SiC MOSFET (Metal-Oxide-Semiconductor Field Effect Transistor) device capable of better protecting gate oxide and preparation method
By forming a heavily doped PP region in the SiC MOSFET device and achieving ohmic contact, the problem of easy breakdown of the gate oxide layer under high voltage is solved, and the long-term reliability and service life of the device are improved.
Patent Information
- Application Number
- CN202411176629.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-11-29
AI Technical Summary
The gate oxide layer of SiC MOSFET devices is prone to breakdown due to concentrated field strength during long-term use, resulting in low reliability and cannot meet the strict requirements in the field of high voltage and high power.
By forming a heavily doped PP region at the middle bottom of the gate of the SiC MOSFET device and ohmic contact is achieved on the top surface of the PP region, the gate Poly layer is connected to the PP region, reducing the voltage stress of the gate oxide layer, and in the device The electric field generated by the shielding drain voltage during the blocking process is concentrated to protect the gate oxide layer.
It effectively reduces the voltage stress of the gate oxide layer, improves its reliability for long-term use, prevents field strength concentration, and extends the service life of the device.
Smart Images

Figure CN119050150A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a SiC MOSFET device with better gate oxide protection and a preparation method thereof. Background Art
[0002] Si-based IGBTs have always been the main device for high-power applications. Although IGBTs have weak switching performance, they can withstand high voltages due to their special bipolar structure, and the conductivity modulation effect under high currents will also reduce the internal resistance of the device, resulting in better static performance. However, with the continuous development of society, many markets are moving towards higher voltage and more efficient technology, such as new energy vehicles, photovoltaic energy storage, charging piles, etc., which has increasingly stringent requirements for power devices, and traditional Si-based devices can no longer meet these usage requirements.
[0003] As a typical product of the third generation wide bandgap semiconductor devices, SiC MOSFET has many advantages in performance, such as high withstand voltage, low conduction loss, high switching frequency, and low thermal resistance. Therefore, it is considered to be the main product in the future high voltage and high power field. However, in addition to the high cost of SiC, the quality of the gate oxide layer formed by direct growth of SiC MOSFET by thermal oxidation has always been a major problem. Since the gate oxide layer SiO2 grown on the SiC material is rich in many defects, such as clusters and vacancies, it will easily cause field concentration and breakdown failure in the long-term use of the device if the design is improper. Therefore, it is crucial to better protect the gate oxide layer and improve the long-term reliability of the gate oxide layer. Summary of the invention
[0004] In view of the above problems, the present invention provides a SiC MOSFET device and a preparation method for better protecting the gate oxide, which can reduce the voltage stress on the gate oxide layer, protect the gate oxide layer, and shield the electric field concentration generated by the drain voltage.
[0005] The technical solution of the present invention is: A method for preparing a SiC MOSFET device with better gate oxide protection comprises the following steps: S100, forming a SiC Drift layer and a JFET region on the SiC Sub layer; S200, forming a P-body region, a NP region and a PP region in sequence on the top surface of the JFET region by an ion implantation process; and completely forming the JFET region, the P-body region, the NP region and the PP region implantation regions by high temperature ion activation; S300, sputtering an ohmic contact layer on the top surface of the PP region in the JFET region; and growing a gate oxide layer on the side of the ohmic contact layer by dry oxygen oxidation; S400, forming a Poly layer by a polycrystalline silicon Poly deposition method, which serves as a gate electrode of the device; S500, forming an isolation dielectric layer by depositing an oxide layer, which serves as a dielectric to prevent a short circuit between a gate electrode and a source electrode of the device; S600, forming a source ohmic contact layer on the top surfaces of the NP region and the PP region by sputtering Ni metal; finally, forming a front electrode metal layer on the top of the device by sputtering metal.
[0006] Specifically, in step S100, the bottom depth of the JFET region is 1.2um-2um, and the doping concentration is 5E16-1E18cm -2 .
[0007] Specifically, the bottom depth of the P-body region in step S200 is 0.8um-1.2um, and the doping concentration is 1E17-3E18cm -2 .
[0008] Specifically, the bottom depth of the NP region in step S200 is 0.3um-0.6um, and the doping concentration is 1E18-1E19cm -2 .
