Semiconductor Device

The semiconductor device addresses warping and cracking issues by using a control layer with a lower expansion coefficient to mitigate thermal stress, ensuring stable operation and reliable mounting.

JP7551554B2Active Publication Date: 2024-09-17KK TOSHIBA +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021057051
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-30
Publication Date
2024-09-17
Estimated Expiration
2041-03-30

AI Technical Summary

Technical Problem

Semiconductor devices experience warping and cracking due to the mismatch in thermal expansion coefficients between the thick metal drain electrode and the thin semiconductor element region, leading to manufacturing and mounting issues.

Method used

A semiconductor device design that includes a first and second transistor with a common drain electrode composed of multiple metal layers, where the thickest metal layer is sandwiched between a semiconductor layer and a control layer with a lower linear expansion coefficient, reducing stress and warping.

Benefits of technology

The design effectively suppresses warping and cracking by mitigating thermal stress, ensuring stable operation and reliable mounting on wiring boards while maintaining low resistance during ON operations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007551554000008
    Figure 0007551554000008
  • Figure 0007551554000007
    Figure 0007551554000007
  • Figure 0007551554000009
    Figure 0007551554000009
Patent Text Reader

Abstract

To provide a semiconductor device in which the warpage of a semiconductor element and the occurrence of breakdown can be suppressed.SOLUTION: In an embodiment, a semiconductor device includes a first transistor, a second transistor, a third electrode, and a control layer. The first transistor includes a first region of a semiconductor layer with a first surface and a second surface, a first electrode, and a first gate electrode. The first electrode is electrically connected to the second surface of the first region. The first gate electrode is provided in the first region. The second transistor includes a second region of the semiconductor layer provided adjacent to the first region, a second gate electrode, and a second electrode. The second gate electrode is provided in the second region. The second electrode is electrically connected to the second surface of the second region. The third electrode is provided on the first surface side and electrically connected to the first transistor and the second transistor. The control layer is provided so that the third electrode comes between the control layer and the first surface, and has a linear expansion coefficient smaller than that of the third electrode.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD An embodiment of the present invention relates to a semiconductor device. [Background technology]

[0002] There is a technology for forming two transistors, for example, metal oxide semiconductor field effect transistors (MOSFETs), on one semiconductor chip. The two MOSFETs have a common drain electrode.

[0003] The metal layer of the common drain electrode is formed thick to reduce resistance during ON operation. On the other hand, the semiconductor element region of the semiconductor device tends to be formed thin to reduce resistance during ON operation. Therefore, during the manufacturing process of the semiconductor device or when the semiconductor device is mounted on a wiring board, the semiconductor element region may warp, which may cause cracks. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2013-69852 A Summary of the Invention [Problem to be solved by the invention]

[0005] An object of the present invention is to provide a semiconductor device capable of suppressing warpage and cracking of a semiconductor element. [Means for solving the problem]

[0006] The semiconductor device of the embodiment has a first transistor, a second transistor, a third electrode, and a control layer. The first transistor has a first region of a semiconductor layer, a first electrode, and a first gate electrode. The first region of the semiconductor layer has a first surface and a second surface facing the first surface in a first direction. The first electrode is electrically connected to the second surface of the first region. The first gate electrode is provided in the first region. The second transistor has a second region of the semiconductor layer, a second gate electrode, and a second electrode. The second region of the semiconductor layer is provided adjacent to the first region in a second direction intersecting with the first direction, and has a first surface and a second surface. The second gate electrode is provided in the second region. The second electrode is electrically connected to the second surface of the second region and is provided spaced apart from the first electrode. The third electrode is provided on the first surface side and is electrically connected to the first transistor and the second transistor. The third electrode has a first metal layer, a second metal layer provided on the second surface side of the first metal layer, a third metal layer provided between the first metal layer and the second metal layer, and a fourth metal layer provided between the first metal layer and the control layer. The control layer is provided such that the third electrode is located between the control layer and the first surface. In the third electrode, the first metal layer has the greatest thickness in the first direction, and the control layer has a smaller linear expansion coefficient than the first metal layer. [Brief description of the drawings]

