Structure anti-floating construction method

By using steel pipe mixing composite pile technology, large-diameter mixing piles are used to obtain soil friction resistance, while the steel pipe bears the buoyancy. This solves the problem of insufficient friction resistance in existing technologies, achieving a highly efficient and economical anti-buoyancy effect, and is suitable for anti-buoyancy construction of various buildings.

CN119021282APending Publication Date: 2024-11-26CHINA RAILWAY SHANGHAI DESIGN INST GRP CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411415675.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-11
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Among existing structural anti-buoyancy methods, pile foundations or anti-buoyancy anchors have limited frictional resistance and high cost, resulting in insufficient anti-buoyancy capacity.

Method used

Steel pipe mixing composite piles are adopted. The frictional resistance of the surrounding soil layer is obtained through large-diameter mixing piles, and the buoyancy is borne and transmitted by the steel pipe. The combination of steel pipe and cement soil creates a rigid-flexible composite anti-buoyancy pile.

Benefits of technology

It significantly improves anti-buoyancy capabilities, reduces construction costs, and is suitable for anti-buoyancy engineering of various buildings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119021282A_ABST
    Figure CN119021282A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of pile foundation engineering, in particular to a structure anti-floating construction method which comprises the following steps: forming a hole in a bottom plate of an existing building, rotating and sinking the steel pipe, enabling a stirring head arranged at the bottom of the steel pipe to cut a soil body, and synchronously spraying cement paste to the stirring head through a grouting steel pipe so as to form a stirring pile; and the top of the steel pipe is connected with a structural bottom plate of the existing building to form the steel pipe stirring composite anti-floating pile, and the steel pipe stirring composite anti-floating pile is used for anti-floating of the existing building. The method has the advantages that the peripheral large-diameter mixing pile is adopted to obtain the frictional resistance of the peripheral soil layer, and the steel pipe of the pile core bears and transmits upward buoyancy; respective characteristics of rigid and flexible composite piles are fully exerted, stress is reasonable, and the advantages of being large in anti-floating capacity, easy to construct and low in manufacturing cost are achieved; the method can be widely applied to structural anti-floating projects of various existing buildings (such as houses, tunnels, U-shaped grooves and the like), and has a wide application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of pile foundation engineering, in particular to a structural anti-floating construction method. Background Art

[0002] Existing structures generally use pile foundations or anti-floating anchor rods to prevent floating. The anti-floating piles have limited side friction and are relatively expensive. The anti-floating anchor rods have a small diameter and limited anti-floating capacity. Summary of the invention

[0003] The purpose of the present invention is to provide a structural anti-floating construction method based on the above-mentioned deficiencies of the prior art, using steel pipe mixing composite piles as anti-floating piles, using peripheral large-diameter mixing piles to obtain the friction resistance of the surrounding soil layer, and the upward buoyancy is borne and transmitted by the steel pipe of the pile core to achieve anti-floating.

[0004] The purpose of the present invention is achieved by the following technical solutions: A structural anti-floating construction method, characterized in that the construction method comprises the following steps: Drill holes in the existing building floor, with the hole diameter larger than the steel pipe and mixing head; The steel pipe is rotated and sunk, so that the mixing head arranged at the bottom of the steel pipe cuts the soil and cement slurry is simultaneously sprayed to the mixing head through the grouting steel pipe to form a mixing pile; The top of the steel pipe is connected to the structural bottom plate of the existing building to form a steel pipe mixing composite anti-floating pile, and the steel pipe mixing composite anti-floating pile is used for the anti-floating of the existing building.

[0005] The sinking of the steel pipe and the stirring head is achieved by arranging a frame. If repeated stirring is required, the frame drives the steel pipe and the stirring head to stir reciprocally up and down.

[0006] After the construction of one section of the mixing pile is completed, the steel pipe and the grouting steel pipe are extended and repeatedly constructed to the designed pile length to form a steel pipe mixing composite pile.

[0007] Ribs are arranged on the outer wall of the steel pipe.

[0008] The ribs are evenly spaced and arranged along the length direction of the steel pipe.

[0009] The ribs are symmetrically arranged along the circumference of the steel pipe.

[0010] The advantages of the present invention are: using peripheral large-diameter mixing piles to obtain the friction resistance of the surrounding soil layer, and the upward buoyancy is borne and transmitted by the steel pipe of the pile core; giving full play to the respective characteristics of the rigid-flexible composite piles, reasonable force, large anti-floating ability, simple construction, and low cost; it can be widely used in structural anti-floating projects of various existing buildings (such as houses, tunnels, U-grooves, etc.), and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 The construction steps of the present invention Figure I ; Figure 2 The construction steps of the present invention Figure II ; Figure 3 The construction steps of the present invention Figure III ; Figure 4 It is a structural schematic diagram of the present invention. DETAILED DESCRIPTION

[0012] The features of the present invention and other related features are further described in detail below through embodiments in conjunction with the accompanying drawings to facilitate understanding by those skilled in the art: like Figure 1-4 As shown in the figure, marks 1-14 respectively represent: cement slurry pump 1, grouting hose 2, folding mixing head 3, steel pipe 4, grouting steel pipe 5, rotary power head 6, frame 7, rib plate 8, steel pipe joint 9, steel pipe mixing composite anti-floating pile 10, cement soil 11, concrete 12, connecting steel plate 13, and structural bottom plate 14.

[0013] Example: Figures 1 to 4 As shown, the main body of the anti-floating steel pipe mixing composite pile in this embodiment is a steel pipe mixing anti-floating pile 1, which is constructed simultaneously with the structural bottom plate 7 of the underground building to play an anti-floating role for the underground building after construction.

