HEMT device and preparation method thereof

By introducing a strain compensation layer and a barrier compensation layer in the HEMT device, adjusting the two-dimensional electron air density and electric field distribution in the channel area, the problems of large on-resistance, current collapse and thermal electron effects are solved, and reliability is improved and breakdown voltage.

CN119008680APending Publication Date: 2024-11-22CHINA RESOURCES MICROELECTRONICS (CHONGQING) CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202310559908.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-17
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing AlGaN/(Al)GaN high electron mobility transistor (HEMT) devices have large on-resistance, current collapse effect and thermal electron effect, resulting in poor reliability and low breakdown voltage.

Method used

A first strain compensation layer and a second strain compensation layer are introduced into the HEMT device, and a barrier compensation layer is formed on the barrier layer to adjust the two-dimensional electron air density in the channel area, uniform electric field distribution, and increase the breakdown voltage.

Benefits of technology

It effectively reduces the on-resistance of the device, alleviates current collapse and thermal electronic effects, and improves the reliability and performance of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008680A_ABST
    Figure CN119008680A_ABST
Patent Text Reader

Abstract

The invention provides an HEMT device and a preparation method thereof, the HEMT device comprises a semiconductor structure, a gate structure, a source electrode, a drain electrode, a first strain compensation layer, a second strain compensation layer and a barrier compensation layer, the semiconductor structure comprises a substrate, a buffer layer, a channel layer and a barrier layer; the gate structure comprises a cap layer located on the upper surface of the barrier layer; the source electrode is electrically connected with the barrier layer; the drain is electrically connected with the barrier layer on one side of the gate structure away from the source; the first strain compensation layer is located on the upper surface of the barrier layer between the gate structure and the source electrode and is adjacent to the cap layer; the second strain compensation layer is located on the upper surface of the barrier layer between the gate structure and the drain and is spaced from the cap layer by a preset distance; the barrier compensation layer covers an exposed surface of the barrier layer between the gate structure and the second strain compensation layer. Through the arrangement of the first strain compensation layer, the second strain compensation layer and the barrier compensation layer, the current collapse effect and the hot electron effect at the drain electrode are relieved, and the on resistance of the device is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of semiconductor integrated circuit manufacturing and relates to a HEMT device and a preparation method thereof. Background Art

[0002] Gallium nitride (GaN), as a typical representative of the third generation wide bandgap semiconductor materials, has the advantages of large bandgap width, high breakdown electric field, and high electron saturation drift velocity. In addition, gallium nitride materials have the characteristics of high temperature resistance and corrosion resistance, so gallium nitride devices are widely used in high temperature, high voltage, high frequency, and high power electronic systems. For AlGaN / (Al)GaN high electron mobility transistor (HEMT) devices, breakdown voltage is its key performance parameter, but the breakdown voltage of power devices produced by the current structure and process is still far from the theoretical limit that GaN materials can reach, such as Figure 1 and Figure 2 As shown, there are schematic cross-sectional structures of a HEMT device and another HEMT device, respectively, including a semiconductor structure 01, a substrate 011, a buffer layer 012, a channel layer 013, a barrier layer 014, a gate structure 02, a cap layer 021, a gate 022, a source 03, a drain 04 and a passivation layer 05, wherein the source and the drain form ohmic contacts with the barrier layer respectively, the gate forms a Schottky contact with the barrier layer, or the gate forms an ohmic contact with the cap layer (P-GaN gate), and a PN junction is formed between the cap layer and the barrier layer. The source and the drain form ohmic contacts with the barrier layer to reduce the contact resistance, and a passivation layer is grown on the barrier layer between the source and the drain to suppress the current collapse effect.

[0003] At present, due to the existence of the current collapse effect, when the device is in the on state, after the drain voltage of the device exceeds a certain value, as the drain voltage increases, the source-drain current begins to decrease, the on-resistance of the device increases, and the current is lower than the ideal value. When the device is working in the off state, the electric field below the edge of the metal gate is relatively concentrated. When the electric field value exceeds the critical breakdown voltage of the material, the carriers in the channel are driven by the high electric field and are continuously accelerated and collision ionized. The current density below the edge of the metal gate continues to increase, and finally the device breaks down prematurely. In addition, gallium nitride devices also have the problem of hot electrons. When the device works at a large drain bias, the hot electrons generated by the channel electric field, especially the electric field peak on the drain side of the gate, will emit phonons to heat the lattice, reduce the carrier mobility of the device, and the saturated drain current will decrease with the increase of the drain voltage, which will affect the reliability of the device.

[0004] Therefore, there is an urgent need to find a HEMT device that reduces the on-resistance of the device and improves the device reliability and breakdown voltage. Summary of the invention

[0005] In view of the above-mentioned shortcomings of the prior art, the object of the present invention is to provide a HEMT device and a preparation method thereof, so as to solve the problems of large on-resistance of the HEMT device in the prior art and poor reliability and low breakdown voltage of the device caused by current collapse effect and hot electron effect.

