A lamination tool and lamination method for lithium-ion battery

By designing the lithium-ion battery laminate tooling and multi-stage operation, the positive and negative electrode plates are glued with the heating structure, the misalignment problem caused by the loose state after lamination is solved, the quality and safety of the battery are ensured, and the efficiency of lamination is improved .

CN113725476BActive Publication Date: 2024-11-05HUNAN LEAD POWER TECH GRP CO LTD +4
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202111040939.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-09-06
Publication Date
2024-11-05
Estimated Expiration
2041-09-06

AI Technical Summary

Technical Problem

The loose state of the lithium-ion battery after stacking the chip causes the positive electrode plate to be misaligned with the negative electrode plate, which may cause short circuits and safety accidents and affect battery quality.

Method used

Design a laminated tool for lithium-ion batteries, including tablet pressing assembly and motion control structure, and melt the glue layer with adhesive layer diaphragm through heating structure, stick to the positive electrode sheet and negative electrode sheet to prevent misalignment, and use lamination and heating , multi-stage operation of cooling ensures the stability of the battery chip.

Benefits of technology

It effectively avoids the misalignment between the positive electrode sheet and the negative electrode sheet, ensures the quality and safety of the battery chip, and improves the stability and stacking efficiency of the battery chip.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113725476B_ABST
    Figure CN113725476B_ABST
Patent Text Reader

Abstract

This invention provides a stacking fixture for lithium-ion batteries, including a stacking platform with a pressing structure mounted on it. The pressing structure includes at least two pressing assemblies evenly distributed around the outer periphery of the stacking area on the stacking platform. Each pressing assembly includes a support, the lower end of which is rotatably mounted on the stacking platform. A track is vertically positioned on the upper part of the support facing the stacking area, and a stacking pressing block is mounted on the track. A first heating structure is provided within the stacking pressing block. The stacking fixture also includes a control structure, comprising a motion control structure and a first heating control structure. The motion control structure controls the position of the stacking pressing block relative to the stacking area, and the first heating control structure controls the heating of the stacking pressing block by the first heating structure. A stacking method is also provided, comprising performing multiple operations in groups of stacking, heating, and cooling to form a battery chip. The stacking operation and stacking method of this invention has the advantages of simple operation and high efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of lithium ion battery manufacturing, in particular to a stacking tool and a stacking method for lithium ion batteries. Background Art

[0002] Lithium-ion batteries usually use stacked cells, which are formed by stacking the positive electrode sheet, separator, and negative electrode sheet in sequence to form a flat, loose cubic cell, which is then output to the next process for corresponding operations.

[0003] At present, since the stacked cubic battery cells are in a loose state, it is very easy for the positive and negative electrodes to be misaligned during the transfer process. If the misalignment is too large, the positive and negative electrodes may be misaligned (such as Figure 1 The contact situation shown in the figure may cause short circuit during battery charging and discharging, or even fire and explosion accidents. Summary of the invention

[0004] In order to solve the problems that the cubic battery cell formed by stacking the positive electrode sheet, the separator and the negative electrode sheet in sequence is in a loose state, the battery cell is deformed due to misalignment during the transfer to the subsequent process, or the positive electrode sheet contacts with the negative electrode sheet and causes a short circuit, etc., the present invention designs a stacking tool and a stacking method for lithium-ion batteries with simple structure and easy operation, which can ensure that the cubic battery cell formed after stacking is a whole, so as to avoid the problem of unqualified quality of lithium-ion batteries caused by misalignment of the positive electrode sheet and the negative electrode sheet, and also ensure the safety of lithium-ion batteries.

[0005] The technical solution to achieve the purpose of the invention is as follows:

[0006] In a first aspect, the present invention provides a stacking tool for lithium-ion batteries, which is used to stack positive electrode sheets, negative electrode sheets, and rubber-layered separators multiple times to form battery cells. The stacking tool includes a stacking table, on which a pressing structure is installed. The pressing structure includes at least two pressing assemblies evenly distributed on the periphery of the stacking area on the stacking table.

[0007] Among them, the pressing assembly includes a bracket, the lower end of which is rotatably mounted on the lamination table; a track is provided on the bracket facing the lamination area in the vertical direction, a lamination pressing block is installed on the track, and a first heating structure is provided in the lamination pressing block.

