Glass melting furnace
The design of the glass melting furnace through the stainless steel casing and coil cooling system solves the problems of refractory erosion and induction heating design defects of traditional glass melting furnaces, achieving continuous and efficient production of high-purity glass and high-level radioactive liquid waste glass, and extending Extend equipment life and reduce costs.
Patent Information
- Application Number
- CN202011019152.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-24
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-09-24
AI Technical Summary
The erosion of refractory materials at high temperatures in traditional glass melting furnaces leads to a decrease in glass performance and a short furnace life. In addition, the existing induction heating cold crucible design has problems such as arc risk, large electromagnetic induction loss, and difficulty in controlling the glass flow rate.
The glass melting furnace assembled with stainless steel casing uses coil cooling and induction heating freeze-thaw valve leakage device, combined with frame stirrer and mica sheet insulation to achieve glass flow rate control and precious metal discharge, reducing electromagnetic induction loss.
It extends the service life of the glass melting furnace, improves the quality of the glass, realizes the continuous production of high-purity glass and high-level radioactive liquid waste glass, reduces the production cost, and enhances the safety and controllability of the equipment.
Smart Images

Figure CN114249522B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a glass melting furnace, in particular to a glass melting furnace for solidifying high-purity glass and high-level radioactive waste liquid. Background Art
[0002] Traditional glass production technology usually involves adding glass batch materials to a Joule-heated ceramic tank furnace, heating and melting the batch materials using electric heating, gas heating, etc., and then forming glass products after clarification and molding. With the development of science and technology, the quality requirements for glass materials are getting higher and higher, and the quality of glass is closely related to the impurity content in the glass. During the melting process of glass, the refractory materials of the tank furnace enter the glass as impurities under the erosion of the high-temperature glass melt, which has an adverse effect on the performance of the glass material (for example, the erosion of the refractory materials causes an increase in the optical loss of laser glass). Therefore, solving the problem of refractory erosion in glass melting furnaces is a key link in further improving glass performance.
[0003] The Joule-heated ceramic furnace glass solidification process is an important spent fuel reprocessing high-level waste liquid solidification technology, which has been industrialized in the United States, Russia, Germany and Japan. Its advantage is the high glass yield per unit time. The Joule-heated ceramic furnace glass solidification technology evolved from commercial glass production technology. Its disadvantage is that the life of the glass furnace is limited due to the erosion of refractory materials. On the other hand, in order to increase the glass yield, the Joule-heated ceramic furnace is relatively large in size, and there is a lot of decommissioning waste, which makes decommissioning difficult.
[0004] In order to solve the problem of short furnace life and glass performance caused by refractory corrosion during glass melting, scientists were inspired by the cold crucible high-purity metal smelting technology and applied the cold crucible technology to the solidification of high-level waste glass and the production of high-purity glass. The cold crucible technology uses high-frequency induction heating of the glass material in the split metal crucible, and passes cooling water through the crucible petals to keep the crucible wall temperature at 100-200℃, forming a 5-10mm thick glass shell on the crucible wall. Under the protection of the shell, the metal crucible wall does not directly contact the molten glass, which enhances the corrosion resistance of the crucible and extends the service life of the crucible. Since there is no corrosion from refractory materials, the glass maintains its original composition, so it has more excellent performance.
[0005] Patent US6996153 / CN1628233A of the French Atomic Energy Commission discloses an induction heating cold crucible, in which the crucible is divided into two parts using an arc plate, and a cooling circuit is formed by drilling holes in the middle of the arc plate, which has a complex processing and installation process. In addition, the arc plate is prone to produce tip voltage and local overheating. Although the patent proposes measures such as edge rounding and arc plate surface insulation spraying, compared with the round tube cold crucible, under the action of high-frequency power supply, there is still a higher risk of arcing and local overheating.
[0006] Russian patent RU2392675C1 discloses an induction heating cold crucible melting device, in which the crucible is divided into petals using stainless steel tubes, and several stainless steel tubes form a group, and are provided with upper and lower water cooling rings, the upper water cooling ring is provided with water inlet and outlet pipes, and the lower water cooling ring conducts the cooling water path. The bottom of the crucible of this design is welded with stainless steel, and there is no insulation between the petals, resulting in large electromagnetic induction losses.
[0007] US Patent US20160091249A1 discloses an induction heating cold crucible, the crucible is divided into two parts using stainless steel tubes, the bottom leakage is achieved by using a gate valve, and the leakage rate is achieved by controlling the furnace pressure. This design makes it easy for glass to splash out when the gate valve is closed, and it is difficult to control the glass flow rate and direction.
