Method for manufacturing cleaning tool with surface roughness by cutting bubbles
The method of processing konjac powder with a foaming agent and controlled steam heating and freezing creates cleaning tools with adjustable surface roughness and pore size, addressing skin irritation and environmental issues, and offering enhanced cleaning efficacy and longevity.
Patent Information
- Application Number
- PCT/KR2024/006893
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-31
- Filing Date
- 2024-05-22
- Publication Date
- 2024-12-05
AI Technical Summary
Conventional cleaning tools made from chemical fibers or cotton often cause skin irritation, fluffing, tearing, and environmental pollution, and lack differentiated cleaning power due to uncontrolled surface roughness and pore size.
A method involving konjac powder mixed with a foaming agent and purified water, whipped to generate bubbles, then processed through steam heating and freezing to control bubble size and surface roughness, resulting in konjac pads, puffs, and towels with adjustable pore size and surface texture for specific cleaning applications.
The method produces cleaning tools with controlled surface roughness and pore size, providing superior cleaning power and skin benefits by preventing irritation and extending product lifespan, while being environmentally friendly.
Smart Images

Figure KR2024006893_05122024_PF_FP_ABST
Abstract
Description
Method for manufacturing a cleaning tool having a rough surface by cutting bubbles
[0001] The present invention relates to a method for manufacturing a cleaning tool by controlling the amount of bubbles by whipping a konjac mixture, controlling the size of bubbles according to bubble expansion by steam heating, determining the size of pores according to the use of the pad, puff, towel, etc., and cutting the bubbles to differentiate the surface roughness.
[0002] Typically, we use towels or sponges to cleanse our skin or face. Most towels and sponges are made from chemically-based fibers. Furthermore, cotton, cotton pads, non-woven fabrics, or other chemically-based fibers used in skin toners, facial cleansers, and partial massage packs can cause problems like pilling, tearing, physical skin irritation, and adverse skin reactions. Furthermore, they can be made of materials that don't decompose easily, potentially contributing to environmental pollution.
[0003] To address these issues, sponges and gauze products made from natural ingredients for cleansing and cleansing the skin are being released. However, sponges have been plagued by issues such as shrinking or losing their shape over time, remaining wet without penetrating, and producing less foam. Furthermore, they have also been plagued by shorter replacement cycles.
[0004] As a prior art, the method for manufacturing a konjac sponge of Patent Document 1 had a problem in that it did not control the size of the pores or the roughness of the surface, and thus did not differentiate the subdivision and cleaning power according to the intended use.
[0005] The present invention is intended to solve the above problem, and the purpose is to control the amount of air bubbles by whipping time of a konjac mixture with a foaming agent added in a kneader, and to control the size of the air bubbles according to the expansion of the air bubbles by steam heating, thereby manufacturing konjac pads, puffs, towels, etc. as cleaning tools with different pore sizes and surface roughness according to their intended use.
[0006] In order to achieve the above object, the present invention comprises the steps of: (a) adding a konjac mixture, which is a mixture of konjac powder with a viscosity of 30,000 to 35,000 mPa.s and purified water at a certain ratio, to a kneader and whipping the mixture at a maximum speed of 360 rpm for 8 to 10 seconds or a minimum speed of 166 rpm for 50 seconds to generate air bubbles; (b) adding the konjac mixture, in which air bubbles are generated by the whipping, to a dispensing machine and then putting the mixture into a mold of a certain shape and form and maturing it at 7 to 5°C for 12 to 15 hours; (c) adding the mold into which the maturing konjac mixture has been added to a steam heater and heating it for 50 to 70 minutes by applying steam at a certain temperature; (d) heating the mold into which the konjac mixture has been added to steam and then cooling it at room temperature for 3 to 5 hours; (e) a step of placing the mold containing the konjac mixture into a freezer and rapidly freezing it at -30°C for 2 hours when it has cooled; (f) a step of rapidly freezing the mold containing the konjac mixture and then maintaining it frozen at -7°C for 24 hours in a freezer; (g) a step of taking out the frozen mold and thawing it for 12 hours; (h) a step of separating the konjac mixture from the thawed mold, placing it into a freezer, and maintaining it again frozen at -7°C for 24 hours; (i) a step of cutting the frozen konjac mixture into a washing tool with a cutter into a certain thickness and classifying it according to the roughness of the surface; (j) a step of placing the classified washing tool into a freezer and freeze-drying it at -7°C for 72 hours; (k) a step of taking out the freeze-dried washing tool and washing it 2 to 3 times; (l) a step of placing the washed washing tool into a freeze-dryer and freeze-drying it for 12 to 18 hours; (m) It is characterized by providing a method for manufacturing a cleaning tool having a surface roughness by cutting bubbles, including a step of packaging the freeze-dried cleaning tool by classifying it according to use, thickness, and size.
