Method and device for preparing cyclopentadiene through dicyclopentadiene gas phase depolymerization
By using the mixing of dicyclopentadiene and superheated steam and direct heat transfer between inert solid particles in the gas phase depolymerization process, the poor heat exchange efficiency and coking problems in the traditional gas phase depolymerization process are solved, and the efficient cyclopentadiene is achieved preparation.
Patent Information
- Application Number
- CN202411048452.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-22
AI Technical Summary
In the traditional gas phase depolymerization process, the tubular reactor heated by the inter-wall has poor heat exchange efficiency and coking problems, which affects the equipment life and the yield of cyclopentadiene.
After mixing dicyclopentadiene with superheated steam, it is used to depolymerize with inert solid particles in the down tube reactor. Inert solid particles are used as a heat carrier with high heat capacity for direct heat transfer, reducing the temperature and residence of the heat exchange medium. Time suppresses coking of the reactor wall.
It improves heat exchange efficiency, reduces coking phenomenon, extends the equipment operation time, and improves the yield and product purity of cyclopentadiene.
Smart Images

Figure CN118993831A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of comprehensive utilization of petrochemical products, and in particular to a method and a device for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene. Background Art
[0002] Cyclopentadiene and its dimer dicyclopentadiene are mainly byproducts of petroleum cracking to produce ethylene. In the cracking C5 fraction, it exists in the form of cyclopentadiene, with a content of about 15% to 20%, and in the cracking C9 fraction, it exists in the form of dicyclopentadiene, with a content of about 25% to 30%. The content is mainly affected by the cracking raw materials and cracking depth. Cyclopentadiene or dicyclopentadiene is widely used in the fields of synthetic resins, synthetic rubbers, and synthetic raw materials for the preparation of fine chemicals, and is an important chemical raw material.
[0003] Cyclopentadiene is a conjugated diene with an active methylene group, and its chemical properties are very active. It is also easy to undergo Diels-Alde reaction at room temperature, dimerizing into dicyclopentadiene, and therefore is usually stored and transported in the form of dicyclopentadiene. Dicyclopentadiene can still be depolymerized into cyclopentadiene by heating (>170 ℃), so when using cyclopentadiene, it is usually prepared by heating with dicyclopentadiene as a raw material. At the same time, the dimerization reaction and depolymerization reaction of cyclopentadiene and dicyclopentadiene are often used in production to separate and purify cyclopentadiene from cracked carbon five fractions or cracked carbon nine fractions. In summary, the depolymerization reaction of dicyclopentadiene is a key step and has always been the research focus in this field.
[0004] The depolymerization process of dicyclopentadiene is roughly divided into two types: liquid phase depolymerization and gas phase depolymerization. The liquid phase depolymerization process is to directly heat the liquid phase dicyclopentadiene to 165-220℃ for depolymerization reaction. The advantages of this process are relatively mild reaction conditions, short process route, and simple equipment. The disadvantage is that the reaction rate is relatively slow, and the depolymerization process is often accompanied by the polymerization reaction of cyclopentadiene, which generates more by-products and leads to low yield. The gas phase depolymerization process is to first vaporize dicyclopentadiene and then heat it to 280-370℃ for depolymerization reaction. This process has the following characteristics: fast reaction rate, high conversion rate, and complete reaction in a very short time; the probability of intermolecular collision under gaseous conditions is reduced, which inhibits the occurrence of side reactions such as polymerization reaction, and greatly improves the yield of cyclopentadiene. However, the gas phase depolymerization process equipment is complex, and if the conditions are not well controlled at high temperature, it is easy to coke, which affects the life of the equipment.
[0005] The reactor of the traditional gas phase depolymerization process mostly adopts a tubular reactor with partition wall heating. This method has certain limitations, such as: low heat exchange efficiency, easy coking on the heat exchange wall due to local over-high temperature, affecting heat exchange efficiency and medium flow, coking cannot be removed during operation, and can only be stopped and cleaned regularly. Therefore, those skilled in the art are in urgent need of disclosing a method and device for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene to solve the problems of coking and poor heat exchange efficiency in the above gas phase depolymerization process. Summary of the invention
[0006] The object of the present invention is to provide a method and device for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene, so as to solve the coking problem caused by poor heat exchange efficiency when depolymerizing dicyclopentadiene in a tubular reactor with partition heating.
