Energy storage device stacking
By using inkjet printing and laser ablation technology to form parallel battery structures in energy storage devices, the problem of low stacking efficiency in existing technologies has been solved, enabling efficient and low-cost battery production.
Patent Information
- Application Number
- CN201980048216.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-07-20
- Filing Date
- 2019-07-19
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2039-07-19
AI Technical Summary
Existing technologies are inefficient in forming and processing stacked energy storage devices, making commercialization difficult.
Inkjet printing technology is used to deposit electrically insulating and conductive materials, which are then combined with laser ablation to form a parallel battery structure, reducing material usage and improving production efficiency.
It enables flexible, efficient, and reliable battery production, reduces costs, and improves the discharge rate and production efficiency of energy storage devices.
Smart Images

Figure CN112470303B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a stack for an energy storage device and more particularly, but not exclusively, to a method and apparatus for handling a stack for an energy storage device. Background Art
[0002] A known method of producing an energy storage device such as a solid-state thin-film battery comprising an electrode layer, an electrolyte layer and a current collector layer is to first form a stack comprising a first current collector layer, an electrode layer, an electrolyte layer, a second electrode layer and a second current collector layer formed on a substrate. The stack is then cut into individual parts to form individual cells. A protective layer may then be applied to each cell, for example, to prevent passivation of the layers and possible short circuits.
[0003] To make electrical connections with the cells, for example to electrically connect the current collectors of multiple cells stacked one on top of another, portions of the protective layer may be removed, for example by etching. Alternatively, a mask may be applied prior to the coating process to ensure that a portion of each current collector is exposed.
[0004] However, known formation and processing of stacks for energy storage devices such as solid-state thin film batteries can be inefficient, making effective commercialization difficult. It is therefore desirable to provide efficient methods of forming and processing stacks for energy storage devices. Summary of the invention
[0005] According to a first aspect of the present invention, a method is provided, comprising: obtaining a stack for an energy storage device, the stack comprising a first electrode layer, a second electrode layer, and an electrolyte layer between the first electrode layer and the second electrode layer; depositing a first material on an exposed portion of the first electrode layer and an exposed portion of the electrolyte layer; depositing a second material on the first material and in contact with the second electrode layer to provide an electrical connection to the second electrode layer to connect to another such second electrode layer through the second material, whereby the first material insulates the exposed portion of the first electrode layer and the exposed portion of the electrolyte layer from the second material.
[0006] Depositing the second material on the first material and in contact with the second electrode layer may allow efficient and / or reliable parallel connection of cells formed from the stack and thus, for example, for efficient production of energy storage devices therefrom.
[0007] In an example, depositing the first material comprises inkjet material deposition of the first material. Depositing the first material by inkjet material deposition such as inkjet printing can allow for flexible, efficient and / or reliable deposition of the first material. For example, inkjet printing can be performed at relatively low (e.g., ambient) temperatures and / or pressures, e.g., compared to thermal spraying, and thus can allow for economical and / or efficient deposition and therefore battery production.
[0008] The stack includes a substrate adjacent to one of the first electrode layer and the second electrode layer, wherein the other of the first electrode layer and the second electrode layer is an anode layer. Having the stack in this configuration can allow the anode material to be used as the second material, which can provide efficient energy storage device production.
[0009] The anode layer comprises an anode material, and the second material is the same as the anode material. For example, the anode material may be relatively cheap. For example, the anode material may be cheap compared to conductive ink and / or to cathode material. Therefore, using the anode material to provide the anode layer with electrical connections to other such anode layers of other batteries can allow for reduced costs of battery production, and therefore can allow for more efficient battery production. As another example, deposition of the anode material, such as by flood deposition, can be relatively fast and / or cheap, for example, compared to inkjet printing.
[0010] In an example, depositing the second material includes depositing the second material on the anode layer. This can allow efficient deposition of the second material, and therefore efficient battery production. For example, depositing the anode material can allow the anode layer of the obtained stack to be only partially formed, and allow the deposited anode material to complete the anode layer. This can reduce the total amount of conductive and / or anode material used to produce a battery from the stack.
[0011] In an example, depositing the second material comprises inkjet material deposition of the second material. Depositing the second material by inkjet material deposition, such as inkjet printing, can allow for flexible, efficient and / or reliable deposition of the second material. For example, inkjet printing can be performed at relatively low (e.g., ambient) temperatures and / or pressures, e.g., compared to thermal spraying, and thus can allow for economical and / or efficient deposition and, therefore, battery production.
[0012] In an example, the first electrode layer, the electrolyte layer, and the second electrode layer are recessed from the substrate so that the substrate provides a ledge portion on which the first material and / or the second material are at least partially supported. Having a ledge portion can allow the first material and / or the second material to be supported during and / or after deposition, and / or can prevent or reduce undesirable migration of the first material and / or the second material, which in turn can facilitate accurate deposition of the first material and / or the second material.
[0013] In an example, the first electrode layer and the electrolyte layer are recessed from the second electrode layer so that the second electrode layer provides a ledge portion on which the first material and / or the second material is at least partially supported. Having a ledge portion can allow the first material and / or the second material to be supported during and / or after deposition, and / or can prevent or reduce undesirable migration of the first material and / or the second material, which in turn can facilitate accurate deposition of the first material and / or the second material.
[0014] In an example, another such second electrode layer belongs to another such stack. This may provide for a parallel connection of the individual batteries formed by the stack. Connecting batteries in parallel may provide an energy storage device with a relatively large discharge rate, which may be useful in certain applications.
[0015] In an example, the stack includes another second electrode layer, and another electrolyte layer between the another second electrode layer and the first electrode layer, depositing the first material also includes depositing the first material on the exposed portion of the another electrolyte layer, and depositing the second material also includes depositing the second material to contact the another second electrode layer, thereby connecting the second electrode layer and the another second electrode layer via the second material, so that the first material further insulates the exposed portion of the another electrolyte layer from the second material. Such a stacking arrangement can provide layers constituting multiple batteries on one substrate. This may be an effective arrangement because it can reduce the amount of substrate, anode and / or cathode material required to form multiple batteries.
[0016] In an example, the electrolyte layer, the first electrode layer, the further electrolyte layer and the further second electrode layer are recessed from the second electrode layer so that the second electrode layer provides a ledge on which the first material and / or the second material is supported. Having a ledge portion may allow the first material and / or the second material to be supported during and / or after deposition, and / or may prevent or reduce undesired migration of the first material and / or the second material, which in turn may facilitate accurate deposition of the first material and / or the second material.
[0017] In an example, the method includes laser ablating the stack, and exposing one or more of the exposed portions by laser ablating the stack. Laser ablation can provide an efficient, reliable, fast and effective way to expose portions of the stack to allow connection of cells formed from the stack, which in turn can provide efficient production of energy storage devices.
[0018] According to a second aspect of the present invention, a stack for an energy storage device is provided, the stack comprising a first electrode layer, a second electrode layer and an electrolyte layer between the first electrode layer and the second electrode layer, the stack comprising a first material on a portion of the first electrode layer and a portion of the electrolyte layer; a second material, which is on the first material and in contact with the second electrode layer to provide an electrical connection to the second electrode layer so as to be connected to another such second electrode layer through the second material, wherein the first material insulates the portion of the first electrode layer and the portion of the electrolyte layer from the second material.
[0019] According to a third aspect of the present invention, there is provided an energy storage device formed according to the method of the first aspect.
