Treatment method of galaxolide waste aluminum water
Through the maturation polymerization reaction of the modifier with hydrochloric acid solution and calcium aluminate powder, the problems of low treatment efficiency of Jiale Musk waste aluminum water and chlorobenzene contamination are solved, achieving efficient extraction of polyaluminum water and reducing costs.
Patent Information
- Application Number
- CN202411162264.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-22
AI Technical Summary
In Jiale Musk waste aluminum water treatment, the existing technology is inefficient and uses chlorobenzene as the extraction agent, resulting in increased environmental pollution and cost, making it difficult to effectively extract aluminum salts.
A modified agent (composed of aluminum phosphate precursor and silica gel particles) is used to carry out a maturation polymerization reaction with hydrochloric acid solution and calcium aluminate powder. Through the acidolysis and maturation polymerization steps, polymerized aluminum chloride is generated, avoiding the use of chlorobenzene.
The extraction efficiency of aluminum in waste aluminum water is improved, environmental pollution and tail water treatment costs are reduced, the polyaluminum water generated meets the standards, and the modifier can be recycled.
Smart Images

Figure CN118993286A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical tail water treatment, and in particular to a method for treating galaxolide waste aluminum water. Background Art
[0002] Galaxolide, also known as hexamethylindanonepyran, is a synthetic musk raw material widely used in cosmetics, perfumes and detergents. Galaxolide is known for its unique smell of clean, sweet, floral and woody musk. Galaxolide has various preparation processes, mainly including using α-methylstyrene and tert-amyl alcohol as raw materials, generating pentamethylindane under the catalysis of sulfuric acid, and then finally obtaining it through multi-step reactions; or using benzene and propylene oxide as raw materials, generating intermediate products under the catalysis of aluminum chloride, and further reacting to synthesize galaxolide. In addition, there is a new process using isopentene and methylstyrene as raw materials. The reaction conditions of this process are mild, the operation is simple, and the yield of the finished product is high, which effectively solves the problem of low yield of traditional processes. Galaxolide not only performs well in aroma, but also occupies an important position in the market due to its stability, non-toxicity, good penetration and diffusibility. However, due to the extremely poor fluidity of galaxolide and its easy local solidification after long storage, it is often diluted to an appropriate concentration with a diluent in practical applications. In terms of safety assessment, multiple studies have shown that under normal conditions of use, galaxol does not pose significant risks to human health and the environment.
[0003] However, the output of waste aluminum water in the production of galaxol is relatively large (1 ton of galaxol produces about 5 tons of waste aluminum water). At present, the treatment of waste aluminum water in production is mostly evaporation concentration and crystallization salt, but because waste aluminum water has flocculation, evaporation concentration efficiency is poor, and most of the pastes obtained are organic matter, and it is difficult to obtain aluminum salts (such as polyaluminum chloride). In addition, as the invention patent of patent publication number CN111732118A, a treatment method of galaxol waste aluminum salt water is disclosed, and the waste aluminum salt water is made into qualified polyaluminum water by evaporation, extraction, and evaporation. However, the applicant found in actual production that a large amount of extraction agent chlorobenzene needs to be added in the extraction process. Chlorobenzene has moderate toxicity, has irritation to skin mucosa and upper respiratory tract, is not suitable for large-scale continuous production, and may cause secondary pollution to the environment, and chlorobenzene also increases the cost of tail water treatment to a certain extent. Summary of the invention
[0004] In order to solve the problems mentioned in the above background technology, the present invention provides a method for treating galaxol waste aluminum water.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] A method for treating galaxol waste aluminum water, characterized in that it comprises the following steps:
[0007] S1. Put the lower layer of waste aluminum water obtained after hydrolysis (methanol 4-6%, Al2O3 7-9%, national standard polyaluminum water based on aluminum oxide, hydrochloric acid 0.05-1.5%, chlorobenzene 0.05-1.5%) into the reactor, add hydrochloric acid solution and modifier, and stir evenly;
[0008] S2, turn on the heating steam, and let the steam directly enter the kettle for acid hydrolysis;
[0009] S3, stop steam heating, add calcium aluminate powder for aging polymerization, the reaction self-exothermic reaction makes the temperature of the reactor rise to 100-105°C, keep warm to complete the aging polymerization reaction;
[0010] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0011] Furthermore, in step S1, the mass ratio of waste aluminum water, hydrochloric acid solution and modifier is 25:(13-15):(2-3), and the hydrochloric acid content is 20-24%.
