Combined large-scale reaction sintering silicon carbide ceramic impeller
Through modular design and structural optimization, the problems of low yield and poor impact resistance of large reaction-sintered silicon carbide ceramic impellers have been solved, achieving efficient manufacturing and cost reduction.
Patent Information
- Application Number
- CN202420878775.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-25
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-25
AI Technical Summary
Existing technologies make it difficult to manufacture large reaction-sintered silicon carbide ceramic impellers, resulting in low yield, poor impact resistance, and high cost.
The design employs a modular approach, dividing the reaction-sintered silicon carbide ceramic impeller into multiple alternating components. It incorporates cavity and skeleton structures, optimizes the splicing line and sealing cone surface, and reduces residual stress and blank density differences.
This improved the yield and impact resistance of large reaction-sintered silicon carbide ceramic impellers, reduced manufacturing costs, and enhanced overall strength and reliability.
Smart Images

Figure CN222067166U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of functional ceramic materials, and more specifically relates to a combined large-scale reaction-sintered silicon carbide ceramic impeller. Background Art
[0002] The impeller of a slurry pump is the most severely worn component of a slurry pump, and is generally made of wear-resistant alloy or wear-resistant rubber. However, in some working conditions with severe wear, wear-resistant alloy impellers and wear-resistant rubber impellers often cannot meet the use requirements. In order to increase the life of the impeller, silicon carbide ceramic materials with good wear resistance are currently being tried to be used to make the impeller. Depending on the process and raw materials, common silicon carbide ceramics mainly include pressureless sintered silicon carbide, hot-pressed sintered silicon carbide, reaction-sintered silicon carbide, silicon nitride combined with silicon carbide, and oxide combined with silicon carbide. Among them, pressureless sintered silicon carbide and hot-pressed sintered silicon carbide can only manufacture some simple-shaped workpieces due to the complex molding and sintering processes, and cannot manufacture complex large parts such as slurry pump impellers; the latter three can be formed by casting or grouting processes, so they can manufacture workpieces with complex shapes. At present, almost all silicon carbide ceramic impellers are made of the latter three materials.
[0003] Silicon nitride bonded with silicon carbide and oxide bonded with silicon carbide can be cast, which is easy to manufacture workpieces with complex shapes such as impellers. The basic production process of silicon nitride bonded with silicon carbide and oxide bonded with silicon carbide is: mix α-SiC particles with metal silicon powder, binder, water, etc. evenly, inject into the mold for molding, demold and dry; heat the blank to 1420℃ under high-purity nitrogen, then the metal silicon powder and nitrogen in the blank react to form silicon nitride, and finally obtain silicon nitride bonded with silicon carbide; place the blank in oxygen or air and heat to 1420℃, then the metal silicon powder and oxygen in the blank react to form silicon oxide, and finally obtain oxide bonded with silicon carbide. The porosity of silicon nitride bonded with silicon carbide is generally 8%-15%, and the α-Si C content is generally 65%-80%. The flexural strength is generally 30-60Mpa. The porosity of oxide bonded with silicon carbide is generally 15%-20%, and the α-Si C content is generally 75%-85%. The flexural strength is generally 20-30Mpa.
[0004] Reaction-bonded silicon carbide ceramics generally refer to reaction-bonded silicon carbide. There is also reaction-formed silicon carbide, sometimes also called reaction-bonded silicon carbide, that is, the material is all β-SiC generated by carburization reaction, but this material has poor processability and high cost, and there is no report of its commercial application in manufacturing impellers. When manufacturing workpieces with complex shapes such as impellers, they are all reactively bonded silicon carbide, and grouting molding is generally used. The manufacturing process is: raw materials containing α-SiC micropowder and carbon black micropowder are mixed with water, binders, dispersants, etc. to form a slurry, which is then injected into the cavity of a gypsum mold (or other water-absorbing mold). The gypsum mold absorbs the water in the slurry. After the slurry loses some of its moisture, the binder gives the blank a certain strength. The gypsum mold is removed to obtain the blank. After the ceramic blank is dried, the blank and excess metal silicon particles are stacked in a reaction sintering furnace, and the temperature is raised to about 800°C in a vacuum or inert gas. The binder and dispersant are completely carbonized. The temperature is further raised to 1500-1700°C, and the metal silicon is liquefied or vaporized. Under the action of capillaries, it penetrates into the blank and reacts with the carbon in the blank to form β-SiC, and the