Press-fit type semiconductor device
By designing the protection area and conductor film in the crimp-type semiconductor device, the problems of chip cracks and contact resistance changes are solved, and the reliability and productivity of the device are improved.
Patent Information
- Application Number
- CN201980093656.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-03-12
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2039-03-12
AI Technical Summary
In a crimp type semiconductor device, the semiconductor chip causes cracks due to local pressure concentration, and the pressure deviation in the module causes changes in the contact resistance between the intermediate electrode and the chip, which affects the reliability of the device.
A plurality of semiconductor chips are designed, with a first main electrode and a second main electrode on the surface and the back surface respectively, and are opposite to the first main electrode through the first intermediate electrode, and pressurized by the first common electrode plate to form a protective area and connection. In the region, a conductor film is partially formed to achieve electrical contact and avoid contact of the peripheral portion, thereby suppressing resistance changes.
It effectively suppresses the increase in the area of the semiconductor chip, and at the same time improves the uniformity of the electrical contact between the intermediate electrode and the chip, improves the reliability and productivity of the device, and reduces the disadvantages during assembly.
Smart Images

Figure CN113544828B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a pressure-contact semiconductor device. Background Art
[0002] Power modules for electric power convert or control high voltages of several thousand volts and large currents of several thousand amperes, and are required to have a further increased capacity. In a large-capacity power module, multiple semiconductor elements are installed in parallel. In recent years, the demand for power modules has increased in harsh environments such as offshore wind power generation, and power modules with high reliability and redundancy are required. Under such circumstances, crimping-type semiconductor devices have attracted attention instead of the previous bonding type. In a crimping-type semiconductor device, multiple semiconductor chips are mounted, and metal blocks are provided above and below the semiconductor chips as intermediate electrodes. Moreover, the intermediate electrode is pressed from above and below through a common electrode plate to maintain electrical contact inside the device.
[0003] Prior art literature
[0004] Patent Document 1: Japanese Patent Application Publication No. 2003-264266
[0005] Patent Document 2: Japanese Patent Application Publication No. 2005-72351 Summary of the invention
[0006] In a press-bonded semiconductor device, when the intermediate electrode presses the surface electrode of the semiconductor chip, the pressure is concentrated on the periphery of the intermediate electrode. Due to this local pressure application, the semiconductor chip may crack and be destroyed. In addition, the following problem occurs: due to the pressure deviation within the module surface, the contact resistance between the intermediate electrode and the semiconductor chip changes according to the pressure applied.
[0007] As a solution to this problem, the following method is disclosed in Patent Document 1: a buffer region is provided between the active region and the terminal region of the IGBT chip, a pedestal portion higher than the active region is provided in the buffer region, the outer periphery of the surface intermediate electrode is pressurized while squeezing the pedestal portion, and the central portion of the block contacts the active region. This method can suppress the contact between the outer periphery of the surface intermediate electrode and the surface electrode of the semiconductor chip. However, in order to newly provide the buffer region, the chip size needs to be increased, which leads to a large module and a reduction in productivity. In addition, a process of forming a pedestal on the buffer region is required, so the manufacturing process becomes complicated.
[0008] The present invention has been made to solve the above-mentioned problems, and an object of the present invention is to suppress the electrical contact between the outer peripheral portion of the intermediate electrode and the surface electrode of the semiconductor chip without increasing the area of the semiconductor chip.
[0009] The press-contact semiconductor device of the present invention comprises: a plurality of semiconductor chips, each having a first main electrode and a second main electrode on the front and back sides, respectively; a first intermediate electrode, which is opposite to the first main electrode of the semiconductor chip; a first common electrode plate, which is arranged on the side of the first intermediate electrode opposite to the surface facing the first main electrode; and a second common electrode plate, which is arranged opposite to the second main electrode, wherein the surface facing the first intermediate electrode to the first main electrode is smaller than the surface facing the first main electrode to the first intermediate electrode, and comprises a peripheral protection area and a connection area surrounded by the protection area. The press-contact semiconductor device of the present invention comprises: a plurality of first conductor films partially formed in the connection area; and a first insulating film, which is formed in the area where the first conductor film is not formed and the protection area in the connection area.
[0010] According to the press-contact type semiconductor device of the present invention, the first intermediate electrode is electrically connected to the first main electrode in the connection region through the first conductor film, so that the area of the semiconductor chip is not increased, and the outer periphery of the first intermediate electrode can be prevented from being electrically in contact with the outer periphery of the semiconductor chip. The purpose, features, aspects and advantages of the present invention will become more apparent through the following detailed description and drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 It is a cross-sectional view of a pressure-bonded semiconductor device of the underlying technique.
[0012] Figure 2 This is a diagram showing the structure of the contact portion between the anode intermediate electrode and the diode chip in the first embodiment.
[0013] Figure 3 This is a diagram showing the structure of the contact portion between the emitter intermediate electrode and the IGBT chip in the first embodiment.
[0014] Figure 4 This is a plan view of a contact surface of a surface intermediate electrode with respect to a semiconductor chip in a modification of the first embodiment.
[0015] Figure 5 This is a plan view of a contact surface of a surface intermediate electrode with respect to a semiconductor chip in a modification of the first embodiment.