[0012] Furthermore, in step S1, the stirring speed is 200-300 rpm, and the stirring time is 1.5-2 h.
[0013] Furthermore, in step S2, the temperature in the reactor is 70-75°C.
[0014] Furthermore, in step S3, the content of aluminum oxide in the calcium aluminate powder is ≥48.5%, the added amount is 5-20% of the total material mass, and the insulation time is 1-1.5h.
[0015] Furthermore, the modifying agent in step S1 is prepared by the following steps:
[0016] A1. Add a surfactant to phosphoric acid and aluminum hydroxide in deionized water, heat and keep warm for 1-2 hours under stirring, and cool to room temperature to obtain an aluminum phosphate precursor solution;
[0017] A2. Add silica gel particles and magnesium sulfate to the aluminum phosphate precursor solution, stir and immerse for 2-3 hours at room temperature, filter, wash, place in a muffle furnace, heat and roast under nitrogen protection, and after roasting, cool to room temperature to obtain a modifier.
[0018] Furthermore, in step A1, the mass ratio of phosphoric acid, aluminum hydroxide, deionized water and surfactant is (1-1.2): (1.2-1.5): (20-30): (0.005-0.008), the surfactant is sodium dodecyl sulfate or hexadecyltrimethylammonium bromide, the stirring speed is 400-500 rpm, and the temperature is 60-70°C.
[0019] Furthermore, in step A2, the mass ratio of silica gel particles, magnesium sulfate and aluminum phosphate precursor solution is (5-6):(1-3):(10-15), and the stirring speed is 300-600 rpm.
[0020] Furthermore, in step A2, the heating rate in the muffle furnace is 2-5°C / min, firstly the temperature is raised to 300-350°C and kept for 1-2h, then the temperature is further raised to 500-550°C and kept for 2-3h to complete the roasting.
[0021] Compared with the prior art, the present invention has the following beneficial effects:
[0022] 1. Phosphoric acid and aluminum hydroxide react in deionized water, add surfactant and stir and heat to generate aluminum phosphate precursor. Subsequently, silica gel particles and magnesium sulfate are added to the precursor solution and stirred and impregnated. The porous structure of silica gel particles enables it to adsorb aluminum phosphate and magnesium sulfate. Aluminum phosphate and magnesium sulfate are attached to the pore structure of silica gel particles and play a role of skeleton support. After high-temperature roasting, the pore structure of silica gel particles is prevented from collapsing or reconstructing due to high temperature, so that its surface properties are improved. In the process of waste aluminum water treatment, the porous structure and active groups on the surface of the modifier can adsorb aluminum ions and other impurity ions in the waste aluminum water, which is beneficial to subsequent separation and purification. In addition, anionic groups such as phosphate and sulfate in the modifier can form stable complexes with aluminum ions, which are easier to disperse in water and not easy to precipitate, which is beneficial to subsequent polymerization reactions.
[0023] 2. Waste aluminum water mainly contains methanol, aluminum oxide (in the form of Al 2 O 3 The dissolution and conversion of aluminum ions in the waste aluminum water are promoted by adding hydrochloric acid solution and modifier and stirring evenly. In this process, hydrochloric acid, as a strong acid, reacts with aluminum oxide in the waste aluminum water to form soluble aluminum salts. At the same time, the addition of modifiers further promotes the dissociation and dispersion of aluminum ions through surface adsorption, complexation or bridging, thereby improving the efficiency of subsequent reactions.
[0024] 3. Steam heating promotes the further dissociation of aluminum ions in the waste aluminum water and the reaction with hydrochloric acid, generating more soluble aluminum salts. Subsequently, calcium aluminate powder is added in step S3 for aging polymerization reaction, and the aluminum oxide in the calcium aluminate powder and the aluminum ions in the waste aluminum water undergo polymerization reaction at a suitable pH value and temperature to generate macromolecular aluminum salts such as polyaluminum chloride (PAC). The self-exothermic effect of the polymerization reaction increases the temperature of the reactor, further promoting the reaction.
