MEMS sensor and preparation method therefor
By using interval-set movable mass structure and DRIE process in MEMS sensors, the structural problems caused by multi-epitaxial growth of the equipment layer are solved, and higher sensitivity and driving force are achieved, improving the performance of the sensor and the complexity of the mold design are improved. .
Patent Information
- Application Number
- PCT/CN2023/098007
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-24
- Filing Date
- 2023-06-02
- Publication Date
- 2024-11-28
AI Technical Summary
When implementing multi-layer equipment structures, the multi-epitaxial growth of the equipment layer requires a high budget and may lead to problems such as structural warping, limiting the improvement of performance, reliability and mold size.
Using a spaced movable mass structure, the bottom electrode layer is supported by anchor points and a preset gap is formed between the top electrode layer. The DRIE process is used to etch the movable mass of different heights to realize the equipment layer. Multi-layer height structure.
Improves sensor sensitivity and driving force, allows for more complex designs and miniaturization of molds, enhances signal-to-noise ratio and anti-interference capabilities, and achieves higher accuracy and audio performance.
Smart Images

Figure CN2023098007_28112024_PF_FP_ABST
Abstract
Description
A MEMS sensor and its preparation method Technical Field
[0001] The present invention relates to the technical field of micro-electromechanical systems, in particular to a MEMS sensor and a preparation method thereof. Background Art
[0002] Many current designs of MEMS sensors, such as microphones, pressure sensors, and inertial sensors, use a single device layer and one or more sacrificial layers. Releasing the sacrificial layer allows the device layer to move. Without increasing the mold size, single-piece device layer designs are approaching limitations in performance, robustness, and sensibility. Therefore, the demand for dual-layer or multi-layer device structures is increasing.
[0003] In existing technologies, one possible process involves multi-epitaxial growth of the device layer, while other processes such as chemical vapor deposition (CVD) and silicon dioxide etching are used to achieve the dual device layer. However, multi-epitaxial growth of the device layer requires a very high budget and may cause unexpected effects such as warping. Technical issues
[0004] The object of the present invention is to provide a MEMS sensor and a method for manufacturing the same to solve the technical problems in the prior art, which can allow the design of multi-layer devices and further improve performance, reliability, complexity and mold size. Technical Solutions
[0005] The present invention provides a MEMS sensor, comprising:
[0006] A bottom electrode layer and a top electrode layer are spaced apart, with a cavity formed between the bottom electrode layer and the top electrode layer;
[0007] A device layer is housed in the cavity, and the device layer includes a plurality of movable mass blocks arranged at intervals. The movable mass blocks are supported on the bottom electrode layer through anchor points. A preset gap is formed between the movable mass blocks and the top electrode layer, and the preset gaps formed by different movable mass blocks are different.
[0008] A MEMS sensor as described above, wherein preferably, the plurality of movable mass blocks include a first movable mass block, a second movable mass block and a third movable mass block, the second movable mass block is located between the first movable mass block and the third movable mass block, a first preset gap is formed between the first movable mass block and the top electrode layer, a second preset gap is formed between the second movable mass block and the top electrode layer, and a third preset gap is formed between the third movable mass block and the top electrode layer, and there are differences in the height values of the first preset gap, the second preset gap and the third preset gap.
[0009] In the MEMS sensor as described above, preferably, the height value of the first preset gap, the height value of the third preset gap, and the height value of the second preset gap increase in sequence.
[0010] In the MEMS sensor as described above, preferably, the height value of the first preset gap is the same as the height value of the third preset gap, and the height value of the second preset gap is greater than the height values of the first preset gap and the third preset gap.
[0011] In the MEMS sensor as described above, preferably, the bottoms of the first movable mass block and the third movable mass block are connected to one anchor point, and the bottom of the second movable mass block is connected to two anchor points.
[0012] In the MEMS sensor as described above, preferably, a plurality of openings are formed on the top electrode layer, and the openings are distributed at intervals along the radial direction of the top electrode layer.