α-SiC in the blank is formed. C powder is combined together, and the excess metallic silicon fills the pores in the blank at the same time. After cooling, a ceramic material with very low porosity (generally less than 0.1%) is obtained, and the main components are silicon carbide (generally α-SiC+β-SiC content is 85-93%) and free silicon (also called residual silicon, generally 7-15%). Reaction-sintered silicon carbide not only has much higher wear resistance than silicon nitride combined with silicon carbide and oxide combined with silicon carbide, but also has much higher mechanical strength than the latter two. Generally, the bending strength can reach 250-500Mpa. Therefore, the impeller made of reaction-sintered silicon carbide ceramic impeller material should be significantly better than that of silicon nitride combined with silicon carbide and oxide combined with silicon carbide in terms of wear resistance and strength. However, the actual situation is not the case. The impeller using the latter two materials can currently achieve a diameter of about 1700mm, and its reliability can meet the use requirements. The reaction-sintered silicon carbide impeller manufactured by conventional technology can only achieve a diameter of about 500mm; for example, China's authorized utility model patent (authorization announcement number is CN209687784U) discloses "an integral ceramic impeller". At present, some models of reaction-sintered silicon carbide ceramic impellers manufactured according to this technical solution have been put into commercial use. However, the current successful market use is limited to some small models and their diameters generally do not exceed 500mm. When manufacturing reaction-sintered silicon carbide impellers with larger diameters, it is found that the yield rate is very low, which leads to a sharp increase in costs, and the manufactured impellers have poor impact resistance. Not only are they prone to rupture when used under strong impact conditions, but the probability of rupture is also high under slight impact conditions.
[0005] In order to solve the problem that the impeller is difficult to enlarge, the Chinese authorized utility model patent (authorization announcement number is CN209687784U) also discloses another ceramic impeller. The utility model concept of this ceramic impeller is to split the large ceramic impeller into several easy-to-manufacture parts for separate manufacturing, and then splice these parts into one. In practice, it is found that when this technical solution is used to manufacture large impellers, if the ceramic material is silicon nitride combined with silicon carbide or oxide combined with silicon carbide, under the current process technology conditions, larger impellers can indeed be manufactured; the maximum impeller diameter can currently be about 1700mm; but if the ceramic material is reaction sintered silicon carbide, when the impeller is enlarged, especially when the impeller diameter exceeds 700mm, there are still problems that the impeller is easy to break and the yield is low, and the mechanical strength and reliability of the impeller are much lower than those of silicon nitride combined with silicon carbide impellers or oxide combined with silicon carbide impellers.
[0006] In view of the above problems, technicians naturally thought of increasing the thickness of impeller-related parts to improve the strength of the impeller. For example, the
[0063] paragraph in the Chinese authorized utility model patent (authorization announcement number CN209687784U) points out that increasing the thickness of the blades can improve the strength of the impeller. This is also consistent with the experience of ordinary technicians. Therefore, in the design, the thickness of the front cover plate, rear cover plate or blade of a large ceramic impeller is often designed to reach 70-120mm. Our further research found that this experience should be correct for other ceramics, such as silicon nitride combined with silicon carbide, oxide combined with silicon carbide, alumina ceramics, etc., and the expected effect can be obtained after thickening; but for reaction-sintered silicon carbide, this is not entirely true. In many cases, the reliability of the impeller after thickening has not been improved, and even many contrary cases have occurred. Through further calculations, it can be found that the theoretical strength of these reaction-sintered silicon carbide impellers that are broken during use is not only much greater than that of silicon nitride combined with silicon carbide or oxide combined with silicon carbide, but also the strength safety factor is much greater than the actual requirements of the impeller.
[0007] Through in-depth research on this phenomenon, it was found that for silicon nitride bonded silicon carbide ceramics and oxide bonded silicon carbide ceramics, due to the high porosity, these tiny pores can greatly reduce the internal stress generated during the ceramic sintering process and absorb the stress caused by external impact. Therefore, the residual stress of the workpiece is small. After the front cover plate, rear cover plate and blades of the impeller are thickened, the mechanical strength of the impeller can also be improved accordingly.