[0016] Figure 6 This is a plan view of a contact surface of a surface intermediate electrode with respect to a semiconductor chip in a modification of the first embodiment.
[0017] Figure 7 This is a plan view of a contact surface of a surface intermediate electrode with respect to a semiconductor chip in a modification of the first embodiment.
[0018] Figure 8 This is a plan view of a contact surface of a surface intermediate electrode with respect to a semiconductor chip in a modification of the first embodiment.
[0019] Fig. 9 This is a diagram showing the structure of a contact portion between an emitter intermediate electrode and an IGBT chip in the second embodiment.
[0020] Fig.10 This is a diagram showing a mounting example of a pressure-bonded semiconductor device according to the second embodiment.
[0021] Fig.11 This is a schematic diagram of a cross section passing through the gate wiring of the IGBT chip according to the second embodiment.
[0022] Fig.12 This is a diagram showing the structure of the contact portion between the emitter intermediate electrode and the IGBT chip in the third embodiment.
[0023] Fig.13 It is along Fig.12 The cross-sectional view of the IGBT chip along the A-A' line.
[0024] Fig.14 This is a diagram showing the structure of the contact portion between the anode intermediate electrode and the diode chip in the third embodiment.
[0025] Fig.15 It is along Fig.14 Cross-sectional view of the diode chip along line BB'.
[0026] Fig.16 This is a top view of an IGBT chip according to the fourth embodiment.
[0027] Fig.17 It is along Fig.16 The cross-sectional view of the IGBT chip along the C-C' line.
[0028] Fig.18 This is a cross-sectional view of a section passing through the gate wiring of the IGBT chip according to the fourth embodiment.
[0029] Fig.19 This is a plan view of the contact surface of the emitter intermediate electrode with respect to the IGBT chip in the fourth embodiment.
[0030] Fig. 20 This is an equivalent circuit diagram of an IGBT chip according to the fourth embodiment.
[0031] (Explanation of symbols)
[0032] 102: Chip guiding part; 103: Adhesive; 104: Collector intermediate electrode guiding part; 200: IGBT chip; 201, 303: Terminal area; 202: Emitter electrode; 203: Gate pad; 204: Collector electrode; 205: Gate wiring; 206, 210, 304, 306: Insulating film; 207, 207b, 305, 407, 407b: Conductor film; 208: Semiconductor layer; 209: Polysilicon layer; 211: Gate metal layer; 212: Protective film; 300: Diode chip; 301: Anode electrode; 302: Cathode electrode; 400: Surface intermediate electrode; 401: Emitter intermediate electrode; 402: Anode intermediate electrode; 403: Emitter common electrode plate; 404: Connection area; 405: Protection area; 500: Back surface intermediate electrode; 501: Collector intermediate electrode; 502: Cathode intermediate electrode; 503: Collector common electrode plate; 601: Control terminal; 701: IGBT terminal; 702: Parasitic buffer circuit. Detailed implementation mode
[0033] <A. Basic technology>
[0034] Figure 1 It is a cross-sectional view of the press-pack type semiconductor device 100 of the basic technology. The press-pack type semiconductor device 100 includes a plurality of IGBT (Insulated Gate Bipolar Transistor) chips 200 and a plurality of diode chips 300. Here, as examples of semiconductor chips, IGBT chips and diode chips are listed.
[0035] On the surface of the IGBT chip 200, there are provided a terminal area 201, an emitter electrode 202 as a surface electrode, and a gate pad 203, and on the back surface, there is provided a collector electrode 204. The emitter electrode 202 is also referred to as the first main electrode, and the collector electrode 204 is also referred to as the second main electrode. An emitter intermediate electrode 401 is provided directly above the emitter electrode 202. In other words, the emitter intermediate electrode 401 faces the emitter electrode 202 of the IGBT chip 200. A collector intermediate electrode 501 is provided directly below the collector electrode 204.
[0036] An anode electrode 301 and an end region 303 as surface electrodes are provided on the surface of the diode chip 300, and a cathode electrode 302 is provided on the back surface. An anode intermediate electrode 402 is provided just above the anode electrode 301. A cathode intermediate electrode 502 is provided just below the cathode electrode 302. In this specification, the emitter intermediate electrode 401 and the anode intermediate electrode 402 are collectively referred to as the surface intermediate electrode 400, and the collector intermediate electrode 501 and the cathode intermediate electrode 502 are collectively referred to as the back intermediate electrode 500. In addition, the surface intermediate electrode 400 is also referred to as the first intermediate electrode. In addition, the surface intermediate electrode 400 and the back intermediate electrode 500 are also simply collectively referred to as the intermediate electrode.
[0037] An emitter common electrode plate 403 as the first common electrode plate is provided on the upper part of the surface intermediate electrode 400, and a collector common electrode plate 503 as the second common electrode plate is provided on the lower part of the back intermediate electrode 500. In this specification, the emitter common electrode plate 403 and the collector common electrode plate 503 are simply collectively referred to as common electrode plates. By pressurizing the common electrode plate from top to bottom, the IGBT chips 200 and the diode chips 300 are connected in parallel via the intermediate electrode, and the IGBT chip 200 and the diode chip 300 are connected in anti-parallel. That is, the diode chip 300 functions as a freewheeling diode (FWD). In addition, the semiconductor chip can also be in direct contact with the collector common electrode plate 503, in which case the back intermediate electrode 500 is not required.