[0013] In a second aspect, the present invention further provides a method for preparing a MEMS sensor, which is used to prepare the aforementioned MEMS sensor, comprising the following steps:
[0014] Step S1: forming a bottom electrode layer, a sacrificial layer, a device layer and a top electrode layer in sequence from bottom to top;
[0015] Step S2: etching the device layer to form a plurality of movable mass blocks spaced apart from each other;
[0016] Step S3: releasing the sacrificial layer in the device layer.
[0017] In the method for preparing a MEMS sensor as described above, preferably, step S1 includes:
[0018] Step 101: forming a bottom electrode layer;
[0019] Step 102: forming a sacrificial layer on the bottom electrode layer, and etching a top surface of the sacrificial layer to form a stepped interface and a plurality of grooves;
[0020] Step 103: forming a device layer on the sacrificial layer, wherein the movable mass block of the device layer is stacked on the step interface, and the anchor point of the device layer is formed in the groove;
[0021] Step 104: forming the top electrode layer and forming a plurality of openings on the top electrode layer.
[0022] In the method for preparing a MEMS sensor as described above, preferably, in step S2, the device layer is etched by a DRIE process to form a plurality of movable mass blocks arranged at intervals.
[0023] In the method for preparing a MEMS sensor as described above, preferably, the material of the device layer is lead zirconium titanate, aluminum nitride, barium titanate or a mixture of the above materials. Beneficial effects
[0024] Compared with the prior art, the present invention forms a differential output electrical signal by setting the device layer as several movable mass blocks arranged at intervals. The preset gaps formed by different movable mass blocks are different. This structure allows greater design flexibility and provides the sensor with higher sensitivity and greater driving force. It can also achieve a reduction in mold size and realize a more complex design with higher precision and miniaturization. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] FIG1 is a cross-sectional schematic diagram of a MEMS sensor according to a first embodiment of the present invention;
[0026] 2a-2c are flow charts of the preparation of the MEMS sensor according to the first embodiment of the present invention;
[0027] FIG3 is a cross-sectional schematic diagram of a MEMS sensor according to a second embodiment of the present invention;
[0028] 4a-4c are flowcharts of the preparation of the MEMS sensor according to the second embodiment of the present invention.
[0029] Explanation of the accompanying drawings: 1-bottom electrode layer, 2-top electrode layer, 21-opening, 3-cavity, 4-device layer, 41-movable mass block, 411-first movable mass block, 412-first preset gap, 413-second movable mass block, 414-second preset gap, 415-third movable mass block, 416-third preset gap, 42-anchor point, 5-sacrificial layer, 51-groove. Best Mode for Carrying Out the Invention
[0030] The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and are not to be construed as limiting the present invention.
[0031] As shown in FIG1 and FIG3 , an embodiment of the present invention provides a MEMS sensor, including:
[0032] The bottom electrode layer 1 and the top electrode layer 2 are spaced apart, and a cavity 3 is formed between the bottom electrode layer 1 and the top electrode layer 2 .
[0033] The device layer 4 is housed in the cavity 3, and at least a portion of the device layer 4 is conductive, so that a capacitor is formed between the device layer 4 and the top electrode layer 2 opposite to the device layer 4. Specifically, when the MEMS sensor is used as a microphone, when the microphone is powered on, the top electrode layer 2 and the device layer 4 will carry charges of opposite polarities, thereby forming a capacitor. When the device layer 4 vibrates under the action of sound waves, the distance between the top electrode layer 2 and the device layer 4 will change, thereby causing the capacitance of the capacitor to change, and then converting the sound wave signal into an electrical signal, thereby realizing the corresponding function of the microphone.
[0034] In the embodiment provided in the present application, the device layer 4 includes a plurality of movable mass blocks 41 arranged at intervals. The movable mass blocks 41 are supported on the bottom electrode layer 1 by anchor points 42. A preset gap is formed between the movable mass blocks 41 and the top electrode layer 2. The preset gaps formed by different movable mass blocks 41 are different, thereby forming a differential output electrical signal. This structure allows for greater design flexibility and provides the sensor with higher sensitivity and greater driving force. It can also achieve a reduction in mold size while achieving a more complex design with higher precision and miniaturization. Specifically, when a MEMS sensor is used in a microphone, it can enable the capacitive microphone to obtain a higher signal-to-noise ratio, improve the ability to suppress linear distortion, and at the same time improve the microphone's anti-interference ability, making the signal transmission distance longer and the microphone's audio performance better.
