Built-in polaroid and preparation method thereof
By incorporating a hemispherical protective bump and a silicone pressure-sensitive adhesive layer on the polarizer, the problem of peeling and poor performance during the bending process is solved, and higher bending and impact resistance is achieved.
Patent Information
- Application Number
- CN202411013284.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing polarizers have poor performance during bending, which is prone to peeling from other film layers, resulting in poor bending performance.
Adopt a built-in polarizer design, including a polarizing film layer and a protective film layer. The protective film layer is composed of multiple hemispherical protective bumps, which are attached to the surface of the polarizing film layer to improve adhesion stability and bending resistance, and through The silicone pressure-sensitive adhesive layer achieves uniform heat absorption and heat exothermic.
The bending resistance and impact resistance of the polarizer are improved, the impact of bending stress and temperature on the polarizer is reduced, and the overall performance is enhanced.
Smart Images

Figure CN119001944A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of polarizers, and in particular to a built-in polarizer and a preparation method thereof. Background Art
[0002] Polarizer is an optical element used to control and filter light waves in a specific direction. Polarizers do this by absorbing or converting the vibration direction of light; polarizers take advantage of the vibration direction of light waves, which propagate in space in the form of waves. The vibration direction of these waves can be in different planes, perpendicular or parallel to the propagation direction of light. Polarizers are designed to allow light in a specific direction to pass through, while absorbing or converting light in other directions.
[0003] In daily life, polarizers are often used in sunglasses, which can reduce the sunlight reflected from different directions, reduce glare and provide a clearer view. Camera lenses also often use polarizers to eliminate or reduce reflections, enhance color saturation and provide clear images. In scientific research and industrial applications, polarizers are used in microscopes, laser technology, LCD screens and other optical devices to adjust the properties and direction of light. In laboratory settings, polarizers are also used to analyze and study the properties of light, such as studying the polarization state of light and the optical properties of materials. In general, polarizers are an important optical component that can play an important role in a variety of fields, from daily necessities to advanced scientific and industrial applications.
[0004] The existing polarizer has a defect of poor bending performance due to its low bending performance, which causes the polarizer to peel off from other film layers during the bending process. Summary of the invention
[0005] In order to solve the defect of poor bending performance of polarizers, the present application provides a built-in polarizer and a preparation method.
[0006] In the first aspect, the present application provides a built-in polarizer, adopting the following technical scheme: including: a polarizing film layer, used to control and filter light waves in a specific direction; a protective film layer, attached to the surface of the polarizing film layer, used to protect the polarizing film layer; the protective film layer includes an attachment layer and a protective layer; the protective layer is composed of a plurality of protective protrusions arranged in sequence; the protective protrusion is hemispherical, and the plane of the protective protrusion is attached to the same side of the attachment layer.
[0007] By adopting the above technical solution, after the polarizer is bonded to other film layers, the provision of the protective protrusion increases the stability of the polarizer and the film layer after bonding, reduces the occurrence of peeling between the polarizer and other film layers, and thereby improves the bending resistance of the polarizer; at the same time, when the polarizer is bent, since the protective protrusion is hemispherical, when the polarizer is bent in different directions, the bending stress on the protective film layer is reduced, thereby improving the integrity of the polarizer when bent; thereby achieving the effect of improving the bending performance of the polarizer.
[0008] Preferably, the attachment layer and the protective layer are each provided with two layers; the two layers of the protective layers are located between the two layers of the attachment layers; the line connecting the center points of the planes of adjacent protective bumps vertically or horizontally along the same protective layer is a straight line; and the lines connecting the centers of adjacent rows or columns are parallel; adjacent protective bumps abut against each other; the protective bumps of the upper and lower protective layers are staggered in two columns along the length direction of the protective layers; or the protective bumps of the upper and lower protective layers are staggered in two rows along the width direction of the protective layers; the protective bumps of the two protective layers abut against each other.
[0009] By adopting the above technical scheme, when the polarizer is bent during use, the distance between adjacent protective protrusions in the lower layer gradually decreases, and the protective layer located above is squeezed under the guiding action of the protective protrusions; thereby reducing the bending stress concentration and improving the bending performance of the polarizer; the protective layer composed of protective protrusions neatly and evenly arranged vertically or horizontally along the same protective layer, when the upper and lower protective layers are bonded, if the two rows of protective protrusions in the width direction of the attachment layer are staggered, then the adjacent protective protrusions between the two protective layers in the length direction of the attachment layer are not overlapped and staggered, so that the deformability of the protective film layer arranged in this way is larger, which increases the upper limit of breakage when the polarizer is bent, thereby achieving the effect of improving the bending performance of the polarizer.
