A packaging structure and implementation method of an integrated ceramic cold platform

By using a combination of brazing and high-energy beam welding in Dewar packages, the ceramic cold platform is integrated on the Dewar core column, which solves the structural complexity and weight increase problems caused by traditional metal cold platform, and realizes the ceramic cold platform High integration and lightweighting improve cooling capacity utilization and temperature uniformity.

CN113351951BActive Publication Date: 2024-11-19SHANGHAI INSTITUTE OF TECHNICAL PHYSICS CHINESE ACADEMY OF SCIENCES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110674843.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-06-18
Publication Date
2024-11-19
Estimated Expiration
2041-06-18

AI Technical Summary

Technical Problem

In the deep and low temperature package of large-scale surface array detectors, the use of metal cold platforms in traditional Dewar packages leads to structural complexity and weight increase, and it is difficult to achieve compatibility between ceramic materials and metal materials, which affects the utilization of cold volume. rate and temperature uniformity.

Method used

Using a combination of brazing and high-energy beam welding, the ceramic cold platform is directly integrated on the Dewar core column. By setting a metal transition ring on the back of the ceramic cold platform, the airtight concentric connection between the ceramic material and the metal core column is realized, instead Traditional metal cold platform.

Benefits of technology

The assembly structure is simplified, the weight is reduced, the cooling capacity utilization and temperature uniformity are improved, and the reliability and high integration of the ceramic cooling platform are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113351951B_ABST
    Figure CN113351951B_ABST
Patent Text Reader

Abstract

The present invention discloses a packaging structure and implementation method of an integrated ceramic cold platform. The packaging structure includes a detector module, a ceramic cold platform, a metal transition ring, a core column and other components, and is characterized in that: the upper surface of the ceramic cold platform is equipped with a detector module, and the lower surface is airtightly integrated with a metal transition ring, and the metal transition ring is airtightly and concentrically connected to the core column. The ceramic cold platform is integrated on the Dewar core column by a method combining brazing and laser welding, and the detector module is installed on the upper surface of the ceramic cold platform by epoxy glue. In this structure, the ceramic cold platform material is silicon carbide, silicon nitride or aluminum nitride material with high thermal conductivity and low expansion. Since silicon carbide, silicon nitride or aluminum nitride material is thermally matched with silicon material used for integrated circuits at low temperature, the balance layer structure used in the packaging of large-scale focal plane detectors can be omitted. The structure is simple, the utilization rate of refrigerator cooling is high, and the temperature uniformity is good. It is particularly suitable for the deep low temperature packaging of large-scale array detectors.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a packaging structure and a realization method of an integrated ceramic cold platform, which is applied to Dewar packaging, and is particularly suitable for the occasion of deep-cryogenic packaging of large-scale area array detectors. Background Art

[0002] Cooling infrared detector technology has a wide range of applications in space astronomy, earth observation, resources and environment. With the increasing requirements of spatial resolution, spectral resolution and other requirements of system applications, the scale of array detectors is expanding. 640×512 and 1K×1K products have matured, and international advanced manufacturers have launched 4K×4K products. With the expansion of detector scale, in order to achieve low-temperature thermal matching with silicon integrated circuits, new ceramic materials such as silicon carbide have begun to be used in detector packaging substrates. On the other hand, due to the increase in integration, the system has put forward more and more stringent indicators for component power consumption, lightweight and other indicators. The development of highly integrated, highly reliable, low-power and lightweight Dewar packaging has become a development trend. Summary of the invention

[0003] The purpose of the present invention is to provide a packaging structure and implementation method of an integrated ceramic cold platform, propose to remove the metal cold platform in the traditional Dewar, and directly integrate the ceramic cold platform on the Dewar core column by combining brazing and high-energy beam welding, thereby providing a new way to prepare a new type of highly integrated Dewar.

[0004] The directional terms such as "upper surface" and "lower surface" appearing in the present invention are used for the convenience of expression, and any description of the connection relationship based on the concept of the present invention belongs to the protection scope of the present invention.