[0035] Furthermore, the several movable mass blocks 41 include a first movable mass block 411, a second movable mass block 413 and a third movable mass block 415. The second movable mass block 413 is located between the first movable mass block 411 and the third movable mass block 415. A first preset gap 412 is formed between the first movable mass block 411 and the top electrode layer 2, a second preset gap 414 is formed between the second movable mass block 413 and the top electrode layer 2, and a third preset gap 416 is formed between the third movable mass block 415 and the top electrode layer 2. There are differences in the height values of the first preset gap 412, the second preset gap 414 and the third preset gap 416.
[0036] A first capacitor is formed between the first movable mass block 411 and the top electrode layer 2. When the height value of the first preset gap 412 formed between the first movable mass block 411 and the top electrode layer 2 changes, the capacitance of the first capacitor changes accordingly. A second capacitor is formed between the second movable mass block 413 and the top electrode layer 2. When the height value of the second preset gap 414 formed between the second movable mass block 413 and the top electrode layer 2 changes, the capacitance of the second capacitor changes accordingly. A third capacitor is formed between the third movable mass block 415 and the top electrode layer 2. When the height value of the third preset gap 416 formed between the third movable mass block 415 and the top electrode layer 2 changes, the capacitance of the third capacitor changes accordingly. The electrical signals output by the first capacitor, the second capacitor and the third capacitor form a differential output, and the sensor has higher sensitivity.
[0037] Two embodiments are listed below to provide a more detailed description of the MEMS sensor provided by the present invention when used as a microphone. Those skilled in the art will appreciate that variations can be made based on these embodiments, all of which fall within the scope of protection of the present invention.
[0038] Example 1
[0039] As shown in Figure 1, in this embodiment, the height value of the first preset gap 412, the height value of the third preset gap 416, and the height value of the second preset gap 414 increase sequentially. Since the value of the capacitor is proportional to the facing area between the two plates of the capacitor and inversely proportional to the distance between the two plates of the capacitor, that is, C = kε0εrS / d, k is a constant, ε0 is a constant, and εr is a constant. After the capacitive microphone is manufactured, the value of ε0εr is fixed, S is the area directly opposite to the two plates of the capacitor, d is the distance between the two plates, and when the surfaces of the first movable mass block 411, the second movable mass block 413 and the third movable mass block 415 are roughly the same, the larger the height value of the preset gap, the smaller the capacitance. In this embodiment, the initial capacitance value of the first capacitor formed by the first movable mass block 411 is the largest, the initial capacitance value of the third capacitor formed by the third movable mass block 415 is the second largest, and the initial capacitance value of the third capacitor formed by the second movable mass block 413 is the smallest. The second movable mass block 413 is located in the middle of the device layer 4, which is the part with the most severe deformation, thereby providing higher sensitivity and greater driving force.
[0040] In this embodiment, as shown in Figure 1, the bottom of the first movable mass block 411 and the third movable mass block 415 are connected to an anchor point 42, and the bottom of the second movable mass block 413 is connected to two anchor points 42. The first movable mass block 411, the second movable mass block 413, the third movable mass block 415 and the anchor points 42 can all be made of conductive materials.
[0041] Since the bottom support of the second movable mass block 413 has two anchor points 42 set at intervals, the movable part of the second movable mass block 413 is located between the two anchor points 42. When the device layer 4 vibrates under the action of sound waves, the movable part of the second movable mass block 413 forms a bending deformation, thereby changing the distance between it and the top electrode layer 2, and the capacitance of the second capacitor changes accordingly, forming a differential output electrical signal between the first capacitor, the second capacitor and the third capacitor.
