Railway vehicle wheels
By designing the structure of the annular plate part and the linear plate thickness centerline in the railway wheel, the problem of thermal deformation and snaking of the rim part is solved, the effect of reducing the displacement of the rim part and the thermal stress of the plate part is achieved, and the safety of the railway vehicle is improved. stability and wheel life.
Patent Information
- Application Number
- CN202080039439.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-05-29
- Filing Date
- 2020-05-20
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2040-05-20
AI Technical Summary
Existing railway wheels are prone to thermal deformation of the rim and snaking or derailment during the braking process, and it is difficult to reduce the displacement of the rim and the thermal stress of the plate at the same time.
A new wheel structure is designed, in which the plate part forms an annular shape. The center line of the plate thickness is linear in longitudinal section and tilts outward in the radial direction. It is located between the flange and the center of the tread to hinder the movement of the rim part. and reduce thermal stress concentration.
It effectively reduces the rim displacement and plate thermal stress in the axial direction, and improves the driving stability and wheel life of the railway vehicle.
Smart Images

Figure CN113891806B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to wheels for use in railway vehicles. Background Art
[0002] The wheel of a railway vehicle comprises a hub, a rim, and a plate. The axle is inserted into the hub. The rim constitutes the outer periphery of the wheel and has a tread and a flange. The tread is the surface that contacts the top surface of the rail. The flange protrudes outwardly from the tread in the radial direction of the wheel. The plate connects the rim and the hub.
[0003] In the past, there have been various shapes of wheels for railway vehicles. For example, Patent Document 1 discloses a wheel with a curved plate portion, where the plate portion connects the rim portion and the hub portion. In Patent Document 1, the plate portion has a curved plate thickness center line in a longitudinal section of the wheel. The plate thickness center line is symmetrical with respect to the center, with the center being the inflection point.
[0004] Patent Documents 2 and 3 also disclose wheels with curved plate portions. In Patent Documents 2 and 3, the plate thickness centerline of the plate portion has a convex shape on the opposite side of the flange in a longitudinal section of the wheel. That is, the plate thickness centerline is a curve whose two ends are arranged closer to the flange than the center.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Laid-Open No. 10-29401
[0008] Patent Document 2: Japanese Patent Application No. 2009-545484
[0009] Patent Document 3: Japanese Patent Application No. 2015-500177 Summary of the invention
[0010] Technical problem to be solved by the invention
[0011] However, as a kind of braking device for railway vehicle wheels, tread brakes are known. The tread brake presses the brake block against the tread of the wheel to brake the railway vehicle. During the braking of the railway vehicle, friction heat is generated between the tread and the brake block. Therefore, the temperature of the wheel, especially the rim portion constituting the outer peripheral portion of the wheel, rises, and thermal deformation of the rim portion occurs. When the rim portion is thermally deformed and displaced, it affects the running stability of the railway vehicle. In particular, when the rim portion is displaced in the axial direction of the wheel, it may induce meandering or derailment of the railway vehicle. In addition, during the braking of the railway vehicle, the rim portion will be thermally deformed, and thermal stress will be generated in the plate portion, so there is also the possibility of fatigue failure of the wheel. Therefore, in the braking of the railway vehicle by the tread brake, it is necessary to reduce the displacement of the rim portion in the axial direction of the wheel and reduce the thermal stress generated in the plate portion. However, in the existing wheels exemplified in Patent Documents 1 to 3, it is difficult to simultaneously reduce both the displacement of the rim portion and the thermal stress of the plate portion generated during braking.
[0012] An object of the present disclosure is to provide a railway vehicle wheel capable of simultaneously reducing displacement of a rim portion in the axial direction of the wheel and thermal stress generated in a plate portion during braking of the railway vehicle by a tread brake.
