Method for preparing oxide-based solid electrolyte powder
The production of oxide-based solid electrolyte powder using a specific precursor solution and high-temperature processing improves ionic conductivity and sintering density, addressing the limitations of existing oxide-based electrolytes and enhancing the performance and capacity of all-solid-state batteries.
Patent Information
- Application Number
- PCT/KR2024/005432
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2024-04-19
- Filing Date
- 2024-04-22
- Publication Date
- 2024-10-24
AI Technical Summary
Current oxide-based solid electrolytes in all-solid-state batteries have low ionic conductivity, limiting their application in small electronic devices where increased energy density and safety are required, and existing methods for improving conductivity are inefficient.
A method involving the production of oxide-based solid electrolyte powder using a precursor solution of Li2CO3, H3BO3, and Al2O3, which is vibrated to generate fine droplets, sprayed into a tube furnace at high temperatures, and collected to produce powder with a D50 of 2.0 μm or less, enhancing ionic conductivity and sintering density.
The method results in oxide-based solid electrolyte powder with improved ionic conductivity and sintering density, enabling increased battery capacity and energy density in all-solid-state batteries, while ensuring safety and reducing sintering temperatures, thus enhancing battery performance and lifespan.
Smart Images

Figure KR2024005432_24102024_PF_FP_ABST
Abstract
Description
Method for producing oxide-based solid electrolyte powder
[0001] The present invention relates to a method for producing an oxide-based solid electrolyte powder.
[0002] Recently, the use of secondary batteries has increased significantly in various fields, from IT devices such as mobile phones to electric vehicles and energy storage devices.
[0003] Lithium-ion batteries using liquid electrolytes are the most widely used secondary batteries, but liquid electrolytes have a risk of leakage when the battery is subjected to external impact, and therefore require additional components and devices to ensure safety.
[0004] Recently, active development of all-solid-state batteries using solid electrolytes has been underway to improve the safety of secondary batteries. Solid electrolytes for all-solid-state batteries include polymer electrolytes, oxide electrolytes, and sulfide electrolytes. Sulfide solid electrolytes have the highest ionic conductivity, but they have the problem of reacting with moisture to produce hydrogen sulfide gas. Polymer electrolytes offer the advantages of a relatively simple process and compatibility with existing lithium-ion battery processes, but their significantly low ionic conductivity is a drawback.
[0005] Oxide-based electrolytes offer superior safety compared to sulfide-based electrolytes, but their ionic conductivity is relatively low. Consequently, there is a growing demand for technologies that can improve the ionic conductivity of oxide-based solid electrolytes for use in all-solid-state batteries.
[0006] Meanwhile, all-solid-state batteries can be used as batteries for small electronic devices. For all-solid-state batteries to be used in small electronic devices, they must also be miniaturized. This requires improved energy density to increase battery capacity. As electronic devices become increasingly miniaturized, the demand for higher capacity all-solid-state batteries is also increasing.
[0007] The present invention is intended to solve the problems of the above-described prior art, and its purpose is to provide a method for producing an oxide solid electrolyte powder capable of improving the capacity of an all-solid-state battery.
[0008] In addition, the present invention also aims to provide a method for producing an oxide-based solid electrolyte powder capable of improving the ionic conductivity of the oxide-based solid electrolyte.
[0009] A representative configuration of the present invention to achieve the above purpose is as follows.
[0010] A method for manufacturing an oxide-based solid electrolyte powder according to one embodiment of the present invention comprises the steps of vibrating a precursor aqueous solution containing Li2CO3, H3BO3, Al2O3 and LiCl to generate fine droplets, spraying the fine droplets, heating the sprayed fine droplets to generate powder, and collecting the generated powder.
[0011] According to one embodiment of the present invention, in the step of spraying the fine droplets, the fine droplets can be sprayed into the interior of a tube furnace.
[0012] According to one embodiment of the present invention, in the step of generating the powder, the sprayed fine droplets can be heated to a temperature of 1,000°C or higher.
[0013] According to one embodiment of the present invention, in the step of collecting the powder, the powder can be collected through at least one of a bag filter and a cyclone.
[0014] The D50 of the powder produced by the method according to one embodiment of the present invention may be 2.0 μm or less.
[0015] In addition, other additional components may be further included within a range that does not impair the technical idea of the present invention, including the oxide solid electrolyte powder manufactured according to one embodiment of the present invention.
[0016] According to one embodiment of the present invention, the particle size of the oxide-based solid electrolyte powder can be manufactured to be small, thereby increasing the capacity of the all-solid-state battery by stacking more electrolyte layers within the all-solid-state battery of the same volume.
