Laser processing method, semiconductor device manufacturing method and inspection apparatus
The method addresses the challenge of observing small cracks in semiconductor substrates by using focused laser light propagation through the substrate to confirm crack extension, ensuring reliable cutting and preventing wasteful grinding in semiconductor device manufacturing.
Patent Information
- Application Number
- JP2023108163
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-06-30
- Publication Date
- 2024-09-19
- Estimated Expiration
- 2038-10-04
AI Technical Summary
Existing laser processing methods struggle to reliably confirm whether cracks spanning multiple rows of modified regions in a semiconductor substrate extend sufficiently toward the surface side, as they are difficult to observe due to the small width of the cracks relative to the wavelength of infrared light used for observation.
A method involving irradiating a wafer with a laser beam from the back side to form modified regions, inspecting the tip position of cracks using focused laser light that propagates through the substrate, and evaluating the crack extension by detecting light from the back side to the front side, utilizing an objective lens with a numerical aperture of 0.45 or more.
This approach allows for accurate confirmation of crack extension, ensuring reliable cutting of the wafer along intended lines and preventing wasteful grinding processes by identifying cracks that do not reach the surface, thereby enhancing the efficiency and reliability of semiconductor device manufacturing.
Smart Images

Figure 0007554318000014 
Figure 0007554318000011 
Figure 0007554318000016
Abstract
Description
[Technical field]
[0001] The present invention relates to a laser processing method, a semiconductor device manufacturing method, and an inspection apparatus. [Background technology]
[0002] A laser processing device is known that cuts a wafer, which includes a semiconductor substrate and a functional element layer formed on the surface of the semiconductor substrate, along each of a plurality of lines by irradiating the wafer with laser light from the back side of the semiconductor substrate to form a plurality of rows of modified regions inside the semiconductor substrate along each of the plurality of lines. The laser processing device described in Patent Document 1 is equipped with an infrared camera, and makes it possible to observe the modified regions formed inside the semiconductor substrate and processing damage formed in the functional element layer from the back side of the semiconductor substrate. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2017-64746 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the laser processing apparatus as described above, the wafer may be irradiated with laser light from the back side of the semiconductor substrate under conditions that cause cracks to be formed across multiple rows of modified regions. In such a case, if the cracks across the multiple rows of modified regions do not extend sufficiently to the front side of the semiconductor substrate due to, for example, a malfunction of the laser processing apparatus, the wafer may not be reliably cut along each of the multiple lines in a subsequent process. In particular, when grinding the back side of the semiconductor substrate after the formation of the modified regions, if it is not possible to confirm whether the cracks across the multiple rows of modified regions extend sufficiently to the front side of the semiconductor substrate before the grinding process, the wafer may not be reliably cut along each of the multiple lines after the grinding process, and the grinding process may be wasted.
[0005] It is difficult to confirm whether the cracks across the multiple rows of modified regions have sufficiently extended to the front surface side of the semiconductor substrate by only observing the modified regions. Although it is possible to observe the cracks across the multiple rows of modified regions, it is difficult to observe the cracks by simply using an infrared camera because the width of the cracks is usually smaller than the wavelength of infrared light.
[0006] The present invention aims to provide a laser processing method, a semiconductor device manufacturing method, and an inspection apparatus that can confirm whether cracks spanning multiple rows of modified regions extend sufficiently toward the surface side of a semiconductor substrate. [Means for solving the problem]
[0007] The laser processing method of the present invention includes a first step of preparing a wafer comprising a semiconductor substrate having a front and back surface and a functional element layer formed on the front surface, and irradiating the wafer with laser light from the back surface side along each of the multiple lines to form multiple rows of modified regions inside the semiconductor substrate along each of the multiple lines, and a second step of inspecting the tip position of a crack extending from the modified region closest to the back surface to the back surface side in an inspection area between the modified region closest to the back surface among the multiple rows of modified regions and the back surface, where in the first step, the laser light is irradiated to the wafer from the back surface side along each of the multiple lines under conditions such that a crack is formed across the multiple rows of modified regions, and in the second step, the tip position is inspected by focusing the laser light within the inspection area from the back surface side and detecting light propagating through the semiconductor substrate from the front surface side to the back surface side.
[0008] In this laser processing method, the light propagating through the semiconductor substrate from the front side to the back side is detected by focusing on an inspection area between the modified area closest to the back side of the semiconductor substrate from the back side of the semiconductor substrate. By detecting the light in this manner, the tip position of the crack extending from the modified area closest to the back side to the back side of the semiconductor substrate can be confirmed in the inspection area. When the tip position of the crack is located on the front side of the semiconductor substrate with respect to the reference position between the modified area closest to the back side of the semiconductor substrate and the back side of the semiconductor substrate, it is assumed that the crack extending across the multiple rows of modified regions does not extend sufficiently to the front side of the semiconductor substrate. Therefore, according to this laser processing method, it is possible to confirm whether the crack extending across the multiple rows of modified regions extends sufficiently to the front side of the semiconductor substrate.
[0009] In the laser processing method of the present invention, in the first step, the wafer may be irradiated with laser light from the backside along each of the multiple lines under the condition that the cracks across the multiple rows of modified regions reach the surface. This makes it possible to check whether the cracks across the multiple rows of modified regions reach the surface of the semiconductor substrate.
[0010] The laser processing method of the present invention further includes a third step of evaluating the processing result of the first step based on the inspection result of the second step, and in the third step, when the tip position is located on the back side of a reference position between the back side and the modified area closest to the back side, it may be evaluated that the cracks spanning the multiple rows of modified areas have reached the front surface, and when the tip position is located on the front side of the reference position, it may be evaluated that the cracks spanning the multiple rows of modified areas have not reached the front surface. In this way, the implementation of the subsequent steps can be determined based on the evaluation result.
[0011] In the laser processing method of the present invention, the inspection area is an area extending from the reference position to the back surface side and not reaching the back surface, and in the third step, when the tip position is located in the inspection area, it may be evaluated that the crack spanning the multiple rows of modified areas has reached the front surface, and when the tip position is not located in the inspection area, it may be evaluated that the crack spanning the multiple rows of modified areas has not reached the front surface. The tip position of the crack is more stable when the crack spanning the multiple rows of modified areas has reached the front surface of the semiconductor substrate than when the crack spanning the multiple rows of modified areas has not reached the front surface of the semiconductor substrate. Therefore, by setting the inspection area to the area extending from the reference position to the back surface side of the semiconductor substrate and not reaching the back surface, it is possible to efficiently inspect the crack spanning the multiple rows of modified areas.