[0008] Among them, the lamination tooling also includes a control structure, which includes a motion control structure and a first heating control structure. The motion control structure is used to control the position between the lamination block transformation and the lamination area, and the first heating control structure is used to control the first heating structure to heat the lamination block.

[0009] The present invention designs the stacking tooling of the battery cell. On the one hand, by designing the pressing assembly and the motion control structure, it is convenient to timely move the stacking pressing blocks out of or into the stacking area for corresponding operations during the stacking process; on the other hand, by designing the first heating structure and the first heating control structure, the unformed stacked battery chips after stacking at each stage can be heated in time, so that the glue layer of the adhesive layer diaphragm melts and sticks the positive or negative electrode sheets on both sides thereof, so as to avoid displacement between the positive electrode sheet, the negative electrode sheet and the adhesive layer diaphragm in subsequent operations, thereby affecting the quality of the battery.

[0010] Furthermore, the above-mentioned motion control structure includes a first motion control structure and a second motion control structure. The first motion control structure is used to control the bracket to rotate in the mounting hole of the lamination table, and the second motion control structure is used to control the lamination pressing block to move upward or downward on the track.

[0011] Furthermore, the contact area between each of the stacked blocks and the unformed stacked battery chip is 1 / 15 to 1 / 30 of the surface area of ​​the unformed stacked battery chip.

[0012] Furthermore, the above-mentioned laminated blocks are one of circular, square and rectangular.

[0013] In one embodiment of the present invention, a second heating structure is provided in the lamination table, and the second heating structure is located directly below the pressing position of the lamination pressing block.

[0014] The control structure also includes a second heating control structure, and the second heating control structure is used to control the second heating structure to heat the lamination table.

[0015] In a second aspect, the present invention further provides a lamination method for a lithium ion battery, wherein the lamination tooling of the first aspect is used to perform a lamination operation, comprising the following steps:

[0016] S1, the motion control structure controls the lamination pressing block to move out of the lamination area to eliminate the obstruction of the lamination area by the lamination pressing block;

[0017] S2. On a stacking table, stacking operations are performed multiple times with the separator with a glue layer, the positive electrode sheet, the separator with a glue layer, and the negative electrode sheet as a group to form an unformed stacked battery chip;

[0018] S3, the motion control structure controls the stacking pressing block to move to the top of the stacking area, and moves the stacking pressing block downward to press the unformed stacked battery chips in S2;

[0019] S4, the first heating control structure starts to heat the laminated block, and the laminated block heats each of the adhesive layer separators in the unformed stacked battery chips in S3, so that the adhesive layer in the adhesive layer separator is melted;

[0020] S5, after heating is finished, the motion control structure controls the stacking block to move out of the stacking area to eliminate the blocking of the stacking area on the stacking table by the stacking block, and restores the unformed stacked battery chips after heating to room temperature, and the adhesive layer diaphragm adheres the positive and negative electrodes on both sides thereof;

[0021] S6. Repeat S2 to S5 until the battery chip is formed.

[0022] The stacking method of lithium-ion batteries of the present invention designs the stacking process of battery chips into multiple stages with stacking, heating and cooling as groups. The stacking block is heated by a first heating structure, so that the stacking block heats the layers of adhesive layer diaphragms close to it. On the one hand, it can ensure that the layers of adhesive layer diaphragms can adhere to the positive electrode sheets or negative electrode sheets on both sides thereof, thereby ensuring the stability of the layers in the battery chip; on the other hand, it can also avoid that the adhesive layers of the layers of adhesive layer diaphragms with the positive electrode sheets or negative electrode sheets bonded at the bottom are melted again, thereby affecting the stacking efficiency and quality of the battery chips.

[0023] Furthermore, in the above step S4, the heating temperature of the first heating control structure is 70-130°C.