[0017] In addition, according to one embodiment of the present invention, the oxide-based solid electrolyte powder has a uniform particle size, thereby improving the sintered density and enhancing the ionic conductivity of the solid electrolyte.
[0018] FIG. 1 is a drawing schematically showing the configuration of an oxide-based solid electrolyte powder manufacturing device according to one embodiment of the present invention.
[0019] FIG. 2 is a flowchart exemplarily showing a process for manufacturing an oxide-based solid electrolyte powder according to one embodiment of the present invention.
[0020] Figure 3 is an electron microscope image showing the appearance of an oxide-based solid electrolyte powder according to one embodiment and a comparative example of the present invention.
[0021] Figure 4 is an electron microscope image showing the appearance of an oxide-based solid electrolyte powder after sintering according to one embodiment and a comparative example of the present invention.
[0022] FIG. 5 is a drawing schematically showing the cross-sectional structure of an all-solid-state battery manufactured using an oxide-based solid electrolyte powder according to one embodiment and a comparative example of the present invention.
[0023] [Explanation of symbols]
[0024] 100: Oxide-based solid electrolyte powder manufacturing device
[0025] 101: Injection tube
[0026] 103: Inlet valve
[0027] 105: Vibration device
[0028] 107: Gwansang-ro
[0029] 109: Capture Device
[0030] 111: Exhaust valve
[0031] Hereinafter, embodiments of the present invention will be described in detail with reference to the attached drawings. Detailed descriptions of previously known functions and configurations will be omitted if deemed likely to unnecessarily obscure the gist of the present invention. Furthermore, it should be noted that the following description relates only to one embodiment of the present invention and is not intended to limit the present invention.
[0032] The terms used in this invention are used solely to describe specific embodiments and are not intended to limit the invention. For example, a singular element should be understood to include plural elements, unless the context clearly indicates only a singular element.
[0033] As used herein, expressions such as “comprising” and the like should be understood as open-ended terms implying the possibility of including other embodiments, unless otherwise stated in the phrase or sentence in which the expression is included.
[0034] The size, thickness, position, etc. of each component shown in the drawings are arbitrarily shown for convenience of explanation, and therefore the present invention is not necessarily limited to what is shown. That is, it should be understood that the specific shapes, structures, and characteristics described in the specification may be changed and implemented from one embodiment to another without departing from the spirit and scope of the present invention, and the position or arrangement of individual components may also be changed without departing from the spirit and scope of the present invention.
[0035] Additionally, unless otherwise defined, all terms used in this invention, including technical or scientific terms, have the same meaning as commonly understood by those of ordinary skill in the art to which this invention pertains. Terms defined in commonly used dictionaries should be interpreted as having a meaning consistent with the contextual meaning of the relevant technology, and should not be interpreted in an unduly limiting or expansive manner unless explicitly defined otherwise herein.
[0036] Typically, an all-solid-state battery comprises a positive electrode, a negative electrode, and a solid electrolyte layer. The solid electrolyte layer is positioned between the positive electrode and the negative electrode and can be in contact with the positive electrode and the negative electrode, respectively. The positive electrode and the negative electrode may each have a positive electrode active material layer and a negative electrode active material layer, and the positive electrode active material layer and the negative electrode active material layer may each be in contact with a solid electrolyte layer. The positive electrode and the negative electrode may each be joined to the solid electrolyte layer by sintering. That is, the positive electrode, the negative electrode, and the solid electrolyte layer may be sintered as a single body.
[0037] The positive electrode, negative electrode, and solid electrolyte layers may each be formed into multiple layers to form an all-solid-state battery. Alternatively, the positive electrode, negative electrode, and solid electrolyte layers may be formed into a so-called laminated all-solid-state battery in which multiple layers are alternately laminated.
[0038] A solid electrolyte for an all-solid-state battery according to one embodiment of the present invention may have a boron oxide crystal structure, such as boracite. In one embodiment, the solid electrolyte for an all-solid-state battery may be formed of an oxide having a composition system of Li-B-Al-O-Cl. For example, the solid electrolyte for an all-solid-state battery may include Li2O, B2O3, Al2O3, and LiCl.
[0039] FIG. 1 is a drawing schematically showing the configuration of an oxide-based solid electrolyte powder manufacturing device according to one embodiment of the present invention, and FIG. 2 is an operational flowchart exemplarily showing a process for manufacturing an oxide-based solid electrolyte powder according to one embodiment of the present invention. Hereinafter, a method for manufacturing an oxide-based solid electrolyte powder according to one embodiment of the present invention will be described with reference to FIGS. 1 and 2.
[0040] According to one embodiment of the present invention, an oxide-based solid electrolyte powder can be manufactured by generating fine droplets of a precursor aqueous solution (S201), spraying the fine droplets (S203), heating the sprayed fine droplets (S205), and collecting the generated oxide solid electrolyte powder (S207).