[0006] To achieve the above-mentioned object and other related objects, the present invention provides a HEMT device, comprising:

[0007] A semiconductor structure comprising a substrate, a buffer layer, a channel layer and a barrier layer stacked in sequence;

[0008] A gate structure, comprising a cap layer located on an upper surface of the barrier layer and electrically connected to the barrier layer;

[0009] A source electrode, electrically connected to the barrier layer, wherein the source electrode is spaced a preset distance from the gate structure;

[0010] a drain electrode, electrically connected to the barrier layer on a side of the gate structure away from the source electrode, the drain electrode being spaced apart from the gate structure by a preset distance;

[0011] A first strain compensation layer is located on an upper surface of the barrier layer between the gate structure and the source electrode, and the first strain compensation layer is adjacent to the cap layer;

[0012] A second strain compensation layer is located on an upper surface of the barrier layer between the gate structure and the drain electrode, and the second strain compensation layer is spaced a preset distance from the cap layer;

[0013] A barrier compensation layer covers an exposed surface of the barrier layer between the gate structure and the second strain compensation layer.

[0014] Optionally, the gate structure further includes a gate located on an upper surface of the cap layer and electrically connected to the cap layer.

[0015] Optionally, the first strain compensation layer includes aluminum elements and nitrogen elements; and the second strain compensation layer includes aluminum elements and nitrogen elements.

[0016] Optionally, the first strain compensation layer and the second strain compensation layer have the same thickness.

[0017] Optionally, the type of elements in the barrier compensation layer is the same as the type of elements in the barrier layer.

[0018] Optionally, the bandgap width of the barrier compensation layer is greater than the bandgap width of the barrier layer.

[0019] Optionally, a groove having a bottom surface lower than a bottom surface of the cap layer is provided in the barrier layer, and the groove is embedded in an upper surface layer of the barrier layer below a gap between the gate structure and the second strain compensation layer.

[0020] Optionally, the depth of the groove does not exceed 2 nm.

[0021] Optionally, an upper surface of the barrier compensation layer is higher than a lower surface of the cap layer and lower than an upper surface of the cap layer.

[0022] The present invention also provides a method for preparing a HEMT device, comprising the following steps:

[0023] A semiconductor structure is provided, the semiconductor structure comprising a substrate, a buffer layer, a channel layer and a barrier layer stacked in sequence, and a gate structure including a cap layer electrically connected to the barrier layer is formed on an upper surface of the barrier layer;

[0024] forming a strain compensation material layer with a preset thickness on the exposed surface of the barrier layer, and etching the strain compensation material layer to obtain a first strain compensation layer and a second strain compensation layer located on opposite sides of the gate structure, wherein the first strain compensation layer is adjacent to the cap layer, and the second strain compensation layer is spaced a preset distance from the cap layer;

[0025] forming a barrier compensation layer covering an exposed surface of the barrier layer between the gate structure and the second strain compensation layer;

[0026] A source electrode electrically connected to the barrier layer is formed, and a drain electrode electrically connected to the barrier layer is formed, wherein the source electrode is located on a side of the first strain compensation layer away from the gate structure, and the drain electrode is located on a side of the second strain compensation layer away from the gate structure.

[0027] As described above, the HEMT device and the preparation method thereof of the present invention respectively arrange the first strain compensation layer and the second strain compensation layer on the upper surface of the barrier layer on the opposite side of the gate structure, and the first strain compensation layer is adjacent to the gate structure, and the second strain compensation layer is spaced apart from the gate structure by a preset distance, thereby improving the two-dimensional electron gas density in the channel region of the gate structure close to the source side and the drain close to the gate structure side, and arranges the barrier compensation layer covering the exposed surface of the barrier layer in the gap between the second strain compensation layer and the gate structure, thereby eliminating the defects introduced in the process of forming the second strain compensation layer, ensuring that the two-dimensional electron gas density in the channel region below the barrier compensation layer remains unchanged, making the electric field in the channel region of the device more uniform, thereby improving the breakdown voltage of the device, alleviating the current collapse effect of the device, and also alleviating the hot electron effect at the drain of the device, reducing the on-resistance of the device, and improving the reliability and performance of the device, and having a high industrial utilization value. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 Shown is a schematic diagram of the cross-sectional structure of a HEMT device.

[0029] Figure 2 Shown is a schematic diagram of the cross-sectional structure of another HEMT device.

[0030] Figure 3 It is a schematic diagram showing the cross-sectional structure of the HEMT device of the present invention.

[0031] Figure 4 The diagram shows the change of the two-dimensional electron gas density in the channel region from below the barrier compensation layer to below the second strain compensation layer of the HEMT device of the present invention.

[0032] Figure 5 The graph shows the distribution of the channel electric field intensity from the source to the drain of the HEMT device of the present invention.

[0033] Figure 6 The process flow chart of the HEMT device manufacturing method of the present invention is shown.

[0034] Figure 7 The cross-sectional structure schematic diagram shows the semiconductor structure of the method for preparing the HEMT device of the present invention.

[0035] Figure 8 It is a schematic diagram showing the cross-sectional structure after forming a gate material layer in the method for preparing a HEMT device of the present invention.

[0036] Fig. 9 It is a schematic diagram showing the cross-sectional structure of the HEMT device manufacturing method of the present invention after forming the gate structure.