[0012] In the laser processing method of the present invention, the multiple rows of modified regions may be two rows of modified regions. This makes it possible to efficiently form the multiple rows of modified regions and inspect for cracks across the multiple rows of modified regions.
[0013] The semiconductor device manufacturing method of the present invention comprises the first, second and third steps of the laser processing method described above, and a fourth step of, if it is determined in the third step that a crack spanning multiple rows of modified regions has reached the surface, grinding the back surface to expose the crack spanning multiple rows of modified regions on the back surface, and cutting the wafer into multiple semiconductor devices along each of the multiple lines.
[0014] According to this semiconductor device manufacturing method, if it is evaluated that cracks spanning multiple rows of modified regions have not reached the surface of the semiconductor substrate, grinding of the back surface of the semiconductor substrate is not performed, thereby preventing a situation in which the wafer cannot be reliably cut along each of the multiple lines after the grinding process.
[0015] In the semiconductor device manufacturing method of the present invention, in the fourth step, the back surface may be ground at least to the reference position, thereby making it possible to reliably cut the wafer along each of the multiple lines.
[0016] The inspection apparatus of the present invention is a wafer comprising a semiconductor substrate having a front and back surface, and a functional element layer formed on the front surface, the wafer comprising a plurality of rows of modified regions formed inside the semiconductor substrate along each of a plurality of lines, a light source that outputs light that is transparent to the semiconductor substrate, an objective lens that passes the light output from the light source and propagated through the semiconductor substrate, a light detection unit that detects the light that has passed through the objective lens, and an inspection unit that inspects the tip position of a crack extending from the modified region closest to the back surface to the back surface side in an inspection area between the modified region closest to the back surface among the plurality of rows of modified regions and the back surface based on the signal output from the light detection unit, the objective lens focuses on the inspection area from the back surface side, and the light detection unit detects the light propagating through the semiconductor substrate from the front surface side to the back surface side.
[0017] This inspection device focuses from the back side of the semiconductor substrate on an inspection area between the modified area closest to the back side of the semiconductor substrate and the back side, and detects light propagating through the semiconductor substrate from the front side to the back side. By detecting light in this manner, it is possible to confirm the tip position of a crack extending from the modified area closest to the back side to the back side of the semiconductor substrate in the inspection area.
[0018] In the inspection device of the present invention, the numerical aperture of the objective lens may be 0.45 or more, which makes it possible to more reliably confirm the tip position of the crack in the inspection area.
[0019] In the inspection apparatus of the present invention, the objective lens may have a correction collar, which makes it possible to more reliably confirm the tip position of the crack in the inspection area. Effect of the Invention
[0020] According to the present invention, it is possible to provide a laser processing method, a semiconductor device manufacturing method, and an inspection apparatus that can confirm whether cracks spanning multiple rows of modified regions extend sufficiently toward the surface side of a semiconductor substrate. [Brief description of the drawings]
[0021] [Figure 1] 1 is a configuration diagram of a laser processing apparatus equipped with an inspection device according to an embodiment; [Diagram 2] FIG. 2 is a plan view of a wafer of one embodiment. [Diagram 3] 3 is a cross-sectional view of a portion of the wafer shown in FIG. 2. [Figure 4] FIG. 2 is a configuration diagram of a laser irradiation unit shown in FIG. [Diagram 5] FIG. 2 is a configuration diagram of an inspection imaging unit shown in FIG. [Figure 6] FIG. 2 is a configuration diagram of an alignment correction imaging unit shown in FIG. [Figure 7] 6A to 6C are cross-sectional views of a wafer for explaining the imaging principle by the inspection imaging unit shown in FIG. 5, and images at various locations by the inspection imaging unit. [Figure 8] 6A to 6C are cross-sectional views of a wafer for explaining the imaging principle by the inspection imaging unit shown in FIG. 5, and images at various locations by the inspection imaging unit. [Figure 9] 1 is a SEM image of modified regions and cracks formed within a semiconductor substrate. [Figure 10] 1 is a SEM image of modified regions and cracks formed within a semiconductor substrate. [Figure 11] 6 is a light path diagram for explaining the imaging principle of the inspection imaging unit shown in FIG. 5, and a schematic diagram showing an image at a focal point of the inspection imaging unit. FIG. [Figure 12] 6 is a light path diagram for explaining the imaging principle of the inspection imaging unit shown in FIG. 5, and a schematic diagram showing an image at a focal point of the inspection imaging unit. FIG. [Figure 13] 6A to 6C are cross-sectional views of a wafer for explaining the inspection principle by the inspection imaging unit shown in FIG. 5, images of a cut surface of the wafer, and images at various points taken by the inspection imaging unit. [Figure 14] 6A to 6C are cross-sectional views of a wafer for explaining the inspection principle by the inspection imaging unit shown in FIG. 5, images of a cut surface of the wafer, and images at various points taken by the inspection imaging unit. [Figure 15] 1 is a flowchart of a semiconductor device manufacturing method according to an embodiment. [Figure 16] 16 is a cross-sectional view of a portion of a wafer in a grinding and cutting step of the semiconductor device manufacturing method shown in FIG. 15. [Figure 17] 16 is a cross-sectional view of a portion of a wafer in a grinding and cutting step of the semiconductor device manufacturing method shown in FIG. 15. [Figure 18] FIG. 13 is a configuration diagram of a laser processing system including an inspection device according to a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. In each drawing, the same or corresponding parts are denoted by the same reference numerals, and duplicated explanations will be omitted. [Laser processing equipment configuration]
[0023] 1, the laser processing apparatus 1 includes a stage 2, a laser irradiation unit 3, a plurality of imaging units 4, 5, and 6, a drive unit 7, and a control unit 8. The laser processing apparatus 1 is an apparatus that forms a modified region 12 in an object 11 by irradiating the object 11 with laser light L.
[0024] The stage 2 supports the object 11, for example, by adsorbing a film attached to the object 11. The stage 2 is movable along both the X direction and the Y direction, and is rotatable about an axis parallel to the Z direction. The X direction and the Y direction are a first horizontal direction and a second horizontal direction that are perpendicular to each other, and the Z direction is a vertical direction.
[0025] The laser irradiation unit 3 focuses laser light L, which is transparent to the object 11, and irradiates the object 11. When the laser light L is focused inside the object 11 supported by the stage 2, the laser light L is particularly absorbed in a portion corresponding to a focusing point C of the laser light L, and a modified region 12 is formed inside the object 11.