[0038] A control terminal 601 provided with a spring pin or the like is connected to the gate pad 203 of the IGBT chip 200. The control terminal 601 is led out of the frame and connected to a gate drive circuit (not shown). The common electrode plate is formed of a metal plate such as copper. The intermediate electrode is formed of a metal such as copper, tungsten or molybdenum. The back intermediate electrode 500 is fixed to the collector electrode 204 and the cathode electrode 302, for example, by solder or the like. In order to reduce the contact resistance, a plating film such as nickel may also be formed on the contact surface between the intermediate electrode and the semiconductor chip.
[0039] The surface intermediate electrode 400 is Figure 1 Although it is shown as a simple metal block in the figure, it can also be a structure in which the metal block and the spring on the top are integrated. If it is such a structure, the deviation of the pressure applied between the semiconductor chips can be absorbed by the spring.
[0040] When pressing the flip-chip semiconductor device 100 from above and below, the pressure applied to the surface intermediate electrode 400 concentrates on the outermost periphery of the metal block. In order to reduce the resistance between the semiconductor chip and the surface intermediate electrode 400 or to suppress the occurrence of arc discharge during short-circuit breakdown, it is necessary to apply a sufficiently high pressure to the common electrode plate. Thus, if a high pressure is locally applied to the outer peripheral portion of the semiconductor chip via the surface intermediate electrode 400, it will cause cracks in the semiconductor chip.
[0041] The contact area between the surface electrode of the semiconductor chip and the surface intermediate electrode 400 gradually increases from the outer periphery toward the inside as the pressure increases. If there is a deviation in the pressure applied to each semiconductor chip, the contact resistance between the surface electrode of each semiconductor chip and the surface intermediate electrode 400 will deviate, resulting in uneven current, so the reliability of the flip-chip semiconductor device 100 is reduced.
[0042] Therefore, in the following embodiments, a flip-chip semiconductor device will be described that suppresses changes in the contact resistance between the outer peripheral portion of the surface intermediate electrode 400 and the surface electrode of the semiconductor chip without increasing the area of the semiconductor chip.
[0043] <B. Embodiment 1>
[0044] The flip-chip semiconductor device of Embodiment 1 is a structure obtained by studying the contact portion between the surface intermediate electrode 400 and the semiconductor chip with respect to the flip-chip semiconductor device 100 of the basic technology shown in Figure 1 The other structures are the same as those of the flip-chip semiconductor device 100. Hereinafter, Figure 2 and Figure 3 will be used to describe the structure of the contact portion between the surface intermediate electrode 400 and the semiconductor chip in the flip-chip semiconductor device of Embodiment 1.
[0045] Figure 2 The structure on the side of the diode chip 300 is shown. In Figure 2 the upper part shows the contact surface of the anode intermediate electrode 402 with the diode chip 300, the middle part shows the cross-sectional view of the anode intermediate electrode 402, and the lower part shows the cross-sectional view of the diode chip 300.
[0046] Figure 2 The dotted line in
[0047] The contact surface of the surface intermediate electrode 400 with respect to the semiconductor chip is divided into a protection region 405 at the outer periphery and a connection region 404 inside the protection region 405. A plurality of conductor films 407 are formed in the connection region 404, and electrical contact between the surface intermediate electrode 400 and the semiconductor chip is achieved through the connection region 404. The width 405b of the protection region 405 is preferably about 5 to 15% of the length of one side of the metal block constituting the anode intermediate electrode 402. The region where the conductor film 407 is not formed in the protection region 405 and the connection region 404 is covered with an insulating film 406. The conductor film 407 is preferably arranged point-symmetrically with respect to the center of gravity of the contact surface of the anode intermediate electrode 402 with respect to the diode chip 300.
[0048] Figure 3 FIG. 2 shows the structure of the IGBT chip 200 side. Figure 3 In FIG. 1 , the upper portion shows the contact surface of the emitter intermediate electrode 401 with the IGBT chip 200 , the middle portion shows a cross-sectional view of the emitter intermediate electrode 401 , and the lower portion shows a cross-sectional view of the IGBT chip 200 .
[0049] Figure 3 The dotted line indicates the positional relationship between the emitter intermediate electrode 401 and the IGBT chip 200. As shown by the dotted line, the contact surface of the emitter intermediate electrode 401 with respect to the IGBT chip 200 is smaller than the emitter electrode 202 of the IGBT chip 200. In other words, the emitter intermediate electrode 401 is arranged inside the emitter electrode 202. As long as this condition is met, the contact surface of the emitter intermediate electrode 401 with respect to the IGBT chip 200 can have any size and shape.
[0050] Similar to the anode intermediate electrode 402 , the contact surface of the emitter intermediate electrode 401 with respect to the IGBT chip 200 is divided into a protection region 405 and a connection region 404 . The arrangement of the conductor film 407 in the protection region 405 is the same in the anode intermediate electrode 402 and the emitter intermediate electrode 401 .
[0051] While the pressure applied to the surface intermediate electrode 400 is small, pressure is applied only to the outer periphery of the surface intermediate electrode 400. However, as the pressure increases, pressure is gradually applied to the inner side of the surface intermediate electrode 400. Figure 2 , Figure 3 Since the contact surface of the surface intermediate electrode 400 with respect to the semiconductor chip is configured as shown, each conductor film 407 and the semiconductor chip are pressed in a well-balanced manner, and variations in contact resistance are suppressed.
