Stainless steel cabinet drilling process and structure

Through hot-melt drilling technology and intelligent quality control, the drilling thread generation function and hot-melt drilling function of stainless steel cabinet plates are realized, which solves the problems of low connection efficiency and short service life in the existing technology, and improves the strength of the cabinet. and aesthetics.

CN118720743APending Publication Date: 2024-10-01FOSHAN GAODE KITCHEN TECH CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410759568.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-13
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The existing technology cannot effectively realize the drilling thread generation function, surface treatment function, hot melt drilling function and strength support function of the drilling thread of stainless steel cabinet panels, resulting in low tension and torque on the thread during connection, low connection efficiency and waste material, short service life.

Method used

Hot melt drilling technology is used combined with high-speed rotation and axial thrust to drill holes and inner wall extrusions on stainless steel plates. The temperature is instantly raised to 650° to 750°C to form an inner wall that is about three times thicker. Then a tapping machine is used to Thread cutting on the inner wall, combined with intelligent quality control and optimization steps, ensures high precision and consistency in drilling and threading.

Benefits of technology

It improves the strength and reliability of stainless steel cabinet connections, simplifies the manufacturing process, saves material and time costs, extends the service life, and improves the overall quality of the product and user satisfaction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720743A_ABST
    Figure CN118720743A_ABST
Patent Text Reader

Abstract

The invention discloses a stainless steel cabinet drilling process and structure, and relates to the technical field of metal material drilling, and the stainless steel cabinet drilling process comprises the following steps: step S1, drilling a stainless steel cabinet plate by using a hot melting drilling process, generating violent friction between a drill bit and the plate through high-speed rotation and axial thrust, and raising the temperature to 650-750 DEG C; s2, after the temperature rises, the axial pressure continues to be applied, the inner wall is rapidly extruded on the surface of the plate, and the thickness of the inner wall is three times that of the initial plate; and S3, tapping is conducted on the inner wall through a tapping machine, and a thread structure is formed. By designing the thread generation step, the drilling thread generation function of the stainless steel plate is achieved, the problem that a traditional stainless steel cabinet plate needs to be perforated and additionally provided with an embedded part is solved, the tensile force and torsion borne by the thread during connection are effectively improved, connection is more efficient, more materials are saved, and the production cost is reduced. Meanwhile, the service life of the stainless steel cabinet is effectively prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metal material drilling, in particular to a stainless steel cabinet drilling process and structure. Background Art

[0002] Stainless steel cabinets are becoming increasingly popular in modern kitchens, mainly due to their corrosion resistance, durability and aesthetics. However, in the manufacturing process of stainless steel cabinets, especially in the connection and fixing of the plates, traditional processes have many challenges. Traditional processes usually require drilling holes in the plates and installing embedded parts, which is not only time-consuming and labor-intensive, but also easy to leave defects on the stainless steel plates, affecting the strength and aesthetics of the overall structure.

[0003] In order to solve these problems, the present application proposes a stainless steel cabinet drilling process and structure, which uses hot melt drilling technology, combined with high-speed rotation and adaptive axial thrust, to drill holes and squeeze the inner wall on the stainless steel plate. Under the high temperature condition of instantly raising the temperature to 650°~750°C, the plate area softens rapidly, and then forms an inner wall with a thickness of about three times that of the initial plate through axial pressure. Then, a tapping machine is used to cut threads on the inner wall to form a firm and precise thread structure.

[0004] This innovative process not only improves the strength and reliability of stainless steel cabinet connections, but also simplifies the manufacturing process, saving material and time costs. In addition, through intelligent quality control and optimization steps, the process can monitor and adjust key parameters in real time to ensure high precision and consistency in drilling and thread formation. The application of this technology effectively extends the service life of stainless steel cabinets and improves the overall product quality and user satisfaction.

[0005] Patent document CN104260146B discloses a BT plate drilling process. The above patent realizes simple operation and saves operation time. Moreover, through the precise measurement of the particularity of step one and step two, it can effectively ensure the reliability of accuracy during post-production. Through strict inspection in the later stage, the qualified rate of the product will be greatly improved. However, the above patent cannot realize the function of drilling and threading for stainless steel plates.

[0006] Patent document CN109209222B discloses a drilling process. The above patent achieves that there are basically no debris particles in the entire large hole, thereby ensuring the subsequent smooth drilling and improving the drilling efficiency. However, the above patent cannot achieve the surface treatment function of the plate.