[0013] Technical means for solving technical problems
[0014] The wheel disclosed in the present invention is used in a railway vehicle. The wheel includes a hub portion, a rim portion, and a plate portion. The hub portion constitutes the inner circumference of the wheel. The axle of the railway vehicle is inserted into the hub portion. The rim portion constitutes the outer circumference of the wheel. The rim portion includes a tread and a flange. The tread contacts the top surface of the track on which the railway vehicle travels. The flange protrudes further outward than the tread in the radial direction of the wheel. The plate portion is formed in an annular shape, connecting the hub portion and the rim portion. In a longitudinal section of the wheel, the plate portion has a straight plate thickness center line, and the plate thickness center line is tilted in a manner approaching the flange side as it moves toward the outer side in the radial direction. In a longitudinal section of the wheel, the outer end of the plate thickness center line is located between the center of the flange and the tread in the axial direction of the wheel. The outer end of the plate thickness center line is the end located on the outer side in the radial direction of the two ends of the plate thickness center line.
[0015] Effects of the Invention
[0016] According to the railway vehicle wheel disclosed herein, during braking of the railway vehicle using the tread brake, it is possible to simultaneously reduce displacement of the rim portion in the axial direction of the wheel and thermal stress generated in the plate portion. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a longitudinal sectional view of the railway vehicle wheel according to the embodiment.
[0018] Figure 2This is a diagram showing an exaggerated example of the deformation of the wheel during braking using a tread brake.
[0019] Figure 3 It is a diagram showing a wheel shape that the analysis model of the embodiment has.
[0020] Figure 4 It is a diagram showing a wheel shape that an analysis model of a comparative example has. DETAILED DESCRIPTION
[0021] The wheel of the embodiment is used in a railway vehicle. The wheel includes a hub portion, a rim portion, and a plate portion. The hub portion constitutes the inner periphery of the wheel. The axle of the railway vehicle is inserted into the hub portion. The rim portion constitutes the outer periphery of the wheel. The rim portion includes a tread and a flange. The tread contacts the top surface of the track on which the railway vehicle travels. The flange protrudes outwardly more than the tread in the radial direction of the wheel. The plate portion is formed in a ring shape, connecting the hub portion and the rim portion. In a longitudinal section of the wheel, the plate portion has a straight plate thickness center line, and the plate thickness center line is tilted in a manner approaching the flange side as it approaches the outer side in the radial direction. In a longitudinal section of the wheel, the outer end of the plate thickness center line is located between the center of the flange and the tread in the axial direction of the wheel. The outer end of the plate thickness center line is one of the two ends of the plate thickness center line that is located outward in the radial direction (first structure).
[0022] When the brake block of the tread brake is pressed against the tread of the wheel and friction heat is generated, the rim portion will be thermally deformed and displaced in the axial direction of the wheel. In the axial direction of the wheel, when the side with the flange is taken as the flange direction and the opposite side is taken as the flange counter direction, generally speaking, the rim portion is easily displaced in the flange direction. In response to this, in the wheel of the first structure, the plate thickness center line of the plate portion forms a straight line in the longitudinal section of the wheel, and tilts in a manner approaching the flange side as it approaches the outer side in the radial direction of the wheel. The plate portion having such a plate thickness center line will resist the displacement of the rim portion when the rim portion is to be displaced in the flange direction, and can hinder the displacement. Therefore, in the braking of a railway vehicle using a tread brake, the displacement of the rim portion in the axial direction can be reduced. In addition, since the plate thickness center line has no inflection point, it is not easy to generate stress concentration in the plate portion. Therefore, in the braking of a railway vehicle based on a tread brake, the thermal stress generated in the plate portion can be reduced.
[0023] According to the first structure, the displacement of the rim portion in the axial direction can be reduced, and the rim portion is not easy to swing relative to the plate portion. Therefore, the stress generated in the plate portion at the root portion of the rim portion can be reduced. In addition, by positioning the outer end of the plate thickness centerline between the flange and the center of the tread, the thermal stress generated in the plate portion during the braking of the railway vehicle can be reduced.
[0024] Preferably, the distance in the axial direction from the side surface on the flange side of the rim portion to the outer end of the plate thickness centerline is 0.3 times or more the length of the rim portion in the axial direction (second structure).
[0025] Preferably, the angle formed by the plate thickness center line with respect to the axial direction on the flange side is 87° or less (third configuration).
[0026] Preferably, the plate portion has a plate thickness which decreases toward the outer side in the radial direction and becomes the smallest before the outer end of the plate thickness centerline (fourth configuration).
