Method for preparing o, o-EDDHA-Fe through one-pot method
O,o-EDDHA-Fe is prepared by one-pot method, using phase transfer catalysts and organic extractants, combined with iron salt solution and iminodisuccinic acid, the problems of cumbersome process and unstable product quality in the prior art are solved, and the problem of cumbersome process and unstable product quality is achieved. Efficient and safe o,o-EDDHA-Fe preparation improves production efficiency and product performance.
Patent Information
- Application Number
- CN202411027933.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
AI Technical Summary
In the prior art, the preparation process of o,o-EDDHA-Fe is cumbersome, time-consuming and labor-intensive, the product has low adjacent value and unstable quality, making it difficult to meet actual production needs.
The method of preparing o,o-EDDHA-Fe is adopted by a one-pot method, including glyoxylic acid, phenol, ethylenediamine and liquid alkali reaction to prepare phase transfer catalysts, extracted by heat treatment and organic extraction agent, and added iron salt solution for chelation. Then complexed with iminodisuccinic acid, and finally dried and ground to produce an efficient o,o-EDDHA-Fe powder.
It has achieved short preparation time, high product orthogonal value, high iron content, low insoluble matter, safe and controllable operation, meet standard requirements, and saves costs through by-product recycling, improving production efficiency and product quality.
Smart Images

Figure CN118955312A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical industry, and in particular to a method for preparing o,o-EDDHA-Fe by a one-pot process. Background Art
[0002] Iron is one of the essential trace elements for plant growth and development. Iron deficiency in plants can lead to low chlorophyll content and nutritional imbalance. This will cause white and yellow necrotic spots to appear on the leaves and stems of plants, thus affecting the development of plants. For crops, it will reduce their yields. Ordinary fertilizers on the market can improve this symptom of plants, but they will destroy the acid-base balance of the soil and reduce the quality of the soil. Therefore, researchers have developed a new fertilizer, o,o-EDDHA-Fe. o,o-EDDHA-Fe is the most effective soil fertilizer for improving chlorosis caused by iron deficiency in plants in calcareous soils. The solution can be quickly absorbed by plants, and can also fix the beneficial components in the soil, which is beneficial to regulating the pH of the soil. When used correctly, it can make plants grow vigorously, has a special effect on the root cause of this chlorosis of plants, and is widely used in agricultural production.
[0003] At present, there are many domestic production methods of o, o-EDDHA-Fe. Most types of processes are cumbersome, time-consuming and labor-intensive; individual processes are relatively simple, but the product has a low ortho value and unstable quality. Sichuan Tongfeng Technology Co., Ltd. One-step synthesis of EDDHA chelated iron production process: CN201010580658.6 mentions the preparation of o, o-EDDHA-Fe, and its process steps are to weigh each raw material component in molar ratio, phenol 1.0, ethylenediamine 0.4-0.6, sodium hydroxide 2-4, glyoxylic acid 0.8-1.2, iron ion 0.5, water 20, first synthesize EDDHA aqueous solution; then react with iron salt to synthesize o, o-EDDHA-Fe chelate solution. The o, o-EDDHA-Fe prepared by this method has a low ortho value, large insoluble matter, and is easy to precipitate.
[0004] Therefore, the o,o-EDDHA-Fe developed by the present invention not only has a high ortho value, high solubility, an iron content of 7%-8%, and a safe and controllable operation process, but also effectively reduces the energy consumption in the production process. In summary, it is more suitable for promotion and use in actual production. Summary of the invention
[0005] In view of the shortcomings of the prior art, the object of the present invention is to provide a method for preparing o,o-EDDHA-Fe by a one-pot process.