[0024] In a third aspect, the present invention further provides a lamination method for a lithium-ion battery, wherein the lamination tooling of the first aspect is used to perform a lamination operation, comprising the following steps:

[0025] S1, the motion control structure controls the lamination pressing block to move out of the lamination area to eliminate the blocking of the lamination area on the lamination table by the lamination pressing block;

[0026] S2. On a stacking table, stacking operations are performed multiple times with the separator with a glue layer, the positive electrode sheet, the separator with a glue layer, and the negative electrode sheet as a group to form an unformed stacked battery chip;

[0027] S3, the motion control structure controls the stacking pressing block to move to the top of the stacking area, and moves the stacking pressing block downward to press the unformed stacked battery chips in S2;

[0028] S4, the first heating control structure starts to heat the laminated block, and the laminated block heats each of the adhesive layer separators in the unformed stacked battery chips in S3, so that the adhesive layer in the adhesive layer separator is melted;

[0029] and / or the second heating control structure starts heating the laminating table, and the laminating table heats each of the adhesive layer separators in the unformed stacked battery chips in S3 to melt the adhesive layer in the adhesive layer separators;

[0030] S5, after heating is finished, the motion control structure controls the stacking block to move out of the stacking area to eliminate the shielding of the stacking block on the stacking area, and restore the unformed stacked battery chips after heating to room temperature, and the adhesive layer diaphragm adheres the positive and negative electrodes on both sides thereof;

[0031] S6. Repeat S2 to S5 until the battery chip is formed.

[0032] The stacking method of lithium-ion batteries of the present invention designs the stacking process of battery chips into a multi-stage stacking operation with stacking, heating and cooling as groups. The stacking block is heated by a first heating structure, and / or the stacking table is heated by a second heating structure. Through the reasonable application of the first heating structure and the second heating structure, the stacking block heats the layers of adhesive layer diaphragms close to it. On the one hand, it can ensure that the layers of adhesive layer diaphragms can adhere to the positive electrode sheets or negative electrode sheets on both sides thereof, thereby ensuring the stability of the layers in the battery chip; on the other hand, it can also avoid that the adhesive layers of the layers of adhesive layer diaphragms with the positive electrode sheets or negative electrode sheets at the bottom are melted again, thereby affecting the stacking efficiency and quality of the battery chip.

[0033] Furthermore, in the above step S4, the heating temperatures of the first heating control structure and the second heating control structure are the same, and the heating range is 70-130°C.

[0034] Furthermore, the pressing force of the laminated blocks in step S3 in the second aspect and the third aspect is 200-1000N.

[0035] Compared with the prior art, the present invention has the following beneficial effects:

[0036] 1. By designing the stacking tooling of the battery cell, the stacking block can be conveniently moved out or moved into the stacking area in time for corresponding operations through the pressing assembly and the motion control structure, and the operation is simple and convenient; at the same time, the first heating structure and the first heating control structure can timely heat the unformed stacked battery chips after stacking at each stage, so that the glue layer of the glue-layer diaphragm melts and sticks the positive or negative electrodes on both sides thereof, so as to avoid displacement between the positive electrode sheet, the negative electrode sheet and the glue-layer diaphragm in subsequent operations, thereby affecting the quality of the battery.

[0037] 2. By designing a second heating structure in the stacking table and adding a second heating control structure to the control structure, a reasonable combination of the second heating structure and the first heating structure can be achieved, further improving the stacking efficiency of the battery chip.

[0038] 3. The stacking method of the present invention adopts a multi-stage stacking operation consisting of stacking, heating, and cooling, which can ensure that each layer of the adhesive layer diaphragm in the battery chip can adhere to the positive electrode sheets or negative electrode sheets on both sides thereof.

[0039] 4. In the stacking method of the present invention, the first heating structure and the second heating structure can be used in combination to ensure that each layer of the adhesive layer diaphragm can adhere to the positive electrode sheets or negative electrode sheets on both sides thereof, and can also avoid repeated melting of the adhesive layer of the adhesive layer diaphragm of the already adhered positive electrode sheets or negative electrode sheets, thereby reducing the cooling time in step S5 and affecting the stacking efficiency of the battery chips. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for the description of the embodiments. Obviously, the drawings described below are only for the purpose of more clearly illustrating the technical solutions of the embodiments of the present invention or the prior art. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0041] Figure 1 A schematic diagram of the misalignment of the positive electrode sheet and the negative electrode sheet in a battery cell in the prior art;

[0042] Figure 2 It is a top view of the lamination tooling of the lithium-ion battery in Example 1 and Example 2;

[0043] Figure 3 It is a side view of the lamination tooling of the lithium ion battery in Example 1 and Example 2;

[0044] Among them, 1. stacking table; 2. pressing assembly; 3. bracket; 4. track; 5. stacking block. DETAILED DESCRIPTION

[0045] The present invention will be further described below in conjunction with specific embodiments, and the advantages and features of the present invention will become clearer as the description proceeds. However, these embodiments are exemplary only and do not constitute any limitation to the scope of the present invention. It should be understood by those skilled in the art that the details and forms of the technical solution of the present invention may be modified or replaced without departing from the spirit and scope of the present invention, but these modifications and replacements all fall within the scope of protection of the present invention.