[0042] In a feasible embodiment, when the device layer 4 vibrates under the action of sound waves, the first movable mass block 411 and the third movable mass block 415 can also pivot around the anchor point 42, so that one end of the first movable mass block 411 and the third movable mass block 415 tilts upward and the other end tilts downward, thereby changing the distance between the top electrode layer 2, and the capacitance of the first capacitor and the third capacitor changes accordingly, forming a differential output electrical signal.
[0043] In this embodiment, a plurality of openings 21 are formed on the top electrode layer 2 . The openings 21 are spaced apart along the radial direction of the top electrode layer 2 . The openings 21 are evenly distributed to provide channels for sound waves to pass through and provide structural support for subsequent molding processes.
[0044] 2a-2c are flow charts of a MEMS sensor fabrication process according to an embodiment of the present invention. The MEMS sensor fabrication process includes the following steps:
[0045] Step S1: As shown in FIG. 2 a , a bottom electrode layer 1 , a sacrificial layer 5 , a device layer 4 , and a top electrode layer 2 are sequentially formed from bottom to top. In a feasible embodiment, the steps include:
[0046] Step 101: A bottom electrode layer 1 is formed on a silicon substrate by electron beam lift-off or magnetron sputtering. The bottom electrode layer 1 is connected to a bottom electrode pad (not shown) via a bottom electrode lead (not shown). The material of the bottom electrode layer 1 can be one or more of Al, Mo, W, Pt, Cu, Ag, Au, ZrN, or other materials with good electrical conductivity.
[0047] Step 102: forming a sacrificial layer 5 on the bottom electrode layer 1, and etching the top surface of the sacrificial layer 5 to form a stepped interface and a plurality of grooves 51. The material of the sacrificial layer 5 can be PSG. A patterned hard mask is formed on the sacrificial layer 5, and the grooves 51 are etched on the sacrificial layer 5 by dry etching or wet etching.
[0048] Step 103: Forming a device layer 4 on the sacrificial layer 5. The material of the device layer 4 is lead zirconium titanate, aluminum nitride, barium titanate, or a mixture of these materials. The movable mass 41 of the device layer 4 is stacked on the stepped interface to form a device layer 4 with a height difference. The anchor point 42 of the device layer 4 is formed in the groove 51 and fills the groove 51 until it forms an electrical coupling with the bottom electrode layer 1.
[0049] Step 104: forming a top electrode layer 2, which is connected to a top electrode pad (not shown) via a bottom electrode lead (not shown). The material of the top electrode layer 2 may be one or more of Al, Mo, W, Pt, Cu, Ag, Au, and ZrN, or other materials with good conductive properties. A patterned hard mask is formed on the top electrode layer 2, and an opening 21 is formed by etching the top electrode layer 2 by dry etching or wet etching.
[0050] Step S2: As shown in Figure 2b, the device layer 4 is etched to form a number of movable mass blocks 41 spaced apart. Preferably, the device layer 4 is etched by a DRIE (deep reactive ion etching) process. By using this innovation of DRIE to isolate and create movable mass blocks at different heights, a device layer with a multi-layer height structure can be achieved, allowing greater design flexibility, providing higher sensitivity and greater driving force for the sensor, and also achieving a reduction in mold size while achieving more complex designs with higher precision and miniaturization. The same DRIE process steps can also be used to pattern the device layer while avoiding an increase in the number of thermal cycles. Since DRIE creates a device step height, the gap between the electrodes can also be changed, which is particularly useful for sensors using a parallel plate electrode structure. The sacrificial layer 5 can be used as a hard mask to prevent the DRIE process from etching the bottom electrode layer 1.
[0051] Specifically, the several movable mass blocks 41 include a first movable mass block 411, a second movable mass block 413 and a third movable mass block 415. A first preset gap 412 is formed between the first movable mass block 411 and the top electrode layer 2, a second preset gap 414 is formed between the second movable mass block 413 and the top electrode layer 2, and a third preset gap 416 is formed between the third movable mass block 415 and the top electrode layer 2. The height values of the first preset gap 412, the third preset gap 416 and the second preset gap 414 increase sequentially.