[0020] Other features and advantages of the present invention will become apparent from the following description of preferred embodiments of the invention, given by way of example only, which description refers to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 is a schematic diagram showing a stack for an energy storage device according to an example;
[0022] Figure 2 is a diagram showing a method for processing according to an example Figure 1 A schematic diagram of a method of stacking to make an energy storage device;
[0023] Figure 3 is a flow chart illustrating a method of processing a stack according to an example;
[0024] Figure 4 and Figure 5 is a schematic diagram showing one way of processing a stack according to a first example;
[0025] Figure 6 and Figure 7 is a schematic diagram showing one way of processing a stack according to a second example;
[0026] Figure 8 and Fig. 9 is a schematic diagram showing one way of processing a stack according to a third example;
[0027] Fig.10 and Fig.11 is a schematic diagram showing one way of processing a stack according to a fourth example.
[0028] Fig.12 and Fig.13 is a schematic diagram showing one way of processing a stack according to a fifth example; DETAILED DESCRIPTION
[0029] Details of the methods, structures and devices according to the examples will become apparent with reference to the accompanying drawings, according to the examples. In this specification, many specific details of certain examples are set forth for the purpose of explanation. Reference to "example" or similar language in the specification means that a particular feature, structure or characteristic described in conjunction with the example is included in at least one example, but not necessarily in other examples. It should also be noted that certain examples are schematically described, in which certain features are omitted and / or must be simplified in order to facilitate explanation and understanding of the concepts underlying the examples.
[0030] Figure 1 A stack 100 of layers for an energy storage device is shown. For example, Figure 1 The stack 100 may be used as part of a thin film energy storage device having a solid electrolyte.
[0031] The stack 100 includes a substrate 102, a cathode layer 104, an electrolyte layer 106, and an anode layer 108. Figure 1 In the example of FIG. 1 , the anode layer 108 is further away from the substrate 102 than the cathode layer 104, and the electrolyte layer 106 is located between the cathode layer 104 and the anode layer 108. The substrate 102 contacts the cathode layer 104 and supports the stack. Although in this example, the substrate 102 contacts the cathode layer 104, in other examples, there may be other layers (not shown) between the substrate 102 and the cathode layer 104.
[0032] In some examples, substrate 102 may be or may include nickel foil; however, it should be understood that any suitable metal may be used, such as aluminum, copper, or steel, or metallized materials including metallized plastics, such as aluminum on polyethylene terephthalate (PET). In some examples, substrate 102 may not be metallic and / or may not conduct electrical current. For example, in some examples, the substrate may be polyethylene terephthalate (PET).
[0033] The cathode layer 104 may serve as a positive current collecting layer. The cathode layer 104 may form a positive electrode layer (i.e., corresponding to the cathode during discharge of a battery of an energy storage device including the stack 100). The cathode layer 104 may include a material suitable for storing lithium ions through a stable chemical reaction, such as lithium cobalt oxide, lithium iron phosphate, or an alkali metal polysulfide salt.
[0034] Anode layer 108 may serve as a negative current collecting layer. Anode layer 108 may form a negative electrode layer (ie, corresponding to the anode during discharge of a battery including an energy storage device of stack 100). Anode layer 108 may include lithium metal, graphite, silicon, or indium tin oxide.
[0035] In some examples, anode layer 108 may include a negative current collector and a separate negative electrode layer (not shown). In these examples, the negative electrode layer may include lithium metal, graphite, silicon, or indium tin oxide, and / or the negative current collector may include nickel foil. However, it should be understood that any suitable metal may be used, such as aluminum, copper, or steel, or metallized materials including metallized plastics, such as aluminum on polyethylene terephthalate (PET).
[0036] The electrolyte layer 106 may include any suitable material that is ionically conductive but is also an electrical insulator, such as lithium phosphorus oxynitride (LiPON). The electrolyte layer 106 may be a solid layer and may be referred to as a fast ion conductor. A solid electrolyte layer may have a structure between a liquid electrolyte and a crystalline solid, where a liquid electrolyte, for example, lacks a regular structure and contains ions that can move freely. Crystalline materials, for example, have a regular structure with an ordered arrangement of atoms that may be arranged in a two-dimensional or three-dimensional lattice. The ions of a crystalline material are generally immobile and therefore may not be able to move freely throughout the material.
[0037] For example, stack 100 may be fabricated by depositing cathode layer 104 on substrate 102. Electrolyte layer 106 is subsequently deposited on cathode layer 104, and then anode layer 108 is deposited on electrolyte layer 106. Each layer of stack 100 may be deposited by vapor deposition, such as physical vapor deposition, such as flooding deposition, which provides a simple and efficient way to produce highly uniform layers, although other deposition methods are possible.
[0038] Figure 1 The stack 100 may be processed to fabricate an energy storage device.
[0039] exist Figure 2 The schematic diagram shows the Figure 1 A general overview of an example of a process of stacking 100 .
[0040] exist Figure 2 In the example, stack 100 is processed to make an energy storage device. In this example, stack 100 is flexible, allowing it to be wound around roll 112, for example as part of a roll-to-roll manufacturing process (sometimes referred to as a reel-to-reel manufacturing process). Stack 100 can be gradually unwound from roll 112 and processed.
[0041] exist Figure 2 In an example of FIG. 1 , a cut or groove may be formed in the stack 100 using the first laser 114. The first laser 114 is arranged to apply a laser beam 116 to the stack 100 to remove a portion of the stack 100 by laser ablation, thereby forming the cut or groove.
[0042] After forming the cutouts or grooves, an insulating material system 118 can be used to introduce an electrically insulating material into the region of at least some of the cutouts or grooves. Electrically insulating materials can be considered to be non-conductive, so they can conduct a relatively small amount of current when subjected to an electric field. Typically, electrically insulating materials (sometimes referred to as insulators) conduct less current than semiconductor materials or conductive materials. However, there is still a small amount of current flowing through the electrically insulating material under the influence of the electric field, because even insulators may include a small amount of charge carriers that carry current. In the examples herein, such a material can be considered to be electrically insulating, where the material is electrically insulating enough to perform the function of an insulator. For example, this function can be performed when a material fully insulates one element from another element to avoid a short circuit.
[0043] Reference Figure 2 After the electrical insulating material is introduced, the stack 110 is cut to form individual cells for an energy storage device. In some examples, hundreds or even thousands of cells may be cut from a roll of the stack 100, allowing multiple batteries to be manufactured in an efficient manner.
[0044] exist Figure 2 In the embodiment, the cutting operation is performed using a second laser 122, which is arranged to apply a laser beam 124 to the stack 100. Each cut may, for example, pass through the center of the insulating plug so that the plug is divided into two parts, each part forming a protective covering on the exposed surface including the edge to which it has been attached.
[0045] Although not in Figure 2 , but it will be appreciated that after the insulating material is introduced (or otherwise), the stack may be folded back on itself to form a z-fold structure having, for example, tens, possibly hundreds, or even thousands of layers, with each insulating plug aligned. The laser cutting process performed by the second laser 122 may then be used to cut the z-fold structure for each of the aligned plug groups in a single cutting operation.
[0046] After cutting the battery, electrical connectors can be arranged along opposite sides of the battery so that a first electrical connector on one side of the battery contacts (multiple) cathode layers 104, but is prevented from contacting other layers by an electrically insulating material. Similarly, a second electrical connector on the opposite side of the battery can be arranged to contact (multiple) anode layers 108, but is prevented from contacting other layers by an insulating material. Thus, the insulating material can reduce the risk of short circuits between the anode layer 108 and the cathode layer 104 and between the other layers in each battery. The first and second electrical connectors can, for example, comprise a metallic material applied to the edge of the stack 100. Thus, the batteries can be effectively connected in parallel.