[0010] Preferably, the attachment layer and the protective layer are each provided with two layers; the two layers of the protective layers are located between the two layers of the attachment layers; the line connecting the center points of the planes of adjacent protective bumps vertically or horizontally along the same protective layer is a straight line, and the lines connecting the centers of adjacent rows or columns are parallel, and adjacent protective bumps are abutted; one of the protective bumps of the upper protective layer is located between two adjacent rows and two adjacent columns of protective bumps of the lower protective layer; or one of the protective bumps of the lower protective layer is located between two adjacent rows and two adjacent columns of protective bumps of the upper protective layer; the protective bumps of the two protective layers are abutted.
[0011] By adopting the above technical solution, when the polarizer is used and is subjected to an impact force perpendicular to the polarizer, since one of the protective protrusions on the upper layer is located between four adjacent protective protrusions on the lower layer, when the polarizer is impacted, the protective protrusions on the lower layer absorb and transmit external pressure, thereby improving the compressive resistance of the polarizer; and since the protective protrusions are evenly distributed along the width and length directions of the attachment layer, all parts of the polarizer have good impact resistance.
[0012] Preferably, an adhesive layer is filled between the two protective layers.
[0013] Preferably, the adhesive layer is made of organic silicon pressure-sensitive adhesive as raw material.
[0014] By adopting the above technical scheme, the adhesive layer made of silicone pressure-sensitive adhesive as raw material can not only bond the upper and lower protective layers, but also the heat generated during the use of the equipment is first transferred to the protective protrusion before being transferred to the polarizing film layer. The protective protrusion transfers the heat to the adhesive layer and diffuses it to the entire protective layer under the action of the adhesive layer; at the same time, after the polarizing film layer absorbs the heat, it transfers the heat to the protective protrusion, and then quickly diffuses it again under the action of the adhesive layer; thereby achieving uniform heat absorption and heat release of the polarizer, reducing the influence of temperature on the polarizer; at the same time, the hemispherical protective protrusion has a large contact area with the adhesive layer, thereby achieving rapid heat transfer.
[0015] Preferably, the protective film layer is attached to both surfaces of the polarizing film layer, and any one of the attachment layers is attached to the polarizing film layer.
[0016] By adopting the above technical solution, the protective film layers are pasted on both sides to improve the bending resistance and impact resistance of the polarizer, while also improving the heat dissipation performance of the polarizer, thereby improving the integrity of the polarizer.
[0017] In a second aspect, the present application provides a method for preparing a built-in polarizer, which adopts the following technical solution: The method for preparing a built-in polarizer comprises the following steps: S1, preparation of polarizing film layer; S2, preparation of the protective film layer, forming a plurality of protective bumps on the same surface of the attachment layer to form a protective layer; the line connecting the centers of the planes of adjacent protective bumps vertically or horizontally along the same protective layer is a straight line; the lines connecting the centers of adjacent rows or columns are parallel; and adjacent protective bumps are in contact; S3. The protective film layer is bonded to the polarizing film layer.
[0018] Preferably, in step S2, the protective protrusions of the upper and lower protective layers are staggered in two columns along the length direction of the protective layer; or the protective protrusions of the upper and lower protective layers are staggered in two rows along the width direction of the protective layer; the protective protrusions of the two protective layers are abutted.
[0019] Preferably, in step S2, one of the protective bumps of the upper protective layer is located between two adjacent rows and two adjacent columns of protective bumps of the lower protective layer; or one of the protective bumps of the lower protective layer is located between two adjacent rows and two adjacent columns of protective bumps of the upper protective layer; the protective bumps of the two protective layers are abutted.
