Semiconductor device and method for forming the same
By forming an isolation layer and a hard mask layer on the substrate of the semiconductor device to define the fin pattern, the problem of poor formation quality of semiconductor devices in traditional technology is solved, higher quality and flexible fin formation is achieved, and the device efficiency is improved. electrical properties.
Patent Information
- Application Number
- CN201910498537.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-06-10
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2039-06-10
AI Technical Summary
In the process of reducing the size and increasing the density of traditional semiconductor devices, it is difficult to ensure the formation quality, resulting in short channel effects and leakage current problems, which affect electrical performance.
An isolation layer is formed on the substrate, and a hard mask layer is used to define the fin pattern. The covering isolation layer is removed to form an opening. A first fin and a second fin are formed in the NMOS area and PMOS area respectively, using epitaxial growth. Technology to control fin material and height.
By omitting the redundant fin removal process, the quality and flexibility of the fins are improved, and the performance and density of the semiconductor device are enhanced.
Smart Images

Figure CN112071805B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a semiconductor device and a method for forming the same. Background Art
[0002] With the rapid development of semiconductor manufacturing technology, semiconductor devices are developing towards higher component density and higher integration. As the most basic semiconductor device, the device is currently being widely used. The control ability of traditional planar devices on channel current has weakened, resulting in short channel effect and leakage current, which ultimately affects the electrical performance of semiconductor devices.
[0003] In order to overcome the short channel effect of the device and suppress leakage current, the prior art proposes a fin field effect transistor (Fin FET). The fin field effect transistor is a common multi-gate device. The structure of the fin field effect transistor includes: a fin and an isolation structure located on the surface of a semiconductor substrate, the isolation structure covers a portion of the sidewall of the fin, a gate structure located on the substrate and across the fin; and a source region and a drain region in the fin located on both sides of the gate structure.
[0004] However, as the size of semiconductor devices continues to shrink and the device density increases, how to ensure the formation of semiconductor devices with good quality has become an urgent problem that needs to be solved. Summary of the invention
[0005] The problem solved by the present invention is to provide a semiconductor device and a method for forming the same, thereby ensuring that the formed semiconductor device has higher quality.
[0006] To solve the above problems, the present invention provides a method for forming a semiconductor device, comprising: providing a substrate, the substrate comprising an NMOS region and a PMOS region; forming an isolation layer on the substrate; forming a plurality of discretely arranged hard mask layers on the isolation layer, the plurality of discretely arranged hard mask layers defining a fin pattern; removing the isolation layer covered by the hard mask layer until the substrate is exposed, and forming an opening in the isolation layer; forming a first fin in the opening in the NMOS region; and forming a second fin in the opening in the PMOS region.
[0007] Optionally, the material of the first fin includes silicon, and the material of the second fin includes silicon germanium.
[0008] Optionally, the first fin and the second fin are formed by epitaxial growth.
[0009] Optionally, the step of forming the first fin includes: forming a mask layer between adjacent hard mask layers; forming a first photoresist layer on the hard mask layer and the mask layer in the PMOS region; removing the hard mask layer in the NMOS region, using the mask layer in the NMOS region as a mask, etching the isolation layer in the NMOS region until the substrate is exposed, and forming an opening in the isolation layer in the NMOS region; and forming the first fin in the opening.
[0010] Optionally, the step of forming the second fin includes: removing the first photoresist layer; forming a second photoresist layer on the first fin in the NMOS region and on the mask layer; removing the hard mask layer in the PMOS region, and using the mask layer in the PMOS region as a mask, etching the isolation layer in the PMOS region until the substrate is exposed, forming an opening in the isolation layer in the PMOS region; and forming a second fin in the opening.
[0011] Optionally, a plurality of discretely arranged hard mask layers are formed on the isolation layer, and the step of defining the fin pattern by the plurality of discretely arranged hard mask layers includes: forming the hard mask layers initially discretely arranged on the isolation layer; forming a third photoresist layer on the isolation layer, the openings of the third photoresist layer exposing a portion of the hard mask layers initially discretely arranged; and removing the hard mask layers exposed by the openings of the third photoresist layer.