[0008] Through research, it is also found that: since reaction sintered silicon carbide is currently slurry-formed by gypsum mold or other water-absorbing mold, the surface of the workpiece is in contact with the mold during slurry injection, and the moisture in the slurry is quickly absorbed. However, the moisture in the part far from the mold inside the workpiece is significantly higher than the surface of the workpiece at the end of molding due to the relatively weak capillary action of the mold, which makes the density of the surface of the blank after drying significantly higher than the inside of the blank. After the carbonization reaction is completed during sintering, the excess metal silicon liquid will fill the gaps between the silicon carbides, so that the free silicon content of the part with higher density of the blank after sintering will be lower than that of the part with lower density of the blank, that is, the free silicon content of the workpiece surface will be lower than that of the inside of the workpiece. According to the normal process of the prior art, the free silicon content of the surface can be controlled at 8-12%, and the farther away from the surface, the higher the free silicon content, and the free silicon content of the core can reach 15-18%. Free silicon not only reduces wear resistance and bending strength, but more importantly, it increases the brittleness of the ceramic and reduces impact resistance. Therefore, in production, efforts are generally made to increase the density of the blank to reduce the free silicon content of the product. However, in production practice, improving the density of the blank is restricted by various factors, and the existing gypsum mold grouting molding technology is difficult to significantly improve the density and consistency of the blank. Therefore, for impellers with smaller diameters, such as impellers with a diameter of 500mm, the thickness of the blades and cover plates generally does not exceed 50mm. At this time, appropriately increasing the thickness of the blades or cover plates has a relatively small effect on the density of the impeller blank, which is an important reason for the relatively high reliability of small reaction-sintered silicon carbide impellers. However, for large impellers, for strength and wear resistance considerations, the thickness of the blades and cover plates is often designed to be 80-120mm. At this time, the density of the cast impeller blank is quite different, which will lead to large differences in the microstructure of the ceramic organization after sintering. In some cases, the so-called silicon core even appears, and the free silicon content in the center is close to 100%, which will cause the workpiece to produce large residual stress when cooling after sintering; the greater the thickness of the workpiece and the larger the outer dimensions, the greater the residual stress. Unlike silicon nitride bonded silicon carbide or oxide bonded silicon carbide ceramics which have a large number of pores, the porosity of reaction-sintered silicon carbide ceramics is close to zero, so the stress generated by sintering cannot be eliminated through the pores. Therefore, for thicker workpieces, under the same external dimensions, the residual stress of reaction-sintered silicon carbide workpieces is much greater than that of silicon nitride bonded silicon carbide and oxide bonded silicon carbide. On the one hand, the larger residual stress causes the workpiece to break or produce hidden cracks during the sintering process, which reduces the yield of the product. On the other hand, it causes the workpiece to have a larger residual stress, which is easy to break from the part with greater stress when subjected to external force or impact. Therefore, for reaction-sintered silicon carbide impellers, increasing the thickness of the blades or cover plates does not necessarily increase the strength and impact resistance of the impeller, and sometimes it may even be counterproductive.
[0009] Therefore, through the above research, it is found that the main or important reason why the existing technology cannot achieve large-scale and high reliability of reaction-sintered silicon carbide ceramic impellers is precisely the key to solving the problem. Utility Model Content
[0010] In order to solve the deficiencies and shortcomings of the prior art, the purpose of the utility model is to provide a combined large-scale reaction-sintered silicon carbide ceramic impeller.
[0011] The technical solution of the utility model for solving the problems of the prior art is:
[0012] A combined large-scale reaction-sintered silicon carbide ceramic impeller is formed by splicing together a number of components including a plurality of ceramic impeller bodies made of reaction-sintered silicon carbide; the ceramic impeller body is divided into a first ceramic impeller body and a second ceramic impeller body, wherein the first ceramic impeller body and the second ceramic impeller body are alternately arranged in a circumferential direction; wherein a first blade plate is provided on the first ceramic impeller body, and a second blade plate is provided on the second ceramic impeller body; when the first ceramic impeller body and the second ceramic impeller body are spliced together, the first blade plate and the second blade plate are spliced together to form a blade; a first cavity is provided in the blade, and the first cavity extends along the working surface of the blade toward the impeller outlet direction of the ceramic impeller body; the splicing line between adjacent first ceramic impeller bodies and second ceramic impeller bodies passes through the first cavity.
[0013] Preferably, the ceramic impeller body includes a front plate, a rear plate, a first blade plate or a second blade plate sintered into one piece, wherein after the first ceramic impeller body and the second ceramic impeller body are assembled, the first blade plate in the first ceramic impeller body, the second blade plate in the second ceramic impeller body, the front plate and the rear plate are assembled to form a channel; and the two ends of the channel are respectively connected to the impeller suction port and the impeller outlet in the ceramic impeller body.
[0014] Preferably, the extension length of the first cavity along the working surface of the blade toward the impeller outlet direction of the ceramic impeller body is 25%-80% of the blade length; through the above setting, when the extension length of the first cavity is too long, the length of the first cavity from the head or tail of the blade will be too short, and the wear resistance of the blade is poor; on the contrary, there are more areas with larger thickness on the blade, the density difference of the cast blank is large, the residual silicon amount in the sintered ceramic impeller body is large, the residual internal stress is large, and the probability of impeller rupture is high. According to the size of the impeller and the shape of the blade, when the length of the first cavity is set to 25%-80% of the blade length, the above contradiction can be better balanced. When a suitable adhesive is selected to fill the first cavity, the strength of the blade will not be affected by the provision of the first cavity.