[0052] For example, the insulating film 406 is formed by depositing oxide or nitride by sputtering or evaporation. Alternatively, the insulating film 406 is formed by spraying an insulating paint or resin with a sprayer or by spin coating an insulating paint or resin with a spin coater. At this time, the region where the conductor film 407 is formed is protected by a metal mask or a tape to prevent the insulating film from being formed in the region. Alternatively, after the insulating film is formed as a whole, the insulating film in the region where the conductor film 407 is formed is removed.
[0053] The conductor film 407 is formed by forming a metal film by sputtering, vapor deposition, or the like, similarly to the insulating film 406. Alternatively, a thick metal film may be formed by electroplating to serve as the conductor film 407.
[0054] The press-bonded semiconductor device of the first embodiment includes: a plurality of semiconductor chips having a first main electrode and a second main electrode on the front and back surfaces, respectively; a front intermediate electrode 400 as a first intermediate electrode facing the first main electrode of the semiconductor chip; an emitter common electrode plate 403 as a first common electrode plate provided on the side of the front intermediate electrode 400 opposite to the surface facing the first main electrode; and a collector common electrode plate 503 as a second common electrode plate provided facing the second main electrode. The surface facing the first main electrode of the front intermediate electrode 400 is smaller than the surface facing the first main electrode of the first main electrode, and the surface facing the first main electrode of the front intermediate electrode 400 has a peripheral protection region 405 and a connection region 404 surrounded by the protection region 405. The press-contact semiconductor device of the first embodiment includes: a plurality of conductor films 407 as first conductor films partially formed in a connection region 404; and an insulating film 406 as a first insulating film formed in a region of the connection region 404 where the conductor film 407 is not formed and a protection region 405.
[0055] Through the above structure, according to the compression-bonded semiconductor device of embodiment 1, the surface intermediate electrode 400 is not connected to the first main electrode of the semiconductor chip in the protection area 405 of the periphery but in the connection area 404, so the area of the semiconductor chip will not be increased, and the peripheral part of the surface intermediate electrode 400 can be prevented from electrically contacting the peripheral part of the semiconductor chip.
[0056] In addition, when the conductive film 407 is arranged point-symmetrically with respect to the center of gravity of the contact surface of the surface intermediate electrode 400, that is, the opposing surface of the contact surface with respect to the semiconductor chip, the contact resistance between each surface intermediate electrode 400 and the semiconductor chip is uniformized. As a result, the deviation of the current flowing between the semiconductor chips in the press-bonded semiconductor device is suppressed, and the reliability of the press-bonded semiconductor device is improved.
[0057] In addition, by using a soft resin such as polyimide as the material of the insulating film 406, the insulating film 406 can also function as a buffer material in the outer periphery of the surface intermediate electrode 400 to which high pressure is applied. Thus, even if high pressure is applied, cracks in the semiconductor chip are suppressed, and the productivity and reliability of the press-bonded semiconductor device can be improved.
[0058] Furthermore, by covering the outer periphery of the surface intermediate electrode 400 with the insulating film 406, even if a positional misalignment occurs between the semiconductor chip and the surface intermediate electrode 400 and the surface intermediate electrode 400 presses the gate pad 203 or the terminal region 201, 303, electrical short circuits will not occur, thereby reducing defects during assembly.
[0059] In one embodiment of the prior art document 2, a buffer plate is provided opposite to the emitter electrode of the IGBT chip. The buffer plate of the prior art document 2 includes a plurality of electrode components and an insulating component separating the electrode components. The buffer plate is considered to be equivalent to the surface intermediate electrode in the present embodiment 1. The common point between the press-contact type semiconductor device of the embodiment 1 and the prior art document 2 is that the area where the surface intermediate electrode can be energized is limited. However, in the prior art document 2, there is no record related to the configuration and area of the conductor area in the surface intermediate electrode.
[0060] For example, when multiple conductor regions are designed to contact each other in the periphery and the center of the IGBT chip, the pressure of the surface intermediate electrode is generally concentrated on the periphery, so the periphery of the IGBT chip and the conductor portion of the surface intermediate electrode are preferentially in contact. In this case, the current-carrying area is limited in the periphery, so the electrical resistance between the collector-emitter electrode increases, and the loss of the power module increases. Or, since the current-carrying area is excessively limited, the current is concentrated and heat is generated, and the IGBT chip may be damaged. Moreover, if the pressure is increased, the center of the IGBT chip also contacts the emitter electrode of the surface intermediate electrode, so as the pressure increases, the contact area between the IGBT chip and the surface intermediate electrode increases, and the resistance between the collector-emitter electrode decreases. The resistance of the IGBT chip changes according to the pressure, so the amount of current flowing between the IGBT chips in the press-contact semiconductor device becomes uneven, and the reliability of the device decreases.
[0061] On the other hand, according to this embodiment, the conduction region is limited to the region where uniform pressure is applied, so a stable collector-emitter electrode resistance can be obtained regardless of pressure variations. Thus, a highly reliable press-bonded semiconductor device can be obtained without increasing losses.