[0005] A packaging structure of an integrated ceramic cold platform includes 1 detector module, 2 ceramic cold platforms, 3 metal transition rings, and 4 core columns. The upper surface of the 2 ceramic cold platforms is equipped with 1 detector module, and the lower surface is airtightly integrated with 3 metal transition rings, which are airtightly and concentrically connected with 4 core columns.

[0006] The 2 ceramic cold platform material is silicon carbide, silicon nitride or aluminum nitride, which has high thermal conductivity and a low-temperature expansion coefficient that matches that of silicon material.

[0007] The material of the four core columns is titanium alloy or stainless steel with low thermal conductivity and high strength.

[0008] The 3 metal transition rings are made of metal materials with expansion coefficients similar to those of the 2 ceramic cold platform materials and good metallurgical compatibility with the 4 core column materials; a 3-1 solder chamfer is provided on the inner side of the welding surface of the 3 metal transition rings and the 2 ceramic cold platform for storing overflow solder.

[0009] A method for implementing an integrated ceramic cold platform, the implementation steps are as follows:

[0010] ① Cleaning the sample surface: degreasing, pickling and alcohol cleaning of 2 ceramic cold platform, 3 metal transition ring and 4 core column;

[0011] ② Brazing connection: Silver-based brazing material is used to clamp between the 2 ceramic cold platform and the 3 metal transition ring, and fixed by vacuum brazing.

[0012] ③ Brazing leak detection: Check the brazing welds and detect leaks

[0013] ④ High-energy beam welding: After the 3 metal transition rings and the 4 core columns are concentrically assembled, they are connected and fixed by laser circumferential welding or electron beam circumferential welding.

[0014] ⑤ High-energy beam welding leak detection: Inspect and leak the high-energy beam seam.

[0015] ⑥ The detector module is bonded to the upper surface of (2) the ceramic cold platform by epoxy glue.

[0016] The most important feature of the packaging structure and implementation method of an integrated ceramic cold platform of the present invention is that a metal cold platform is no longer used in the structure, but a new type of low-expansion and high-thermal-conductivity ceramic cold platform is used. However, since the Dewar core column is made of metal material, the airtight connection between the cold platform and the core column needs to be considered. The present invention proposes to set a metal transition ring on the back of the ceramic, realize the heterogeneous connection between the ceramic material and the metal transition ring by vacuum brazing, and then connect the metal transition ring to the metal core column by high-energy beam welding, which solves the process compatibility problem. The structure of the present invention has two main advantages: since a metal cold platform and a balance layer structure are no longer required, the assembly structure is simpler, and the density of the ceramic material itself is small, which is beneficial to the lightweight of the Dewar and the reliability of the cold platform; second, the heat transfer interface in the structure is greatly reduced, which is beneficial to improving the utilization rate of the cold capacity of the refrigerator. In addition, the thermal conductivity of the ceramic material is very high, which is also beneficial to ensuring the temperature uniformity of the cold platform. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a cross-sectional view of the overall structure.

[0018] Figure 2 This is a cross-sectional view of the metal transition ring.

[0019] In the attached figure: 1—detector module, 2—ceramic cold platform, 3—metal transition ring, 4—core column, 3-1—solder chamfer. DETAILED DESCRIPTION

[0020] The present invention is further described in detail below in conjunction with the embodiments. However, it should not be understood that the scope of the above subject matter of the present invention is limited to the following embodiments, and all technologies realized based on the content of the present invention belong to the scope of the present invention.

[0021] Example 1

[0022] The present invention provides a packaging structure and implementation method of an integrated ceramic cold platform, such as Figure 1-2 , including detector module 1, ceramic cold platform 2, metal transition ring 3, and core column 4. The ceramic cold platform 2 is made of silicon carbide, the metal transition ring is made of Invar alloy, the solder chamfer 3-1 is R0.5, and the core column is made of 304 stainless steel; the 2 ceramic cold platform, 3 metal transition ring, and 4 core column are degreased, pickled with dilute sulfuric acid, and cleaned with alcohol ultrasonic; silver-copper-titanium active brazing material is clamped between the 2 ceramic cold platform and the 3 metal transition ring, and fixed by vacuum brazing. After brazing, the weld is inspected and the leakage rate is tested, and the leakage rate is better than 2×10 -10 Torr·L / s; After the 3 metal transition ring and the 4 core columns are concentrically assembled, they are connected and fixed by laser circumferential welding. After the laser welding is completed, the weld inspection and leakage rate test are carried out. The leakage rate is better than 2×10 -10 Torr·L / s; finally, the qualified detector module 1 is bonded to the upper surface of the ceramic cold platform 2 by epoxy glue.