[0015] Preferably, the splicing line between the adjacent first ceramic impeller body and the second ceramic impeller body is composed of a first splicing line, a second splicing line and a third splicing line, wherein the first splicing line passes through the tail of the first cavity and the tail of the blade; the second splicing line passes through the head of the first cavity and the working surface or back surface of the blade; the third splicing line is the splicing line between the second ceramic impeller body and the first ceramic impeller body; wherein the distance between the second splicing line from the working surface or back surface of the impeller to the head of the blade is 1-2 times the average thickness of the blade.
[0016] Since the blade head is the part of the entire impeller that is most severely impacted and worn, when the second splicing line of the adjacent first ceramic impeller body and the second ceramic impeller body passes through the head of the first cavity and the back side or working surface of the blade, the second splicing line can be avoided from passing through the blade head, thereby preventing the life of the blade head from being significantly reduced due to the provision of the second splicing line. At the same time, the length of the splicing line exposed in the flow channel can also be significantly reduced, thereby reducing the efficiency reduction caused by splicing errors or wear at the splicing points.
[0017] If the distance between the second splicing line on the back side or working surface of the blade and the blade head is small, the blade head will wear rapidly due to the second splicing line after it is worn to the splicing line. On the contrary, if the distance between the second splicing line on the back side or working surface of the blade and the blade head is large, a thicker and longer part will be formed on the blade head, resulting in a large difference in the density of the resulting blank and a large residual stress after sintering, thereby reducing the impact resistance of the impeller. According to the shape or size of the blade, when the distance from the second splicing line on the back side or working surface of the blade to the blade head is set to 1-2 times the average thickness of the blade, the above contradiction can be better balanced.
[0018] The first joint line between the adjacent first ceramic impeller body and the second ceramic impeller body passes through the tail of the first cavity and the tail of the blade, which can make the length of the joint line between the adjacent first ceramic impeller body and the second ceramic impeller body that is washed as short as possible, which is beneficial to reducing the wear of the impeller and improving the efficiency of the impeller.
[0019] Preferably, the first blade plate of the first ceramic impeller body is provided with a protrusion at its head position, and the head of the second blade plate of the second ceramic impeller body adjacent to the first ceramic impeller body after splicing is arranged at the rear end of the protrusion; or, the second blade plate of the second ceramic impeller body is provided with a protrusion at its head position, and the head of the first blade plate of the first ceramic impeller body adjacent to the second ceramic impeller body after splicing is arranged at the rear end of the protrusion. Through the above arrangement, the protrusion provided on the first blade plate can protect the head of the second blade plate, preventing the head of the second blade plate at the splicing line from being quickly worn, and vice versa.
[0020] Preferably, a first mounting groove is provided on the front plate of the first ceramic impeller body, and a second mounting groove is provided on the front plate of the second ceramic impeller body; when the first ceramic impeller body and the second ceramic impeller body are assembled, the first mounting groove and the second mounting groove are assembled to form a second cavity; a front lining plate and a second skeleton are installed in the second cavity, wherein the second skeleton is arranged between the front lining plate and the first ceramic impeller body or the second ceramic impeller body.
[0021] Since the front cover plates of large impellers are relatively thick, often reaching 60mm-100mm, for large ceramic impellers with thicker front cover plates, if the second cavity is not set, the thickness of the front cover plate will be significantly higher than the blades or rear cover plates, resulting in a large difference in the density of the blank after grouting, and a large residual stress will be generated after sintering, increasing the probability of hidden cracks or ruptures in the ceramic impeller body and reducing the impact resistance of the impeller. After setting the second cavity, the thickness of the ceramic impeller body on the front cover plate can be reduced, thereby reducing the residual stress of the ceramic impeller body. Since the bending strength of reaction-sintered silicon carbide ceramic material is very high, the theoretical strength of large ceramic impellers designed according to the prior art is already much higher than the actual needs, but in actual use, the main reason for the low reliability of large impellers is that it is difficult to consider the influence of residual stress in theoretical calculations, and this factor has a great influence on the results. After the front liner and the ceramic impeller body are bonded, on the one hand, the residual stress at the front cover plate is significantly reduced due to the thickness reduction. On the other hand, the probability of the hidden cracks at the front cover plate of the ceramic impeller body overlapping with the hidden cracks and stress concentration parts on the front liner is very low, so that the transmission of residual stress can be blocked, and the influence of residual stress on the strength of the impeller is much smaller. Therefore, after the front liner and the second cavity are set, although the theoretical mechanical strength of the ceramic impeller body will be reduced, the theoretical mechanical strength calculation cannot consider the influence of residual stress, and the filling adhesive reinforces the first cavity. Therefore, the actual reliability of the ceramic impeller body of the utility model is significantly improved compared with the scheme without the first cavity, and its impact resistance is also significantly improved. In addition, another function of setting the front liner is to cover the joint line between the ceramic impeller bodies to prevent the adhesive in the joint line from being quickly worn and causing damage to the impeller.