[0062] Furthermore, according to the manufacturing method of the prior art, the conductor component and the insulating component are made of different materials, and a single surface intermediate electrode is formed by combining the two. On the other hand, in the manufacturing method of this embodiment, the insulating region and the conductor region are formed by patterning the surface of the surface intermediate electrode 400. Therefore, the number of components does not increase, so the advantages of easy manufacturing and high degree of freedom in designing the conductor region can be obtained.
[0063] Figures 4 to 8 FIG. 4 shows a modified example of the contact surface of the surface intermediate electrode 400 with respect to the semiconductor chip. Figure 2 and Figure 3 In the embodiment, the conductor film 407 is not formed at the center of gravity of the surface intermediate electrode 400. However, Figure 4 As shown in FIG. 4 , a conductor film 407 is formed at the center of gravity of the surface intermediate electrode 400. The number of divisions of the conductor film 407 is arbitrary, and for example, Figure 5 There are 4 as shown. Figure 6 The following are 16 Figure 7 The conductor films 407 are preferably shaped the same, but the above-mentioned effects can be obtained even if the sizes are not necessarily the same. In addition, the shape of the conductor films 407 may not be circular, for example, Figure 8 A rectangular shape is shown. Alternatively, conductor films 407 having a plurality of shapes may be used in combination.
[0064] exist Figure 1 In the present invention, an IGBT and a freewheeling diode are used in the semiconductor chip mounted on the compression-contact semiconductor device 100, but the type of semiconductor chip is not limited to this. For example, a MOSFET (Metal-Oxide-Semiconductor Field-Effect Transistor) can be used instead of an IGBT. In addition, the number of IGBT chips 200 and the number of diode chips 300 can be arbitrarily changed according to the rated current of the module. The number of IGBT chips 200 and the number of diode chips 300 can also be different. For example, the number of IGBT chips 200 can also be twice the number of diode chips 300. In the substrate of the semiconductor chip, any material such as silicon, gallium nitride, silicon carbide, aluminum nitride, gallium oxide or diamond is used according to the application.
[0065] In addition, a reverse-conducting IGBT (RC-IGBT) may be used instead of the IGBT chip 200 and the diode chip 300. In this case, the structure of the contact surface of the surface intermediate electrode 400 with respect to the reverse-conducting IGBT chip can be applied. Figure 3 The structure shown.
[0066] <C. Embodiment 2>
[0067] This is an embodiment obtained by changing the structure of the contact portion between the emitter intermediate electrode 401 and the IGBT chip 200 in the press-fit type semiconductor device of Embodiment 1. Hereinafter, using Figures 9 to 11 , the structure of the contact portion between the emitter intermediate electrode 401 and the IGBT chip 200 in the press-fit type semiconductor device of Embodiment 2 will be described.
[0068] In Fig. 9 , the upper part shows the contact surface of the emitter intermediate electrode 401 with the IGBT chip 200, and the lower part is a top view of the IGBT chip 200. In the IGBT chip 200, in order to supply gate current to each unit from the gate pad 203, gate wirings 205 are provided as control wirings electrically separated from the emitter electrode 202. The gate wirings 205 are low-resistance wiring layers formed on the chip surface隔着SiO2 or the like on the semiconductor substrate. The gate wirings 205 can also be, for example, a metal film such as aluminum, a polysilicon film highly doped with impurities, or a stacked film thereof. In addition, in Fig. 9 , two gate wirings 205 are depicted at the lower part, but the number of gate wirings 205 can be arbitrarily changed according to the chip size. Also, the gate pad 203 is arranged at an arbitrary position within the IGBT chip 200.
[0069] In Fig. 9 , the dotted circle depicted within the emitter electrode 202 at the lower part indicates the position where the conductor film 407 at the upper part of Fig. 9 contacts. In the press-fit type semiconductor device of Embodiment 2, the conductor film 407 is formed so as not to contact the gate wirings 205 of the IGBT chip 200, which is different from the press-fit type semiconductor device of Embodiment 1. In order to achieve this structure, the alignment accuracy between the emitter intermediate electrode 401 and the IGBT chip 200 must be sufficiently high.
[0070] Fig.10 An installation example of a press-fit type semiconductor device that achieves high alignment accuracy is shown. In Fig.10 , the IGBT chip 200 is fixed to the collector intermediate electrode 501 using solder. A collector intermediate electrode guide portion 104 is provided in the collector common electrode plate 503, and the collector intermediate electrode 501 is arranged on the collector common electrode plate 503 along the collector intermediate electrode guide portion 104. That is, the position of the collector intermediate electrode 501 within the module is defined by the collector intermediate electrode guide portion 104.
[0071] On the outer periphery of the IGBT chip 200, a protective film 212 of the end region 201 is formed using polyimide or the like. The chip guide portion 102 is placed on the protective film 212 and fixed using the adhesive 103. The chip guide portion 102 is formed of, for example, silicone resin. Next, the emitter intermediate electrode 401 is placed on the IGBT chip 200 using the chip guide portion 102, thereby preventing the positional deviation between the emitter intermediate electrode 401 and the IGBT chip 200.