[0012] Optionally, the hard mask layer includes a first hard mask layer and a second hard mask layer, and a material of the first hard mask layer is different from a material of the second hard mask layer.
[0013] Optionally, the third photoresist layer is formed at least twice, the opening of the third photoresist layer is formed for the first time to expose a portion of the first hard mask layer, and the opening of the third photoresist layer is formed for the second time to expose a portion of the second hard mask layer.
[0014] Optionally, the step of forming the hard mask layer initially discretely arranged on the isolation layer includes: forming the first hard mask layer initially discretely arranged on the isolation layer; forming a sacrificial sidewall on the sidewall of the first hard mask layer; forming the second hard mask layer between adjacent sacrificial sidewalls; and removing the sacrificial sidewall.
[0015] Optionally, the material of the hard mask layer includes one or more of silicon nitride, silicon oxynitride, silicon carbonitride, silicon oxycarbide, silicon or silicon germanium.
[0016] Compared with the prior art, the technical solution of the present invention has the following advantages:
[0017] First, an isolation layer is formed on the substrate, and then a hard mask layer is formed on the isolation layer to define the pattern of the fin, the isolation layer covered by the hard mask layer is removed, and an opening is formed in the isolation layer, thereby forming a first fin in the opening of the NMOS region and a second fin in the opening of the PMOS region respectively; by defining the pattern of the fin using the hard mask layer on the isolation layer and setting the fin to be formed at the required position, no redundant fins will be formed, and there will be no process of removing redundant fins, thereby ensuring the quality of the formed fins; at the same time, since the first fin and the second fin are respectively formed in the opening of the isolation layer, on the one hand, the formation height of the first fin and the second fin can be controlled according to actual needs, making the process of forming the fins flexible; on the other hand, the first fin is formed in the opening of the NMOS region, and the second fin is formed in the opening of the PMOS region, so that the material of the first fin and the material of the second fin can be selected and formed according to actual needs, and the required fins are formed at the set position at one time, so that the quality of the formed fins is controlled, thereby improving the quality of the formed semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figures 1 to 8 is a structural schematic diagram of a semiconductor device forming process in one embodiment;
[0019] Figures 9 to 20 is a structural schematic diagram of a semiconductor device forming process in a first embodiment of the present invention;
[0020] Figures 21 to 35 It is a structural schematic diagram of the semiconductor device forming process in the second embodiment of the present invention. DETAILED DESCRIPTION
[0021] In the process of forming a semiconductor device, it is usually necessary to form a fin of silicon material in the NMOS region and a fin of silicon germanium material in the PMOS region. However, due to the limitation of process conditions, the quality of the formed fin is poor, thereby reducing the quality of the formed semiconductor device. The specific method of forming a semiconductor device is as follows:
[0022] refer to Figure 1 , providing a substrate 1, wherein the substrate 1 includes an NMOS region and a PMOS region, and a plurality of discretely arranged initial fins 2 are formed on the substrate 1, wherein the material of the initial fins 2 is silicon.
[0023] refer to Figure 2 , an isolation layer 3 is formed on the substrate 1 , and a top of the isolation layer 3 is flush with a top of the initial fin 2 .
[0024] refer to Figure 3 , forming a first photoresist layer 4 on surfaces of the initial fin 2 and the isolation layer 3 in the NMOS region.
[0025] refer to Figure 4 , removing the initial fin 2 of the PMOS region to form an opening 5.
[0026] refer to Figure 5 A modified fin 6 is formed in the opening 5 , and the material of the modified fin 6 is silicon germanium.
[0027] refer to Figure 6 , removing the first photoresist layer 4 , forming a second photoresist layer 7 on the initial fin 2 , the isolation layer 3 and the modified fin 6 , wherein the opening 701 of the second photoresist layer 7 exposes a portion of the initial fin 2 and the modified fin 6 .
[0028] refer to Figure 7 , the opening 701 of the second photoresist layer 7 is removed to expose a portion of the initial fin 2 and the modified fin 6 .
[0029] refer to Figure 8 , the second photoresist layer 7 and a partial thickness of the isolation layer 3 are removed, and the top surface of the isolation layer 3 is lower than the top surfaces of the initial fin 2 and the modified fin 6 .