[0025] 4. Chlorobenzene is often used as an extractant in the prior art, but chlorobenzene has moderate toxicity, may cause secondary pollution to the environment, and increase the cost of tail water treatment. The present invention avoids the use of chlorobenzene, thereby eliminating its potential harm to the environment and human body. In addition, the improver of the present invention can be recycled after washing and drying, further reducing the cost of tail water treatment. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0027] Figure 1 It is a flowchart of the present invention. DETAILED DESCRIPTION
[0028] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] Unless otherwise specified, the raw materials used in the present invention are all conventional products purchased from the market.
[0030] Preparation Example 1
[0031] The modifying agent in step S1 is prepared by the following steps:
[0032] A1. Add 0.05 kg of sodium dodecyl sulfate to 10 kg of phosphoric acid and 12 kg of aluminum hydroxide in 20 kg of deionized water, heat to 60 ° C and keep warm for 1 hour while stirring at 400 rpm, and cool to room temperature to obtain an aluminum phosphate precursor solution;
[0033] A2. Add 5kg of silica gel particles and 1kg of magnesium sulfate to 10kg of aluminum phosphate precursor solution, stir and immerse at 300rpm for 2h at room temperature, filter, wash, place in a muffle furnace, and under nitrogen protection, heat up at a rate of 2℃ / min, first heat to 300℃ and keep warm for 1h, then continue to heat to 500℃ and keep warm for 2h. After calcination, cool to room temperature to obtain a modifier.
[0034] Preparation Example 2
[0035] The modifying agent in step S1 is prepared by the following steps:
[0036] A1. Add 0.06 kg of sodium dodecyl sulfate to 11 kg of phosphoric acid and 13.5 kg of aluminum hydroxide in 25 kg of deionized water, heat to 65 ° C and keep warm for 1.5 hours under stirring at 450 rpm, and cool to room temperature to obtain an aluminum phosphate precursor solution;
[0037] A2. Add 5.5 kg of silica gel particles and 2 kg of magnesium sulfate to 12.5 kg of aluminum phosphate precursor solution, stir and immerse at 400 rpm for 2.5 hours at room temperature, filter, wash, and place in a muffle furnace. Under nitrogen protection, heat up at a rate of 3°C / min, first heat to 330°C and keep warm for 1 hour, then continue to heat to 530°C and keep warm for 2.5 hours. After calcination, cool to room temperature to obtain a modifier.
[0038] Preparation Example 3
[0039] The modifying agent in step S1 is prepared by the following steps:
[0040] A1. Add 0.08 kg of sodium dodecyl sulfate to 12 kg of phosphoric acid and 15 kg of aluminum hydroxide in 30 kg of deionized water, heat to 70 ° C and keep warm for 2 hours under stirring at 500 rpm, and cool to room temperature to obtain an aluminum phosphate precursor solution;
[0041] A2. Add 6 kg of silica gel particles and 3 kg of magnesium sulfate to 15 kg of aluminum phosphate precursor solution, stir and immerse at 600 rpm for 3 hours at room temperature, filter, wash, and place in a muffle furnace. Under nitrogen protection, heat up at a rate of 5 ° C / min, first heat to 350 ° C and keep warm for 2 hours, then continue to heat to 550 ° C and keep for 3 hours. After calcination, cool to room temperature to obtain a modifier.