[0006] A one-pot method for preparing o,o-EDDHA-Fe comprises the following steps:
[0007] S1: Glyoxylic acid, phenol, ethylenediamine and liquid alkali react to prepare solution a and heat treat the phase transfer catalyst
[0008] Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed to prepare a phase transfer catalyst, glyoxylic acid is added dropwise to a mixed solution of phenol, ethylenediamine and liquid alkali at 40° C. to 55° C., and then a phase transfer catalyst is added to obtain a reaction solution to be treated, the reaction solution to be treated is separated, and the pH of the aqueous phase of the reaction solution to be treated is adjusted and heated to obtain a solution a;
[0009] S2: organic extractant extraction solution a
[0010] Add 20%-40% of the mass of solution a in distilled water to solution a, then add NaOH solution to adjust the pH of the system to 8-9.5, then add an organic extractant to extract, and take the aqueous phase after extraction as solution b, and take the organic phase after extraction;
[0011] S3: Add iron salt solution to prepare o,o-EDDHA-Fe chelate solution c
[0012] Adding the solution b obtained in step S2 to the iron salt solution, stirring and standing the mixture to obtain a chelated iron solution, and then complexing the chelated iron solution with iminodisuccinic acid to obtain an o,o-EDDHA-Fe chelated solution c;
[0013] S4: drying and grinding the o,o-EDDHA-Fe chelating solution c to obtain the o,o-EDDHA-Fe powder product.
[0014] Preferably, step S1, in which glyoxylic acid, phenol, ethylenediamine and liquid alkali react to prepare solution a and heat-treat a phase transfer catalyst, comprises the following steps:
[0015] S1.1: Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed in a volume ratio of 1:(5-10) to obtain a phase transfer catalyst;
[0016] S1.2: at 40°C-55°C, add glyoxylic acid dropwise to a mixed solution of phenol, ethylenediamine and liquid caustic soda, wherein the molar ratio of glyoxylic acid, phenol, ethylenediamine and liquid caustic soda is 2:(2-8):1:(1-1.5), the glyoxylic acid is added dropwise for 2 hours, and then a phase transfer catalyst of 12%-15% by mass of the mixed solution is added, and the mixture is stirred evenly to obtain a reaction solution to be treated;
[0017] S1.3: The reaction liquid to be treated is separated into an organic phase and an aqueous phase, and then the aqueous phase of the reaction liquid to be treated is added into a reactor, the pH is adjusted to 9-10 with a NaOH solution, and the reactor is heated to 65°C-70°C. The gas emitted during heating is introduced into a recovery container filled with recovered liquid, and then the reactor is kept warm for 3h-6h to obtain solution a in the reactor.
[0018] Preferably, step S3 adds an iron salt solution to prepare an o,o-EDDHA-Fe chelate solution c, comprising the following steps:
[0019] S3.1: adding the solution b obtained in step S2 to the iron salt solution to chelate the iron salt solution with the solution b, wherein the volume ratio of the iron salt solution to the solution b is (10-15):1, stirring well and standing for 1-2 hours to obtain a chelated iron solution;
[0020] S3.2: The iminodisuccinic acid and the chelated iron solution are then mixed evenly for complexation. The volume ratio of the iminodisuccinic acid to the chelated iron solution is (10-15):1, and the pH of the system is adjusted to 8-9.5 using a NaOH solution to obtain an o,o-EDDHA-Fe chelated solution c.
[0021] Preferably, the recovered liquid in step S1 is specifically a 60-85 wt % ethanol aqueous solution.
[0022] Preferably, the recovery container in step S1 is subjected to distillation, condensation and reflux to obtain by-products 1-butene and ethanol, and the ethanol is added to the recovery container for secondary utilization.
[0023] Preferably, the iron salt solution in step S3 is prepared by mixing ferric chloride, ferrous sulfate and ferric sulfate in a ratio of (2-3):1:1.
[0024] Preferably, the organic extractant in step S2 is one of esters, ethers, chlorinated hydrocarbons or benzene.
[0025] Preferably, the drying temperature in step S4 is 55° C.-60° C., and the drying time is 5 h-6 h.
[0026] Preferably, the grinding time in step S4 is 15-60 min, and the product is sieved through a 40-80 mesh screen.