[0007] [Figure 1] 1 is a cross-sectional view of a semiconductor device 100 according to a first embodiment. [Diagram 2] 13 is a graph showing the linear expansion coefficient of materials used for a drain electrode and a control layer. [Diagram 3] 1 is a plan view of a semiconductor device 100 according to a first embodiment. [Figure 4] 1 is an equivalent circuit diagram of a semiconductor device 100 according to a first embodiment. [Diagram 5] 2A and 2B are diagrams showing a method for manufacturing the semiconductor device 100 according to the first embodiment. [Figure 6] 2A and 2B are diagrams showing a method for manufacturing the semiconductor device 100 according to the first embodiment. [Figure 7] 2A and 2B are diagrams showing a method for manufacturing the semiconductor device 100 according to the first embodiment. [Figure 8] 2A to 2C are views showing a method for manufacturing the semiconductor device 100 according to the first embodiment. [Figure 9]1 is a schematic diagram showing a semiconductor device 100 according to a first embodiment mounted on a wiring board. [Figure 10] FIG. 1 is a cross-sectional view of a semiconductor device 300 according to a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In this description, common parts are denoted by common reference numerals throughout the drawings. Furthermore, the dimensional ratios of the drawings are not limited to the ratios shown in the drawings. Note that the present embodiment does not limit the present invention.

[0009] [First embodiment] (Structure of the semiconductor device 100) A detailed structure of the semiconductor device 100 according to the first embodiment will be described with reference to Figures 1, 2, and 3. Figure 1 is a cross-sectional view of the semiconductor device 100 according to the first embodiment. Figure 2 shows the linear expansion coefficients of materials used in the drain electrode 40 and the control layer 50. Figure 3 is a plan view of the semiconductor device 100 according to the first embodiment.

[0010] In the following description, n + , n, n - And, p + , p, p - The notation indicates the relative level of impurity concentration in each conductivity type. + has a relatively higher n-type impurity concentration than n, - indicates that the n-type impurity concentration is relatively lower than that of n. + has a relatively higher p-type impurity concentration than p, - indicates that the p-type impurity concentration is relatively lower than that of p. + type, n - The types are simply n-type and p-type. + type, p - The type is sometimes simply referred to as p-type.

[0011] The semiconductor device 100 according to the first embodiment shown in Fig. 1 is a switching device that controls bidirectional current flow. The semiconductor device 100 according to the first embodiment is used, for example, in a battery protection circuit. In the semiconductor device 100 according to the first embodiment, two trench-gate MOSFETs are connected so that their drain electrodes are common.

[0012] The semiconductor device 100 of the first embodiment has a semiconductor layer 10, a first source electrode (first electrode) 21, a second source electrode (second electrode) 22, a first gate electrode 31, a second gate electrode 32, a drain electrode (third electrode) 40, a control layer 50, a first source electrode pad 81, a second source electrode pad 82, a first gate electrode pad 91, and a second gate electrode pad 92.

[0013] The semiconductor layer 10 has a first surface P1, a second surface P2, a first region 10a, and a second region 10b. In Fig. 1, the first region 10a is indicated by a chain line, and the second region 10b is indicated by a dashed line.

[0014] The direction from the first surface P1 to the second surface P2 is the Z direction (first direction). The direction perpendicular to the Z direction is the X direction (second direction), and the direction perpendicular to the X and Z directions is the Y direction (third direction). The semiconductor device 100 shown in Figures 1 and 2 shows a cross-sectional view in the XZ plane. For the sake of explanation, the direction from the first surface P1 to the second surface P2 is referred to as "up" and the opposite direction is referred to as "down".

[0015] The first region 10a is a region provided in the semiconductor layer 10, and has a first surface P1 and a second surface P2. The second region 10b has the first surface P1 and the second surface P2, and is provided adjacent to the first region 10a in the X direction.

[0016] The first region 10a is + A drain region 11 of n - a p-type drift region 12, a p-type first base region 13a, and + and a first source region 14a of the n-type.

[0017] n + The n-type drain region 11 is provided on the first face P1 side of the semiconductor layer 10. - The drift region 12 of the type has a n + The drain region 11 of the semiconductor substrate 10 is provided on the drain region 11 of the semiconductor substrate 10 .

[0018] A plurality of p-type first base regions 13a are provided in the first region 10a. The plurality of p-type first base regions 13a are adjacent to each other in the X direction via a first insulating film 61 described later. - It is provided above the drift region 12 of the mold.