[0007] Patent document CN107520907B discloses a tablet center hole drilling device and drilling process. The above patent realizes batch drilling, which has the advantages of saving production costs, high drilling effect and low loss, but the above patent cannot realize the hot melt drilling function of stainless steel cabinet panels.

[0008] Patent document CN114619514B discloses a secondary drilling process. The above patent can ensure that the alignment accuracy between the hole formed by the secondary drilling and the first drilled hole is high, thereby improving product quality. However, the above patent cannot achieve the strength support function for the drill thread.

[0009] In summary, the above patents cannot realize the function of generating drilling threads for stainless steel plates, the function of surface treatment of plates, the function of hot-melt drilling of stainless steel cabinet plates, and the function of strength support for drilling threads, resulting in small tension and torque on the threads when stainless steel cabinets are connected, low connection efficiency, waste of materials, and shortened service life of stainless steel cabinets; To this end, the present application proposes a stainless steel cabinet drilling process and structure that can realize the functions of drilling thread generation for stainless steel plates, surface treatment of plates, hot-melt drilling of stainless steel cabinet plates, and strength support for drilling threads. Summary of the invention

[0010] The purpose of the present invention is to provide a stainless steel cabinet drilling process and structure to solve the technical problems proposed in the above background technology that the drilling thread generation function of the stainless steel plate, the surface treatment function of the plate, the hot melt drilling function of the stainless steel cabinet plate and the strength support function of the drilling thread cannot be realized, resulting in small tension and torsion of the thread when the stainless steel cabinet is connected, low connection efficiency, waste of materials, and shortened service life of the stainless steel cabinet.

[0011] To achieve the above object, the present invention provides the following technical solution: a stainless steel cabinet drilling process, comprising the following steps: Step S1, using a hot melt drill process to drill holes on a stainless steel cabinet plate, causing intense friction between the drill bit and the plate through high-speed rotation and axial thrust, raising the temperature to 650 degrees Celsius to 750 degrees Celsius; Step S2, after the temperature rises, continue to apply axial pressure to quickly extrude an inner wall on the surface of the plate, and the thickness of the inner wall is 3 times that of the initial plate; Step S3: tapping the inner wall using a tapping machine to form a thread structure.

[0012] Preferably, the step S1 further includes step S11 and step S12: Step S11, select a drill bit of appropriate diameter, install it on the hot melt drill equipment as required, adjust the fixed position, and check the status and sharpness of the drill bit; before starting the equipment, confirm that the operator has worn protective gloves and goggles, start the hot melt drill equipment, slowly move the drill bit to the predetermined drilling position, and start the drilling process; during the drilling process, ensure that the stainless steel cabinet plate reaches the preset temperature range by real-time monitoring the heating temperature of the equipment, and adjust the heating temperature according to different plate materials and thicknesses to ensure the drilling effect and inner wall extrusion quality; Step S12: Install a temperature sensor in the drilling area to monitor the temperature changes of the drill bit and the plate in real time. The control system automatically adjusts the water spray volume and spray angle of the cooling system according to the real-time monitoring data to ensure that the temperature during the drilling process is stably controlled within a safe range.

[0013] Preferably, the step S2 further includes step S21: Step S21, after reaching the preset temperature, stop the rotation of the drill bit, maintain the axial thrust of the equipment, soften the material at high temperature, and monitor the softening state of the material in real time; when the material is softened, gradually increase the axial thrust so that the drill bit forms an inner wall on the surface of the plate, and control the thickness and shape of the inner wall to ensure smooth extrusion of the inner wall and avoid deformation or breakage of the metal material. After completing the extrusion of the inner wall, stop heating, cool the plate to room temperature, and inspect the cooled plate to ensure that the quality of the inner wall and the thread structure meet the requirements.

[0014] Preferably, the step S3 further includes step S31: Step S31, after the inner wall is extruded, use a tapping machine to cut threads on the inner wall. According to the design requirements and standard specifications, select appropriate tapping tools and parameters to ensure that the size and shape of the thread meet the requirements; inspect and test the formed threads, use a thread measuring instrument to perform precise measurements, and confirm that the size, pitch and tolerance of the threads meet the design standards; after the thread is formed, clean the surface of the plate, and perform anti-corrosion treatment and surface coating as needed to improve the corrosion resistance and aesthetics of the connection structure.

