Preparation method of high-purity aconitate
By destroying fat-soluble pigments in one-step oxidation and treating water-soluble pigments with two-step decolorization, the problem of difficult removal of pigment impurities in aconitate is solved, and the purity and color of the product are improved. It is suitable for expanding its application in plastics and other materials .
Patent Information
- Application Number
- CN202310580674.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-22
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2043-05-22
AI Technical Summary
In the existing preparation methods for aconitate, the products obtained by the fermentation method have pigment impurities that are difficult to remove, resulting in low purity and high chromaticity, which affects subsequent esterification reactions and product applications.
The one-step decolorization and two-step decolorization process are adopted, and the fat-soluble pigments are first destroyed by oxidation of hydrogen peroxide, and then the water-soluble pigments are selectively removed using decolorizers such as activated carbon and diatomaceous earth to improve the purity and colority of aconitine.
It significantly improves the purity of aconitate to more than 99%, reduces the color, expands its application range in materials such as plastics, and reduces production energy consumption.
Smart Images

Figure CN118993883A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to a method for preparing high-purity aconitate ester, and belongs to the technical field of aconitate ester preparation. Background Art
[0002] At present, the production of aconitic acid is mainly divided into fermentation and chemical synthesis. The fermentation method mainly relies on bacterial strains to convert sugar into aconitic acid. The chemical synthesis method is to heat citric acid to remove a molecule of water to form aconitic acid. However, this process requires extremely high temperatures and harsh production processes, making it difficult to achieve mass production of aconitic acid. Therefore, the fermentation method is currently the most widely used method. However, the aconitic acid obtained by the fermentation method will produce many impurities during the preparation process, accounting for between 2% and 40%. The impurities are mainly polysaccharides, pigments, and trace amounts of mycelium and protein.
[0003] The proportion of pigments is relatively small, generally between 1% and 5%, but their presence will greatly affect the color of the product. Aconitic acid is the synthetic raw material for aconitate esters. If it is not decolorized, the pigment impurities will continue to remain in the synthesized aconitate esters. When aconitate esters are used to prepare subsequent products, the pigment impurities in the aconitate esters have a great coloring effect on the final product and also have a huge impact on the subsequent application of the product; and the presence of polysaccharides will greatly affect the purity and yield of aconitate esters. On the one hand, polysaccharides themselves will be hydrolyzed into monosaccharides under acidic conditions, and monosaccharides have abundant hydroxyl groups and alcohols that compete with aconitate for the esterification reaction, making the aconitate ester product not pure enough, thereby reducing the yield of the final target product; on the other hand, polysaccharides will undergo a caramelization reaction under high temperature conditions, which will increase the chromaticity of aconitate esters and reduce the purity of aconitate esters, further affecting the use of aconitate esters.
[0004] At present, for the decolorization and purification methods of acids, the dissolution-precipitation method is used for acids with low solubility. By preparing a concentrated solution of the acid and heating it, due to its low solubility, it precipitates as the temperature decreases. At this time, the pigment impurities have not reached the precipitation limit, so they can be effectively purified; while the salt precipitation method is used for acids with high solubility. The acid is prepared into a concentrated solution and salt (such as calcium salt) is added to form a precipitate with the acid. The higher solubility can precipitate as much as possible, while the pigment impurities are precipitated less and can be further washed away, so effective purification can also be achieved.
[0005] Aconitic acid has a high solubility. When its concentrated solution is cooled and the product is precipitated, pigment impurities will also precipitate together. However, when using the salt precipitation method, it is difficult to effectively precipitate the aconitate because the solubility of the aconitate is still high, and it is even more difficult to retain the precipitated product during further cleaning and purification. If aconitic acid is decolorized and purified, it needs to be extracted with a polar organic solvent and then decolorized with an adsorbent. The above steps are cumbersome and if the organic extract is not removed cleanly, it will affect the subsequent synthesis reaction of aconitate. Therefore, the aconitate obtained by fermentation has the problem of being difficult to separate from the pigment, and the synthesized aconitate will inevitably carry pigment impurities, which increases the chromaticity of the aconitate product and reduces the purity.
[0006] The Chinese patent application number 200810195075.4 discloses a method for preparing tributyl citrate by catalysis of rare earth salt binary composite solid acid, wherein activated carbon and hydrogen peroxide are simultaneously added to the crude tributyl citrate product without washing and desolventizing steps for decolorization, but such method has poor effect, and this method can effectively remove the citrate ester with high raw material purity and low chromaticity. However, for aconitate ester with high pigment content and high pigment color, this method is difficult to effectively remove the pigment in the aconitate ester. Summary of the invention
[0007] In order to solve the above problems, a method for preparing high-purity aconitate is provided. The method performs a decolorization step before the desolventizing step, first destroys and oxidizes the fat-soluble pigment in the aconitate, and reduces the chromaticity effect caused by the fat-soluble pigment. After the desolventizing, a decolorizer is used to selectively remove the water-soluble pigment and the destroyed fat-soluble pigment in the aconitate. The combination of the two can improve the decolorization and impurity removal effect of the aconitate, so as to obtain high-purity aconitate and expand the application range of the aconitate.
[0008] The present application provides a method for preparing high-purity aconitate, comprising the following steps:
[0009] (1) reacting aconitic acid obtained by fermentation with alcohol to obtain a solution containing aconitic acid ester, neutralizing the solution containing aconitic acid ester and separating the solution to obtain an upper organic phase;
[0010] (2) adding hydrogen peroxide to the upper organic phase for one-step decolorization, followed by washing, separation, and desolventization to obtain a crude aconitate product;
[0011] (3) adding a decolorizing agent to the crude aconitate ester to perform a two-step decolorization, and then filtering to obtain aconitate ester with high purity;
[0012] The decolorizing agent is selected from at least one of activated carbon, diatomaceous earth, kaolin and alumina.
[0013] Since the aconitic acid raw material obtained by the fermentation method contains more pigments and different types of pigments have obvious differences in solubility in organic solvents and water, there are two types of pigments in the fermented aconitic acid. One is fat-soluble pigments, mainly anthraquinone compounds, most of which contain double bonds in their structures, have good compatibility with aconitic acid esters and are difficult to be adsorbed; the other is water-soluble pigments, which enter the organic phase with a small amount of water during the washing process and remain in the product after desolventization and water removal, so it is difficult to completely wash off in the water washing stage.
