Oil tank mold for making fixings, fixing manufacturing method and fixing
By improving the design of the oil tank mold, the flange part is formed by using the oil tank parison to form and connect it to the bolt column part during the blow molding of the oil tank, the problem of verticality deviation and high cost in the transportation of the fixture is solved, and the stability of the fixture is achieved and cost reduction.
Patent Information
- Application Number
- CN202111194754.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-13
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-10-13
AI Technical Summary
During transportation, the existing oil tank fixing parts are prone to deviation of the perpendicularity between the flange part and the bolt column part, which leads to difficulty in assembly. The overall fixing parts have large packaging space, high transportation costs, and relatively fixed processing costs.
Using an improved oil tank mold design, the flange part is formed by using the excess part of the oil tank parison during the blow molding process of the oil tank, and embedded, riveted or welded with the prefabricated bolt column to form a fixture to ensure the flange part and bolt The perpendicularity and connection of the column are stable.
It effectively avoids the change in the verticality between the flange part and the bolt column part during transportation, reduces the processing and transportation costs of fixtures, and improves the utilization rate of packaging space.
Smart Images

Figure CN113895017B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of oil tank processing, and in particular to an oil tank mold for manufacturing a fixing part, a fixing part manufacturing method and the fixing part. Background Art
[0002] The accessories on the plastic fuel tank (including internal and external parts, etc.) need to be connected with special plastic fixings, which usually consist of a bolt part and a flange part fixed at the end of the bolt part. When the fuel tank is equipped with internal or external parts, the support rod of the bolt part connects the fuel tank body with the accessories, and the flange part penetrates and is welded to the surface of the fuel tank, thus completing the assembly process of the accessories.
[0003] At present, fuel tank manufacturers usually need to purchase complete fixings from external parts suppliers, that is, the flange part and the bolt part have been processed and manufactured at the parts supplier. After the two parts are fixedly connected to form a fixing, the parts supplier supplies the fuel tank manufacturer in the form of a complete fixing.
[0004] Since the materials and manufacturing processes of the fixings are relatively mature at the parts suppliers, there is little room for cost reduction. In addition, when the parts suppliers supply the tank manufacturers as a whole, the integral fixings have relatively more packaging space, resulting in a certain increase in transportation costs. At the same time, it is difficult to reliably ensure the verticality of the flange and the bolt part during transportation. It is often found that a certain number of the fixings in a batch of purchased fixings are deformed, that is, the verticality deviation between the flange and the bolt part is large, and they cannot be used for the subsequent assembly of accessories. Summary of the invention
[0005] In view of the above, the present invention aims to provide a fuel tank mold, a method for manufacturing a fixing and a fixing for making a fixing, which utilizes the high-temperature softening characteristics of the fuel tank parison during the fuel tank blow molding process, so that the excess parison located at the edge of the fuel tank during mold closing is connected and formed with the independently prefabricated bolt column part, thereby forming a flange part and fixing the fixing part which is fixed to the bolt column part as an integral form, thereby solving the aforementioned drawbacks of purchasing and transporting the integral fixing parts and also reducing the processing and manufacturing costs of the fixing parts.
[0006] The technical solution adopted by the present invention is as follows:
[0007] In the first aspect, a fuel tank mold for making a fixing part comprises a first mold for blow molding of the fuel tank and a second mold, wherein: a first flange molding groove is formed at a preset position on the first mold, and a bolt receiving groove is formed on the second mold at a center position corresponding to the first flange molding groove.
[0008] In at least one possible implementation manner, a second flange molding groove is formed on the second mold, and the second flange molding groove is located outside the bolt accommodating groove.
[0009] In at least one possible implementation manner, the second flange forming groove corresponds to an edge position of the first flange forming groove.
[0010] In at least one possible implementation manner, a stabilizing device is provided in the bolt receiving groove, and the stabilizing device is used to fasten a support rod of the bolt portion placed in the bolt receiving groove.
[0011] In at least one possible implementation manner, the stabilizing device includes any one or more of the following: a claw-shaped clamp, an elastic mechanism, a snap-fit component, or a filler.
[0012] A second aspect is a method for manufacturing a fixing member, comprising:
[0013] Placing the bolt part in the bolt receiving groove on the second mold, and making the end of the bolt part protrude from the second mold;
[0014] During the blow molding process of the fuel tank, when the first mold and the second mold are closed, the softened fuel tank blank residue between the first flange molding groove on the first mold and the bolt accommodating groove is subjected to extrusion force, and a flange portion is formed through the first flange molding groove, and at the same time, the end of the bolt portion is inserted into the flange portion and connected to the flange portion.
[0015] In at least one possible implementation manner, the connection manner between the end of the bolt portion and the flange portion includes any one or more of the following: embedding, welding or riveting.