[0009] Specifically, the bottom depth of the PP region in step S200 is 0.4um-0.8um, and the doping concentration is 1E18-1E19cm -2 .
[0010] Specifically, the thickness of the ohmic contact layer in step S300 is 0.1 um-0.5 um.
[0011] Specifically, the thickness of the gate oxide layer in step S300 is 30 nm-70 nm.
[0012] Specifically, the thickness of the Poly layer in step S400 is 0.5um-1.2um.
[0013] A SiC MOSFET device with better gate oxide protection, comprising a SiC Sub layer, a SiCDrift layer and a JFET region arranged in sequence from bottom to top; The JFET region is provided with: A P-body region extending downward from the top surface of the JFET region; a depth of the P-body region is less than a depth of the JFET region; The NP region extends downward from the top surface of the P-body region and is spaced apart from the bottom surface of the P-body region; that is, the depth of the P-body region is greater than the depth of the NP region; PP regions are formed in the middle of the JFET region and in the P-body region respectively; the PP region in the P-body region extends downward from the top surface of the NP region and is connected thereto; An ohmic contact layer is formed on the top surface of the PP region in the JFET region; Gate oxide layers are formed on the top surfaces of the NP region, the P-body region and the PP region respectively; A Poly layer, formed on the top surface of the gate oxide layer and the ohmic contact layer; The isolation dielectric layer is wrapped on the gate oxide layer and the Poly layer, the bottom surface of which is connected to the NP region, and the top surface of which is provided with a front electrode metal layer connected thereto.
[0014] In order to better protect the gate oxide layer of SiC MOSFET, the present invention forms a heavily doped PP region by ion implantation into the SiC Drift layer at the middle bottom of the device gate, and realizes ohmic contact on the top surface of the PP region through preparation, so that the gate Poly layer is connected to the PP region. The advantage brought by this is that when the gate Poly layer is subjected to a driving voltage, the PP region can release a part of the gate driving voltage stress, thereby reducing the voltage stress on the gate oxide layer, and protecting the gate oxide layer to a certain extent. In the device blocking process, the PP region can shield the electric field concentration generated by the drain voltage because it is at the bottom of the gate, thereby protecting the gate oxide layer again. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 Schematic diagram of the structure of SiC MOSFET of the present invention; Figure 2 is a structural schematic diagram of step S100 of the present invention; Figure 3 is a schematic structural diagram of step S200 of the present invention; Figure 4 is a schematic structural diagram of step S300 of the present invention; Figure 5 is a structural schematic diagram of step S400 of the present invention; Figure 6 is a schematic structural diagram of step S500 of the present invention; Figure 7 is a schematic structural diagram of step S700 of the present invention; Figure 8 is a structural schematic diagram of step S800 of the present invention; Fig. 9 is a structural schematic diagram of step S900 of the present invention; Fig.10 is a structural schematic diagram of step S1000 of the present invention; Fig.11 is a schematic diagram of the structure of step S1100 of the present invention; In the figure, 1 is SiC Sub layer, 2 is SiCDrift layer, 3 is JFET region, 4 is P-body region, 5 is NP region, 6 is PP region, 7 is ohmic contact layer, 8 is gate oxide layer, 9 is Poly layer, 10 is isolation dielectric layer, 11 is source ohmic contact layer, and 12 is front electrode metal layer. DETAILED DESCRIPTION
[0016] The present invention is described in detail below in conjunction with specific practical cases. Examples of the embodiments are shown in the accompanying drawings, and the schematic implementation methods of the present invention and their descriptions are only used to explain the present invention and are not intended to limit the present invention.
[0017] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0018] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0019] A method for preparing a SiC MOSFET device with better gate oxide protection comprises the following steps: S100, epitaxially growing a SiC Drift layer 2 on the SiC Sub layer 1; Figure 2 As shown; S200, a JFET region 3 is initially formed on the top surface of the SiC Drift layer 2 by oblique N ion implantation; Figure 3 As shown; The bottom depth of JFET region 3 in step S200 is 1.2um-2um, and the doping concentration is 5E16-1E18cm -2 .