[0027] Hereinafter, the embodiments of the present disclosure will be described with reference to the accompanying drawings. In each of the drawings, the same reference numerals are used for the same or corresponding structures, and the same description will not be repeated.
[0028] Figure 1 1 is a longitudinal cross-sectional view of the wheel 100 of this embodiment. The so-called longitudinal cross-sectional view refers to a cross-section obtained by cutting the wheel 100 along a plane including the central axis X. The longitudinal cross-section of the wheel 100 is symmetrical with respect to the central axis X, so Figure 1 , only one side of the center axis X in the wheel 100 is shown. In the present embodiment, the direction in which the center axis X of the wheel 100 extends is referred to as an axial direction, and the radial direction of the wheel 100 is simply referred to as a radial direction.
[0029] Reference Figure 1 The wheel 100 is used in a railway vehicle and includes a hub portion 10 , a rim portion 20 , and a plate portion 30 .
[0030] The hub portion 10 constitutes the inner peripheral portion of the wheel 100 . The hub portion 10 is formed in a substantially cylindrical shape with the central axis X as the axis. An axle (not shown) of a railway vehicle is inserted into the hub portion 10 .
[0031] The rim portion 20 constitutes the outer periphery of the wheel 100. The rim portion 20 is disposed outside the hub portion 10 in the radial direction. In addition, the rim portion 20 is located on the outer side relative to the hub portion 10 in the track width direction. Figure 1 The center of the rim width shown by the two-dot dash line is C 20 Located at the center C of the wheel hub width which is also shown by the two-dot chain line 10 More outside the track.
[0032] The rim portion 20 includes a tread 21 and a flange 22. The tread 21 is a surface facing outward in the radial direction. The tread 21 contacts the top surface of the track on which the railway vehicle travels. The diameter of the tread 21 gradually increases toward the flange 22 side. The shape of the tread 21 is not particularly limited. The tread 21 may be, for example, a conical tread or an arc tread.
[0033] In the rim portion 20, a flange 22 is provided at one end in the axial direction. In the axial direction of the wheel 100, the side where the flange 22 is provided is referred to as the flange direction, and the opposite side is referred to as the flange reverse direction. The flange 22 protrudes outwardly from the tread 21 in the radial direction. When the railway vehicle travels on the track, the flange 22 is located on the inner side of the left and right tracks. The flange 22 includes side surfaces 221 and 222. Each of the side surfaces 221 and 222 is a curve including one or more arcs in a longitudinal section of the wheel 100.
[0034] The side surface 221 is arranged on the tread 21 side in the axial direction. The side surface 221 is connected to the tread 21 via the throat portion 23. In the longitudinal section of the wheel 100, the throat portion 23 is a curve including one or more arcs, and smoothly connects the side surface 221 to the tread 21. The curvature of the surface of the rim portion 20 changes at the boundary 24 between the throat portion 23 and the tread 21. The absolute value of the curvature of the portion of the tread 21 adjacent to the boundary 24 is intentionally smaller than the absolute value of each curvature of the side surface 221 of the flange 22 and the throat portion 23.
[0035] The side surface 222 is arranged on the opposite side of the side surface 221 in the axial direction. Of the two side surfaces 25 and 26 of the rim portion 20 , the side surface 222 is connected to one side surface 25 .
[0036] The plate portion 30 is formed in a ring shape. The plate portion 30 connects the hub portion 10 and the rim portion 20. The plate thickness of the plate portion 30 is smaller than the thickness of the hub portion 10 and the rim portion 20 as a whole. The thickness of the hub portion 10 and the rim portion 20 refer to the length of the hub portion 10 and the rim portion 20 in the axial direction, respectively. The plate thickness of the plate portion 30 is the length of the plate portion 30 in the axial direction. The plate thickness of the plate portion 30 is larger on the hub portion 10 side and smaller on the rim portion 20 side.
[0037] The plate portion 30 has side surfaces 31 and 32. The side surface 31 is a surface disposed on the flange 22 side in the axial direction. The side surface 32 is located on the opposite side of the side surface 31 in the axial direction. In the longitudinal section of the wheel 100, the side surfaces 31 and 32 are connected to the rim portion 20 via arcs 41 and 42, respectively. The side surfaces 31 and 32 are connected to the hub portion 10 via arcs 43 and 44, respectively.