[0007] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:
[0008] The present invention provides a method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene, comprising the following steps:
[0009] 1) mixing dicyclopentadiene with superheated steam to obtain a gas-liquid mixture, and vaporizing the gas-liquid mixture to obtain a gas mixture;
[0010] 2) The gas mixture and the inert solid particles are introduced into a reactor to carry out a depolymerization reaction to obtain cyclopentadiene.
[0011] Preferably, the temperature of the superheated steam in step 1) is 140-200°C.
[0012] Preferably, the mass ratio of dicyclopentadiene to superheated steam in step 1) is 1.5 to 3.5:1.
[0013] Preferably, the temperature of the gas mixture in step 1) is 160-200°C.
[0014] Preferably, the particle size of the inert solid particles in step 2) is 50 to 100 μm;
[0015] The temperature of the inert solid particles is 280-380°C;
[0016] The inert solid particles include one or more of diatomaceous earth, kaolin and natural white clay.
[0017] Preferably, in step 2), the mass ratio of the gas mixture to the inert solid particles is 15 to 25:1.
[0018] Preferably, the gas mixture in step 2) stays in the reactor for 2 to 10 seconds;
[0019] The temperature of the depolymerization reaction is 280-380°C.
[0020] The present invention also provides a device for preparing cyclopentadiene by gas-phase depolymerization of dicyclopentadiene used in the above-mentioned method for preparing cyclopentadiene by gas-phase depolymerization of dicyclopentadiene, the device comprising a gas-liquid mixing tank (1), a vaporizer (3), a downcomer reactor (4), a gas-solid primary separation device (5), a cyclone separator (8), a spray cooling tower (10) and a dehydration tank (11) connected in sequence.
[0021] Preferably, it further comprises a riser (6), a regeneration chamber (7) and a heat carrier cooler (9);
[0022] The discharge port of the downcomer reactor (4) is cyclically connected in sequence to the gas-solid primary separation device (5), the riser (6), the regeneration chamber (7), the heat carrier cooler (9) and the feed port of the downcomer reactor (4).
[0023] The present invention has at least the following beneficial effects:
[0024] 1. Dicyclopentadiene is gasified with superheated steam and then introduced into the reactor. Preheating and reaction are all completed in the reactor, eliminating the need for a separate preheater, shortening the process flow before the reactor, and helping to reduce the possibility of coking.
[0025] 2. In the reactor, the present invention uses inert solid particles as heat carriers, which are in direct contact with gaseous reactants in a fluidized state and carry out heat transfer process at the same time. The advantages are that the heat carrier has high heat capacity and large heat storage capacity, and does not require very high temperature to provide the heat required for preheating and reaction. The heat exchange medium is in direct contact, and the fluidized state is disturbed violently, which greatly enhances the heat exchange efficiency and shortens the required residence time. The gas-solid two-phase medium is evenly distributed in the reactor, without back mixing, with fast flow speed and short residence time, which can effectively inhibit overreaction, and the gas-solid medium feed amount can be flexibly adjusted according to needs.
[0026] 3. Using inert solid particles as heat carriers can also inhibit coking on the reactor wall. The coke attached to the solid particles can be removed from the reactor in time and decomposed by itself in a high-temperature flue gas environment. The inert solid particles can also be recycled. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 A schematic diagram of a device for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene;
[0028] Among them, 1-gas-liquid mixing tank, 2-atomizing nozzle, 3-vaporizer, 4-down pipe reactor, 5-gas-solid primary separation device, 6-rising pipe, 7-regeneration chamber, 8-cyclone separator, 9-heat carrier cooler, 10-spray cooling tower, 11-dehydration tank. DETAILED DESCRIPTION
[0029] The present invention provides a method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene, comprising the following steps:
[0030] 1) mixing dicyclopentadiene with superheated steam to obtain a gas-liquid mixture, and vaporizing the gas-liquid mixture to obtain a gas mixture;
[0031] 2) The gas mixture and the inert solid particles are introduced into a reactor to carry out a depolymerization reaction to obtain cyclopentadiene.