[0007] Additionally, in the present invention, the konjac powder and purified water can be mixed in a ratio of 1:16, and the purified water can be mixed with water in a ratio of 1:20.
[0008] In addition, in the present invention, when whipping the konjac mixture in the kneader, a pack pad as a cleaning tool may be whipped at 360 rpm for 8 to 10 seconds and then whipped at 166 rpm for 50 seconds, a toner pad as a cleaning tool may be whipped at 360 rpm for 15 to 18 seconds and then whipped at 166 rpm for 50 seconds, and a cleansing pad, puff, or towel as a cleaning tool may be whipped at 360 rpm for 20 to 25 seconds and then whipped at 166 rpm for 50 seconds.
[0009] In addition, in the present invention, when the mold into which the konjac mixture is introduced is steam-heated with a steam heater, the thickness of the pack pad as a cleaning tool is 0.5 to 1 mm, the bubble diameter is 0.3 to 0.8 mm, and the heating temperature is 80 to 90°C, the thickness of the toner pad as a cleaning tool is 1.2 to 1.5 mm, the bubble diameter is 1.0 to 1.3 mm, and the heating temperature is 90 to 100°C, the thickness of the cleansing pad as a cleaning tool is 2.0 to 3.0 mm, the bubble diameter is 1.5 to 2.0 mm, and the heating temperature is 100 to 110°C, the thickness of the cleansing puff as a cleaning tool is 5.0 to 15.0 mm, the bubble diameter is 1.5 to 3.0 mm, and the heating temperature is 100 to 110°C, and the thickness of the cleansing towel as a cleaning tool is The bubble diameter is 1.5 to 3.0 mm, 5.0 to 8.0 mm, and the heating temperature can be 100 to 110°C.
[0010] Additionally, in the present invention, the mold may be formed into a cylindrical or polygonal columnar shape.
[0011] According to the present invention, the amount of air bubbles can be controlled by the whipping speed and time of the konjac mixture kneaded using konjac powder as the main ingredient, the size of the air bubbles can be controlled by the expansion of the air bubbles formed by steam heating, and excellent cleansing power is exhibited according to the roughness of the surface by cutting countless formed air bubbles, and by providing them as cleansing tools for packs, toners, cleansing, puffs, towels, etc. according to the size of the pores or the roughness of the surface, it is possible to prevent fluffing, tearing, physical skin irritation, and skin side effects that may occur when using products made of cotton, cotton pads, non-woven fabrics, and chemical products used for skin toners, facial cleansing, and partial massage packs, and toners, essences, etc. are filled on the cut surface of the air bubbles formed for each use on the konjac pad, and unlike existing products that are simply soaked on the surface of cotton or non-woven fabrics, several times more functional solutions are provided to the skin, thereby obtaining superior effects than existing cotton products, and by cutting the air bubbles (pores) of cleansing konjac pads, puffs, and towels, Surface roughness has the advantage of being able to improve the skin by removing waste and dead skin cells without irritating the skin with excellent cleansing power.
[0012] Figure 1 is a flow chart illustrating a method for manufacturing a cleaning tool having a surface roughness by cutting bubbles according to an embodiment of the present invention.
[0013] Fig. 2 is a schematic diagram illustrating a mold for manufacturing a cleaning tool having a surface roughness by cutting bubbles according to the present invention.
[0014] Figure 3 is a product photograph showing a cleaning tool manufactured using a method for manufacturing a cleaning tool having a surface roughness by cutting bubbles according to the present invention.
[0015] FIG. 4 is a photograph showing a method for manufacturing a cleaning tool having a surface roughness by cutting bubbles according to the present invention, in which a konjac mixture separated from a mold is cut into a certain thickness using a cutter.