[0008] Chinese patent CN205048973 U discloses a cold crucible device, in which the crucible is divided into petals using stainless steel pipes. The cold crucible is designed with upper and lower water cooling rings, wherein the lower water cooling ring is a group of 3 steel pipes, which are connected for water inlet, and the adjacent 3 steel pipes are connected for water outlet. The water cooling ring design has a large electromagnetic induction loss because there is no insulation measure between the petals. On the other hand, the hard connection part between the pipes is a stainless steel pipe, and the soft connection part is a PVC pipe. When the cold crucible is used for high-level waste liquid glass solidification, the PVC pipe is prone to aging after being exposed to radioactive irradiation, which affects the service life of the crucible.
[0009] Chinese patent CN106123588 A discloses a cold crucible high temperature melt discharge device, the discharge pipe is designed in the form of a sleeve, and the medium frequency induction coil is wound outside the discharge pipe. This design blocks the entire discharge pipe with solid glass when the discharge pipe is closed. When restarting, the glass of the entire discharge pipe needs to be melted, which makes the discharge time-consuming. When the discharge pipe is restarted, glass wire drawing is easily formed at the gate, affecting the discharge flow direction. The discharge pipe extends 2 cm into the crucible, which is not conducive to the discharge of precious metals deposited at the bottom when the high-level waste liquid glass solidifies. Summary of the invention
[0010] The technical problem to be solved by the present invention is to provide a glass melting furnace, which is suitable for the field of high-purity glass production and high-level nuclear waste glass solidification. The glass melting furnace adopts induction heating, and the furnace body does not directly contact the molten glass, which increases the service life of the furnace and improves the quality of the glass. The furnace is assembled from stainless steel sleeves and is easy to install. The glass leakage adopts a coil cooling closure and induction heating to open the freeze-thaw valve leakage device, which avoids the change of glass flow direction caused by glass drawing. The stainless steel pipes at the lower end of the furnace are insulated and installed on a refractory concrete base, which enhances the magnetic permeability of induction heating. The glass melting furnace of the present invention can realize the continuous production of high-purity glass and high-level waste liquid glass solidification, is simple and controllable to operate, has a long furnace life, low production cost, and can improve the quality of high-purity glass.
[0011] The technical solution adopted by the present invention is as follows:
[0012] A glass melting furnace, comprising a furnace body and a refractory concrete base with supporting legs, wherein the furnace body is fixed to the base by a screw rod, a furnace cover is provided on the top of the furnace body, and a furnace bottom is provided on the bottom of the furnace body, wherein the furnace cover is a cavity structure, a cooling channel with a rectangular cross section is welded inside the cavity, an air inlet and an air outlet are provided on the furnace cover, which are respectively connected to the cooling channel, and a stirrer installation port is provided at the center of the furnace cover for the stirrer to extend into the furnace body; a liquid level measuring port, a viewing window, an exhaust gas discharge port, a temperature measuring port and a feeding port are also provided on the furnace cover;
[0013] The furnace body is a cylinder surrounded by a plurality of stainless steel sleeves, the top and bottom surfaces of which are welded by an upper circular water outlet distribution ring and a lower circular water inlet distribution ring, each stainless steel sleeve is composed of an inner tube, an outer tube sleeved outside the inner tube and a cover plate covering the bottom of the outer tube, the inner tube and the outer tube are connected by a bracket, the upper end of the inner tube is provided with a water outlet, and the upper end of the outer tube is provided with a water inlet;
[0014] The furnace bottom is radially divided into petals, and the central angle corresponding to each petal is 30-45°. The length of the petal slit is 1 / 2 to 2 / 3 of the radius of the furnace bottom. The petal gap is filled with aluminate refractory cement. A bubbler is arranged on each petal. A water cooling box is welded under each petal. The water cooling box is divided into an outer water inlet box and an inner water outlet box by a metal plate. The volume of the water inlet box is smaller than that of the water outlet box. The water inlet box and the water outlet box are respectively equipped with a water inlet pipe and a water outlet pipe; a material leakage hole is opened in the center of the furnace bottom, and a conical freeze-thaw valve installation interface is welded on the furnace bottom for connecting the freeze-thaw valve;
[0015] The cooling water in the frame-type agitator flows from top to bottom through the water inlet pipes on both sides of the agitator rod, turns back through the agitator frames on both sides, and flows upward through the central pipe of the agitator rod to discharge the water;
[0016] A furnace body mounting groove is provided in the base, the furnace bottom is mounted on the mounting groove, and the mounting groove and the furnace bottom are insulated by an insulating mica sheet; the furnace body is mounted on the furnace bottom, the upper end of the frame-type agitator is mounted in the agitator mounting opening in the center of the furnace cover, and the upper end of the freeze-thaw valve is aligned with the leakage hole and installed under the base; the furnace cover is covered on the furnace body by the furnace cover buckle and the mounting buckle of the upper circular water outlet distribution ring, so that the stainless steel metal ball is above the leakage hole of the furnace bottom, and the symmetry axis of the frame-type agitator, the center of the stainless steel metal ball, the center of the leakage hole, and the symmetry axis of the freeze-thaw valve are on the same straight line.