[0032] In the present invention, dicyclopentadiene is preferably atomized before being mixed with superheated steam, which is beneficial to strengthening the gas-liquid mixing process and the heat transfer process. The uniform gas-liquid mixing is beneficial to lowering the temperature required for complete vaporization and reducing the load of the vaporizer.
[0033] In the present invention, the temperature of the superheated steam in step 1) is 140-200°C, preferably 150-190°C, more preferably 160-180°C, and more preferably 170°C.
[0034] In the present invention, the temperature of the dicyclopentadiene in step 1) is preferably 80-100°C, more preferably 85-95°C, and more preferably 90°C.
[0035] In the present invention, the mass ratio of dicyclopentadiene to superheated steam in step 1) is 1.5 to 3.5:1, preferably 1.8 to 3.2:1, more preferably 2 to 3:1, and more preferably 2.3 to 2.7:1.
[0036] In the present invention, the temperature of the gas mixture in step 1) is 160-200°C, preferably 165-195°C, more preferably 170-190°C, and more preferably 175-185°C.
[0037] In the present invention, the particle size of the inert solid particles in step 2) is 50 to 100 μm, preferably 60 to 90 μm, and more preferably 70 to 80 μm.
[0038] In the present invention, the temperature of the inert solid particles is 280-380°C, preferably 300-360°C, more preferably 320-340°C, and even more preferably 330°C.
[0039] In the present invention, the inert solid particles include one or more of diatomaceous earth, kaolin and natural clay.
[0040] In the present invention, the mass ratio of the gas mixture to the inert solid particles in step 2) is 15 to 25:1, preferably 17 to 23:1, and more preferably 18 to 20:1.
[0041] In the present invention, the gas mixture in step 2) stays in the reactor for 2 to 10 seconds, preferably 4 to 9 seconds, more preferably 5 to 8 seconds, and even more preferably 6 seconds.
[0042] In the present invention, the temperature of the depolymerization reaction is 280 to 380°C, preferably 300 to 370°C, and more preferably 320 to 350°C.
[0043] The present invention also provides a device for preparing cyclopentadiene by gas-phase depolymerization of dicyclopentadiene used in the above-mentioned method for preparing cyclopentadiene by gas-phase depolymerization of dicyclopentadiene, the device comprising a gas-liquid mixing tank (1), a vaporizer (3), a downcomer reactor (4), a gas-solid primary separation device (5), a cyclone separator (8), a spray cooling tower (10) and a dehydration tank (11) connected in sequence.
[0044] In the present invention, it also includes a riser (6), a regeneration chamber (7) and a heat carrier cooler (9);
[0045] The discharge port of the downcomer reactor (4) is cyclically connected in sequence to the gas-solid primary separation device (5), the riser (6), the regeneration chamber (7), the heat carrier cooler (9) and the feed port of the downcomer reactor (4).