[0019] n + The n-type first source region 14a is provided on the p-type first base region 13a in the Z direction. + The first source region 14a is provided on the second face P2 side of the first region 10a.

[0020] The second region 10b is n + A drain region 11 of n - a p-type drift region 12, a p-type second base region 13b, and + and a second source region 14b of the same type.

[0021] A plurality of p-type second base regions 13b are provided in the second region 10b. The plurality of p-type second base regions 13b are spaced apart from each other in the X direction and are arranged in the n-type region of the second region 10b. - It is provided above the drift region 12 of the mold.

[0022] n + The n-type second source region 14b is provided on the p-type second base region 13b in the Z direction. + The first source region 14a is provided on the second face P2 side of the second region 10b.

[0023] The semiconductor layer 10 includes, for example, silicon (Si) or silicon carbide (SiC) as a semiconductor material. When silicon is used as the semiconductor material, the thickness of the semiconductor layer 10 in the Z direction is 100 μm or less.

[0024] The first source electrode 21 is + The first source electrode 21 is provided on the first source region 14a of the n-type. + The first source region 14a is electrically connected to the first source region 14a.

[0025] A plurality of first gate electrodes 31 are provided in the first region 10a. The first gate electrodes 31 are provided adjacent to the p-type first base region 13a in the X direction. A first insulating film 61 is provided between the first gate electrodes 31 and the semiconductor layer 10.

[0026] The second source electrode 22 is + The second source electrode 22 is provided on the n-type second source region 14b. + The source region 14b is electrically connected to the second source region 14b.

[0027] A plurality of second gate electrodes 32 are provided in the second region 10b. The second gate electrodes 32 are provided adjacent to the p-type second base region 13b in the X direction. A second insulating film 62 is provided between the second gate electrodes 32 and the semiconductor layer 10.

[0028] A part of the first source electrode 21, a part of the second source electrode 22, and a part of the semiconductor layer 10 are covered with an insulating film 60.

[0029] 2, the drain electrode 40 includes a first metal layer 41, a second metal layer 42, a third metal layer 43, and a fourth metal layer 44. The drain electrode 40 includes an n + A drain region 11 is provided under the n + The drain region 11 of the semiconductor substrate 10 is electrically connected to the drain region 11 of the semiconductor substrate 10 .

[0030] The first metal layer 41 is a main path for a current that flows when the semiconductor device 100 is in an on-state, and is the thickest in the Z direction among the metal layers of the drain electrode 40. The thickness of the first metal layer 41 in the Z direction is, for example, 10 μm or more. The first metal layer 41 is, for example, silver (Ag) or copper (Cu). The second metal layer 42 is, for example, n + The second metal layer 42 is provided under the drain region 11 of the semiconductor layer 10. The second metal layer 42 is made of a metal that improves adhesion to the semiconductor layer 10, such as titanium (Ti). The thickness of the second metal layer 42 in the Z direction is, for example, 1 μm or less. The third metal layer 43 is provided between the first metal layer 41 and the second metal layer 42. The third metal layer 43 is a metal that is formed on the semiconductor layer (for example, n + The fourth metal layer 44 is a barrier metal layer that prevents oxidation of the first metal layer 41 (the drain region 11) and diffusion of metal into the semiconductor layer, and is made of, for example, nickel (Ni). The thickness of the third metal layer 43 in the Z direction is, for example, 1 μm. The fourth metal layer 44 is provided under the first metal layer 41. The fourth metal layer 44 is a corrosion prevention layer that prevents corrosion of the first metal layer 41, and is made of, for example, nickel (Ni). The thickness of the fourth metal layer 44 in the Z direction is, for example, 1 μm. Note that the second metal layer 42, the third metal layer 43, and the fourth metal layer 44 can be omitted.

[0031] The control layer 50 is provided under the fourth metal layer 44. The control layer 50 is made of a material having a smaller linear expansion coefficient than the metal layer having the largest thickness in the Z direction among the metal layers of the drain electrode 40, that is, the first metal layer 41. Examples of materials used for the control layer 50 include Si, tungsten (W), molybdenum (Mo), and chromium (Cr). The linear expansion coefficients of the materials used for the metal layers of the drain electrode 40 and the control layer 50 are shown in FIG. 2. Furthermore, it is preferable that the control layer 50 is made of a hard material.