[0020] S300, a P-body region 4 is initially formed on the top surface of the JFET region 3 by oblique Al ion implantation; Figure 4 As shown; The bottom depth of the P-body region 4 in step S300 is 0.8um-1.2um, and the doping concentration is 1E17-3E18cm -2 .
[0021] S400, the NP region 5 is initially formed on the top surface of the P-body region 4 by oblique N ion implantation; Figure 5 As shown; The bottom depth of the NP region 5 in step S400 is 0.3um-0.6um, and the doping concentration is 1E18-1E19cm -2 .
[0022] S500, a PP region 6 is initially formed on the top surface of the JFET region 3 and the P-body region 4 by oblique Al ion implantation; Figure 6 As shown; The bottom depth of the PP region 6 in step S500 is 0.4um-0.8um, and the doping concentration is 1E18-1E19cm -2 .
[0023] S600, the JFET region 3, the P-body region 4, the NP region 5 and the PP region 6 implantation regions are completely formed by high temperature ion activation; The high temperature activation annealing temperature in step S600 is between 1600°C and 1900°C.
[0024] S700, forming an ohmic contact layer 7 on the top surface of the PP region 6 in the JFET region 3 by sputtering Ni metal and then thermal annealing; Figure 7 As shown; The Ni metal thickness in step S700 is 0.1um-0.5um.
[0025] S800, a gate oxide layer 8 is grown on the top surfaces of the JFET region 3, the P-body region 4 and the NP region 5 by dry oxygen oxidation; Figure 8 As shown; The thickness of the gate oxide layer 8 in step S800 is between 30 nm and 70 nm.
[0026] S900, forming a Poly layer 9 on the top surface of the ohmic contact layer 7 and the gate oxide layer 8 by polysilicon Poly deposition, which is used as the gate electrode of the device; Fig. 9 As shown; The thickness of the Poly layer 9 in step S900 is 0.5um-1.2um.
[0027] S1000, an isolation dielectric layer 10 is formed on the top surface of the NP region 5 and the Poly layer 9 by depositing an oxide layer, and is used as a dielectric to prevent the gate electrode and the source electrode of the device from being short-circuited; Fig.10 As shown; S1100, a source ohmic contact layer 11 is formed on the top surface of the NP region 5 and the PP region 6 by sputtering Ni metal and then thermally annealing; Fig.11 As shown; The Ni metal thickness in step S1100 is 0.1um-0.5um.
[0028] S1200, forming a front electrode metal layer 12 on the top of the device by sputtering Ti / AlCu metal. Figure 1 shown.
[0029] In the Ti / AlCu in step S1200, the thickness of the Ti metal is 0.1um-0.3um, and the thickness of the AlCu metal is 3um-5um.
[0030] A SiC MOSFET device with better gate oxide protection includes a SiC Sub layer 1, a SiC Drift layer 2 and a JFET region 3 arranged in sequence from bottom to top; The JFET region 3 is provided with: The P-body region 4 extends downward from the top surface of the JFET region 3 and is spaced apart from the bottom surface of the JFET region 3; that is, the depth of the P-body region 4 is less than the depth of the JFET region 3; The NP region 5 extends downward from the top surface of the P-body region 4 and is spaced apart from the bottom surface of the P-body region 4; that is, the depth of the P-body region 4 is greater than the depth of the NP region 5; PP region 6, respectively formed in the middle of the JFET region 3 and in the P-body region 4; the PP region 6 in the P-body region 4 extends downward from the top surface of the NP region 5 and is connected thereto; the depth of the PP region 6 is greater than the depth of the NP region 5; An ohmic contact layer 7 is formed on the top surface of the PP region 6 in the JFET region 3; A gate oxide layer 8 is formed on the top surfaces of the NP region 5, the P-body region 4 and the PP region 6 respectively; A Poly layer 9 formed on the top surface of the gate oxide layer 8 and the ohmic contact layer 7; The isolation dielectric layer 10 is wrapped on the gate oxide layer 8 and the Poly layer 9, the bottom surface of which is connected to the NP region 5, and the top surface of which is provided with a front electrode metal layer 12 connected thereto.