[0014] Usually react with an oxidant (such as hydrogen peroxide) (bleaching). In the preparation method, one-step decolorization and two-step decolorization are performed during the preparation of aconitate. The one-step decolorization mainly oxidizes and destroys the structure of the fat-soluble pigment. The double bonds in the pigment are oxidized by hydrogen peroxide, causing an oxidation reaction to decompose the organic skeleton of the pigment, producing hydroquinone, aldehyde substances, etc. Therefore, the chromaticity can be effectively reduced by destroying the main structure of the fat-soluble pigment. While hydrogen peroxide removes the chromaticity of the fat-soluble pigment, it increases the absorbance of the fat-soluble pigment adsorbed by the decolorizer, thereby combining with the two-step decolorization to effectively reduce the content of the fat-soluble pigment in the aconitate, but hydrogen peroxide and aconitate are not miscible, and washing with clean water is required after decolorization. Therefore, the one-step decolorization with hydrogen peroxide is placed before the washing and desolventizing steps, which can not only fully decolorize the fat-soluble pigments, but also ensure that the hydrogen peroxide is removed by the subsequent washing step. If the one-step decolorization is placed after the desolventizing step, the introduction of hydrogen peroxide will cause aconitate to form oil-water separation, and the hydrogen peroxide still needs to be further removed, resulting in cumbersome steps and reducing the removal rate of fat-soluble pigments.
[0015] After the desolventizing step, a second-step decolorization is performed, and water-soluble pigments are mainly removed. The decolorizing agent used can be evenly distributed in aconitate, and the aconitate is evenly decolorized in only one phase, thereby effectively reducing the content of water-soluble pigments in the aconitate. If the decolorizing agent is placed before the washing step or decolorized together with hydrogen peroxide, the decolorizing agent has different affinities with the aconitate and the solvent liquid phase, resulting in the decolorizing agent being absorbed by different liquid phases to form agglomerates. The agglomerates are dispersed in the aconitate and are difficult to be evenly mixed with the aconitate, resulting in insufficient contact between the aconitate and the aconitate, a decrease in the decolorization effect, and a reduction in the removal rate of the water-soluble pigment.
[0016] Optionally, the concentration of the hydrogen peroxide is 33-40%, and the weight of the hydrogen peroxide accounts for 1-5% of the weight of the upper organic phase.
[0017] Optionally, the weight ratio of the decolorizing agent to the crude aconitate is 1:(2-100).
[0018] The double bond in the fat-soluble pigment is the double bond in the alkyl chain, which has no large steric hindrance around itself and is easily destroyed. The double bond of aconitate is between two large steric hindrance ester groups and is difficult to be destroyed. Therefore, the concentration and weight of the above-mentioned hydrogen peroxide can quickly destroy the double bond of the fat-soluble pigment, thereby improving the removal rate of the fat-soluble pigment, and the hydrogen peroxide of this concentration and weight will not destroy the double bond in the aconitate, thereby improving the yield of the aconitate. The strong oxidizing property of hydrogen peroxide oxidizes the chromogenic functional group in the fat-soluble pigment into a non-color functional group, so the fat-soluble pigment material structure with the destroyed double bond changes and has no absorption to light. The hydrogen peroxide under this concentration has the best bleaching effect on the pigment in the aconitate, and the consumption of the decolorant can ensure that the decolorant is evenly dispersed in the aconitate, improves the adsorption effect on the fat-soluble pigment and water-soluble pigment with changed structure, and is conducive to the later removal of the decolorant. When the consumption exceeds 5%, hydrogen peroxide can cause the hydrolysis of aconitate, thereby affecting the yield.
[0019] Optionally, the temperature for one-step decolorization with hydrogen peroxide is 20-70° C. and the time is 15-30 min.
[0020] Optionally, the temperature for the two-step decolorization by the decolorizing agent is 20-70°C and the time is 10-120 min.
[0021] Optionally, the fat-soluble pigment includes anthraquinone compounds; and the water-soluble pigment includes terreusin.
[0022] Temperature is an important factor affecting the decolorization of pigment impurities in aconitic acid. The higher the temperature, the lower the viscosity of the product system, the better the fluidity, and the more evenly the decolorant is distributed in the system. However, the higher the temperature, the more violent the Brownian motion of the molecules, the more difficult it is for the decolorant to adsorb the pigment, which leads to a decrease in the removal rate of pigment impurities. In the decolorization of citrate esters, since citric acid contains hydroxyl groups in its structure, the hydroxyl groups easily form hydrogen bonds with hydroxyl groups and ester groups on other molecules, causing the product molecules to aggregate. The activated carbon used has poor adsorption effect, so high temperature is required to destroy the aggregation of molecules to achieve the purpose of decolorization.
[0023] The one-step decolorization temperature and the two-step decolorization temperature of the present application are relatively low. First, they can reduce energy consumption in the decolorization step. Second, after research, it is found that the lower the decolorization temperature, the lower the Brownian motion of the molecules, and the better the decolorization effect. Therefore, the above-mentioned decolorization temperature and time can effectively improve the removal efficiency and removal rate of pigment impurities, thereby improving the purity of aconitate.
[0024] Optionally, the iodine value of the activated carbon is greater than 800, and the Aran value is greater than 10; the particle size of the diatomaceous earth is 200-300 mesh; the particle size of the kaolin is 200-300 mesh; the particle size of the basic alumina and the neutral alumina are both 100-200 mesh, and the specific surface area is 60-90m 2 / g, average pore size 10-20nm. Under the setting of the above decolorizing agent, the decolorizing agent is evenly dispersed in the aconitate phase, avoiding agglomeration or aggregation of the decolorizing agent, and the decolorizing agent can increase the contact area with the water-soluble pigment and the fat-soluble pigment with the double bond destroyed, so that the above two pigments and other impurities are adsorbed and stored in the pores of the decolorizing agent itself, thereby improving the adsorption force on the pigment, preventing the pigment from escaping again after being adsorbed, and thus improving the removal effect of the water-soluble pigment, the fat-soluble pigment and the impurities.
[0025] Alumina itself has a large adsorption area and pores for adsorbing pigments. In the above system, since sugar and pigment impurities are generally acidic, when alkaline alumina and neutral alumina are selected in the decolorizer, the adsorption capacity for sugar and pigment impurities can be increased, and the removal rate of pigment impurities and sugars can be improved.
[0026] Optionally, the decolorizing agent is selected from activated carbon.
[0027] Optionally, the purity of the high-purity aconitate is not less than 99%.
[0028] Optionally, the chromaticity of the high-purity aconitate is no higher than 50Pt-Co.
[0029] The purity of aconitate prepared by the traditional method can reach up to 95%, and the chromaticity is above 500Pt-Co, which is obtained by testing with the platinum-cobalt colorimetry. In the preparation method of the present application, one-step decolorization and two-step decolorization are performed during the synthesis of aconitate, and the decolorization effect is improved by an order of magnitude, which not only reduces the chromaticity, but also reduces the impurity content, and increases the purity of the product to greater than or equal to 99%, and the purification effect is obvious.
[0030] Optionally, the content of fat-soluble pigments in the high-purity aconitate is less than 1000 ppm, and the content of water-soluble pigments is less than 1000 ppm.
[0031] The preparation method of the present application is applicable to the reaction of aconitic acid and any alcohol, and the alcohol can be a single alcohol, in which case a single aconitic acid ester is prepared, and the substituents on the single aconitic acid are the same; or it can be a mixed alcohol, in which case a mixed aconitic acid ester is prepared, and the substituents on the single aconitic acid are three the same, two the same and one different, or all three different.