[0047] The foregoing description provides a general overview of an example of a stack 100 for an energy storage device, and examples of processes that may be applied to the stack 100 (e.g., for use in manufacturing an energy storage device). The following description provides examples of processes for processing the stack (which may be similar to those described in reference to Figure 1 Exemplary methods and apparatus for stack 100 (the same or similar to) described herein may provide improvements in processing efficiency of stack 200 and, therefore, for efficiently producing energy storage devices, such as batteries produced therefrom.
[0048] refer to Figure 3 , schematically illustrates a method of processing an energy storage device stack 200 according to an example.
[0049] In summary, the method includes obtaining a stack for an energy storage device in step 201, the stack including a first electrode layer, a second electrode layer, and an electrolyte layer between the first electrode layer and the second electrode layer. The method further includes, in step 203, depositing a first material on an exposed portion (e.g., a surface) of the first electrode layer and an exposed portion (e.g., a surface) of the electrolyte layer. The method further includes, in step 205, depositing a second material on the first material and in contact with the second electrode layer to provide an electrical connection to the second electrode layer for connection to another such second electrode layer through the second material. The first material insulates the exposed portion (e.g., a surface) of the first electrode layer and the electrolyte layer from the second material.
[0050] As explained in more detail below, the method may allow for an efficient and / or reliable parallel connection of batteries for an energy storage device and thus, for example, for an efficient production of an energy storage device.
[0051] Reference now Figure 4 and Figure 5 , schematically shows an energy storage device stack 200 according to a first example (i.e., can be based on reference Figure 3 ) obtained by an example of step 201 of the described method.
[0052] Stack 200 can be compared with reference Figure 1 The stack 100 described above is the same or similar. Figure 4 In the example shown, energy storage device stack 200 includes substrate layer 202, cathode layer 204, electrolyte layer 206, and anode layer 208. Figure 4 In the example shown, the first electrode layer 204 is a cathode layer 204 and the second electrode layer 208 is an anode layer 208. The layers 202-208 of the stack 200 may be similar to those of the reference Figure 1 The layers of the stack 100 described are the same or similar. For example, the cathode layer 204 may include a cathode electrode and a cathode current collector ( Figure 4), and the anode layer 208 may include an anode electrode and an anode current collector ( Figure 4 (not shown). Figure 4 In the example shown, electrolyte layer 206 is between cathode layer 204 and anode layer 208, cathode layer 204 is adjacent to substrate layer 202, electrolyte layer 206 is adjacent to cathode layer 204, and anode layer 208 is adjacent to electrolyte layer 206. In this example, substrate layer 202 is adjacent to cathode layer 204 relative to anode layer 208. In this example, substrate layer 202 may be or include a non-conductive material such as polyethylene terephthalate (PET), although other materials may be used.
[0053] like Figure 4 As shown, the energy storage device stack 200 has a cutout 212 formed therein. The cutout 212 may be formed in the stack 200 by laser ablation (not shown). The cutout 212 is formed in a first side 200a of the stack 200 away from the substrate layer 202. Figure 4 As shown, cutout 212 is formed through each of anode layer 208, electrolyte layer 206, and cathode layer 204, but not through substrate layer 202. Laser ablation to form the cutout may expose portions of substrate layer 202, cathode layer 204, electrolyte layer 206, and anode layer 208, such as surfaces (e.g., edges) 273, 274, 276, 278.
[0054] In some examples, such as Figure 4 and 5 As shown, the cutout 212 is defined only by exposed portions 274, 276, 278 of the cathode layer 204, electrolyte layer 206, and anode layer 208 (which in this example may also be considered as sides of the cutout 212) and by exposed portions (e.g., ledge 273) of the substrate layer 202 (which in this example may also be considered as a base surface or bottom surface forming the cutout 212). For example, the stack 200 may represent a segmented battery for an energy storage device, such as one that has been segmented from a larger stack structure (not shown). In these examples, Figure 4 and Figure 5 The portion of the stack 200 schematically shown in FIG. 1 may be the end of a terminal of a battery. In other words, in these examples, the stack 200 may be Figure 4 and Figure 5 It should be understood that in some examples, reference may be made to Figures 4 to 13 to describe the stacking of each example described in this article.
[0055] However, in other examples, the cutout 212 may be in the form of a groove. In the case where the cutout 212 is a groove, Figure 4 and 5It can be considered that only the left side of the groove is shown. As used herein, the term "groove" refers to a channel, slot or groove that can be continuous or discontinuous, can be elongated in some examples, and can only partially extend through the layers 202-208 of the stack 200. For example, the groove can be defined on a first side by exposed portions 274, 276, 278 of the cathode layer 204, electrolyte layer 206 and anode layer 208 (which can also be considered as the first side of the groove in this example), on a second side by an exposed ledge 273 of the substrate layer 202 (which can also be considered as the base surface or bottom surface forming the groove in this example), and on a third side (similar to the first side) by another exposed portion, such as a surface (not shown), of the cathode layer, electrolyte layer and anode layer (not shown) of the stack 200 (which can also be considered as the second side of the groove in this example). One or more such grooves 212 can be formed to divide the stack 200 into partial battery structures, but without (at this stage) completely separating those individual battery structures. It should be understood that in some examples, reference can be made to Figures 4 to 13 to describe the stacking of each example described in this article.
[0056] In the example where the cutout 212 is a groove, the (or each) groove may have a depth extending into the stack 200 in a direction substantially perpendicular to the plane of the layers 202-208; a width substantially perpendicular to the depth (in Figure 4 In the sense that each groove has a width and depth in the plane of the page), and a length extending in a direction substantially parallel to the plane of the layers 202-208 and substantially perpendicular to the width (i.e., in the plane of the page). Figure 4 In the case of multiple first grooves, they can be substantially parallel to each other in depth and length. Therefore, it should be understood that although reference will be made to cutouts 212 below, in each of the examples described herein, cutouts 212 can take the form of grooves, and in some examples there can be multiple such grooves formed in stack 200.
[0057] In either case, due to the cutout 212, as Figure 4 As shown, the first electrode layer (in this example, the cathode layer 204), the electrolyte layer 206, and the second electrode layer (in this example, the anode layer 208) are recessed from the substrate layer 202 so that the substrate layer 202 provides a ledge portion, such as a surface 273, on which, for example, the first material 210 and / or the second material 214 can be at least partially supported.
[0058] It should be noted that Figure 4 (similar to other figures) are schematic diagrams for illustration purposes only. For example, Figure 4The sizes and relative spacing of the features (eg, layers 202 - 208 , cutouts 212 or grooves) shown in are merely schematic and are used only to illustrate the example structures and processes described herein.
[0059] As used herein, "laser ablation" may refer to the use of a laser-based process to remove material from the stack 200. Such removal of material may include any of a number of physical processes. For example, the removal of material may include (but is not limited to) any or a combination of melting, melt expulsion, vaporization (or sublimation), photon decomposition (single photon), photon decomposition (multi-photon), mechanical shock, thermomechanical shock, other shock-based treatments, surface plasma processing, and removal by evaporation (ablation).
[0060] Specific reference Figure 4 , depositing the first material 210 on the exposed portion of the first electrode layer (in this example, the cathode layer 204), such as the surface 274, and the exposed portion of the electrolyte layer 206, such as the surface 276 (according to reference Figure 3 203 of the method described herein). The first material 210 is an electrically insulating material. An electrically insulating material can be considered to be non-conductive and therefore can conduct a relatively small amount of current when subjected to an electric field. Typically, electrically insulating materials (sometimes called insulators) conduct less current than semiconductor materials or conductive materials. However, a small amount of current still flows through the electrically insulating material under the influence of the electric field because even insulators may include a small amount of charge carriers that carry current. In the examples herein, such a material can be considered to be electrically insulating, where the material is electrically insulating enough to perform the function of an insulator. For example, this function can be performed where the material is sufficiently insulating to prevent a short circuit from occurring.
