Production process and production equipment of microporous heat-insulating self-flowing material
By preparing flowable microporous particles and using special mixing devices for uniform mixing, the existing microporous thermal insulation materials are solved in the construction of easy damage and uneven filling bodies, achieving efficient thermal insulation and convenient construction. Improved thermal insulation and structural strength.
Patent Information
- Application Number
- CN202411088570.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
Existing microporous thermal insulation materials are prone to missing corners and difficult to cut during construction, and the filling body structure is uneven, resulting in inconsistent insulation effects, and common materials are difficult to apply in complex structures and irregular spaces.
Using microporous particles composed of micro-nano powders, functional fillers, glidants, dispersants and reinforcing fiber materials, flowable microporous particles are prepared through specific mixing and drying processes, and uniformly mixed using a special mixing device. With atomization treatment, the formed micropore heat-insulated self-flow material can be directly filled into the special-shaped space and is shaped after light pressure or high temperature treatment.
It realizes uniform filling and efficient heat insulation of microporous heat insulation self-flow materials, avoids heat leakage gaps and cost improvements, has high structural strength of the material, good construction convenience, low thermal conductivity, and better thermal insulation effect than traditional materials.
Smart Images

Figure CN118993690A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of microporous thermal insulation materials, in particular to a microporous thermal insulation self-flowing material production process and production equipment thereof. Background Art
[0002] Microporous insulation materials have extremely low thermal conductivity and good thermal insulation effects. They are widely used in thermal insulation linings of various containers, equipment and kilns. They can be used stably for long-term use at temperatures ranging from room temperature to 1100°C. They are usually in the form of plates or thin plates with slight curvature. The strength of the material is not high, and the hardness is generally not higher than 90HC. The compressive strength (10% compression strength) is generally lower than 0.35MPa, which makes it easy for the material to be chipped or even cracked or damaged during construction, making it difficult to construct. If the material needs to be cut and constructed on the job site, it is also difficult to cut to the exact size, and it is even more difficult to apply to complex structures and irregular spaces that require insulation.
[0003] At present, the commonly used thermal insulation materials are loose fiber cotton, fiber insulation felt and lightweight thermal insulation self-flowing castables. Among them, loose fiber cotton can be well filled into irregular and complex spaces, with convenient construction and high temperature resistance. However, fiber is a friction material that does not flow and has a large resilience, which will lead to the non-dense space after filling, and there are a large number of pores with serious uneven distribution, resulting in uneven filling structure, different densities in different parts, and large differences in insulation effect in different parts, which ultimately leads to the overall insulation effect; fiber insulation felt can be cut and assembled according to the space, but it will cause a large number of splicing gaps in the space, which will lose a lot of heat. At the same time, cutting and assembly will also cause a significant increase in costs. In addition, the material cannot be applied to the position where the space is distorted; while lightweight thermal insulation self-flowing castables are similar to concrete, with convenient construction and uniform filling structure, but the final filling molding has poor insulation effect, and the thermal conductivity is about 3 to 5 times that of fiber cotton or insulation felt materials. Summary of the invention
[0004] The technical problem to be solved by the present invention is to overcome the existing defects and provide a microporous thermal insulation self-flowing material production process and production equipment, which can be directly filled into any special-shaped space, has low thermal conductivity and no heat leakage gaps, and can effectively solve the problems in the background technology.
[0005] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a production process of microporous thermal insulation self-flowing material, which is composed of flowable microporous particles, wherein the microporous particles contain the following components in parts by weight: 40 to 85 parts of micro-nano powder, 10 to 50 parts of functional filler, 1 to 5 parts of flow aid, 0.1 to 5 parts of dispersant, and 0.5 to 8 parts of reinforcing fiber material. The above raw materials except the dispersant are poured into a mixing device in proportion and mixed evenly. The dispersant is prepared into an aqueous solution and mixed with the raw materials in an atomized manner. After mixing, the blocks are pressed into blocks, and then crushed into particles after high-temperature drying at 80 to 100°C, and finally qualified microporous particles are screened out.