[0026] The modified region 12 is a region that differs from the surrounding non-modified region in terms of density, refractive index, mechanical strength, and other physical properties. Examples of the modified region 12 include a melting treatment region, a crack region, a dielectric breakdown region, and a refractive index change region. The modified region 12 has a property that cracks tend to extend from the modified region 12 to the incident side of the laser light L and to the opposite side. Such a property of the modified region 12 is utilized for cutting the target object 11.
[0027] As an example, when the stage 2 is moved along the X direction and the focal point C is moved along the X direction relative to the object 11, multiple modified spots 12s are formed in a row along the X direction. One modified spot 12s is formed by irradiating one pulse of laser light L. One row of modified regions 12 is a collection of multiple modified spots 12s lined up in a row. Adjacent modified spots 12s may be connected to each other or separated from each other depending on the relative moving speed of the focal point C with respect to the object 11 and the repetition frequency of the laser light L.
[0028] The imaging unit 4 captures images of the modified region 12 formed in the target object 11 and the tip of a crack extending from the modified region 12. In this embodiment, the control unit 8 functions as an inspection unit, and the stage 2, the imaging unit 4, and the control unit 8 function as an inspection device 10 (details will be described later).
[0029] Under the control of the control unit 8, the imaging units 5 and 6 capture an image of the object 11 supported on the stage 2 by light transmitted through the object 11. The images obtained by the imaging units 5 and 6 are used, for example, to align the irradiation position of the laser light L.
[0030] The drive unit 7 supports the laser irradiation unit 3 and the multiple imaging units 4, 5, and 6. The drive unit 7 moves the laser irradiation unit 3 and the multiple imaging units 4, 5, and 6 along the Z direction.
[0031] The control unit 8 controls the operations of the stage 2, the laser irradiation unit 3, the multiple imaging units 4, 5, and 6, and the drive unit 7. The control unit 8 is configured as a computer device including a processor, a memory, a storage, a communication device, and the like. In the control unit 8, the processor executes software (programs) loaded into the memory, and controls the reading and writing of data in the memory and storage, as well as communication by the communication device. In this way, the control unit 8 realizes the function of, for example, an inspection unit (details will be described later). [Object composition]
[0032] The object 11 of this embodiment is a wafer 20, as shown in FIG. 2 and FIG. 3. The wafer 20 includes a semiconductor substrate 21 and a functional element layer 22. The semiconductor substrate 21 has a front surface 21a and a back surface 21b. The semiconductor substrate 21 is, for example, a silicon substrate. The functional element layer 22 is formed on the front surface 21a of the semiconductor substrate 21. The functional element layer 22 includes a plurality of functional elements 22a arranged two-dimensionally along the front surface 21a. The functional elements 22a are, for example, light receiving elements such as photodiodes, light emitting elements such as laser diodes, circuit elements such as memories, etc. The functional elements 22a may be three-dimensionally configured by stacking a plurality of layers. Note that the semiconductor substrate 21 is provided with a notch 21c indicating the crystal orientation, but an orientation flat may be provided instead of the notch 21c.
[0033] The wafer 20 is cut into functional elements 22a along each of the lines 15. The lines 15 pass between the functional elements 22a when viewed from the thickness direction of the wafer 20. More specifically, the lines 15 pass through the center of the street region 23 (the center in the width direction) when viewed from the thickness direction of the wafer 20. The street region 23 extends in the functional element layer 22 so as to pass between adjacent functional elements 22a. In this embodiment, the functional elements 22a are arranged in a matrix along the surface 21a, and the lines 15 are set in a lattice pattern. The lines 15 are virtual lines, but may be lines that are actually drawn. [Laser irradiation unit configuration]
[0034] As shown in Fig. 4, the laser irradiation unit 3 has a light source 31, a spatial light modulator 32, and a condensing lens 33. The light source 31 outputs laser light L, for example, by a pulse oscillation method. The spatial light modulator 32 modulates the laser light L output from the light source 31. The spatial light modulator 32 is, for example, a reflective liquid crystal (LCOS: Liquid Crystal on Silicon) spatial light modulator (SLM: Spatial Light Modulator). The condensing lens 33 condenses the laser light L modulated by the spatial light modulator 32.
[0035] In this embodiment, the laser irradiation unit 3 irradiates the wafer 20 with laser light L from the back surface 21b side of the semiconductor substrate 21 along each of the multiple lines 15, thereby forming two rows of modified regions 12a, 12b inside the semiconductor substrate 21 along each of the multiple lines 15. The modified region (first modified region) 12a is the modified region closest to the front surface 21a among the two rows of modified regions 12a, 12b. The modified region (second modified region) 12b is the modified region closest to the modified region 12a and closest to the back surface 21b among the two rows of modified regions 12a, 12b.
[0036] The two rows of modified regions 12a, 12b are adjacent to each other in the thickness direction (Z direction) of the wafer 20. The two rows of modified regions 12a, 12b are formed by moving the two focusing points C1, C2 along the line 15 relative to the semiconductor substrate 21. The laser light L is modulated by the spatial light modulator 32 so that the focusing point C2 is located on the rear side of the focusing point C1 in the traveling direction and on the incident side of the laser light L.
[0037] The laser irradiation unit 3 irradiates the wafer 20 with the laser light L from the back surface 21b of the semiconductor substrate 21 along each of the multiple lines 15 under the condition that the cracks 14 across the two rows of modified regions 12a, 12b reach the front surface 21a of the semiconductor substrate 21. As an example, the semiconductor substrate 21 is a single crystal silicon substrate having a thickness of 775 μm, and the laser light L is irradiated from the back surface 21b of the semiconductor substrate 21 along each of the multiple lines 15 to the wafer 20 by aligning two focusing points C1, C2 at positions 54 μm and 128 μm from the front surface 21a, respectively. At this time, the wavelength of the laser light L is 1099 nm, the pulse width is 700 ns, and the repetition frequency is 120 kHz. The output of the laser light L at the focal point C1 is 2.7 W, the output of the laser light L at the focal point C2 is 2.7 W, and the relative moving speed of the two focal points C1 and C2 with respect to the semiconductor substrate 21 is 800 mm / sec.