[0061] exist Figure 4 In the example shown, the first (insulating) material 210 is deposited by inkjet material deposition. That is, in this example, the deposition of the first material 210 uses inkjet technology to accurately deposit the first material 210 as droplets 224. In this example, the first material 210 is deposited in the form of ink by inkjet printing. The ink solidifies to form a solid material. However, it will be understood that in other examples, the first material can be deposited in a form other than ink, but can still be deposited using inkjet technology.
[0062] As mentioned, in this example, the first material is deposited by inkjet printing. That is, in this example, depositing the first material 210 includes inkjet printing the first material 210. In this example, the insulating ink is inkjet printed from an inkjet printing component (e.g., a nozzle 220 of a deposition device 230). The nozzle 220 prints droplets 224 of the insulating ink on the exposed portion 274 of the cathode layer 204 and the exposed portion 276 of the electrolyte layer 206.
[0063] In this example, the inkjet printing of the first material 210 is performed from top to bottom. In other words, in this example, the droplet 224 travels from the nozzle 220 to the stack 200 at a speed that has a component in the same direction as the force acting on the droplet 224 due to gravity. Performing the inkjet printing from top to bottom can allow the first material 210 to be accurately and efficiently deposited.
[0064] exist Figure 4 In the example of , the first (insulating) material 210 so printed is deposited onto and supported by an exposed portion or ledge 273 of the substrate layer 202. In this example, the print nozzle 220 is angled relative to the plane of the stack 200 to direct the ink droplets 224 into the corner region of the cutout 212, which is bounded by the exposed surfaces 274, 276 of the cathode layer 204 and the electrolyte layer 206 and the ledge 273 provided by the substrate layer 202. This can allow the first material 210 supported by the ledge 273 to accumulate on the exposed portions 274, 276 of the cathode layer 204 and the electrolyte layer 206, thereby covering the exposed portions 274, 276 of the cathode layer 204 and the electrolyte layer 206. In this example, the first material 210 is deposited so that it does not cover the exposed portion 278 of the anode layer 208.
[0065] Once printed, the insulating ink 210 can be cured. For example, the insulating ink can be cured by evaporation of a carrier solvent of the insulating ink, for example, occurring at ambient temperature. As another example, the curing of the insulating ink can be facilitated by an external curing device (not shown), such as by a heat source or an ultraviolet (UV) light source (not shown), for example, if the curing of the insulating ink is thereby facilitated.
[0066] Reference Figure 5 , as already mentioned in reference Figure 4 The first material 210 is deposited as described, and the second material 214 is deposited on the first material 210 and in contact with the second electrode layer (in this example, the anode layer 208) to provide an electrical connection with the second electrode layer 208 (according to reference Figure 3 205 of the method described above).
[0067] The second material 214 is used to electrically connect the second electrode layer 208 to another such second electrode layer ( Figure 4 or Figure 5200). The first material 210 insulates (i.e., electrically insulates) the exposed portions 276, 274 of the first electrode layer 204 and the electrolyte layer 206 from the second material 214. Thus, the second electrode layer 208 can be electrically connected to other such second electrode layers (not shown) of another such stack portion or battery (not shown) via the second material 214 to allow parallel electrical connection of the batteries, but the second material 214 does not cause a short circuit between the first electrode layer 204 and the second electrode layer 208 of the stack 200.
[0068] The second material 214 is a conductive material. For example, the second material 214 can have a lower electrical resistance, e.g., a significantly lower electrical resistance, than the first material 210. In any case, the second material 214 has an electrical conductivity sufficient to provide an effective electrical connection to the second electrode layer (in this example, the anode layer 208) for electrical connection to another such second electrode layer (not shown) via the second material 214.
[0069] exist Figure 5 In the example shown, the second (conductive) material 214 is deposited by inkjet material deposition, in this example, inkjet printing of a conductive ink. That is, in this example, depositing the second material 214 includes inkjet printing the second material 210. In this example, the conductive ink is inkjet printed from an inkjet printing component (e.g., a nozzle 220a of a deposition device 230). The nozzle 220a prints droplets 226 of the conductive ink on the first material 210 and in contact with the anode layer 208. In this example, the conductive ink 212 contacts and prints on the exposed portion 278 of the anode layer 208. In this example, the second (conductive) material 210 so printed is deposited onto and supported by the exposed portion or ledge 273 of the substrate layer 202, and supported by the first material. In this example, the print nozzle 220 is again angled relative to the plane of the stack 200 to direct a droplet 210 of conductive ink onto the first material 210 toward a corner region of the cutout 212, which is bounded by the surfaces 274, 276 of the cathode layer 204 and electrolyte layer 206 (which were once exposed but are now covered by the first material 210) and the ledge 273 provided by the substrate layer 202. This can allow the second material 214 deposited on and supported by the ledge 273 and / or the first material 210 to build up against the first material 210, thereby covering the exposed portion 278 of the anode layer 208. Once printed, the conductive ink can be cured in an appropriate manner. For example, the conductive ink can be cured in the same or similar manner as described for the insulating ink.
[0070] The second material 214 is used to connect (eg, electrically connect) the second electrode layer 208 to another such second electrode layer ( Figure 4 or Figure 5208 to the anode layer 208 of the battery. The first material 210 insulates (i.e., electrically insulates) the exposed portions 276, 274 of the cathode layer 204 and the electrolyte layer 206 from the second material 214, thereby preventing a short circuit between the anode layer 208 and the cathode layer 204. Therefore, the electrical connection of the anode layer 208 of the battery can be via the second material 214 to allow parallel electrical connection of the battery, but the second material 214 does not cause a short circuit between the anode layer 208 and the cathode layer 204. The connection of multiple batteries can allow the production of a relatively large capacity energy storage device. Connecting batteries in parallel can provide an energy storage device that can have a relatively large discharge rate, which may be useful in certain applications.
[0071] Depositing the first material 210 and / or the second material 214 by inkjet material deposition, such as inkjet printing, can allow for flexible, efficient, and / or reliable deposition. For example, inkjet printing can allow for more flexible, efficient, and / or reliable deposition than, for example, thermal spraying, in which the material is sprayed onto the stack at high temperature and vacuum. For example, thermal spraying can rely on the edges of the stack to be exposed and substantially perpendicular to the direction of spraying to be covered, or rely on wetting the material onto the edges. This can limit the arrangement of the stack or layers of the stack and can be unreliable. However, the higher degree of spatial and directional control provided by inkjet printing can allow small areas of the stack to be precisely and reliably targeted, which can improve the flexibility and reliability of deposition and, therefore, improve the efficiency of the battery produced thereby. As another example, the high temperatures associated with thermal spraying can deform or damage the stack or stack. However, deposition by inkjet printing can be performed at relatively low, for example, ambient temperatures, and can therefore reduce or prevent damage to the stack, thereby improving battery production efficiency. As another example, the vacuum conditions and / or high temperatures associated with thermal spraying may be energy intensive and thus may result in uneconomical or inefficient deposition. Inkjet printing, however, may be performed at relatively low (e.g., ambient) temperatures and / or pressures and thus may allow for economical and / or efficient deposition and, therefore, battery production.
[0072] In reference Figure 4 and Figure 5 In the first example described, the first electrode layer (on which the first material 210 is deposited) is the cathode layer 204 and the second electrode layer (contacted by the second material 214) is the anode layer 208. It will be appreciated that this need not necessarily be the case, as will be described below with reference to Figure 6 and 7 Described in more detail.