[0032] The semiconductor device 100 according to the first embodiment has the structure described above, and thus forms a first transistor 71 and a second transistor 72. The first transistor 71 has a first region 10a, a first source electrode 21, a first gate electrode 31, a first insulating film 61, and a drain electrode 40. The second transistor 72 has a second region 10b, a second source electrode 22, a second gate electrode 32, a second insulating film 62, and a drain electrode 40. That is, the first transistor 71 and the second transistor 72 have a common drain electrode 40.

[0033] The first gate electrode 31 and the second gate electrode 32 extend in the Y direction. Like the first gate electrode 31 and the second gate electrode 32, each region provided in the semiconductor device 100, such as the first base region 13a, the second base region 13b, the first source region 14a, and the second source region 14b, each extends in the Y direction.

[0034] FIG. 4 shows a plan view of the semiconductor device 100 according to the first embodiment in the XY plane. A cross-sectional view taken along line A-A' in FIG. 4 is shown in FIG. 1. A first source electrode pad 81 and a first gate electrode pad 91 are provided on the upper part of the first transistor 71 and are exposed to the outside of the insulating film 60. The first source electrode pad 81 is electrically connected to the first source electrode 21. The first gate electrode pad 91 is electrically connected to the first gate electrode 31. A second source electrode pad 82 and a second gate electrode pad 92 are provided on the upper part of the second transistor 72 and are exposed to the outside of the insulating film 60. The second source electrode pad 82 is electrically connected to the second source electrode 22. The second gate electrode pad 92 is electrically connected to the second gate electrode 32.

[0035] (Operation of the semiconductor device 100) The operation of the semiconductor device 100 will be described with reference to Fig. 3. Fig. 3 shows an equivalent circuit diagram of the semiconductor device 100 according to the first embodiment.

[0036] As described above, the semiconductor device 100 according to the first embodiment is used in, for example, a battery protection circuit.

[0037] During charging and discharging, a voltage equal to or greater than the threshold is applied to the first gate electrode 31 and the second gate electrode, and the first transistor 71 and the second transistor 72 are turned on. During charging, a current flows from the first source electrode 21 to the drain electrode 40. The current then passes through the first metal layer 41 of the drain electrode 40 in the X direction, and reaches the second transistor 72. During discharging, a current flows from the second source electrode 22 to the drain electrode 40. The current then passes through the first metal layer 41 of the drain electrode 40 in the X direction, and reaches the first transistor 71.

[0038] During overcharging or over-discharging, one of the first transistor 71 and the second transistor 72 is turned off by a control circuit (not shown).

[0039] As described above, the semiconductor device 100 controls the flow of current in both directions.

[0040] (Method of Manufacturing Semiconductor Device 100) 5 to 7 are cross-sectional views showing manufacturing steps of the semiconductor device 100 according to the first embodiment. An example of a manufacturing method of the semiconductor device 100 according to the first embodiment will be described with reference to FIGS.

[0041] First, n + A semiconductor substrate 11 of the type 11 is prepared. + Next, in the Z direction, + By epitaxially growing the n-type semiconductor substrate 11, - A mold drift region 12 is formed.

[0042] As shown in FIG. 5(a), in the drift region 12, a first base region 13a, a second base region 13b, a first source region 14a, a second source region 14b, a first gate electrode 31, a second gate electrode 32, a first insulating film 61, a second insulating film 62, a first source electrode 21, a second source electrode 22, a first source electrode pad 81, a second source electrode pad 82, a first gate electrode pad 91, a second gate electrode pad 92, and an insulating film 60 are formed.

[0043] As shown in Figure 5(b), n + The mold semiconductor substrate 11 is ground to reduce the thickness of the semiconductor layer 10 in the Z direction.

[0044] As shown in FIG. 6(a), a second metal layer 42 and a third metal layer 43 are formed by, for example, sputtering.

[0045] As shown in Fig. 6(b), a part of the first metal layer 41 is formed by sputtering. Then, as shown in Fig. 7(a), the first metal layer 41 is formed by plating.

[0046] As shown in FIG. 7(b), a fourth metal layer 44 is formed by, for example, plating.

[0047] As shown in FIG. 8, the control layer 50 is formed by, for example, sputtering.

[0048] (Effects of the First Embodiment) The effect of the semiconductor device 100 according to the first embodiment will be described using a comparative semiconductor device 300. Fig. 10 shows a cross-sectional view of the semiconductor device 300 according to the comparative example. The comparative semiconductor device 300 differs from the semiconductor device 100 according to the first embodiment in that the control layer 50 is not provided.