[0020] In summary, the present application includes at least one of the following beneficial technical effects: 1. After the polarizer is laminated with other film layers, the provision of the protective convex block increases the stability of the polarizer and the film layer after lamination, reduces the occurrence of peeling between the polarizer and other film layers, and thus improves the bending resistance of the polarizer; at the same time, when the polarizer is bent, since the protective convex block is hemispherical, when the polarizer is bent in different directions, the bending stress on the protective film layer is reduced, thereby improving the integrity of the polarizer when bent; thus achieving the effect of improving the bending performance of the polarizer; 2. When the polarizer is used, when it is subjected to an impact force perpendicular to the polarizer, since one of the protective bumps on the upper layer is located between the four adjacent protective bumps on the lower layer, when the polarizer is impacted, the protective bumps on the lower layer absorb and transmit the external pressure, thereby improving the compressive resistance of the polarizer; and since the protective bumps are evenly distributed along the width and length directions of the attachment layer, all parts of the polarizer have good impact resistance; 3. The adhesive layer made of silicone pressure-sensitive adhesive can not only bond the upper and lower protective layers, but also transfer the heat generated during the use of the equipment to the protective bumps before transferring to the polarizing film layer. The protective bumps transfer the heat to the adhesive layer and diffuse it to the entire protective layer under the action of the adhesive layer. At the same time, after the polarizing film layer absorbs the heat, it transfers the heat to the protective bumps, and then diffuses it rapidly again under the action of the adhesive layer. This achieves uniform heat absorption and heat release of the polarizer and reduces the influence of temperature on the polarizer. At the same time, the hemispherical protective bumps have a large contact area with the adhesive layer, which enables rapid heat transfer. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic diagram of the overall structure of Example 1 of the present application; Figure 2 yes Figure 1 A partial enlarged schematic diagram of part A; Figure 3 is a schematic diagram showing a protective film layer in Example 1 of the present application; Figure 4 is a cross-sectional view showing the adhesive layer of Example 1 of the present application; Figure 5 It is a schematic diagram of the overall structure of Example 2 of the present application; Figure 6 yes Figure 5 A partial enlarged schematic diagram of part B.
[0022] In the figure, 1, polarizing film layer; 2, protective film layer; 21, attachment layer; 22, protective layer; 221, protective bump; 3, adhesive layer. DETAILED DESCRIPTION
[0023] The following is combined with Figure 1-Figure 6 This application is described in further detail.
[0024] The embodiments of the present application disclose a built-in polarizer and a preparation method thereof.
[0025] Example 1 refer to Figure 1 and Figure 2 A built-in polarizer includes: a polarizing film layer 1 and a protective film layer 2; the polarizing film layer 1 is used to control and filter light waves in a specific direction; the protective film layer 2 is attached to the surface of the polarizing film layer 1 and is used to protect the polarizing film layer 1; specifically, the protective film layer 2 includes an attachment layer 21 and a protective layer 22; the protective layer 22 is composed of a plurality of sequentially arranged protective bumps 221, the protective bumps 221 are hemispherical, and the plane of the protective bumps 221 is attached to the same side of the attachment layer 21.
[0026] refer to Figure 3 and Figure 4 , the attachment layer 21 and the protective layer 22 are both provided with two layers, and the two protective layers 22 are located between the two attachment layers 21; the built-in polarizer also includes an adhesive layer 3, which is filled and adhered between the two protective layers 22 of the same protective film layer 2, and is used to adhere the two protective layers 22; in this application, the adhesive layer 3 is made of organic silicon pressure-sensitive adhesive as a raw material, and the organic silicon pressure-sensitive adhesive is flexible and has good thermal conductivity. The protective film layer 2 is attached to the two surfaces of the polarizing film layer 1, and any one of the attachment layers 21 is attached to the polarizing film layer 1.
[0027] refer to Figure 1 and Figure 2 , the line connecting the centers of the planes of adjacent protective protrusions 221 vertically or horizontally along the same protective layer 22 is a straight line; the lines connecting the centers of adjacent rows or columns are parallel; adjacent protective protrusions 221 abut against each other; the protective protrusions 221 of the upper and lower protective layers 22 are staggered in two rows of protective protrusions 221 along the length direction of the protective layer 22; or the protective protrusions 221 of the upper and lower protective layers 22 are staggered in two rows of protective protrusions 221 along the width direction of the protective layer 22; the protective protrusions 221 of the two protective layers 22 abut against each other. That is, one of the protective protrusions 221 on the upper layer is located between two protective protrusions 221 on the lower layer.
[0028] When in use, after the polarizer is bonded to other film layers, the provision of the protective protrusions 221 increases the stability of the polarizer and the film layer after bonding, reduces the occurrence of peeling between the polarizer and other film layers, and thus improves the bending resistance of the polarizer; at the same time, when the polarizer is bent, since the protective protrusions 221 are hemispherical, the bending stress on the protective film layer 2 is reduced when the polarizer is bent in different directions. The protective layer 22 composed of protective protrusions 221 neatly and evenly arranged vertically or horizontally along the same protective layer 22, when the upper and lower protective layers 22 are bonded, if the two rows of protective protrusions 221 in the width direction of the attached layer 21 are staggered, then the adjacent protective protrusions 221 between the two protective layers 22 in the length direction of the attached layer 21 are not overlapped and staggered, so that the deformability of the protective film layer 2 arranged in this way is larger, which increases the upper limit of the breakage of the polarizer when it is bent, and achieves the effect of improving the bending performance of the polarizer.
