Biodegradable label manufacturing method and labels manufactured using this method
A biodegradable label manufacturing method addresses the non-biodegradability of existing labels by applying a water-soluble polymer solution, forming a film, and adding a water-repellent coating, achieving controlled adhesion and recyclability.
Patent Information
- Application Number
- KR1020230193363
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-12-27
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2043-12-27
AI Technical Summary
Existing PP or PET labels used in the bottled water market are difficult to recycle and pose environmental pollution due to non-biodegradability and the use of environmentally harmful adhesives.
A method for manufacturing a biodegradable label involving the application of a water-soluble polymer solution, formation of a water-soluble polymer film, printing an ink layer, and applying a water-repellent coating to control surface adhesion and facilitate biodegradation.
The method produces a label that is biodegradable through water decomposition, allowing for controlled adhesive strength and recyclability by adjusting surface roughness and using eco-friendly materials.
Smart Images

Figure 112023146461012-PAT00001_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a method for manufacturing a label, and more specifically, to a method for manufacturing a biodegradable label and a label manufactured by this method. Background Technology
[0003] The bottled water market has shown steady growth over the past few years, reaching a scale of 1 trillion won in 2020. There are approximately 70 domestic bottled water manufacturers, and in proportion to that number, there are about 300 diverse brands.
[0004] Recently, overseas exports of bottled water have been increasing, which is expected to lead to a rise in demand for eco-friendly labels. This is because the demand for eco-friendly products is growing alongside consumers' interest in environmental protection.
[0005] The increasing demand for eco-friendly products has also impacted the packaging market, naturally leading to an increase in its size. The global packaging market was valued at approximately $16.8 billion in 2018 and is projected to grow to approximately $28.6 billion by 2024.
[0006] However, existing PP or PET labels have the problem of releasing environmentally harmful substances during the manufacturing process. Furthermore, due to the adhesives used for label attachment, they are difficult to recycle and pose challenges in post-use disposal, resulting in environmental pollution.
[0007] Therefore, there is a continuing demand for biodegradable recyclable labels to wrap bottles of bottled water and beverages. To meet this demand, it is necessary to conduct research and development on labels manufactured using eco-friendly materials for the adhesive and film layers that are biodegradable. Prior art literature
[0009] Republic of Korea Registered Patent No. 10-2095156 The problem to be solved
[0010] The technical problem that the present invention aims to solve is to provide a method for manufacturing a biodegradable label, which is intended to resolve the problems of the aforementioned prior art.
[0011] Another technical objective of the present invention is to provide a label manufactured by a method for manufacturing a biodegradable label.
[0012] The technical problems that the present invention aims to solve are not limited to those mentioned above, and other unmentioned technical problems will be clearly understood by those skilled in the art to which the present invention belongs from the description below. means of solving the problem
[0014] To achieve the above technical objectives, one embodiment of the present invention provides a method for manufacturing a biodegradable label.
[0015] In one embodiment of the present invention, a method for manufacturing a biodegradable label may include: a step of applying a water-soluble polymer solution; a step of drying the applied water-soluble polymer solution to form a water-soluble polymer film; a step of printing an ink layer on the water-soluble polymer film; and a step of applying a water-repellent coating to the water-soluble polymer film on which the ink layer is printed to form a water-repellent coating layer.
[0016] In addition, in one embodiment of the present invention, the water-degradable polymer may include one or more from the group consisting of polyethylene oxide, carboxymethyl cellulose, methyl cellulose, polyvinyl alcohol, polyvinylpyrrolidone, and hydroxypropyl methylcellulose.
[0017] In addition, in one embodiment of the present invention, in the step of applying the water-soluble polymer solution, the weight of the water-soluble polymer may be 0.1 to 20 parts by weight relative to 100 parts by weight of the total water-soluble polymer solution.
[0018] In addition, in one embodiment of the present invention, the water-repellent coating layer may include one or more types from the group consisting of Heptadeca-fluoro-1,1,2,2,2 tetrahydrodecyl trichlorosilane and Sylgard 184.
[0019] In addition, in one embodiment of the present invention, in the step of applying the water-soluble polymer solution, the water-soluble polymer solution may be applied by a method comprising one or more of the group consisting of spray coating, dip coating, spin coating, and casting methods.
[0020] In addition, in one embodiment of the present invention, in the step of forming the water-soluble polymer film, the thickness of the water-soluble polymer film may be 0.1 μm to 2000 μm.