[0038] In the present embodiment, the end 411 of the arc 41 on the plate 30 side and the end 421 of the arc 42 on the plate 30 side, which is located further in the radial direction, is defined as the outer peripheral end of the plate 30. In addition, the end 431 of the arc 43 on the plate 30 side and the end 441 of the arc 44 on the plate 30 side, which is located further outward in the radial direction, is defined as the inner peripheral end of the plate 30. The outer peripheral end of the plate 30 may also be referred to as the root of the rim portion 20 of the plate 30. The inner peripheral end of the plate 30 may also be referred to as the root of the hub portion 10 of the plate 30. In the present embodiment, the end 421 of the arc 42 and the end 441 of the arc 44 are respectively the outer peripheral end and the inner peripheral end of the plate 30.
[0039] The thickness of the plate portion 30 decreases toward the outside in the radial direction and is the smallest near the outer peripheral end 421. That is, the plate portion 30 has the smallest plate thickness near the outer peripheral end 421, which is closer to the inner side in the radial direction than the outer peripheral end 421. The position where the plate portion 30 has the smallest plate thickness substantially coincides with the position where the bending stress generated in the plate portion 30 due to the bending load received by the wheel 100 from the track when the railway vehicle is in a curve is the smallest. For example, the plate thickness of the plate portion 30 can be set to the smallest at a position 5 mm to 30 mm inward in the radial direction from the outer peripheral end 421.
[0040] The plate portion 30 has a plate thickness center line A. The plate thickness center line A is a line that passes through the middle of the side surfaces 31 and 32 and extends from the hub portion 10 side to the rim portion 20 side. The plate thickness center line A is straight in the longitudinal section of the wheel 100. The so-called straight line here does not only refer to a completely straight line, but also includes the concept of a very gentle arc with a curvature radius of more than 1000 mm, or a broken line. That is, the plate thickness center line A can be identified as being substantially a straight line in the longitudinal section of the wheel 100. In the longitudinal section of the wheel 100, the plate thickness center line A is straight, so the plate portion 30 forms a roughly flat plate shape and does not bend in the axial direction.
[0041] In the longitudinal section of the wheel 100, the plate thickness center line A is tilted relative to the radial direction so that it approaches the flange 22 side as it goes to the outer side in the radial direction. Of the two ends Aa and Ab of the plate thickness center line A, the end Aa located on the outer side in the radial direction is called the outer end of the plate thickness center line A, and the end Ab located on the inner side in the radial direction is called the inner end of the plate thickness center line A. The outer end Aa of the plate thickness center line A is the point where the plate thickness center line A is connected to a straight line passing through the outer peripheral end 421 of the plate portion 30 and extending in the axial direction. The inner end Ab of the plate thickness center line A is the point where the plate thickness center line A is connected to a straight line passing through the inner peripheral end 441 of the plate portion 30 and extending in the axial direction.
[0042] In the axial direction, the outer end Aa of the plate thickness centerline A is located in the range R between the flange 22 and the center 211 of the tread 21. That is, the outer end Aa is arranged in the opposite direction of the flange relative to the side 221 of the flange 22. In addition, the outer end Aa is arranged in the flange direction relative to the center 211 of the tread 21. The so-called center 211 of the tread 21 refers to the middle position in the axial direction between the boundary 24 of the tread 21 and the throat 23 and the side 26 of the rim portion 20.
[0043] By arranging the outer end Aa of the plate thickness centerline A between the flange 22 and the center 211 of the tread 21, the distance in the axial direction between the plate portion 30 and the side surface 25 on the flange 22 side of the rim portion 20 is ensured. The distance in the axial direction from the side surface 25 of the rim portion 20 to the outer end Aa of the plate thickness centerline A is set as the plate portion position Pw. The plate portion position Pw is appropriately determined according to the specifications of the tread brake used by the wheel 100, etc. For example, the plate portion position Pw [mm] is preferably more than 0.3 times the width Wr [mm] of the rim portion 20 (Pw / Wr≧0.3). The plate portion position Pw [mm] is preferably less than 0.6 times the width Wr [mm] of the rim portion 20 (Pw / Wr≦0.6). The width Wr of the rim portion 20 is the length of the rim portion 20 in the axial direction, and is the maximum distance in the axial direction from the side surface 25 on the flange 22 side to the opposite side surface 26.