[0038] The formation of the two rows of modified regions 12a, 12b and the cracks 14 is performed in the following case: in a later process, the back surface 21b of the semiconductor substrate 21 is ground to thin the semiconductor substrate 21 and expose the cracks 14 on the back surface 21b, and the wafer 20 is cut into a plurality of semiconductor devices along each of the plurality of lines 15. [Configuration of the inspection imaging unit]
[0039] 5, the imaging unit 4 includes a light source 41, a mirror 42, an objective lens 43, and a light detection unit 44. The light source 41 outputs light I1 that is transparent to the semiconductor substrate 21. The light source 41 is, for example, composed of a halogen lamp and a filter, and outputs light I1 in the near-infrared region. The light I1 output from the light source 41 is reflected by the mirror 42, passes through the objective lens 43, and is irradiated onto the wafer 20 from the rear surface 21b side of the semiconductor substrate 21. At this time, the stage 2 supports the wafer 20 on which the two rows of modified regions 12a, 12b are formed as described above.
[0040] The objective lens 43 passes the light I1 reflected by the surface 21a of the semiconductor substrate 21. In other words, the objective lens 43 passes the light I1 propagating through the semiconductor substrate 21. The numerical aperture (NA) of the objective lens 43 is 0.45 or more. The objective lens 43 has a correction collar 43a. The correction collar 43a corrects aberrations occurring in the light I1 within the semiconductor substrate 21, for example, by adjusting the distances between the multiple lenses that make up the objective lens 43. The light detection unit 44 detects the light I1 that has passed through the objective lens 43 and the mirror 42. The light detection unit 44 is, for example, composed of an InGaAs camera, and detects the light I1 in the near-infrared region.
[0041] The imaging unit 4 can capture images of each of the two rows of modified regions 12a, 12b and the tips of each of the multiple cracks 14a, 14b, 14c, and 14d (details will be described later). The crack 14a is a crack that extends from the modified region 12a to the front surface 21a. The crack 14b is a crack that extends from the modified region 12a to the back surface 21b. The crack 14c is a crack that extends from the modified region 12b to the front surface 21a. The crack 14d is a crack that extends from the modified region 12b to the back surface 21b. The control unit 8 controls the laser irradiation unit 3 to irradiate laser light L under conditions such that the cracks 14 spanning the two rows of modified regions 12a, 12b reach the surface 21a of the semiconductor substrate 21 (see Figure 4). However, if the cracks 14 do not reach the surface 21a due to some kind of malfunction or the like, multiple cracks such as these 14a, 14b, 14c, and 14d are formed. [Configuration of the imaging unit for alignment correction]
[0042] 6, the imaging unit 5 has a light source 51, a mirror 52, a lens 53, and a light detection unit 54. The light source 51 outputs light I2 that is transparent to the semiconductor substrate 21. The light source 51 is composed of, for example, a halogen lamp and a filter, and outputs light I2 in the near-infrared region. The light source 51 may be shared with the light source 41 of the imaging unit 4. The light I2 output from the light source 51 is reflected by the mirror 52 and passes through the lens 53, and is irradiated onto the wafer 20 from the back surface 21b side of the semiconductor substrate 21.
[0043] The lens 53 passes the light I2 reflected by the surface 21a of the semiconductor substrate 21. That is, the lens 53 passes the light I2 propagated through the semiconductor substrate 21. The numerical aperture of the lens 53 is 0.3 or less. That is, the numerical aperture of the objective lens 43 of the imaging unit 4 is larger than the numerical aperture of the lens 53. The light detection unit 54 detects the light I2 that has passed through the lens 53 and the mirror 52. The light detection unit 55 is composed of, for example, an InGaAs camera, and detects the light I2 in the near-infrared region.
[0044] The imaging unit 5, under the control of the control unit 8, irradiates the wafer 20 with light I2 from the back surface 21b side and detects the light I2 returning from the front surface 21a (functional element layer 22), thereby capturing an image of the functional element layer 22. Similarly, under the control of the control unit 8, the imaging unit 5, under the control of the control unit 8, irradiates the wafer 20 with light I2 from the back surface 21b side and detects the light I2 returning from the positions where the modified regions 12a and 12b are formed in the semiconductor substrate 21, thereby acquiring an image of the region including the modified regions 12a and 12b. These images are used for alignment of the irradiation position of the laser light L. The imaging unit 6 has a similar configuration to the imaging unit 5, except that the lens 53 has a lower magnification (for example, 6x in the imaging unit 5 and 1.5x in the imaging unit 6), and is used for alignment in the same manner as the imaging unit 5. [Principle of imaging by inspection imaging unit]
[0045] Using the imaging unit 4 shown in FIG. 5, the focal point F (the focal point of the objective lens 43) is moved from the back surface 21b side to the front surface 21a side with respect to the semiconductor substrate 21 in which the cracks 14 extending across the two rows of modified regions 12a, 12b reach the front surface 21a as shown in FIG. 7. In this case, when the focal point F is adjusted from the back surface 21b side to the tip 14e of the crack 14 extending from the modified region 12b to the back surface 21b side, the tip 14e can be confirmed (the image on the right side in FIG. 7). However, even if the focal point F is adjusted from the back surface 21b side to the cracks 14 themselves and the tip 14e of the cracks 14 reaching the front surface 21a, they cannot be confirmed (the image on the left side in FIG. 7). It should be noted that when the focal point F is adjusted from the back surface 21b side to the front surface 21a of the semiconductor substrate 21, the functional element layer 22 can be confirmed.
[0046] 5, the focal point F is moved from the back surface 21b side to the front surface 21a side for the semiconductor substrate 21 in which the cracks 14 extending across the two rows of modified regions 12a, 12b have not yet reached the front surface 21a, as shown in FIG. 8. In this case, even if the focal point F is aligned from the back surface 21b side to the tip 14e of the crack 14 extending from the modified region 12a to the front surface 21a side, the tip 14e cannot be confirmed (the image on the left side in FIG. 8). However, when the focal point F is aligned from the back surface 21b side to the region on the opposite side of the back surface 21b with respect to the front surface 21a (i.e., the region on the functional element layer 22 side with respect to the front surface 21a) and a virtual focal point Fv symmetrical to the focal point F with respect to the front surface 21a is positioned at the tip 14e, the tip 14e can be confirmed (the image on the right side in FIG. 8). The virtual focal point Fv is a point symmetrical with respect to the front surface 21a to the focal point F taking into account the refractive index of the semiconductor substrate 21.