[0015] Preferably, the step S1 also includes pre-drilling processing, and the pre-drilling processing steps are as follows: Plate preparation: Before drilling, check the stainless steel cabinet plate to ensure that the surface is flat, free of cracks and stains, clean the plate surface, remove oil and impurities, and ensure a clean operating environment during drilling; Equipment settings: Set the working parameters of the hot melt drill equipment, including rotation speed, axial thrust and heating temperature, and equipment safety protection measures in the working area to ensure the safety of operators; Process plan confirmation: According to the design requirements and actual conditions, confirm the drilling location and quantity, as well as the specifications and dimensions of the thread structure, and conduct a comprehensive assessment of the process flow to ensure that the sequence of each step and the operation method are reasonable and effective; Step S2 also includes an intelligent quality control stage, and the processing steps of the intelligent quality control stage are as follows: Install sensors in the drilling area to monitor the temperature, pressure and vibration parameters in real time during the drilling process, detect abnormal conditions in time and issue alarms; Collect and analyze real-time monitoring data during the drilling process, establish a drilling quality prediction model, optimize drilling parameters and process flow based on the analysis results, and provide timely feedback to the production system to achieve closed-loop control and continuous optimization.

[0016] Preferably, the step S1 further includes a drilling optimization step, which is as follows: Before drilling, the stainless steel plate should be degreased, polished and cleaned to ensure that the surface is flat and clean to reduce friction and resistance during drilling; The introduction of an intelligent positioning system automatically identifies the position and size of the plate through image recognition / laser measurement technology, performs high-precision positioning and alignment, and automatically adjusts the rotation speed, feed speed and cutting depth of the drill bit by combining real-time monitoring data and machine learning algorithms. It uses stainless steel plates of different materials and thicknesses to improve drilling efficiency and quality.

[0017] Preferably, the step S2 further includes an extrusion optimization step, which is as follows: An intelligent control system is used to control the extrusion process. The pressure sensor and displacement sensor installed inside the drill bit monitor the axial force and displacement changes during the extrusion process in real time. The intelligent control system uses real-time monitoring data to adjust the working pressure of the hydraulic system and the oil pump speed to intelligently control the axial thrust and speed during the extrusion process, thereby achieving precise control of the inner wall extrusion thickness.

[0018] Preferably, the step S3 further includes a thread optimization step, and the thread optimization step is as follows: The data system is used to control the working parameters of the tapping machine. According to the preset thread specifications and sizes, the CNC system automatically adjusts the cutting parameters to achieve efficient and accurate thread cutting. A high-resolution camera is used to capture the surface image of the thread after cutting. Image processing and machine learning algorithms are used to analyze and identify the thread image, automatically detect the size, shape and quality of the thread, and generate a corresponding thread inspection report to facilitate the optimization and improvement of the thread generation parameters.

[0019] Preferably, the stainless steel cabinet plate used in the drilling process step S1 is 304 stainless steel plate with a thickness of 1.0mm~1.5mm, good corrosion resistance and mechanical properties, suitable for long-term use in a humid kitchen environment, the drilling diameter is Φ6mm~Φ10mm, and the depth is determined according to the length and thickness of the connecting piece to ensure that the connecting piece can be completely embedded in the plate, and the drilling size and specification match the size and thread specification of the connecting piece to ensure that the connecting piece can be firmly fixed in the plate and is not easy to loosen; reinforcing ribs and supporting structures are added around the drilling structure to improve the bearing capacity and stability of the drilling area to prevent deformation and fracture of the plate due to load.

[0020] Preferably, in step S1 of the drilling process, during the drilling process, a cooling and lubrication system is used to cool and lubricate the drill bit and the plate to reduce heat accumulation and friction loss, and the periphery of the drilling structure is deburred and polished to make the drill hole smooth and flat, thereby improving the overall aesthetics and tactile comfort.

[0021] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention realizes the function of drilling and threading stainless steel plates by designing a thread generation step, which solves the problem that traditional stainless steel cabinet plates need to be drilled and pre-embedded, effectively increases the tension and torsion that the threads can withstand during connection, makes the connection more efficient, saves more materials, and effectively prolongs the service life of stainless steel cabinets; 2. The present invention realizes the surface treatment function of the plate by designing a pre-drilling treatment step, preventing the surface dirt from affecting the drilling process, reducing friction and wear during the drilling process, and ensuring that the surface of the material is free of dirt, thereby improving the aesthetics; 3. The present invention realizes the hot-melt drilling function of the stainless steel cabinet plate by designing a drilling step, ensuring the uniformity of the hole diameter in the drilling area, improving the connection's ability to withstand tension and torsion, and ensuring the cabinet's use strength and service life; 4. The present invention realizes the strength support function for the drill thread by designing an extrusion step, thereby increasing the load range of the cabinet connection and making the connection more efficient and stronger. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of hot melt drilling of the present invention; Figure 2 It is a schematic diagram of the extruded inner wall of the present invention; Figure 3 It is a schematic diagram of thread generation of the present invention; Figure 4 It is a schematic diagram of the drilling process flow of the present invention. DETAILED DESCRIPTION