[0021] In addition, in one embodiment of the present invention, between the step of forming the water-soluble polymer film and the step of printing the ink layer, a step of improving the surface adhesion of the water-soluble polymer film by increasing the surface roughness of the water-soluble polymer film may be further included.
[0022] In addition, in one embodiment of the present invention, the process for increasing the surface roughness of the water-soluble polymer film may include one or more processes selected from the group consisting of an etching process, a polishing process, a lapping process, and a blasting process on the water-soluble polymer film.
[0023] To achieve the above technical problem, another embodiment of the present invention provides a biodegradable label.
[0024] In one embodiment of the present invention, the label can be manufactured according to the aforementioned method for manufacturing a biodegradable label. Effects of the invention
[0026] A label manufactured by the method for manufacturing a biodegradable label according to one embodiment of the present invention can be biodegradable by being capable of water decomposition, and can provide the effect of controlling the adhesive strength of the label by controlling the roughness of the label surface.
[0027] The effects of the present invention are not limited to the effects described above, and should be understood to include all effects that can be inferred from the configuration of the invention described in the detailed description of the invention or the claims. Brief explanation of the drawing
[0029] FIG. 1 is a flowchart showing the steps of a method for manufacturing a biodegradable label according to one embodiment of the present invention. FIG. 2 is a schematic diagram briefly illustrating the process of a method for manufacturing a biodegradable label according to one embodiment of the present invention. Figure 3 is a photograph of a label manufactured by a method for manufacturing a biodegradable label according to one embodiment of the present invention. Specific details for implementing the invention
[0030] The present invention will be described below with reference to the attached drawings. However, the present invention may be implemented in various different forms and is therefore not limited to the embodiments described herein. Furthermore, in order to clearly explain the present invention in the drawings, parts unrelated to the explanation have been omitted, and similar parts throughout the specification have been given similar reference numerals.
[0031] Throughout the specification, when it is stated that a part is "connected (connected, in contact, combined)" with another part, this includes not only cases where they are "directly connected," but also cases where they are "indirectly connected" with other members interposed between them. Furthermore, when it is stated that a part "includes" a certain component, this means that, unless specifically stated otherwise, it does not exclude other components but rather allows for the inclusion of additional components.
[0032] The terms used herein are merely for describing specific embodiments and are not intended to limit the invention. Singular expressions include plural expressions unless the context clearly indicates otherwise. In this specification, terms such as “comprising” or “having” are intended to indicate the presence of the features, numbers, steps, actions, components, parts, or combinations thereof described in the specification, and should be understood as not precluding the existence or addition of one or more other features, numbers, steps, actions, components, parts, or combinations thereof.
[0033] Embodiments of the present invention will be described in detail below with reference to the attached drawings.
[0034] Conventional labels have had problems that make recycling difficult due to strong adhesive properties or non-biodegradability. Accordingly, the present invention provides a method for manufacturing a biodegradable label that is biodegradable by manufacturing a label with water-soluble properties and controlling the adhesive properties of the label through surface roughness, as well as a label manufactured thereby.
[0035] Hereinafter, the present invention will be described with reference to the drawings presented in this specification. For reference, the drawings may be partially exaggerated to illustrate the features of the present invention. In such cases, it is preferable to interpret them in light of the entire intent of this specification.
[0036] A method for manufacturing a biodegradable label according to one embodiment of the present invention is described.
[0037] FIG. 1 is a flowchart showing the steps of a method for manufacturing a biodegradable label according to one embodiment of the present invention.
[0038] FIG. 2 is a schematic diagram briefly illustrating the process of a method for manufacturing a biodegradable label according to one embodiment of the present invention.
[0039] Referring to FIG. 1 and FIG. 2, a method for manufacturing a biodegradable label according to one embodiment of the present invention may include the step of applying a water-soluble polymer solution (S100); the step of drying the applied water-soluble polymer solution to form a water-soluble polymer film (S200); the step of printing an ink layer on the water-soluble polymer film (S300); and the step of applying a water-repellent coating to the water-soluble polymer film on which the ink layer is printed to form a water-repellent coating layer (S400).
[0040] The first step may include applying a water-soluble polymer solution. (S100)
[0041] In this case, the above-mentioned water-degradability refers to the characteristic of being able to decompose by moisture, literally.
[0042] In addition, biodegradable properties may include water-degradable properties.
