By designing a bending layer and a deformation-resistant layer in the reflective lettering film, the bending piece with a wavy cross-section and the deformation-resistant block that abuts each other can be solved, and the pattern layer is realized effective protection and service life.
Patent Information
- Application Number
- CN202420434214.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-06
- Publication Date
- 2025-02-14
- Estimated Expiration
- 2034-03-06
AI Technical Summary
The reflective lettering film printed on clothing is prone to cracks due to folding during the clothing storage process, resulting in the pattern being lost or falling.
A deformation-resistant reflective lettering film is designed, by sequentially providing a protective layer, a pattern layer, a bending layer and a hot melt adhesive layer from the outside to the inside, wherein the bending layer includes a bending member extending along the length of the pattern layer. The cross-section of the bending-resistant member is wavy to enhance the load-bearing capacity, and a deformation-resistant layer is provided between the bending-resistant layer and the hot melt adhesive layer. The deformation-resistant layer is composed of deformation-resistant blocks that abut each other.
Through the design of the anti-bending layer and the anti-deforming layer, the load can be effectively offset when the bending force of the pattern layer is subjected to, prevent excessive bending and damage of the pattern layer, and prolong the service life of the lettering film.
Smart Images

Figure CN222482451U_ABST
Abstract
Description
Technical Field
[0001] The utility model discloses an anti-deformation reflective lettering film, belonging to the field of thin films. Background Art
[0002] Lettering film is a kind of retro-reflective material that has been made into a film and can be directly used. It is made using glass bead technology, micro-prism technology, synthetic resin technology, thin film technology, coating technology and micro-replication technology. Reflective lettering film is a kind of reflective lettering film, which is often used to print on clothing as decoration.
[0003] The lettering film patterns printed on clothing are often folded during the storage process. If the crease is located at the pattern position, the lettering film pattern will also bend and crack over time, eventually causing the pattern to fade or fall off.
[0004] In view of the above problems, a new improvement plan is proposed. Utility Model Content
[0005] The purpose of the utility model is to provide an anti-deformation reflective lettering film in order to solve the above problems.
[0006] The utility model achieves the above-mentioned purpose through the following technical scheme: a deformation-resistant reflective lettering film, which includes a protective layer, a pattern layer, an anti-bending layer and a hot-melt adhesive layer from the outside to the inside. The anti-bending layer includes an anti-bending part and an adhesive layer wrapping the anti-bending part, and the anti-bending part extends along the length direction of the pattern layer.
[0007] Preferably, the anti-bending member has a wavy cross-section.
[0008] Preferably, an anti-deformation layer is further provided between the anti-bending layer and the hot-melt adhesive layer, and the anti-deformation layer comprises a plurality of first anti-deformation blocks and second anti-deformation blocks abutting against each other, and the first anti-deformation blocks and the second anti-deformation blocks are wrapped with an adhesive layer.
[0009] Preferably, one side where the first anti-deformation block and the second anti-deformation block abut against each other is arc-shaped.
[0010] Preferably, the first anti-deformation block and the second anti-deformation block extend along the width direction of the pattern layer.
[0011] Preferably, a plurality of protrusions are formed on a side of the protection layer away from the pattern layer.
[0012] Preferably, micro-ridges are embedded in the protrusions.
[0013] Preferably, the anti-bending member, the first anti-deformation block and the second anti-deformation block are all made of silicone.
[0014] Compared with the prior art, the beneficial effects of the utility model are:
[0015] 1. By setting an anti-bending layer extending along the length direction of the pattern layer, and providing a wavy anti-bending part in the anti-bending layer, when subjected to bending force, the anti-bending part can offset most of the load, thereby ensuring that the pattern layer will not be damaged by excessive bending.
[0016] 2. An anti-deformation layer extending along the width direction of the pattern layer is provided. The first anti-deformation block and the second anti-deformation block in the anti-deformation layer can offset part of the load when the lettering film is subjected to bending force in another direction, and cooperate with the anti-bending layer to withstand bending deformation in different directions. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is a schematic diagram of a three-dimensional cross-sectional structure of an anti-deformation reflective lettering film of the utility model;
[0018] Figure 2 The utility model is a schematic diagram of the internal cross-sectional structure of the protrusion of the anti-deformation reflective lettering film.
[0019] Figure numerals: 1, protective layer; 2, pattern layer; 3, anti-bending layer; 4, hot melt adhesive layer; 5, anti-bending part; 6, anti-deformation layer; 7, first anti-deformation block; 8, second anti-deformation block; 9, protrusion; 10, micro-prism block. DETAILED DESCRIPTION
[0020] The technical solutions in the embodiments of the utility model will be described clearly and completely below in conjunction with the drawings in the embodiments of the utility model. In the description of the utility model, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside" and the like indicate directions or positional relationships based on the directions or positional relationships shown in the drawings, which are only for the convenience of describing the utility model and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, rather than all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.