[0031] In order to better protect the gate oxide layer of SiC MOSFET, the present invention forms a heavily doped PP region 6 by ion implantation into the SiC Drift layer 2 at the middle bottom of the device gate, and realizes ohmic contact 7 on the top surface of the PP region 6 by preparation, so that the gate Poly layer is connected to the PP region 6. The benefit brought by this is that when the gate Poly layer is driven by voltage, the PP region 6 can release part of the gate drive voltage stress, thereby reducing the voltage stress on the gate oxide layer, and protecting the gate oxide layer to a certain extent. In the device blocking process, the PP region 6 can shield the electric field concentration generated by the drain voltage because it is at the bottom of the gate, and protect the gate oxide layer again.
Claims
1. A method for preparing a SiC MOSFET device with better gate oxide protection, characterized in that: The steps include: S100, forming a SiC Drift layer (2) and a JFET region (3) on the SiC Sub layer (1); S200, forming a P-body region (4), a NP region (5) and a PP region (6) in sequence on the top surface of the JFET region (3) by an ion implantation process; and completely forming the implanted regions of the JFET region (3), the P-body region (4), the NP region (5) and the PP region (6) by high temperature ion activation; S300, sputtering an ohmic contact layer (7) on the top surface of the PP region (6) in the JFET region (3); and growing a gate oxide layer (8) on the side of the ohmic contact layer (7) by dry oxygen oxidation; S400, forming a Poly layer (9) by a polycrystalline silicon Poly deposition method, which serves as a gate electrode of the device; S500, forming an isolation dielectric layer (10) by an oxide layer deposition method, as a dielectric to prevent a short circuit between a gate electrode and a source electrode of a device; S600, forming a source ohmic contact layer (11) on the top surface of the NP region (5) and the PP region (6) by Ni metal sputtering; finally, forming a front electrode metal layer (12) on the top of the device by metal sputtering.
2. A method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: In step S100, the bottom depth of the JFET region (3) is 1.2um-2um.
3. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: The bottom depth of the P-body region (4) in step S200 is 0.8um-1.2um, and the doping concentration is 1E17-3E18cm -2 .
4. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: The bottom depth of the NP region (5) in step S200 is 0.3um-0.6um, and the doping concentration is 1E18-1E19cm -2 .
5. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: The bottom depth of the PP region (6) in step S200 is 0.4um-0.8um, and the doping concentration is 1E18-1E19cm -2 .
6. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: The thickness of the ohmic contact layer (7) in step S300 is between 0.1 um and 0.5 um.
7. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: In step S100, the doping concentration of the JFET region (3) is 5E16-1E18cm -2 .
8. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: The thickness of the gate oxide layer (8) in step S300 is between 30 nm and 70 nm.
9. The method for preparing a SiC MOSFET device with better gate oxide protection according to claim 1, characterized in that: The thickness of the Poly layer (9) in step S400 is between 0.5um and 1.2um.
10. A SiC MOSFET device with better gate oxide protection, prepared by the method for preparing a SiC MOSFET device with better gate oxide protection according to any one of claims 1 to 9, characterized in that: It includes a SiC Sub layer (1), a SiC Drift layer (2) and a JFET region (3) which are arranged in sequence from bottom to top; The JFET region (3) is provided with: A P-body region (4) extending downward from the top surface of the JFET region (3); a depth of the P-body region (4) is less than a depth of the JFET region (3); The NP region (5) extends downward from the top surface of the P-body region (4) and is spaced apart from the bottom surface of the P-body region (4); that is, the depth of the P-body region (4) is greater than the depth of the NP region (5); PP regions (6) are formed in the middle of the JFET region (3) and in the P-body region (4) respectively; the PP region (6) in the P-body region (4) extends downward from the top surface of the NP region (5) and is connected thereto; An ohmic contact layer (7) formed on the top surface of the PP region (6) in the JFET region (3); A gate oxide layer (8) is formed on the top surfaces of the NP region (5), the P-body region (4) and the PP region (6) respectively; A Poly layer (9) formed on the top surface of the gate oxide layer (8) and the ohmic contact layer (7); An isolation dielectric layer (10) is wrapped on the gate oxide layer (8) and the Poly layer (9), the bottom surface of which is connected to the NP region (5), and the top surface of which is provided with a front electrode metal layer (12) connected thereto.