents peeling of the coating (4) from the metal material (3) of the diaphragm (2); the adhesion promoter layer is disposed between the metal material (3) of the diaphragm (2) and the coating (4); The adhesion promoter layer (5) comprises aluminum, a rare earth metal or a refractory metal, the refractory metal being, for example, titanium, vanadium, chromium, zirconium, niobium, hafnium, tantalum, molybdenum or tungsten, preferably zirconium or tungsten.
10. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 9, comprising: the adhesion promoter layer has a purity of at least 75% by weight, or A diaphragm (2) characterized in that the adhesion promoter layer comprises at least 90% by weight of zirconium or tungsten.
11. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 10, comprising: The diaphragm (2) comprises an internal coating (22) for reducing the permeability to molecular hydrogen and / or atomic hydrogen, the internal coating (22) being disposed in the second space (15) on a side of the metallic material (3) of the diaphragm (2) opposite the fluid medium (13).
12. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 11, comprising: The inner coating (22) is a non-stoichiometric mixture of carbides (1-y)M-yMC x (0 < x < x M,C And 0<y≦1, where M=Si and x Si,C = 1, or M = Al and x Al,C = 3 / 4, or M = Ti and x Ti,C = 1), preferably non-stoichiometric titanium carbide (1-y) Ti-y TiC x(0<x<1 and 0<y≦1), or The coating (4) is a mixture of non-stoichiometric nitrides (1-y)M-yMN x (0 < x < x M,N And 0<y≦1, where M=Al and x Al,N = 1, or M = Cr and x Cr,N = 1, or M = Si and x Si,N = 4 / 3, or M = Ti and x Ti,N = 1) or The coating (4) is a non-stoichiometric mixture of oxides (1-y)M-yMO x (0 < x < x M,O And 0<y≦1, where M=Al and x Al、O = 1.5, or M = Cr and x Cr、O = 1.5, or M = Si and x Si、O = 2, or M = Ti and x Ti、O = 2, or M = Zr and x Zr、O = 2, or M = rare earth element and x 希土類元素、O = 1 to 2), preferably non-stoichiometric aluminum oxide (1-y)Al-yAlO x (0<x≦1.5 and 0≦y≦1).
13. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15) according to any one of claims 1 to 12, comprising: The diaphragm (2), characterized in that the diaphragm (4) has at least partially a thickness of less than 500 μm.
14. A diaphragm (2) for tightly separating a first space (14) containing a hydrogen-containing fluid medium (13) from a second space (15), comprising: The diaphragm (2) is characterized in that the metallic material (3) is a fine-grained steel having a structure of martensite, bainite, needle ferrite, Widmanstätten ferrite or a mixture of these structures, particularly preferably martensite with partially coherent or incoherent precipitates.
15. A transducer (1) for measuring the pressure of a hydrogen-containing fluid medium (13), comprising: The transducer (1) comprises a pressure exposed end (11) facing the fluid medium (13); The transducer (1) comprises a housing (7), The transducer (1) comprises a measuring device (16), A transducer (1), characterized in that it comprises a diaphragm (2) as claimed in any one of claims 1 to 14.
Citation Information
Patent Citations
Device with piezoelectric element and manufacturing method thereof
JP2002084011A
Strain detector and its manufacturing method
JP2006038540A
Pressure sensor and method of manufacturing the same
JP2011002393A
Semiconductor pressure sensor
JP2017083187A
Cylinder pressure transducer and related method
US20050109114A1