[0073] Reference now Figure 6 and Figure 7 , schematically shows an energy storage device stack 200 according to a second example (i.e., it can be based on reference Figure 3 ) obtained by an example of step 201 of the described method.
[0074] Stacking 200' can be compared with reference Figure 4 For the sake of brevity, the stack 200 described above will not be described in detail. Figure 4 and 5 The features of the stack 200 described are the same or similar Figure 6 and 7 Like features are denoted by like reference numerals.
[0075] exist Figure 6 In the example shown, similar to the first example, the energy storage device stack 200' includes a substrate layer 202, a cathode layer 204, an electrolyte layer 206, and an anode layer 208. However, in Figure 6 In the example shown, the first electrode layer 208 is an anode layer 208 and the second electrode layer 204 is a cathode layer 204. Figure 4 and 5 In the embodiment, the cathode layer 204, the electrolyte layer 206 and the anode layer 208 of the stack 200 are aligned with each other and recessed from the substrate layer 202, but in Figure 6 and 7 In the example of , the anode layer 208 and the electrolyte layer 206 are recessed from the cathode layer 204, thereby exposing the ledge of the cathode layer 204, such as the surface 275. The ledge 275 of the cathode layer 204 is used to at least partially support the first material 210 and / or the second material 214 deposited thereon. Figure 4 and Figure 5 , cathode layer 204 is recessed from substrate layer 202 such that substrate layer 202 provides a ledge, such as surface 273 , for at least partially supporting second material 214 .
[0076] Specific reference Figure 6 , a first material 210 is deposited on an exposed portion 278 of a first electrode layer (in this example, an anode layer 208) and an exposed portion 276 of an electrolyte layer 206. The first material 210 is an electrically insulating material. Again, the first material 210 can be deposited by inkjet material deposition such as inkjet printing. That is, in this example, again, the nozzle 200 of the deposition device 230 prints droplets 224 of insulating ink on the exposed portion 278 of the anode layer 208 and the exposed portion 276 of the electrolyte layer 206.
[0077] The insulating material 210 is supported by the exposed portions or ledges 275 of the cathode layer 204. Again, the print nozzles 220 are arranged to print from top to bottom and at an angle relative to the plane of the stack 200' to direct the ink drops 224 into the corner regions of the cutouts 212', which are defined by the exposed surfaces 278, 276 of the anode layer 208 and the electrolyte layer 206 and the ledges 275 provided by the cathode layer 204. This can allow the first material 210 supported by the ledges 275 to accumulate on the exposed portions 278, 276 of the anode layer 208 and the electrolyte layer 206, thereby covering the exposed portions 278, 276 of the anode layer 208 and the electrolyte layer 206.
[0078] In this example, the first material 210 is deposited so that it does not cover the exposed portion 274 of the cathode layer 204. Once printed, the insulating ink can be cured, for example, as described above with reference to Figure 4 and Figure 5 As described.
[0079] Reference Figure 7 , as already mentioned in reference Figure 6 The first material 210 is deposited as described, and the second material 214 is deposited on the first material 210 and in contact with the second electrode layer (in this example, the cathode layer 208). The second material 214 is a conductive material. Figure 7 In the example shown, the second (conductive) material 214 is deposited by inkjet material deposition, in this example inkjet printing, i.e., by printing droplets of conductive ink 226 from a nozzle 220a of a deposition device 230. The nozzle 220a prints droplets 226 of conductive ink on the first material 210 and in contact with the cathode layer 204. In this example, the conductive ink 212 contacts and prints on the exposed portion 274 of the cathode layer 204. In this example, the second (conductive) material 210 so printed is supported by a portion or ledge 273 of the substrate layer 202, a ledge 275 of the cathode layer 204, and the first material. The printing nozzle 220a can again be arranged for top-down printing and can be at an angle relative to the plane of the stack 200 so as to direct the droplets of conductive ink 226 so that the second material 214 supported by the ledges 273, 274 and / or the first material 210 accumulates to cover the exposed portion 274 of the cathode layer 274. Once printed, the conductive ink can be cured, for example, as described above with reference to Figure 4 and Figure 5 As described.
[0080] The second material 214 can provide an electrical connection from the cathode layer 204 to the cathode layers (not shown) of other batteries (not shown), thereby connecting the cathodes of the batteries in parallel. In this example, therefore, the second material 214 can form a negative terminal of an energy storage device including such a battery. The first material 210 insulates (i.e., electrically insulates) the anode layer 208 and portions 276, 278 of the electrolyte layer 206 (once exposed but now covered by the first material) from the second material 214, thereby preventing a short circuit between the anode layer 208 and the cathode layer 204. Thus, the electrical connection of the cathode layer 204 of the battery can be via the second material 214 to allow parallel electrical connection of the batteries, but the second material 214 does not cause a short circuit between the anode layer 208 and the cathode layer 204. Connecting batteries together can allow for the manufacture of relatively large capacity energy storage devices. Connecting batteries in parallel can allow for higher discharge rates for the energy storage device, which can be useful in certain applications. Depositing the first and / or second materials by inkjet material deposition such as inkjet printing can allow for flexible, efficient and / or reliable deposition, as described in reference Figure 4 and 5 Described.
[0081] exist Figures 4 to 7 In the first and second examples, the second (conductive) material 214 is deposited by inkjet material deposition, such as inkjet printing. It will be appreciated that this need not necessarily be the case, as will be described below with reference to Figure 8 and 9 Described in more detail.
[0082] refer to Figure 8 and Fig. 9 , showing a stack 200 according to a third example" (i.e., according to reference Figure 3 ) obtained by an example of step 201 of the described method.
[0083] Stack 200" similar to the reference above Figure 4 and Figure 5 The stack 200 is described, and therefore, for simplicity, features of the stack 200 of this third example that are the same or similar to the stack 200 of the first example will not be described again. Like features are represented by like reference numerals. Figure 8 Stacking 200" with Figure 4 The difference of stack 200 is that in Figure 8 In the stack 200 ″, the anode layer 208 ″ is only partially formed, i.e., Figure 8 The thickness of the anode layer 208" is less than Figure 4 The thickness of the anode layer 208 is determined by the thickness of the anode layer 208. The partially formed anode layer 208" defines a first exposed portion, such as a surface 278" formed by the cutout 212", and a second exposed portion or ledge 279. Figure 4The stack of 200 is the same as in Figure 8 In the stack 200", the substrate layer 202 is adjacent to the cathode layer 204 relative to the anode layer 208", that is, Figure 8 In other words, the anode layer 208 is positioned toward the first side 200a of the stack 200", opposite to the second side 200b of the stack 200" toward which the substrate layer 202 is positioned. Figure 8 In the sense that the partially formed anode layer 208" the second exposed portion or ledge 279 is upward.
[0084] Specific reference Figure 8 , depositing the first material 210 on the exposed portion 274 of the first electrode layer (in this example, the cathode layer 204) and the exposed portion 276 of the electrolyte layer 206. This process can be similar to that described above with reference to Figure 4 As shown, the first material 210 is deposited so that it does not cover the first exposed portion 278" of the partially formed anode layer 208". However, in this example, the first material 210 can be deposited to cover the first exposed portion 278" because as described in reference Fig. 9 Described in more detail, in this example, the second material 214" need not necessarily contact the first exposed portion 278" of the anode layer 208", and may alternatively or additionally contact a second exposed surface, such as a ledge 279 of the anode layer 208".