[0047] As described above, the reason why the crack 14 itself cannot be confirmed is assumed to be because the width of the crack 14 is smaller than the wavelength of the light I1, which is the illumination light. Figures 9 and 10 are SEM (Scanning Electron Microscope) images of the modified region 12 and the crack 14 formed inside the semiconductor substrate 21, which is a silicon substrate. (b) of Figure 9 is an enlarged image of the region A1 shown in (a) of Figure 9, (a) of Figure 10 is an enlarged image of the region A2 shown in (b) of Figure 9, and (b) of Figure 10 is an enlarged image of the region A3 shown in (a) of Figure 10. Thus, the width of the crack 14 is about 120 nm, which is smaller than the wavelength (e.g., 1.1 to 1.2 μm) of the light I1 in the near-infrared region.
[0048] Based on the above, the imaging principle is assumed as follows. As shown in FIG. 11(a), when the focal point F is located in air, the light I1 does not return, and a dark image is obtained (the image on the right side of FIG. 11(a)). As shown in FIG. 11(b), when the focal point F is located inside the semiconductor substrate 21, the light I1 reflected by the front surface 21a returns, and a whitish image is obtained (the image on the right side of FIG. 11(b)). As shown in FIG. 11(c), when the focal point F is aligned with the modified region 12 from the rear surface 21b side, the modified region 12 absorbs, scatters, or the like a part of the light I1 reflected by the front surface 21a and returned, and an image is obtained in which the modified region 12 appears dark against a whitish background (the image on the right side of FIG. 11(c)).
[0049] As shown in (a) and (b) of FIG. 12, when the focal point F is focused on the tip 14e of the crack 14 from the back surface 21b side, for example, due to optical singularities (stress concentration, distortion, discontinuity of atomic density, etc.) occurring near the tip 14e, light confinement occurring near the tip 14e, etc., scattering, reflection, interference, absorption, etc. occur for a part of the light I1 reflected by the surface 21a and returned, so an image is obtained in which the tip 14e appears dark on a whitish background (the right image in (a) and (b) of FIG. 12). As shown in (c) of FIG. 12, when the focal point F is focused on a part other than the vicinity of the tip 14e of the crack 14 from the back surface 21b side, at least a part of the light I1 reflected by the surface 21a returns, so a whitish image is obtained (the right image in (c) of FIG. 12). [Inspection principle using the inspection imaging unit]
[0050] When the control unit 8 causes the laser irradiation unit 3 to irradiate the laser light L under the condition that the crack 14 across the two rows of the modified regions 12a, 12b reaches the surface 21a of the semiconductor substrate 21, and the crack 14 across the two rows of the modified regions 12a, 12b reaches the surface 21a as planned, the state of the tip 14e of the crack 14 is as follows. That is, as shown in Fig. 13, the tip 14e of the crack 14 does not appear in the region between the modified region 12a and the surface 21a and the region between the modified region 12a and the modified region 12b. The position of the tip 14e of the crack 14 extending from the modified region 12b to the back surface 21b side (hereinafter simply referred to as the "tip position") is located on the back surface 21b side with respect to the reference position P between the modified region 12b and the back surface 21b.
[0051] On the other hand, when the control unit 8 causes the laser irradiation unit 3 to irradiate the laser light L under the condition that the crack 14 across the two rows of the modified regions 12a, 12b reaches the surface 21a of the semiconductor substrate 21, if the crack 14 across the two rows of the modified regions 12a, 12b does not reach the surface 21a due to some malfunction contrary to the plan, the state of the tip 14e of the crack 14 will be as follows. That is, as shown in Fig. 14, the tip 14e of the crack 14a extending from the modified region 12a to the surface 21a appears in the region between the modified region 12a and the surface 21a. The tip 14e of the crack 14b extending from the modified region 12a to the back surface 21b and the tip 14e of the crack 14c extending from the modified region 12b to the surface 21a appear in the region between the modified region 12a and the modified region 12b. The tip position of the crack 14d extending from the modified region 12b toward the back surface 21b is located on the front surface 21a with respect to a reference position P between the modified region 12b and the back surface 21b.
[0052] As described above, if the control unit 8 performs at least one of the following first, second, third and fourth inspections, it is possible to evaluate whether or not the crack 14 across the two rows of modified regions 12a, 12b reaches the front surface 21a of the semiconductor substrate 21. In the first inspection, the region between the modified region 12a and the front surface 21a is set as the inspection region R1, and it is an inspection as to whether or not the tip 14e of the crack 14a extending from the modified region 12a to the front surface 21a is present in the inspection region R1. In the second inspection, the region between the modified region 12a and the modified region 12b is set as the inspection region R2, and it is an inspection as to whether or not the tip 14e of the crack 14b extending from the modified region 12a to the back surface 21b is present in the inspection region R2. In the third inspection, it is an inspection as to whether or not the tip 14e of the crack 14c extending from the modified region 12b to the front surface 21a is present in the inspection region R2. The fourth inspection is an inspection in which the area extending from the reference position P toward the back surface 21b but not reaching the back surface 21b is defined as the inspection area R3, and whether the tip position of the crack 14d extending from the modified area 12b toward the back surface 21b is located in the inspection area R3.
[0053] Each of the inspection regions R1, R2, and R3 can be set based on the position where the two light condensing points C1 and C2 are aligned with respect to the semiconductor substrate 21 before forming the two rows of modified regions 12a and 12b. When the crack 14 across the two rows of modified regions 12a and 12b reaches the front surface 21a of the semiconductor substrate 21, the tip position of the crack 14 extending from the modified region 12b to the back surface 21b side is stable, so the reference position P and the inspection region R3 can be set based on the results of the test processing. Note that, since the imaging unit 4 can image each of the two modified regions 12a and 12b as shown in Figures 13 and 14, each of the inspection regions R1, R2, and R3 may be set based on the positions of the two modified regions 12a and 12b after forming the two rows of modified regions 12a and 12b. [Laser processing method and semiconductor device manufacturing method]
[0054] The semiconductor device manufacturing method of the present embodiment will be described with reference to Fig. 15. Note that the semiconductor device manufacturing method of the present embodiment includes a laser processing method carried out in a laser processing apparatus 1.
[0055] First, the wafer 20 is prepared and placed on the stage 2 of the laser processing device 1. Next, the laser processing device 1 irradiates the wafer 20 with laser light L from the back surface 21b side of the semiconductor substrate 21 along each of the multiple lines 15, thereby forming two rows of modified regions 12a, 12b inside the semiconductor substrate 21 along each of the multiple lines 15 (S01, first step). In this step, the laser processing device 1 irradiates the wafer 20 with laser light L from the back surface 21b side of the semiconductor substrate 21 along each of the multiple lines 15 under the condition that the cracks 14 spanning the two rows of modified regions 12a, 12b reach the front surface 21a of the semiconductor substrate 21.