[0072] Fig.11 FIG. 4 is a schematic cross-sectional view showing the gate wiring 205 of the IGBT chip 200. The IGBT chip 200 has a structure in which a semiconductor layer 208, an insulating film 210, a polysilicon layer 209, a gate metal layer 211, and an insulating film 206 are laminated in sequence. Among them, the polysilicon layer 209 and the gate metal layer 211 correspond to the gate wiring 205. The insulating films 206 and 210 are second insulating films covering the gate wiring 205. The insulating film 210 is made of SiO2 or the like, and the insulating film 206 is made of SiN or the like. The gate wiring 205 is a low-resistance wiring layer located above the trench in a trench-gate type MOSFET or IGBT, and is a low-resistance wiring layer electrically connected to the gate electrodes of the respective transistors in a planar MOSFET or IGBT.
[0073] In a conventional press-pack type semiconductor device, when the emitter intermediate electrode 401 presses the gate wiring 205, cracks may sometimes occur in the insulating film 206 in the vertical direction, and the lower gate metal layer 211 may be exposed to the surface. If the emitter intermediate electrode 401 comes into contact with the gate metal layer 211, a short circuit occurs between the gate electrode and the emitter electrode of the IGBT, and the switching operation cannot be performed. On the other hand, in the press-pack type semiconductor device of Embodiment 2, as Fig.11 shown, in the region of the emitter intermediate electrode 401 directly above the gate wiring 205, an insulating film 406 is formed. In other words, the conductor film 407 is formed at a position that does not overlap the gate wiring 205 in a top view. Therefore, even if cracks occur in the insulating film 206, the gate metal layer 211 is electrically separated from the emitter intermediate electrode 401 through the insulating film 406. Therefore, a high pressure can be applied to the press-pack type semiconductor device, the contact resistance between the semiconductor chip and the intermediate electrode is reduced, and a low-loss press-pack type semiconductor device is achieved. In addition, since a high pressure can be applied between the common electrodes, the gap between the IGBT chip 200 and the intermediate electrode is reduced. Therefore, in the case of a short-circuit breakdown of the IGBT chip 200, the occurrence of arc discharge and destruction in the gap between the IGBT chip 200 and the intermediate electrode is suppressed, and the reliability of the module is improved.
[0074] <D. Embodiment 3>
[0075] The pressure-bonded semiconductor device of the third embodiment is obtained by changing the structure of the contact portion between the surface intermediate electrode 400 and the semiconductor chip in the pressure-bonded semiconductor device of the first embodiment. Figures 12 to 15 , the structure of the contact portion between the surface intermediate electrode 400 and the semiconductor chip in the compression-bonded semiconductor device of the third embodiment will be described.
[0076] Fig.12 and Fig.13 The structure of the IGBT side of the pressure-contact type semiconductor device according to the third embodiment is shown. Fig.12 A plan view of the contact surface of the emitter intermediate electrode 401 with respect to the IGBT chip 200 , a cross-sectional view of the emitter intermediate electrode 401 , and a plan view of the IGBT chip 200 are shown. Fig.13 It is along Fig.12 AA′ line is a cross-sectional view of the IGBT chip 200 .
[0077] like Fig.12 As shown in FIG. 1 , a gate wiring 205 is radially arranged from the center of the cell region of the IGBT chip 200. The emitter electrode 202 is divided into radial shapes by the gate wiring 205, specifically, by the insulating films 206 and 210 covering the gate wiring 205. Fig.13 As shown, multiple island electrodes are formed. That is, the insulating films 206 and 210 are the third insulating films that divide the emitter electrode 202 into multiple islands. Most of the upper surface of each divided emitter electrode 202 is covered with the insulating film 206 composed of silicon dioxide or silicon nitride, and a conductor film 207 as a second conductor film is formed in the remaining portion. The conductor film 207 is connected to the lower emitter electrode 202. It is preferred that the conductor film 207 is point-symmetrically arranged with respect to the center of gravity of the contact surface in the contact surface of the IGBT chip 200 for the emitter intermediate electrode 401. In addition, as Fig.12 As shown, it is preferable that the conductor film 207 is evenly arranged on each emitter electrode 202 divided by the gate wiring 205. Evenly arranged means that the surface area of the conductor film 207 formed on each emitter electrode 202 is equal.
[0078] On the contact surface of the emitter intermediate electrode 401 with respect to the IGBT chip 200, a conductor film 407 is formed at a position corresponding to the conductor film 207 in the connection region 404 and is in contact with the conductor film 207. An insulating film 406 is formed at other positions on the contact surface.
[0079] Fig.14 and Fig.15 The structure of the diode side of the pressure-contact type semiconductor device according to the third embodiment is shown. Fig.14A plan view of the contact surface of the anode intermediate electrode 402 with respect to the diode chip 300, a sectional view of the anode intermediate electrode 402, and a plan view of the diode chip 300 are shown. Fig.15 is a sectional view of the diode chip 300 along the B - B' line of Fig.14 .
[0080] As Fig.14 and Fig.15 shown, the anode electrode 301 is radially divided from the center by an insulating film 306 made of silicon dioxide or the like, becoming a plurality of island - shaped electrodes. Most of the upper surface of the anode electrode 301 is covered by an insulating film 304 made of silicon dioxide or silicon nitride, and a conductor film 305 is formed in the remaining part. That is, the insulating films 304 and 306 function as a third insulating film that divides the anode electrode 301 into a plurality of islands. The conductor film 305 is connected to the lower anode electrode 301. Preferably, in the contact surface of the diode chip 300 with respect to the anode intermediate electrode 402, the conductor film 305 is arranged point - symmetrically with respect to the center of gravity of the contact surface. In addition, as Fig.14 shown, it is preferable that the conductor films 305 are evenly arranged on each anode electrode 301 divided by the insulating film 306. Evenly arranged means that the surface areas of the conductor films 305 in each anode electrode 301 are equal.