[0044] In the longitudinal section of the wheel 100, the plate thickness center line A forms an angle θ with respect to the axial direction on the flange 22 side. When the plate thickness center line A is a very gentle curve, the angle θ is the angle formed by the tangent line at the center of the plate thickness center line A (the midpoint between the outer end Aa and the inner end Ab) with respect to the axial direction. When the plate thickness center line A is a broken line, the angle θ is the angle formed by the longest line segment among the line segments constituting the plate thickness center line A with respect to the axial direction.
[0045] The angle θ is smaller than 90°. Although it depends on the specifications of the tread brake used for the wheel 100, the angle θ is preferably 87° or less. The angle θ is preferably 75° or more.
[0046] [Effects of Embodiment]
[0047] Figure 2 Only shows Figure 1 FIG. 1 is a cross-sectional view of the wheel 100, which exaggerates the deformation of the wheel 100 during braking by the tread brake. Figure 2When the brake block of the tread brake is pressed onto the tread 21 of the wheel 100, the rim portion 20 is thermally deformed due to friction and is displaced toward the flange 22 side (flange direction) in the axial direction. However, according to the wheel 100 of this embodiment, such displacement of the rim portion 20 can be reduced. That is, in the wheel 100, the plate thickness center line A of the plate portion 30 forms a straight line in the longitudinal section of the wheel 100. Moreover, the plate thickness center line A tilts in a manner approaching the flange 22 side as it moves toward the outer side in the radial direction. Therefore, during the braking of the railway vehicle by the tread brake, even if the rim portion 20 is to be displaced in the flange direction, the plate portion 30 will resist the displacement of the rim portion 20 and can hinder the displacement. Therefore, the displacement of the rim portion 20 in the axial direction can be reduced.
[0048] In the wheel 100 of the present embodiment, the plate thickness center line A is formed in a straight line in a longitudinal section of the wheel 100, so that the plate portion 30 has substantially no inflection point. Therefore, during the braking of the railway vehicle using the tread brake, stress concentration is less likely to occur in the plate portion 30. Therefore, not only the displacement of the rim portion 20 in the axial direction is reduced, but also the thermal stress generated in the plate portion 30 can be reduced.
[0049] In the present embodiment, the plate portion position Pw is preferably 0.3 times or more the width Wr of the rim portion 20. This can further reduce the displacement of the rim portion 20 in the axial direction.
[0050] In this embodiment, the angle θ formed by the plate thickness centerline A with respect to the axial direction on the flange 22 side is preferably set to 87° or less. This can more reliably reduce the displacement of the rim portion 20 in the axial direction and the thermal stress generated in the plate portion 30 .
[0051] In this embodiment, the plate thickness of the plate portion 30 decreases toward the outside in the radial direction and is smallest before the outer end Aa of the plate thickness centerline A. More specifically, the position where the bending stress generated by the bending load from the rail when passing through a curve is smallest is made substantially consistent with the position where the plate thickness is smallest. In this way, fatigue damage of the plate portion 30 can be prevented, and the life of the wheel 100 can be increased.
[0052] As mentioned above, although embodiment of this disclosure was described, this disclosure is not limited to the said embodiment, Various changes can be made within the range which does not deviate from the summary.
[0053] [Example]
[0054] The present disclosure is further described in detail below by way of examples, but the present disclosure is not limited by the following examples.
[0055] In order to evaluate the effect of the railway vehicle wheel based on the present disclosure, a numerical analysis (FEM analysis) based on the finite element method was performed. In the FEM analysis, a wheel 100 ( Figure 1 ) were used to evaluate the same analysis model with different plate thickness centerline A angles (plate angles) θ[°] and plate position Pw[mm]. For comparison, an analysis model with a wheel shape commonly used in Europe and North America was also evaluated.