[0041] First, in step (S201), the precursor solution is vibrated to generate fine droplets. Here, the precursor solution may include Li2CO3, H3BO3, Al2O3, and LiCl. Referring to FIG. 1, the precursor solution may be introduced into a vibration device (105) through an inlet pipe (101) to generate fine droplets. At this time, a carrier gas may be introduced into the vibration device (105) together with the precursor solution through an inlet valve (103). Thereafter, the precursor solution may be vibrated inside the vibration device (105) to generate fine droplets of the precursor solution. In one embodiment, the vibration device (105) may be an ultrasonic vibration device.
[0042] In step (S203), the previously generated fine droplets are sprayed. Referring to Fig. 1, the fine droplets inside the vibration device (105) can be transported and sprayed into the inside of the tube furnace (107) by a carrier gas.
[0043] In step (S205), the sprayed fine droplets are heated to produce a powder. Referring to FIG. 1, the interior of the tube furnace (107) can be heated to a high temperature to heat the sprayed fine droplets. At this time, the sprayed fine droplets undergo thermal decomposition by heating. Specifically, the nitride component in the fine droplets is converted to oxide, and the moisture within the fine droplets is evaporated, thereby forming a solid electrolyte powder in the form of solid fine particles.
[0044] According to one embodiment of the present invention, the sprayed fine droplets can be heated to a temperature of 1,000°C or higher. Accordingly, vitrification of the solid electrolyte powder produced through pyrolysis can be achieved.
[0045] In step (S207), the generated powder is collected. Referring to FIG. 1, the powder can be collected through a collection device (109) equipped with at least one of a bag filter and a cyclone. At this time, the carrier gas can be exhausted through an exhaust valve (111) connected to the collection device (109), and the solid electrolyte powder can be collected in the collection device (109).
[0046] According to one embodiment of the present invention, a fine spherical oxide-based solid electrolyte powder can be obtained, and the produced oxide-based solid electrolyte powder can have a uniform particle size distribution.
[0047]
[0048] Experimental example
[0049] Hereinafter, the effect of the manufacturing method according to an embodiment of the present invention will be specifically described by comparing an oxide-based solid electrolyte powder manufactured according to an embodiment of the present invention with an oxide-based solid electrolyte powder manufactured according to a conventional manufacturing method.
[0050] As an embodiment of the present invention, an oxide-based solid electrolyte powder having a composition of Li-B-Al-O-Cl was manufactured using a precursor aqueous solution containing Li2CO3, H3BO3, Al2O3, and LiCl according to the above-described method.
[0051] As a comparative example for the embodiment of the present invention, a solid electrolyte powder was prepared using a known melting method. Specifically, a precursor powder containing Li2CO3, H3BO3, Al2O3, and LiCl was prepared, the precursor powders were mixed, placed in an Al crucible, melted at about 1,000°C for 30 minutes, and the melt was rapidly cooled on a brass roller, then crushed and sieved to obtain a solid electrolyte powder having a size of 10 μm or less.
[0052] Figure 3 is an electron microscope image showing the appearance of an oxide-based solid electrolyte powder according to one embodiment of the present invention and a comparative example. Figure 3 (a) shows an electron microscope image of an oxide-based solid electrolyte powder according to a comparative example of the present invention, and Figure 3 (b) shows an electron microscope image of an oxide-based solid electrolyte powder according to one embodiment of the present invention.
[0053] Referring to FIG. 3, it is confirmed that the powder manufactured according to one embodiment of the present invention has a D50 of 1.0 ㎛ or less, and a smaller particle size and a more even particle size distribution than the comparative example having a D50 of about 3 ㎛. In addition, it is confirmed that the oxide-based solid electrolyte powder according to the comparative example has a rough particle surface and an irregular shape, whereas the oxide-based solid electrolyte powder according to one embodiment of the present invention is formed of spherical particles.
[0054] In this way, the oxide-based solid electrolyte powder manufactured through the manufacturing method according to one embodiment of the present invention has a uniform particle size distribution and a spherical particle shape, enabling the fundamental removal of large particles and significantly improving defects due to short-circuiting of the solid electrolyte layer during the manufacture of an all-solid-state battery.
[0055] Figure 4 is an electron microscope image showing the appearance after sintering of oxide-based solid electrolyte powders according to one embodiment and a comparative example of the present invention. Figure 4 (a) shows the appearance after sintering of oxide-based solid electrolyte powders according to a comparative example of the present invention, that is, manufactured according to a conventional technique (e.g., a melting method), and Figure 4 (b) shows the appearance after sintering of oxide-based solid electrolyte powders manufactured according to one embodiment of the present invention.