[0023] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0024] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "front end", "rear end", "two ends", "one end", "the other end" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.

[0025] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. Example

[0026] See also Figure 1 , Figure 2 and Figure 3 , an embodiment provided by the present invention: a stainless steel cabinet drilling process, comprising the following steps: Step S1, using a hot melt drill process to drill holes on a stainless steel cabinet plate, causing intense friction between the drill bit and the plate through high-speed rotation and axial thrust, raising the temperature to 650 degrees Celsius to 750 degrees Celsius; Step S2, after the temperature rises, continue to apply axial pressure to quickly extrude an inner wall on the surface of the plate, and the thickness of the inner wall is 3 times that of the initial plate; Step S3, tapping the inner wall using a tapping machine to form a thread structure; Further, process preparation: place the stainless steel cabinet plate on the processing table, prepare the hot melt drill and tapping machine equipment, start the hot melt drill equipment, place the drill bit on the surface of the plate, and apply appropriate axial thrust and rotation speed to generate high-temperature friction between the drill bit and the plate to form a cavity. During the drilling process, as the temperature rises, continue to apply axial pressure to form extrusion inside the plate and increase the internal thickness to 3 times that of the initial plate. After drilling is completed, place the tapping machine inside the drill hole and perform tapping operations to form a threaded structure. Inspect the drilling quality to ensure that the hole diameter, depth and thread size meet the design requirements, perform necessary finishing and lubrication, and achieve no need for pre-drilling and adding embedded parts, saving time and labor costs, improving connection efficiency and quality, and extending the service life of the stainless steel cabinet. The hot melt drill process and extrusion technology make the connection more secure and not easy to loosen. Example

[0027] See also Figure 1 and Figure 4 , an embodiment provided by the present invention: a stainless steel cabinet drilling process, the step S1 further includes step S11 and step S12: Step S11, select a drill bit of appropriate diameter, install it on the hot melt drill equipment as required, adjust the fixed position, and check the status and sharpness of the drill bit; before starting the equipment, confirm that the operator has worn protective gloves and goggles, start the hot melt drill equipment, slowly move the drill bit to the predetermined drilling position, and start the drilling process; during the drilling process, ensure that the stainless steel cabinet plate reaches the preset temperature range by real-time monitoring the heating temperature of the equipment, and adjust the heating temperature according to different plate materials and thicknesses to ensure the drilling effect and inner wall extrusion quality; Step S12: Install a temperature sensor in the drilling area to monitor the temperature changes of the drill bit and the plate in real time. The control system automatically adjusts the water spraying amount and spraying angle of the cooling system according to the real-time monitoring data to ensure that the temperature during the drilling process is stably controlled within a safe range; Furthermore, when selecting a drill bit of appropriate diameter, determine the appropriate drill bit specifications according to the plate thickness and the size of the connector, install the selected drill bit on the hot melt drill equipment, and adjust the fixed position to ensure the alignment and stability between the drill bit and the plate. Before starting the equipment, the operator needs to wear protective gloves and goggles to ensure safe operation; A temperature sensor is installed in the drilling area to ensure that the temperature changes of the drill bit and the plate can be accurately monitored. The hot melt drill equipment is started, the drill bit is slowly moved to the predetermined drilling position, and the drilling process begins. The heating temperature of the equipment is monitored in real time to ensure that the stainless steel cabinet plate reaches the preset temperature range. The heating temperature is adjusted according to the monitoring data to ensure the drilling effect and the inner wall extrusion quality. The control system automatically adjusts the water spray volume and spray angle of the cooling system according to the real-time monitoring data to ensure that the temperature during the drilling process is stably controlled within a safe range. The above-mentioned implementation method adopts the intelligent monitoring and adjustment of the temperature sensor and the control system to realize the precise control of the temperature during the drilling process, thereby improving the quality and safety of the drilling. Example