[0029] At the same time, the adhesive layer 3 made of silicone pressure-sensitive adhesive can bond the upper and lower protective layers 22. At the same time, before the heat generated during the use of the equipment is transferred to the polarizing film layer 1, it is first transferred to the protective protrusion 221. The protective protrusion 221 transfers the heat to the adhesive layer 3 and diffuses it to the entire protective layer 22 under the action of the adhesive layer 3; when the polarizing film layer 1 absorbs the heat, the heat is transferred to the protective protrusion 221, and the heat is quickly diffused again under the action of the adhesive layer 3; thereby achieving uniform heat absorption and heat release of the polarizer and reducing the influence of temperature on the polarizer; at the same time, the hemispherical protective protrusion 221 has a large contact area with the adhesive layer 3, thereby achieving rapid heat transfer.
[0030] The implementation principle of a built-in polarizer in Example 1 of the present application is: when the polarizer is bent, since the protective protrusion 221 is hemispherical, the bending stress on the protective film layer 2 is reduced when the polarizer is bent in different directions, thereby improving the integrity of the polarizer when bent; achieving the effect of improving the bending performance of the polarizer.
[0031] Example 1 of the present application also discloses a method for preparing a built-in polarizer.
[0032] The following steps are involved: S1, preparation of polarizing film layer 1; S2, preparing the protective film layer 2, forming a plurality of protective bumps 221 on the same surface of the attachment layer 21 to form a protective layer 22; the line connecting the center points of the planes of adjacent protective bumps 221 vertically or horizontally along the same protective layer 22 is a straight line; the lines connecting the centers of adjacent rows or columns are parallel; and adjacent protective bumps 221 are in contact with each other; The protective bumps 221 of the upper and lower protective layers 22 are staggered in two rows of protective bumps 221 along the length direction of the protective layer 22; or the protective bumps 221 of the upper and lower protective layers 22 are staggered in two rows of protective bumps 221 along the width direction of the protective layer 22; the protective bumps 221 of the two protective layers 22 are abutted; S3, the protective film layer 2 is bonded to the polarizing film layer 1.
[0033] Example 2 refer to Figure 5 and Figure 6 The difference between this embodiment 2 and embodiment 1 is that: one of the protective bumps 221 of the upper protective layer 22 is located between two adjacent rows and two adjacent columns of protective bumps 221 of the lower protective layer 22; or one of the protective bumps 221 of the lower protective layer 22 is located between two adjacent rows and two adjacent columns of protective bumps 221 of the upper protective layer 22; the protective bumps 221 of the two layers of protective layers 22 are abutted.
[0034] During use, when the polarizer is subjected to an impact force perpendicular to the polarizer, since one of the protective protrusions 221 of the upper layer is located between four adjacent protective protrusions 221 of the lower layer; when the polarizer is impacted, the protective protrusions 221 of the lower layer absorb and transmit the external pressure, thereby improving the compressive resistance of the polarizer; and since the protective protrusions 221 are evenly distributed along the width and length directions of the attachment layer 21, all parts of the polarizer have good impact resistance.
[0035] The implementation principle of a built-in polarizer in Example 2 of the present application is as follows: since one of the protective bumps 221 of the upper layer is located between four adjacent protective bumps 221 of the lower layer; when the polarizer is impacted, the protective bumps 221 of the lower layer absorb and transmit external pressure, thereby improving the pressure resistance of the polarizer.
[0036] Example 2 of the present application also discloses a method for preparing a built-in polarizer.
[0037] The following steps are involved: S1, preparation of polarizing film layer 1; S2, preparing the protective film layer 2, forming a plurality of protective bumps 221 on the same surface of the attachment layer 21 to form a protective layer 22; the line connecting the center points of the planes of adjacent protective bumps 221 vertically or horizontally along the same protective layer 22 is a straight line; the lines connecting the centers of adjacent rows or columns are parallel; and adjacent protective bumps 221 are in contact with each other; One of the protective bumps 221 of the upper protective layer 22 is located between two adjacent rows and two adjacent columns of protective bumps 221 of the lower protective layer 22; or one of the protective bumps 221 of the lower protective layer 22 is located between two adjacent rows and two adjacent columns of protective bumps 221 of the upper protective layer 22; the protective bumps 221 of the two protective layers 22 are in contact with each other; S3, the protective film layer 2 is bonded to the polarizing film layer 1.
