Crystalline silicon battery, crystal silicon battery assembly and solar energy system
By arranging a metal thin film layer to replace the TCO layer in the crystalline silicon cell, combined with the PVD process, the problems of high cost and weak conductivity of the TCO layer are solved, and cost reduction and conductive performance improvement are achieved.
Patent Information
- Application Number
- CN201910519969.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-06-17
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2039-06-17
AI Technical Summary
The transparent conductive oxide film (TCO) in existing crystalline silicon cells has high cost and weak conductivity, which affects battery performance and economy.
A metal thin film layer is provided on the front and/or back of the crystalline silicon cell to partially replace the TCO layer. It is prepared by combining PVD methods such as magnetron sputtering. The metal thin film layer can be Ag, Au, Al, Cu, Ti, Ni, Bi or Mo material, with a thickness of 10~50nm or 50~300nm, equipped with a transparent conductive oxide protective layer.
It reduces the cost of crystalline silicon cells, improves conductivity, avoids an increase in contact resistance, and improves light incident efficiency through a metal film layer of appropriate thickness.
Smart Images

Figure CN110212041B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of crystalline silicon cell manufacturing, and in particular to a crystalline silicon cell, a crystalline silicon cell assembly and a solar energy system. Background Art
[0002] Crystalline silicon cells, such as heterojunction cells, use n-type monocrystalline silicon wafers (c-Si) as substrates. On the front of the cleaned and textured n-type monocrystalline silicon wafer (c-Si), intrinsic amorphous silicon films (ia-Si:H) and p-type amorphous films (pa-Si:H) are deposited in sequence to form a pn heterojunction; on the back of the n-type monocrystalline silicon wafer (c-Si), intrinsic amorphous silicon films (ia-Si:H) and n-type amorphous silicon films (na-Si:H) are deposited in sequence to form a back surface field; transparent conductive oxide films (TCO) are deposited on both sides of the doped a-Si:H film; and finally, metal collectors are formed on the TCO layers on both sides by screen printing technology. Although the transparent conductive oxide film (TCO) of this crystalline silicon cell has good transparency, it is expensive and has weak conductivity. Summary of the invention
[0003] The object of the present invention is to provide an improved crystalline silicon cell in view of the problems in the prior art.
[0004] In order to achieve the above object, the technical solution adopted by the present invention is:
[0005] A crystalline silicon cell comprises a conductive film layer respectively arranged on the front and / or back of the crystalline silicon cell, wherein the conductive film layer comprises a TCO layer and at least one metal film layer, and the metal film layer is arranged on the TCO layer.
[0006] Preferably, the metal thin film layer is a thin film layer prepared by any single metal material among Ag, Au, Al, Cu, Ti, Ni, Bi or Mo.
[0007] Preferably, the metal thin film layer is formed by stacking thin film layers made of any single metal material selected from Ag, Au, Al, Cu, Ti, Ni, Bi or Mo.
[0008] Preferably, the thickness of the metal film layer is 10-50 nm.
[0009] Preferably, the thickness of the metal film layer is 50-300 nm.
[0010] Preferably, the crystalline silicon cell further comprises a gate electrode arranged on the metal film layer.
[0011] Preferably, the crystalline silicon cell further comprises a protective layer arranged on the metal film layer.
[0012] Furthermore, the protective layer is a transparent conductive oxide layer.
[0013] Preferably, the metal thin film layer is prepared by a PVD method.
[0014] Furthermore, the PVD method at least includes a magnetron sputtering method.
[0015] Preferably, the TCO layer is a thin film layer formed by any one oxide of ITO, AZO, GZO, GIO, IGZO, IZO, STO, FTO, and ZTO.
[0016] Preferably, the TCO layer is a thin film layer formed by overlapping film layers formed by at least two oxides selected from ITO, AZO, GZO, GIO, IGZO, IZO, STO, FTO and ZTO.
[0017] The present invention also provides a crystalline silicon cell assembly, comprising the crystalline silicon cell as described in any one of the above items.
[0018] Preferably, the crystalline silicon cell assembly includes at least one crystalline silicon cell.
[0019] The present invention also provides a solar energy system, comprising the crystalline silicon cell as described in any one of the above items.
[0020] Preferably, the solar energy system comprises at least one crystalline silicon cell.
[0021] Due to the application of the above technical solution, the present invention has the following advantages compared with the prior art: the crystalline silicon cell of the present invention partially replaces the conductive oxide film layer in the prior art by setting a metal film layer on the front and / or back of the crystalline silicon cell, thereby reducing the cost of the crystalline silicon cell and improving the conductive performance of the crystalline silicon cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Attached Figure 1 It is a schematic diagram of the structure of the crystalline silicon battery of the present invention. DETAILED DESCRIPTION
[0023] The technical solution of the present invention is further described below.
[0024] The crystalline silicon cell of the present invention is specifically described by taking a heterojunction cell as an example.
[0025] like Figure 1 As shown, the heterojunction cell includes a single crystal silicon substrate 1, an intrinsic amorphous silicon layer 2, an n-type amorphous silicon layer 3 and a conductive film layer 5 sequentially stacked on the front side of the single crystal silicon substrate, and an intrinsic amorphous silicon layer 2, a p-type amorphous layer 4 and a conductive film layer 5 sequentially stacked on the back side of the single crystal silicon substrate 1.
