Measurement and control method for overhaul oxidation operation of nuclear power plant

By purifying, dosing and measuring control of oxidation operation during overhaul of nuclear power plant, the problems of unsatisfactory oxidation operation effect and low measurement accuracy are solved, the radiation dose and operating costs are reduced, and the oxidation operation effect and measurement accuracy are improved. sex.

CN118942752AActive Publication Date: 2024-11-12CNNC NUCLEAR POWER OPERATION MANAGEMENT CO LTD

Patent Information

Application Number
CN202410961656.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-12
Estimated Expiration
2044-07-18

AI Technical Summary

Technical Problem

During the overhaul of the nuclear power plant, the oxidation operation process has problems such as cumbersome measurement methods, low accuracy and unsatisfactory oxidation operation effect, and lack of effective control and detection methods, resulting in an increase in radiation dose and a decrease in heat transfer efficiency.

Method used

Provide a measurement and control method for oxidation operation of nuclear power plant overhaul, including purification of the exchange water tank before overhaul, operation control of the second desalter, injection of hydrogen peroxide solution and sample sampling during oxidation operation, gamma nuclide The measurement and calibration of the spectrum and the operation time control of the main pump form a complete set of chemical control and analysis methods.

Benefits of technology

Through this method, the radiation dose during the oxidation operation is reduced, filter blockage is avoided, oxidation operation effect and measurement accuracy are improved, operating costs are reduced, and operation is simplified, and safety is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118942752A_ABST
    Figure CN118942752A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of nuclear power, and particularly relates to a measurement and control method for overhaul oxidation operation of a nuclear power plant. The invention provides a complete set of chemical control and analysis method for overhaul oxidation operation of a nuclear power plant through preparation of overhaul oxidation operation, dosing and control and measurement of an oxidation operation platform, parameters and control and analysis means of each stage are determined, the oxidation operation effect and the measurement level are improved, and the method is suitable for large-scale popularization and application. Meanwhile, the method is easy to operate, cost is remarkably reduced, safety is high, and wide application and popularization can be achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of nuclear power technology, and in particular relates to a method for measuring and controlling oxidation operation of a nuclear power plant during overhaul. Background Art

[0002] In the operation of pressurized water reactor nuclear power plants, corrosion products produced by corrosion or wear on the surface of equipment such as primary circuit pipelines often form surface oxide films, or dissolve or suspend in the primary circuit water in small amounts, and flow with the flow of primary circuit coolant, and partially deposit on the surface of metals, especially in dead corners and narrow gaps between equipment and pipelines. These products are very easy to generate corrosion activation products under neutron irradiation. During the shutdown process of nuclear power plant units, due to the cooling and pressure reduction of the reactor, the rapid increase in boron concentration, the decrease in dissolved hydrogen, the entry of air and other factors, the reactor coolant system changes from an alkaline and reducing environment to an acidic and oxidizing environment, which greatly increases the solubility of corrosion products in the coolant. If they are not effectively removed and controlled, the dose level of overhaul and maintenance workers will be greatly increased. Long-term accumulation of corrosion products will also cause local blockage and reduced heat transfer efficiency. Therefore, in the specific stage of cooling and pressure reduction of the unit, an oxidation operation process is carried out in the primary circuit, which can not only remove the released oxidation activation products, but also form an oxide film on the inner wall surface of the pipeline, further slowing down or preventing the generation of activation products. However, in the current oxidation operation process, there are problems such as unsatisfactory oxidation operation effect; the measurement method of oxidation operation radionuclides is cumbersome and inaccurate, and there is no method control and detection method for the oxidation operation process. Summary of the invention

[0003] In order to overcome the problems existing in the related technologies, a method for measuring and controlling oxidation operation during overhaul of a nuclear power plant is provided.