[0042] Example 1
[0043] A method for treating galaxol waste aluminum water comprises the following steps:
[0044] S1, the 25kg lower layer of waste aluminum water obtained after hydrolysis (after testing, the waste water contains 4.6% methanol, 7.3% Al2O3, 0.08% hydrochloric acid, and 0.05% chlorobenzene) is poured into the reactor, 13kg 20% hydrochloric acid solution and 2kg modifier prepared in Preparation Example 1 are added, and stirred at a speed of 200rpm for 1.5h;
[0045] S2, turn on the heating steam, and directly introduce the steam into the kettle until the temperature in the reactor reaches 70°C for acid hydrolysis;
[0046] S3, stop steam heating, add 5kg calcium aluminate powder (alumina content 53.8%) for aging polymerization, and keep warm to complete the aging polymerization reaction;
[0047] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0048] Example 2
[0049] A method for treating galaxol waste aluminum water comprises the following steps:
[0050] S1, the 25kg lower layer waste aluminum water obtained after hydrolysis (after testing, the waste water contains 4.2% methanol, 7.8% Al2O3, 0.06% hydrochloric acid, and 0.06% chlorobenzene) is poured into the reactor, 14kg 22% hydrochloric acid solution and 2.5kg modifier prepared in Preparation Example 2 are added, and stirred at a speed of 250rpm for 1.5h;
[0051] S2, turn on the heating steam, and directly introduce the steam into the reactor until the temperature in the reactor reaches 73°C for acid hydrolysis;
[0052] S3, stop steam heating, add 5kg calcium aluminate powder (alumina content 53.8%) for aging polymerization, and keep warm to complete the aging polymerization reaction;
[0053] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0054] Example 3
[0055] A method for treating galaxol waste aluminum water comprises the following steps:
[0056] S1. Add 25 kg of the lower layer of waste aluminum water obtained after hydrolysis (after testing, the waste water contains 4.2% methanol, 7.8% Al2O3, 0.06% hydrochloric acid, and 0.06% chlorobenzene) into the reactor, add 13.5 kg of 22% hydrochloric acid solution and 2.5 kg of the modifier obtained in Preparation Example 3, and stir at a speed of 250 rpm for 1.5 h;
[0057] S2, turn on the heating steam, and directly introduce the steam into the reactor until the temperature in the reactor reaches 73°C for acid hydrolysis;
[0058] S3, stop steam heating, add 5kg calcium aluminate powder (alumina content 53.8%) for aging polymerization, and keep warm to complete the aging polymerization reaction;
[0059] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0060] Example 4
[0061] A method for treating galaxol waste aluminum water comprises the following steps:
[0062] S1, 25kg of the lower layer of waste aluminum water obtained after hydrolysis (after testing, the waste water contains 4.9% methanol, 7.0% Al2O3, 0.1% hydrochloric acid, and 0.06% chlorobenzene) is poured into a reactor, 14kg of 22% hydrochloric acid solution and 2.6kg of the modifier obtained in Preparation Example 1 are added, and stirred at a speed of 250rpm for 1.5h;
[0063] S2, turn on the heating steam, and directly introduce the steam into the reactor until the temperature in the reactor reaches 73°C for acid hydrolysis;
[0064] S3, stop steam heating, add 5kg calcium aluminate powder (alumina content 53.8%) for aging polymerization, and keep warm to complete the aging polymerization reaction;
[0065] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0066] Example 5
[0067] A method for treating galaxol waste aluminum water comprises the following steps:
[0068] S1, put 25kg of the lower layer of waste aluminum water obtained after hydrolysis (after testing, the waste water contains 5.5% methanol, 7.9% Al2O3, 0.06% hydrochloric acid, and 0.05% chlorobenzene) into the reactor, add 15kg of 24% hydrochloric acid solution and 3kg of the modifier obtained in Preparation Example 2, and stir at a speed of 300rpm for 2h;
[0069] S2, turn on the heating steam, and directly introduce the steam into the reactor until the temperature in the reactor reaches 75°C for acid hydrolysis;
[0070] S3, stop steam heating, add 5kg calcium aluminate powder (alumina content 53.8%) for aging polymerization, and keep warm to complete the aging polymerization reaction;
[0071] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0072] Example 6
[0073] A method for treating galaxol waste aluminum water comprises the following steps:
[0074] S1, 25kg of the lower layer of waste aluminum water obtained after hydrolysis (after testing, the waste water contains 4.4% methanol, 8.1% Al2O3, 0.11% hydrochloric acid, and 0.09% chlorobenzene) is poured into a reactor, 15kg of 24% hydrochloric acid solution and 3kg of the modifier obtained in Preparation Example 3 are added, and stirred at a speed of 300rpm for 2h;
[0075] S2, turn on the heating steam, and directly introduce the steam into the reactor until the temperature in the reactor reaches 75°C for acid hydrolysis;
[0076] S3, stop steam heating, add 5kg calcium aluminate powder (alumina content 60.5%) for aging polymerization, and keep warm to complete the aging polymerization reaction;
[0077] S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump. The clear liquid, i.e. the finished product of polyaluminum water, flows into the ground trough and is pumped to the storage area.