[0046] In the description of this embodiment, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the invention.

[0047] In addition, the terms "first", "second", "third", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0048] Embodiment 1:

[0049] This specific embodiment provides a stacking tool for lithium-ion batteries, which is used to stack positive electrode sheets, negative electrode sheets, and separators with adhesive layers multiple times to form a battery cell.

[0050] In one structure of the lamination tooling in this specific embodiment, as Figure 2 and Figure 3 As shown, the lamination tooling includes a lamination platform 1 , on which a pressing structure is installed. The pressing structure includes at least two pressing assemblies 2 evenly distributed on the periphery of the lamination area on the lamination platform 1 .

[0051] Specifically, the pressing assembly 2 is used to press the unformed stacked battery chips onto the stacking table 1 for subsequent operations. The pressing assembly 2 can be distributed at any position around the unformed stacked battery chips. Among the distribution positions of the pressing assembly 2, it is the best choice to symmetrically arrange the pressing assembly 2 on the unformed stacked battery chips. For example, Figure 3 A schematic diagram of a stacking tooling of the present invention, in which a pressing assembly 2 is designed on one side of the unformed stacked battery chip and near the corner position, and the unformed stacked battery chips can be well pressed and held by four pressing assemblies 2.

[0052] Among them, Figure 2 and Figure 3 The shown pressing assembly 2 includes a bracket 3, the lower end of which is rotatably mounted on the lamination table 1; a track 4 is provided in the vertical direction on the bracket 3 facing the lamination area, a lamination pressing block 5 is installed on the track 4, and a first heating structure (not shown in the drawing) is provided inside the lamination pressing block 5.

[0053] Specifically, the contact area between the stacking block 5 and the unformed stacked battery chip is 1 / 15 to 1 / 30 of the surface area of ​​the unformed stacked battery chip. Since the purpose of this design is to solve the problem of unformed stacked battery chips being scattered or misaligned after stacking, in order to control the operating cost while ensuring the bonding quality and efficiency, this specific implementation method limits the contact area between the stacking block 5 and the unformed stacked battery chip.

[0054] Furthermore, the laminated block 5 of the present invention can be in any shape, preferably selected. For ease of processing and installation, the laminated block 5 of this specific embodiment is preferably selected to be one of round, square, and rectangular.

[0055] The lamination tooling also includes a control structure (not shown in the drawings), and the control structure includes a motion control structure and a first heating control structure.

[0056] Specifically, the motion control structure is used to control the position of the lamination pressing block 5 between the lamination area and the lamination area. The motion control structure controls the movement of the lamination pressing block 5 so that it moves out of the lamination area to perform the lamination operation; or moves into the lamination area to perform the pressing operation.

[0057] Furthermore, the motion control structure includes a first motion control structure and a second motion control structure, wherein the first motion control structure is used to control the bracket to rotate in the mounting hole of the lamination table, and the second motion control structure is used to control the lamination pressing block 5 to move upward or downward on the track 4. Specifically, the first motion control structure uses an existing drive structure (such as a motor, a cylinder, etc.), as long as it can realize the rotation of the bracket 3 in the mounting hole of the lamination table 1; the second motion control structure is similarly selected, and an existing drive structure is used, as long as it can realize the upward or downward movement of the lamination pressing block 5 on the track 4.

[0058] Specifically, the first heating control structure is used to control the first heating structure to heat the laminated block 5. The first heating structure may be a heating plate or a heating wire. The first heating control structure is used to set the heating temperature and heating process of the first heating structure.

[0059] Embodiment 2:

[0060] This specific embodiment provides a lamination method for lithium-ion batteries, which uses the lamination tooling in Example 1 to perform lamination operations, including the following steps:

[0061] S1. The motion control structure controls the lamination pressing block to move out of the lamination area to eliminate the obstruction of the lamination area by the lamination pressing block.