[0017] The upper circular water outlet distribution ring and the lower circular water inlet distribution ring are divided into N partitions by partitions, and the value range of N is 8 to 16. N stainless steel sleeves are connected in each partition, and the value range of n is 6 to 8. The gaps between adjacent stainless steel sleeves are filled with mica sheets for insulation; the distance between the upper circular water outlet distribution ring and the lower circular water inlet distribution ring is 1-3cm, and the effective volume in the cavity of the upper circular water outlet distribution ring is greater than the effective volume in the cavity of the lower circular water inlet distribution ring.
[0018] The upper circular water outlet distribution ring is welded by a top cover, an outer plate, a bottom plate and an inner plate, and is divided into N partitions by a partition. A water outlet pipe and a pressure relief safety valve are installed on the outer plate of each partition. There is a stainless steel sleeve inner pipe welding opening on the bottom plate, and two mounting buckles are installed on the outer plate of the upper circular water outlet distribution ring;
[0019] The lower circular water inlet distribution ring is welded by a top plate, an outer plate, a bottom plate and an inner plate, and is divided into N partitions by partitions. A water inlet pipe is welded on the outer plate of each partition. There is a stainless steel casing outer pipe welding opening on the bottom plate, and there is a stainless steel casing inner pipe welding opening on the top plate. The cooling water in the stainless steel casing flows as follows: enters the outer pipe through the water inlet, goes downward along the outer pipe, folds the cover plate, and goes upward along the inner pipe, and flows out from the water outlet.
[0020] The freeze-thaw valve is made of NiCrFe alloy or platinum. The freeze-thaw valve adopts water cooling or air cooling of a rectangular cross-section spiral tube and is heated by a medium-frequency induction coil. The inner conical surface of the upper end interface of the freeze-thaw valve matches the conical interface of the furnace bottom. The freeze-thaw valve is installed by bolt-tightening lug installation or thread-tightening installation:
[0021] When the freeze-thaw valve is installed in a threaded fastening manner, the threaded interface at the upper end of the freeze-thaw valve is screwed into the threaded hole at the furnace bottom and tightened by an octagonal nut so that the inner conical surface of the threaded interface of the freeze-thaw valve and the outer conical surface of the conical interface at the furnace bottom fit closely;
[0022] When the freeze-thaw valve is installed in a bolt-tightening lug installation mode, three mounting lugs are welded at the conical interface at the upper end of the freeze-thaw valve, and three L-shaped stainless steel blocks are welded on the furnace bottom. The L-shaped stainless steel blocks have threaded holes, and mounting tightening bolts are arranged in the threaded holes.
[0023] The diameter of the stainless steel metal ball on the lower end of the frame-type stirrer is 30-50 mm.
[0024] The inner tube of the stainless steel sleeve has a diameter of 8-18 mm and a wall thickness of 1-2 mm, and the outer tube has a diameter of 16-30 mm and a wall thickness of 2-5 mm.
[0025] The gap between adjacent petal stainless steel sleeves of the furnace body 2 is 1-2 mm, and the gap is filled with mica sheets for insulation.
[0026] The bubblers are located on the same circumference with the center of the furnace bottom 5 as the center.
[0027] The distance between the water cooling box and the center of the furnace bottom circle is 1 / 3 to 1 / 2 of the radius of the furnace bottom.
[0028] The thickness of the furnace bottom is 3-4 cm, the upper end diameter of the central leakage hole is 20-30 mm, and it narrows downward at an angle of 10-15 degrees. A conical leakage interface is welded on the furnace bottom, and the interface also narrows downward at an angle of 10-15 degrees.
[0029] The thickness of the insulating mica sheet between the furnace body installation groove and the furnace bottom is 3-5 mm.
[0030] The beneficial effects of the present invention are:
[0031] 1) The glass melting furnace body is welded by stainless steel sleeve, upper ring water outlet distribution ring and lower ring water inlet distribution ring. The furnace body is installed on the refractory cement concrete plate, with a solid structure and simple installation process. The upper ring water outlet distribution ring is equipped with a pressure relief safety valve to eliminate the risk of overpressure of the upper ring water outlet ring caused by excessive outlet water temperature.
[0032] 2) The lower part of the adjacent stainless steel sleeves constituting the furnace body, the furnace body and the furnace bottom are insulated by mica sheets, thereby reducing electromagnetic induction losses.