[0028] See also Figure 2 and Figure 4 , an embodiment provided by the present invention: a stainless steel cabinet drilling process, step S2 also includes step S21: Step S21, after reaching the preset temperature, stop the rotation of the drill bit, maintain the axial thrust of the equipment, soften the material at high temperature, and monitor the softening state of the material in real time; when the material is softened, gradually increase the axial thrust so that the drill bit forms an inner wall on the surface of the plate, and control the thickness and shape of the inner wall to ensure that the inner wall extrusion process is smooth and avoid deformation or breakage of the metal material. After the inner wall extrusion is completed, stop heating, cool the plate to room temperature, and inspect the cooled plate to ensure that the quality of the inner wall and the thread structure meet the requirements; Step S2 also includes an intelligent quality control stage, and the processing steps of the intelligent quality control stage are as follows: Install sensors in the drilling area to monitor the temperature, pressure and vibration parameters in real time during the drilling process, detect abnormal conditions in time and issue alarms; Collect and analyze real-time monitoring data during the drilling process, establish a drilling quality prediction model, optimize drilling parameters and process flow based on the analysis results, and promptly feed back to the production system to achieve closed-loop control and continuous optimization; Furthermore, during the drilling process, when the stainless steel cabinet plate reaches the preset temperature, the rotation of the drill bit is automatically stopped, and the equipment maintains the axial thrust unchanged to soften the material at high temperature. At the same time, the softening state of the material is monitored in real time. When the material is softened, the axial thrust is gradually increased to allow the drill bit to form an inner wall on the surface of the plate, and the thickness and shape of the inner wall are controlled to ensure that the inner wall extrusion process is smooth. After the inner wall extrusion is completed, the heating is stopped and the plate is cooled to room temperature to solidify the inner wall structure. The cooled plate is inspected to ensure that the quality of the inner wall and the thread structure meet the requirements. Install temperature, pressure, vibration and other sensors in the drilling area to monitor key parameters and data in real time during the drilling process. When abnormal conditions are found, the alarm system is triggered immediately to notify relevant personnel to handle the situation. Collect and analyze real-time monitoring data during the drilling process, establish a drilling quality prediction model to evaluate drilling quality and performance, and optimize drilling parameters and process flow based on the model analysis results, such as adjusting heating temperature, axial thrust, etc., to improve drilling quality and efficiency. Feedback the optimization results to the production system in a timely manner to achieve closed-loop control and continuous optimization, and ensure the stability and efficiency of the production process. The intelligent quality control stage in this embodiment adopts sensor monitoring and data analysis technology to realize intelligent monitoring and optimization adjustment of the drilling process, thereby improving production efficiency and product quality. Example

[0029] See also Figure 3 and Figure 4 , an embodiment provided by the present invention: a stainless steel cabinet drilling process, step S3 also includes step S31: Step S31, after the inner wall is extruded, the inner wall is threaded using a tapping machine, and appropriate tapping tools and parameters are selected according to the design requirements and standard specifications to ensure that the size and shape of the thread meet the requirements; the formed thread is inspected and tested, and a thread measuring instrument is used for precise measurement to confirm that the size, pitch and tolerance of the thread meet the design standards; after the thread is formed, the surface of the plate is cleaned, and anti-corrosion treatment and surface coating are performed as needed to improve the corrosion resistance and aesthetics of the connection structure; Step S3 also includes a thread optimization step, which is as follows: The data system is used to control the working parameters of the tapping machine. According to the preset thread specifications and sizes, the CNC system automatically adjusts the cutting parameters to achieve efficient and accurate thread cutting. A high-resolution camera is used to capture the surface image of the thread after cutting. Image processing and machine learning algorithms are used to analyze and identify the thread image, automatically detect the size, shape and quality of the thread, and generate the corresponding thread inspection report, which is convenient for optimizing and improving the thread generation parameters. Furthermore, after the inner wall is extruded, the plate is moved to the working area of ​​the tapping machine, and the inner wall is threaded using a suitable tapping tool and parameters. According to the design requirements and standard specifications, the formed thread is accurately measured using a thread measuring instrument to confirm that the size, pitch and tolerance of the thread meet the design standards. After the thread is formed, the surface of the plate is cleaned, and anti-corrosion treatment and surface coating are performed as needed to improve the corrosion resistance and aesthetics of the connection structure. Use the CNC system to control the working parameters of the tapping machine, automatically adjust the cutting parameters according to the preset thread specifications and sizes, and achieve efficient and accurate thread cutting. Use a high-resolution camera to capture the surface image of the thread after cutting, and use image processing and machine learning algorithms to analyze and identify the thread image, automatically detect the size, shape and quality of the thread, and generate the corresponding thread inspection report, so as to optimize and improve the thread generation parameters; In the above embodiments, the thread forming process and the thread optimization step are interconnected, and through automated control and detection, the quality and accuracy of the thread are ensured, thereby improving production efficiency and product quality. Example