[0037] Fig.10 It is a schematic diagram showing the cross-sectional structure after forming the strain compensation material layer in the method for preparing the HEMT device of the present invention.

[0038] Fig.11 It is a schematic diagram showing the cross-sectional structure after forming the second strain compensation layer in the method for preparing the HEMT device of the present invention.

[0039] Fig.12 It is a schematic diagram showing the cross-sectional structure after forming the barrier layer in the method for preparing the HEMT device of the present invention.

[0040] Fig.13 It is a schematic diagram showing the cross-sectional structure after forming a passivation layer in the method for preparing a HEMT device of the present invention.

[0041] Fig.14 It is a schematic diagram showing the cross-sectional structure after forming the contact hole in the method for preparing the HEMT device of the present invention.

[0042] Description of Figure Numbers

[0043] 01 Semiconductor Structure

[0044] 011 Substrate

[0045] 012 Buffer layer

[0046] 013 Channel layer

[0047] 014 Barrier layer

[0048] 02 Gate structure

[0049] 021 Cap layer

[0050] 022 Gate

[0051] 03 Source

[0052] 04 Drain

[0053] 05 Passivation layer

[0054] 1 Semiconductor structure

[0055] 11 Substrate

[0056] 12 Buffer layer

[0057] 13 Channel layer

[0058] 14 Barrier layer

[0059] 15 Grooves

[0060] 2 Gate structure

[0061] 21 Cap layer

[0062] 22 Gate

[0063] 23 Cap material layer

[0064] 24 Gate material layer

[0065] 3 Source

[0066] 4 Drain

[0067] 5. First strain compensation layer

[0068] 50 layers of strain compensation material

[0069] 6 Second strain compensation layer

[0070] 7 Barrier compensation layer

[0071] 8 Passivation layer

[0072] 81 Contact hole DETAILED DESCRIPTION

[0073] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0074] See also Figures 3 to 14 It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0075] Embodiment 1

[0076] This embodiment provides a HEMT device, such as Figure 3, which is a schematic diagram of the cross-sectional structure of the HEMT device, including a semiconductor structure 1, a gate structure 2, a source 3, a drain 4, a first strain compensation layer 5, a second strain compensation layer 6 and a barrier compensation layer 7, wherein the semiconductor structure 1 includes a substrate 11, a buffer layer 12, a channel layer 13 and a barrier layer 14 stacked in sequence; the gate structure 2 includes a cap layer 21 located on the upper surface of the barrier layer 14 and electrically connected to the barrier layer 14; the source 3 is electrically connected to the barrier layer 14, and the source 3 is spaced apart from the gate structure 2 by a preset distance; the drain 4 and the gate structure 2 are separated from the source The barrier layer 14 on one side of the drain electrode 3 is electrically connected, and the drain electrode 4 is spaced a preset distance from the gate structure 2; the first strain compensation layer 5 is located on the upper surface of the barrier layer 14 between the gate structure 2 and the source electrode 3, and the first strain compensation layer 5 is adjacent to the cap layer 21; the second strain compensation layer 6 is located on the upper surface of the barrier layer 14 between the gate structure 2 and the drain electrode 4, and the second strain compensation layer 6 is spaced a preset distance from the cap layer 21; the barrier compensation layer 7 covers the exposed surface of the barrier layer 14 between the gate structure 2 and the second strain compensation layer 6.

[0077] Specifically, the material of the substrate 11 includes sapphire, SiC, Si, GaN, diamond, Al2O3 or other suitable materials.

[0078] Specifically, while ensuring device performance, the shape, size and thickness of the substrate 11 can be selected according to actual conditions and are not limited here.

[0079] Specifically, the material of the buffer layer 12 includes AlN, AlGaN, GaN, InN or other suitable semiconductor materials.

[0080] Specifically, the buffer layer 12 can be a single-layer structure or a composite layer structure, and when the buffer layer 12 is a single-layer structure, the size and thickness of the buffer layer 12 can be set according to actual conditions while ensuring device performance, and are no longer restricted here; when the buffer layer 12 is a composite layer, the size and thickness of each film layer in the buffer layer 12 can be set according to actual conditions while ensuring device performance, and are no longer restricted here.

[0081] Specifically, the material of the channel layer 13 includes a nitride-based semiconductor or other suitable semiconductor materials, such as nitride and III-V group compounds (such as GaN, Al x Ga 1-x N、In x Ga 1-x N, etc.).

[0082] Specifically, while ensuring device performance, the shape, size and thickness of the channel layer 13 can be selected according to actual conditions and are not limited here.

[0083] Specifically, the material of the barrier layer 14 includes a nitride-based semiconductor or other suitable semiconductor materials, such as nitride and III-V compound (such as In x Al y Ga 1-x-y N、In x Al 1-x N、Al x Ga 1-x N、In x Ga 1-x N, etc.).

[0084] Specifically, under the condition of ensuring the device performance, the thickness of the barrier layer 14 can be selected according to actual conditions and is not limited here.

[0085] Specifically, due to the difference in material properties between the channel layer 13 and the barrier layer 14, a polarization effect occurs at the interface between the channel layer 13 and the barrier layer 14, and then a two-dimensional electron gas (2DEG) is generated, that is, electrons gather in a narrow and deep quantum well at the interface between the channel layer 13 and the barrier layer 14, so that a two-dimensional electron gas is formed at the interface between the channel layer 13 and the barrier layer 14.