[0046] In the present invention, an atomizing nozzle (2) is provided at the top of the gas-liquid mixing tank (1). The preheated dicyclopentadiene is atomized into tiny droplets through the atomizing nozzle (2) and sprayed downward. At the same time, superheated steam enters from the bottom of the gas-liquid mixing tank. The dicyclopentadiene and the superheated steam are mixed and heated in the gas-liquid mixing tank (1) and then discharged from the bottom to enter the vaporizer (3). The temperature of the vaporizer is controlled by a heat medium so that the mixture is completely vaporized in the vaporizer to obtain a gas mixture. The gas mixture enters the downcomer reactor (4) from the top. At the same time, the high-temperature inert solid particles in the regeneration chamber (7) are cooled to a suitable temperature by a heat carrier cooler (9) and then enter from the top of the downcomer reactor. They fall freely in the downcomer reactor and flow in parallel with the gas mixture. During this process, the gas mixture is rapidly heated to a predetermined reaction temperature to undergo a depolymerization reaction. After the reaction, the gas-solid mixture is discharged from the bottom of the reactor, and most of the solid particles are separated by the gas-solid primary separation device (5). The gas enters the spray cooling tower (9) after the remaining particles are separated by the cyclone separator (8). The spray cooling tower adopts a water spraying method to make the gas mixture directly exchange heat with cooling water to achieve the purpose of rapid cooling. Since cyclopentadiene and water have a large boiling point difference, the water in the mixture is condensed by controlling the cooling water amount, and the waste water is discharged from the bottom of the tower. The uncondensed cyclopentadiene is discharged from the top of the tower, and the entrained water is removed through the dehydration tank (10) to obtain a gas phase cyclopentadiene product. The inert solid particles separated after the reaction are returned to the regeneration chamber through the riser. The bottom of the regeneration chamber is blown with high-temperature flue gas to decompose or burn the cyclopentadiene entrained by the solid particles and the coke generated on the surface of the solid particles, and the solid particles are heated at the same time. The regenerated solid particles are cooled by the heat carrier cooler (9) and enter the downcomer reactor for recycling.
[0047] In the present invention, the lifting pipe (6) uses air as lifting wind.
[0048] In the present invention, the regeneration chamber (7) is a storage and regeneration place for inert solid particles, and an annular gap pipeline is provided at the bottom, through which high-temperature flue gas is blown into the regeneration chamber; the outlet of the downcomer reactor (4) is connected to the lifting pipe (6) through a gas-solid primary separation device (5) and a cyclone separator (8), and the mixture after the reaction is completed is separated from the gas and solid by the gas-solid primary separation device and the cyclone separator. The solid is an inert solid particle, which is lifted to the cyclone separator at the entrance of the regeneration chamber (7) through the lifting pipe (6), and the inert solid particles enter the regeneration chamber (7) through the discharge pipe of the cyclone separator, and a dense phase area is formed in the middle and lower part of the regeneration chamber (7). In this area, the inert solid particles are heated again, the entrained organic matter is decomposed, and the exhaust gas is discharged after passing through the cyclone separator.
[0049] In the present invention, the high-temperature flue gas can be high-temperature flue gas generated by other processes in the factory or heated high-temperature air.
[0050] The gas-solid preliminary separation device (5) utilizes the inertia difference between gas and solid to achieve preliminary gas-solid separation, and can separate most of the solids, thereby reducing the load of the subsequent cyclone separator.
[0051] In the present invention, the temperature in the regeneration chamber (7) is preferably 500 to 600°C, more preferably 550 to 600°C.
[0052] In the present invention, a coil is provided inside the heat carrier cooler (9), cooling water is passed through the coil, the heat carrier enters from the top of the cooler, excess heat is removed by the cooling water, the heat carrier is cooled to a suitable temperature, flows out from the bottom of the cooler, and enters the downcomer reactor (4).
[0053] In the present invention, the cooling medium of the spray cooling tower (9) is water, which rapidly cools the gas mixture after the reaction to prevent overreaction, condenses the water in the system and discharges it from the bottom of the tower. The outlet temperature of the gas from the spray cooling tower is controlled at 50-80°C.
[0054] The technical solutions provided by the present invention are described in detail below in conjunction with the embodiments, but they should not be construed as limiting the protection scope of the present invention.