[0032] Optionally, the alcohol in step (1) is selected from methanol, ethanol, 2-methoxyethanol, 2-ethoxyethanol, 2-butoxyethanol, propanol, isopropanol, n-butanol, isobutanol, tert-butanol, 4-methyl-2-butanol, 2-ethylbutanol, 3,3-dimethyl-2-butanol, 4-phenylbutanol, n-pentanol, isopentanol, tert-pentanol, 2-methylpentanol, 2-methyl-2-pentanol, 2-methyl-3-pentanol, 3-ethyl-3-pentanol, 4-methyl-1-pentanol, 4-methyl-2-pentanol, n-hexanol, 2-hexanol, 3-hexanol, 2-ethylhexanol , 3,5,5-trimethylhexanol, n-heptanol, 2-heptanol, 3-heptanol, 2-methylheptanol, 4-methyl-3-heptanol, 3-propylheptanol, 2,6-dimethyl-4-heptanol, n-octanol, 2-octanol, n-nonanol, 2-nonanol, 3-nonanol, 5-ethyl-2-nonanol, 2,6,8-trimethyl-4-nonanol, n-decanol, isodecanol, undecanol, dodecanol, cyclohexanol, cyclohexylmethanol, chloroethanol, 1-chloro-2-propanol, 3-chloro-1-propanol and 2-chloro-1-propanol, benzyl alcohol and phenylethyl alcohol.
[0033] Optionally, the temperature of the reaction of the fermented aconitic acid and alcohol is 75-145°C, and the reaction time is 2-8h. Under the action of the catalyst of the present application, the above reaction temperature and reaction time can not only improve the efficiency of the esterification reaction, but also avoid the fermented aconitic acid from reducing the purity of aconitic acid ester and improving the color of aconitic acid ester.
[0034] When the temperature is lower than 75℃, the efficiency of the esterification reaction will be greatly reduced. If a higher utilization rate or yield is required, a longer reaction time must be required. Polysaccharides are difficult to undergo esterification due to their large volume steric hindrance. However, a longer reaction time will cause the acidic catalyst to promote the hydrolysis of polysaccharides into monosaccharides, resulting in monosaccharides with rich hydroxyl groups competing with alcohols and esterification reactions of aconitic acid. When the temperature is higher than 145℃, polysaccharides will undergo caramelization, which will produce dark brown sugar dehydrated polymers, deepening the color of aconitic acid esters. A small amount of sugar dehydrated polymers can be absorbed by activated carbon. When the content is too high, it is difficult to remove and will block the adsorption pores of activated carbon, reducing the adsorption efficiency of activated carbon. Therefore, only at this temperature and after effective treatment can low-color and high-purity aconitic acid esters be obtained.
[0035] The esterification time of the present application is also determined by the fermentation-derived aconitic acid, which has many impurities and greatly affects the reaction rate. When the time is too short, the reaction is incomplete and it is difficult to obtain a higher yield; when the time is long, a large amount of polysaccharide hydrolysis will occur in the reaction, and the hydrolyzed monosaccharides will compete with alcohols for the esterification reaction, resulting in low product purity. Therefore, the esterification reaction can only be carried out within this time period to obtain high-purity, low-chroma, high-yield aconitate.
[0036] Optionally, in step (1), a water-carrying agent and a catalyst are added to aconitic acid and an alcohol solvent in a molar ratio of 1:(3-9), and the mixture is stirred at 75-145° C. for 2-8 h to obtain a solution containing aconitic acid ester, and the solution containing aconitic acid ester is neutralized with an alkaline washing solution and then separated to obtain an upper organic phase.
[0037] Preferably, the stirring speed is 100-1200 rpm.
[0038] Optionally, the water-carrying agent is selected from at least one of toluene, benzene, and cyclohexane, preferably toluene, and the molar ratio of the water-carrying agent to the aconitic acid is (0-5):1.
[0039] Optionally, the weight ratio of the catalyst to aconitic acid is 1:(2-100), and the catalyst is selected from a homogeneous catalyst and a heterogeneous catalyst. When a heterogeneous catalyst is used, it is not necessary to add a water-carrying agent, and the molar ratio of the water-carrying agent to aconitic acid is 0:1. When a homogeneous catalyst is used, it is necessary to add a water-carrying agent, and the molar ratio of the water-carrying agent to aconitic acid is (1-5):1.
[0040] Preferably, the homogeneous catalyst is selected from at least one of p-toluenesulfonic acid, p-toluenesulfonic acid monohydrate, dinitrobenzoic acid, diethylaminetetraacetic acid, trichloroacetic acid, methanesulfonic acid, ethanesulfonic acid, propanesulfonic acid, butanesulfonic acid, alkylsulfuric acid, dodecylbenzenesulfonic acid, aminosulfonic acid, tetrabutyl titanate, isopropyl titanate, stannous octoate, stannous chloride, antimony acetate, cobalt acetate, and manganese acetate, preferably p-toluenesulfonic acid and p-toluenesulfonic acid monohydrate. The above-mentioned homogeneous catalyst can promote the esterification reaction to be completed efficiently, fully, and rapidly to the greatest extent, reduce the generation of by-products, and the esterification reaction efficiency is high, the product quality is good, and the energy consumption is low. In the presence of the homogeneous catalyst, toluene, benzene or cyclohexane is used as a water-carrying agent to take water away from the reaction and separate the water, and at the same time, aconitic acid can be effectively mixed with alcohols to promote catalytic efficiency and increase reaction speed.
[0041] Preferably, the heterogeneous catalyst is selected from sodium bisulfate monohydrate, sodium bisulfate, potassium bisulfate, copper sulfate, ferric sulfate, titanium sulfate, aluminum sulfate, yttrium, cerium sulfate, lanthanum sulfate, magnesium sulfate, ferrous sulfate, ferrous ammonium sulfate, cerium methanesulfonate, ferric chloride, tin tetrachloride, titanium chloride, rare earth chloride, potassium hydroxide, sodium hydroxide, potassium bicarbonate, sodium bicarbonate, sodium carbonate, anion exchange resin, strong acid cation exchange resin, weak acid cation exchange resin, potassium sulfamate, sodium sulfamate, tetrabutylammonium chloride, tetrabutylammonium bromide, copper methanesulfonate at least one, preferably sodium bisulfate monohydrate, sodium bisulfate. The heterogeneous catalyst can achieve under relatively low temperature conditions, to the greatest extent promote the esterification reaction to be completed efficiently, fully and rapidly, reduce the generation of by-products, the esterification reaction efficiency is high, the product quality is good, the energy consumption is low, and it is easy to separate, convenient for post-processing, and the recovered catalyst can continue to be used, further reducing the industrialization cost.