[0004] According to one aspect of an embodiment of the present disclosure, a method for measuring and controlling oxidation operation of a nuclear power plant overhaul is provided, the method comprising:

[0005] Step 101, pre-overhaul control: before the overhaul, the first desalter is put into operation to purify the first refueling water tank. Under the action of the cooling circulation pump, the refueling water tank purification circuit flows through the first filter, the first desalter, and the second filter at a preset flow rate for a preset time;

[0006] Step 102, control of the operation of the second desalter during the down-going phase of overhaul: the second desalter is put into operation after the reactor reaches a preset subcritical time. During the down-going phase of overhaul, the second line is used as a downflow loop, and the second line is a downflow loop composed of a reactor pressure vessel, a reactor coolant pump, a third filter, a second desalter, and a fourth filter connected in series in this order;

[0007] Step 103, preparation and implementation of oxidation operation in the down stage of overhaul: at the beginning of the overhaul oxidation operation, a preset volume and a preset concentration of hydrogen peroxide solution are all injected into the chemical mixing and dosing box at one time, and when the hydrogen peroxide solution reaches a preset temperature, the hydrogen peroxide solution is injected into the primary circuit, and then samples are taken at 10, 20, 30, 45, 60 minutes, 2 hours, 3 hours, 4 hours, and 6 hours respectively to observe the change trends of Co-58, Co-60, Sb-122, Sb-124, Ag-110m, I-131, Xe-133 and total γ;

[0008] Step 104, measurement of oxidation operation during the down-going phase of overhaul: measure and obtain the γ-nuclides spectrum of the preset volume standard mixed radioactive source, so that the area counts of each main peak reach the preset threshold, input the energy peak on the γ-nuclides spectrum into the activity, calibration date, and uncertainty information of the corresponding nuclides on the standard source certificate, fit the efficiency curve, and complete the efficiency calibration;

[0009] Step 105, operation control of the oxidation operation main pump during the overhaul down stage: the operation purification time of the overhaul oxidation operation main pump is controlled to be 18 hours.

[0010] In a possible implementation, the resin volume of the first desalter 4 is 1.5m 3 The maximum working pressure is 0.05MPa.g, the maximum working temperature is 60℃, and the maximum working flow rate is 65m 3 / h, at 60m 3 / h flow rate for purification.

[0011] In a possible implementation, before the overhaul unit is decoupled, the 0.1 μm filter element of the third filter is replaced with a 0.45 μm filter element, and the replacement pressure difference is adjusted to 0.25 MPa.

[0012] In a possible implementation, in an actual measurement process, 1 g of the main system sample is taken during the oxidation operation and diluted to 20 g with high-purity water for measurement, and the measurement time is 100 seconds.

[0013] In a possible implementation, before measurement, a high-purity germanium multi-channel gamma spectrometer and the above-mentioned mixed standard solution source with a preset volume are used to measure radioactive nuclides, and a nuclide library dedicated to oxidation operation is established.

[0014] The beneficial effects of the present disclosure are:

[0015] The present invention provides a chemical control and analysis method for overhaul oxidation operation through preparation for overhaul oxidation operation, dosing, control and measurement of oxidation operation platform, and purification, providing a complete solution for the current mainstream oxidation operation process of pressurized water reactor nuclear power plants.

[0016] The present invention implements a strategy for purifying the refueling water tank and replacing the third filter before overhaul, which not only reduces the source of radiation dose during oxidation operation, but also avoids the problem of frequent clogging of the third filter during water tank filling, which affects the overhaul period and increases the workload of overhaul personnel.

[0017] The present invention purifies the main system by controlling the operation of the second desalter in the down-going phase of overhaul to replace the traditional third or fourth desalter through the chemical and volume control system downflow loop, with excellent results, while greatly reducing the operating costs and the additional re-commissioning work of the fifth desalter for removing the lithium bed.

[0018] The present invention obtains a testing method with good peak shape, stable and reliable results by setting test conditions, controlling sample sampling amount and selecting measurement activity time.

[0019] In summary, the present disclosure provides a complete set of chemical control and analysis methods for nuclear power plant overhaul oxidation operation through preparation for overhaul oxidation operation, dosing, control and measurement of oxidation operation platform, and purification. The parameters and control and analysis methods of each stage are clarified to improve the oxidation operation effect and measurement level. At the same time, the present disclosure is simple to operate, significantly reduces costs, and has high safety, and can be widely promoted and used. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a flow chart of a method for measuring and controlling oxidation operation of a nuclear power plant overhaul shown in an embodiment of the present disclosure.