[0022] Preferably, the ceramic impeller body is provided with a sealing cone surface at the position of the impeller suction port, and the distance from the inner edge of the second cavity to the outer edge of the sealing cone surface is 5mm-50mm. The cavitation resistance of the impeller can be improved by providing a sealing cone surface at the impeller suction port. The cone angle of the sealing cone surface is generally 10°-30°. If the second cavity is not provided, the front liner and the ceramic impeller body will be spliced on the sealing cone surface, so that the front liner will be a sharp angle at the splicing line position, which greatly reduces its wear resistance and impact resistance. If the distance between the inner edge of the second cavity and the outer edge of the sealing cone surface is set to 5mm-60mm, the above-mentioned sharp angle splicing problem can be prevented, and at the same time, the excessive thickness of the ceramic impeller body at the sealing cone surface portion can be avoided to form a large residual stress.
[0023] Preferably, a first skeleton is arranged in the first cavity; a third mounting groove is arranged on the rear plate of the first ceramic impeller body, and a fourth mounting groove is arranged on the rear plate of the second ceramic impeller body; when the first ceramic impeller body and the second ceramic impeller body are assembled, the third mounting groove and the fourth mounting groove are assembled to form a third cavity; a third skeleton is installed in the third cavity; the first skeleton and the third skeleton are connected; a third cavity for accommodating the third skeleton is arranged on the impeller driving side, which is formed by alternately assembling the first ceramic impeller body and the second ceramic impeller body, so that the area of the ceramic impeller body in the third cavity is much smaller than the area of the rear plate, so that the residual stress of the ceramic impeller body can be reduced, and after being bonded into one with the third skeleton and the rear lining plate, the probability of the impeller breaking due to impact can be further reduced.
[0024] Preferably, the first cavity, the second cavity and the third cavity are interconnected; through the above arrangement, the first cavity, the second cavity and the third cavity penetrate each other, and when the adhesive therein hardens, a high-strength organic skeleton that penetrates most of the impeller and completely fits the impeller and has a certain toughness can be formed, thereby enhancing the overall strength of the impeller. If it is combined with a metal skeleton, the strength can be even higher.
[0025] Compared with the prior art, the utility model has the following beneficial effects:
[0026] 1. The combined large-scale reaction-sintered silicon carbide ceramic impeller of the utility model is formed by alternately splicing a plurality of first ceramic impeller bodies and second ceramic impeller bodies made of reaction-sintered silicon carbide, so that the outer dimensions of the ceramic impeller body are significantly smaller than the dimensions of the silicon carbide ceramic impeller, which is conducive to reducing the manufacturing difficulty of the combined large-scale reaction-sintered silicon carbide ceramic impeller of the utility model, and can improve the yield rate and reduce the manufacturing cost.
[0027] 2. The first ceramic impeller body and the second ceramic impeller body in the combined large-scale reaction-sintered silicon carbide ceramic impeller of the utility model are alternately spliced; wherein, the first ceramic impeller body and the adjacent second ceramic impeller body are spliced into blades at the splicing point, so that the thickness of the first ceramic impeller body and the second ceramic impeller body at the blade part can be significantly smaller than the blade, thereby reducing the density difference of the blank at the blade part, making the residual silicon content in the ceramic impeller body after sintering relatively uniform, and the residual internal stress is small, thereby reducing the probability of cracking of the ceramic impeller body.
[0028] 3. A first cavity is provided in the blades of the combined large-scale reaction-sintered silicon carbide ceramic impeller of the utility model, and the splicing line between the adjacent first ceramic impeller body and the second ceramic impeller body passes through the first cavity, so that the thickness of the working surface blade and the back surface can be adjusted as needed, thereby further reducing the residual stress of the blade after sintering. At the same time, since the splicing line passing through the first cavity does not contact the medium, it will not be worn, so it can prevent the impeller life from being greatly reduced due to the poor wear resistance of the joint line.