[0042] In the traditional esterification reaction, concentrated sulfuric acid is used as a catalyst. Concentrated sulfuric acid has strong oxidizing properties and strong acidity at the same time. Although it can catalyze the reaction, it will carbonize the mycelium and protein in the fermented aconitic acid, resulting in the complexity and difficulty of aconitate. The above-mentioned homogeneous catalyst and heterogeneous catalyst replace the traditional concentrated sulfuric acid. The catalyst does not have strong oxidizing properties and acidity at the same time, and the side reactions in the esterification reaction can be effectively suppressed. For example, the acidity of p-toluenesulfonic acid is strong but non-oxidizing, and the acidity of sodium bisulfate itself is weaker than concentrated sulfuric acid, and the side reactions are less than concentrated sulfuric acid, and the product chromaticity purity is high. Therefore, the types of the above-mentioned homogeneous catalyst and heterogeneous catalyst are all arranged based on the aconitic acid obtained by fermentation, which can further improve the yield and purity of aconitate in the esterification reaction of aconitic acid and alcohols, and reduce the chromaticity of aconitate.
[0043] Optionally, when a heterogeneous catalyst is used, the reaction solution is obtained by filtering after the reaction between aconitic acid and alcohol.
[0044] Optionally, the reaction solution is neutralized by alkali washing three times with an alkali washing solution, and the alkali washing residue and salts generated by the alkali washing reaction in the solution are removed by water washing three times, and the upper organic phase is separated and collected.
[0045] Optionally, the solute of the alkaline washing solution is NaOH, NaHCO 3 and Na 2 CO 3 At least one of .
[0046] Preferably, the mass fraction of the solute in the alkaline washing solution is 5-25%.
[0047] Preferably, the reaction temperature for neutralizing the reaction solution by alkali washing is 20-70° C. and the reaction time is 15-30 min.
[0048] Optionally, the desolventizing temperature in step (2) is 40-100° C., and the vacuum degree is 0.01 mbar-100 mbar.
[0049] The impurities in aconitic acid are mainly monosaccharides and polysaccharides. Monosaccharides have a small molecular weight, such as mannose, glucose and galactose. Their molecules contain a large number of hydroxyl groups, which compete with alcohol for esterification, greatly reducing the purity of the product. Polysaccharides have a large molecular weight and a complex structure. They contain a large number of hydroxyl groups and have a large steric hindrance. Although the reaction rate with aconitic acid is slow, once esterified, its large steric hindrance makes it difficult for the other two carboxylic acids to esterify, thus affecting the yield and purity of the product. Therefore, whether it is a monosaccharide or a polysaccharide, the rate and purity of the aconitate esterification reaction will be greatly reduced.
[0050] Therefore, at the above temperature, the reaction rate of aconitic acid with alcohols is much greater than the reaction rate with impure sugars, and the reaction amount of catalyst and alcohol allows aconitic acid to be esterified with alcohols as much as possible, thereby improving the reaction conversion rate of aconitic acid. In addition, the above unreacted sugars and other impurities can also be removed through one-step decolorization and two-step decolorization processes, further improving the purity of aconitic acid esters.
[0051] The beneficial effects of this application include but are not limited to:
[0052] 1. According to the preparation method of the present application, the pigment impurities in the aconitic acid raw material obtained by fermentation are removed during the preparation of aconitate ester. On the basis of ensuring the smooth progress of the aconitate ester reaction, the purity of the aconitate ester can be effectively improved, solving the color problem of the aconitate esterification product from the fermentation source.
[0053] 2. According to the preparation method of the present application, the fat-soluble pigments and water-soluble pigments carried by aconitic acid are decolorized and removed step by step by using a one-step decolorization process and a two-step decolorization process, which can improve the impurity removal effect of aconitic acid esters, and the purity of aconitic acid esters can be increased from 95% to greater than or equal to 99%, so as to obtain high-purity aconitic acid esters.
[0054] 3. The aconitate obtained according to the preparation method of the present application has high purity and low chroma. When added to plastic products as a plasticizer, it will not affect the coloring of the plastic products themselves, improve the appearance quality, and improve the plasticizing effect on the plastic products.
[0055] 4. According to the preparation method of the present application, the decolorization process of hydrogen peroxide and decolorizing agent can achieve decolorization at low temperature, which can not only reduce the energy consumption in the decolorization process, but also improve the decolorization efficiency and pigment removal rate.
[0056] 5. According to the preparation method of the present application, the esterification reaction conditions of aconitic acid and alcohols, the type and amount of catalyst, the type and amount of water-carrying agent, the type of alkaline washing solution and the neutralization temperature are coordinated with each other to improve the reaction conversion rate of aconitic acid, and combined with the one-step decolorization and two-step decolorization processes, the synthesized aconitic acid ester has the characteristics of high purity, low acid value and low chroma. BRIEF DESCRIPTION OF THE DRAWINGS
[0057] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0058] Figure 1 This is a product picture of tributyl aconitate involved in Comparative Example 1 of the present application.
[0059] Figure 2 This is a product picture of tributyl aconitate involved in Example 1 of the present application.
[0060] Figure 3 This is a product picture of tributyl citrate involved in Comparative Example 4 of the present application.
[0061] Figure 4 This is a product picture of tributyl citrate involved in Comparative Example 5 of the present application.
[0062] Figure 5 This is the liquid phase spectrum of tributyl aconitate involved in Comparative Example 1 of the present application.
[0063] Figure 6 This is the liquid phase spectrum of tributyl aconitate involved in Example 1 of the present application. DETAILED DESCRIPTION
[0064] The present application is described in detail below with reference to embodiments, but the present application is not limited to these embodiments.
[0065] Unless otherwise specified, the raw materials in the examples of this application were purchased through commercial channels.
[0066] Example 1
[0067] This embodiment provides a method for preparing pure tributyl aconitate, comprising the following steps:
[0068] (1) 30 g of aconitic acid and 51 g of n-butanol were mixed and stirred to dissolve. After the aconitic acid was completely dissolved, 2.7 g of sodium bisulfate catalyst (purity 99%) was added. The esterification reaction was carried out at 125° C. and 300 rpm for 6 h. The water produced by the esterification was separated in time during the reaction process. After the reaction was completed, a solution containing aconitic acid ester was obtained. An equal volume of alkaline washing solution was added to the solution containing aconitic acid ester for neutralization reaction. After repeating three times, the upper organic phase was taken out. The mass fraction of the solute in the alkaline washing solution was 5%, and the solute was Na 2 CO 3 , the neutralization temperature is 40℃, and the neutralization time is 20min;
[0069] (2) adding 35% hydrogen peroxide (3% by weight of the upper organic phase) to the upper organic phase for one-step decolorization at 30° C. for 15 min, then washing with clean water to remove the hydrogen peroxide, the alkali washing residue, and the salts generated by the alkali washing reaction, separating the liquid and taking the upper layer, and desolventizing at 70° C. and a vacuum degree of 50 mbar until no fraction is distilled out to obtain a crude aconitate;
[0070] (3) Add activated carbon with an iodine value of 810 and a ylan value of 12 to the crude aconitate ester, the weight ratio of activated carbon to the crude aconitate ester being 1:7, and perform two-step decolorization at 30°C for 30 minutes, followed by filtration to obtain a pure tributyl aconitate product. The product appearance is shown in FIG. Figure 2 , liquid phase spectrum see Figure 6 , detection wavelength is 230nm, and specific detection information is shown in Table 1 below, wherein Peak 6 is cis-tributyl aconitate, and Peak 8 is trans-tributyl aconitate. The sum of the two gives a product purity of 99.818%, which is rounded off to 99.8%.