[0033] 3) The stainless steel ball of the frame agitator is used as a glass leakage method that combines the plug valve and the freeze-thaw valve, which is convenient for controlling the glass flow rate and direction and is conducive to discharging the precious metals deposited at the bottom of the furnace. The freeze-thaw valve is cooled by air-cooled or water-cooled coils with rectangular cross-sections, which increases the heat exchange efficiency, makes the glass in the freeze-thaw valve solidify quickly, and reduces the closing time of the freeze-thaw valve. The freeze-thaw valve is installed with threads or bolts to facilitate installation and maintenance. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 Schematic diagram of the structure of the glass melting furnace of the present invention
[0035] Figure 2 This is a schematic diagram of the glass melting furnace cover structure
[0036] Figure 3 This is a cross-sectional view of the glass melting furnace cover
[0037] Figure 4 This is the schematic diagram of the upper ring cooling water outlet distribution ring structure
[0038] Figure 5 This is the cross-section of the upper ring cooling water outlet distribution ring
[0039] Figure 6 This is the schematic diagram of the lower ring cooling water inlet distribution ring structure
[0040] Figure 7 This is the cross-section of the lower ring cooling water inlet distribution ring
[0041] Figure 8 is a schematic diagram of the furnace body split stainless steel casing structure. Fig. 8A Schematic diagram of the upper structure of the stainless steel casing. Figure 8B Schematic diagram of the lower structure of the stainless steel casing
[0042] Fig. 9 This is a schematic diagram of the cooling water flow inside the stainless steel casing.
[0043] Fig.10 This is the installation diagram of the stainless steel casing and the upper ring cooling water outlet distribution ring and the lower ring cooling water inlet distribution ring.
[0044] Fig.11 This is a schematic diagram of the furnace bottom structure
[0045] Fig.12 This is a cross-section of the furnace bottom
[0046] Fig.13 This is the installation diagram of the furnace body and furnace bottom
[0047] FIG. 14 is a schematic diagram of freeze-thaw valve installation embodiment 1. Fig.14A Freeze-thaw valve installation example 1 furnace bottom structure schematic diagram, Fig. 14B Installation Example 1 Freeze-thaw valve structure diagram, Fig. 14C Installation Example 1 Installation Process Schematic Diagram
[0048] FIG. 15 is a schematic diagram of freeze-thaw valve installation embodiment 2. Fig.15A This is a schematic diagram of the furnace bottom structure of the freeze-thaw valve installation embodiment 2. Fig. 15B This is a schematic diagram of the freeze-thaw valve structure of the second installation embodiment. Fig. 15C Installation Example 1 Installation Process Schematic Diagram
[0049] Fig.16 Schematic diagram of frame agitator structure
[0050] Fig.17 This is a cross-sectional view of the glass melting furnace after installation. DETAILED DESCRIPTION
[0051] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments:
[0052] See Figure 1As shown in the figure, it can be seen that the glass melting furnace of the present invention includes a furnace cover 10, a furnace body 2, a furnace bottom 5, a frame stirrer 9, a freeze-thaw valve 62 and a refractory concrete base 7. The furnace cover 10, the furnace body 2, the furnace bottom 5, and the frame stirrer 9 with a stainless steel ball 74 are made of stainless steel 304 or 316. The glass melting furnace heats the glass material in the furnace body 2 through an induction coil 3 with a copper bar 6. The glass melting furnace 1 is fixed on the refractory concrete base 7 with a support leg 8 through a screw rod 4.