[0021] Figure 2 A schematic diagram of a refueling tank purification system in one example.

[0022] Figure 3 A schematic diagram of an overhaul oxidation operation purification system in an example.

[0023] In the figure:

[0024] 1. Refueling water tank; 2. Cooling circulation pump; 3. Second filter; 4. First desalter;

[0025] 5. First filter; 6. Heat exchanger; 7. Reactor pressure vessel; 8. Reactor coolant pump;

[0026] 9. The third filter; 10. The isolation valve before the second desalter; 11. The isolation valve before the third desalter;

[0027] 12. Isolation valve before the fourth desalter; 13. Second desalter; 14. Third desalter;

[0028] 15. The fourth desalter; 16. The isolation valve before the fifth desalter; 17. The fifth desalter;

[0029] 18. The fourth filter. DETAILED DESCRIPTION

[0030] The present disclosure is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0031] Unless otherwise defined, the technical and scientific terms used in the present disclosure have the same meanings as those generally understood by those skilled in the art to which the present disclosure belongs; the terms used in the present disclosure are only for the purpose of describing specific embodiments and are not intended to limit the present disclosure; the term "including" and any variations thereof in the present disclosure are intended to cover non-exclusive inclusions. Obviously, the embodiments described in the present disclosure are only part of the embodiments of the present disclosure, not all of the embodiments. Based on the embodiments in the present disclosure, all other embodiments obtained by ordinary technicians in the field without making creative efforts are within the scope of protection of the present disclosure.

[0032] Reference to "embodiments" in this disclosure means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the disclosure. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.

[0033] Figure 1 is a flow chart of a method for measuring and controlling oxidation operation of a nuclear power plant overhaul shown in an embodiment of the present disclosure, Figure 2 This is a schematic diagram of the refueling water tank purification system in an example. Figure 3 A schematic diagram of an overhaul oxidation operation purification system is shown in the example. Figure 1 and Figure 2 The refueling water tank 1 purification system includes a refueling water tank 1 (equipment number PTR001BA), a cooling circulation pump 2, a second filter 3 (equipment number PTR002FI, which is a resin retention filter downstream of the reactor refueling water pool and the spent fuel water pool cooling and treatment system 001DE), a first desalinator 4 (equipment number PTR001DE, which is a desalinator of the reactor refueling water pool and the spent fuel water pool cooling and treatment system 001DE), a first filter 5 (equipment number PTR001FI, which is an upstream filter of the reactor refueling water pool and the spent fuel water pool cooling and treatment system 001DE) and a heat exchanger 6; Figure 2 As shown, the cooling circulation pump 2, the first filter 5, the first desalter 4 and the second filter 3 are connected in series to form a refueling water tank 1 purification circuit, which is used to purify the medium output from the refueling water tank 1. The medium purified by the refueling water tank 1 purification circuit flows back to the refueling water tank 1 through the heat exchanger 6.

[0034] See also Figure 1 and Figure 3 The overhaul oxidation operation purification system includes: reactor pressure vessel 7, reactor coolant pump 8, third filter 9 (equipment number RCV001FI, which is the downstream filter of chemical and volume control system), fourth filter 18 (equipment number RCV002FI, which is the resin retention filter of chemical and volume control system), second desalter 13 (equipment number TEP006DE, which is the mixed bed desalter of boron recovery system), third desalter 14 (equipment number RCV001DE, which is the mixed bed desalter No. 1 of chemical and volume control system), fourth desalter 15 (equipment number RCV002DE, which is the mixed bed desalter No. 2 of chemical and volume control system), and fifth desalter 17 (equipment number RCV003DE, which is the cation bed desalter of chemical and volume control system).