[0056] Next, the laser processing device 1 inspects the tip position of the crack 14d extending from the modified region 12b to the back surface 21b in the inspection region R3 between the modified region 12b and the back surface 21b (S02, second step). In this step, the laser processing device 1 adjusts the focus F from the back surface 21b side within the inspection region R3 and detects the light I1 propagating through the semiconductor substrate 21 from the front surface 21a side to the back surface 21b side to inspect whether the tip position of the crack 14d is located in the inspection region R3. Thus, in this embodiment, the laser processing device 1 performs the fourth inspection.
[0057] More specifically, the objective lens 43 of the imaging unit 4 focuses F from the back surface 21b side in the inspection region R3, and the light detection unit 44 of the imaging unit 4 detects the light I1 propagating through the semiconductor substrate 21 from the front surface 21a side to the back surface 21b side. At this time, the imaging unit 4 is moved along the Z direction by the driving unit 7, and the focus F is relatively moved along the Z direction within the inspection region R3. As a result, the light detection unit 44 acquires image data at each point in the Z direction. Then, the control unit 8 inspects whether the tip position of the crack 14d is located in the inspection region R3 based on the signal output from the light detection unit 44 (i.e., the image data at each point in the Z direction). In this way, in this embodiment, the control unit 8 functions as an inspection unit, and the stage 2, the imaging unit 4, and the control unit 8 function as an inspection device 10.
[0058] Next, the control unit 8 evaluates the processing result in step S01 based on the inspection result in step S02 (S03, third step). In this step, if the tip position of the crack 14d is located in the inspection region R3, the tip position of the crack 14d is located on the back surface 21b side with respect to the reference position P, and the control unit 8 evaluates that the crack 14 across the two rows of modified regions 12a, 12b has reached the front surface 21a of the semiconductor substrate 21. On the other hand, if the tip position of the crack 14d is not located in the inspection region R3, the tip position of the crack 14d is considered to be located on the front surface 21a side with respect to the reference position P, and the control unit 8 evaluates that the crack 14 across the two rows of modified regions 12a, 12b has not reached the front surface 21a of the semiconductor substrate 21.
[0059] Next, when it is evaluated that the crack 14 spanning the two rows of modified regions 12a, 12b has reached the surface 21a of the semiconductor substrate 21, the control unit 8 performs a passing process (S04). In this step, as the passing process, the control unit 8 controls the display of the laser processing apparatus 1 to display the fact that the laser processing apparatus 1 has passed, the display to display image data, the memory unit of the laser processing apparatus 1 to record the fact that the laser processing apparatus 1 has passed (storing as a log), and the memory unit to store the image data. In this way, the display of the laser processing apparatus 1 functions as a notification unit that notifies the operator of the fact that the laser processing apparatus 1 has passed.
[0060] On the other hand, if it is determined that the crack 14 spanning the two rows of modified regions 12a, 12b has not reached the surface 21a of the semiconductor substrate 21, the control unit 8 performs a rejection process (S05). In this step, as the rejection process, the control unit 8 controls the laser processing device 1 to light up a lamp to indicate rejection, the laser processing device 1 to display a display to indicate rejection, and the laser processing device 1 to record the rejection (store as a log) in a memory unit of the laser processing device 1. In this way, at least one of the lamp and the display of the laser processing device 1 functions as a notification unit that notifies the operator of the rejection.
[0061] The above steps S01 to S05 are the laser processing method performed by the laser processing device 1. The timing of performing the fourth inspection is not limited to after two rows of modified regions 12a, 12b are formed inside the semiconductor substrate 21 along each of all the lines 15. The timing of performing the fourth inspection may be a timing after the formation of the modified regions 12a, 12b along each of the multiple lines 15 extending in one direction and before further formation of the modified regions 12a, 12b along each of the multiple lines 15 extending in one direction, and may be a timing at which alignment of the irradiation position of the laser light L with respect to the lines 15 extending in one direction is performed. Alternatively, the timing of performing the fourth inspection may be a timing at which the formation of the modified regions 12a, 12b along each of the multiple lines 15 extending in one direction is switched from the formation of the modified regions 12a, 12b along each of the multiple lines 15 extending in one direction to the formation of the modified regions 12a, 12b along each of the multiple lines 15 extending in another direction. The location of the fourth inspection may be at least one of the multiple lines 15 set in a lattice pattern. However, when switching from forming modified regions 12a, 12b along each of the multiple lines 15 extending in one direction to forming modified regions 12a, 12b along each of the multiple lines 15 extending in another direction, it is preferable that the fourth inspection be performed at a location other than the intersection of the lines 15 extending in the other direction (the intersection of the line 15 extending in the other direction with each of the multiple lines 15 extending in the one direction). This is because the state of the crack 14 is likely to become unstable at the intersection of the lines 15 extending in the other direction.
[0062] If the passing process of step S04 is performed (i.e., if it is evaluated in step S03 that the crack 14 spanning the two rows of modified regions 12a, 12b has reached the front surface 21a of the semiconductor substrate 21), a grinding device grinds the back surface 21b of the semiconductor substrate 21 to expose the crack 14 spanning the two rows of modified regions 12a, 12b on the back surface 21b, and cuts the wafer 20 into a plurality of semiconductor devices along each of the plurality of lines 15 (S06, fourth step).
[0063] The above steps S01 to S06 constitute the semiconductor device manufacturing method including the laser processing method performed in the laser processing apparatus 1. If a rejection process is performed in step S05 (i.e., if it is evaluated in step S03 that the crack 14 spanning the two rows of modified regions 12a, 12b does not reach the front surface 21a of the semiconductor substrate 21), the laser processing apparatus 1 is inspected and adjusted, and the wafer 20 is subjected to laser processing again (recovery processing), etc.
[0064] Here, the grinding and cutting of the wafer 20 in step S06 will be described in more detail. As shown in Fig. 16, the grinding device 200 grinds (polishes) the back surface 21b of the semiconductor substrate 21 to thin the semiconductor substrate 21 and expose the cracks 14 on the back surface 21b, and cuts the wafer 20 into a plurality of semiconductor devices 20a along each of the plurality of lines 15. In this step, the grinding device 200 grinds the back surface 21b of the semiconductor substrate 21 to the reference position P for the fourth inspection.