[0053] See also Figure 2 Figure 3 The furnace cover 10 is a cavity structure, a cooling channel 25 with a rectangular cross section is welded inside the cavity, an air inlet 16 and an air outlet 19 of the cooling channel 25 are arranged on the furnace cover, a stirrer installation port 24 is arranged at the center of the furnace cover 10, a liquid level measuring port 17, a viewing window 18, an exhaust gas discharge port 21, a temperature measuring port 22 and a feeding port 23 are also arranged on the furnace cover 10, and a buckle 20 for mounting with the furnace body 2 is arranged on the outer wall of the furnace cover 10;
[0054] The furnace body 2 is a cylinder formed by welding a stainless steel sleeve 14 through an upper circular water outlet distribution ring 12 and a lower circular water inlet distribution ring 13. Each stainless steel sleeve 14 (see Fig. 8A , Figure 8B ) comprises an inner tube 43, an outer tube 42 and a cover plate 47, wherein the inner tube 43 and the outer tube 42 are connected by a bracket 44, and the bottom end is covered by the cover plate 47, the upper end of the inner tube 43 is provided with a water outlet 45, the upper end of the outer tube 42 is provided with a water inlet 46, the upper annular water outlet distribution ring 12 and the lower annular water inlet distribution ring 13 are divided into N partitions by a partition, the value range of N is 8 to 16, and n stainless steel sleeves are placed in each partition The tube 14 is connected, the value range of n is 6 to 8, the gap between adjacent stainless steel sleeves 14 is filled with mica sheets for insulation, the upper part of the stainless steel sleeve 14 is welded on the upper circular water outlet distribution ring 12 and the lower circular water inlet distribution ring 13, there is a certain distance of 1-3cm between the upper circular water outlet distribution ring 12 and the lower circular water inlet distribution ring 13, and the effective volume in the cavity of the upper circular water outlet distribution ring 12 is greater than the effective volume in the cavity of the lower circular water inlet distribution ring 13;
[0055] The upper circular water outlet distribution ring 12 is welded by a top cover 29, an outer plate 30, a bottom plate 31 and an inner plate 32 (see Figure 4 , Figure 5 ), divided into N partitions by a partition (33), the partitions connect n stainless steel sleeves 14, an outlet pipe 26 and a pressure relief safety valve 27 are installed on the outer plate 30 of the partition, the bottom plate 31 has a stainless steel sleeve inner pipe welding opening 28, and two mounting buckles 11 are installed on the outer plate of the upper annular water outlet distribution ring 12;
[0056] See also Figure 6 , Figure 7 The lower annular water inlet distribution ring 13 is welded by a top plate 40, an outer plate 39, a bottom plate 38 and an inner plate 37, and is divided into N partitions by a partition (41). The n stainless steel sleeves 14 of each partition are connected. A water inlet pipe 36 is welded on the outer plate 39 of each partition. There is a stainless steel sleeve outer pipe welding opening 35 on the bottom plate 38, and there is a stainless steel sleeve inner pipe welding opening 34 on the top plate 40. The cooling water in the stainless steel sleeve 14 flows as follows: enter the outer pipe 42 through the water inlet 46, go downward along the outer pipe 42, turn the cover plate 47, go upward along the inner pipe 43, and flow out from the water outlet 45, see FIG. 8, Fig. 9 ;
[0057] See also Fig.10 , stainless steel casing 14 through Figure 4 The inner tube welding opening 28 shown, Figure 6 The inner tube welding opening 34 and the outer tube welding opening 35 are welded and fixed, and the gap between adjacent stainless steel sleeves 14 is 1.5 mm;
[0058] See also Fig.11 , 12 The furnace bottom 5 is a petal 48 structure, each petal corresponds to a central angle of 40°, and the length of the petal slit 52 is 3 / 5 of the furnace bottom radius. The petal 48 is provided with a bubbler 49, and the bubbler 49 on each petal is on a circumference with the center of the furnace bottom 5 as the center. A leakage hole 50 is opened in the center of the furnace bottom. The hole is conical, with an upper end diameter of 30mm, and it narrows downward at an angle of 15°. A conical interface 51 is welded on the furnace bottom, and the interface also narrows downward at an angle of 15°;
[0059] See also Fig.12 A water cooling box 57 is welded below the furnace bottom petal 48. The water cooling box 57 is divided into a water inlet box 58 and a water outlet box 59 by a metal plate 55. The volume of the water inlet box 58 is smaller than that of the water outlet box 59. The water inlet box 58 and the water outlet box 59 are respectively installed with a water inlet pipe 53 and a water outlet pipe 54. The distance between the water cooling box 57 and the center of the furnace bottom circle is 2 / 5 of the radius of the furnace bottom;
[0060] See also Fig.13 , 17The base 7 is provided with a mounting groove 60 for the furnace body 2, the furnace bottom 5 is mounted on the mounting groove 60, and the mounting groove 60 and the furnace bottom 5 are insulated by an insulating mica sheet 61; the furnace body 2 is mounted on the furnace bottom 5, the upper end of the frame-type agitator 9 is mounted in the agitator mounting port 24 at the center of the furnace cover 10, and the upper end of the freeze-thaw valve 62 is aligned with the leakage hole 50 and installed under the base 7; the furnace cover 10 is covered on the furnace body 2 through the furnace cover buckle 20 and the mounting buckle 11 of the upper circular water outlet distribution ring 12, so that the stainless steel metal ball 74 is above the leakage hole 50 of the furnace bottom 5, and the symmetry axis of the frame-type agitator 9, the center of the stainless steel metal ball 74, the center of the leakage hole 50, and the symmetry axis of the freeze-thaw valve 62 are on the same straight line;
[0061] 14 and 15 , there are two ways to install the freeze-thaw valve 62 on the furnace bottom 5: bolt-tightening freeze-thaw valve lug installation and thread-tightening installation. The following describes two installation embodiments of the freeze-thaw valve 62:
[0062] See also Fig.14A , 14B 14C Installation Example 1, the external shape of the freeze-thaw valve installation interface 51 of the furnace bottom 5 is conical and welded on the furnace bottom 5. Three L-shaped stainless steel blocks 68 are welded on the furnace bottom 5, and the L-shaped stainless steel blocks 68 have threaded holes, and the threaded holes have mounting bolts 69. The freeze-thaw valve 62 is made of platinum, and its upper end is a conical interface 64, and the taper is the same as the furnace bottom conical interface 51. Three mounting lugs 63 are welded at the conical interface 64. The lower end of the freeze-thaw valve is a cylinder 67 with an inner diameter of 16 mm. A water-cooled or air-cooled spiral tube 65 with a rectangular cross-section is welded to the upper end of the cylinder 67. The lower end of the cylinder 67 is a medium-frequency induction coil 66. During installation, the freeze-thaw valve lug 63 is located between two L-shaped stainless steel blocks 68, close to the furnace bottom, and then rotated counterclockwise to place the lug 63 above the L-shaped stainless steel block 68, and then tightened the three tightening bolts 69 to make the inner conical surface of the freeze-thaw valve conical interface 64 and the outer conical surface of the furnace bottom conical interface 51 fit closely to prevent glass from entering the gap between the two.