[0035] See also Figures 1 to 3 The measurement and control method of the nuclear power plant overhaul oxidation operation disclosed in the present invention includes:

[0036] Step 101, pre-overhaul control. Before the overhaul, the first desalter 4 is put into operation to purify the first refueling water tank 1. Under the action of the cooling circulation pump 2, the refueling water tank 1 purification circuit is cooled to a preset flow rate (e.g. 60m 3 / h), respectively through the first filter 5, the first desalter 4, and the second filter 3. In an application example, after a preset purification time (the preset time can be, for example, 168 hours), the total gamma content measured after purification is 0.6MBq / m 3 , turbidity <0.11NTU is far below the target value (the target value is total γ content <15MBq / m 3 , turbidity <1.0 NTU), effectively reducing the activated corrosion products and particulate impurities in the water of the refueling water tank 1, thereby reducing the impurity content that may be introduced into the main system, reducing the deposition of corrosion products in the core, and reducing the source term. In a possible implementation, the resin volume of the first desalter 4 can be 1.5m 3 The maximum working pressure can be 0.05MPa.g, the maximum working temperature can be 60℃, and the maximum working flow rate can be 65m 3 / h, daily 60m 3 / h flow rate for purification, wherein the exchange capacity of anion exchange resin (strong base) and cation exchange resin (strong acid) is roughly equal. The first filter 5 and the second filter 3 use filters with a filtration capacity of 0.45 μm.

[0037] Step 102, the second desalter 13 is put into operation during the downtime phase of the overhaul. Figure 1 and Figure 3, the second desalter 13 is put into operation 3 hours after the reactor reaches subcriticality (nuclear power is 0), and the second line is used as the downflow loop during the overhaul downtime. The second line is a loop composed of the reactor pressure vessel 7, the reactor coolant pump 8, the third filter 9, the second desalter 13 (the second desalter front isolation valve 10 can be set at the water inlet of the second desalter 13), and the fourth filter 18 connected in series in sequence, to replace the technical route of the first line used as the downflow loop in the related art, see Figure 3 , the first line can be a loop composed of the reactor pressure vessel 7, the reactor coolant pump 8, the third filter 9, the third desalter 14 (the third desalter front isolation valve 11 can be set at the water inlet of the third desalter 14), and the fourth filter 18 in series in order, or the first line can also be a downstream loop composed of the reactor pressure vessel 7, the reactor coolant pump 8, the third filter 9, the fourth desalter 15 (the fourth desalter front isolation valve 12 can be set at the water inlet of the fourth desalter 15), and the fourth filter 18 in series in order. Figure 3 As shown, the water inlet and the water outlet of the fifth desalter 17 are respectively connected to the main line to form a loop, and a fifth desalter front isolation valve 16 can be provided at the water inlet of the fifth desalter 17 .

[0038] After the purification efficiency calculation, the purification efficiency of the second desalter 13 during the whole process is always greater than 95%, which greatly meets the standard requirement of greater than 80%. And because the second desalter 13 is a hydrogen-oxygen type yin-yang mixed resin, and the third desalter 14 or the fourth desalter 15 is a lithium-oxygen type resin (currently replaced once every two fuel cycles, about 1 million yuan each time), the replacement cost of the second desalter 13 is only 1 / 10 of the latter, so it can greatly save economic costs; at the same time, the second desalter 13 can act as a lithium removal bed, and there is no need to invest in an additional lithium removal bed. The fifth desalter 17 removes lithium. After commissioning, the measured lithium concentration is less than 0.02 mg / kg, and the lithium removal effect is also better than the fifth desalter 17, which can better meet the requirement of as low a lithium concentration as possible before oxidation operation (target value: lithium concentration is less than 0.3 mg / kg).

[0039] See also Figure 3, the third filter 9 uses a 0.1μm filter element during normal power. Before the overhaul unit is decoupled, the 0.1μm filter element of the third filter 9 is replaced with a 0.45μm filter element, and the replacement pressure difference is adjusted to 0.25Mpa. During the upward stage of the unit, after the loading is completed and the refueling pool is drained, the filter element of the third filter 9 is replaced with a 0.1μm filter element. This can not only ensure that as many impurities as possible are filtered out, but also avoid frequent filter blockage and replacement caused by excessive impurity products during the overhaul oxidation operation, which delays the overhaul period. Using this method, during the entire oxidation operation stage of a certain overhaul, the third filter 9 did not become blocked and replaced. During the entire oxidation operation stage of another overhaul, the filter element of the third filter 9 was replaced three times because the above-mentioned filter element replacement was not performed on the third filter 9. In comparison, the above-mentioned filter element replacement effectively improves the purification effect of corrosion products in particle form.