[0065] As described above, when the crack 14 across the two rows of modified regions 12a, 12b reaches the front surface 21a of the semiconductor substrate 21, the tip position of the crack 14 extending from the modified region 12b to the back surface 21b side is located on the back surface 21b side with respect to the reference position P. Therefore, by grinding the back surface 21b of the semiconductor substrate 21 up to the reference position P, the crack 14 across the two rows of modified regions 12a, 12b can be exposed on the back surface 21b. In other words, the wafer 20 is irradiated with laser light L from the back surface 21b side of the semiconductor substrate 21 along each of the multiple lines 15 under the condition that the crack 14 across the two rows of modified regions 12a, 12b reaches the front surface 21a of the semiconductor substrate 21 and the reference position P, with the planned grinding end position being the reference position P.
[0066] 17, an expanding device 300 expands the expanding tape 201 attached to the rear surface 21b of the semiconductor substrate 21, thereby separating the multiple semiconductor devices 20a from each other. The expanding tape 201 is, for example, a DAF (Die Attach Film) composed of a base material 201a and an adhesive layer 201b. In this case, the adhesive layer 201b arranged between the rear surface 21b of the semiconductor substrate 21 and the base material 201a is cut into individual semiconductor devices 20a by expanding the expanding tape 201. The cut adhesive layer 201b is picked up together with the semiconductor devices 20a. [Action and Effects]
[0067] In the above-mentioned laser processing method, the focal point F is set from the back surface 21b side in the inspection area R3 between the modified area 12b and the back surface 21b of the semiconductor substrate 21, and the light I1 propagating through the semiconductor substrate 21 from the front surface 21a side to the back surface 21b side is detected. By detecting the light I1 in this way, the tip position of the crack 14d extending from the modified area 12b to the back surface 21b side can be confirmed in the inspection area R3. When the tip position of the crack 14d is located on the front surface 21a side with respect to the reference position P, it is assumed that the crack 14 across the two rows of modified areas 12a, 12b has not reached the front surface 21a of the semiconductor substrate 21. Therefore, according to the above-mentioned laser processing method, it can be confirmed whether the crack 14 across the two rows of modified areas 12a, 12b has reached the front surface 21a of the semiconductor substrate 21.
[0068] Furthermore, in the above-described laser processing method, when the tip position of the crack 14d is not located on the surface 21a side of the reference position P, it is evaluated that the crack 14 spanning the two rows of modified regions 12a, 12b has reached the surface 21a of the semiconductor substrate 21, and when the tip position of the crack 14d is located on the surface 21a side of the reference position P, it is evaluated that the crack 14 spanning the two rows of modified regions 12a, 12b has not reached the surface 21a of the semiconductor substrate 21. This makes it possible to determine the implementation of the subsequent process based on the evaluation results.
[0069] In the above-described laser processing method, an area extending from the reference position P toward the back surface 21b and not reaching the back surface 21b is defined as the inspection area R3, and when the tip position of the crack 14d is located in the inspection area R3, it is evaluated that the crack 14 across the two rows of modified areas 12a, 12b has reached the surface 21a of the semiconductor substrate 21, and when the tip position of the crack 14d is not located in the inspection area R3, it is evaluated that the crack 14 across the two rows of modified areas 12a, 12b has not reached the surface 21a of the semiconductor substrate 21. The tip position of the crack 14d is more stable when the crack 14 across the two rows of modified areas 12a, 12b has reached the surface 21a of the semiconductor substrate 21 than when the crack 14 across the two rows of modified areas 12a, 12b has not reached the surface 21a of the semiconductor substrate 21. Therefore, by setting the region extending from the reference position P toward the back surface 21b but not reaching the back surface 21b as the inspection region R3, it is possible to efficiently inspect for cracks 14 spanning two rows of modified regions 12a, 12b.
[0070] Furthermore, in the above-described laser processing method, two rows of modified regions 12a and 12b are formed as the multiple rows of modified regions 12. This makes it possible to efficiently form the multiple rows of modified regions 12 and inspect for cracks 14 that span the multiple rows of modified regions 12.
[0071] Furthermore, according to the above-described semiconductor device manufacturing method, if it is evaluated that the crack 14 spanning two rows of modified regions 12a, 12b has not reached the front surface 21a of the semiconductor substrate 21, grinding of the back surface 21b of the semiconductor substrate 21 is not performed, thereby preventing a situation from occurring in which the wafer 20 cannot be reliably cut along each of the multiple lines 15 after the grinding process.
[0072] Moreover, in the above-described semiconductor device manufacturing method, the back surface 21b of the semiconductor substrate 21 is ground up to the reference position P. This makes it possible to cut the wafer 20 along each of the multiple lines 15 reliably.
[0073] The inspection device 10 also focuses F from the back surface 21b side onto an inspection region R3 between the modified region 12b and the back surface 21b of the semiconductor substrate 21, and detects light I1 propagating from the front surface 21a side to the back surface 21b side of the semiconductor substrate 21. By detecting the light I1 in this manner, the tip position of the crack 14d can be confirmed in the inspection region R3.
[0074] Furthermore, in the inspection device 10, the numerical aperture of the objective lens 43 is 0.45 or more. This makes it possible to more reliably confirm the tip position of the crack 14d in the inspection region R3.
[0075] Furthermore, in the inspection device 10, the objective lens 43 has a correction collar 43a, which makes it possible to more reliably confirm the tip position of the crack 14d in the inspection region R3. [Variations]
[0076] The present invention is not limited to the above-described embodiment. For example, in the inspection step S02 shown in Fig. 15, the control unit 8 may perform at least one of the first inspection, the second inspection, and the third inspection in addition to the above-described fourth inspection. In the fourth inspection, for example, the entire area between the modified area 12b and the back surface 21b may be set as the inspection area R3, and it may be inspected whether the tip position of the crack 14d is located on the back surface 21b side with respect to the reference position P.
[0077] In the above embodiment, the laser processing apparatus 1 forms two rows of modified regions 12a, 12b in the semiconductor substrate 21 along each of the multiple lines 15, but the laser processing apparatus 1 may form three or more rows of modified regions 12 in the semiconductor substrate 21 along each of the multiple lines 15. The number and positions of the rows of modified regions 12 formed in one line 15 can be set appropriately taking into consideration the thickness of the semiconductor substrate 21 in the wafer 20 and the thickness of the semiconductor substrate 21 in the semiconductor device 20a. Note that multiple rows of modified regions 12 may be formed by relatively moving the focal point C of the laser light L multiple times in one line 15.