[0021] like Figure 1As shown, an anti-deformation reflective lettering film comprises, from outside to inside, a protective layer 1, a pattern layer 2, an anti-bending layer 3 and a hot-melt adhesive layer 4. The protective layer 1 can be made of a transparent material to protect the pattern layer 2 from being scratched without affecting the viewing of the pattern layer 2. The hot-melt adhesive layer 4 is used to be bonded to clothing during the thermal transfer process. The anti-bending layer 3 comprises an anti-bending member 5 and an adhesive layer wrapping the anti-bending member 5. The adhesive layer is used to be bonded to the adjacent layer. The anti-bending member 5 extends along the length direction of the pattern layer 2. The anti-bending layer 3 is used to withstand the bending force on the clothing area printed with the pattern, so as to provide a better bearing capacity for the pattern and prevent it from being excessively deformed and damaged. Since the cross-section of the anti-bending member 5 is wavy, in the field of construction, the material with a wavy cross-section has a stronger ability to bear loads. Under the same load, the deformation of the material with a wavy cross-section is the smallest. Therefore, the anti-bending member 5 with a wavy cross-section can well protect the pattern layer 2 from being damaged by bending when the lettering film is about to bend and deform in the length direction.
[0022] An anti-deformation layer 6 is also provided between the anti-bending layer 3 and the hot melt adhesive layer 4. The anti-deformation layer 6 includes a plurality of first anti-deformation blocks 7 and second anti-deformation blocks 8 abutting against each other. The first anti-deformation blocks 7 and the second anti-deformation blocks 8 are wrapped with an adhesive layer, which is used to glue the adjacent layers. The anti-deformation blocks abutting against each other can squeeze each other when subjected to a bending load, providing a higher reaction force to bear the load. Figure 1 It can be seen that the cross-sections of the first anti-deformation block 7 and the second anti-deformation block 8 are both triangular, and by utilizing the stability of the triangle, they can withstand a greater bending load.
[0023] At the same time, the side where the first anti-deformation block 7 and the second anti-deformation block 8 abut against each other is arc-shaped. When subjected to a force that causes the lettering film to bend, the side where the first anti-deformation block 7 and the second anti-deformation block 8 abut against each other will squeeze each other, and the arc-shaped contact surface can reduce the stress generated during squeezing, thereby preventing premature failure. The first anti-deformation block 7 and the second anti-deformation block 8 extend along the width direction of the pattern layer 2. This design allows the lettering film to withstand a larger bending load by utilizing the triangular cross-section of the anti-deformation block when the lettering film is about to bend and deform in the width direction, thereby preventing the lettering film from being damaged due to excessive bending.
[0024] The protective layer 1 of the product is formed with a plurality of protrusions 9 on one side away from the pattern layer 2. The protrusions 9 can improve the friction resistance of the surface of the product and prevent the pattern from being scratched during daily use. Figure 2 As shown, micro-prisms 10 are embedded in the protrusions 9. The micro-prisms 10 can refract in different directions when sunlight shines on the surface of the engraving film, making the surface of the product look more colorful.
[0025] Finally, the anti-bending part 5, the first anti-deformation block 7 and the second anti-deformation block 8 are all made of silicone. The silicone material has good elasticity and recovery ability. When the anti-bending part 5, the first anti-deformation block 7 and the second anti-deformation block 8 are subjected to bending load, they can recover quickly.
[0026] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.
[0027] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. An anti-deformation reflective lettering film, characterized in that: From outside to inside, it includes a protective layer, a pattern layer, an anti-bending layer and a hot-melt adhesive layer in sequence. The anti-bending layer includes an anti-bending component and an adhesive layer wrapping the anti-bending component. The anti-bending component extends along the length direction of the pattern layer.
2. The anti-deformation reflective lettering film according to claim 1, characterized in that: The cross section of the anti-bending member is wavy.
3. The anti-deformation reflective lettering film according to claim 2, characterized in that: An anti-deformation layer is also arranged between the anti-bending layer and the hot-melt adhesive layer. The anti-deformation layer includes a plurality of first anti-deformation blocks and second anti-deformation blocks abutting against each other. The first anti-deformation blocks and the second anti-deformation blocks are wrapped with an adhesive layer.
4. The anti-deformation reflective lettering film according to claim 3, characterized in that: One side where the first anti-deformation block and the second anti-deformation block abut against each other is arc-shaped.
5. The anti-deformation reflective lettering film according to claim 4, characterized in that: The first anti-deformation block and the second anti-deformation block extend along the width direction of the pattern layer.
6. The anti-deformation reflective lettering film according to claim 1, characterized in that: A plurality of protrusions are formed on a side of the protection layer away from the pattern layer.
7. The anti-deformation reflective lettering film according to claim 6, characterized in that: Micro-ridges are embedded in the protrusions.