[0085] Reference Fig. 9 , as already mentioned in reference Figure 8A first material 210 is deposited as described, and a second material 214" is deposited on the first material 210 and in contact with a second electrode layer (in this example, the partially formed anode layer 208"). The second material 214" is a conductive material. In this example, the second material 214" is or includes an anode material. For example, the second material 214" can be or include the same material as the anode layer 208". In this example, the second (anode) material 214" is deposited on the partially formed anode layer 208". That is, in this example, the second (anode) material 214" is deposited on a second exposed surface or ledge 279 of the partially formed anode layer 208", thereby completing the anode layer 208. That is, after depositing the second (anode) material 214, the anode layer 208 can be formed completely rather than partially. The second (anode) material 214" is deposited on the first material 210 and on the ledge 273 of the substrate layer 202. The second (anode) material 214" can be deposited in the same or similar manner as the partially formed anode layer 208" is deposited. For example, the second (anode) material 214" can be deposited by vapor deposition, such as physical vapor deposition, such as overflow deposition, but other deposition methods can be used. For example, the deposition device 220b of the deposition equipment 230 can be arranged to deposit 226b the second (anode) material 214" on substantially the entire first side 200a of the stack 200".
[0086] The second (anode) material 214" is used to connect (e.g., electrically connect) to another such anode layer ( Figure 8 or Fig. 9208). For example, the conductive material 214" can provide an electrical connection from the anode layer 208 to the anode layers of other batteries (not shown), thereby connecting the anodes of the batteries in parallel. In this example, therefore, the second material 214 can form a positive terminal of an energy storage device including such a battery. The first material 210 insulates (i.e., electrically insulates) the exposed portions 274, 276 of the cathode layer 204 and the electrolyte layer 206 from the second (anode) material 214", thereby preventing a short circuit between the anode layer 208 and the cathode layer 204. Therefore, the electrical connection of the anode layer 208 of the battery can be via the second material 214 to allow parallel electrical connection of the batteries, but the second material 214 does not cause a short circuit between the anode layer 208 and the cathode layer 204. Depositing the anode material as the second material 214" can allow efficient deposition of the second material 214", and therefore efficient battery production. For example, depositing the anode material can allow the anode layer 208" of the resulting stack 200" to be only partially formed, and allow the deposited anode material to complete the anode layer 208". This can reduce the total amount of conductive and / or anode material used to produce a battery from the stack 200". As another example, the anode material can be relatively inexpensive. For example, the anode material can be inexpensive compared to conductive inks and / or to cathode materials. Therefore, using the anode material to provide the anode layer 208" with electrical connections to other such anode layers of other batteries can allow for reduced costs of battery production, and therefore can allow for more efficient battery production. As another example, deposition of the anode material can be relatively fast and / or inexpensive, for example by vapor deposition, such as physical vapor deposition, such as overflow deposition, for example, compared to inkjet printing. As another example, it can be efficient to use the same method and / or means to deposit the partially formed anode layer 208" and to deposit the second (anode) material 214", for example, compared to providing separate methods and / or means for each function.
[0087] It should be understood that in some examples, the second material provides electrical connection to the cathode layer 204. Figure 6 and Figure 7 The stack 200' is shown, and the second material provides electrical connection to the anode layer 208. Figure 4 and Figure 5 The stack 200 or Figure 8 and 9 The stack 200" shown may be different parts of the same stack, i.e., different terminals of the same battery (not shown). For example, Figure 6 and Figure 7 The electrical connection 212 shown for the cathode layer 204 can be provided on a first side of a cell (not shown) to provide a negative terminal for a given cell and for Figure 4 and 5 or Figure 8The electrical connection 212 of the anode 208 shown in Figure 9 can be provided on the opposite side of a given cell (not shown) to provide the positive terminal of the given cell. This can allow the above-described improvements in efficiency and / or reliability for providing the electrical connections of the cathode layer 204 and the anode layer 208 to the same cell, and thus can further improve the efficiency or reliability of the energy storage device provided thereby.
[0088] exist Figures 4 to 9 In the first to third examples of the stack 200, 200", there is only one anode layer 208, electrolyte layer 206 and cathode layer 204 supported on the substrate layer 202. It will be appreciated that this need not necessarily be the case, as will be described below with reference to Figures 10 to 13 Described in more detail.
[0089] refer to Fig.10 , shows a stack 200"' according to a fourth example (ie, it can be based on reference Figure 3 The stack 200"' may be similar to that of step 201 of the method described above. Figure 4 The stack 200 is described, therefore, for the sake of brevity, the same features will not be described in detail. Like features are represented by like reference numerals.
[0090] Fig.10 Stacking of 200"' with Figure 4 The difference of stack 200 is that Fig.10The stack 200'' includes another second electrode layer 208a (in this example, another anode layer 208a) and another electrolyte layer 206a between the another second electrode layer 208a and the first electrode layer (in this example, the cathode layer 204). More specifically, in this example, the stack 200'' includes not only the substrate layer 202, the cathode layer 204, the electrolyte layer 206 and the anode layer 208, but also includes a first another electrolyte layer 206a (deposited on the anode layer 208), another cathode layer 204a (deposited on the first another electrolyte layer 206a), a second another electrolyte layer 206b (deposited on the another cathode layer 204a) and another anode layer 208a (deposited on the second another electrolyte layer 206b). The stack 200'' of this fourth example can be referred to as a "multi-stack" or "multi-battery" stack because the stack 200'' has been formed on one substrate layer 202 that can constitute multiple batteries. For example, the cathode layer 204, the electrolyte layer 206 and the anode layer 208 may constitute a first battery, the anode layer 208, the first further electrolyte layer 206a and the further cathode layer 204a may constitute a second battery, and the further cathode layer 204a, the second further electrolyte layer 206b and the further anode layer 208a may constitute a third battery of the multi-battery stack 200″′. That is, in these examples, the anode layer 208 may serve as the anode layer for both the first battery and the second battery, and the further cathode layer 204a may serve as the cathode layer for both the second battery and the third battery. This may be an efficient arrangement because it may reduce the amount of anode and / or cathode material required to form multiple batteries.
[0091] and Figure 4 The stack of 200 is the same, Fig.10 The cutout 212'' in the stack 200'' causes the cathode layer 204, the electrolyte layer 206, and the anode layer 208 to be aligned and recessed from the substrate layer 202, such that the substrate layer provides a ledge 273. However, in Fig.10 In the stack 200", the cut 212" or groove is aligned with the first further electrolyte layer 206a, the further cathode layer 204a, the second further electrolyte layer 206b and the further anode layer 208a and recessed from the anode layer 208 so that the anode layer provides a ledge 279. In this example, the cut 212'" can be formed by multiple cutting steps, for example by laser ablation using different and / or offset laser beams. For example, the cut 212'" can be formed by first cutting the stack 200'" to expose the first further electrolyte layer 206a, the further cathode layer 204a, the second further electrolyte layer 206b and the further anode layer 208. Portions 276a, 274a, 276b, 278a and the ledge 279 of the anode layer 208; and then cutting the stack 200'" to expose the cathode layer 204, the electrolyte layer 206 and the portions 274, 276, 278 of the anode layer and the ledge 273 of the substrate layer 202.
[0092] and Figure 4 The stack of 200 is the same as in Fig.10 In the example of FIG. 2 , the first material 210 is deposited on the exposed edges 274 , 276 of the cathode layer 204 and the electrolyte layer 206 , and the first material 210 is supported by the ledge 273 of the substrate layer 202 . Fig.10 In the stack 200″, the first material 210 is also deposited on the exposed portions 276a, 276b of the other electrolyte layers 206a, 206b. More specifically, as Fig.10 As shown, the first material 210 is deposited on the exposed portions 276a, 274a, 276b of the first further electrolyte layer 206a, the further cathode layer 204a and the second further electrolyte layer 206b. The first material 210 is supported by the ledge 279 provided by the anode layer 208. As a result, the exposed portions 278, 278a of the anode layer 208 and the further anode layer 208a remain exposed. The first material can be deposited, for example, by inkjet printing, for example with reference to Figure 4 and Figure 5 As described.