[0056] Figure 3 The diagram shows the wheel shapes (outline in 1 / 2 section) of the analysis models of Examples 1 to 4. The wheel shapes of the analysis models of Examples 1 to 4 are all such that the hub portion is located closer to the track center (closer to the axle center) than the rim portion. Figure 4 FIG. 1 is a diagram showing the wheel shapes (outline in the 1 / 2 cross section) of the analysis models of Comparative Examples 1 to 5. Figure 3 and Figure 4 In Examples 1 to 4 and Comparative Examples 1 to 3, the plate thickness centerline A is straight. In Examples 1 to 4, the plate angle θ is less than 90°, whereas in Comparative Examples 1 to 3, the plate angle θ is greater than 90°. Figure 4 As shown, in Comparative Examples 4 and 5, the plate thickness centerline A is curved, unlike in Examples 1 to 4 and Comparative Examples 1 to 3. The analysis model of Comparative Example 4 has a wheel shape commonly used in Europe. The analysis model of Comparative Example 5 has a wheel shape commonly used in North America. Table 1 shows the shape parameters of each analysis model.
[0057] [Table 1]
[0058] Plate angle θ[°] Plate position Pw[mm] Plate position Pw / Rim width Wr Example 1 85 36 0.26 Example 2 85 52 0.37 Example 3 85 66 0.47 Example 4 87 66 0.47 Comparative Example 1 90 52 0.37 Comparative Example 2 100 52 0.37 Comparative Example 3 110 52 0.37 Comparative Example 4 - 72 0.51 Comparative Example 5 - 93 0.66
[0059] FEM analysis was performed using general software (ABAQUS Ver.6.12, manufactured by Dassault Systemes). In the analysis, in order to simulate the braking of a railway vehicle by a tread brake, a heat flux was applied to the area in the tread of the wheel that was in contact with the brake block of the tread brake. The braking time was set to 1200 seconds, and the inner circumference of the wheel was set to be fully restrained. In addition, in order to evaluate the stress (mechanical stress) generated in the wheel when the railway vehicle travels on the track, a load was applied to the position in the tread of the wheel that was in contact with the track. The load at this time was 40t per wheel axle.
[0060] The results of the FEM analysis are shown in Table 2. In Table 2, the rim displacement [mm] is the maximum displacement of the rim in the axial direction during braking, with the flange direction being negative and the flange reverse direction being positive. The rim displacement is evaluated at a position of 890 mm in diameter of the wheel in the side surface on the flange side of the rim. The plate thermal stress is the maximum stress of the plate during braking. The plate mechanical stress is the maximum value of the stress amplitude (1 / 2 of the variation range) of the plate generated during one rotation of the wheel on the track. In Table 2, for each embodiment and each comparative example, the plate thermal stress is expressed as a ratio to the plate thermal stress of Example 1, and the plate mechanical stress is expressed as a ratio to the plate mechanical stress of Example 1.
[0061] [Table 2]
[0062] Rim displacement [mm] Thermal stress in plate[-] Mechanical stress of plate[-] Example 1 -1.5 1.00 1.00 Example 2 -0.7 0.96 1.00 Example 3 -0.2 0.86 0.91 Example 4 -0.4 0.75 0.99 Comparative Example 1 -2.0 0.78 1.05 Comparative Example 2 -3.8 0.99 0.78 Comparative Example 3 -3.8 0.92 1.00 Comparative Example 4 -0.2 1.29 0.99 Comparative Example 5 -2.4 0.77 1.14
[0063] Comparative Example 5 The plate thickness center line A is formed into a substantially S-shape, and the root portion of the hub portion and the root portion of the rim portion are separated in the axial direction in the plate portion ( Figure 4 ). In such a wheel shape, although the thermal stress of the plate can be reduced, the displacement of the rim cannot be reduced. In fact, in Comparative Example 5, the displacement of the rim is -2.4 mm, resulting in a large displacement of the rim toward the flange. On the other hand, in Examples 1 to 4 where the plate thickness centerline A is a straight line, the displacement of the rim is -1.5 mm to -0.2 mm, which is smaller than that of Comparative Example 5.