[0049] The semiconductor device 300 of the comparative example and the semiconductor device 100 according to the first embodiment are mounted on a wiring substrate 200 with the drain electrode 40 facing upward, as shown in Fig. 9. That is, the first source electrode pad 81, the second source electrode pad 82, the first gate electrode pad 91, and the second gate electrode pad 92 of the semiconductor device 100 are bonded to the conductor portion 220 of the wiring substrate 200 via a bonding material 210. The bonding material 210 is, for example, solder. The semiconductor device 100 is sealed with a resin or the like, but the resin is omitted in Fig. 9.

[0050] In order to connect the first source electrode pad 81, the second source electrode pad 82, the first gate electrode pad 91, and the second gate electrode pad 92 of the semiconductor device 100 with the bonding material 210, the temperature of the reflow furnace is increased.

[0051] At that time, the drain electrode 40 thermally expands due to the rise in temperature. The semiconductor layer 10 also thermally expands, but since the linear expansion coefficient of the drain electrode 40 is generally greater than that of the semiconductor layer 10, the amount of expansion of the drain electrode 40 is greater than that of the semiconductor layer 10. For example, if the main material of the semiconductor layer 10 is Si, and the main material of the first metal layer 41, which is the thickest in the Z direction among the metal layers of the drain electrode 40, is Ag, the linear expansion coefficient of Si is 2.8×10 -6 , the linear expansion coefficient of Ag is 19.7×10 -6 , Since the semiconductor layer 10 and the first metal layer 41 of the drain electrode 40 are fixed to each other via the second metal layer 42 and the third metal layer 43, the area of ​​the part where the semiconductor layer 10 and the drain electrode 40 are fixed to each other must be constant.

[0052] Therefore, bending stress is generated so that the area of ​​the drain electrode 40, which has a large amount of expansion, becomes larger, and the semiconductor layer 10 and the drain electrode 40 are warped convexly toward the drain electrode 40. There is a risk that cracks will occur in the semiconductor layer 10 due to the warping caused by the bending stress.

[0053] In order to reduce the resistance during on-operation of the semiconductor device 100, the thickness of the semiconductor layer 10 is small and the thickness of the first metal layer 41, which is the main current path of the drain electrode 40, is large. In particular, when the semiconductor layer 10 is 100 μm or less, warping becomes large and cracks are easily generated in the semiconductor layer 10.

[0054] In light of the above, the effects of the semiconductor device 100 according to the first embodiment will be described. In the semiconductor device 100 according to the first embodiment, a control layer 50 having a smaller linear expansion coefficient than the drain electrode 40 is provided below the drain electrode 40. With the drain electrode 40 sandwiched between the semiconductor layer 10 and the control layer 50, the temperature of the reflow furnace is increased.

[0055] The drain electrode 40, which is susceptible to bending stress, is sandwiched between the semiconductor layer 10 and the control layer 50, which have a smaller linear expansion coefficient than the drain electrode 40, and therefore the occurrence of bending stress due to the difference in linear expansion coefficient can be suppressed. Therefore, the occurrence of convex warping of the semiconductor layer 10 and the drain electrode 40 due to bending stress is suppressed, and by providing the control layer 50, the occurrence of cracks in the semiconductor layer 10 can be suppressed while maintaining low resistance during on-operation.

[0056] Furthermore, when the semiconductor device 100 according to the first embodiment is used, heat is generated, and the temperature around the semiconductor device 100 may rise. In this case, too, there is a risk that cracks will occur in the semiconductor layer 10 due to warping caused by bending stress, but the provision of the control layer 50 can suppress the occurrence of cracks in the semiconductor layer 10.