[0043] At this time, The above water-degradable polymer may be a water-degradable polymer comprising one or more types from the group consisting of polyethylene oxide, carboxymethyl cellulose, methyl cellulose, polyvinyl alcohol, polyvinylpyrrolidone, and hydroxypropyl methylcellulose.
[0044] Conventional PP or PET material labels used in label manufacturing pose an environmental pollution problem because biodegradation is difficult, but the water-degradable label of the present invention can decompose by water, thereby solving the environmental pollution problem.
[0045] Meanwhile, the solvent of the above-mentioned water-degradable polymer solution may be a solvent comprising one or more types from the group consisting of ultra-pure water, ethanol, methanol, formic acid, glycerol, and dimethyl sulfoxide.
[0046] At this time, any type of solvent capable of uniformly dispersing water-degradable polymers and allowing drying is not limited to the aforementioned types of solvents.
[0047] also, In the step of applying the above water-soluble polymer solution, the weight of the water-soluble polymer may be 0.1 to 20 parts by weight relative to 100 parts by weight of the total water-soluble polymer solution.
[0048] At this time, if the weight of the water-soluble polymer is less than 0.1 parts by weight relative to 100 parts by weight of the total water-soluble polymer solution, problems such as incomplete film formation, reduced cohesion, and reduced mechanical strength may occur, and if it exceeds 20 parts by weight, problems such as reduced dispersibility may occur.
[0049] Accordingly, the weight portion of the water-soluble polymer may be 0.1 to 20 parts by weight, and the preferred weight portion may be 1 to 10 parts by weight.
[0050] Looking at Figure 2(b), one can see the application of a water-degradable polymer solution, which is a simplified representation of the application process. Various methods can be used to apply the above-mentioned water-degradable polymer solution.
[0051] Specifically, In the step of applying the above water-soluble polymer solution, the water-soluble polymer solution may be applied by a method comprising one or more of the group consisting of spray coating, dip coating, spin coating, and casting methods.
[0052] At this time, any method that allows the water-soluble polymer solution to be applied uniformly is not limited to the aforementioned group of application methods.
[0053] Meanwhile, looking at Figure 2(a) before applying the above-mentioned water-soluble polymer solution, one can see the process of dispersing the water-soluble polymer solution. This is a dispersion process to ensure that the thickness of the water-soluble label is manufactured uniformly. For example, the stirrer can be stirred at a speed of 100 rpm to 600 rpm, and the stirring temperature can be carried out at a temperature of 50℃ to 90℃.
[0054] A second step may include drying the applied water-soluble polymer solution to form a water-soluble polymer film. (S200)
[0055] At this time, a solid polymer film can be formed by drying the above-mentioned water-degradable polymer solution to evaporate the solvent.
[0056] In addition, the water-soluble polymer film prepared with the above-mentioned water-soluble polymer solution has the characteristic of being biodegradable in moisture, so if a label is manufactured using this, a biodegradable label can be manufactured.
[0057] In addition, in the step of forming the water-soluble polymer film, the thickness of the water-soluble polymer film may be 0.1 μm to 2000 μm.
[0058] At this time, if the thickness of the water-degradable polymer film is less than 0.1 μm, there may be a problem with weak mechanical strength, and if it exceeds 2000 μm, there may be a problem with reduced flexibility and transparency.
[0059] Accordingly, the thickness of the above water-degradable polymer film may be 0.1 μm to 2000 μm, and a more preferable thickness may be 10 μm to 100 μm.
[0060] Looking at Figure 2(c), you can see that the solvent of the coated water-soluble polymer film is evaporated and dried.
[0061] At this time, to dry the applied water-soluble polymer solution, drying can be carried out at a temperature of, for example, 20°C to 100°C.
[0062] However, the above drying temperature range is a temperature range for drying the solution, and is not limited to the aforementioned range as long as it is a temperature at which the solution can be dried.
[0063] Meanwhile, between the step of forming the water-soluble polymer film and the step of printing the ink layer, a step of improving the surface adhesion of the water-soluble polymer film by increasing the surface roughness of the water-soluble polymer film may be further included.
[0064] At this time, if the surface roughness of the water-soluble polymer film is increased, a microstructure is formed on the surface of the water-soluble polymer film, and the adhesion of the film can be improved through this.
[0065] Specifically, a microstructure is formed on the surface of the film. For example, a microstructure can be formed on the surface of the film in the form of a structure in which micro-sized protrusions are repeatedly formed as a microstructure on the surface of a label.