[0030] The inventors have found that the semiconductor device formed by this method has poor stability in performance and is prone to failure, which limits the use of the semiconductor device. After forming the initial fin in the NMOS region and the modified fin in the PMOS region, a second photoresist layer is formed on the initial fin and the modified fin, and the opening of the second photoresist layer is used to expose the redundant initial fin and the modified fin so as to be removed to form the required fin pattern. In the actual process, due to the limitation of the size of the formed semiconductor device, the surface of the formed fin is easily damaged or incompletely removed during the removal of the redundant fin, so that the surface quality of the formed fin cannot be controlled, and the formed semiconductor device has poor performance.
[0031] The inventors have found that by forming an isolation layer on a substrate and defining a fin pattern by forming a hard mask layer on the isolation layer, there are no redundant fins when the fins are formed, so the process of cutting off the redundant fins is omitted, thereby ensuring the quality of the formed fins. In addition, openings are formed in the isolation layer, and a first fin is formed in the opening of the NMOS region and a second fin is formed in the opening of the PMOS region. The materials and heights of the first and second fins can be set according to actual needs, making the process flexible. The formation process of this semiconductor device well controls the quality of the formed fins and improves the performance of the formed semiconductor device.
[0032] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0033] First embodiment
[0034] Figures 9 to 20 It is a structural schematic diagram of the semiconductor device forming process in the first embodiment of the present invention.
[0035] First reference Fig. 9 , providing the substrate 100, wherein the substrate 100 includes an NMOS region and a PMOS region.
[0036] In this embodiment, the material of the substrate 100 is single crystal silicon; in other embodiments, the substrate 100 may be single crystal silicon, polycrystalline silicon or amorphous silicon; the substrate 100 may also be a semiconductor material such as silicon, germanium, germanium silicon, gallium arsenide, etc.
[0037] refer to Fig.10 , an isolation layer 200 is formed on the substrate 100 .
[0038] In this embodiment, the material of the isolation layer 200 is silicon oxide; in other embodiments, the material of the isolation layer 200 may also be silicon nitride or silicon oxynitride.
[0039] In this embodiment, the isolation layer 200 adopts a shallow trench isolation (STI) structure, and the shallow trench isolation structure is formed in a traditional manner.
[0040] In this embodiment, the isolation layer 200 not only protects the substrate 100 but also serves as an etching stop layer in a subsequent etching process.
[0041] refer to Fig.11 , a plurality of hard mask layers 300 initially arranged discretely are formed on the isolation layer 200 .
[0042] In this embodiment, the material of the hard mask layer 300 is silicon nitride; in other embodiments, the material of the hard mask layer 300 may also be silicon oxynitride or silicon carbonitride or silicon oxycarbide or silicon or silicon germanium or a stacked structure of silicon oxynitride and silicon carbide.
[0043] In this embodiment, a self-aligned double patterning process is used to set the position of the hard mask layer 300. This is done to predetermine the position where the fin may be formed.
[0044] In this embodiment, the material of the hard mask layer 300 is formed by a chemical vapor deposition process, and then the material of the hard mask layer 300 is etched back to form the hard mask layer 300 initially arranged discretely on the isolation layer 200 .
[0045] refer to Fig.12 , a third photoresist layer 201 is formed on the isolation layer 200 , and the opening 2011 of the third photoresist layer 201 exposes a portion of the hard mask layer 300 that is initially discretely arranged.
[0046] In this embodiment, first, a number of hard mask layers 300 are initially discretely arranged on the isolation layer 200. This step is to preliminarily set the position where the fin is to be formed. However, according to the design requirements of the actual circuit, the hard mask layer 300 at the position where the fin is not needed is removed. The required removal of the hard mask layer 300 can be achieved by controlling the size of the opening 2011 of the third photoresist layer 201. The variability of the opening 2011 makes the process flexible.
[0047] refer to Fig.13 , remove the hard mask layer 300 exposed by the opening 2011 of the third photoresist layer 201 , define the fin pattern, and remove the third photoresist layer 201 .