[0086] Specifically, the cap layer 21 is used to deplete electrons in the two-dimensional electron gas generated at the interface between the barrier layer 14 and the channel layer 13 below the cap layer 21. The material of the cap layer 21 includes a P-type doped III-V compound semiconductor material or other suitable semiconductor materials. In this embodiment, a P-type GaN layer is used as the cap layer 21.

[0087] Specifically, while ensuring device performance and the cap layer 21 depleting electrons in the two-dimensional electron gas below the cap layer 21 , the shape, size, thickness and doping concentration of the cap layer 21 can be selected according to actual conditions and are not limited here.

[0088] As an example, the gate structure 2 further includes a gate 22 located on the upper surface of the cap layer 21 and electrically connected to the cap layer 21 .

[0089] Specifically, the gate 22 is made of titanium, titanium nitride, silver, gold, copper, tungsten, nickel, platinum, aluminum or other suitable conductive materials.

[0090] As an example, the first strain compensation layer 5 includes aluminum, nitrogen or other suitable elements, for example, AlN.

[0091] Specifically, the first strain compensation layer 5 is used to adjust the two-dimensional electron gas concentration in the channel below the first strain compensation layer 5, so that the concentration of the two-dimensional electron gas in the channel below the first strain compensation layer 5 is higher than the two-dimensional electron gas concentration in the channel in the area where the first strain compensation layer 5 is not set.

[0092] As an example, the thickness of the first strain compensation layer 5 is smaller than the thickness of the cap layer 21 .

[0093] Specifically, under the condition of ensuring device performance, the side wall of the first strain compensation layer 5 away from the gate structure 2 may be adjacent to the source 3 , or may be spaced apart from the source 3 by a preset distance.

[0094] As an example, the second strain compensation layer 6 includes aluminum, nitrogen or other suitable elements. For example, an AlN layer may be selected as the second strain compensation layer 6 .

[0095] Specifically, the second strain compensation layer 6 is used to adjust the two-dimensional electron gas concentration in the channel region below the second strain compensation layer 6, so that the two-dimensional electron gas concentration in the channel region below the second strain compensation layer 6 is higher than the two-dimensional electron gas concentration in the channel region above which the second strain compensation layer 6 is not disposed.

[0096] As an example, the thickness of the second strain compensation layer 6 is smaller than the thickness of the cap layer 21 .

[0097] Specifically, under the condition of ensuring device performance, the distance between the side wall of the second strain compensation layer 6 away from the drain 4 and the gate structure 2 can be selected according to actual conditions and is not limited here.

[0098] Specifically, by arranging the second strain compensation layer 6 and the gate structure 2 at intervals, and using the second strain compensation layer 6 to adjust the two-dimensional electron gas concentration close to the drain 4 side, so that the two-dimensional electron gas concentration close to the drain 4 side is higher than the two-dimensional electron gas concentration in the channel region below the gap between the second strain compensation layer 6 and the gate structure 2, the problem of electric field concentration on the gate structure 2 close to the drain 4 side in the device when the device is in the off state can be alleviated, the electric field distribution of the channel can be made more uniform, the breakdown voltage of the device can be improved, and the current collapse effect of the device can be alleviated.

[0099] As an example, the first strain compensation layer 5 and the second strain compensation layer 6 have the same thickness.

[0100] As an example, the element type in the barrier compensation layer 7 is the same as the element type in the barrier layer 14 , that is, the barrier compensation layer 7 and the barrier layer 14 are both composed of the same element atoms.

[0101] As an example, the bandgap width of the barrier compensation layer 7 is greater than the bandgap width of the barrier layer 14 .

[0102] As an example, a groove 15 having a bottom surface lower than the bottom surface of the cap layer 21 is provided in the barrier layer 14 , and the groove 15 is embedded in the upper surface layer of the barrier layer 14 below the gap between the gate structure 2 and the second strain compensation layer 6 .

[0103] Specifically, the opening size of the groove 15 is the same as the size of the gap between the gate structure 2 and the second strain compensation layer 6 , and the barrier compensation layer 7 fills the groove 15 .

[0104] As an example, the depth of the groove 15 does not exceed 2 nm. The depth here refers to the distance between the bottom surface of the groove 15 and the bottom surface of the cap layer 21.

[0105] Specifically, the barrier compensation layer 7 is used to eliminate defects caused by damage to the barrier layer 14 during the formation of the second strain compensation layer 6, so as to prevent the defects generated during the formation of the second strain compensation layer 6 from affecting the concentration of the two-dimensional electron gas in the channel region below the gap between the second strain compensation layer 6 and the gate structure 2, so that the two-dimensional electron gas in the channel region below the gap between the second strain compensation layer 6 and the gate structure 2 maintains a normal value.

[0106] As an example, the upper surface of the barrier compensation layer 7 is higher than the lower surface of the cap layer 21 and lower than the upper surface of the cap layer 21 .

[0107] Specifically, the device is further provided with a passivation layer 8 covering the barrier compensation layer 7 , the first strain compensation layer 5 , the second strain compensation layer 6 and the exposed surface of the barrier layer 14 .