[0052] Step S3: Referring to FIG. 2 c , the sacrificial layer 5 in the device layer 4 is released to allow the device layer 4 to move.
[0053] Example 2
[0054] As shown in Figure 3, the difference between this embodiment and Example 1 is that the height value of the first preset gap 412 is the same as the height value of the third preset gap 416, and the height value of the second preset gap 414 is greater than the height values of the first preset gap 412 and the third preset gap 416. In this embodiment, the initial capacitance value of the first capacitor formed by the first movable mass block 411 is the same, and the initial capacitance value of the third capacitor formed by the second movable mass block 413 is relatively small. The second movable mass block 413 is located in the middle of the device layer 4, which is the part with the most severe deformation, thereby providing higher sensitivity and greater driving force.
[0055] 4a-4c are flow charts of a MEMS sensor fabrication process according to an embodiment of the present invention. The MEMS sensor fabrication process includes the following steps:
[0056] Step S1: Referring to FIG. 4 a , a bottom electrode layer 1 , a sacrificial layer 5 , a device layer 4 , and a top electrode layer 2 are sequentially formed from bottom to top. In a feasible embodiment, the steps include:
[0057] Step 101: A bottom electrode layer 1 is formed on a silicon substrate by electron beam lift-off or magnetron sputtering. The bottom electrode layer 1 is connected to a bottom electrode pad (not shown) via a bottom electrode lead (not shown). The material of the bottom electrode layer 1 can be one or more of Al, Mo, W, Pt, Cu, Ag, Au, ZrN, or other materials with good electrical conductivity.
[0058] Step 102: forming a sacrificial layer 5 on the bottom electrode layer 1, and etching the top surface of the sacrificial layer 5 to form a stepped interface and a plurality of grooves 51. The material of the sacrificial layer 5 can be PSG. A patterned hard mask is formed on the sacrificial layer 5, and the grooves 51 are etched on the sacrificial layer 5 by dry etching or wet etching.
[0059] Step 103: Forming a device layer 4 on the sacrificial layer 5. The material of the device layer 4 is lead zirconium titanate, aluminum nitride, barium titanate, or a mixture of these materials. The movable mass 41 of the device layer 4 is stacked on the stepped interface to form a device layer 4 with a height difference. The anchor point 42 of the device layer 4 is formed in the groove 51 and fills the groove 51 until it forms an electrical coupling with the bottom electrode layer 1.
[0060] Step 104: forming a top electrode layer 2, which is connected to a top electrode pad (not shown) via a bottom electrode lead (not shown). The material of the top electrode layer 2 may be one or more of Al, Mo, W, Pt, Cu, Ag, Au, and ZrN, or other materials with good conductive properties. A patterned hard mask is formed on the top electrode layer 2, and an opening 21 is formed by etching the top electrode layer 2 by dry etching or wet etching.
[0061] Step S2: As shown in Figure 4b, the device layer 4 is etched to form a number of movable mass blocks 41 spaced apart. Preferably, the device layer 4 is etched by a DRIE (deep reactive ion etching) process. By using this innovation of DRIE to isolate and create movable mass blocks at different heights, a device layer with a multi-layer height structure can be achieved, allowing greater design flexibility, providing higher sensitivity and greater driving force for the sensor, and also achieving a reduction in mold size while achieving more complex designs with higher precision and miniaturization. The same DRIE process steps can also be used to pattern the device layer while avoiding an increase in the number of thermal cycles. Since DRIE creates a device step height, the gap between the electrodes can also be changed, which is particularly useful for sensors using a parallel plate electrode structure. The sacrificial layer 5 can be used as a hard mask to prevent the DRIE process from etching the bottom electrode layer 1.
[0062] Specifically, the several movable mass blocks 41 include a first movable mass block 411, a second movable mass block 413 and a third movable mass block 415. A first preset gap 412 is formed between the first movable mass block 411 and the top electrode layer 2, a second preset gap 414 is formed between the second movable mass block 413 and the top electrode layer 2, and a third preset gap 416 is formed between the third movable mass block 415 and the top electrode layer 2. The height value of the first preset gap 412 is the same as the height value of the third preset gap 416, and the height value of the second preset gap 414 is greater than the height values of the first preset gap 412 and the third preset gap 416.