[0048] In this embodiment, etching is used to remove the exposed hard mask layer 300 ; in other embodiments, ashing or other processes may be used to remove the exposed hard mask layer 300 .
[0049] In the present embodiment, the purpose of removing the hard mask layer 300 exposed by the opening 2011 is to define the fin pattern and ensure that fins are formed at required positions and no fins are present at unnecessary positions. In this way, there will be no redundant fins, and the process of removing redundant fins is omitted, thereby ensuring that the quality of the formed fins is not damaged, thereby facilitating improving the quality of the formed semiconductor device.
[0050] refer to Fig.14 , a mask layer 301 is formed between adjacent hard mask layers 300 that define the fin pattern.
[0051] In this embodiment, the material of the mask layer 301 is silicon carbide; in other embodiments, the mask layer 301 may also be a photoresist layer or a stacked structure of a photoresist layer and an anti-reflective coating.
[0052] In this embodiment, the material of the mask layer 301 is chemically vapor deposited on the isolation layer 200 , and chemical mechanical polishing (CMP) is performed to make the top surface of the mask layer 301 flush with the top of the hard mask layer 300 .
[0053] refer to Fig.15 , forming a first photoresist layer 202 on the hard mask layer 300 and the mask layer 301 in the PMOS region.
[0054] In this embodiment, a first photoresist layer 202 is formed on the hard mask layer 300 and the mask layer 301 of the PMOS region, so that the NMOS region is processed first and a first fin is formed in the NMOS region.
[0055] In other embodiments, the first photoresist layer 202 may be first formed on the hard mask layer 300 and the mask layer 301 of the NMOS region, so that the PMOS region is processed first and the second fin is formed in the PMOS region.
[0056] In this embodiment, the material of the first photoresist layer 202 is krypton fluoride (KrF); in other embodiments, argon fluoride (ArF) may also be used.
[0057] refer to Fig.16 , remove the hard mask layer 300 of the NMOS region, use the mask layer 301 of the NMOS region as a mask, etch the isolation layer 200 of the NMOS region until the substrate 100 is exposed, and form an opening 400 in the isolation layer 200 of the NMOS region.
[0058] In this embodiment, dry etching is used to remove the hard mask layer 300 ; in other embodiments, wet etching or other processes may be used to remove the hard mask layer 300 .
[0059] In this embodiment, the process used to etch the isolation layer 200 is an isotropic dry etching process, and the dry etching process parameters include: the gases used include CF4 gas, CH3F gas and O2, the flow rate of CF4 gas is 5sccm~100sccm, the flow rate of CH3F gas is 8sccm~50sccm, the flow rate of O2 is 10sccm~100sccm, the chamber pressure is 10mtorr~2000mtorr, the RF power is 50W~300W, the bias voltage is 30V~100V, and the time is 4 seconds~50 seconds.
[0060] refer to Fig.17 , a first fin 401 is formed in the opening 400 .
[0061] In this embodiment, the first fin 401 is formed in the opening 400 by epitaxial growth. In other embodiments, the first fin 401 may be formed by atomic layer vapor deposition or chemical vapor deposition.
[0062] In this embodiment, the fins are formed by epitaxial growth because the fins formed by epitaxial growth have fewer defects and a material with better conductivity can be formed by epitaxial growth.
[0063] In this embodiment, the material of the first fin 401 is silicon material, and the process parameters for forming the first fin 401 include using silane (SiH4) as the ambient atmosphere, the gas flow rate of the SiH4 gas is 10 to 700 sccm; the pressure range is 1 to 100 Torr; the temperature is between 400°C and 600°C, and the reaction time is controlled between 10min and 20min.
[0064] In this embodiment, since the first fin 401 is formed in the opening 400 , the height of the first fin 401 can be controlled to different heights according to actual needs, which makes the formation of the fins flexible and reduces the restrictions on process conditions.
[0065] refer to Fig.18 , remove the first photoresist layer 202 , and form a second photoresist layer 203 on the first fin 401 of the NMOS region and on the mask layer 301 .
[0066] In this embodiment, the material of the second photoresist layer 203 is the same as that of the first photoresist layer 202 ; in other embodiments, different materials may also be used.