[0078] Comparative Example 1
[0079] The difference between this comparative example and Example 1 is that no modifier is added, and the remaining steps are the same as those of Example 1.
[0080] Comparative Example 2
[0081] The difference between this comparative example and Example 2 is that silica gel particles are used instead of the modifier, and the remaining steps are the same as those in Example 2.
[0082] Comparative Example 3
[0083] The difference between this comparative example and Example 3 is that magnesium sulfate is used instead of the modifier, and the remaining steps are the same as those in Example 3.
[0084] Comparative Example 4
[0085] The difference between this comparative example and Example 4 is that an aluminum phosphate precursor is used instead of the modifier, and the remaining steps are the same as those of Example 4.
[0086] Comparative Example 5
[0087] The difference between this comparative example and Example 5 is that no hydrochloric acid solution is added, and the remaining steps are the same as those in Example 5.
[0088] Comparative Example 6
[0089] The difference between this comparative example and Example 6 is that calcium aluminate powder is not added, and the remaining steps are the same as those of Example 6.
[0090] Record the volume of aluminum water in Examples 1-6 and Comparative Examples 1-6, and calculate the yield of Examples 1-6 and Comparative Examples 1-6. Yield = (actual mass / initial mass) × 100%, initial mass = waste aluminum water mass × initial aluminum content (converted Al 2 O 3 ), actual mass = volume of polyaluminium water × mass percentage of alumina in polyaluminium water × density of alumina (take 3.95 g / cm 3 ), the results are shown in Table 1:
[0091] Table 1. Yields of Examples 1-6 and Comparative Examples 1-6
[0092] serial number Yield (%) Example 1 50.68 Example 2 51.20 Example 3 50.18 Example 4 51.52 Example 5 50.42 Example 6 52.21 Comparative Example 1 24.71 Comparative Example 2 45.02 Comparative Example 3 43.84 Comparative Example 4 43.11 Comparative Example 5 1.64 Comparative Example 6 16.25
[0093] The polyaluminium water obtained in Examples 1-3 was selected as a sample, and some technical requirements for the sample were tested with reference to GB / T 22627-2022 "Polyaluminium Chloride, Water Treatment Agent", as shown in Table 2:
[0094] Table 2. Some technical requirements of samples of Examples 1-3
[0095]
[0096]
[0097] As can be seen from Table 1, the yields of Examples 1-6 are all above 50%, indicating that the addition amounts of modifier, hydrochloric acid solution and calcium aluminate powder and the reaction conditions are all relatively suitable, and aluminum can be effectively extracted from waste aluminum water and converted into polyaluminum water. The yield of Comparative Example 1 is relatively low (24.71%), indicating that not adding a modifier will greatly reduce the extraction efficiency of aluminum. The yields of Comparative Examples 2-4 are also lower than those of the embodiments, indicating that replacing the modifier with silica gel particles, magnesium sulfate or aluminum phosphate precursor alone cannot achieve the comprehensive effect of the modifier. The yield of Comparative Example 5 is extremely low (1.64%), indicating that the addition of hydrochloric acid solution is one of the important steps for the acidolysis of waste aluminum water and the extraction of aluminum. The yield of Comparative Example 6 is also relatively low (16.25%), indicating that the addition of calcium aluminate powder has an important influence on the aging polymerization reaction and the formation of polyaluminum water.
[0098] It can be seen from Table 2 that the polyaluminum water samples obtained in Examples 1-3 all meet some of the technical requirements of GB / T22627-2022 "Water Treatment Agent Polyaluminum Chloride", indicating that this treatment method can effectively extract aluminum from waste aluminum water.