[0027] Compared with the prior art, the present invention has at least the following beneficial effects:
[0028] 1. The one-pot o,o-EDDHA-Fe prepared by the method provided by the present invention is a purple-red to black-red powder. The technical solution of the present invention has a short preparation time, a high ortho value of the product, which can reach above 5.3, an iron content of 7%-8%, and an insoluble matter of ≤0.05%. The operation process is safe and controllable, and meets the standard requirements.
[0029] 2. The present invention prepares a phase transfer catalyst by mixing tetrabutylammonium bromide and tetrabutylammonium hydroxide, and increases the yield of o,o-EDDHA by the phase transfer catalyst. The phase transfer catalyst is thermally decomposed by heating, and the gas generated after the phase transfer catalyst is decomposed is absorbed by an ethanol aqueous solution to obtain a by-product 1-butene. While protecting the environment, economic benefits can be brought about by the produced by-products and the recovered ethanol, thereby saving costs.
[0030] 3. The iminodisuccinic acid added in the present invention can be well chelated with ferrous ions, so that the ferrous ions in the iron salt solution that are not chelated with o,o-EDDHA are combined with iminodisuccinic acid to form IDHA chelated iron. The IDHA chelated iron can be well absorbed by plants, thereby achieving the effect of acting together with o,o-EDDHA-Fe to provide iron elements for plants. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] The accompanying drawings, which are incorporated herein and constitute a part of the specification, illustrate embodiments of the present disclosure and, together with the description, further serve to explain the principles of the present disclosure and to enable those skilled in the relevant art to make and use the present disclosure.
[0032] Figure 1 The present invention is a flowchart of a one-pot method for preparing o,o-EDDHA-Fe adopted in an embodiment of the present invention.
[0033] Figure 2 This is the liquid phase diagram of Comparative Example 1. DETAILED DESCRIPTION
[0034] The following is a detailed description of a soothing amino acid cleansing cream and its preparation process provided by the present invention in conjunction with the accompanying drawings and specific embodiments. At the same time, it is explained here that in order to make the embodiments more detailed, the following embodiments are the best and preferred embodiments, and those skilled in the art may also adopt other alternative methods to implement some known technologies; and the accompanying drawings are only for a more specific description of the embodiments, and are not intended to specifically limit the present invention.
[0035] Embodiment 1:
[0036] A one-pot method for preparing o,o-EDDHA-Fe, such as Figure 1 As shown, the following steps are included:
[0037] S1: Glyoxylic acid, phenol, ethylenediamine and liquid alkali react to prepare solution a and heat treat the phase transfer catalyst
[0038] Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed in a volume ratio of 1:10 to obtain a phase transfer catalyst;
[0039] At 50° C., glyoxylic acid is added dropwise to a mixed solution of phenol, ethylenediamine and liquid caustic soda, wherein the molar ratio of glyoxylic acid, phenol, ethylenediamine and liquid caustic soda is 2:2:1:1, and the glyoxylic acid is added dropwise for 2 hours. A phase transfer catalyst of 12% by mass of the mixed solution is then added, and the mixture is stirred evenly to obtain a reaction solution to be treated;
[0040] The reaction liquid to be treated is separated into an organic phase and an aqueous phase, and then the aqueous phase of the reaction liquid to be treated is added into a reactor, the pH is adjusted to 9 with a NaOH solution, and the reactor is heated to 70°C. The escaping gas during heating is introduced into a recovery container filled with a 60wt% ethanol aqueous solution, and then the reactor is kept warm for 3 hours to obtain a solution a in the reactor.