[0063] See also Fig.15A , 15B , 15C installation embodiment 2, with the center of the furnace bottom 5 as the center of the circle, a circular threaded hole 70 is welded. Fig. 15BThe structure diagram of the freeze-thaw valve 62 for installing Example 2 is shown below. The freeze-thaw valve 62 is made of nickel-chromium-iron alloy, and its upper end is a threaded interface 64, with threads on the outside, which matches the threaded hole 70 of the furnace bottom 5. The inner side of the threaded interface 64 is a cone, which matches the conical interface 51 of the furnace bottom 5. The lower end of the freeze-thaw valve 62 is a cylinder 71, and a water-cooled or air-cooled spiral tube 65 with a rectangular cross-section is welded to its upper end, and a medium-frequency induction coil 66 is provided at the lower end, and an octagonal nut 72 is welded in the middle. During installation, the freeze-thaw valve 62 is placed in the threaded hole 70 of the furnace bottom and tightened through the octagonal nut 72, so that the inner conical surface of the freeze-thaw valve threaded interface 64 and the outer conical surface of the conical interface 51 of the furnace bottom fit closely to prevent glass from entering the gap between the two.
[0064] See also Fig.16 The frame-type agitator 9 is a stainless steel water-cooled agitator, which is composed of a stirring rod 77, a stirring frame 73 and a stainless steel metal ball 74 at the lower end. The cooling water inside the frame-type agitator 9 flows from top to bottom through the water inlet pipes 75 on both sides of the stirring rod, the stirring frames 73 on both sides, and then turns back through the central pipe 76 of the stirring rod and then discharges water upward.
[0065] The use process of the glass melting furnace of the present invention is described as follows:
[0066] Add starting glass similar to the target product composition through the furnace cover charging port 23, and lower the frame agitator 9 after part of the starting glass enters the leakage hole 50 and the freeze-thaw valve 62 to block the leakage hole 50. Then continue to add starting glass to the furnace starting position, and place a metal zirconium ring on the starting glass. Turn on the cooling water of the glass melting furnace, the cooling water of the frame agitator, the cooling gas of the freeze-thaw valve and the bubbler gas, turn on the high-frequency power supply, and the induction coil 3 first heats the metal zirconium ring, which transfers heat to the starting glass to melt the starting glass. After the starting glass is completely melted, start to add product glass raw materials (powder raw materials, glass beads, mud or waste liquid) through the charging port 23. Since the furnace body and the furnace bottom are water-cooled, a glass shell of 5-10mm and 15-30mm is formed on the furnace wall and the furnace bottom respectively, so that the furnace wall and the furnace bottom do not directly contact the molten glass, which protects the furnace wall and the furnace body, prolongs the service life of the glass melting furnace, and maintains the original composition of the glass unaffected, thereby improving the glass performance. The liquid level is measured through the liquid level measuring port 17, the temperature is measured through the temperature measuring port 22, and the window 18 monitors the situation inside the furnace.
[0067] When the glass melting process parameters reach the target value, lift the frame agitator 9 to the stirring position and start rotating. When the glass liquid level reaches the leakage level, stop the spiral tube cooling 65 of the freeze-thaw valve 62, start the medium-frequency induction heating coil 66, and the glass starts to leak. When the leakage stops, start the spiral tube cooling 65, stop and lower the agitator 9, so that the metal ball 74 of the agitator 9 blocks the leakage hole 50 at the bottom of the furnace, gradually reduce the power of the medium-frequency induction heating coil 66, and drain the glass from the freeze-thaw valve. At the same time, the glass solidifies at the spiral cooling tube 65 of the freeze-thaw valve, and the glass leakage stops. After the glass leakage stops, lift the agitator 9 to enter the next cycle of glass melting.