[0029] 4. The first ceramic impeller body and the second ceramic impeller body on the adjacent side of the combined large-scale reaction-sintered silicon carbide ceramic impeller of the utility model are assembled to form a channel, and the two ends of the channel are respectively connected to the impeller suction port and the impeller outlet. This assembly method can reduce the number or length of the joint seams in the flow channel, and reduce the efficiency reduction caused by too many or too long joint seams. At the same time, this structure can use gypsum molds for all molds when manufacturing the first ceramic impeller body and the second ceramic impeller body, without the need for lost foam, which can prevent the poor consistency of the blank density due to the lost foam's inability to absorb water or poor water absorption, and the large residual stress of the ceramic after sintering and poor impact resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is a cross-sectional view of the combined large-scale reaction-sintered silicon carbide ceramic impeller of the utility model in Example 1.
[0031] Figure 2 for Figure 1 Section view at AA.
[0032] Figure 3 This is a cross-sectional view of the ceramic impeller body after assembly in Example 1.
[0033] Figure 4 for Figure 3 Sectional view at BB.
[0034] Figure 5 This is a front view of the ceramic impeller body after assembly in Example 1.
[0035] Figure 6 This is a three-dimensional diagram of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 1 before being assembled.
[0036] Figure 7 It is a three-dimensional diagram of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 1 after being assembled.
[0037] Figure 8 It is a cross-sectional view of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 1 after being assembled at the center plane of the impeller outlet.
[0038] Fig. 9 for Figure 8 Section view at CC.
[0039] Fig.10 This is a three-dimensional diagram of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 1 before being assembled.
[0040] Fig.11 It is a three-dimensional diagram of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 1 after being assembled.
[0041] Fig.12 It is a cross-sectional view of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 1 after being assembled at the center plane of the impeller outlet.
[0042] Fig.13 for Fig.12 Sectional view at DD.
[0043] Fig.14 A cross-sectional view of the rear lining plate in Example 1
[0044] Fig.15 This is a cross-sectional view of Example 2.
[0045] Fig.16 for Fig.14 Cross-sectional view at EE.
[0046] Fig.17 This is a cross-sectional view of the ceramic impeller body of Example 2 after assembly.
[0047] Fig.18 It is a cross-sectional view of the ceramic impeller body of Example 2 at the center plane of the impeller outlet after being assembled.
[0048] Fig.19 It is a cross-sectional view of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 2 after being assembled.
[0049] Fig. 20 for Fig.18 Cross-sectional view at FF.
[0050] Fig.21 It is a cross-sectional view of the first ceramic impeller body and the adjacent second ceramic impeller body in Example 2 after being assembled at the center plane of the impeller outlet.
[0051] In the figure: 01-first ceramic impeller body, 02-second ceramic impeller body, 011-first blade plate, 021-second blade plate, 2-first skeleton, 3-hub, 4-third skeleton, 5-rear lining, 6-front lining, 7-joining line, 7A-first joint line, 7B-second joint line, 7C-third joint line, 8-second cavity, 9-second skeleton, 10-sealing cone, 11-first cavity, 12-protrusion, 13-channel, 14-third cavity. DETAILED DESCRIPTION
[0052] The present invention is further described in detail below in conjunction with embodiments and drawings, but the implementation manner of the present invention is not limited thereto.
[0053] Example 1
[0054] like Figure 1-Figure 14 As shown, the impeller diameter of the combined large reaction-sintered silicon carbide ceramic impeller of the utility model is 1435 mm, including a hub 3 and a ceramic impeller body made of reaction-sintered silicon carbide; in this embodiment, the number of blades is 5, so the number of the first ceramic impeller body 01 and the second ceramic impeller body 02 are also 5.
[0055] like Figure 8 , Fig. 9 , Fig.12 , Fig.13 As shown, a first blade plate 011 is provided on the first ceramic impeller body 01, and a second blade plate 021 is provided on the second ceramic impeller body 02; the first ceramic impeller body 01 and the second ceramic impeller body 02 are alternately spliced; the first blade plate 011 of the first ceramic impeller body 01 and the second blade plate 021 of the second ceramic impeller body 02 on the adjacent side are spliced into a blade at the splicing position, and a first cavity 11 is provided in the spliced blade, and the splicing line 7 between the adjacent first ceramic impeller bodies 01 and the second ceramic impeller bodies 02 passes through the first cavity 11.
[0056] like Figure 6 , Fig. 9As shown, the ceramic impeller body includes a front plate, a rear plate, a first blade plate 011 (arranged on the first ceramic impeller body 01) or a second blade plate 021 (arranged on the second ceramic impeller body 02) sintered into one piece, wherein after the first ceramic impeller body 01 and the second ceramic impeller body 02 are assembled, the first blade plate 011 in the first ceramic impeller body 01, the second blade plate 021 in the second ceramic impeller body 02, the front plate and the rear plate are assembled to form a channel 13, wherein the two ends of the channel 13 are respectively connected to the impeller suction port and the impeller outlet in the ceramic impeller body.