[0016] Figure 5 is a photograph showing the surface and an enlarged view of the surface of a cleaning tool manufactured using a method for manufacturing a cleaning tool having surface roughness by cutting bubbles according to the present invention.
[0017] The present invention relates to a method for manufacturing a cleaning tool by controlling the amount of bubbles by whipping a konjac mixture, controlling the size of bubbles according to bubble expansion by steam heating, determining the size of pores according to the use of pads, puffs, towels, etc., and distinguishing the roughness of the surface by cutting the bubbles, wherein (a) a viscosity of 30,000 to 35,000 mPa with added foaming agent.A step of mixing konjac powder and purified water in a certain ratio, putting the konjac mixture into a mixer and whipping it at a maximum speed of 360 rpm for 8 to 10 seconds or a minimum speed of 166 rpm for 50 seconds to generate air bubbles; (b) a step of putting the konjac mixture in which air bubbles are generated by the whipping into a dispensing machine and then putting it into a mold of a certain shape and form and maturing it at 7 to 5°C for 12 to 15 hours; (c) a step of putting the mold containing the konjac mixture, in which the maturation is completed, into a steam heater and heating it for 50 to 70 minutes by applying steam at a certain temperature; (d) a step of cooling the mold containing the konjac mixture at room temperature for 3 to 5 hours after heating it with steam; (e) a step of putting the mold containing the konjac mixture into a freezer and rapidly freezing it at -30°C for 2 hours when it has cooled. (f) a step of rapidly freezing a mold containing the konjac mixture and then maintaining it frozen in a freezer at -7°C for 24 hours; (g) a step of taking out the frozen mold and thawing it for 12 hours; (h) a step of separating the konjac mixture from the thawed mold, placing it in a freezer, and maintaining it again frozen at -7°C for 24 hours; (i) a step of classifying the washing utensils by cutting the frozen konjac mixture into a certain thickness with a cutter and dividing them by surface roughness; (j) a step of placing the classified washing utensils in a freezer and freeze-drying them at -7°C for 72 hours; (k) a step of taking out the freeze-dried washing utensils and washing them 2 to 3 times; (l) a step of placing the washed washing utensils in a freeze-dryer and freeze-drying them for 12 to 18 hours; and (m) a step of classifying the freeze-dried washing utensils by use, thickness, and size and packaging them.
[0018] Hereinafter, a method for manufacturing a cleaning tool having a surface roughness by cutting bubbles according to the present invention will be described in detail.
[0019] The present invention is to manufacture pads, puffs, towels, etc. for packs, toners, or cleansing, using plant materials with konjac as the main ingredient. Konjac is a plant of the Araceae family, and the corm of konjac is composed of 75 to 83% moisture, 11 to 14% carbohydrates, and 2 to 4.5% protein. The main component of the paste is a polysaccharide called mannan, and this sugar, also known as konjac mannan, is contained in specific cells of parenchymal tissue. The concentrate of konjac mannan is called jeongbun, and the main component of jeongbun is glucomannan, and 99% of the carbohydrate of konjac is glucomannan. Glucomannan is a sugar formed by combining the six-carbon sugar mannose and glucose.
[0020] Next, an embodiment is described with reference to a flow chart showing a method for manufacturing a cleaning tool having a surface roughness by cutting the bubbles of Fig. 1.
[0021] (Example)
[0022] Purified water is mixed in a certain ratio with konjac powder having a viscosity of 30,000 mPa.s or higher to which a foaming agent is added (S1). At this time, the mixture is mixed in a ratio of 1 part konjac powder to 16 parts purified water. The foaming agent can be added in an amount of 0.2 to 0.3 wt% of the total mixing ratio. In addition, the purified water is added in a ratio of 1 part water to 20 parts purified water. At this time, the viscosity of the konjac powder is preferably 30,000 to 35,000 mPa.s. In addition, dyes and mordants can be added and mixed so that various colors can be expressed on the konjac pad.
[0023] A konjac mixture containing a foaming agent, konjac powder, and purified water is placed in a mixer and whipped to generate air bubbles (S2). The whipped konjac mixture contains fine air bubbles, and the high viscosity of the konjac powder maintains the formed fine air bubbles without extinguishing them. At this time, the whipping blade in the mixer whips at a maximum rotation speed of 360 rpm for approximately 8 to 10 seconds or at a minimum speed of 166 rpm for approximately 50 seconds. Furthermore, the rotation of the whipping blade in the mixer can be whipped by distinguishing between the maximum rotation speed (rpm) and the minimum rotation speed (rpm), or by reducing the speed from the maximum rotation speed to the minimum rotation speed.