[0055] Example 1
[0056] Use Figure 1 The device shown depolymerizes dicyclopentadiene, and dicyclopentadiene at a temperature of 90°C is atomized by an atomizing nozzle and then mixed with superheated steam at 140°C in a gas-liquid mixing tank to obtain a gas-liquid mixture, and the mass ratio of dicyclopentadiene to superheated steam is 1.5:1. The gas-liquid mixture is passed into a vaporizer (partitioning wall heat exchanger, heat medium is hot oil), and the temperature of the mixed gas at the outlet of the vaporizer is 170°C, and the material is completely vaporized. The mixed gas is introduced into the downcomer reactor, mixed with inert solid particles of diatomaceous earth with a temperature of 280°C and a particle size of 50 μm from the regeneration chamber, and flows downward. The mass ratio of the mixed gas to the inert solid particles is 20:1. The time for the mixed gas to pass through the downcomer reactor is controlled to be 10s, and the temperature in the downcomer reactor is 320°C. After the reaction is completed, the product and the inert solid particles flow out from the bottom of the reactor, and the gas-solid mixture is separated by a gas-solid primary separation device and a cyclone separator. The solid is an inert solid particle, which returns to the regeneration chamber (550°C) through a riser, is heated again by the high-temperature flue gas (550°C), and is cooled to the reaction temperature by a heating carrier cooler; the gas is a crude cyclopentadiene product, which is introduced into a spray cooling tower, and the gas is cooled by water as a spray medium. The generated liquid is discharged from the bottom of the tower, and the gas (50°C) is introduced into a dehydration tank for dehydration. The dehydration medium in the dehydration tank is a molecular sieve (3A molecular sieve), and finally a cyclopentadiene product is obtained. The composition of the product was analyzed by gas chromatography, and the result showed that the cyclopentadiene content was 99.1%.
[0057] Example 2
[0058] Use Figure 1 The device shown depolymerizes dicyclopentadiene, and dicyclopentadiene at a temperature of 90°C is atomized by an atomizing nozzle and then mixed with superheated steam at 170°C in a gas-liquid mixing tank to obtain a gas-liquid mixture, and the mass ratio of dicyclopentadiene to superheated steam is 2.5:1. The gas-liquid mixture is passed into a vaporizer (partitioning wall heat exchanger, the heat medium is hot oil), the temperature of the mixed gas at the outlet of the vaporizer is 170°C, and the material is completely vaporized. The mixed gas is introduced into the downcomer reactor, mixed with the inert solid particles of natural clay with a temperature of 330°C and a particle size of 70 μm from the regeneration chamber, and flows downward. The mass ratio of the mixed gas to the inert solid particles is 25:1. The time for the mixed gas to pass through the downcomer reactor is controlled to be 6s, and the temperature in the downcomer reactor is 300°C. After the reaction is completed, the product and the inert solid particles flow out from the bottom of the reactor, and the gas-solid mixture is separated by a gas-solid primary separation device and a cyclone separator. The solid is an inert solid particle, which returns to the regeneration chamber (500°C) through a riser, is heated again by the high-temperature flue gas (500°C), and is cooled to the reaction temperature by a heating carrier cooler. The gas is a crude cyclopentadiene product, which is introduced into a spray cooling tower, and the gas is cooled by water as a spray medium. The generated liquid is discharged from the bottom of the tower. The gas (65°C) is introduced into a dehydration tank for dehydration. The dehydration medium in the dehydration tank is a molecular sieve (3A molecular sieve), and finally a cyclopentadiene product is obtained. The composition of the product was analyzed by gas chromatography, and the result showed that the cyclopentadiene content was 99.4%.
[0059] Example 3
[0060] Use Figure 1The device shown depolymerizes dicyclopentadiene, and dicyclopentadiene at a temperature of 90°C is atomized by an atomizing nozzle and then mixed with superheated steam at 200°C in a gas-liquid mixing tank to obtain a gas-liquid mixture, and the mass ratio of dicyclopentadiene to superheated steam is 3.5:1. The gas-liquid mixture is passed into a vaporizer (partitioning wall heat exchanger, the heat medium is hot oil), the temperature of the mixed gas at the outlet of the vaporizer is 200°C, and the material is completely vaporized. The mixed gas is introduced into the downcomer reactor, mixed with inert solid particles of kaolinite with a temperature of 380°C and a particle size of 100 μm from the regeneration chamber, and flows downward. The mass ratio of the mixed gas to the inert solid particles is 15:1. The time for the mixed gas to pass through the downcomer reactor is controlled to be 2s, and the temperature in the downcomer reactor is 380°C. After the reaction is completed, the product and the inert solid particles flow out from the bottom of the reactor, and the gas-solid mixture is separated by a gas-solid primary separation device and a cyclone separator. The solid is an inert solid particle, which returns to the regeneration chamber (600°C) through a riser, is heated again by the high-temperature flue gas (600°C), and is cooled to the reaction temperature by a heating carrier cooler. The gas is a crude cyclopentadiene product, which is introduced into a spray cooling tower, and the gas is cooled by water as a spray medium. The generated liquid is discharged from the bottom of the tower. The gas (80°C) is introduced into a dehydration tank for dehydration. The dehydration medium in the dehydration tank is a molecular sieve (3A molecular sieve), and finally a cyclopentadiene product is obtained. The composition of the product was analyzed by gas chromatography, and the result showed that the cyclopentadiene content was 99.3%.