[0006] As a preferred technical solution of the present invention, the critical particle size of the microporous particles is 2 to 4 mm, the minimum particle size is not less than 0.1 to 0.3 mm, and the loose bulk density is 140 to 320 kg / m 3 .
[0007] As a preferred technical solution of the present invention, the micro-nano powder is composed of one or more of silica aerogel, silicon oxide, aluminum oxide and titanium oxide;
[0008] The functional filler is one or more of metallic silicon, zinc oxide, rutile, silicon carbide, manganese oxide and zircon;
[0009] The flow aid is one or more of graphite, silicon nitride, mica and talc;
[0010] The reinforcing fiber material is one or more of high-silica glass fiber, basalt fiber, aluminum silicate fiber and alkaline earth silicate fiber;
[0011] The dispersant is one or more of polysodium phosphate, ammonium polyacrylate and tetramethylammonium hydroxide.
[0012] As a preferred technical solution of the present invention, the surface area of the micro-nano powder is not less than 20g / m 2 .
[0013] As a preferred technical solution of the present invention, the particle size of the functional filler is not less than 200 meshes.
[0014] As a preferred technical solution of the present invention, the reinforcing fiber material needs to be heat treated at a temperature of 600 to 1000° C. for a time of 1 to 10 hours.
[0015] As a preferred technical solution of the present invention, the viscosity of the prepared dispersant aqueous solution is 1 to 4 mpa·s.
[0016] A production equipment for a microporous thermal insulation self-flowing material production process, the mixing device comprises a base, the upper end of the base is symmetrically provided with a bracket, a mixing barrel is horizontally placed on the bracket, the upper end of the outer side surface of the mixing barrel is provided with a feed inlet, the lower end of the outer side surface of the mixing barrel is provided with a discharge outlet, one end of the mixing barrel is provided with a rotating motor, the output end of the rotating motor is connected to a stirring shaft, the stirring shaft is located in the mixing barrel, the outer side surface of the stirring shaft is provided with a stirring blade, the stirring blade is a spiral structure, the outer end of the stirring blade is in contact with the inner side surface of the mixing barrel, the lower end of the outer side surface of the mixing barrel is provided with an air collecting box, the air collecting box is evenly distributed with a plurality of air outlet holes, the air outlet holes penetrate the mixing barrel, the air outlet holes are located at the gap between the stirring blade and the inner wall of the mixing barrel, one end of the air collecting box is connected to an air pump through a connecting air pipe, and the air pump is fixed on the upper surface of the base;
[0017] An atomizing material inlet is arranged on one side of the feed port, an atomizing nozzle is arranged in the atomizing material inlet, the atomizing nozzle faces the inside of the mixing barrel, the upper end of the atomizing nozzle is connected to the atomizer through an atomizing connecting pipe, and the atomizer is fixed on the upper surface of the base.
[0018] As a preferred technical solution of the present invention, an exhaust pipe is arranged on the upper end of the outer side surface of the mixing cylinder, and a filter is arranged inside the exhaust pipe.
[0019] Compared with the prior art, the beneficial effects of the present invention are: (1) the self-flowing material is composed of microporous particles with a critical size of no more than 4 mm that can flow. The overall structure of the lining formed after filling is uniform and can be shaped by light pressing or high-temperature treatment. It is easy to construct and has good thermal insulation. (2) the material does not require shearing, assembly or even stacking, and there are no leakage hot spots. (3) through reasonable particle grading, the granular material can be densely packed and the molded body can have high strength. (4) the raw materials are mixed by a special mixing device to ensure the uniformity of the raw material mixing and improve the quality of the microporous particles. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the structure of the present invention;
[0021] Figure 2 It is the front view of the present invention;
[0022] Figure 3 It is a main cross-sectional view of the present invention;
[0023] Figure 4 for Figure 2 Left view of
[0024] Figure 5 for Figure 2 Top view of the .