[0024] Meanwhile, when the present invention is to manufacture a pack pad as a cleansing tool by whipping a konjac mixture in a mixer, it can be manufactured by whipping at 360 rpm for about 8 to 10 seconds and then whipping at 166 rpm for about 50 seconds. And, when the konjac mixture is to manufacture a toner pad as a cleansing tool by whipping it, it can be manufactured by whipping at 360 rpm for about 15 to 18 seconds and then whipping at 166 rpm for about 50 seconds. In addition, when the konjac mixture is to manufacture a cleansing pad, puff, or towel as a cleansing tool by whipping it, it can be manufactured by whipping at 360 rpm for about 20 to 25 seconds and then whipping at 166 rpm for about 50 seconds.
[0025] Next, the dough in which bubbles are generated by controlling the number of rotations and time of whipping in the mixer, i.e., the konjac mixture, is fed into the extruder (S3), and the konjac mixture is placed in a plurality of molds having a certain shape, form, and capacity and aged at approximately 7 to 5°C for approximately 12 to 15 hours (S4). At this time, if the maturation temperature and time of the konjac mixture are approximately 7°C or higher, the manufactured konjac mixture will not be cleanly separated from the mold. In addition, the maturation time of the konjac mixture should be maintained for approximately 12 hours or longer to have less of an impact on the quality of cleaning tools such as pads, puffs, and towels manufactured as finished products.
[0026] And in Fig. 2a, a molding die of various sizes and capacities is schematically illustrated, and the molding die is a container with an open top, such as a cylindrical or polygonal prism shape. Furthermore, in Fig. 2b, the upper edge of the molding die is formed with a protruding flange to function as a handle, and a separate handle may be formed on the side of the molding die, and it is preferable that a plurality of support legs are formed on the bottom of the molding die. Furthermore, in the case where the molding die is a square prism, it is preferable that the corners are rounded into an arc shape. In addition, the molding die may be manufactured by having different inlets for feeding the konjac mixture and separate outlets. In addition, it is preferable that the molding die is made of a material that can maintain its shape and form even when exposed to a certain temperature range.
[0027] The mold after maturation is placed in a steam heater, steam of a certain temperature is applied, and heating is performed for approximately 50 to 70 minutes, preferably 60 minutes (S5). At this time, the heating temperature of the steam heating the mold varies depending on the product being manufactured. For example, in the case of a pack pad, the thickness is approximately 0.5 to 1 mm and the bubble diameter is approximately 0.3 to 0.8 mm, and the heating temperature is approximately 80 to 90°C. In addition, in the case of a toner pad, the thickness is approximately 1.2 to 1.5 mm and the bubble diameter is approximately 1.0 to 1.3 mm, and the heating temperature is approximately 90 to 100°C. In addition, in the case of a cleansing pad, the thickness is approximately 2.0 to 3.0 mm and the bubble diameter is approximately 1.5 to 2.0 mm, and the heating temperature is approximately 100 to 110°C. In addition, the steam heating of the steam heater is performed when the thickness of the cleansing puff as a cleaning tool is approximately 5.0 to 15.0 mm and the diameter of the bubbles is approximately 1.5 to 3.0 mm, and the heating temperature is approximately 100 to 110°C. In addition, the steam heating of the steam heater is performed when the thickness of the cleansing towel as a cleaning tool is approximately 5.0 to 8.0 mm and the diameter of the bubbles is approximately 1.5 to 3.0 mm, and the heating temperature is approximately 100 to 110°C.
[0028] When the steam heating of the konjac mixture placed in the mold using the above steam heater is completed, the steam-heated mold is cooled at room temperature for approximately 3 to 5 hours (S6).
[0029] And the cooled mold is placed in a freezer and rapidly frozen at approximately -30℃ for approximately 2 hours (S7). The rapidly frozen mold is kept frozen in the freezer at approximately -7℃ for approximately 24 hours (S8). Then, the frozen mold is taken out and thawed for approximately 12 hours (S9). In addition, after separating the konjac mixture from the mold that has been thawed for a certain period of time (S10), it is placed in a freezer and refrozen at approximately -7℃ for approximately 24 hours (S11).