[0038] The embodiments of this specific implementation method are all preferred embodiments of the present application, and are not intended to limit the protection scope of the present application. Therefore, all equivalent changes made based on the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A built-in polarizer, Features: include: A polarizing film layer (1), used to control and filter light waves in a specific direction; The protective film layer (2) is attached to the surface of the polarizing film layer (1) and is used to protect the polarizing film layer (1); the protective film layer (2) comprises an attachment layer (21) and a protective layer (22); the protective layer (22) is composed of a plurality of sequentially arranged protective bumps (221); the protective bumps (221) are hemispherical, and the planes of the protective bumps (221) are attached to the same side of the attachment layer (21).
2. The built-in polarizer according to claim 1, Features: The attachment layer (21) and the protective layer (22) are both provided with two layers; the two layers of the protective layer (22) are located between the two layers of the attachment layer (21); A line connecting the center points of the planes of adjacent protective convex blocks (221) in the vertical or horizontal direction along the same protective layer (22) is a straight line; and lines connecting the centers of adjacent rows or columns are parallel; and adjacent protective convex blocks (221) are in contact with each other; The protective protrusions (221) of the upper and lower protective layers (22) are staggeredly distributed in two rows of protective protrusions (221) along the length direction of the protective layer (22); or the protective protrusions (221) of the upper and lower protective layers (22) are staggeredly distributed in two rows of protective protrusions (221) along the width direction of the protective layer (22); the protective protrusions (221) of the two layers of protective layers (22) are abutted.
3. The built-in polarizer according to claim 1, Features: The attachment layer (21) and the protective layer (22) are both provided with two layers; the two layers of the protective layer (22) are located between the two layers of the attachment layer (21); A line connecting the center points of adjacent protective protrusions (221) in the vertical or horizontal direction along the same protective layer (22) is a straight line, and a line connecting the centers of adjacent rows or columns is parallel, and adjacent protective protrusions (221) are in contact with each other; One of the protective bumps (221) of the upper protective layer (22) is located between two adjacent rows and two adjacent columns of protective bumps (221) of the lower protective layer (22); or one of the protective bumps (221) of the lower protective layer (22) is located between two adjacent rows and two adjacent columns of protective bumps (221) of the upper protective layer (22); the protective bumps (221) of the two protective layers (22) are in abutment with each other.
4. A built-in polarizer according to any one of claims 2 or 3, Features: An adhesive layer (3) is filled between the two protective layers (22).
5. The built-in polarizer according to claim 4, Features: The adhesive layer (3) is made of organic silicon pressure-sensitive adhesive as raw material.
6. The built-in polarizer according to claim 4, Features: The protective film layer (2) is adhered to the two surfaces of the polarizing film layer (1), and any one of the attachment layers (21) is adhered to the polarizing film layer (1).
7. A method for preparing a built-in polarizer, Features: The following steps are involved: S1, preparing a polarizing film layer (1); S2, preparing a protective film layer (2), forming a plurality of protective bumps (221) on the same surface of an attachment layer (21) to form a protective layer (22); a line connecting the center points of adjacent protective bumps (221) in the vertical or horizontal direction along the same protective layer (22) is a straight line; and lines connecting the centers of adjacent rows or columns are parallel; and adjacent protective bumps (221) are in contact with each other; S3. The protective film layer (2) is bonded to the polarizing film layer (1).
8. The method for preparing a built-in polarizer according to claim 7, It is characterized in that In step S2, the protective protrusions (221) of the upper and lower protective layers (22) are arranged in two rows of protective protrusions (221) in a staggered manner along the length direction of the protective layer (22); or the protective protrusions (221) of the upper and lower protective layers (22) are arranged in two rows of protective protrusions (221) in a staggered manner along the width direction of the protective layer (22); and the protective protrusions (221) of the two layers of the protective layers (22) are abutted.
9. The method for preparing a built-in polarizer according to claim 7, It is characterized in that In step S2, one of the protective bumps (221) of the upper protective layer (22) is located between two adjacent rows and two adjacent columns of protective bumps (221) of the lower protective layer (22); or one of the protective bumps (221) of the lower protective layer (22) is located between two adjacent rows and two adjacent columns of protective bumps (221) of the upper protective layer (22); the protective bumps (221) of the two protective layers (22) are abutted.