[0041] S2: organic extractant extraction solution a
[0042] Add 20% of the mass of solution a in distilled water to solution a, then add NaOH solution to adjust the pH of the system to 8, then add dichloromethane to extract, and take the aqueous phase after extraction as solution b, and take the organic phase after extraction;
[0043] S3: Add iron salt solution to prepare o,o-EDDHA-Fe chelate solution c
[0044] Adding the solution b obtained in step S2 to the iron salt solution, chelating the iron salt solution with the solution b, wherein the volume ratio of the iron salt solution to the solution b is 10:1, fully stirring and standing for 1 hour to obtain a chelated iron solution, wherein the iron salt solution is prepared by mixing ferric chloride, ferrous sulfate and ferric sulfate in a ratio of 2:1:1;
[0045] Then, the iminodisuccinic acid and the chelated iron solution were evenly mixed for complexation, the volume ratio of the iminodisuccinic acid to the chelated iron solution was 15:1, and the pH of the system was adjusted to 8.5 by using a NaOH solution to obtain an o,o-EDDHA-Fe chelated solution c.
[0046] S4: drying the o,o-EDDHA-Fe chelate solution c at 55°C for 6 hours and grinding for 30 minutes, and passing through an 80-mesh sieve to obtain an o,o-EDDHA-Fe powder product having an ortho value of 5.32.
[0047] Embodiment 2:
[0048] S1: Glyoxylic acid, phenol, ethylenediamine and liquid alkali react to prepare solution a and heat treat the phase transfer catalyst
[0049] Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed in a volume ratio of 1:10 to obtain a phase transfer catalyst;
[0050] At 50° C., glyoxylic acid is added dropwise to a mixed solution of phenol, ethylenediamine and liquid caustic soda, wherein the molar ratio of glyoxylic acid, phenol, ethylenediamine and liquid caustic soda is 2:2:1:1.1, and the glyoxylic acid is added dropwise for 1.5 h. A phase transfer catalyst of 12% by mass of the mixed solution is added, and the mixture is stirred evenly to obtain a reaction solution to be treated;
[0051] The reaction liquid to be treated is separated into an organic phase and an aqueous phase, and then the aqueous phase of the reaction liquid to be treated is added into a reactor, the pH is adjusted to 9 with a NaOH solution, and the reactor is heated to 68°C. The escaping gas during heating is introduced into a recovery container filled with a 60wt% ethanol aqueous solution, and then the reactor is kept warm for 3 hours to obtain a solution a in the reactor.
[0052] S2: organic extractant extraction solution a
[0053] Add 25% of the mass of solution a in distilled water to solution a, then add NaOH solution to adjust the pH of the system to 8, then add dichloromethane to extract, and take the aqueous phase after extraction as solution b, and take the organic phase after extraction;
[0054] S3: Add iron salt solution to prepare o,o-EDDHA-Fe chelate solution c
[0055] Adding the solution b obtained in step S2 to the iron salt solution, chelating the iron salt solution with the solution b, wherein the volume ratio of the iron salt solution to the solution b is 12:1, fully stirring and standing for 1 hour to obtain a chelated iron solution, wherein the iron salt solution is prepared by mixing ferric chloride, ferrous sulfate and ferric sulfate in a ratio of 2:1:1;
[0056] Then, the iminodisuccinic acid and the chelated iron solution were evenly mixed for complexation, the volume ratio of the iminodisuccinic acid to the chelated iron solution was 12:1, and the pH of the system was adjusted to 8.5 by using a NaOH solution to obtain an o,o-EDDHA-Fe chelated solution c.
[0057] S4: drying the o,o-EDDHA-Fe chelate solution c at 58°C for 5.5 hours and grinding for 30 minutes, and passing through an 80-mesh sieve to obtain the o,o-EDDHA-Fe powder product, the ortho value of which is 5.45
[0058] Embodiment 3:
[0059] A one-pot method for preparing o,o-EDDHA-Fe, such as Figure 1 As shown, the following steps are included:
[0060] S1: Glyoxylic acid, phenol, ethylenediamine and liquid alkali react to prepare solution a and heat treat the phase transfer catalyst
[0061] Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed in a volume ratio of 1:10 to obtain a phase transfer catalyst;
[0062] At 45° C., glyoxylic acid is added dropwise to a mixed solution of phenol, ethylenediamine and liquid caustic soda, wherein the molar ratio of glyoxylic acid, phenol, ethylenediamine and liquid caustic soda is 2:6:1:1, and the glyoxylic acid is added dropwise for 2 hours. A phase transfer catalyst of 12% by mass of the mixed solution is then added, and the mixture is stirred evenly to obtain a reaction solution to be treated;
[0063] The reaction liquid to be treated is separated into an organic phase and an aqueous phase, and then the aqueous phase of the reaction liquid to be treated is added into a reactor, the pH is adjusted to 9 with a NaOH solution, and the reactor is heated to 68°C. The escaping gas during heating is introduced into a recovery container filled with a 60wt% ethanol aqueous solution, and then the reactor is kept warm for 3 hours to obtain a solution a in the reactor.