[0062] Specifically, the first motion control structure in the motion control structure controls the bracket 3 to rotate on the stacking table 1, so that the bracket 3 drives the stacking block 5 to move out of the stacking area; the second motion control structure controls the stacking block 5 to move upward on the track 4 to have a certain distance from the stacking table 1 or the unformed stacked battery chips, so as to avoid friction between the stacking block 5 and the stacking table 1 or the unformed stacked battery chips when the bracket 3 rotates.

[0063] S2. On a stacking table, multiple stacking operations are performed with the adhesive layer separator, the positive electrode sheet, the adhesive layer separator, and the negative electrode sheet as a group to form an unformed stacked battery chip.

[0064] Specifically, during the initial operation, first, place the adhesive layer diaphragm on the stacking area; secondly, place the positive electrode sheet on the adhesive layer diaphragm, and use the adhesive layer diaphragm to flip upward to cover the positive electrode sheet; then, place the negative electrode sheet on the adhesive layer diaphragm; the above steps are regarded as a group, and after multiple operations (that is, 3 to 5 groups), an unformed stacked battery chip with a certain thickness is formed.

[0065] S3, the motion control structure controls the stacking pressing block to move to the top of the stacking area, and moves the stacking pressing block downward to press the unformed stacked battery chips in S2.

[0066] Specifically, the first motion control structure in the motion control structure controls the bracket 3 to rotate on the lamination table 1, so that the bracket 3 drives the lamination block 5 to move into the lamination area; the second motion control structure controls the lamination block 5 to move downward on the track 4 to press the unformed stacked battery chips.

[0067] Specifically, the pressing force of the lamination pressing block 5 in this step is 200-1000N.

[0068] S4, the first heating control structure starts to heat the stacked block, and the stacked block heats each of the separators with glue layers in the unformed stacked battery chips in S3, so that the glue layers in the separators with glue layers melt.

[0069] Specifically, the heating temperature of the first heating control structure is 70-130° C., which can ensure that the glue layer in the glue-layered separator is melted quickly without damaging the positive electrode sheet and the negative electrode sheet.

[0070] S5, after heating is finished, the motion control structure controls the stacking block to move out of the stacking area to eliminate the blocking of the stacking area on the stacking table by the stacking block, and restores the unformed stacked battery chips after heating to room temperature, and the adhesive layer diaphragm adheres the positive and negative electrodes on both sides thereof;

[0071] After heating, first, the second motion control structure controls the stacking block 5 to move upward along the track 4 to separate from the unformed stacked battery chip; secondly, the first motion control structure controls the bracket 3 to rotate and move out of the stacking area. The process of restoring the unformed stacked battery chip to room temperature after heating can be cooled by natural cooling of room temperature or cold air, or by other existing cooling methods, which will not be described in detail here.

[0072] S6. Repeat S2 to S5 until the battery chip is formed.

[0073] The stacking method of the lithium-ion battery of the present embodiment designs the stacking process of the battery chip into multiple stages consisting of stacking, heating and cooling. The stacking block is heated by the first heating structure, so that the stacking block heats the layers of adhesive layer separators close to it. On the one hand, it can ensure that the layers of adhesive layer separators can adhere to the positive electrode sheets or negative electrode sheets on both sides thereof, thereby ensuring the stability of the layers in the battery chip; on the other hand, it can also avoid that the adhesive layers of the layers of adhesive layer separators that have been bonded to the positive electrode sheets or negative electrode sheets at the bottom will melt again, thereby affecting the stacking efficiency and quality of the battery chip.

[0074] Embodiment 3:

[0075] In another structure of the lamination tooling of this specific embodiment, in addition to the structure in Example 1, the lamination tooling is provided with a second heating structure (not shown in the attached drawings) in the lamination table 1, and the second heating structure is located directly below the holding position of the lamination block 5. At the same time, the control structure also includes a second heating control structure, and the second heating control structure is used to control the second heating structure to heat the lamination table 1. In the lamination tooling of this structure, the first heating structure and the second heating structure can be used at the same time, or only one can be used. The specific use needs to be selected according to the thickness of the unformed stacked battery chip. For example: when the thickness of the unformed stacked battery chip is small, the first heating structure and the second heating structure can be heated at the same time; as the thickness of the unformed stacked battery chip gradually increases, in order to avoid the adhesive layer diaphragm at the bottom of the unformed stacked battery chip from being repeatedly heated and melted, thereby affecting the quality of the unformed stacked battery chip or the cooling time of the unformed stacked battery chip, only the first heating structure needs to be used.