[0025] In the figure: 1 base, 2 bracket, 3 mixing barrel, 4 rotating motor, 5 stirring shaft, 6 stirring blade, 7 feeding port, 8 discharging port, 9 air pump, 10 connecting air pipe, 11 air collecting box, 12 air outlet, 13 exhaust pipe, 14 filter screen, 15 atomizing material inlet, 16 atomizing nozzle, 17 atomizing connecting pipe, 18 atomizer. DETAILED DESCRIPTION
[0026] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] Example 1: A process for producing microporous thermal insulation self-flowing materials, wherein the microporous particles contain the following components in parts by weight: 10 parts of silica aerogel powder, 47 parts of silicon oxide powder (22 g / m 2 ), 20 parts of alumina powder (specific surface 80g / m 2 ) is composed of micro-nano powder, 20 parts of rutile, 2 parts of graphite, 0.7 parts of aluminum silicate fiber, and 0.3 parts of tetramethyl ammonium hydroxide, and the tetramethyl ammonium hydroxide is prepared into a 3% solution. The above raw materials except the dispersant are poured into a mixing device in proportion and mixed evenly. The dispersant is prepared into an aqueous solution and mixed with the raw materials in an atomized manner. The mixing time is 20 minutes. After mixing, it is pressed into a block, and then dried at 85°C and broken into particles. Finally, microporous particles of 0.1-2.5 mm are screened out. The loose bulk density of the particles is 295kg / m 3 When the molding density is 350kg / m 3 When the thermal conductivity of the material is 800℃ on the hot surface, it is 0.045W / (mK).
[0028] Example 2: A process for producing microporous thermal insulation self-flowing materials, wherein the microporous particles contain the following components in parts by weight: 40 parts of silicon oxide powder (specific weight 130 g / m 2 ) and 40 parts of alumina powder (specific surface 80g / m 2 ) is composed of micro-nano powder, 16 parts of zinc oxide, 2 parts of graphite, 1.6 parts of alkaline earth silicate fiber, and 0.4 parts of polysodium phosphate, and the polysodium phosphate is prepared into a 3% solution. The above raw materials except the dispersant are poured into a mixing device in proportion and mixed evenly. The dispersant is prepared into an aqueous solution and mixed with the raw materials in an atomized manner. The mixing time is 20 minutes. After mixing, it is pressed into a block, and then dried at 90°C and broken into particles. Finally, microporous particles of 0.5-4mm are screened out. The loose bulk density of the particles is 191kg / m 3 When the molding density is 246kg / m 3When the thermal conductivity of the material is 800℃ on the hot surface, it is 0.033W / (mK).
[0029] Example 3: A process for producing microporous thermal insulation self-flowing materials, wherein the microporous particles contain the following components in parts by weight: 55 parts of silicon oxide powder (specific weight 180 g / m 2 ) and 30 parts of titanium oxide powder (specification 80g / m 2 ) is composed of micro-nano powder, 13 parts of zircon, 2 parts of silicon nitride, 0.7 parts of high silica glass fiber, and 0.3 parts of ammonium polyacrylate, and the ammonium polyacrylate is configured into a 3% solution. The above raw materials except the dispersant are poured into a mixing device in proportion and mixed evenly. The dispersant is prepared into an aqueous solution and mixed with the raw materials in an atomized manner. The mixing time is 20 minutes. After mixing, it is pressed into blocks, and then dried at 100°C and broken into particles. Finally, microporous particles of 0.1 to 4 mm are screened out. The loose bulk density of the particles is 178kg / m 3 When the molding density is 227kg / m 3 When the thermal conductivity of the material is 800℃ on the hot surface, it is 0.031W / (mK).