[0071] Table 1
[0072] Characteristic peak Retention time area high Area percentage (%) 1 2.898 1632 367 0.015 2 3.209 3346 582 0.030 3 4.282 2300 288 0.021 4 5.375 4709 673 0.043 5 6.114 1551 228 0.014 6 7.547 125317 14261 1.134 7 9.273 4619 449 0.042 8 11.021 10901651 880085 98.684 9 13.226 1933 130 0.017
[0073] Example 2
[0074] This embodiment provides a method for preparing pure tri(2-ethylhexyl)aconitate, comprising the following steps:
[0075] (1) 30 g of aconitic acid, 112 g of 2-ethylhexanol, and 50 g of toluene with water were mixed and stirred to dissolve. After the aconitic acid was completely dissolved, 15 g of p-toluenesulfonic acid monohydrate catalyst (purity 99%) was added, and the esterification reaction was carried out at 145° C. and 1200 rpm for 8 h. During the reaction process, the water produced by the esterification was separated in time. After the reaction was completed, a solution containing aconitic acid ester was obtained. An equal volume of alkaline washing solution was added to the solution containing aconitic acid ester for neutralization reaction. After repeating three times, the upper organic phase was taken out. The mass fraction of the solute in the alkaline washing solution was 5%, and the solute was Na 2 CO 3, the neutralization temperature is 40℃, and the neutralization time is 20min;
[0076] (2) adding 40% hydrogen peroxide in a concentration of 1% by weight of the upper organic phase to the upper organic phase for one-step decolorization at 50° C. for 20 min, then washing with clean water to remove the hydrogen peroxide, the alkali washing residue and the salts generated by the alkali washing reaction, separating the liquid and taking the upper layer, and desolventizing at 90° C. and a vacuum degree of 10 mbar until no fraction is distilled out to obtain a crude aconitate;
[0077] (3) Add activated carbon with an iodine value of 810 and a ylan value of 12 to the crude aconitate ester, the weight ratio of activated carbon to the crude aconitate ester being 1:9, and perform two-step decolorization at 50° C. for 40 min, followed by filtration to obtain a pure aconitate tri(2-ethylhexyl) ester product.
[0078] Example 3
[0079] This embodiment provides a method for preparing pure triethyl aconitate, comprising the following steps:
[0080] (1) 30 g of aconitic acid, 71.4 g of ethanol, and 50 g of toluene with water were mixed and stirred to dissolve. After the aconitic acid was completely dissolved, 15 g of p-toluenesulfonic acid monohydrate catalyst (purity 99%) was added, and the esterification reaction was carried out at 75° C. and 100 rpm for 2 h. The water produced by the esterification was separated in time during the reaction process. After the reaction was completed, a solution containing aconitic acid ester was obtained. An equal volume of alkaline washing solution was added to the solution containing aconitic acid ester for neutralization reaction. After repeating three times, the upper organic phase was taken out. The mass fraction of the solute in the alkaline washing solution was 25%, the solute was NaOH, the neutralization temperature was 20° C., and the neutralization time was 30 min.
[0081] (2) adding 33% hydrogen peroxide in a concentration of 5% by weight of the upper organic phase to the upper organic phase for decolorization at 70° C. for 30 min, then washing with clean water to remove the hydrogen peroxide, the alkali washing residue and the salts generated by the alkali washing reaction, separating the liquid and taking the upper layer, and desolventizing at 40° C. and a vacuum degree of 100 mbar until no fraction is distilled out to obtain a crude aconitate;
[0082] (3) adding diatomaceous earth with a particle size of 200 mesh to the crude aconitate ester, with the weight ratio of diatomaceous earth to the crude aconitate ester being 1:2, and performing two-step decolorization at 50° C. for 120 min, followed by filtration to obtain a pure aconitate tri(2-ethylhexyl) ester product.
[0083] Example 4
[0084] This embodiment provides a method for preparing a pure aconitic acid mixed ester, comprising the following steps:
[0085] (1) 30 g of aconitic acid, 25.5 g of n-butanol and 22.4 g of 2-ethylhexanol were mixed and stirred to dissolve. After the aconitic acid was completely dissolved, 2.7 g of sodium bisulfate catalyst (purity 99%) was added, and the esterification reaction was carried out at 125° C. and 600 rpm for 6 h. During the reaction process, the water produced by the esterification was separated in time. After the reaction was completed, a solution containing aconitic acid ester was obtained. An equal volume of alkaline washing solution was added to the solution containing aconitic acid ester for neutralization reaction. After repeating three times, the upper organic phase was taken out. The mass fraction of the solute in the alkaline washing solution was 5%, and the solute was NaHCO 3 , the neutralization temperature is 70℃, and the neutralization time is 15min;
[0086] (2) adding 35% hydrogen peroxide (3% by weight of the upper organic phase) to the upper organic phase for decolorization at 30° C. for 15 min, then washing with clean water to remove the hydrogen peroxide, the alkali washing residue and the salts generated by the alkali washing reaction, separating the upper layer, and desolventizing at 100° C. and a vacuum degree of 0.01 mbar until no fraction is distilled out to obtain a crude aconitate;
[0087] (3) adding kaolin with a particle size of 300 mesh to the crude aconitic acid ester, with the weight ratio of kaolin to the crude aconitic acid ester being 1:100, performing two-step decolorization at 30° C. for 10 min, and then filtering to obtain a pure aconitic acid mixed ester product.
[0088] Example 5
[0089] The difference between this embodiment and embodiment 1 is that the concentration of hydrogen peroxide in step (2) is 30%, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0090] Example 6
[0091] The difference between this embodiment and embodiment 1 is that the concentration of hydrogen peroxide in step (2) is 45%, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0092] Example 7
[0093] The difference between this embodiment and embodiment 1 is that the weight of hydrogen peroxide in step (2) accounts for 8% of the weight of the upper organic phase, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0094] Example 8
[0095] The difference between this embodiment and embodiment 1 is that the weight of hydrogen peroxide in step (2) accounts for 0.5% of the weight of the upper organic phase, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0096] Example 9
[0097] The difference between this embodiment and embodiment 1 is that the decolorization temperature of hydrogen peroxide in step (2) is 80° C., and the amounts of other substances and the steps are the same as those in embodiment 1.
[0098] Example 10
[0099] The difference between this embodiment and embodiment 1 is that the decolorization time of hydrogen peroxide in step (2) is 10 minutes, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0100] Embodiment 11
[0101] The difference between this embodiment and embodiment 1 is that the weight ratio of activated carbon to crude aconitate in step (3) is 1:120, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0102] Example 12
[0103] The difference between this embodiment and embodiment 1 is that the decolorization temperature of the activated carbon in step (3) is 80° C., and the amounts of other substances and the steps are the same as those in embodiment 1.