[0076] Embodiment 4:

[0077] This specific embodiment provides a lamination method for lithium-ion batteries, using the lamination tooling in Example 3 to perform lamination operations, including the following steps:

[0078] S1. The motion control structure controls the lamination pressing block to move out of the lamination area to eliminate the blocking of the lamination area on the lamination table by the lamination pressing block.

[0079] Specifically, the first motion control structure in the motion control structure controls the bracket 3 to rotate on the stacking table 1, so that the bracket 3 drives the stacking block 5 to move out of the stacking area; the second motion control structure controls the stacking block 5 to move upward on the track 4 to have a certain distance from the stacking table 1 or the unformed stacked battery chips, so as to avoid friction between the stacking block 5 and the stacking table 1 or the unformed stacked battery chips when the bracket 3 rotates.

[0080] S2. On a stacking table, multiple stacking operations are performed with the separator with glue layer, the positive electrode sheet, the separator with glue layer, and the negative electrode sheet as one to form an unformed stacked battery chip.

[0081] Specifically, during the initial operation, first, place the adhesive layer diaphragm on the stacking area; secondly, place the positive electrode sheet on the adhesive layer diaphragm, and use the adhesive layer diaphragm to flip upward to cover the positive electrode sheet; then, place the negative electrode sheet on the adhesive layer diaphragm; the above steps are regarded as a group, and after multiple operations (that is, 3 to 5 groups), an unformed stacked battery chip with a certain thickness is formed.

[0082] S3, the motion control structure controls the stacking pressing block to move to the top of the stacking area, and moves the stacking pressing block downward to press the unformed stacked battery chips in S2.

[0083] Specifically, the first motion control structure in the motion control structure controls the support 3 to rotate on the lamination table 1, so that the support 3 drives the lamination pressing block 5 to move into the lamination area; the second motion control structure controls the lamination pressing block 5 to move downward on the track 4 to press the unformed stacked battery chips. Specifically, the pressing force of the lamination pressing block 5 in this step is 200-1000N.

[0084] S4, the first heating control structure starts to heat the laminated block, and the laminated block heats each of the adhesive layer separators in the unformed stacked battery chips in S3, so that the adhesive layer in the adhesive layer separator is melted;

[0085] And / or the second heating control structure starts heating the stacking table, and the stacking table heats each adhesive layer separator in the unformed stacked battery chip in S3 to melt the adhesive layer in the adhesive layer separator.

[0086] The difference between this step and the step in Example 2 is that in this embodiment, each adhesive layer separator in the unformed stacked battery chip is heated by the cooperation of the first heating structure and the second adding structure.

[0087] The heating temperature of the first heating control structure and the second heating control structure is the same, and the heating temperature is 70-130°C. 70-130°C can ensure that the glue layer in the glue layer separator is quickly melted without damaging the positive electrode sheet and the negative electrode sheet.

[0088] S5. After heating is completed, the motion control structure controls the stacking block to move out of the stacking area to eliminate the shielding of the stacking area by the stacking block, and restores the unformed stacked battery chips after heating to room temperature, and the adhesive layer diaphragm adheres the positive and negative electrodes on both sides thereof.

[0089] After heating, first, the second motion control structure controls the stacking block 5 to move upward along the track 4 to separate from the unformed stacked battery chip; secondly, the first motion control structure controls the bracket 3 to rotate and move out of the stacking area. The process of restoring the unformed stacked battery chip to room temperature after heating can be cooled by natural cooling of room temperature or cold air, or by other existing cooling methods, which will not be described in detail here.

[0090] S6. Repeat S2 to S5 until the battery chip is formed.