[0108] Specifically, the passivation layer 8 is further provided with a contact hole 81 penetrating the passivation layer 8 and exposing the barrier layer 14 at the bottom, and the source electrode 3 and the drain electrode 4 are respectively filled with different contact holes 81 .

[0109] Specifically, the source electrode 3 is made of titanium, titanium nitride, silver, gold, copper, tungsten, nickel, platinum, aluminum or other suitable conductive materials.

[0110] Specifically, the material of the drain electrode 4 includes titanium, titanium nitride, silver, gold, copper, tungsten, nickel, platinum, aluminum or other suitable conductive materials.

[0111] Specifically, Figure 4As shown, it is a diagram of the change of the two-dimensional electron gas density in the channel region from the edge of the gate structure 2 close to the drain 4 to the bottom of the second strain compensation layer 6, wherein region A refers to the channel region of the second barrier compensation layer 6 close to the gate structure 2 side, that is, the channel region below the barrier compensation layer 7, and region B refers to the channel region below the second strain compensation layer 6. It can be seen from the figure that the two-dimensional electron density of the channel region below the barrier compensation layer 7 close to the second strain compensation layer 6 is lower than the two-dimensional electron gas density of the channel region below the second strain compensation layer 6, that is, the two-dimensional electron gas density in the channel region where the second strain compensation layer 6 is set is greater than the two-dimensional electron gas density in the channel region where the compensation layer is not set.

[0112] Specifically, by arranging the first strain compensation layer 5 located on the upper surface of the barrier layer 14 between the source 3 and the gate structure 2, and the first strain compensation layer 5 is adjacent to the gate structure 2 near the side wall of the gate structure 2, the two-dimensional electron gas density in the channel region below the first strain compensation layer 5 on the side of the gate structure 2 near the source 3 is improved, and at the same time, the second strain compensation layer 6 located on the upper surface of the barrier layer 14 is arranged between the drain 4 and the gate structure 2, and the second strain compensation layer 6 is spaced a preset distance from the gate structure 2, so that the two-dimensional electron gas density in the channel region below the second strain compensation layer 6 at the preset distance from the gate structure 2 is increased, the electric field distribution in the channel region of the device is more uniform, and the problem of electric field concentration at the side edge of the gate structure 2 near the drain 4 is improved, thereby improving the breakdown voltage of the device, alleviating the current collapse effect of the device, and improving the performance of the device.

[0113] Specifically, Figure 5 As shown, it is a distribution diagram of the channel electric field strength from the source 3 to the drain 4. It can be seen from the figure that due to the setting of the first strain compensation layer 5 and the second strain compensation layer 6, the electric field strength in the channel region between the source 3 and the drain 4 of the device has two peaks, thereby making the electric field distribution in the channel region of the device more uniform, avoiding the problem of electric field concentration at the edge of the gate structure 2 close to the drain 4 side.

[0114] Specifically, since the second strain compensation layer 6 is spaced apart from the gate structure 2 and the two-dimensional electron gas concentration in the channel region below the second strain compensation layer 6 is increased, the current density in the channel region below the second strain compensation layer 6 is relatively large, thereby alleviating the thermal electron effect at the drain 4 and improving the reliability of the device.

[0115] Specifically, due to the provision of the barrier compensation layer 7, defects introduced by forming the second strain compensation layer 6 are eliminated, and the defects are prevented from affecting the two-dimensional electron gas concentration in the channel region below the gap between the second strain compensation layer 6 and the gate structure 2, thereby ensuring that the density of the two-dimensional electron gas on the side of the gate structure 2 close to the drain 4 remains unchanged.

[0116] Specifically, due to the arrangement of the first strain compensation layer 5, the second strain compensation layer 6 and the barrier compensation layer 7, the two-dimensional electron gas density in the channel region of the gate structure 2 close to the drain 4 side remains unchanged, and the two-dimensional electron gas density in the channel region below the first strain compensation layer 5 and the second strain compensation layer 6 is higher than the two-dimensional electron gas density in the channel region without the strain compensation layer, thereby increasing the migration speed of the two-dimensional electron gas and reducing the on-resistance of the device.

[0117] The HEMT device of this embodiment improves the two-dimensional electron gas concentration in the channel region of the gate structure 2 close to the source 3 side by disposing the first strain compensation layer 5 and the second strain compensation layer 6, and at the same time improves the two-dimensional electron gas concentration in the channel region of the drain 4 close to the gate structure 2 side. Moreover, by disposing the barrier compensation layer 7, the two-dimensional electron gas concentration in the channel region below the gap between the second strain compensation layer 6 and the gate structure 2 remains unchanged, thereby making the electric field distribution in the conductive channel of the device more uniform, improving the problem of electric field concentration at the side edge of the gate structure 2 close to the drain 4 side, improving the breakdown voltage of the device, alleviating the current collapse effect of the device, and at the same time alleviating the hot electron effect at the drain 4 of the device, thereby improving the reliability of the device and reducing the on-resistance of the device.