[0030] See also Figure 1 , an embodiment provided by the present invention: a stainless steel cabinet drilling process, step S1 also includes a drilling optimization step, the drilling optimization step is as follows: Before drilling, the stainless steel plate should be degreased, polished and cleaned to ensure that the surface is flat and clean to reduce friction and resistance during drilling; The introduction of intelligent positioning system, through image recognition / laser measurement technology, automatically identifies the position and size of the plate, performs high-precision positioning and alignment, combines real-time monitoring data and machine learning algorithms to automatically adjust the rotation speed, feed speed and cutting depth of the drill bit, and uses stainless steel plates of different materials and thicknesses to improve drilling efficiency and quality; The step S2 also includes an extrusion optimization step, which is as follows: The extrusion process is controlled by an intelligent control system. The axial force and displacement changes during the extrusion process are monitored in real time by the pressure sensor and displacement sensor installed inside the drill bit. The intelligent control system is used to adjust the working pressure of the hydraulic system and the oil pump speed according to the real-time monitoring data to intelligently control the axial thrust and speed during the extrusion process, thereby achieving precise control of the inner wall extrusion thickness. Furthermore, the surface of the stainless steel sheet is treated with a suitable degreasing agent to remove oil and impurities, and then polished to make the surface of the sheet flat and smooth. Finally, it is cleaned to ensure that the surface is free of dust and debris. The intelligent positioning system is started to automatically identify the position and size of the sheet through image recognition or laser measurement technology. The system positions and aligns the sheet to ensure accurate drilling positions. According to the material and thickness of the sheet, the machine parameters and drill specifications are adjusted. The rotation speed, feed speed and cutting depth during the drilling process are monitored in real time. Combined with machine learning algorithms, the working parameters of the drill bit are automatically adjusted to achieve the best drilling efficiency and quality. An intelligent control system is introduced to control the extrusion process. Pressure sensors and displacement sensors are installed inside the drill bit to monitor the axial force and displacement changes during the extrusion process in real time. Based on the real-time monitoring data, the working pressure and oil pump speed of the hydraulic system are adjusted through the intelligent control system to achieve intelligent control of the axial thrust and speed during the extrusion process, so as to accurately control the inner wall extrusion thickness. In the above-mentioned embodiment, the drilling preparation and optimization process covers degreasing, grinding and cleaning, as well as the application of the intelligent positioning system and the optimization and adjustment of the drilling parameters, which can improve the accuracy, efficiency and quality of the drilling process. The extrusion optimization process introduces an intelligent control system, which realizes precise control of the extrusion process through real-time monitoring and adjustment, thereby improving the quality and stability of the inner wall extrusion. Example

[0031] See also Figure 1 , an embodiment provided by the present invention: a stainless steel cabinet drilling process, the step S1 also includes drilling pre-processing, the drilling pre-processing steps are as follows: Plate preparation: Before drilling, check the stainless steel cabinet plate to ensure that the surface is flat, free of cracks and stains, clean the plate surface, remove oil and impurities, and ensure a clean operating environment during drilling; Equipment settings: Set the working parameters of the hot melt drill equipment, including rotation speed, axial thrust and heating temperature, and equipment safety protection measures in the working area to ensure the safety of operators; Process plan confirmation: According to the design requirements and actual conditions, confirm the drilling location and quantity, as well as the specifications and dimensions of the thread structure, and conduct a comprehensive assessment of the process flow to ensure that the sequence of each step and the operation method are reasonable and effective; Further, check the stainless steel cabinet plate to ensure that the surface is flat, free of cracks and stains, clean the plate surface, remove oil and impurities, keep the operating environment clean to reduce friction and resistance during drilling, set the working parameters of the hot melt drill equipment, including rotation speed, axial thrust and heating temperature, adjust according to the thickness and material of the plate, set equipment safety protection measures in the working area, including safety helmets, goggles, protective gloves, etc., to ensure the safety of operators, confirm the drilling position and number according to design requirements and actual conditions, determine the specifications and dimensions of the threaded structure, including parameters such as thread diameter and pitch, and conduct a comprehensive evaluation of the process to ensure that each step sequence and operation method is reasonable and effective.