[0057] like Figure 2 , Figure 4 , Figure 5 , Fig.11 , Fig.12 As shown, the first cavity 11 extends along the direction of the blade working surface toward the impeller outlet of the ceramic impeller body.
[0058] like Fig.12 As shown, on the cross-section of the center plane of the impeller outlet (i.e., the distance from the plane to the front cover plate and the rear cover plate of the impeller outlet is the same), L1 is the longest length of the first cavity 11 in this plane, which is measured to be 475 mm; L2 is the longest dimension of the blade in this plane, which is measured to be 742 mm, i.e., the length of the first cavity 11 is 64.0% of the length of the blade.
[0059] The “front cover plate” described in this embodiment is a general term for the front side plate of the silicon carbide ceramic impeller of the present invention, including the front plate and the front lining plate 6; correspondingly, the “rear cover plate” described in this embodiment is a general term for the rear side plate of the silicon carbide ceramic impeller of the present invention, including the rear plate and the rear lining plate 5.
[0060] like Fig.12 As shown, the second splicing line 7B passes through the head of the first cavity 11 and the back of the blade, and the distance L3 from the back of the blade to the head of the blade is 159 mm, which is 1.34 times the average thickness of the blade.
[0061] like Figure 8 , Fig.12 As shown, the first blade plate 011 of the first ceramic impeller body 01 is provided with a protrusion 12 at the head, and the head of the second blade plate 021 of the adjacent second ceramic impeller body 02 after assembly is provided at the rear end of the protrusion 12 .
[0062] like Figure 1 , Figure 3 As shown, the impeller suction port is provided with a sealing cone surface 10, and the distance between the inner edge of the second cavity 8 and the outer edge of the sealing cone surface 10 is 5 mm.
[0063] like Figure 1As shown, a front liner 6 is disposed in the second cavity 8. The front liner 6 is made of pressureless sintered silicon carbide and is composed of 8 to 12 sectors assembled into a ring shape.
[0064] like Figure 1 As shown, a third cavity 14 for accommodating a third skeleton 4 is provided on the impeller driving side, and a rear liner 5 is provided on the outside of the third skeleton 14. The rear liner 5 is made of reaction-sintered silicon carbide and is composed of 8 to 12 sectors assembled into a ring.
[0065] like Figure 3 As shown, the depth h of the third cavity 14 is 15 mm, and the thickness H of the front cover plate is 60 mm, that is, the depth h of the third cavity 14 is 25% of the thickness H of the front cover plate.
[0066] like Figure 1 As shown, a first frame 2 is disposed in the first cavity 11 , and the first frame 2 and the third frame 4 are both made of carbon steel and are connected into a whole by welding.
[0067] like Figure 3 As shown, the first cavity 11, the second cavity 8 and the third cavity 14 are interconnected.
[0068] Example 2
[0069] like Figure 15-Figure 21 As shown, the combined large-scale reaction sintered silicon carbide ceramic impeller of the utility model has an impeller diameter of 1650mm, and its structure is similar to that of Example 1, except that:
[0070] like Fig.15 As shown, a second skeleton 9 made of carbon steel is also arranged in the second cavity 8 .
[0071] like Fig.16 As shown, the splicing line 7 between the adjacent first ceramic impeller body 01 and the second ceramic impeller body 02 is composed of a first splicing line 7A, a second splicing line 7B and a third splicing line 7C, wherein the first splicing line 7A passes through the tail of the first cavity 11 and the tail of the blade; the second splicing line 7B passes through the head of the first cavity 11 and the working surface or back surface of the blade; the third splicing line 7C is the splicing line between the second ceramic impeller body 02 and another adjacent first ceramic impeller body 01.
[0072] like Fig.21 As shown, the length of the first cavity 11 is 80% of the length of the blade.
[0073] like Fig.16 , Fig.18 , Fig.21As shown, the second joint line 7B passes through the head of the first cavity 11 and the working surface of the blade, and the distance L3 from the second joint line 7B on the working surface of the blade to the head of the blade is 1 times the average thickness of the blade.
[0074] like Fig.16 , Fig.18 , Fig.21 As shown, the second blade plate 021 of the second ceramic impeller body 02 is provided with a protrusion 12 at the head, and the head of the first blade plate 011 of the adjacent first ceramic impeller body 01 after assembly is arranged at the rear end of the protrusion 12 .
[0075] Example 3
[0076] This embodiment is substantially the same as Embodiment 1, and the main differences are:
[0077] A second frame 9 is arranged in the second cavity 8 .