[0081] In the contact surface of the anode intermediate electrode 402 with respect to the diode chip 300, a conductor film 407 is formed at a position in the connection region 404 where it contacts the conductor film 207, and an insulating film 406 is formed at other positions.
[0082] In the press - contact type semiconductor device of Embodiment 3, the surface electrode of the semiconductor chip is divided into a plurality of island - shaped electrodes, and conductor films are evenly formed on each of the divided surface electrodes. As a result, the contact resistance between each of the divided surface electrodes and the surface intermediate electrode 400 becomes uniform. In addition, when a large current is switched on and the amount of current flowing through each surface electrode becomes uneven for some reason, the surface electrode with a small resistance is energized, and its temperature rises compared to other surface electrodes. As the temperature rises, the resistance of this surface electrode increases, so the current non - uniformity in the semiconductor chip naturally decreases. Thus, the local temperature rise in the semiconductor chip can be suppressed, and the reliability of the press - contact type semiconductor device is improved.
[0083] <E. Embodiment 4>
[0084] The press - contact type semiconductor device of Embodiment 4 is an embodiment obtained by changing the structure of the contact portion between the emitter intermediate electrode 401 and the IGBT chip 200 in the press - contact type semiconductor device of Embodiment 2. Hereinafter, using Figures 16 to 20The structure of the contact portion between the emitter intermediate electrode 401 and the IGBT chip 200 in the compression-bonded semiconductor device according to the fourth embodiment will be described. This embodiment can also be combined with the third embodiment.
[0085] Fig.16 is a top view of the IGBT chip 200 . Fig.17 It is along Fig.16 A cross-sectional view of the IGBT chip 200 taken along line CC'. Fig.18 1 is a schematic diagram of a cross section passing through the gate wiring 205 of the IGBT chip 200 . Fig.19 FIG. 4 is a plan view of the contact surface of the emitter intermediate electrode 401 with respect to the IGBT chip 200 .
[0086] The press-bonded semiconductor device of the fourth embodiment is a semiconductor device obtained by providing a conductor film 207b as a third conductor film on the IGBT chip 200 in the press-bonded semiconductor device of the second embodiment, and providing a conductor film 407b on the emitter intermediate electrode 401. The structure of the press-bonded semiconductor device of the fourth embodiment is the same as that of the press-bonded semiconductor device of the second embodiment except for these. The conductor film 207b is provided on the outermost surface of the region where the gate wiring 205 is formed in the IGBT chip 200. The conductor film 407b is provided in a region in contact with the conductor film 207b in the connection region 404 of the emitter intermediate electrode 401. That is, the conductor film 207b is in contact with the conductor film 407b.
[0087] like Fig.18 As shown, the IGBT chip 200 is a structure in which a semiconductor layer 208, an insulating film 210, a polysilicon layer 209, a gate metal layer 211, an insulating film 206 and a conductor film 207b are stacked in sequence. The insulating film 206 is made of silicon dioxide or silicon nitride. The conductor film 207b is formed of a single film or a stacked film of, for example, nickel or gold.
[0088] In order to make the conductor film 207b contact the conductor film 407b and the conductor film 207 contact the conductor film 407, high positional accuracy is required between the emitter intermediate electrode 401 and the IGBT chip 200. Therefore, it is preferable to Fig.10 The emitter intermediate electrode 401 is positioned in the same manner.
[0089] The pressure-bonded semiconductor device of the fourth embodiment has been described above as a modification of the pressure-bonded semiconductor device of the second embodiment. However, this embodiment can also be applied to the third embodiment.
[0090] like Fig.18As shown in FIG. 1 , by forming the conductor film 207b, which is a relatively soft metal film, on the gate wiring 205, the unevenness existing in the emitter intermediate electrode 401 is absorbed by the conductor film 207b, thereby preventing the gate wiring 205 from being locally subjected to high pressure. As a result, the insulating film 206 on the gate wiring 205 is prevented from being damaged by the pressure, thereby preventing the gate metal layer 211 from contacting the emitter intermediate electrode 401. As a result, the reliability of the press-contact type semiconductor device is improved, damage during manufacturing is suppressed, and productivity is improved.
[0091] When the emitter intermediate electrode 401 and the IGBT chip 200 are pressed and the conductor film 407 b and the conductor film 207 b come into contact, the conductor film 207 b reaches the emitter potential. On the other hand, the gate metal layer 211 reaches the gate potential due to the gate current supplied from the gate pad 203 . Fig. 20 The equivalent circuit diagram of the IGBT chip 200 at this time is shown. The power supply voltage Vcc and the gate-emitter voltage Vge are applied to the IGBT element 701. The gate electrode is connected to the internal gate resistor Rg1 and the external gate resistor Rg2 or one of them. In addition, as shown by the dotted line, the gate-collector capacitance Cgc and the gate-emitter capacitance Cge are connected as parasitic capacitances. And, according to Fig.18 The gate metal layer 211 and the conductor film 207b form a parallel plate capacitor via the insulating film 206. In addition, the gate wiring 205 has a parasitic resistance, so Fig. 20 As shown by the dotted line, a parasitic buffer circuit 702 is formed between the gate and the emitter in parallel with the main gate wiring 205. This can suppress the oscillation of the gate voltage. The capacitance of the parasitic buffer circuit 702 can be controlled by the film thickness of the insulating film 206.