[0091] The stacking method of the lithium-ion battery of the present embodiment designs the stacking process of the battery chip into a multi-stage stacking operation with stacking, heating and cooling as groups. The stacking block is heated by the first heating structure, and / or the stacking table is heated by the second heating structure. Through the reasonable application of the first heating structure and the second heating structure, the stacking block heats the layers of adhesive layer diaphragms close to it. On the one hand, it can ensure that the layers of adhesive layer diaphragms can adhere to the positive electrode sheets or negative electrode sheets on both sides thereof, thereby ensuring the stability of the layers in the battery chip; on the other hand, it can also avoid that the adhesive layers of the layers of adhesive layer diaphragms with the positive electrode sheets or negative electrode sheets bonded at the bottom are melted again, thereby affecting the stacking efficiency and quality of the battery chip.

[0092] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

[0093] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

Claims

1. A stacking tool for lithium-ion batteries, used to stack positive electrode sheets, negative electrode sheets, and rubber-layered separators multiple times to form a battery cell, characterized in that: The lamination tooling comprises a lamination platform, on which a pressing structure is installed, wherein the pressing structure comprises at least two pressing assemblies evenly distributed on the periphery of the lamination area on the lamination platform, and the pressing assemblies press and heat the unformed stacked battery chips on the lamination platform to form the battery core; The sheet pressing assembly comprises a bracket, the lower end of which is rotatably mounted on the stacking table; a track is provided on the bracket in a vertical direction at a position facing the stacking area, a stacking block is installed on the track, and a first heating structure is provided in the stacking block; The lamination tooling also includes a control structure, the control structure includes a motion control structure and a first heating control structure, the motion control structure is used to control the position between the lamination block transformation and the lamination area, and the first heating control structure is used to control the first heating structure to heat the lamination block; The motion control structure includes a first motion control structure and a second motion control structure, wherein the first motion control structure is used to control the bracket to rotate in the mounting hole of the lamination table, and the second motion control structure is used to control the lamination pressing block to move upward or downward on the track; The contact area between each of the stacked blocks and the unformed stacked battery chip is 1 / 15 to 1 / 30 of the surface area of ​​the unformed stacked battery chip; A second heating structure is provided in the lamination table, and the second heating structure is located directly below the pressing position of the lamination pressing block; The control structure further includes a second heating control structure, and the second heating control structure is used to control the second heating structure to heat the lamination table.

2. The lamination tooling according to claim 1, characterized in that: The laminated blocks are in the shape of a circle, a square or a rectangle.

3. A method for laminating a lithium-ion battery, using the laminating tooling according to any one of claims 1 to 2 to perform a laminating operation, characterized in that: The following steps are involved: S1, the motion control structure controls the lamination pressing block to move out of the lamination area to eliminate the blocking of the lamination area on the lamination table by the lamination pressing block; S2. On a stacking table, stacking operations are performed multiple times with the separator with a glue layer, the positive electrode sheet, the separator with a glue layer, and the negative electrode sheet as a group to form an unformed stacked battery chip; S3, the motion control structure controls the stacking pressing block to move to the top of the stacking area, and moves the stacking pressing block downward to press the unformed stacked battery chips in S2; S4, the first heating control structure starts to heat the laminated block, and the laminated block heats each of the adhesive layer separators in the unformed stacked battery chips in S3, so that the adhesive layer in the adhesive layer separator is melted; and / or the second heating control structure starts heating the laminating table, and the laminating table heats each of the adhesive layer separators in the unformed stacked battery chips in S3 to melt the adhesive layer in the adhesive layer separators; S5, after heating is finished, the motion control structure controls the stacking block to move out of the stacking area to eliminate the shielding of the stacking block on the stacking area, and restore the unformed stacked battery chips after heating to room temperature, and the adhesive layer diaphragm adheres the positive and negative electrodes on both sides thereof; S6. Repeat S2 to S5 until the battery chip is formed.

4. The lamination method according to claim 3, characterized in that: In step S4, the heating temperature of the first heating control structure and the second heating control structure is the same, and the heating range is 70-130°C.

5. The lamination method according to claim 3, characterized in that: The pressing force of the laminated blocks in step S3 is 200-1000N.

Citation Information

Patent Citations

  • Laminating tool

    CN110364767A

  • Lithium ion battery lamination method and device

    CN112259802A

  • Lamination device for improving wrinkles of lithium ion battery diaphragm

    CN212113907U

  • Lamination tool of lithium ion battery

    CN217214832U

  • Lamination device having dual lamination platforms and lamination method therefor

    WO2021022655A1