[0032] Working principle: First, pre-drilling treatment is carried out. Check the stainless steel cabinet plate to ensure that the surface is flat, free of cracks and stains. Clean the plate surface to remove oil and impurities, keep the operating environment clean, reduce friction and resistance, set the working parameters of the hot melt drill equipment, including rotation speed, axial thrust and heating temperature, and adjust them according to the thickness and material of the plate. Set equipment safety protection measures in the working area, such as safety helmets, goggles, protective gloves, etc., to ensure the safety of operators; Then the drilling process is carried out. The drill bit rotates at high speed and applies an appropriate axial thrust, causing intense friction between the drill bit and the plate, instantly heating the drill bit and the stainless steel plate to a temperature of 650° to 750° Celsius, rapidly softening the plate area, applying axial pressure, and quickly squeezing out an inner wall about 3 times the thickness of the initial plate on the surface of the plate; Finally, the thread generation process is carried out. A tapping machine is used to cut threads on the inner wall. According to the design requirements and standard specifications, appropriate tapping tools and parameters are selected to ensure that the size and shape of the thread meet the requirements. The formed threads are inspected and tested, and thread measuring instruments are used for precise measurement to confirm that the size, pitch and tolerance of the threads meet the design standards. The surface of the plate is cleaned, and anti-corrosion treatment and surface coating are performed as needed to improve the corrosion resistance and aesthetics of the connection structure.

[0033] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and range of equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.

Claims

1. A stainless steel cabinet drilling process, characterized by: The following steps are involved: Step S1, using a hot melt drill process to drill holes on a stainless steel cabinet plate, causing intense friction between the drill bit and the plate through high-speed rotation and axial thrust, raising the temperature to 650 degrees Celsius to 750 degrees Celsius; Step S2, after the temperature rises, continue to apply axial pressure to quickly extrude an inner wall on the surface of the plate, and the thickness of the inner wall is 3 times that of the initial plate; Step S3: tapping the inner wall using a tapping machine to form a thread structure.

2. A stainless steel cabinet drilling process according to claim 1, characterized in that: The step S1 also includes step S11 and step S12: Step S11, select a drill bit of appropriate diameter, install it on the hot melt drill equipment as required, adjust the fixed position, and check the status and sharpness of the drill bit; before starting the equipment, confirm that the operator has worn protective gloves and goggles, start the hot melt drill equipment, slowly move the drill bit to the predetermined drilling position, and start the drilling process; during the drilling process, ensure that the stainless steel cabinet plate reaches the preset temperature range by real-time monitoring the heating temperature of the equipment, and adjust the heating temperature according to different plate materials and thicknesses to ensure the drilling effect and inner wall extrusion quality; Step S12: Install a temperature sensor in the drilling area to monitor the temperature changes of the drill bit and the plate in real time. The control system automatically adjusts the water spray volume and spray angle of the cooling system according to the real-time monitoring data to ensure that the temperature during the drilling process is stably controlled within a safe range.

3. A stainless steel cabinet drilling process according to claim 1, characterized in that: The step S2 also includes step S21: Step S21, after reaching the preset temperature, stop the rotation of the drill bit, maintain the axial thrust of the equipment, soften the material at high temperature, and monitor the softening state of the material in real time; when the material is softened, gradually increase the axial thrust so that the drill bit forms an inner wall on the surface of the plate, and control the thickness and shape of the inner wall to ensure smooth extrusion of the inner wall and avoid deformation or breakage of the metal material. After completing the extrusion of the inner wall, stop heating, cool the plate to room temperature, and inspect the cooled plate to ensure that the quality of the inner wall and the thread structure meet the requirements.

4. A stainless steel cabinet drilling process according to claim 1, characterized in that: The step S3 also includes step S31: Step S31, after the inner wall is extruded, use a tapping machine to cut threads on the inner wall. According to the design requirements and standard specifications, select appropriate tapping tools and parameters to ensure that the size and shape of the thread meet the requirements; inspect and test the formed threads, use a thread measuring instrument to perform precise measurements, and confirm that the size, pitch and tolerance of the threads meet the design standards; after the thread is formed, clean the surface of the plate, and perform anti-corrosion treatment and surface coating as needed to improve the corrosion resistance and aesthetics of the connection structure.