[0099] Combining Tables 1 and 2, the modifier may improve the dispersibility and extractability of aluminum in the waste aluminum water through its unique surface properties and chemical composition. At the same time, the silica gel particles and magnesium sulfate in the modifier may form a complex complex, which helps to effectively extract aluminum. The addition of hydrochloric acid solution may reduce the pH value of the waste aluminum water, destroy the compound structure of aluminum, and make it easier to extract. The addition of calcium aluminate powder may play a role in aging polymerization, forming polyaluminum water by reacting with the extracted aluminum.
[0100] In summary, this treatment method can effectively extract polyaluminum water that meets the standards from the waste aluminum water of galaxolide.
[0101] In the description of the specification, the description with reference to the terms "preparation example", "embodiment", "various embodiments" and the like means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or preparation example are included in at least one embodiment or preparation example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or preparation example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or preparation examples in a suitable manner.
[0102] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for treating galaxol waste aluminum water, It is characterized in that The following steps are involved: S1. Pour waste aluminum water into a reactor, add hydrochloric acid solution and modifier, and start stirring; S2, turn on the heating steam to carry out acid hydrolysis; S3, stop steam heating, add calcium aluminate powder, and keep warm to complete the aging polymerization reaction; S4. After cooling to room temperature, filter with a plate and frame filter press using a bottom pump, and the clear liquid is the finished product of polyaluminum water.
2. A method for treating galaxolide waste aluminum water according to claim 1, It is characterized in that In step S1, the mass ratio of waste aluminum water, hydrochloric acid solution and modifier is 25:(13-15):(2-3), and the hydrochloric acid content is 20-24%.
3. A method for treating galaxolide waste aluminum water according to claim 1, It is characterized in that In step S1, the stirring speed is 200-300 rpm, and the stirring time is 1.5-2 h.
4. A method for treating galaxolide waste aluminum water according to claim 1, It is characterized in that The temperature in the reactor in step S2 is 70-75°C.
5. A method for treating galaxolide waste aluminum water according to claim 1, It is characterized in that In step S3, the content of aluminum oxide in the calcium aluminate powder is ≥48.5%, and the insulation time is 1-1.5 hours.
6. A method for treating galaxolide waste aluminum water according to claim 1, It is characterized in that The modifying agent in step S1 is prepared by the following steps: A1. Add a surfactant to phosphoric acid and aluminum hydroxide in deionized water, heat and keep warm for 1-2 hours under stirring, and cool to room temperature to obtain an aluminum phosphate precursor solution; A2. Add silica gel particles and magnesium sulfate to the aluminum phosphate precursor solution, stir and immerse for 2-3 hours at room temperature, filter, wash, place in a muffle furnace, heat and roast under nitrogen protection, and after roasting, cool to room temperature to obtain a modifier.
7. A method for treating galaxolide waste aluminum water according to claim 6, It is characterized in that In step A1, the mass ratio of phosphoric acid, aluminum hydroxide, deionized water and surfactant is (1-1.2): (1.2-1.5): (20-30): (0.005-0.008), the surfactant is sodium dodecyl sulfate or hexadecyltrimethylammonium bromide, the stirring speed is 400-500 rpm, and the temperature is 60-70°C.
8. A method for treating galaxolide waste aluminum water according to claim 6, It is characterized in that In step A2, the mass ratio of silica gel particles, magnesium sulfate and aluminum phosphate precursor solution is (5-6): (1-3): (10-15), and the stirring speed is 300-600 rpm.
9. A method for treating galaxolide waste aluminum water according to claim 6, It is characterized in that In step A2, the heating rate in the muffle furnace is 2-5°C / min, firstly the temperature is raised to 300-350°C and kept for 1-2h, then the temperature is further raised to 500-550°C and kept for 2-3h to complete the roasting.
Citation Information
Patent Citations
Method for preparing polyaluminum chloride
CN105967298A
Method for preparing polyaluminium chloride water purifying agent from aluminum residues
CN107265581A
Method for deeply removing soluble residual aluminum in water
CN108975440A
Technology for recycling and preparing polyaluminium chloride from wastewater
CN110282802A
Galaxolide waste aluminum salt water treatment method
CN111732118A