[0067] refer to Fig.19 , remove the hard mask layer 300 of the PMOS region, use the mask layer 301 of the PMOS region as a mask, etch the isolation layer 200 of the PMOS region until the substrate 100 is exposed, and form an opening 500 in the isolation layer 200 of the PMOS region.
[0068] In this embodiment, the process of removing the hard mask layer 300 in the PMOS region is the same as the process of removing the hard mask layer 300 in the NMOS region; in other embodiments, different processes may be used to remove the hard mask layer 300.
[0069] In this embodiment, the process of etching the isolation layer 200 in the PMOS region is the same as the process of etching the isolation layer 200 in the NMOS region; in other embodiments, different etching processes may be used to etch the isolation layer 200.
[0070] refer to Fig. 20 , forming a second fin 501 in the opening 500 , and removing the second photoresist layer 203 , the mask layer 301 and a portion of the thickness of the isolation layer 200 .
[0071] In this embodiment, the material of the second fin 501 is silicon germanium, and the second fin 501 is formed by epitaxial growth. The process parameters of the epitaxial growth include using silane (SiH4) and germane (GeH4) as the ambient atmosphere, wherein the gas percentage ratio of silane (SiH4) and germane (GeH4) is controlled between 20 and 50%, and the pressure range is 1 to 100 torr; the temperature is between 400°C and 600°C.
[0072] A semiconductor device formed by the above method includes: a substrate 100 including an NMOS region and a PMOS region; an isolation layer 200 located on the substrate 100; a first fin 401 discretely arranged on the substrate 100 in the NMOS region; and a second fin 501 discretely arranged on the substrate 100 in the PMOS region.
[0073] Second embodiment
[0074] Figures 21 to 35 It is a structural schematic diagram of the semiconductor device forming process in the second embodiment of the present invention.
[0075] The steps from providing the substrate to forming the isolation layer on the substrate in this embodiment are the same as those in the first embodiment, and will not be described again here.
[0076] refer to Fig.21 , the first hard mask layer 302 initially arranged discretely is formed on the isolation layer 200 .
[0077] In this embodiment, the first hard mask layer 302 is formed by a self-aligned double patterning process (SADP) in order to predetermine a position where a fin may be formed.
[0078] In this embodiment, the material of the first hard mask layer 302 is silicon oxynitride; in other embodiments, the material of the first hard mask layer 302 may also be silicon oxide or silicon nitride.
[0079] refer to Fig. 22 , forming a sacrificial spacer 303 on the sidewall of the first hard mask layer 302 .
[0080] In this embodiment, the material of the sacrificial sidewall 303 is silicon carbonitride; in other embodiments, the sacrificial sidewall 303 may also be one or more of silicon oxide, silicon nitride, silicon carbonitride, and silicon carbonitride oxide.
[0081] In this embodiment, the sacrificial sidewall spacer 303 may be formed by using a conventional process for forming a sidewall spacer.
[0082] refer to Fig.23 , forming the second hard mask layer 304 between adjacent sacrificial sidewalls 303 .
[0083] In this embodiment, the material of the second hard mask layer 304 is silicon nitride; in other embodiments, the material of the second hard mask layer 304 may also be silicon oxide or the like.
[0084] In this embodiment, the material of the first hard mask layer 302 is different from the material of the second hard mask layer 304. At the same time, the first hard mask layer 302 and the second hard mask layer 304 are alternately and discretely arranged on the isolation layer 200. By utilizing the different materials and staggered arrangement of the first hard mask layer 302 and the second hard mask layer 304, when the first hard mask layer 302 or the second hard mask layer 304 is removed respectively, the adjacent hard mask layer will not be damaged, thereby ensuring the accuracy of the pattern transfer and the quality of the fin formation.
[0085] refer to Fig.24 , remove the sacrificial sidewall 303.
[0086] In this embodiment, after the sacrificial spacer 303 is removed, the first hard mask layer 302 and the second hard mask layer 304 formed are the hard mask layers 300 initially arranged discretely on the isolation layer 200 .