[0093] Reference Fig.11 ,and Figure 5 As with the stack 200 of FIG. 1 , the second material 214 is deposited on the first material 210 and in contact with the second electrode layer (in this example, the anode layer 208). Fig.11 In the stack 200'', a second material 214 is deposited to also contact another second electrode layer (in this example, another anode layer 208). As a result, the anode layer 208 and the further anode layer 208 are connected (electrically connected) via the second material 214. In this example, the second material 214 is at least partially supported by a ledge 279 of the anode layer 208 and a ledge 273 of the substrate layer 202. The first material 210 electrically insulates the exposed portions 274, 276, 276a, 274a, 276b of the cathode layer 204, the electrolyte layer 206, the first further electrolyte layer 206a, the further cathode layer 204a and the second further electrolyte layer 206b from the second material 214.
[0094] The second material 214 may be deposited by inkjet material deposition, such as that described in reference Figure 4 or Figure 5 Alternatively, the other anode layer 208a may be partially formed, and the second material 214 may be or include an anode material that may be deposited using, for example, flood deposition, such as described with reference to Figure 8 and 9 described.
[0095] The second material 214 provides electrical connection from the anode layer 208 of the first and second cells of the multi-cell stack 200″′ to the further anode layer 208a of the third cell of the multi-cell stack, thereby connecting the first to third cells in parallel. Thus, the second material 214 can form a positive terminal of an energy storage device including such a cell. The first material 210 insulates (e.g., electrically insulates) the exposed portions 274, 276, 276a, 274a, 276b of the cathode layer 204, the electrolyte layer 206, the first further electrolyte layer 206a, the further cathode layer 204a, and the second further electrolyte layer 206b from the second material 214, thereby preventing a short circuit between the anode layer 208, 208a and the cathode layer 204, 204a. Thus, the electrical connection of the anode layers 208, 208a of the cells can be via the second material 214 to allow parallel electrical connection of the cells, but the second material 214 does not cause a short circuit between the anode layer 208, 208a and the cathode layer 204, 204a.
[0096] In such Fig.10 and 11 Providing electrical connections between cells in a multi-cell stack 200'" can provide efficient battery production. For example, the multi-cell stack 200'" can reduce the amount of substrate layer 202 for each cell, and thus can reduce the cost associated with providing the substrate layer 202. As another example, the second material 214 connecting multiple cells can be deposited in a single deposition, for example, compared to electrically connecting cells one by one, which can reduce time and therefore reduce costs.
[0097] exist Fig.10 and 11 In the fourth example of FIG. 1 , the anode layer 108 and the further anode layer 208a are electrically connected via the second material 214. It will be appreciated that this need not necessarily be the case, as will be described below with reference to Fig.12 and 13 Described in more detail.
[0098] refer to Fig.12 , shows a stack 200" according to a fifth example" (i.e., it can be based on reference Figure 3 The stack 200"" may be obtained by referring to step 201 of the method described above. Figure 6 The stack 200' described is similar. For the sake of brevity, the same features will not be described in detail. Like features are represented by like reference numerals. Fig.12 The stack of 200" and Figure 6 The difference of stacking 200' is that Fig.12The stack 200"" includes another second electrode layer 204a (in this example, another cathode layer 204a) and another electrolyte layer 206a between the another second electrode layer 204a and the first electrode layer (in this example, the anode layer 208). More specifically, in this example, the stack 200"" includes not only the substrate layer 202, the cathode layer 204, the electrolyte layer 206 and the anode layer 208, but also includes a first another electrolyte layer 206a (deposited on the anode layer 208), another cathode layer 204a (deposited on the first another electrolyte layer 206a), a second another electrolyte layer 206b (deposited on the another cathode layer 204a) and another anode layer 208a (deposited on the second another electrolyte layer 206b). Such a stack 200"" may be referred to as a "multi-stack" or "multi-battery" stack 200"" because the stack 200"" has been formed on one substrate 202 that may constitute multiple batteries. For example, the cathode layer 204, the electrolyte layer 206 and the anode layer 208 can constitute a first battery, the anode layer 208, the first another electrolyte layer 206a and another cathode layer 204a can constitute a second battery, and another cathode layer 204a, the second another electrolyte layer 206b and another anode layer 208a can constitute a third battery of the multi-battery stack 200".
[0099] and Figure 6 The cutout 212' of the stack 200' is the same as that of the stack 200'. Fig.12 The cutout 212"" in the stack 200"" causes the cathode layer 204 to be recessed from the substrate layer 202, such that the substrate layer 202 provides a ledge 273, and the electrolyte layer 206 and the anode layer 208 are aligned and recessed from the cathode layer 204, such that the cathode layer 204 provides a ledge 275. However, in Fig.12 In the stack 200", the cut 212"" or groove is such that the first further electrolyte layer 206a and the further cathode layer 204a are aligned with the electrolyte layer 206 and the anode layer 208, and the second further electrolyte layer 206b and the further anode layer 208a are aligned and recessed from the further cathode layer 204a so that the further cathode layer 204a provides a further ledge 275a. The cut 212"" can be formed by multiple cutting steps.
[0100] and Figure 6 The stacking is 200' like in Fig.12 In the example of FIG. 2 , the first material 210 is deposited on the exposed edges 276, 278 of the electrolyte layer 206 and the anode layer 208, and the first material 210 is supported by the ledge 275 of the cathode layer 204. Fig.12 In the stack 200″′′, the first material 210 is also deposited on the exposed portions 276a, 276b of the other electrolyte layers 206a, 206b. More specifically, as Fig.12As shown, the first material 210 is deposited on the exposed portions 276a, 278b, 278a of the first further electrolyte layer 206a, the second further electrolyte layer 206b and the further anode layer 208. The portion of the first material 210 covering the exposed portions 278b, 278a of the second further electrolyte layer 206b and the further anode layer 208 is supported by the ledge 275a provided by the first further cathode layer 204a. As a result, the exposed portions 274, 274a of the cathode layer 204 and the further cathode layer 204a remain exposed. The first material can be deposited, for example, by inkjet material deposition, such as inkjet printing, for example, with reference to Figure 6 and Figure 7 As described.
[0101] Reference Fig.13 ,and Figure 7 The stacking of 200" is the same as Fig.13 As shown, the second material 214 is deposited on the first material 210 and contacts the second electrode layer (in this example, the cathode layer 204). Fig.13 In the stack 200″″, the second material 214 is deposited to also contact the other second electrode layer (in this example, the other cathode layer 204a). As a result, the cathode layer 204 and the other cathode layer 204a are connected (electrically connected) via the second material 214. In this example, the second material 214 is at least partially supported by the ledge 275a of the other cathode layer 204a, the ledge 275 of the cathode layer 204 and the ledge 273 of the substrate layer 202. The first material 210 electrically insulates the exposed portions 276, 278, 276a, 276b, 278a of the electrolyte layer 206, the anode layer 208, the first other electrolyte layer 206a, the second other electrolyte layer 206b and the other anode layer 208a from the second material 214. The second material 214 can be deposited by inkjet printing, such as in reference Figure 6 or Figure 7 As described.
[0102] The second material 214 provides an electrical connection from the cathode layer 204 of the first battery of the multi-battery stack 200″′ to another cathode layer 204a of the second and third batteries of the multi-battery stack, thereby connecting the first to third batteries in parallel. Therefore, the second material 214 can form a negative terminal of an energy storage device including such batteries. The first material 210 prevents short circuits between the anode layers 208, 208a and the cathode layers 204, 204a. Therefore, electrical connection of the cathode layers 204, 204a of the batteries can be via the second material 214 to allow parallel electrical connection of the batteries, but the second material 214 does not cause a short circuit between the anode layers 208, 208a and the cathode layers 204, 204a.