[0040] Step 103, preparation and implementation of oxidation operation during the down-going phase of overhaul.

[0041] At the beginning of the overhaul oxidation operation, a preset volume and preset concentration (e.g. 18L, 30% concentration) of hydrogen peroxide solution is injected into the chemical mixing and dosing tank at one time. When the hydrogen peroxide solution reaches a preset temperature (e.g. 80°C), the hydrogen peroxide solution is injected into the primary circuit, and the chemical and volume control system downstream flow is adjusted to the maximum (e.g. 27m 3 / h), the purification platform is maintained for 8h. After the hydrogen peroxide solution is injected into the main system, samples are taken at 10, 20, 30, 45, 60 minutes, 2h, 3h, 4h, and 6h to observe the change trends of Co-58, Co-60, Sb-122, Sb-124, Ag-110m, I-131, Xe-133 and total γ. Using the above-mentioned dosing method, when the oxidation operation reaches the peak ( 58 Co peak), the measured hydrogen peroxide concentration was 5ppm and the dissolved oxygen was >5ppm, which fully met the oxygen concentration >1ppm requirement, proving that the main circuit was fully oxidized.

[0042] Step 104, measurement of oxidation operation during the down-stream phase of the overhaul. The measurement phase may use a mixed standard solution source of 20 g / bottle as shown in Table 1.

[0043] Table 1

[0044]

[0045] Before the measurement, a high-purity germanium multi-channel gamma spectrometer (model may be, for example, GEM30P4-76) and a mixed standard solution source of the above specifications are used to measure the radioactive nuclides. And establish the following oxidation operation-specific nuclide library Kr-85M, Kr-87, Kr-88, Xe-133M, Xe-133, Xe-135, Xe-138, Ar-41, Na-24, I-131, I-132, I-133, I-134, I-135, Cs-134, Cs-137, Cs-138, Co-58, Co-60, Cr-51, Mn-54, Ag-110M, Sb-122, Sb-124, Sb-125, Te-131M, Zr-95, Nb-95, Mo-99, Be-7, Fe-59, Ba-140, Ru-103, La-140, Np-239.

[0046] Place the sample to be tested in the sample slot of the acrylic sample holder on the probe or directly in the center of the probe;

[0047] Measure and obtain the γ-nuclides spectrum of 20 ml of standard mixed radioactive source, so that the counts of each main peak area reach the preset threshold (recommended to be above 10,000 counts), ensure sufficient statistical accuracy, and complete the energy calibration;

[0048] The energy peak on the γ nuclide spectrum is input into the activity, calibration date, uncertainty and other information of the corresponding nuclide on the standard source certificate, and the efficiency curve is fitted to complete the efficiency calibration.

[0049] Sample measurement: In the actual measurement process, if the radionuclide of the sample is low, it takes a long time to measure, but if the radionuclide of the sample is too large, it is easy to produce measurement dead time, resulting in large measurement errors. The present disclosure adopts the method of taking 1g of the main system sample during the oxidation operation and diluting it to 20g with high-purity water for measurement. The measurement live time is 100 seconds, and a good peak result is obtained, and the result is stable and reliable.

[0050] Step 105, control the operation of the main pump for oxidation operation during the overhaul down phase.

[0051] The purification time of the main pump in overhaul oxidation operation is controlled to 18 hours, during which the purification bed efficiency is monitored regularly to make the purification as complete as possible.

[0052] In an application example, referring to Table 2, the measurement and control method for overhaul oxidation operation of a nuclear power plant provided by the present disclosure is used in the overhaul of a certain unit No. 107, so that when the main pump is stopped in the down stage of the overhaul of No. 107, the total γ of the main system is measured to be 7976MBq / t, 58 Co is 4381MBq / t, which is the lowest in all the overhauls of a certain unit, proving that the method disclosed in the present invention can effectively improve the oxidation operation effect.