[0056] Referring to FIG. 4, it is confirmed that the oxide-based solid electrolyte powder manufactured according to one embodiment of the present invention has a denser sintered structure compared to the oxide-based solid electrolyte powder manufactured according to the conventional technique. As such, the oxide-based solid electrolyte powder manufactured according to one embodiment of the present invention has an increased sintered density, which can lead to an improvement in ionic conductivity. Therefore, the solid electrolyte manufactured using the oxide-based solid electrolyte powder manufactured according to one embodiment of the present invention can have superior battery characteristics compared to an all-solid-state battery manufactured by a conventional method.
[0057] Table 1 shows the results of measuring the sintered density and ionic conductivity of the oxide-based solid electrolyte powder according to one embodiment of the present invention and a comparative example. Referring to Table 1, it can be confirmed that the oxide-based solid electrolyte powder according to one embodiment of the present invention has improved sintered density and ionic conductivity compared to the oxide-based solid electrolyte powder according to the comparative example.
[0058] Sintered density (g / cm) 3 ) Ionic conductivity (S / Cm) Comparison example 1.95 ~ 2.05 1.0 ×10 -5 Less than 2.10 ~ 2.20 1.5 ~ 2.0 ×10 -5
[0059] FIG. 5 is a drawing schematically showing the cross-sectional structure of an all-solid-state battery manufactured from an oxide-based solid electrolyte powder according to one embodiment and a comparative example of the present invention. In manufacturing an oxide-based ultra-small multilayer all-solid-state battery (MLCB: Multi-Layer Ceramic Battery) for substrate mounting, the number of solid electrolyte layers laminated can be determined depending on the thickness of the sheets constituting the solid electrolyte layers. That is, as the thickness of each sheet becomes thinner, more solid electrolyte layers can be laminated within the same volume.
[0060] As described above, since the oxide-based solid electrolyte powder according to one embodiment of the present invention has a uniform particle size distribution and fine spherical particles, the thickness of each sheet constituting the solid electrolyte layer can be made thin to 10 μm or less. Therefore, the all-solid-state battery ((b) of FIG. 5) manufactured with the oxide-based solid electrolyte powder according to one embodiment of the present invention can increase the number of stacked solid electrolyte layers compared to the all-solid-state battery ((a) of FIG. 5) according to the comparative example. This leads to an increase in the energy density of the all-solid-state battery, which can increase the capacity of the battery.
[0061] Meanwhile, it was confirmed that the oxide-based solid electrolyte powder according to an embodiment of the present invention had a vitrification temperature reduced by 15 to 20°C and a crystallization temperature also reduced by 7 to 10°C compared to the oxide-based solid electrolyte powder according to a comparative example. Therefore, the oxide-based solid electrolyte powder according to an embodiment of the present invention can suppress the interface reaction between the electrolyte and the active material by lowering the sintering temperature, thereby improving the lifespan of the all-solid-state battery.
[0062] Although the present invention has been described above with specific details such as specific components and limited examples, the above examples are provided only to help a more general understanding of the present invention, and the present invention is not limited thereto, and those with ordinary knowledge in the technical field to which the present invention pertains can make various modifications and variations based on this description.
[0063] Therefore, the idea of the present invention should not be limited to the embodiments described above, and all things that are modified equally or equivalently to the claims described below as well as the claims are considered to fall within the scope of the idea of the present invention.
Claims
1. A method for manufacturing an oxide-based solid electrolyte powder, A step of generating microdroplets by vibrating a precursor aqueous solution containing Li2CO3, H3BO3, Al2O3 and LiCl, The step of spraying the above fine droplets, A step of heating the sprayed fine droplets to produce powder, and A step of capturing the generated powder including, method.
2. In paragraph 1, A method in which, in the step of spraying the above fine droplets, the above fine droplets are sprayed into the interior of a tube furnace.
3. In paragraph 1, A method in which, in the step of generating the above powder, the sprayed fine droplets are heated to a temperature of 1,000°C or higher.
4. In paragraph 1, A method in which, in the step of collecting the powder, the powder is collected through at least one of a bag filter and a cyclone.
5. In paragraph 1, A method wherein the D50 of the generated powder is 2.0㎛ or less.
6. Oxide-based solid electrolyte powder manufactured by the manufacturing method according to Article 1.
Citation Information
Patent Citations
Lithium manganese composite oxide granule secondary particle and method for producing the same and application thereof
JP2004083388A
Fabrication method of solid electrolyte powder and solid electrolyte using the same
KR1020100033827A
Lithium manganes based cathode material and preparation method of thereof
KR1020130117338A
Nonvolatile memory device and latch comprising the same
KR102412818B1
KR20210106591A