[0092] Consider a structure in which two IGBT elements are connected in series to form an upper and lower branch. The lower branch IGBT is cut off and the upper branch IGBT is turned on. At this time, a displacement current sometimes flows through the feedback capacitor of the lower branch IGBT and the lower branch IGBT is triggered by mistake. This displacement current is proportional to the collector voltage change rate (dV / dt) of the upper branch IGBT, so it becomes one of the main reasons that hinder the increase of the switching speed. On the other hand, in the structure of this embodiment, the displacement current between the gate and the emitter is charged to the parasitic capacitance, so the displacement current flowing between the gate and the emitter is suppressed, suppressing false triggering. In this way, it is possible to prevent the upper branch IGBT and the lower branch IGBT from becoming conductive at the same time and the IGBT chip from being short-circuited and damaged, and the switching speed can be increased.
[0093] In addition, the present invention can freely combine various embodiments within the scope of the invention or appropriately modify or omit various embodiments. Although the present invention has been described in detail, the above description is only illustrative in all aspects, and the present invention is not limited thereto. It should be understood that countless unillustrated variations can be envisioned without departing from the scope of the present invention.
Claims
1. A pressure-bonded semiconductor device comprising: A plurality of semiconductor chips each having a first main electrode and a second main electrode on a front surface and a back surface thereof; a first intermediate electrode facing the first main electrode of the semiconductor chip; a first common electrode plate disposed on a side of the first intermediate electrode opposite to a surface facing the first main electrode; as well as a second common electrode plate disposed opposite to the second main electrode; The first intermediate electrode has a surface facing the first main electrode that is smaller than a surface facing the first main electrode that is facing the first intermediate electrode, and has a peripheral protection region and a connection region surrounded by the protection region. The pressure-contact type semiconductor device comprises: a plurality of first conductor films partially formed in the connection region; as well as A first insulating film is formed in a region of the connection region where the first conductive film is not formed and in the protection region.
2. The pressure-contact type semiconductor device according to claim 1, wherein The plurality of first conductive films are formed point-symmetrically with respect to the center of gravity of a surface of the first intermediate electrode facing the first main electrode.
3. The pressure-contact type semiconductor device according to claim 1 or 2, wherein: The semiconductor chip includes an IGBT chip and a diode chip connected in anti-parallel to the IGBT chip.
4. The pressure-contact type semiconductor device according to claim 1 or 2, wherein: The semiconductor chip includes an IGBT chip, The IGBT chip has: a control wiring electrically separated from the first main electrode; and a second insulating film covering the control wiring, The first conductive film is formed at a position not overlapping with the control wiring in a plan view.
5. The pressure-contact type semiconductor device according to claim 1 or 2, wherein: The first main electrode is divided into a plurality of islands by a third insulating film. The semiconductor chip includes a second conductive film partially formed on each of the divided first main electrodes. The surface areas of the second conductive film are equal between the divided first main electrodes. The first conductor film is formed at a position corresponding to the second conductor film in the connection region and is in contact with the second conductor film.
6. The pressure-contact type semiconductor device according to claim 4, wherein The IGBT chip includes a third conductor film formed on the second insulating film and constituting a surface of the IGBT chip.
7. The pressure-contact type semiconductor device according to claim 3, wherein The semiconductor chip includes an IGBT chip, The IGBT chip has: a control wiring electrically separated from the first main electrode; and a second insulating film covering the control wiring, The first conductive film is formed at a position not overlapping with the control wiring in a plan view.
8. The pressure-contact type semiconductor device according to claim 3, wherein The first main electrode is divided into a plurality of islands by a third insulating film. The semiconductor chip includes a second conductive film partially formed on each of the divided first main electrodes. The surface areas of the second conductive film are equal between the divided first main electrodes. The first conductor film is formed at a position corresponding to the second conductor film in the connection region and is in contact with the second conductor film.
9. The pressure-contact type semiconductor device according to claim 4, wherein The first main electrode is divided into a plurality of islands by a third insulating film. The semiconductor chip includes a second conductive film partially formed on each of the divided first main electrodes. The surface areas of the second conductive film are equal between the divided first main electrodes. The first conductor film is formed at a position corresponding to the second conductor film in the connection region and is in contact with the second conductor film.
10. The pressure-contact type semiconductor device according to claim 7, wherein The first main electrode is divided into a plurality of islands by a third insulating film. The semiconductor chip includes a second conductive film partially formed on each of the divided first main electrodes. The surface areas of the second conductive film are equal between the divided first main electrodes. The first conductor film is formed at a position corresponding to the second conductor film in the connection region and is in contact with the second conductor film.
11. The pressure-contact type semiconductor device according to claim 7, wherein The IGBT chip includes a third conductor film formed on the second insulating film and constituting a surface of the IGBT chip.