[0087] In this embodiment, dry etching is used to remove the sacrificial sidewall 303. The dry etching parameters include: the gases used include CF4 gas, CH2F2 gas and O2, the flow rate of CF4 gas is 30sccm to 200sccm, the flow rate of CH2F2 gas is 8sccm to 50sccm, the flow rate of O2 is 2sccm to 30sccm, the chamber pressure is 10mtorr to 2000mtorr, the source RF power is 100W to 1000W, the bias voltage is 30V to 500V, and the time is 4 seconds to 500 seconds.
[0088] refer to Fig.25 , a third photoresist layer 201 is formed on the isolation layer 200 for the first time, and the opening of the third photoresist layer 201 exposes a portion of the first hard mask layer 302 that is initially discretely arranged.
[0089] refer to Fig.26 , removing the opening of the third photoresist layer 201 to expose a portion of the first hard mask layer 302 initially arranged discretely, forming the first hard mask layer 302 with a modified discrete arrangement, and removing the third photoresist layer 201.
[0090] In this embodiment, a chemical reagent is used to remove the third photoresist layer 201 ; in other embodiments, an ashing process may also be used to remove the third photoresist layer 201 .
[0091] refer to Fig. 27, a third photoresist layer 201 is formed on the isolation layer 200 for a second time, and the opening of the third photoresist layer 201 exposes a portion of the second hard mask layer 304 that is initially discretely arranged.
[0092] refer to Fig.28 , removing the opening of the third photoresist layer 201 to expose a portion of the second hard mask layer 304 initially arranged discretely, forming the second hard mask layer 304 with a modified discrete arrangement, and removing the third photoresist layer 201.
[0093] In this embodiment, the first hard mask layer 302 and the second hard mask layer 304 after correction processing are arranged on the isolation layer 200 to define the fin pattern, so that no extra fins are formed at unnecessary positions, and the process of removing extra fins is omitted, so that the quality of the formed fins is not damaged, thereby improving the quality of the formed semiconductor device.
[0094] refer to Fig.29 , the mask layer 301 is formed on the isolation layer 200 , and the mask layer 301 is filled between the adjacent first hard mask layer 302 and the second hard mask layer 304 .
[0095] In this embodiment, the material and formation process of the mask layer 301 are the same as those of the first embodiment.
[0096] refer to Fig.30 , forming a first photoresist layer 202 on the first hard mask layer 302 , the second hard mask layer 304 and the mask layer 301 in the PMOS region.
[0097] In this embodiment, the material of the first photoresist layer 202 is krypton fluoride (KrF).
[0098] refer to Fig.31 , remove the first hard mask layer 302 and the second hard mask layer 304 of the NMOS region, use the mask layer 301 of the NMOS region as a mask, etch the isolation layer 200 of the NMOS region until the substrate 100 is exposed, and form an opening 400 in the isolation layer 200 of the NMOS region.
[0099] In this embodiment, dry etching is used to remove the first hard mask layer 302 and the second hard mask layer 304. The process parameters of the dry etching are: using fluorine-containing gas (such as CH3F, CH2F2 or CHF3), argon and oxygen, the etching power is 200W~400W, the pressure of the etching chamber is 30mtorr~200mtorr, and the etching temperature is 40℃~60℃.
[0100] In this embodiment, the process of etching the isolation layer 200 is the same as that of the first embodiment.
[0101] refer to Fig.32 , a first fin 401 is formed in the opening 400 .
[0102] In this embodiment, the first fin 401 is also formed by epitaxial growth. The material of the first fin 401 is silicon. The reason for forming the first fin 401 by epitaxial growth is that epitaxial growth can form high-quality silicon material and the process is flexible, which can avoid the formation of defects.
[0103] refer to Fig.33 , remove the first photoresist layer 202 , and form a second photoresist layer 203 on the first fin 401 of the NMOS region and on the mask layer 301 .
[0104] In this embodiment, the material of the second photoresist layer 203 is argon fluoride (ArF).
[0105] In this embodiment, an ashing process is used to remove the first photoresist layer 202 .