[0066] In addition, the surface roughness of the film surface formed with the above microstructure may be 0.01 μm to 6 μm.
[0067] Through this, the surface roughness of the water-soluble polymer film can be controlled according to the intended use of the label, thereby controlling the adhesion of the water-soluble polymer film.
[0068] As a specific method for increasing the surface roughness of the above-mentioned water-soluble polymer film, the process for increasing the surface roughness of the above-mentioned water-soluble polymer film may include one or more processes from the group consisting of an etching process, a polishing process, a lapping process, and a blasting process on the above-mentioned water-soluble polymer film.
[0069] In addition, surface roughness can be controlled by adjusting humidity and temperature while manufacturing the water-degradable polymer film.
[0070] In this case, surface roughness can be adjusted for both the surface attached to the PET bottle and the surface on which the ink is printed; as surface roughness increases, the adhesion of the label and the ink increases.
[0071] The water-repellent coating utilizes a self-assembled monolayer and is coated on the surface at the molecular level, resulting in no significant change in surface roughness; therefore, if a water-repellent coating is applied to the surface of a PET bottle after attaching an ink-printed label, stable adhesion can be maintained without issues regarding the label's adhesion.
[0072] A third step may include printing an ink layer on the water-degradable polymer film. (S300)
[0073] Looking at (d) of Fig. 2, it can be seen that an ink layer is formed on a water-degradable polymer film.
[0074] At this time, the ink used in the ink layer is not particularly limited, and any ink that can be used on the manufactured water-degradable polymer film can be used without restriction.
[0075] In addition, the above-mentioned water-degradable polymer film has hydrophilic properties, which increases the adhesion of the ink layer, allowing a clear ink layer to be printed on the label.
[0076] As a final step, the method may include the step of forming a water-repellent coating layer by applying a water-repellent coating to the water-degradable polymer film on which the ink layer is printed. (S400)
[0077] Looking at Figure 2(e), it can be seen that a water-degradable polymer film with an ink layer printed thereon is immersed in a water-repellent coating solution to perform a water-repellent coating, thereby forming a water-repellent coating layer.
[0078] At this time, the water-repellent coating layer has a barrier effect against oxygen and moisture, and the water-repellent coating layer used in the present invention utilizes a material that is recyclable and possesses the aforementioned characteristics.
[0079] Accordingly, the water-repellent coating layer may be a water-repellent coating layer comprising one or more types from the group consisting of Heptadeca-fluoro-1,1,2,2,2 tetrahydrodecyl trichlorosilane and Sylgard 184.
[0080] At this time, the water-degradable polymer film on which the ink layer is printed can be coated with a water-repellent coating layer to prevent the label from decomposing due to everyday moisture.
[0081] In addition, when water is added to a label formed with a water-repellent coating layer, the label is not initially degraded by the water-repellent coating layer, but over time, the label can be degraded by water, and the water-repellent coating layer can be removed by immersion in, for example, a hexane or xylene solution, thereby allowing the label of the present invention to be biodegraded.
[0082] As a specific example, the water-repellent coating can be removed by first soaking in hexane or xylene, and the ink in the ink layer can be removed using a solvent such as ethanol or acetone.
[0083] Afterwards, if the remaining circuit board is immersed in water, the label decomposes, making it possible to recycle.
[0084] As another example, recycling may be possible by immersing the substrate in water to decompose the label, then using a centrifuge to separate and obtain the water, ink, and water-repellent coating material for reuse.
[0086] A biodegradable label according to another embodiment of the present invention is described.
[0087] A biodegradable label according to one embodiment of the present invention can be manufactured using the aforementioned method for manufacturing a biodegradable label.
[0088] Figure 2 (f) briefly illustrates a label manufactured by a biodegradable label manufacturing method.
[0089] At this time, the above label can be applied not only to label packaging that wraps the surface of the bottle, but also to all packaging materials that can be applied thereto.
[0091] Accordingly, the label manufactured by the method for manufacturing a biodegradable label according to the present invention can control surface adhesion by controlling surface roughness, and can manufacture a label having water-degradable properties to produce a label that is biodegradable and recyclable.
[0093] The present invention will be explained in more detail below through examples and experimental examples. These examples and experimental examples are solely for the purpose of illustrating the present invention, and the scope of the present invention is not limited by these examples and experimental examples.
[0095] Examples
[0096] First, 5g of PVA polymer was dispersed in 95ml of ultra-water to prepare a 5wt% water-soluble polymer solution.