Claims
1. A glass melting furnace, comprising a furnace body (2) and a refractory concrete base (7) having supporting legs (8), wherein the furnace body (2) is fixed to the base (7) by a screw rod (4), and the furnace body (2) is provided with a furnace cover (10) at the top and a furnace bottom (5) at the bottom. It is characterized in that The furnace cover (10) is a hollow structure, a cooling channel (25) with a rectangular cross section is welded inside the cavity, an air inlet (16) and an air outlet (19) are provided on the furnace cover (10), which are respectively connected to the cooling channel (25), a stirrer installation port (24) is provided at the center of the furnace cover (10), and the frame stirrer (9) extends into the furnace body (2); the furnace cover (10) is also provided with a liquid level measuring port (17), a viewing window (18), an exhaust gas discharge port (21), a temperature measuring port (22) and a feeding port (23); The furnace body (2) is a cylinder surrounded by a plurality of stainless steel sleeves (14), the top and bottom surfaces of which are welded by an upper circular water outlet distribution ring (12) and a lower circular water inlet distribution ring (13), each stainless steel sleeve (14) being composed of an inner tube (43), an outer tube (42) sleeved outside the inner tube (43), and a cover plate (47) covering the bottom of the outer tube (42), the inner tube (43) and the outer tube (42) being connected by a bracket (44), the upper end of the inner tube (43) being provided with a water outlet (45), and the upper end of the outer tube (42) being provided with a water inlet (46); The furnace bottom (5) is radially divided into petals (48), the central angle of each petal (48) is 30-45 degrees, the length of the petal slit (52) is 1 / 2-2 / 3 of the radius of the furnace bottom, the petal gap is filled with aluminate refractory cement, each petal (48) is provided with a bubbler (49), a water cooling box (57) is welded below each petal (48), the water cooling box (57) is divided into an outer water inlet box (58) and an inner water outlet box (59) by a metal plate (55), the volume of the water inlet box (58) is smaller than that of the water outlet box (59), and the water inlet box (58) and the water outlet box (59) are respectively installed with a water inlet pipe (53) and a water outlet pipe (54); a material leakage hole (50) is opened in the center of the furnace bottom (5), and a conical freeze-thaw valve (62) installation interface (51) is welded on the furnace bottom for connecting the freeze-thaw valve (62); The cooling water in the frame-type agitator (9) flows from top to bottom through the water inlet pipes (75) on both sides of the agitator rod, the agitator frames (73) on both sides, and then flows back through the central pipe (76) of the agitator rod and outward. The base (7) is provided with a mounting groove (60) for the furnace body (2), the furnace bottom (5) is mounted on the mounting groove (60), and the mounting groove (60) and the furnace bottom (5) are insulated by an insulating mica sheet (61); the furnace body (2) is mounted on the furnace bottom (5), the upper end of the frame-type agitator (9) is mounted in the agitator mounting opening (24) at the center of the furnace cover (10), and the upper end of the freeze-thaw valve (62) is aligned with the material leakage hole ( 50) is installed under the base (7); the furnace cover (10) is covered on the furnace body (2) through the furnace cover buckle (20) and the installation buckle (11) of the upper circular water outlet distribution ring (12), so that the stainless steel metal ball (74) is above the leakage hole (50) of the furnace bottom (5), and the symmetry axis of the frame agitator (9), the center of the stainless steel metal ball (74), the center of the leakage hole (50), and the symmetry axis of the freeze-thaw valve (62) are on the same straight line.
2. The glass melting furnace according to claim 1, It is characterized in that The upper circular water outlet distribution ring (12) and the lower circular water inlet distribution ring (13) are both divided into N partitions by partitions, with N being in the range of 8 to 16. N stainless steel sleeves (14) are connected in each partition, with n being in the range of 6 to 8. The gaps between adjacent stainless steel sleeves (14) are filled with mica sheets for insulation. The distance between the upper circular water outlet distribution ring (12) and the lower circular water inlet distribution ring (13) is 1 to 3 cm, and the effective volume in the cavity of the upper circular water outlet distribution ring (12) is greater than the effective volume in the cavity of the lower circular water inlet distribution ring (13).