[0118] Embodiment 2

[0119] This embodiment provides a method for preparing a HEMT device, such as Figure 6 FIG. 1 is a process flow chart of the method for preparing the HEMT device, comprising the following steps:

[0120] S1: providing a semiconductor structure, the semiconductor structure comprising a substrate, a buffer layer, a channel layer and a barrier layer stacked in sequence, and forming a gate structure including a cap layer electrically connected to the barrier layer on an upper surface of the barrier layer;

[0121] S2: forming a strain compensation material layer with a preset thickness on the exposed surface of the barrier layer, and etching the strain compensation material layer to obtain a first strain compensation layer and a second strain compensation layer located on opposite sides of the gate structure, wherein the first strain compensation layer is adjacent to the cap layer, and the second strain compensation layer is spaced a preset distance from the cap layer;

[0122] S3: forming a barrier compensation layer covering an exposed surface of the barrier layer between the gate structure and the second strain compensation layer;

[0123] S4: forming a source electrode electrically connected to the barrier layer, forming a drain electrode electrically connected to the barrier layer, wherein the source electrode is located on a side of the first strain compensation layer away from the gate structure, and the drain electrode is located on a side of the second strain compensation layer away from the gate structure.

[0124] See also Figures 7 to 11 , performing step S1 and step S2: providing a semiconductor structure 1, the semiconductor structure 1 comprising a substrate 11, a buffer layer 12, a channel layer 13 and a barrier layer 14 stacked in sequence, forming a gate structure 2 including a cap layer 21 electrically connected to the barrier layer 14 on the upper surface of the barrier layer 14; forming a strain compensation material layer 50 of a preset thickness on the exposed surface of the barrier layer 14, and etching the strain compensation material layer 50 to obtain a first strain compensation layer 5 and a second strain compensation layer 6 located on opposite sides of the gate structure 2, the first strain compensation layer 5 being adjacent to the cap layer 21, and the second strain compensation layer 6 being spaced a preset distance from the cap layer 21.

[0125] Specifically, Figure 7 As shown, it is a schematic diagram of the cross-sectional structure of the semiconductor structure 1, in which the substrate 11 is used to provide a process platform for forming a device, and the buffer layer 12 is used to reduce the lattice mismatch and thermal mismatch between the material of the substrate 11 and the material of the channel layer 13, so as to improve the quality of the formed channel layer 13, and a quantum well is formed at the interface between the barrier layer 14 and the channel layer 13, thereby generating a two-dimensional electron gas.

[0126] Specifically, the gate structure 2 further includes a gate 22 located on the upper surface of the cap layer 21 and electrically connected to the cap layer 21 .

[0127] Specifically, Figure 8 and Fig. 9 The figures are respectively a schematic diagram of the cross-sectional structure after forming the gate material layer 24 and a schematic diagram of the cross-sectional structure after forming the gate structure 2. The formation of the gate structure 2 includes the following steps: forming a cap material layer 23 and a gate material layer 24 stacked in sequence on the upper surface of the barrier layer 14; forming a patterned photoresist layer (not shown) on the upper surface of the gate material layer 24, and etching the gate material layer 24 and the cap material layer 23 in sequence based on the patterned photoresist layer to obtain the gate structure 2.

[0128] Specifically, the method of forming the cap material layer 23 includes physical vapor deposition, chemical vapor deposition or other suitable methods.

[0129] Specifically, under the condition of ensuring the performance of the device, the thickness of the cap material layer 23 can be selected according to actual conditions and is not limited here.

[0130] Specifically, the method of forming the gate material layer 24 includes sputtering, physical vapor deposition, chemical vapor deposition, metal compound vapor deposition, molecular beam epitaxy, atomic vapor deposition, atomic layer deposition or other suitable methods.

[0131] Specifically, the method of forming the photoresist layer and patterning the photoresist layer is a commonly used photoresist manufacturing and developing method, which will not be described in detail here.

[0132] Specifically, the method of etching the gate material layer 24 includes dry etching, wet etching or other suitable methods; the method of etching the cap material layer 23 includes dry etching, wet etching or other suitable methods.

[0133] Specifically, after forming the gate structure 2 and before forming the strain compensation material layer 50 , the method further includes a step of removing the photoresist layer.

[0134] Specifically, the method for removing the photoresist layer is a commonly used photoresist removal method, which will not be described in detail here.

[0135] Specifically, Fig.10 , which is a schematic diagram of a cross-sectional structure after forming the strain compensation material layer 50 , the method of forming the strain compensation material layer 50 includes chemical vapor deposition, physical vapor deposition or other suitable methods.

[0136] Specifically, the method of etching the strain compensation material layer 50 includes dry etching, wet etching or other suitable methods.

[0137] Specifically, Fig.11 As shown, it is a schematic diagram of the cross-sectional structure after the second strain compensation layer 6 is formed. In the process of forming the second strain compensation layer 6, in order to ensure that the strain compensation material layer 50 between the second strain compensation layer 6 and the gate structure 2 is completely etched, the strain compensation material layer 50 will be over-etched, thereby damaging the barrier layer 14 at that location, or causing the barrier layer 14 at that location to form a groove 15 and damage the barrier layer 14, thereby introducing defects in the barrier layer 14 between the gate structure 2 and the second strain compensation layer 6.