[0097] Afterwards, 3g of the prepared PVA water-soluble polymer solution was applied using the drop-casting method.
[0098] Next, the applied PVA water-soluble polymer solution was dried for 24 hours at room temperature to produce a PVA water-soluble polymer film with a thickness of 70 μm.
[0099] After printing ink on the surface of the manufactured PVA water-degradable polymer film, a water-repellent coating was applied to the ink-printed PVA water-degradable polymer film using Heptadeca-fluoro-1,1,2,2,2 tetrahydrodecyl trichlorosinane.
[0100] Thus, a water-degradable polymer film was manufactured.
[0102] Experimental Example
[0103] Figure 3 is a photograph of a label manufactured by a method for manufacturing a biodegradable label according to one embodiment of the present invention.
[0104] Referring to Fig. 3, Fig. 3(a) is a photograph of a label formed on a substrate after an ink layer called CHOSUN is formed on a PVA water-soluble polymer film and a water-repellent coating layer is formed.
[0105] Looking at Figures 3(b) and (c), it can be seen that hexane and ethanol are added to the label, and looking at Figure 3(d), it can be seen that the ink layer is gradually decomposing.
[0106] Looking at Figures 3 (e) and (f), it can be seen that after 2 hours, the water-repellent coating layer and ink layer of the label are completely decomposed, leaving only the substrate.
[0108] Through the aforementioned experimental examples, it can be confirmed that the label manufactured by the present biodegradable label manufacturing method decomposes when water is added.
[0110] The foregoing description of the present invention is for illustrative purposes only, and those skilled in the art will understand that other specific forms can be easily modified without altering the technical spirit or essential features of the present invention. Therefore, the embodiments described above should be understood as illustrative in all respects and not restrictive. For example, each component described as a single unit may be implemented in a distributed manner, and components described as distributed may likewise be implemented in a combined form.
[0111] The scope of the present invention is defined by the claims set forth below, and all modifications or variations derived from the meaning and scope of the claims and equivalent concepts thereof should be interpreted as being included within the scope of the present invention.
Claims
Claim 1 A method for manufacturing a biodegradable label comprising: a step of applying a water-soluble polymer solution; a step of drying the applied water-soluble polymer solution to form a water-soluble polymer film; a step of printing an ink layer on the water-soluble polymer film; and a step of applying a water-repellent coating to the water-soluble polymer film on which the ink layer is printed to form a water-repellent coating layer, wherein the weight of the water-soluble polymer is 0.1 to 20 parts by weight relative to 100 parts by weight of the total water-soluble polymer solution, and the thickness of the water-soluble polymer film is 0.1 μm to 2000 μm. Claim 2 A method for manufacturing a biodegradable label according to claim 1, wherein the water-degradable polymer comprises one or more types selected from the group consisting of polyethylene oxide, carboxymethyl cellulose, methyl cellulose, polyvinyl alcohol, polyvinylpyrrolidone, and hydroxypropyl methylcellulose. Claim 3 delete Claim 4 A method for manufacturing a biodegradable label according to claim 1, characterized in that the water-repellent coating layer comprises one or more types from the group consisting of Heptadeca-fluoro-1,1,2,2,2 tetrahydrodecyl trichlorosilane and Sylgard 184. Claim 5 A method for manufacturing a biodegradable label according to claim 1, wherein, in the step of applying the water-soluble polymer solution, the water-soluble polymer solution is applied by a method comprising one or more of the group consisting of spray coating, dip coating, spin coating, and casting methods. Claim 6 delete Claim 7 A method for manufacturing a biodegradable label according to claim 1, further comprising, between the step of forming the water-degradable polymer film and the step of printing the ink layer, a step of improving the surface adhesion of the water-degradable polymer film by a process of increasing the surface roughness of the water-degradable polymer film. Claim 8 A method for manufacturing a biodegradable label according to claim 7, wherein the process for increasing the surface roughness of the water-degradable polymer film comprises performing a process including one or more of the group consisting of an etching process, a polishing process, a wrapping process, and a blasting process on the water-degradable polymer film. Claim 9 A label manufactured by the method for manufacturing a biodegradable label of claim 1.
Citation Information
Patent Citations
Environment friendly label sheet for polyethyleneterephthalate bottle
KR1020130033634A
Plastic circulation system and method for manufacturing product based on biodegradable plastic
KR1020230081579A
Printable water-releasable single-sided adhesive label
KR102503832B1