3. The glass melting furnace according to claim 1 or 2, It is characterized in that The upper circular water outlet distribution ring (12) is welded together by a top cover (29), an upper circular outer plate (30), an upper circular bottom plate (31) and an upper circular inner plate (32), and is divided into N partitions by an upper circular partition plate (33). An upper circular water outlet pipe (26) and a pressure relief safety valve (27) are installed on the upper circular outer plate (30) of each partition. A stainless steel sleeve (14) inner tube (43) welding opening (28) is provided on the upper circular bottom plate (31). Two mounting buckles (11) are installed on the outer plate of the upper circular water outlet distribution ring (12); The lower circular water inlet distribution ring (13) is welded by a top plate (40), a lower circular outer plate (39), a lower circular bottom plate (38) and a lower circular inner plate (37), and is divided into N partitions by a lower circular partition plate (41). A lower circular water inlet pipe (36) is welded on the lower circular outer plate (39) of each partition. A stainless steel sleeve (14) outer tube (42) welding opening (35) is provided on the lower circular bottom plate (38), and a stainless steel sleeve (14) inner tube (43) welding opening (34) is provided on the top plate (40). The cooling water in the stainless steel sleeve (14) flows in the following directions: enters the outer tube (42) through the water inlet (46), flows downward along the outer tube (42), turns around the cover plate (47), flows upward along the inner tube (43), and flows out from the water outlet (45).
4. The glass melting furnace according to claim 1, It is characterized in that The freeze-thaw valve (62) is made of NiCrFe alloy or platinum. The freeze-thaw valve (62) is water-cooled or air-cooled by a rectangular cross-section spiral tube (65) and heated by an induction coil (66). The inner conical surface of the conical interface (64) at the upper end of the freeze-thaw valve (62) matches the furnace bottom installation interface (51). The freeze-thaw valve (62) is installed by bolt-tightening lug installation or thread-tightening installation: When the freeze-thaw valve (62) is installed in a threaded fastening manner, the conical interface (64) at the upper end of the freeze-thaw valve (62) is screwed into the threaded hole (70) at the furnace bottom and tightened by the octagonal nut (72) so that the inner conical surface of the conical interface (64) at the upper end of the freeze-thaw valve and the outer conical surface of the furnace bottom installation interface (51) are closely fitted; When the freeze-thaw valve (62) is installed in a bolt-tightening lug installation manner, three mounting lugs (63) are welded to the conical interface (64) at the upper end of the freeze-thaw valve (62), and three L-shaped stainless steel blocks (68) are welded to the furnace bottom (5). The L-shaped stainless steel blocks (68) have threaded holes, and mounting tightening bolts (69) are arranged in the threaded holes.
5. The glass melting furnace according to claim 1, It is characterized in that The furnace cover (10), furnace body (2), furnace bottom (5), and frame-type stirrer (9) are made of stainless steel 304 or 316. A buckle (20) for mounting with the furnace body (2) is provided on the outer wall of the furnace cover (10).
6. The glass melting furnace according to claim 1, It is characterized in that The frame-type stirrer (9) is a stainless steel water-cooled stirrer, which is composed of a stirring rod (77), a stirring frame (73) and a stainless steel metal ball (74) at the lower end.
7. The glass melting furnace according to claim 6, Features The diameter of the stainless steel metal ball (74) at the lower end of the frame-type agitator (9) is 30 to 50 mm.
8. The glass melting furnace according to claim 1 or 2, Features The inner tube (43) of the stainless steel sleeve (14) has a diameter of 8 to 18 mm and a wall thickness of 1 to 2 mm, and the outer tube (42) has a diameter of 16 to 30 mm and a wall thickness of 2 to 5 mm.
9. The glass melting furnace according to claim 1 or 2, Features The gap between adjacent split stainless steel sleeves (14) of the furnace body (2) is 1 to 2 mm, and the gap is filled with mica sheets for insulation.
10. The glass melting furnace according to claim 1, Features The bubbler (49) is located on a circle with the center of the furnace bottom (5) as the center.
11. The glass melting furnace according to claim 1, Features The distance between the water cooling box (57) and the center of the furnace bottom circle is 1 / 3 to 1 / 2 of the radius of the furnace bottom.
12. The glass melting furnace according to claim 1, Features The thickness of the furnace bottom (5) is 3-4 cm, the diameter of the upper end of the central leakage hole (50) is 20-30 mm, and it narrows downward at an angle of 10-15 degrees. A conical freeze-thaw valve (62) installation interface (51) is welded on the furnace bottom, and the interface also narrows downward at an angle of 10-15 degrees.
13. The glass melting furnace according to claim 1, Features The furnace bottom (5) is embedded in a refractory cement concrete base (7), and the refractory cement concrete base (7) is made of aluminate cement concrete, steel bars and glass fibers.
14. The glass melting furnace according to claim 1, Features The thickness of the insulating mica sheet (61) between the installation groove (60) and the furnace bottom (5) is 3 to 5 mm.