[0138] Specifically, the distance between the upper surface of the barrier layer 14 below the gap between the gate structure 2 and the second strain compensation layer 6 and the lower surface of the gate structure 2 does not exceed 2 nm, that is, the depth of the groove 15 is not greater than 2 nm.

[0139] Specifically, under the condition of ensuring device performance, the sidewall of the second strain compensation layer 6 away from the gate structure 2 may be adjacent to the drain 4 .

[0140] Please see again Figure 12 to Figure 14 , perform step S3 and step S4: form a barrier compensation layer 7 covering the exposed surface of the barrier layer 14 between the gate structure 2 and the second strain compensation layer 6; form a source electrode 3 electrically connected to the barrier layer 14, and form a drain electrode 4 electrically connected to the barrier layer 14, the source electrode 3 is located on a side of the first strain compensation layer 5 away from the gate structure 2, and the drain electrode 4 is located on a side of the second strain compensation layer 6 away from the gate structure 2.

[0141] Specifically, Fig.12 FIG. 2 is a schematic diagram of a cross-sectional structure after forming the barrier compensation layer 7. The method of forming the barrier compensation layer 7 includes chemical vapor deposition, physical vapor deposition or other suitable methods. In this embodiment, the barrier compensation layer 7 is formed by metal organic chemical vapor deposition (MOCVD).

[0142] Specifically, the bandgap width of the formed barrier compensation layer 7 is greater than the bandgap width of the barrier layer 14, so as to adjust the density of the two-dimensional electron gas below the barrier compensation layer 7, so that the two-dimensional electron gas density below the barrier compensation layer 7 is the same as the two-dimensional electron gas density at that location when the first strain compensation layer 5 and the second strain compensation layer 6 are not set.

[0143] Specifically, the side wall of the barrier compensation layer 7 close to the drain 4 is located on the second strain compensation layer 6, and the barrier compensation layer 7 is close to the drain 4 (see the subsequent Fig.13 ) may also be flush with the side wall of the second strain compensation layer 6 close to the drain 4, that is, the barrier compensation layer 7 may partially cover the upper surface of the second strain compensation layer 7, or may completely cover the upper surface of the second strain compensation layer 6.

[0144] Specifically, under the condition of ensuring device performance, the side wall of the barrier compensation layer 7 away from the gate structure 2 and the side wall of the second strain compensation layer 6 can be adjacent to the drain 4 at the same time.

[0145] Specifically, Fig.13 As shown, it is a schematic diagram of the cross-sectional structure after the passivation layer 8 is formed. After the barrier compensation layer 7 is formed, it also includes the step of forming the passivation layer 8 covering the barrier layer 14, the first strain compensation layer 5, the second strain compensation layer 6 and the exposed surface of the barrier compensation layer 7.

[0146] Specifically, the method of forming the passivation layer 8 includes chemical vapor deposition, physical vapor deposition or other suitable methods.

[0147] Specifically, under the condition of ensuring the performance of the device, the thickness of the passivation layer 8 can be selected according to actual conditions and is not limited here.

[0148] Specifically, the material of the passivation layer 8 includes silicon oxide, silicon nitride or other suitable insulating materials.

[0149] Specifically, Fig.14 As shown, it is a schematic diagram of the cross-sectional structure after the contact hole 81 is formed. After the passivation layer 8 is formed and before the source 3 and the drain 4 are formed, it also includes the step of forming the contact hole 81 in the passivation layer 8. The contact hole 81 penetrates the passivation layer 8 and the barrier layer 14 is exposed on the bottom surface.

[0150] Specifically, the method of forming the contact hole 81 includes dry etching, wet etching or other suitable methods.

[0151] Specifically, under the condition of ensuring the device performance, the opening size of the contact hole 81 can be selected according to actual conditions and is not limited here.

[0152] Specifically, the method for forming the source 3 includes sputtering, physical vapor deposition, chemical vapor deposition, metal compound vapor deposition, molecular beam epitaxy, atomic vapor deposition, atomic layer deposition or other suitable methods; the method for forming the drain 4 includes sputtering, physical vapor deposition, chemical vapor deposition, metal compound vapor deposition, molecular beam epitaxy, atomic vapor deposition, atomic layer deposition or other suitable methods.

[0153] Specifically, by forming the barrier compensation layer 7 between the second strain compensation layer 6 and the gate structure 2, the defects of the barrier layer 14 caused by the formation of the second strain compensation layer 6 are eliminated, thereby ensuring that the two-dimensional electron gas density in the channel region below the barrier compensation layer 7 between the second strain compensation layer 6 and the gate structure 2 remains unchanged.

[0154] Specifically, after forming the gate structure 2 and before forming the passivation layer 8, the first strain compensation layer 5 and the second strain compensation layer 6 are respectively formed on opposite sides of the gate structure 2, and the first strain compensation layer 5 is adjacent to the gate structure 2, and the second strain compensation layer 6 is spaced a preset distance from the gate structure 2, thereby improving the two-dimensional electron gas density in the channel region of the gate structure 2 close to the source 3 and the drain 4 close to the gate structure 2. At the same time, the barrier compensation layer 7 is formed to ensure that the two-dimensional electron gas density in the channel region below the gap between the second strain compensation layer 6 and the gate structure 2 remains unchanged, so that the two-dimensional electron gas distribution in the device is more uniform, and then the electric field distribution in the region where the two-dimensional electron gas is located is more uniform, thereby improving the voltage resistance performance of the device.