[0103] For example, Fig.12 and Fig.13Providing electrical connections between cells in a multi-cell stack or multi-cell stack 200"' can provide efficient battery production, such as similar to the above reference Fig.10 and 11 As described.
[0104] It will be understood that although Figures 10 to 13 Only three batteries are provided in the multi-battery stack 200'", 200", but in other examples, there may be more or fewer batteries. For example, the multi-battery stack 200', 200"" may include a plurality of batteries, wherein the stack 200', 200"" includes at least a first electrode layer 204, 208, an electrolyte layer 206, a second electrode layer 204, 208, another electrolyte layer 206a, 206b and another second electrode layer 204a, 208a.
[0105] It should be understood that in some examples, the second material provides electrical connection to the cathode layer 204, 204a. Fig.12 and Fig.13 The stack 200''' is shown, and the second material provides electrical connection to the anode layer 208, 208a. Fig.10 and Fig.11 The stack 200'' shown may be different parts of the same multi-battery stack, ie, different terminals of the same battery (not shown). For example, Fig.12 and Fig.13 The electrical connection 212 shown for the cathode layer 204, 204a can be provided on a first side of a battery (not shown) to provide a negative terminal for the battery and for Fig.10 and 11 Electrical connections 212 to the anodes 208, 208a shown may be provided on opposite sides of a battery (not shown) to provide a positive terminal for the battery.
[0106] It will be understood that although in each of the above examples, the first material 210 is described as being deposited by inkjet material deposition, such as inkjet printing, this need not be the case, and in some examples, the first material 210 and / or the second material 210 may be deposited by methods other than inkjet material deposition.
[0107] It will be understood that reference Figures 3 to 13 The product of each of the examples described may be an intermediate product of an energy storage device production process, and in some examples, further processing may be performed on the stacks 200 - 200 ′″ to produce an energy storage device.
[0108] In the various examples described above, the intermediate product takes the form of a stack 200 - 200 ″″ for an energy storage device, the stack 200 - 200 ″″ including a first electrode layer 204 / 208 , a second electrode layer 204 / 208 , and an electrolyte layer 206 between the first electrode layer 204 / 208 and the second electrode layer 204 / 208 . The stack 200-200'" includes a first material 210 on a portion 274 / 278 of the first electrode layer 204 / 208 (i.e., the portion 274 / 278 to be exposed but covered by the first material 210) and a portion 276 of the electrolyte layer 206 (i.e., the portion 276 to be exposed but covered by the first material 210). The stack includes a second material 214 on the first material 210 and in contact with the second electrode layer 204 / 208 to provide an electrical connection from the second electrode layer 204 / 208 for connection to another second electrode layer 204a / 208a through the second material 214. The first material 210 insulates the exposed portions 274 / 278, 276 of the first electrode layer 204 / 208 and the electrolyte layer 206 from the second material 214.
[0109] The above examples should be understood as illustrative examples of the present invention. It should be understood that any feature described with respect to any one example can be used alone or in combination with other features described, and can also be used in combination with one or more features of any other example or any combination of other examples. In addition, without departing from the scope of the present invention defined in the appended claims, equivalents and modifications not described above may also be adopted.
Claims
1. A method for obtaining an energy storage device, comprising: A stack for an energy storage device is obtained, the stack comprising: a first electrode layer having an exposed portion; a partially formed second electrode layer having an exposed portion, the exposed portion of the partially formed second electrode layer having a first exposed surface and a second exposed surface adjacent to the first exposed surface, the first exposed surface defining a first plane, the second exposed surface defining a second plane different from the first plane, and an electrolyte layer between the first electrode layer and the partially formed second electrode layer, the electrolyte layer having an exposed portion; depositing a first material over the stack such that exposed portions of the first electrode layer and exposed portions of the electrolyte layer are covered by the first material, while exposed portions of the second electrode layer remain at least partially exposed; and depositing a second material on the first material and in contact with the partially formed second electrode layer to provide an electrical connection to the partially formed second electrode layer to connect to another such second electrode layer through the second material, the second material contacting the first exposed surface and the second exposed surface of the exposed portion of the partially formed second electrode layer, The first material thereby insulates the exposed portions of the first electrode layer and the exposed portions of the electrolyte layer from the second material.
2. The method according to claim 1, wherein: Depositing the first material includes inkjet material deposition of the first material.
3. The method according to claim 1, wherein: The stack includes a substrate adjacent to one of the first electrode layer and the second electrode layer, wherein the other of the first electrode layer and the second electrode layer is an anode layer.
4. The method according to claim 3, wherein: The anode layer comprises an anode material, and wherein the second material is the same as the anode material.
5. The method according to claim 3, wherein: Depositing the second material includes depositing the second material on the anode layer.
6. The method according to any one of claims 1 to 3, wherein: Depositing the second material includes inkjet material deposition of the second material.
7. The method according to claim 3, wherein: The first electrode layer, the electrolyte layer and the second electrode layer are recessed from the substrate such that the substrate provides a ledge portion on which the first material and / or the second material is at least partially supported.
8. The method according to any one of claims 1 to 3, wherein: The first electrode layer and the electrolyte layer are recessed from the second electrode layer such that the second electrode layer provides a ledge portion on which the first material and / or the second material is at least partially supported.
9. The method according to any one of claims 1 to 3, wherein: Another such second electrode layer belongs to another such stack.
10. The method according to any one of claims 1 to 3, wherein: The stack includes another second electrode layer, and another electrolyte layer between the another second electrode layer and the first electrode layer, wherein depositing the first material also includes depositing the first material on an exposed portion of the another electrolyte layer, and wherein depositing the second material also includes depositing the second material to contact the another second electrode layer, thereby connecting the second electrode layer and the another second electrode layer via the second material, so that the first material further insulates the exposed portion of the another electrolyte layer from the second material.
11. The method according to claim 10, wherein: The electrolyte layer, the first electrode layer, the further electrolyte layer and the further second electrode layer are recessed from the second electrode layer such that the second electrode layer provides a ledge on which the first material and / or the second material are supported.
12. The method according to any one of claims 1 to 3, wherein: The method comprises laser ablating the stack, and wherein one or more of the exposed portions are exposed by laser ablating the stack.
13. A stack for an energy storage device, the stack comprising a first electrode layer; a partially formed second electrode layer having an exposed portion, the exposed surface comprising a first exposed surface and a second exposed surface adjacent to the first exposed surface, the first exposed surface defining a first plane, the second exposed surface defining a second plane different from the first plane; and an electrolyte layer between the first electrode layer and the second electrode layer, the stack comprising a first material on a portion of the first electrode layer and a portion of the electrolyte layer, the first material not covering an exposed portion of the second electrode layer; A second material is on the first material and in contact with the first exposed surface and the second exposed surface of the exposed portion of the partially formed second electrode layer to provide an electrical connection to the second electrode layer to connect to another such second electrode layer through the second material, wherein the first material insulates the portion of the first electrode layer and the portion of the electrolyte layer from the second material.
14. An energy storage device formed according to the method of any one of claims 1 to 12.
Citation Information
Patent Citations
Process for the fabrication of a vertical lithium-ion battery
CN102035030A
Bipolar secondary battery, battery pack, and vehicle equipped with the same
CN102187504A
Microbattery and method for manufacturing same
CN102812579A
Electrochemical storing device and method of manufacturing the electrochemical storing device
CN103545543A
Stacking and sealing configurations for energy storage devices
CN103620823A