[0014] Specifically, the steel pipe mixing composite anti-floating pile 1 includes an external cement soil 2 and a steel pipe 4 arranged inside the steel pipe 4, and concrete 3 is poured inside the steel pipe 4. The cement soil 2 is arranged below the structural bottom plate 7, the length of the steel pipe 4 matches the depth of the cement soil 2, and the top of the steel pipe 4 extends out of the structural bottom plate 7 and is fixedly connected by connecting steel plates 6 and bolts. At this time, the large-diameter mixing pile formed by the cement soil 2 obtains the friction resistance of the surrounding soil layer, and the steel pipe 4 inserted into the cement soil 2 as the pile core bears and transmits the upward buoyancy, thereby realizing the anti-floating of the underground building.

[0015] In order to ensure that the steel pipe 4 reaches the designed length, when the designed length of the steel pipe 4 is relatively long, several steel pipe segments may be connected by threading and welding.

[0016] In this embodiment, a plurality of ribs 5 are arranged outside the steel pipe 4, and the plurality of ribs 5 are evenly spaced along the length direction of the steel pipe 4 to improve the connection performance between the steel pipe 4 and the cement soil 2, thereby improving the structural performance of the steel pipe mixing composite anti-floating pile 1. At the same time, preferably, the ribs 5 are symmetrically arranged along the circumference of the steel pipe 4 to evenly improve the connection performance between the steel pipe 4 and the cement soil 2.

[0017] A mixing head is provided at the bottom of the steel pipe 4. When the steel pipe 4 rotates and sinks, cement soil 2 is formed by synchronous grouting, thereby realizing the construction of a large-diameter mixing pile.

[0018] During construction, this embodiment includes the following steps: 1) A drilling machine is used to drill a hole in the bottom plate of the existing building, and the hole diameter is larger than the steel pipe 4 and the folding mixing head 3.

[0019] 2) The rotary power head 6 holds the steel pipe 4 and rotates, driving the folding mixing head 3 at the bottom to rotate. The folding mixing head 3 unfolds under the resistance of the soil and cuts the soil as the steel pipe 4 rotates. At the same time, the cement slurry pump 1 sprays cement slurry to the folding mixing head 3 through the connected grouting hose 2 and the grouting steel pipe 5. The pile head soil is fully mixed with the cement slurry under the stirring of the folding mixing head 3 to form a large cement-soil pile. At the same time, the frame 7 drives the steel pipe 4 and the folding mixing head 3 to sink while stirring in the soil. If re-mixing is required, the frame 7 can also drive the steel pipe 4 and the folding mixing head 3 to stir reciprocately up and down to complete the re-mixing.

[0020] In this process, since the outer periphery of the steel pipe 4 in this embodiment is provided with ribs 5, although the outer contour size of the ribs 5 is smaller than the range of the folding mixing head 3, it can further improve the mixing effect, especially the bonding between the cement slurry and the soil, as the steel pipe 4 rotates.

[0021] 3) After the construction of one section of the mixing pile is completed, the next section of the steel pipe and the grouting steel pipe inside the steel pipe are connected by threaded welding, and then the second step is repeated to complete the mixing pile construction section by section to the designed pile length to form a steel pipe mixing composite pile.

[0022] 4) The top of the steel pipe 4 reaching the designed pile length is exposed at the bottom of the foundation pit (the location of the existing building bottom plate), and is connected to the structural bottom plate 14 by a connecting steel plate 13 and a nut to form a steel pipe mixing composite anti-floating pile 10.

[0023] In this embodiment, since the large-diameter mixing pile formed by cement soil 2 obtains the friction resistance of the surrounding soil layer to resist buoyancy, the diameter of the large-diameter mixing pile can be designed according to the anti-buoyancy requirements of the upper building, and the corresponding steel pipe 4 is designed to bear and transmit the upward buoyancy.

[0024] Although the above embodiments have described in detail the concepts and embodiments of the present invention with reference to the accompanying drawings, ordinary technicians in this field can recognize that various improvements and changes can still be made to the present invention without departing from the scope of the claims, so they are not described one by one here.

Claims

1. A structural anti-floating construction method, Features: The construction method comprises the following steps: Drill holes in the existing building floor, with the hole diameter larger than the steel pipe and mixing head; The steel pipe is rotated and sunk, so that the mixing head arranged at the bottom of the steel pipe cuts the soil and cement slurry is simultaneously sprayed to the mixing head through the grouting steel pipe to form a mixing pile; The top of the steel pipe is connected to the structural bottom plate of the existing building to form a steel pipe mixing composite anti-floating pile, and the steel pipe mixing composite anti-floating pile is used for the anti-floating of the existing building.

2. A structural anti-floating construction method according to claim 1, Features: The sinking of the steel pipe and the stirring head is achieved by arranging a frame. If repeated stirring is required, the frame drives the steel pipe and the stirring head to stir reciprocally up and down.

3. A structural anti-floating construction method according to claim 1, Features: After the construction of one section of the mixing pile is completed, the steel pipe and the grouting steel pipe are extended and repeatedly constructed to the designed pile length to form a steel pipe mixing composite pile.

4. A structural anti-floating construction method according to claim 1, Features: Ribs are arranged on the outer wall of the steel pipe.

5. A structural anti-floating construction method according to claim 4, Features: The ribs are evenly spaced apart along the length direction of the steel pipe.

6. A structural anti-floating construction method according to claim 5, Features: The ribs are symmetrically arranged along the circumference of the steel pipe.

Citation Information

Cited By

  • Construction method for rigid-flexible composite pile foundation

    WO2026123990A1