[0030] In addition, the frozen konjac mixture is cut into konjac pads, puffs, and towels of a certain thickness using a cutter (S12). For example, as a cleansing tool, a pack pad is cut to a thickness of approximately 0.5 to 1 mm, a toner pad is cut to a thickness of approximately 1.2 to 1.5 mm, a cleansing pad is cut to a thickness of approximately 2.0 to 3.0 mm, a cleansing puff is cut to a thickness of approximately 5.0 to 15.0 mm, and a cleansing towel is cut to a thickness of approximately 5.0 to 8.0 mm. Then, the cut cleansing tools are classified into konjac pads, puffs, towels, etc. according to the roughness of the surface (S13). The classified konjac pads, puffs, towels, and other cleansing tools are placed in a freezer and dried in a frozen state at approximately -7°C for approximately 72 hours (S14). Freeze-drying of the cleaning agent makes the dietary fiber of konjac tougher and stronger.
[0031] In addition, washing tools such as konjac pads, puffs, and towels that have been freeze-dried by naturally evaporating moisture for approximately 72 hours in the freezer are taken out and washed approximately 2 to 3 times (S15), and the washed washing tools such as konjac pads, puffs, and towels are placed in a freeze dryer and freeze-dried for approximately 12 to 18 hours (S16).
[0032] Afterwards, freeze-dried cleaning tools such as konjac pads, puffs, and towels are packaged in the corresponding packaging materials according to their intended use, thickness, or size (S17).
[0033] Figure 3 is a product photograph showing a cleaning tool, i.e., a konjac pad and a puff, manufactured according to the manufacturing method of the present invention. Figure 3a shows the surface of a konjac pad manufactured to a thickness of 5 mm. Figure 3b shows the surface of a konjac puff manufactured to a thickness of 15 mm. The surface is roughened depending on the size of the pores.
[0034] Figure 4a is a photograph showing a konjac mixture separated from a mold and cut into pieces of a certain thickness using a cutter. Figure 4b also shows konjac pads and puffs cut into various thicknesses, and photographs showing the production of konjac pads and puffs dyed in various colors.
[0035] Fig. 5a is a surface of a konjac pad manufactured by the method of the present invention, and Fig. 5b is an enlarged photograph showing the surface of the konjac pad, from which it can be seen that numerous pores are formed on the surface.
[0036] The cleaning tools such as konjac pads, puffs, and towels according to the present invention have the advantage of being able to control the amount of air bubbles by whipping speed and time of the kneaded konjac mixture, controlling the size of the air bubbles by expansion of the air bubbles formed by steam heating, and exhibiting excellent cleaning power depending on the roughness of the surface by cutting countless formed air bubbles.
[0037] The above-described embodiments of the present invention are merely examples and are not intended to limit the present invention. Anything that has substantially the same configuration and achieves the same operational effects as the technical concepts described in the claims of the present invention is included within the technical scope of the present invention.
[0038] The method for manufacturing a cleansing tool having a surface roughness by cutting air bubbles of the present invention can control the amount of air bubbles by the whipping speed and time of a konjac mixture kneaded with konjac powder as a main ingredient, can control the size of the air bubbles by the expansion of the air bubbles formed by steam heating, and exhibits excellent cleansing power according to the roughness of the surface by cutting countless formed air bubbles, and provides them as cleansing tools for packs, toners, cleansing, puffs, towels, etc. according to the size of the pores or the roughness of the surface, thereby preventing fluffing, tearing, physical skin irritation, and skin side effects that may occur when using products made of cotton, cotton pads, non-woven fabrics, and chemical products used for skin toners, facial cleansing, and partial massage packs, and unlike existing products that are simply soaked on the surface of cotton or non-woven fabrics by filling the cut surface of the air bubbles formed for each use on the konjac pad, the method provides several times more functional solutions to the skin, thereby obtaining an effect superior to that of existing cotton products, and the cleansing konjac pad and puff, The surface roughness created by cutting the air bubbles (pores) of the towel is characterized by its excellent cleansing power, which allows for the removal of waste products and dead skin cells without irritation to the skin, resulting in a skin improvement effect.