[0155] The method for preparing the HEMT device of this embodiment forms the first strain compensation layer 5 located between the gate structure 2 and the source electrode 3 and the second strain compensation layer 6 located between the gate structure 2 and the drain electrode 4 after forming the gate structure 2 and before forming the passivation layer 8, and forms the barrier compensation layer 7 having a bandgap width greater than the barrier layer 14 to eliminate defects introduced by forming the second strain compensation layer 6, thereby ensuring the two-dimensional electron gas density in the channel region of the gate structure 2 close to the drain electrode 4 side, making the electric field distribution in the region where the two-dimensional electron gas is located in the device more uniform, and improving the withstand voltage performance of the device.

[0156] In summary, the HEMT device and preparation method of the present invention provide a first strain compensation layer located on the upper surface of the barrier layer and adjacent to the gate structure between the source and the gate structure, and provide a second strain compensation layer located on the upper surface of the barrier layer and spaced a preset distance from the gate structure between the drain and the gate structure, so as to increase the two-dimensional electron gas density in the channel region of the gate structure close to the source side and the drain close to the gate structure side, and provide a barrier compensation layer on the exposed surface of the barrier layer in the gap between the second strain compensation layer and the gate structure, thereby eliminating the defects introduced by forming the second strain compensation layer, ensuring that the two-dimensional electron gas density in the channel region below the barrier compensation layer remains unchanged, making the electric field in the channel region of the device more uniform, improving the breakdown voltage of the device, alleviating the current collapse effect of the device, and at the same time alleviating the hot electron effect at the drain of the device, improving the reliability of the device, and reducing the on-resistance of the device. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0157] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A HEMT device, characterized in that: include: A semiconductor structure comprising a substrate, a buffer layer, a channel layer and a barrier layer stacked in sequence; A gate structure, comprising a cap layer located on an upper surface of the barrier layer and electrically connected to the barrier layer; A source electrode, electrically connected to the barrier layer, wherein the source electrode is spaced a preset distance from the gate structure; a drain electrode, electrically connected to the barrier layer on a side of the gate structure away from the source electrode, the drain electrode being spaced apart from the gate structure by a preset distance; A first strain compensation layer is located on the upper surface of the barrier layer between the gate structure and the source electrode, and the A first strain compensation layer is adjacent to the cap layer; A second strain compensation layer is located on an upper surface of the barrier layer between the gate structure and the drain electrode, and the second strain compensation layer is spaced a preset distance from the cap layer; A barrier compensation layer covers an exposed surface of the barrier layer between the gate structure and the second strain compensation layer.

2. The HEMT device according to claim 1, characterized in that: The gate structure also includes a gate located on the upper surface of the cap layer and electrically connected to the cap layer.

3. The HEMT device according to claim 1, characterized in that: The first strain compensation layer includes aluminum and nitrogen; the second strain compensation layer includes aluminum and nitrogen.

4. The HEMT device according to claim 1, characterized in that: The first strain compensation layer and the second strain compensation layer have the same thickness.

5. The HEMT device according to claim 1, characterized in that: The element type in the barrier compensation layer is the same as the element type in the barrier layer.

6. The HEMT device according to claim 1, characterized in that: The bandgap width of the barrier compensation layer is greater than the bandgap width of the barrier layer.

7. The HEMT device according to claim 1, characterized in that: The barrier layer is provided with a groove whose bottom surface is lower than the bottom surface of the cap layer, and the groove is embedded in the upper surface layer of the barrier layer below the gap between the gate structure and the second strain compensation layer.

8. The HEMT device according to claim 7, characterized in that: The depth of the groove does not exceed 2 nm.

9. The HEMT device according to claim 1, characterized in that: An upper surface of the barrier compensation layer is higher than a lower surface of the cap layer and lower than an upper surface of the cap layer.

10. A method for preparing a HEMT device, characterized in that: The following steps are involved: A semiconductor structure is provided, the semiconductor structure comprising a substrate, a buffer layer, a channel layer and a barrier layer stacked in sequence, and a gate structure including a cap layer electrically connected to the barrier layer is formed on an upper surface of the barrier layer; forming a strain compensation material layer with a preset thickness on the exposed surface of the barrier layer, and etching the strain compensation material layer to obtain a first strain compensation layer and a second strain compensation layer located on opposite sides of the gate structure, wherein the first strain compensation layer is adjacent to the cap layer, and the second strain compensation layer is spaced a preset distance from the cap layer; forming a barrier compensation layer covering an exposed surface of the barrier layer between the gate structure and the second strain compensation layer; A source electrode electrically connected to the barrier layer is formed, and a drain electrode electrically connected to the barrier layer is formed, wherein the source electrode is located on a side of the first strain compensation layer away from the gate structure, and the drain electrode is located on a side of the second strain compensation layer away from the gate structure.

Citation Information

Cited By

  • HEMT device and preparation method therefor

    WO2026118561A1