[0061] The heating method of the tubular reactor is inter-wall heating, and its heat exchange efficiency is lower than direct heat exchange. In order to maintain the temperature of the reaction tube cavity, the heat medium temperature is usually required to be higher than the reaction temperature, which makes the local temperature of the heat exchange surface too high, resulting in side reactions. A prominent problem of the traditional gas phase depolymerization process of dicyclopentadiene is that the wall of the reaction tube is easily coked due to local high temperature, and it has to be stopped and cleaned regularly. The process of the present invention adopts a direct heat exchange method between reactants and heat carriers, which has high heat exchange efficiency, large heat capacity of heat carriers, does not require excessively high temperatures, can suppress side reactions to a certain extent, and even if coking occurs, it is attached to the heat carrier, and can be moved out of the reactor in time with the flow of the heat carrier, and will not accumulate in the reactor. In the specific implementation process, the reaction unit has been running for more than 100 hours, and no coking phenomenon has been found in the reaction tube.
[0062] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene, characterized in that: The steps include: 1) mixing dicyclopentadiene with superheated steam to obtain a gas-liquid mixture, and vaporizing the gas-liquid mixture to obtain a gas mixture; 2) The gas mixture and the inert solid particles are introduced into a reactor to carry out a depolymerization reaction to obtain cyclopentadiene.
2. The method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to claim 1, characterized in that: The temperature of the superheated steam in step 1) is 140-200°C.
3. The method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to claim 2, characterized in that: The mass ratio of dicyclopentadiene to superheated steam in step 1) is 1.5 to 3.5:
1.
4. The method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to claim 3, characterized in that: The temperature of the gas mixture in step 1) is 160-200°C.
5. The method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to any one of claims 1 to 4, characterized in that: The particle size of the inert solid particles in step 2) is 50 to 100 μm; The temperature of the inert solid particles is 280-380°C; The inert solid particles include one or more of diatomaceous earth, kaolin and natural white clay.
6. The method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to claim 5, characterized in that: The mass ratio of the gas mixture to the inert solid particles in step 2) is 15-25:
1.
7. The method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to claim 5 or 6, characterized in that: The gas mixture in step 2) stays in the reactor for 2 to 10 seconds; The temperature of the depolymerization reaction is 280-380°C.
8. The device for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene used in the method for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to any one of claims 1 to 7, characterized in that: The device comprises a gas-liquid mixing tank (1), a vaporizer (3), a downcomer reactor (4), a gas-solid primary separation device (5), a cyclone separator (8), a spray cooling tower (10) and a dehydration tank (11) which are connected in sequence.
9. The device for preparing cyclopentadiene by gas phase depolymerization of dicyclopentadiene according to claim 8, characterized in that: It also includes a riser (6), a regeneration chamber (7) and a heat carrier cooler (9); The discharge port of the downcomer reactor (4) is cyclically connected in sequence to the gas-solid primary separation device (5), the riser (6), the regeneration chamber (7), the heat carrier cooler (9) and the feed port of the downcomer reactor (4).
Citation Information
Cited By
Device and method for efficiently depolymerizing polycaprolactone to recover high-purity epsilon-CL