[0030] like Figure 1-5 As shown, a mixing device used in a microporous thermal insulation self-flowing material production process comprises a base 1, a bracket 2 is symmetrically arranged on the upper end of the base 1, a mixing barrel 3 is horizontally placed on the bracket 2, a feed port 7 is arranged on the upper end of the outer side surface of the mixing barrel 3, a discharge port 8 is arranged on the lower end of the outer side surface of the mixing barrel 3, a rotating motor 4 is arranged at one end of the mixing barrel 3, the output end of the rotating motor 4 is connected to a stirring shaft 5, the stirring shaft 5 is located in the mixing barrel 3, a stirring blade 6 is arranged on the outer side surface of the stirring shaft 5, the stirring blade 6 is a spiral structure, the outer end of the stirring blade 6 is in contact with the inner side surface of the mixing barrel 3, an air collecting box 11 is arranged at the lower end of the outer side surface of the mixing barrel 3, a plurality of air outlet holes 12 are evenly distributed on the air collecting box 11, the air outlet holes 12 penetrate the mixing barrel 3, the air outlet holes 12 are located at the gap between the stirring blade 6 and the inner wall of the mixing barrel 3, one end of the air collecting box 11 is connected to the air pump 9 through a connecting air pipe 10, and the air pump 9 is fixed on the upper surface of the base 1;
[0031] An atomizing material inlet 15 is provided on one side of the feed port 7 , and an atomizing nozzle 16 is provided in the atomizing material inlet 15 . The atomizing nozzle 16 faces the inside of the mixing barrel 3 , and the upper end of the atomizing nozzle 16 is connected to an atomizer 18 through an atomizing connecting pipe 17 . The atomizer 18 is fixed on the upper surface of the base 1 .
[0032] After weighing the micro-nano powder, functional filler, flow aid and reinforcing fiber material, they are added to the mixing barrel 3 through the feed port 7. After the powder raw materials are added, the rotating motor 4 is started. The rotating motor 4 drives the spiral stirring blade 6 to rotate to mix the raw materials and feed them to the discharge port 8 at the same time. At this time, the air pump 9 is turned on to pass the compressed air into the air collecting box 11, and then the air flow is provided into the mixing barrel 3 through the multiple air outlets 12 on the mixing barrel 3. Under the action of the air flow, the powder raw materials are inflated and fully mixed; the dispersant is prepared into an aqueous solution and poured into the atomizer 18, and sprayed into the mixing barrel 3 through the atomizing nozzle 16, so that the dispersant and the powder raw materials are evenly mixed. The dispersant mainly prevents the powder raw materials from sticking together due to static electricity, which is not conducive to the full mixing of the raw materials.
[0033] In order to prevent the raw materials from escaping during exhaust, an exhaust pipe 13 is provided at the upper end of the outer surface of the mixing barrel 3 , and a filter screen 14 is provided inside the exhaust pipe 13 .
[0034] After the microporous heat insulation self-flowing material is filled into the special-shaped space, the molding density is generally 220-280kg / m 3 According to the molding density of 250kg / m3, its thermal conductivity (hot surface 800℃) is 0.038W / (mK), which is about 1 / 3 to 1 / 4 of conventional fibrous materials, less than 0.14W / (mK) of fiber cotton or fiber felt, 0.05W / (mK) of flexible felt, and 0.35W / (mK) of thermal insulation self-flowing castables, with good thermal insulation effect. Due to the fluidity of this material, the overall structure of the lining formed after filling is uniform, the thermal insulation effect is better, no size processing is required, and it can be shaped by light pressing or high temperature treatment, and the construction is convenient.