Claims
1. (a) A step of adding a konjac mixture, which is a mixture of konjac powder with a viscosity of 30,000 to 35,000 mPa.s and purified water in a certain ratio, to a kneader and whipping at a maximum speed of 360 rpm for 8 to 10 seconds or a minimum speed of 166 rpm for 50 seconds to generate air bubbles; (b) A step of putting the konjac mixture, in which bubbles are generated by the whipping, into an extruder, then putting it into a mold of a certain shape and form, and maturing it at 7 to 5°C for 12 to 15 hours; (c) A step of placing the mold containing the above-mentioned matured konjac mixture into a steam heater and heating it for 50 to 70 minutes by applying steam at a certain temperature; (d) a step of heating the mold containing the konjac mixture with steam and then cooling it at room temperature for 3 to 5 hours; (e) When the mold containing the konjac mixture is cooled, the mold is placed in a freezer and rapidly frozen at -30°C for 2 hours; (f) a step of rapidly freezing the mold into which the konjac mixture is placed and then keeping it frozen in a freezer at -7°C for 24 hours; (g) A step of taking out the frozen mold and thawing it for 12 hours; (h) A step of separating the konjac mixture from the thawed mold, placing it in a freezer, and maintaining refreezing at -7°C for 24 hours; (i) a step of classifying the frozen konjac mixture into washing utensils cut into a certain thickness using a cutter and classifying them according to the roughness of the surface; (j) A step of placing the classified cleaning tools in a freezer and freeze-drying them at -7°C for 72 hours; (k) Step of taking out the freeze-dried washing tool and washing it 2 to 3 times; (l) A step of placing the washed washing tool in a freeze dryer and freeze-drying it for 12 to 18 hours; (m) A method for manufacturing a cleaning tool having a surface roughness by cutting air bubbles, comprising: a step of packaging the freeze-dried cleaning tool by classifying it according to use, thickness, and size; 2. A method for manufacturing a cleaning tool having a surface roughness by cutting air bubbles, wherein the konjac powder and purified water are mixed in a ratio of 1:16 in the first paragraph, and the purified water is mixed with water in a ratio of 1:
20.
3. In the first paragraph, when whipping the konjac mixture in the kneader, a pack pad as a cleaning tool is whipped at 360 rpm for 8 to 10 seconds and then whipped at 166 rpm for 50 seconds, a toner pad as a cleaning tool is whipped at 360 rpm for 15 to 18 seconds and then whipped at 166 rpm for 50 seconds, and a cleansing pad, puff, and towel as a cleaning tool are whipped at 360 rpm for 20 to 25 seconds and then whipped at 166 rpm for 50 seconds, a method for manufacturing a cleaning tool having a surface roughness by cutting air bubbles.
4. In the first paragraph, when the mold into which the konjac mixture is injected is heated with steam by a steam heater, the thickness of the pack pad as a cleaning tool is 0.5 to 1 mm, the diameter of the bubbles is 0.3 to 0.8 mm, and the heating temperature is 80 to 90°C. As a cleaning tool, the thickness of the toner pad is 1.2 to 1.5 mm, the bubble diameter is 1.0 to 1.3 mm, and the heating temperature is 90 to 100°C. As a cleaning tool, the thickness of the cleansing pad is 2.0 to 3.0 mm, the bubble diameter is 1.5 to 2.0 mm, and the heating temperature is 100 to 110℃. As a cleaning tool, the thickness of the cleansing puff is 5.0 to 15.0 mm, the bubble diameter is 1.5 to 3.0 mm, and the heating temperature is 100 to 110°C. A method for manufacturing a cleaning tool having a surface roughness by cutting bubbles, wherein the thickness of the cleansing towel as a cleaning tool is 5.0 to 8.0 mm, the diameter of the bubbles is 1.5 to 3.0 mm, and the heating temperature is 100 to 110°C.
5. A method for manufacturing a cleaning tool having a surface roughness by cutting bubbles, wherein the mold is formed in a cylindrical or polygonal columnar shape in the first or fourth paragraph.
Citation Information
Patent Citations
Konjak sponge, and manufacture thereof
JP1998272075A
SPONGE-LIKE MATERIAL, PRODUCTION METHOD AND APPLICATION THEREOF
JP2001513582A
Method for drying konjac sponge and method for producting konjac sponge
KR101163962B1
Method for producing konjac sponge
KR1020110052954A
Cleaning Implement