[0104] Embodiment 13
[0105] The difference between this embodiment and embodiment 1 is that the decolorization temperature of the activated carbon in step (3) is 10° C., and the amounts of other substances and the steps are the same as those in embodiment 1.
[0106] Embodiment 14
[0107] The difference between this embodiment and embodiment 1 is that the decolorization time of the activated carbon in step (3) is 5 minutes, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0108] Embodiment 15
[0109] The difference between this embodiment and embodiment 1 is that the iodine value of the activated carbon in step (3) is 700, the Alan value is 10, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0110] Example 16
[0111] The difference between this embodiment and embodiment 1 is that the particle size used in step (3) is 200 mesh and the specific surface area is 90m 2 / g, basic alumina with an average pore size of 15 nm is used to replace the activated carbon, and the amounts of other substances and the steps are the same as those in Example 1.
[0112] Embodiment 17
[0113] The difference between this embodiment and embodiment 1 is that in step (1), the raw materials are esterified at 200° C. and 300 rpm for 6 h, and the amounts of other substances and the steps are the same as those in embodiment 1.
[0114] Embodiment 18
[0115] The difference between this embodiment and embodiment 1 is that the neutralization temperature in step (1) is 80° C., and the amounts of other substances and the steps are the same as those in embodiment 1.
[0116] Comparative Example 1
[0117] This comparative example provides a method for preparing pure tributyl aconitate, comprising the following steps:
[0118] (1) 30 g of aconitic acid and 51 g of n-butanol were mixed and stirred to dissolve. After the aconitic acid was completely dissolved, 2.7 g of sodium bisulfate catalyst (purity 99%) was added. The esterification reaction was carried out at 125° C. and 300 rpm for 6 h. The water produced by the esterification was separated in time during the reaction process. After the reaction was completed, a solution containing aconitic acid ester was obtained. An equal volume of alkaline washing solution was added to the solution containing aconitic acid ester for neutralization reaction. After repeating three times, the upper organic phase was taken out. The mass fraction of the solute in the alkaline washing solution was 5%, and the solute was Na 2 CO 3 , the neutralization temperature is 40℃, and the neutralization time is 20min;
[0119] (2) Desolventizing at 70° C. and a vacuum degree of 50 mbar until no fraction is distilled out to obtain aconitate tributyl ester finished product. The product appearance is shown in FIG. Figure 1 , liquid phase spectrum see Figure 5 , detection wavelength is 230nm, and specific detection information is shown in Table 2 below, wherein peak 16 is cis-tributyl aconitate, and peak 20 is trans-tributyl aconitate. The sum of the two gives a product purity of 93.854%, which is rounded off to 93.9%.
[0120] Table 2
[0121]
[0122]
[0123] Comparative Example 2
[0124] This embodiment provides a method for preparing pure tributyl aconitate, comprising the following steps:
[0125] (1) Same as Example 1;
[0126] (2) adding activated carbon having an iodine value of 810 and a yran value of 12 to the upper organic phase, the weight ratio of the activated carbon to the weight of the upper organic phase being 1:7, and performing a one-step decolorization at 30° C. for 30 min, followed by filtering and washing with clean water to remove the alkali washing residue and the salts generated by the alkali washing reaction, and performing desolventization at 70° C. and a vacuum degree of 50 mbar until no fraction is distilled out to obtain a crude aconitate;
[0127] (3) Add 35% hydrogen peroxide with a concentration of 3% by weight of the crude aconitate to the crude aconitate, perform two-step decolorization at 30° C. for 15 min, then use clean water to remove the hydrogen peroxide, and perform desolventization at 70° C. and a vacuum degree of 50 mbar until no fraction is distilled out to obtain a finished product of tributyl aconitate.
[0128] Comparative Example 3
[0129] This embodiment provides a method for preparing pure tributyl aconitate, comprising the following steps:
[0130] (1) Same as Example 1;
[0131] (2) Add 3% by weight of the upper organic phase and 35% hydrogen peroxide, iodine value of 810, and activated carbon with a yran value of 12 to the upper organic phase, and the weight ratio of activated carbon to the upper organic phase is 1:7. Decolorize at 30° C. for 30 minutes, then filter and wash with clean water to remove hydrogen peroxide, alkali washing residue and salts generated by the alkali washing reaction, and desolventize at 70° C. and a vacuum degree of 50 mbar until no fraction is distilled out to obtain a finished product of tributyl aconitate.
[0132] Comparative Example 4
[0133] (1) 33 g of citric acid and 51 g of n-butanol were mixed and stirred to dissolve. After the citric acid was completely dissolved, 2.7 g of sodium bisulfate catalyst (purity 99%) was added. The esterification reaction was carried out at 125° C. and 300 rpm for 8 h. During the reaction process, the water produced by the esterification was separated in time. After the reaction was completed, a solution containing a citric acid ester was obtained. An equal volume of an alkaline washing solution was added to the solution containing the citric acid ester for neutralization reaction. After repeating three times, the upper organic phase was taken out. The mass fraction of the solute in the alkaline washing solution was 5%, and the solute was Na 2 CO 3 , the neutralization temperature is 40℃, and the neutralization time is 20min;
[0134] (2) Desolventize at 70°C and vacuum degree of 50 mbar until no fraction is distilled out to obtain tributyl citrate finished product. The product appearance is shown in FIG. Figure 3 .
[0135] Comparative Example 5
[0136] The difference between this comparative example and comparative example 4 is that in step (2), hydrogen peroxide accounting for 3% of the weight of the upper organic phase and having a concentration of 35% is added to the upper organic phase, and activated carbon having an iodine value of 810 and a yran value of 12 is added at the same time, and the weight ratio of the activated carbon to the upper organic phase is 1:7. The mixture is decolorized at 30°C for 30 minutes, then filtered, and washed with clean water to remove the hydrogen peroxide, the alkali washing residue and the salts generated by the alkali washing reaction. The mixture is desolventized at 70°C and a vacuum degree of 50 mbar until no fraction is distilled out to obtain a finished product of tributyl citrate. The product appearance is shown in FIG. Figure 4 .
[0137] Test Example 1
[0138] The aconitate and citrate prepared in the above examples and comparative examples were tested for acid value, purity, chromaticity, yield, triester conversion rate and water content. The specific test results are shown in Table 3 below. The test method is as follows:
[0139] 1. Acid value: Take 50mL of ethanol and add 0.25mL of phenolphthalein indicator solution to make two portions for later use. -1 Neutralize with potassium hydroxide aqueous solution until it turns slightly pink, and record the consumed volume V 0 Weigh 1g of the sample (accurate to 0.01g) in a ground-mouth conical flask, then add a portion of the neutralized solution above. After the sample is completely dissolved, add 0.02mol·L -1 Titrate the sample with potassium hydroxide ethanol standard titration solution (titration must be completed within 30 seconds) until a slightly pink color appears and remains unchanged for 5 seconds, which is the end point. Record the consumed volume V.