[0064] S2: organic extractant extraction solution a
[0065] Add 35% of the mass of solution a in distilled water to solution a, then add NaOH solution to adjust the pH of the system to 8.2, then add dichloromethane to extract, and take the aqueous phase after extraction as solution b, and take the organic phase after extraction;
[0066] S3: Add iron salt solution to prepare o,o-EDDHA-Fe chelate solution c
[0067] Adding the solution b obtained in step S2 to the iron salt solution, chelating the iron salt solution with the solution b, wherein the volume ratio of the iron salt solution to the solution b is 10:1, stirring thoroughly and standing for 1-2 hours to obtain a chelated iron solution, wherein the iron salt solution is prepared by mixing ferric chloride, ferrous sulfate and ferric sulfate in a ratio of 2:1:1;
[0068] Then, the iminodisuccinic acid and the chelated iron solution were evenly mixed for complexation, the volume ratio of the iminodisuccinic acid to the chelated iron solution was 15:1, and the pH of the system was adjusted to 9.2 by using a NaOH solution to obtain an o,o-EDDHA-Fe chelated solution c.
[0069] S4: drying the o,o-EDDHA-Fe chelate solution c at 56°C for 5 hours and grinding for 30 minutes, and passing through an 80-mesh sieve to obtain an o,o-EDDHA-Fe powder product having an ortho value of 6.33.
[0070] Comparative Example 1:
[0071] Compared with Example 1, Comparative Example 1 is a commercially available o,o-EDDHA-Fe powder, the product description of which states that the ortho value is 4.8, and its liquid phase diagram is as follows Figure 2 shown.
[0072] The parameters of each embodiment are compared with the parameters of comparative example 1, as shown in Table 1.
[0073] Table 1
[0074] Serial number Iron content / % Insoluble matter / % Ortho value Comparative Example 1 6.8 0.03 4.8 Example 1 7.36 0.0037 5.32 Example 2 7.57 0.0028 5.45 Example 3 7.83 0.0013 6.33
[0075] It can be seen from the table that the ortho value and iron content of the embodiment are higher than those of the comparative example, and the higher iron content and the low insoluble content can make the embodiment easier to absorb than the comparative example, and each parameter is superior to the commercially available o,o-EDDHA-Fe powder.
[0076] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A one-pot method for preparing o,o-EDDHA-Fe, It is characterized in that The steps include: S1: glyoxylic acid, phenol, ethylenediamine and liquid alkali are reacted to prepare solution a and a phase transfer catalyst is heat-treated. Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed to prepare a phase transfer catalyst, glyoxylic acid is added dropwise to a mixed solution of phenol, ethylenediamine and liquid alkali at 40° C.-55° C., and a phase transfer catalyst is added to obtain a reaction solution to be treated, the reaction solution to be treated is separated, and the pH of the aqueous phase of the reaction solution to be treated is adjusted and heated to obtain solution a; S2: organic extractant extraction solution a Add 20%-40% of the mass of solution a in distilled water to solution a, then add NaOH solution to adjust the pH of the system to 8-9.5, then add an organic extractant to extract, and take the aqueous phase after extraction as solution b, and take the organic phase after extraction; S3: Add iron salt solution to prepare o,o-EDDHA-Fe chelate solution c Adding the solution b obtained in step S2 to the iron salt solution, stirring and standing the mixture to obtain a chelated iron solution, and then complexing the chelated iron solution with iminodisuccinic acid to obtain an o,o-EDDHA-Fe chelated solution c; S4: drying and grinding the o,o-EDDHA-Fe chelating solution c to obtain the o,o-EDDHA-Fe powder product.