[0026] The conductive film layer 5 on the front and back sides of the crystalline silicon cell includes a TCO layer 51 and at least one metal film layer 52. The TCO layer 51 is respectively arranged on the n-type amorphous silicon layer 3 and the p-type amorphous layer 4, and the metal film layer 52 is arranged on the TCO layer 51. Since the metal film layer 52 has good electrical conductivity and low cost, the present invention partially replaces the TCO layer 51 in the prior art with the metal film layer 52, thereby reducing the amount of the TCO layer 51, which can reduce the cost of the crystalline silicon cell and improve the electrical conductivity of the crystalline silicon cell. Moreover, the metal film layer 52 does not directly contact the n-type amorphous silicon layer 3 and the p-type amorphous layer 4, thereby avoiding increasing the contact resistance of the crystalline silicon cell.
[0027] The metal film layer 52 may be a film layer made of any single metal material among Ag, Au, Al, Cu, Ti, Ni, Bi or Mo. The metal film layer 52 may also be a film layer made of any single metal material among Ag, Au, Al, Cu, Ti, Ni, Bi or Mo, which is formed by sequentially stacking film layers.
[0028] The thickness of the metal film layer 52 can be relatively thin, and its thickness is generally 10-50 nm. At this time, the metal film layer 52 also has good light transmittance. The crystalline silicon cell using the metal film layer 52 can be used as a double-sided cell.
[0029] The thickness of the metal film layer 52 can also be relatively thick, and its thickness is generally 50nm~300nm. At this time, the back side of the crystalline silicon cell cannot transmit light, which can increase the internal reflection of the incident light on the front side of the crystalline silicon cell, thereby improving the efficiency of the front side of the crystalline silicon cell.
[0030] When the thickness of the metal film layer 52 is relatively thin, it is also necessary to set a gate electrode on the metal film layer 52. When the thickness of the metal film layer 52 is relatively thick, the components can be directly welded on the metal film layer 52, so there is no need to print the gate electrode on the metal film layer 52, which reduces the amount of low-temperature silver paste, thereby further reducing the cost of the crystalline silicon cell.
[0031] The crystalline silicon cell further includes a protective layer 6 disposed on the metal film layer 52. The protective layer 6 is a transparent conductive oxide layer. In this embodiment, the protective layer 6 may be a zinc oxide AZO layer or an ITO layer. By providing the protective layer 6, the metal film layer 52 may not be oxidized or scratched.
[0032] There are many processes for preparing the metal film layer 52. In this embodiment, the PVD (physical vapor deposition) process is used for preparation. The PVD process includes at least a magnetron sputtering method. When the magnetron sputtering process is used, the operating gas pressure is 0.1-100 Pa, the sputtering power density is 1-100 W / cm, and the sputtering thickness is 10-2000 nm. Of course, other PVD process methods, such as evaporation, etc., can also be used.
[0033] The TCO layer 51 can be a thin film layer formed by any oxide of ITO, AZO, GZO, GIO, IGZO, IZO, STO, FTO, and ZTO.
[0034] The TCO layer 51 can also be formed by forming a thinner film layer of at least two oxides selected from ITO, AZO, GZO, GIO, IGZO, IZO, STO, FTO, and ZTO, and then stacking the film layers. The present invention also provides a crystalline silicon cell assembly, which includes the above-mentioned crystalline silicon cell, and at least one crystalline silicon cell is provided.
[0035] The present invention further provides a solar energy system, which also includes the above-mentioned crystalline silicon cell, and at least one crystalline silicon cell is provided.
[0036] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with this technology to understand the content of the present invention and implement it. They cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.
Claims
1. A crystalline silicon cell, wherein the crystalline silicon cell is a heterojunction cell, comprising a conductive film layer disposed on the front and / or back of the crystalline silicon cell, wherein: The conductive film layer includes a TCO layer and at least one metal film layer, and the metal film layer is arranged on the TCO layer; the thickness of the metal film layer is 50 to 300 nm, and components can be directly welded on the metal film layer, thereby eliminating the need to print a gate electrode on the metal film layer; the crystalline silicon cell also includes a protective layer arranged on the metal film layer.
2. The crystalline silicon cell according to claim 1, characterized in that: The metal thin film layer is a thin film layer prepared by any single metal material among Ag, Au, Al, Cu, Ti, Ni, Bi or Mo.
3. The crystalline silicon cell according to claim 1, characterized in that: The metal thin film layer is formed by stacking thin film layers made of any single metal material among Ag, Au, Al, Cu, Ti, Ni, Bi or Mo.
4. The crystalline silicon cell according to claim 1, characterized in that: The protective layer is a transparent conductive oxide layer.
5. The crystalline silicon cell according to claim 1, characterized in that: The metal thin film layer is prepared by a PVD method.
6. The crystalline silicon cell according to claim 5, characterized in that: The PVD method includes at least a magnetron sputtering method.
7. The crystalline silicon cell according to claim 1, characterized in that: The TCO layer is a thin film layer formed by any oxide of ITO, AZO, GZO, GIO, IGZO, IZO, STO, FTO, and ZTO.
8. The crystalline silicon cell according to claim 1, characterized in that: The TCO layer is a thin film layer formed by overlapping film layers formed by at least two oxides selected from ITO, AZO, GZO, GIO, IGZO, IZO, STO, FTO, and ZTO.
9. A crystalline silicon battery assembly, characterized in that: Comprising the crystalline silicon cell as described in any one of claims 1 to 8.
10. The crystalline silicon battery assembly according to claim 9, characterized in that: The crystalline silicon cell assembly includes at least one crystalline silicon cell.
11. A solar energy system, characterized in that: Comprising the crystalline silicon cell as described in any one of claims 1 to 8.
12. The solar energy system according to claim 11, characterized in that: The solar energy system comprises at least one crystalline silicon cell.