[0140] Acid value: X = (VV 0 )cM) / m;
[0141] Where: X is the acid value of the sample (in KOH), in milligrams per gram (mg·g -1 ), V is the volume of potassium hydroxide-ethanol standard titration solution consumed by the sample, in milliliters (mL), V 0 is the volume of potassium hydroxide-ethanol standard titration solution consumed in the blank test, in milliliters (mL), c is the exact concentration of potassium hydroxide-ethanol standard titration solution, in moles per liter (mol·L -1 ), m is the mass of the sample in grams (g), M is the molar mass of potassium hydroxide in grams per mole (g·mol -1 )[M=56.11].
[0142] 2. Purity: Use high performance liquid chromatography, and the instrument sensitivity and stability of the detector should comply with the provisions of GB / T16631-2008. Chromatographic column: C18 column; Injector: 10μL micro syringe; Solvent: acetonitrile (HPLC grade); Collection time: 15min; Mobile phase: 80% acetonitrile (HPLC grade), 20% deionized water; Injection volume / : 1μL; Wavelength: 230nm.
[0143] Test: Adjust the instrument as specified above. After the baseline is stable, inject 0.2 μL of sample with a microsyringe. Simultaneously start the integrator or chromatography workstation. The instrument will automatically give the area percentage of each component.
[0144] Purity calculation formula: Purity = (integrated area of aconitate / total integrated area) × 100%.
[0145] 3. Chroma: Preparation of No. 500 platinum-cobalt colorimetric standard stock solution: Weigh 1.2450g potassium chloroplatinate and 1.0000g cobalt chloride to an accuracy of 0.0002g, dissolve in 100mL hydrochloric acid, and then dilute to 1000mL with distilled water. This solution is the No. 500 colorimetric standard colorimetric solution.
[0146] Preparation of colorimetric standards less than No. 500 Take different amounts of No. 500 stock solution and dilute it with distilled water to the volume of the colorimetric tube to prepare colorimetric standards of any number. The calculation formula is as follows:
[0147] V=(N×V 1 ) / 500
[0148] Where: V is the volume of No. 500 standard stock solution used to prepare No. N colorimetric standard solution, mL; V 1 is the volume of the colorimetric tube used, mL; N is the number of the colorimetric standard solution to be prepared.
[0149] After the sample is evenly mixed, it is injected into a colorimetric tube and observed with the naked eye. It should be a transparent oily liquid with no turbidity and no obvious mechanical impurities. The colorimetric determination is carried out at 25°C.
[0150] 4. Yield: The efficiency of the reaction synthesis route is characterized by the yield, and the yield calculation formula is: Yield = (mass of the final product obtained / mass of the theoretically obtained aconitate) × 100%.
[0151] 5. Trisester conversion rate: The characteristic peak of aconitate (about 6.8) was analyzed by NMR spectrum, and the triester conversion rate was calculated as follows: Trisester conversion rate = (integral area of aconitate triester / total area of aconitate and aconitate (monoester, diester, triester) in this area) × 100%.
[0152] 6. Water content: Use Karl Fischer titrator to test the water content (retain to two decimal places).
[0153] 7. Residual amount of fat-soluble pigments and water-soluble pigments:
[0154] High performance liquid chromatography was used, and the instrument sensitivity and stability of the detector should comply with the provisions of GB / T16631-2008. Chromatographic column: C18 column; Injector: 10μL micro-syringe; Solvent: acetonitrile (HPLC grade); Collection time: 15min; Mobile phase: 80% acetonitrile (HPLC grade), 20% deionized water; Injection volume / : 1μL; Wavelength: 230nm.
[0155] Test: Adjust the instrument as specified above. After the baseline is stable, inject 0.2 μL with a micro syringe and start the integrator or chromatographic workstation at the same time. By testing the integrated area of pigments of different concentrations, a standard curve of pigment concentration-integrated area is established. When measuring the pigment content, the instrument automatically gives the corresponding pigment integrated area, and the pigment concentration is obtained by comparing it with the standard curve. The ratio of the pigment concentration to the sample concentration is the pigment content.
[0156] Table 3
[0157]
[0158]
[0159] Combined with the data in Table 3, according to the comparison between Examples 5-8 and Example 1, it can be seen that the concentration and amount of hydrogen peroxide have a great influence on the final chromaticity of the product, and the condition of chromaticity below 50 needs to be achieved within a reasonable range. It is analyzed that excessive concentration or amount of hydrogen peroxide will increase the chromaticity of the product, and more hydrogen peroxide participates in the hydrolysis of aconitate, which reduces the yield although the reaction rate is very slow. Low amount or concentration of hydrogen peroxide will cause incomplete bleaching of the product pigment, and the pigment does not meet the requirements.
[0160] According to the comparison between Examples 9-10 and Example 1, the higher the decolorization temperature of hydrogen peroxide, the more hydrogen peroxide will decompose, and the oxidation effect on fat-soluble pigments will be poor, so that the residual amount of fat-soluble pigments increases, and then the chroma of aconitate increases and the purity decreases, and at the same time, the hydrolysis of aconitate by hydrogen peroxide is promoted, so that the yield of aconitate decreases; the decolorization time of hydrogen peroxide is shortened, which affects the destructive effect of hydrogen peroxide on the main structure of fat-soluble pigments, and then the chroma of aconitate increases and the purity decreases.
[0161] According to the comparison between Example 11 and Example 1, when the amount of activated carbon used is reduced, the adsorption amount of water-soluble pigments decreases, so the residual amount of water-soluble pigments increases, causing the chromaticity of aconitate to increase and the purity to decrease.
[0162] According to the comparison between Examples 12-13 and Example 1, the decolorization temperature of the decolorizing agent affects the decolorization effect on the water-soluble pigment. The higher the temperature, the more violent the Brownian motion of the molecules, and the more difficult it is for the decolorizing agent to adsorb the pigment, which leads to a decrease in the removal rate of water-soluble pigment impurities. The lower the temperature, the lower the adsorption capacity of the decolorizing agent for the water-soluble pigment. In addition, the high viscosity of aconitate is not conducive to the uniform dispersion of the decolorizing agent, which also leads to a decrease in the removal rate of the water-soluble pigment, and then the purity of aconitate decreases and the chromaticity increases.
[0163] According to the comparison between Example 14 and Example 1, the shorter the decolorization time of the decolorizing agent, the worse the decolorization effect on the water-soluble pigment, so that the chromaticity of aconitate increases and the purity decreases.
[0164] According to the comparison between Examples 15-16 and Example 1, it can be seen that the type of decolorizing agent and the parameters of activated carbon will affect the removal effect of water-soluble pigments, thereby affecting the purity and chromaticity of the aconitate product.
[0165] According to the comparison between Example 17 and Example 1, the increase in esterification temperature causes the polysaccharide to undergo a caramelization reaction. Under the same decolorization conditions, the contents of both types of pigments in the final aconitate ester increase, the product pigment increases and the purity decreases; and the monosaccharides produced by the decomposition of the polysaccharide will compete with the alcohols and the esterification reaction of aconitate, resulting in a decrease in the yield of aconitate ester and the triester conversion rate.