5. The stainless steel cabinet drilling process according to claim 1, characterized in that: The step S1 also includes pre-drilling processing, and the pre-drilling processing steps are as follows: Plate preparation: Before drilling, check the stainless steel cabinet plate to ensure that the surface is flat, free of cracks and stains, clean the plate surface, remove oil and impurities, and ensure a clean operating environment during drilling; Equipment settings: Set the working parameters of the hot melt drill equipment, including rotation speed, axial thrust and heating temperature, and equipment safety protection measures in the working area to ensure the safety of operators; Process plan confirmation: According to the design requirements and actual conditions, confirm the drilling location and quantity, as well as the specifications and dimensions of the thread structure, and conduct a comprehensive assessment of the process flow to ensure that the sequence of each step and the operation method are reasonable and effective; Step S2 also includes an intelligent quality control stage, and the processing steps of the intelligent quality control stage are as follows: Install sensors in the drilling area to monitor the temperature, pressure and vibration parameters in real time during the drilling process, detect abnormal conditions in time and issue alarms; Collect and analyze real-time monitoring data during the drilling process, establish a drilling quality prediction model, optimize drilling parameters and process flow based on the analysis results, and provide timely feedback to the production system to achieve closed-loop control and continuous optimization.

6. A stainless steel cabinet drilling process according to claim 1, characterized in that: The step S1 also includes a drilling optimization step, which is as follows: Before drilling, the stainless steel plate should be degreased, polished and cleaned to ensure that the surface is flat and clean to reduce friction and resistance during drilling; The introduction of an intelligent positioning system automatically identifies the position and size of the plate through image recognition / laser measurement technology, performs high-precision positioning and alignment, and automatically adjusts the rotation speed, feed speed and cutting depth of the drill bit by combining real-time monitoring data and machine learning algorithms. It uses stainless steel plates of different materials and thicknesses to improve drilling efficiency and quality.

7. The stainless steel cabinet drilling process according to claim 1, characterized in that: The step S2 also includes an extrusion optimization step, which is as follows: An intelligent control system is used to control the extrusion process. The pressure sensor and displacement sensor installed inside the drill bit monitor the axial force and displacement changes in the extrusion process in real time. The intelligent control system uses real-time monitoring data to adjust the working pressure of the hydraulic system and the oil pump speed to intelligently control the axial thrust and speed in the extrusion process, thereby achieving precise control of the inner wall extrusion thickness.

8. The stainless steel cabinet drilling process according to claim 1, characterized in that: The step S3 also includes a thread optimization step, which is as follows: The data system is used to control the working parameters of the tapping machine. According to the preset thread specifications and sizes, the CNC system automatically adjusts the cutting parameters to achieve efficient and accurate thread cutting. A high-resolution camera is used to capture the surface image of the thread after cutting. Image processing and machine learning algorithms are used to analyze and identify the thread image, automatically detect the size, shape and quality of the thread, and generate a corresponding thread inspection report to facilitate the optimization and improvement of the thread generation parameters.

9. A stainless steel cabinet drilling structure, applicable to a stainless steel cabinet drilling process according to any one of claims 1 to 8, characterized in that: The stainless steel cabinet plate used in the drilling process step S1 is 304 stainless steel plate with a thickness of 1.0mm~1.5mm, good corrosion resistance and mechanical properties, suitable for long-term use in a humid kitchen environment, the drilling diameter is Φ6mm~Φ10mm, and the depth is determined according to the length and thickness of the connector to ensure that the connector can be completely embedded in the plate. The drilling size and specification match the size and thread specification of the connector to ensure that the connector can be firmly fixed in the plate and is not easy to loosen; reinforcing ribs and supporting structures are added around the drilling structure to improve the bearing capacity and stability of the drilling area to prevent deformation and fracture of the plate due to load.

10. The stainless steel cabinet drilling structure according to claim 9, characterized in that: In step S1 of the drilling process, during the drilling process, a cooling and lubrication system is used to cool and lubricate the drill bit and the plate to reduce heat accumulation and friction loss, and the periphery of the drilling structure is deburred and polished to make the drilling mouth smooth and improve the overall aesthetics and tactile comfort.

Citation Information

Cited By

  • Preparation method of electric motorcycle battery pack box body

    CN122539093A

  • Method for manufacturing an electric motorbike battery pack case

    CN122539093B