2. The one-pot method for preparing o,o-EDDHA-Fe according to claim 1, It is characterized in that Step S1: glyoxylic acid, phenol, ethylenediamine and liquid alkali react to prepare solution a and heat-treat a phase transfer catalyst, comprising the following steps: S1.1: Tetrabutylammonium bromide and tetrabutylammonium hydroxide are mixed in a volume ratio of 1:(5-10) to obtain a phase transfer catalyst; S1.2: at 40°C-55°C, add glyoxylic acid dropwise to a mixed solution of phenol, ethylenediamine and liquid caustic soda, wherein the molar ratio of glyoxylic acid, phenol, ethylenediamine and liquid caustic soda is 2:(2-8):1:(1-1.5), the glyoxylic acid is added dropwise for 2 hours, and then a phase transfer catalyst of 12%-15% by mass of the mixed solution is added, and the mixture is stirred evenly to obtain a reaction solution to be treated; S1.3: The reaction liquid to be treated is separated into an organic phase and an aqueous phase, and then the aqueous phase of the reaction liquid to be treated is added into a reactor, the pH is adjusted to 9-10 with a NaOH solution, and the reactor is heated to 65°C-70°C. The gas emitted during heating is introduced into a recovery container filled with recovered liquid, and then the reactor is kept warm for 3h-6h to obtain solution a in the reactor.
3. The method for preparing o,o-EDDHA-Fe by one-pot method according to claim 2, It is characterized in that Step S3: adding an iron salt solution to prepare an o,o-EDDHA-Fe chelating solution c, comprising the following steps: S3.1: adding the solution b obtained in step S2 to the iron salt solution to chelate the iron salt solution with the solution b, wherein the volume ratio of the iron salt solution to the solution b is (10-15):1, stirring well and standing for 1-2 hours to obtain a chelated iron solution; S3.2: The iminodisuccinic acid and the chelated iron solution are then mixed evenly for complexation. The volume ratio of the iminodisuccinic acid to the chelated iron solution is (10-15):1, and the pH of the system is adjusted to 8-9.5 using a NaOH solution to obtain an o,o-EDDHA-Fe chelated solution c.
4. The method for preparing o,o-EDDHA-Fe by one-pot method according to claim 3, It is characterized in that The recovered liquid in step S1 is specifically a 60-85wt% ethanol aqueous solution.
5. The method for preparing o,o-EDDHA-Fe by one-pot method according to claim 4, It is characterized in that The recovery container in step S1 is subjected to distillation, condensation and reflux to obtain by-products 1-butene and ethanol, and the ethanol is added to the recovery container for secondary utilization.
6. The method for preparing o,o-EDDHA-Fe by one-pot method according to claim 5, It is characterized in that The iron salt solution in step S3 is specifically prepared by mixing ferric chloride, ferrous sulfate and ferric sulfate in a ratio of (2-3):1:
1.
7. The one-pot method for preparing o,o-EDDHA-Fe according to claim 6, It is characterized in that In step S2, the organic extractant is one of esters, ethers, chlorinated hydrocarbons or benzene.
8. The one-pot method for preparing o,o-EDDHA-Fe according to claim 7, It is characterized in that The drying temperature in step S4 is 55° C.-60° C., and the drying time is 5 h-6 h.
9. The one-pot method for preparing o,o-EDDHA-Fe according to claim 8, It is characterized in that The grinding time in step S4 is 15-60 min, and the product is passed through a 40-80 mesh sieve.
10. The one-pot method for preparing o,o-EDDHA-Fe according to claim 9, It is characterized in that The concentration of the NaOH solution in step S1, step S2 and step S3 is 10-20 wt%.