[0166] According to the comparison between Example 18 and Example 1, the increase in neutralization temperature will cause the product to be hydrolyzed in an alkaline environment, so that the purity of the obtained product is insufficient. The reduction in purity increases the relative content of pigment in the product, thereby affecting the one-step decolorization and two-step decolorization processes, resulting in an increase in the residual amount of fat-soluble pigments and water-soluble pigments, an increase in the chroma of aconitate and a decrease in purity, and the loss due to high-temperature hydrolysis leads to a decrease in the yield of aconitate.
[0167] According to the comparison between Comparative Examples 1-3 and Example 1, the aconitate obtained without decolorization treatment has a high content of water-soluble pigments and fat-soluble pigments, the chroma of the product is greater than 500, and the purity decreases. When the water-soluble pigment is removed first and then the fat-soluble pigment is removed or the two types of pigments are removed simultaneously, not only the preparation treatment process will be increased, but also the removal effect of the two types of pigments will be affected, resulting in an increase in the chroma of the aconitate and a decrease in purity. When the fat-soluble pigment and the water-soluble pigment are removed at the same time, the activated carbon will agglomerate in the aqueous phase and be distributed in the organic phase. The decolorization effect of the two pigments of the product is poor, and the yield will decrease due to the agglomeration of the activated carbon.
[0168] according to Figure 1-4From the comparison with Comparative Examples 4 and 5, it can be seen that the pigment content of citrate itself is low, so it is easy to decolorize, and it is not as difficult to decolorize as aconitate. Although the chromaticity is reduced before and after bleaching, the decrease in chromaticity after bleaching is much smaller than that of the present application.
[0169] Test Example 2
[0170] The aconitate and tributyl citrate prepared in the above embodiments and comparative examples are added as plasticizers to PVC resin to obtain PVC plastic, which includes 100 parts of PVC resin, 35 parts of plasticizer, 2 parts of oxidized polyethylene wax, and 5 parts of octyltin maleate. The above raw materials are mixed and prepared by the same mixing process to obtain a PVC finished product. The different plasticizers in the above embodiments and comparative examples and the obtained PVC finished products are tested for performance. The results are shown in Table 4 below. The test method is as follows:
[0171] 1. Hardness: According to GB / T531-2008 "Indentation hardness test method, Shore hardness tester method" standard, make specimens and test them. Select 3 points for each group of specimens, measure each point once, and take the median value.
[0172] 2.100% tensile stress, elongation at break, elastic modulus: in accordance with GB / T1040-2006 "Plastic Tensile Properties Test", the stretching speed is 50mm / min, the temperature is 25℃.
[0173] 3. Compatibility: The water price method is used for testing. Since water molecules are polar, the compatibility of plasticizers with water can characterize the compatibility of plasticizers with polar materials (PVC, PLA and nitrile rubber). When a certain plasticizer has good compatibility with water, it has good compatibility with PVC, and vice versa. In the experiment, 2.5g of plasticizer and 25g of acetone were added to a beaker, and titrated with a burette filled with deionized water, stirring while titrating until turbidity appeared, and the volume of deionized water consumed was recorded.
[0174] 4. Glass transition temperature (T g ): The glass transition temperature was tested by a dynamic mechanical analyzer. The test conditions were: nitrogen as the carrier gas, the test temperature range was -40-80°C, the heating rate was 3°C / min, and the frequency was 1 Hz.
[0175] Table 4
[0176]
[0177]
[0178] According to the contents of Table 4, the purity of aconitate has a great influence on the performance of aconitate as a plasticizer. The lower the purity of aconitate, the lower the hardness and T g, the higher the 100% tensile stress and elastic modulus, the worse the elongation at break and compatibility. Especially in the comparison before and after bleaching, the hardness lost 12% and the toughness lost more than 14%. Therefore, bleaching can not only improve the color quality of the product itself, but its purification effect after bleaching can also improve the plasticizing performance of aconitate on PVC.
[0179] The above is only the embodiment of the present application, and the protection scope of the present application is not limited by these specific embodiments, but is determined by the claims of the present application. For those skilled in the art, the present application can have various changes and variations. Any modification, equivalent replacement, improvement, etc. made within the technical ideas and principles of the present application should be included in the protection scope of the present application.
Claims
1. A method for preparing high-purity aconitate, characterized in that: The steps include: (1) reacting aconitic acid obtained by fermentation with alcohol to obtain a solution containing aconitic acid ester, neutralizing the solution containing aconitic acid ester and separating the solution to obtain an upper organic phase; (2) adding hydrogen peroxide to the upper organic phase for one-step decolorization, followed by washing, separation, and desolventization to obtain a crude aconitate product; (3) adding a decolorizing agent to the crude aconitate ester to perform a two-step decolorization, and then filtering to obtain aconitate ester with high purity; The decolorizing agent is selected from at least one of activated carbon, diatomaceous earth, kaolin, basic alumina, and neutral alumina.
2. The preparation method according to claim 1, characterized in that: The concentration of the hydrogen peroxide is 33-40%, and the weight of the hydrogen peroxide accounts for 1-5% of the weight of the upper organic phase.
3. The preparation method according to claim 1, characterized in that: The temperature of the hydrogen peroxide for one-step decolorization is 20-70° C. and the time is 15-30 minutes.
4. The preparation method according to claim 1, characterized in that: The weight ratio of the decolorizing agent to the crude aconitate is 1:(2-100).
5. The preparation method according to claim 1, characterized in that: The temperature of the decolorizing agent for the second step decolorization is 20-70°C and the time is 10-120 minutes.
6. The preparation method according to claim 1, characterized in that: The iodine value of the activated carbon is greater than 800, and the Yran value is greater than 10; The particle size of the diatomaceous earth is 200-300 mesh; The particle size of the kaolin is 200-300 mesh; The particle size of the basic alumina and the neutral alumina is 100-200 mesh, and the specific surface area is 60-90m 2 / g, average pore size 10-20nm; Preferably, the decolorizing agent is selected from activated carbon.
7. The preparation method according to claim 1, characterized in that: The temperature for the reaction of the aconitic acid obtained by fermentation and the alcohol is 75-145° C., and the reaction time is 2-8 hours.
8. The preparation method according to claim 1, characterized in that: The purity of the high-purity aconitate is not less than 99%.
9. The preparation method according to claim 1, characterized in that: The chromaticity of the high-purity aconitate is no higher than 50Pt-Co.
10. The preparation method according to claim 1, characterized in that: The content of fat-soluble pigment in the high-purity aconitate is lower than 1000 ppm, and the content of water-soluble pigment is lower than 1000 ppm.
Citation Information
Patent Citations
Recombinant aspergillus terreus strain capable of producing trans-aconitic acid at high yield as well as construction method and application thereof
CN112011469A
Aconitate polyvinyl chloride plasticizer, and preparation method and application thereof
CN113817223A
Bio-based trans-aconitate, preparation method therefor and use thereof
WO2024235233A1
Cited By
Bio-based trans-aconitate, preparation method therefor and use thereof
EP4715056A1
Bio-based trans-aconitate, preparation method therefor and use thereof
WO2024235233A1