[0078] 15, the grinding device 200 may grind the back surface 21b of the semiconductor substrate 21 beyond the reference position P. The planned grinding end position can be set appropriately depending on whether or not the modified region 12 is to be left on the side surface (cut surface) of the semiconductor device 20a. Note that, when the semiconductor device 20a is, for example, a dynamic random access memory (DRAM), the modified region 12 may be left on the side surface of the semiconductor device 20a.
[0079] 18, the inspection device 10 may be configured as a separate unit from the laser processing device 1. The inspection device 10 shown in FIG. 18 includes a stage 101, a drive unit 102, and a control unit 103 in addition to the imaging unit 4. The stage 101 is configured similarly to the stage 2 described above, and supports the wafer 20 on which multiple rows of modified regions 12 are formed. The drive unit 102 supports the imaging unit 4 and moves the imaging unit 4 along the Z direction. The control unit 103 is configured similarly to the control unit 8 described above, and functions as an inspection unit. In the laser processing system shown in FIG. 18, the wafer 20 is transported between the laser processing device 1 and the inspection device 10 by a transport device such as a robot hand.
[0080] Moreover, the irradiation conditions of the laser light L when irradiating the wafer 20 with the laser light L from the back surface 21b side of the semiconductor substrate 21 along each of the multiple lines 15 are not limited to those described above. For example, the irradiation conditions of the laser light L may be conditions under which the cracks 14 across multiple rows of modified regions 12 (for example, two rows of modified regions 12a, 12b) reach the interface between the semiconductor substrate 21 and the functional element layer 22, as described above. Alternatively, the irradiation conditions of the laser light L may be conditions under which the cracks 14 across multiple rows of modified regions 12 reach the surface of the functional element layer 22 opposite to the semiconductor substrate 21. Alternatively, the irradiation conditions of the laser light L may be conditions under which the cracks 14 across multiple rows of modified regions 12 reach the vicinity of the surface 21a in the semiconductor substrate 21. In this way, the irradiation conditions of the laser light L may be conditions under which the cracks 14 across multiple rows of modified regions 12 are formed. In either case, it can be confirmed whether the cracks 14 across the multiple rows of modified regions 12 have sufficiently extended toward the front surface 21a of the semiconductor substrate 21.
[0081] Furthermore, the respective components in the above-described embodiments are not limited to the materials and shapes described above, and various materials and shapes can be applied. Furthermore, the respective components in one embodiment or modified example described above can be arbitrarily applied to the respective components in other embodiments or modified examples. [Explanation of symbols]
[0082] 2...stage, 8...control unit (inspection unit), 10...inspection device, 12, 12a, 12b...modified area, 14, 14d...crack, 14e...tip, 15...line, 20...wafer, 20a...semiconductor device, 21...semiconductor substrate, 21a...front surface, 21b...back surface, 22...functional element layer, 22a...functional element, 41...light source, 43...objective lens, 43a...correction collar, 44...light detection unit, F...focus, I1...light, L...laser light, P...reference position, R3...inspection area.
Claims
1. a first step of preparing a wafer including a semiconductor substrate having a front surface and a back surface, and a functional element layer formed on the front surface, and irradiating the wafer with laser light from the back surface side along each of a plurality of lines to form a modified region inside the semiconductor substrate along each of the plurality of lines; a second step of inspecting a tip position of a crack extending from the modified region to the back surface side in an inspection region between the modified region and the back surface, In the second step, a laser processing method is provided in which a focus is set within the inspection area from the back side, and the focus is moved relatively within the inspection area along the thickness direction of the wafer while light propagating through the semiconductor substrate from the front side to the back side is detected to obtain image data at each point in the thickness direction, and whether or not the tip position is located in the inspection area is inspected based on the image data.
2. 2. The laser processing method according to claim 1, wherein in the first step, the laser light is irradiated onto the wafer from the back surface side along each of the plurality of lines under a condition that the cracks reach the front surface.
3. A third step of evaluating a processing result in the first step based on a result of the inspection in the second step is further provided. The laser processing method of claim 2, wherein in the third step, when the tip position is located on the back surface side of a reference position between the modified region and the back surface, it is evaluated that the crack has reached the front surface, and when the tip position is located on the front surface side of the reference position, it is evaluated that the crack has not reached the front surface.
4. the inspection area is an area extending from the reference position toward the back surface side but not reaching the back surface, The laser processing method described in claim 3, wherein in the third step, when the tip position is located in the inspection area, it is evaluated that the crack has reached the surface, and when the tip position is not located in the inspection area, it is evaluated that the crack has not reached the surface.
5. The laser processing method according to claim 3 or 4, further comprising the first step, the second step, and the third step; and a fourth step of cutting the wafer into a plurality of semiconductor devices along each of the plurality of lines if it is evaluated in the third step that the crack has reached the surface.
6. a stage for supporting a wafer including a semiconductor substrate having a front surface and a back surface, and a functional element layer formed on the front surface, the wafer having modified regions formed inside the semiconductor substrate along each of a plurality of lines; a light source that outputs light that is transparent to the semiconductor substrate; an objective lens that passes the light output from the light source and propagated through the semiconductor substrate; a light detection unit that detects the light that has passed through the objective lens; an inspection unit that inspects a tip position of a crack extending from the modified region to the back surface side in an inspection region between the modified region and the back surface based on a signal output from the light detection unit; The objective lens is focused within the inspection area from the back side, the light detection unit detects the light propagating through the semiconductor substrate from the front surface side to the back surface side, The inspection unit obtains image data at each point in the thickness direction by detecting light propagating through the semiconductor substrate from the front side to the back side by the light detection unit while the objective lens focuses the focus within the inspection area from the back side and moves the focus relatively along the thickness direction of the wafer within the inspection area, and inspects whether the tip position is located in the inspection area based on the image data.
7. The inspection apparatus according to claim 6 , wherein the numerical aperture of the objective lens is 0.45 or more.
8. The inspection apparatus according to claim 6 or 7, wherein the objective lens has a correction collar.
Citation Information
Patent Citations
Method for processing wafer and laser processing device
JP2013258253A
Wafer processing method
JP2017017290A
Laser processing device and laser processing method
JP2017064746A
Device and method for detecting cracks
JP2017133997A