[0106] refer to Fig.34 , remove the first hard mask layer 302 and the second hard mask layer 304 of the PMOS region, use the mask layer 301 of the PMOS region as a mask, etch the isolation layer 200 of the PMOS region until the substrate 100 is exposed, and form an opening 500 in the isolation layer of the PMOS region.
[0107] In this embodiment, the process of removing the first hard mask layer 302 and the second hard mask layer 304 in the PMOS region is the same as the process of removing the first hard mask layer 302 and the second hard mask layer 304 in the NMOS region.
[0108] In this embodiment, the process of etching the isolation layer 200 is the same as that of the first embodiment.
[0109] refer to Fig.35 , forming a second fin 501 in the opening 500 , and removing the second photoresist layer 203 , the mask layer 301 and a portion of the thickness of the isolation layer 200 .
[0110] In this embodiment, the shape of the fin finally formed meets the actual needs, and there is no need to remove excess fins, which simplifies the process. At the same time, the quality of the formed fins is guaranteed, thereby improving the quality of the formed semiconductor device.
[0111] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor device, characterized in that: include: Providing a substrate, the substrate comprising an NMOS region and a PMOS region; forming an isolation layer on the substrate; forming a plurality of discretely arranged hard mask layers on the isolation layer, wherein the plurality of discretely arranged hard mask layers define fin patterns; removing the isolation layer covered by the hard mask layer until the substrate is exposed, and forming an opening in the isolation layer; forming a first fin in the opening of the NMOS region; A second fin is formed in the opening of the PMOS region, wherein a plurality of discretely arranged hard mask layers are formed on the isolation layer, and the plurality of discretely arranged hard mask layers define a fin pattern, comprising: forming the hard mask layer initially discretely arranged on the isolation layer; forming a third photoresist layer on the isolation layer, wherein the opening of the third photoresist layer exposes a portion of the hard mask layer initially arranged discretely; The hard mask layer exposed by the opening of the third photoresist layer is removed.
2. The method for forming a semiconductor device according to claim 1, wherein: The material of the first fin includes silicon, and the material of the second fin includes silicon germanium.
3. The method for forming a semiconductor device according to claim 1, wherein: The first fin and the second fin are formed by epitaxial growth.
4. The method for forming a semiconductor device according to claim 1, wherein: The step of forming the first fin comprises: forming a mask layer between adjacent hard mask layers; forming a first photoresist layer on the hard mask layer and the mask layer of the PMOS region; removing the hard mask layer in the NMOS region, and etching the isolation layer in the NMOS region using the mask layer in the NMOS region as a mask until the substrate is exposed, thereby forming an opening in the isolation layer in the NMOS region; A first fin is formed in the opening.
5. The method for forming a semiconductor device according to claim 4, wherein: The step of forming the second fin comprises: removing the first photoresist layer; Forming a second photoresist layer on the first fin of the NMOS region and on the mask layer; removing the hard mask layer of the PMOS region, etching the isolation layer of the PMOS region using the mask layer of the PMOS region as a mask until the substrate is exposed, and forming an opening in the isolation layer of the PMOS region; A second fin is formed in the opening.
6. The method for forming a semiconductor device according to claim 1, wherein: The hard mask layer includes a first hard mask layer and a second hard mask layer, and a material of the first hard mask layer is different from a material of the second hard mask layer.
7. The method for forming a semiconductor device according to claim 6, wherein: The third photoresist layer is formed at least twice. The opening of the third photoresist layer is formed for the first time to expose a portion of the first hard mask layer. The opening of the third photoresist layer is formed for the second time to expose a portion of the second hard mask layer.
8. The method for forming a semiconductor device according to claim 6, wherein: The step of forming the hard mask layer initially discretely arranged on the isolation layer comprises: forming the first hard mask layer initially discretely arranged on the isolation layer; forming a sacrificial spacer on the sidewall of the first hard mask layer; forming the second hard mask layer between adjacent sacrificial sidewalls; The sacrificial sidewall is removed.
9. The method for forming a semiconductor device according to claim 1, wherein: The material of the hard mask layer includes one or more of silicon nitride, silicon oxynitride, silicon carbonitride, silicon oxycarbide, silicon or silicon germanium.