[0035] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A production process for microporous thermal insulation self-flowing materials, Features: The invention is composed of flowable microporous particles, wherein the microporous particles contain the following components in parts by weight: 40 to 85 parts of micro-nano powder, 10 to 50 parts of functional filler, 1 to 5 parts of flow aid, 0.1 to 5 parts of dispersant and 0.5 to 8 parts of reinforcing fiber material. The above raw materials except the dispersant are poured into a mixing device in proportion and mixed evenly. The dispersant is prepared into an aqueous solution and mixed with the raw materials in an atomized manner. After mixing, the solution is pressed into blocks, and then dried at a high temperature of 80 to 100° C. and crushed into particles. Finally, qualified microporous particles are screened out.
2. A microporous thermal insulation self-flowing material production process according to claim 1, Features: The critical particle size of the microporous particles is 2-4 mm, the minimum particle size is not less than 0.1-0.3 mm, and the loose bulk density is 140-320 kg / m 3 .
3. A microporous thermal insulation self-flowing material production process according to claim 1, Features: The micro-nano powder is composed of one or more of silicon dioxide aerogel, silicon oxide, aluminum oxide and titanium oxide; The functional filler is one or more of metallic silicon, zinc oxide, rutile, silicon carbide, manganese oxide and zircon; The flow aid is one or more of graphite, silicon nitride, mica and talc; The reinforcing fiber material is one or more of high-silica glass fiber, basalt fiber, aluminum silicate fiber and alkaline earth silicate fiber; The dispersant is one or more of polysodium phosphate, ammonium polyacrylate and tetramethylammonium hydroxide.
4. A microporous thermal insulation self-flowing material production process according to claim 1 or 3, Features: The surface area of the micro-nano powder is not less than 20 g / m 2 .
5. A microporous thermal insulation self-flowing material production process according to claim 1 or 3, Features: The particle size of the functional filler is not less than 200 meshes.
6. A microporous thermal insulation self-flowing material production process according to claim 1 or 3, Features: The reinforcing fiber material needs to be heat treated at a temperature of 600 to 1000° C. for a time of 1 to 10 hours.
7. A microporous thermal insulation self-flowing material production process according to claim 1, Features: The viscosity of the prepared dispersant aqueous solution is 1-4 mpa·s.
8. A production equipment for a microporous thermal insulation self-flowing material production process as claimed in claim 1, Features: The mixing device comprises a base (1), a bracket (2) is symmetrically arranged at the upper end of the base (1), a mixing barrel (3) is horizontally placed on the bracket (2), a feed port (7) is arranged at the upper end of the outer side surface of the mixing barrel (3), a discharge port (8) is arranged at the lower end of the outer side surface of the mixing barrel (3), a rotating motor (4) is arranged at one end of the mixing barrel (3), the output end of the rotating motor (4) is connected to a stirring shaft (5), the stirring shaft (5) is located in the mixing barrel (3), and a stirring blade (6) is arranged on the outer side surface of the stirring shaft (5). The stirring blade (6) is of a spiral structure. The outer end of the stirring blade (6) is in contact with the inner side surface of the mixing barrel (3). An air collecting box (11) is provided at the lower end of the outer side surface of the mixing barrel (3). A plurality of air outlet holes (12) are evenly distributed on the air collecting box (11). The air outlet holes (12) penetrate the mixing barrel (3). The air outlet holes (12) are located at the gap between the stirring blade (6) and the inner wall of the mixing barrel (3). One end of the air collecting box (11) is connected to an air pump (9) via an air pipe (10). The air pump (9) is fixed on the upper surface of the base (1). An atomizing material inlet (15) is provided on one side of the feed port (7), and an atomizing nozzle (16) is provided in the atomizing material inlet (15). The atomizing nozzle (16) faces the interior of the mixing barrel (3), and the upper end of the atomizing nozzle (16) is connected to an atomizer (18) via an atomizing connecting pipe (17). The atomizer (18) is fixed on the upper surface of the base (1).
9. A microporous thermal insulation self-flowing material production equipment according to claim 8, Features: An exhaust pipe (13) is arranged at the upper end of the outer surface of the mixing cylinder (3), and a filter screen (14) is arranged inside the exhaust pipe (13).