[0053] Table 2

[0054]

[0055] The embodiments of the present disclosure have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The selection of terms used herein is intended to best explain the principles of the embodiments, practical applications, or improvements to the technology in the market, or to enable other persons of ordinary skill in the art to understand the embodiments disclosed herein.

Claims

1. A method for measuring and controlling oxidation operation during overhaul of a nuclear power plant, characterized in that: The method comprises: Step 101, pre-overhaul control: before the overhaul, the first desalter is put into operation to purify the first refueling water tank. Under the action of the cooling circulation pump, the refueling water tank purification circuit flows through the first filter, the first desalter, and the second filter at a preset flow rate for a preset time; Step 102, control of the operation of the second desalter during the down-going phase of overhaul: the second desalter is put into operation after the reactor reaches a preset subcritical time. During the down-going phase of overhaul, the second line is used as a downflow loop, and the second line is a downflow loop composed of a reactor pressure vessel, a reactor coolant pump, a third filter, a second desalter, and a fourth filter connected in series in this order; Step 103, preparation and implementation of oxidation operation in the down stage of overhaul: at the beginning of the overhaul oxidation operation, a preset volume and a preset concentration of hydrogen peroxide solution are all injected into the chemical mixing and dosing box at one time, and when the hydrogen peroxide solution reaches a preset temperature, the hydrogen peroxide solution is injected into the primary circuit, and then samples are taken at 10, 20, 30, 45, 60 minutes, 2 hours, 3 hours, 4 hours, and 6 hours respectively to observe the change trends of Co-58, Co-60, Sb-122, Sb-124, Ag-110m, I-131, Xe-133 and total γ; Step 104, measurement of oxidation operation during the down-going phase of overhaul: measure and obtain the γ-nuclides spectrum of the preset volume standard mixed radioactive source, so that the area counts of each main peak reach the preset threshold, input the energy peak on the γ-nuclides spectrum into the activity, calibration date, and uncertainty information of the corresponding nuclides on the standard source certificate, fit the efficiency curve, and complete the efficiency calibration; Step 105, operation control of the oxidation operation main pump during the overhaul down stage: the operation purification time of the overhaul oxidation operation main pump is controlled to be 18 hours.

2. The method according to claim 1, characterized in that The resin volume of the first desalter 4 is 1.5m 3 The maximum working pressure is 0.05MPa.g, the maximum working temperature is 60℃, and the maximum working flow rate is 65m 3 / h, at 60m 3 / h flow rate for purification.

3. The method according to claim 1, characterized in that Before the overhaul unit is decommissioned, the 0.1μm filter element of the third filter is replaced with a 0.45μm filter element, and the replacement pressure difference is adjusted to 0.25Mpa.

4. The method according to claim 1, characterized in that In the actual measurement process, 1g of the main system sample was taken during the oxidation operation and diluted to 20g with high-purity water for measurement, and the measurement time was 100 seconds.

5. The method according to claim 1, characterized in that Before the measurement, a high-purity germanium multi-channel gamma spectrometer and a mixed standard solution source with the above-mentioned preset volume are used to measure the radioactive nuclides, and a nuclide library dedicated to oxidation operation is established.

Citation Information

Patent Citations

  • Loop sulfate pollution controlling method for starting process after nuclear plant major overhaul

    CN101477844A

  • System and method for continuously purifying primary coolant loop of pressurized water reactor nuclear power unit

    CN109166636A

  • Shutdown oxidation operation process for reducing collective dose of nuclear power station

    CN114300169A

  • Method for removing radionuclide 110mAg in loop system of nuclear power station

    CN115472323A

  • Method for preparing nuclear power plant pool activated corrosion product and pipeline mounting device

    CN117368080A

Cited By

  • Method for removing hydrogen after hydrogen rebound of primary loop in descending period of nuclear power plant during overhaul

    CN120183760A

  • Recovery system and method for boric acid solution of nuclear power plant

    CN120319518A