[0064] In Comparative Examples 1 to 3, similarly to Examples 1 to 4, the plate thickness centerline A is a straight line. Among them, the plate angle θ of Examples 1 to 4 is less than 90°, whereas the plate angle θ of Comparative Examples 1 to 3 is greater than 90°. The rim displacement of Comparative Examples 1 to 3 is -2.0 mm to -3.8 mm. On the other hand, in Examples 1 to 4 in which the plate angle θ is less than 90°, the rim displacement is -1.5 mm to -0.2 mm, and the rim displacement is reduced compared to Comparative Examples 1 to 3. In particular, in Examples 2 to 4 in which the ratio of the plate position Pw [mm] to the rim width Wr [mm] is greater than 0.3, the result is that the rim displacement is within the range permitted by the European standard EN13979-1 (-1.0 mm to 3.0 mm).
[0065] Comparative Example 4 sets two inflection points on the plate ( Figure 4). In such a wheel shape, although the displacement of the rim portion can be reduced, the thermal stress of the plate portion cannot be reduced. In fact, in Comparative Example 4, the ratio of the thermal stress of the plate portion (for Example 1) increases to 1.29. On the other hand, in Examples 1 to 4 where the plate thickness centerline A is a straight line, the ratio of the thermal stress of the plate portion (for Example 1) is reduced to 0.75 to 1.00. In Examples 2 to 4 where the plate position Pw is relatively large, the thermal stress of the plate portion is smaller.
[0066] Compared with Comparative Example 4, the plate thermal stress of Comparative Examples 1 to 3 is reduced. In particular, the plate thermal stress of Comparative Example 1, in which the plate angle θ is 90°, is smaller than that of Examples 1 to 3. However, in Comparative Example 1, the plate mechanical stress becomes larger than that of each Example. Therefore, if the plate mechanical stress is taken into consideration, the plate angle θ needs to be less than 90°.
[0067] Thus, it can be confirmed that, in a railway vehicle wheel, the plate thickness center line A is set to a straight line, and the plate thickness center line A is tilted relative to the radial direction in a manner approaching the flange side as it moves toward the outer side in the radial direction. If the plate angle θ is set to less than 90°, the wheel rim displacement and the plate thermal stress can be reduced at the same time. According to the analysis results of Examples 1 to 4, the wheel rim displacement and the plate thermal stress can be more reliably reduced by setting the plate angle θ to less than 87°. In addition, according to the analysis results of Examples 2 to 4, when the ratio of the plate position Pw to the wheel rim width Wr is greater than 0.3, the wheel rim displacement can be further reduced.
[0068] [Explanation of Reference Numerals]
[0069] 100: Wheel
[0070] 10: Hub
[0071] 20: Rim
[0072] 21: Treading
[0073] 22: Flange
[0074] 30: Board
[0075] A: Plate thickness centerline
Claims
1. A wheel is a wheel used in a railway vehicle, having: a hub portion constituting the inner circumference of the wheel and into which the axle of the railway vehicle is inserted; a rim portion constituting an outer peripheral portion of the wheel, including a tread that contacts the top surface of a rail on which the railway vehicle travels, and a flange that protrudes outwardly from the tread in the radial direction of the wheel, the rim portion being located on the outer side in the rail width direction relative to the hub portion; and The annular plate portion connects the hub portion and the rim portion. In the longitudinal section of the wheel, The plate portion has a straight plate thickness center line, and the plate thickness center line is inclined so as to approach the flange side as it goes outward in the radial direction. Of the two ends of the plate thickness center line, one end located on the outside in the radial direction, namely the outer end, is located between the flange and the center of the tread in the axial direction of the wheel.
2. The wheel according to claim 1, A distance in the axial direction from the side surface of the rim portion on the flange side to the outer end of the plate thickness centerline is equal to or greater than 0.3 times the length of the rim portion in the axial direction.
3. The wheel according to claim 1, The angle formed by the plate thickness center line with respect to the axial direction on the flange side is 87° or less.
4. A wheel according to any one of claims 1 to 3, The plate portion has a plate thickness that decreases toward the outer side in the radial direction and is smallest before the outer end of the plate thickness centerline.