[0078] The depth of the second cavity 8 is 45% of the total thickness of the front cover plate.
[0079] The length of the first cavity 11 is 80% of the length of the blade.
[0080] The distance between the inner edge of the second cavity 8 and the outer edge of the sealing cone surface 10 is 50 mm.
[0081] The distance from the second joint line 7B on the back of the blade to the blade head is twice the average thickness of the blade.
[0082] Example 4
[0083] This embodiment is substantially the same as Embodiment 1, and the main differences are:
[0084] The length of the first cavity 11 is 30% of the length of the blade.
[0085] The distance between the inner edge of the second cavity 8 and the outer edge of the sealing cone surface 10 is 40 mm.
[0086] The distance from the second joint line 7B on the back of the blade to the blade head is 1.5 times the average thickness of the blade.
[0087] The above is a preferred implementation mode of the present invention, but the implementation mode of the present invention is not limited by the above content. Any other changes, modifications, substitutions, combinations, and simplifications that do not deviate from the spirit and principle of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.
Claims
1. A combined large-scale reaction-sintered silicon carbide ceramic impeller, It is characterized in that It is composed of several parts including a plurality of ceramic impeller bodies made of reaction-sintered silicon carbide; the ceramic impeller body is divided into a first ceramic impeller body and a second ceramic impeller body, wherein the first ceramic impeller body and the second ceramic impeller body are alternately arranged in a circumferential direction; wherein a first blade plate is arranged on the first ceramic impeller body, and a second blade plate is arranged on the second ceramic impeller body; when the first ceramic impeller body and the second ceramic impeller body are spliced together, the first blade plate and the second blade plate are spliced together to form a blade; a first cavity is arranged in the blade, and the first cavity extends along the working surface of the blade toward the impeller outlet direction of the ceramic impeller body; the splicing line between adjacent first ceramic impeller bodies and second ceramic impeller bodies passes through the first cavity.
2. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 1, It is characterized in that The extension length of the first cavity along the working surface of the blade toward the impeller outlet direction of the ceramic impeller body is 25%-80% of the length of the blade.
3. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 1, It is characterized in that The splicing line between the adjacent first ceramic impeller body and the second ceramic impeller body is composed of a first splicing line, a second splicing line and a third splicing line, wherein the first splicing line passes through the tail of the first cavity and the tail of the blade; the second splicing line passes through the head of the first cavity and the working surface or back surface of the blade; the third splicing line is the splicing line between the second ceramic impeller body and another adjacent first ceramic impeller body.
4. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 3, It is characterized in that The distance between the second joint line from the working surface or the back surface of the impeller to the head of the blade is 1-2 times the average thickness of the blade.
5. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 1, It is characterized in that The first blade plate of the first ceramic impeller body is provided with a protrusion at its head position, and the head of the second blade plate of the second ceramic impeller body adjacent to the first ceramic impeller body after splicing is arranged at the rear end of the protrusion; or, the second blade plate of the second ceramic impeller body is provided with a protrusion at its head position, and the head of the first blade plate of the first ceramic impeller body adjacent to the second ceramic impeller body after splicing is arranged at the rear end of the protrusion.
6. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 1, It is characterized in that A first mounting groove is arranged on the front plate of the first ceramic impeller body, and a second mounting groove is arranged on the front plate of the second ceramic impeller body; when the first ceramic impeller body and the second ceramic impeller body are assembled, the first mounting groove and the second mounting groove are assembled to form a second cavity; a front lining plate is installed in the second cavity.
7. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 6, It is characterized in that A second frame is also installed in the second cavity, and the second frame is arranged between the front lining plate and the first ceramic impeller body or the second ceramic impeller body.
8. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 6, It is characterized in that The ceramic impeller body is provided with a sealing cone surface at the position of the suction port thereof, and the distance from the inner edge of the second cavity to the outer edge of the sealing cone surface is 5mm-50mm.
9. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 7, It is characterized in that A first frame is disposed in the first cavity.
10. The combined large reaction-sintered silicon carbide ceramic impeller according to claim 9, It is characterized in that A third mounting groove is arranged on the rear plate of the first ceramic impeller body, and a fourth mounting groove is arranged on the rear plate of the second ceramic impeller body; when the first ceramic impeller body and the second ceramic impeller body are assembled, the third mounting groove and the fourth mounting groove are assembled to form a third cavity; a third skeleton is installed in the third cavity; the first skeleton and the third skeleton are connected; the first cavity, the second cavity and the third cavity are interconnected.
Citation Information
Cited By
Conveying pump
CN121452212A