[0023] Example 2

[0024] The same assembly structure and component cleaning method as in Example 1 are used, except that the ceramic cold platform 2 is made of silicon nitride, the metal transition ring is made of molybdenum, the solder chamfer 3-1 is R0.5, and the core column is made of TC4 titanium alloy; silver-copper-indium-titanium active solder is clamped between the 2 ceramic cold platforms and the 3 metal transition rings, and the connection is fixed by vacuum brazing. After the brazing is completed, the weld is inspected and the leakage rate is tested, and the leakage rate is better than 2×10 -10 Torr·L / s; After the 3 metal transition ring and the 4 core columns are concentrically assembled, they are connected and fixed by electron beam circumferential welding. After the electron beam welding is completed, the weld inspection and leakage rate test are carried out. The leakage rate is better than 2×10 -10 Torr·L / s; finally, the qualified detector module 1 is bonded to the upper surface of the ceramic cold platform 2 by epoxy glue.

[0025] Example 3

[0026] The same assembly structure and component cleaning method as in Example 1 are used, except that the ceramic cold platform 2 is made of aluminum nitride, the metal transition ring is made of TC4 titanium alloy, the solder chamfer 3-1 is R0.5, and the core column is made of TC4 titanium alloy; a silver-copper-titanium solder is clamped between the 2 ceramic cold platform and the 3 metal transition ring, and fixed by vacuum brazing. After brazing, the weld is inspected and the leakage rate is tested, and the leakage rate is better than 2×10 -10Torr·L / s; 1 detector module was bonded to the upper surface of 2 ceramic cold platform by epoxy glue, and performance screening was carried out. When the detector met the requirements, the detector module with 3 metal transition ring was concentrically assembled with 4 core columns, and then fixed by laser circumferential welding. After laser welding, weld inspection and leakage rate test were carried out, and the leakage rate was better than 2×10 -10 Torr·L / s.

Claims

1. A packaging structure of an integrated ceramic cold platform, comprising a detector module (1), a ceramic cold platform (2), a metal transition ring (3), and a core column (4); characterized in that: The upper surface of the ceramic cold platform (2) is mounted with a detector module (1), and the lower surface is airtightly formed with a metal transition ring (3), and the metal transition ring (3) is airtightly and concentrically connected to the core column (4); The material of the ceramic cold platform (2) is silicon carbide, silicon nitride or aluminum nitride; The core column (4) is made of titanium alloy or stainless steel; The metal transition ring (3) is made of a metal material having an expansion coefficient close to that of the ceramic cold platform (2) material and having good metallurgical compatibility with the core column (4) material. The metal transition ring (3) is made of Invar alloy, molybdenum or TC4 titanium alloy. A solder chamfer (3-1) is provided on the inner side of the welding surface between the metal transition ring (3) and the ceramic cold platform (2). The metal transition ring (3) is connected and fixed to the ceramic cold platform (2) by vacuum brazing using a silver-based solder at the solder chamfer (3-1).

2. A method for implementing a packaging structure of an integrated ceramic cold platform, characterized in that The steps are as follows: ① Cleaning the sample surface: degreasing, pickling and alcohol cleaning the ceramic cold platform (2), metal transition ring (3) and core column (4); ② Brazing connection: silver-based brazing material is selected and clamped between the ceramic cold platform (2) and the metal transition ring (3), and fixed by vacuum brazing; ③ Brazing leak detection: inspect and leak the brazing welds; ④ High-energy beam welding: After the metal transition ring (3) and the core column (4) are concentrically assembled, they are connected and fixed by laser circumferential welding or electron beam circumferential welding; ⑤ High-energy beam welding leak detection: inspect and leak test the high-energy beam welds; ⑥ The detector module is bonded to the upper surface of the ceramic cold platform (2) by epoxy glue.