[0063] Step S3: Referring to FIG. 4 c , the sacrificial layer 5 in the device layer 4 is released to allow the device layer 4 to move.
[0064] The above describes in detail the structure, features and effects of the present invention based on the embodiments shown in the drawings. The above is only a preferred embodiment of the present invention, but the scope of implementation of the present invention is not limited to what is shown in the drawings. Any changes made in accordance with the concept of the present invention, or modifications to equivalent embodiments with equivalent changes, which do not exceed the spirit covered by the description and drawings, should be within the scope of protection of the present invention.
Claims
1. A MEMS sensor, It is characterized in that include: A bottom electrode layer and a top electrode layer are arranged at intervals, and a cavity is formed between the bottom electrode layer and the top electrode layer; The device layer is accommodated in the cavity, and the device layer includes a plurality of movable mass blocks arranged at intervals. The movable mass blocks are supported on the bottom electrode layer through anchor points. A preset gap is formed between the movable mass blocks and the top electrode layer. There are differences in the preset gaps formed by different movable mass blocks.
2. The MEMS sensor according to claim 1, Features: The several movable mass blocks include a first movable mass block, a second movable mass block and a third movable mass block, the second movable mass block is located between the first movable mass block and the third movable mass block, a first preset gap is formed between the first movable mass block and the top electrode layer, a second preset gap is formed between the second movable mass block and the top electrode layer, and a third preset gap is formed between the third movable mass block and the top electrode layer, and there are differences in height values of the first preset gap, the second preset gap and the third preset gap.
3. The MEMS sensor according to claim 2, Features: The height value of the first preset gap, the height value of the third preset gap, and the height value of the second preset gap increase in sequence.
4. The MEMS sensor according to claim 2, Features: The height value of the first preset gap is the same as the height value of the third preset gap, and the height value of the second preset gap is greater than the height values of the first preset gap and the third preset gap.
5. The MEMS sensor according to claim 2, Features: The bottom of the first movable mass block and the third movable mass block is connected to an anchor point, and the bottom of the second movable mass block is connected to two anchor points.
6. The MEMS sensor according to claim 1, Features: A plurality of openings are formed on the top electrode layer, and the openings are distributed at intervals along the radial direction of the top electrode layer.
7. A method for preparing a MEMS sensor, for preparing the MEMS sensor according to any one of claims 1 to 6, It is characterized in that The following steps are involved: Step S1: forming a bottom electrode layer, a sacrificial layer, a device layer and a top electrode layer in sequence from bottom to top; Step S2: etching the device layer to form a plurality of movable mass blocks arranged at intervals; Step S3: releasing the sacrificial layer in the device layer.
8. The method for preparing a MEMS sensor according to claim 7, Features: The step S1 includes: Step 101: forming a bottom electrode layer; Step 102: forming a sacrificial layer on the bottom electrode layer, and etching a top surface of the sacrificial layer to form a stepped interface and a plurality of grooves; Step 103: forming a device layer on the sacrificial layer, wherein the movable mass block of the device layer is stacked on the step interface, and the anchor point of the device layer is formed in the groove; Step 104: Form the top electrode layer, and form a plurality of openings on the top electrode layer.
9. The method for preparing a MEMS sensor according to claim 7, Features: In the step S2, the device layer is etched by a DRIE process to form a plurality of movable mass blocks arranged at intervals.
10. The method for preparing a MEMS sensor according to claim 7, Features: The material of the device layer is lead zirconate titanate, aluminum nitride, barium titanate or a mixture of the above materials.
Citation Information
Patent Citations
Mems tunable device
CN101288137A
Differential MEMS (Micro-electromechanical Systems) capacitive microphone and preparation method thereof
CN102457801A
Functional device, electronic apparatus, and moving object
CN104345173A
Flexible multi-range capacitive-type pressure sensor and preparation method and application thereof
CN109387348A
Variable capacitor, package provided therewith, and method for manufacturing the same
JP2004172504A