[0057] Furthermore, during the manufacture of the semiconductor device 300 of the comparative example, the second metal layer 42, the third metal layer 43, and a part of the first metal layer 41 are formed on the first surface P1 of the semiconductor layer 10 by using sputtering. When using sputtering, high-energy particles collide with the semiconductor layer 10, so that the second metal layer 42, the third metal layer 43, and a part of the first metal layer 41 are formed in a state in which the temperature of the semiconductor layer 10 is elevated. Next, the first metal layer 41 and the fourth metal layer 44 are formed by plating. When plating is used, the metal layer is formed at a temperature close to room temperature. Therefore, the temperature of the semiconductor layer 10 and each metal layer drops during the process from the formation of the second metal layer 42, the third metal layer 43, and a part of the first metal layer 41 to the formation of the first metal layer 41 and the fourth metal layer 44. As described above, the linear expansion coefficient of the drain electrode 40 is generally larger than that of the semiconductor layer 10, so that the amount of contraction of the drain electrode 40 is larger than that of the semiconductor layer 10. Therefore, bending stress is generated so as to reduce the area of ​​the drain electrode 40, which has a large amount of shrinkage, and the semiconductor layer 10 and the drain electrode 40 are distorted in a convex shape toward the semiconductor layer 10. If warping occurs in the wafer state, it becomes difficult to singulate the semiconductor layer 10. Since the warping remains even after singulation, there is a risk of a mounting failure occurring when the semiconductor device 100 is mounted on the wiring board 200.

[0058] On the other hand, in the semiconductor device 100 according to the first embodiment, the control layer 50 is formed after the fourth metal layer 44 is formed. Since the control layer 50 is formed by sputtering, the temperature of the semiconductor layer 10 and the drain electrode 40 rises. The warping that occurs during the formation of the drain electrode 40 is eliminated by the temperature rise. Although the temperature drops after the formation of the control layer 50, the drain electrode 40, which is prone to bending stress, is sandwiched between the semiconductor layer 10 and the control layer 50, which have a smaller linear expansion coefficient than the drain electrode 40, so that the occurrence of bending stress due to the difference in linear expansion coefficient can be suppressed. Therefore, by providing the control layer 50, the occurrence of convex warping of the semiconductor layer 10 and the drain electrode 40 due to bending stress can be suppressed.

[0059] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]

[0060] 10 Semiconductor layer 10a 1st area 10b 2nd area 11 Drain region 12 Drift Region 13a First base region 13b Second base region 14a First source region 14b Second source region 21 First source electrode (first electrode) 22 Second source electrode (second electrode) 31 First gate electrode 32 Second gate electrode 40 Drain electrode (third electrode) 41 1st metal layer 42 Second metal layer 43 Third metal layer 44 4th metal layer 50 Control Layer 60 Insulating film 61 First insulating film 62 Second insulating film 71 First transistor 72 Second transistor 81 First source electrode pad 82 Second source electrode pad 91 First gate electrode pad 92 Second gate electrode pad 100, 300 Semiconductor device 200 Wiring board 210 Bonding material 220 Conductor P1 Page 1 P2 Page 2

Claims

1. a first surface of a semiconductor layer having a first surface and a second surface facing the first surface in a first direction; A region, a first electrode electrically connected to the second surface of the first region; a first gate electrode provided in the first region; a first transistor having The first region is adjacent to the second region in a second direction intersecting the first direction, a second region of the semiconductor layer having a first surface and the second surface; a second gate electrode provided in the second region; a first electrode electrically connected to the second surface of the second region and spaced apart from the first electrode; A second electrode; and a second transistor having The first transistor and the second transistor are provided on the first surface side. a third electrode electrically connected thereto; a control layer provided so that the third electrode is located between the control layer and the first surface; having The third electrode is A first metal layer; a second metal layer provided closer to the second surface than the first metal layer; a third metal layer provided between the first metal layer and the second metal layer; a fourth metal layer provided between the first metal layer and the control layer; having The first metal layer of the third electrode has a largest thickness in the first direction, The control layer has a smaller linear expansion coefficient than the first metal layer.

2. 2 . The semiconductor device according to claim 1 , wherein the thickness of the first metal layer in the first direction is 10 μm or more, and the thickness of the semiconductor layer in the first direction is 100 μm or less.

3. The semiconductor device according to claim 1 , wherein the first metal layer contains either silver or copper.

4. 4. The semiconductor device according to claim 1, wherein the control layer contains any one of silicon, tungsten, molybdenum, and chromium.

Citation Information

Patent Citations

  • Semiconductor device and manufacturing method thereof

    JP2011233643A

  • Semiconductor device

    JP2013069852A

  • Power semiconductor device and manufacturing method thereof

    JP2015053455A

  • Semiconductor device

    WO2019244384A1

  • Sic semiconductor device

    WO2020213603A1