[0016] A third aspect is a fixing member, comprising: a separately prefabricated bolt part and a flange part made from the residual material of the oil tank blank, wherein the end of the bolt part is fixedly connected to the flange part.
[0017] In at least one possible implementation manner, the fixed connection manner between the end of the bolt portion and the flange portion includes any one or more of the following: embedding, riveting or welding.
[0018] In at least one of the possible implementations:
[0019] The side surface of the end head is provided with an embedding groove for engaging with the remaining material of the fuel tank blank; and / or
[0020] The body of the end head is provided with a riveting groove for riveting with the remaining material of the fuel tank blank; and / or
[0021] The upper end surface of the end head is provided with a protrusion for welding with the remaining material of the oil tank blank.
[0022] The design concept of the present invention is that, by improving the fuel tank mold, the flange part of the required fixing part is made from the excess part of the fuel tank parison while the fuel tank is blow-molded, and the flange part and the bolt part are connected and fixed synchronously, thereby obtaining a fixing part for subsequent assembly of internal parts or external parts. Compared with the fixing part obtained by the existing integral processing, it can effectively avoid the change of the verticality of the flange part and the bolt part during transportation, and can significantly reduce the process cost. In actual operation, the present invention only requires the parts supplier to prepare the bolt part separately as needed. Since the shape of the separate bolt part is simple, it is not easy to deform during transportation, and the space utilization rate of the transportation package will also be improved, thereby significantly reducing the transportation cost and packaging difficulty. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] In order to make the purpose, technical solutions and advantages of the present invention more clear, the present invention will be further described below with reference to the accompanying drawings, in which:
[0024] Figure 1 A schematic diagram of a partial structure of a fuel tank mold for making a fixing member provided in an embodiment of the present invention;
[0025] Figure 2 A schematic diagram of a process for manufacturing a fixing member provided by an embodiment of the present invention;
[0026] Figure 3 A schematic diagram of the state before mold closing is completed when manufacturing a fixing member provided by an embodiment of the present invention;
[0027] Figure 4 A schematic diagram of the state after mold closing is completed when manufacturing a fixing member provided by an embodiment of the present invention;
[0028] Figure 5 A schematic diagram of the structure of a fixing member provided in an embodiment of the present invention;
[0029] Figure 6 A schematic diagram of an end structure for riveting of a fixing member provided in an embodiment of the present invention;
[0030] Figure 7 A schematic diagram of an end structure of a fixing member used for welding provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0031] Embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be interpreted as limiting the present invention.
[0032] The present invention proposes an embodiment of a fuel tank mold for making a fixing part, specifically in combination with Figure 1 As shown, it includes a first mold 10 and a second mold 20 for blow molding of the fuel tank (it should be pointed out that the figure is a schematic diagram of the local position of the mold, rather than the complete first and second molds). The first mold 10 and the second mold 20 are usually two groups of fuel tank molds arranged horizontally. During the blow molding process of the fuel tank, the fuel tank parison between the first mold 10 and the second mold 20 is molded into the main body of the fuel tank by closing the first mold 10 and the second mold 20 on both sides. In order to solve the above-mentioned problems raised by the present invention and realize the core concept of the present invention, this embodiment improves the first mold 10 and the second mold 20 as follows. Specifically, a first flange molding groove 11 is formed at a preset position on the first mold 10, and a bolt receiving groove 2 is formed on the second mold 20 corresponding to the center position of the first flange molding groove 11. It should be pointed out that the original intention of the present invention is to utilize the excess part of the fuel tank preform during the fuel tank blow molding process, that is, to use the excess preform part (flash material, scraps) that is not necessary for the fuel tank molding process to make the flange part of the fixing part (it can also be called the flange cap of the fixing part). Therefore, it can be understood that the preset position described here is the mold area on the complete fuel tank mold that is not necessary for the molding process, such as but not limited to the edge part of the first mold. Of course, since the first flange molding groove 11 is opposite to the bolt receiving groove 2, the position where the bolt receiving groove 2 is set on the second mold 20 also belongs to the mold area that is not necessary for the molding process, such as but not limited to the edge part of the second mold.
[0033] As mentioned above, when assembling the internal component or the external component, the flange portion of the fixing component usually needs to be welded to the fuel tank body. Therefore, based on the above embodiment, preferably, a second flange shaping groove 12 can be formed on the second mold 20, and Figure 1 As shown, the second flange shaping groove 12 is located outside the bolt receiving groove 2. More preferably, the second flange shaping groove 12 may correspond to the edge position of the first flange shaping groove 11, that is, when the flange portion of the fixing part is made, a connection portion for subsequent welding with the fuel tank body may be extended at the edge of the flange portion to facilitate the assembly operation of the fuel tank accessories.
[0034] Further, as mentioned above, usually, the first mold 10 and the second mold 20 are placed horizontally, and in order to ensure that the flange part of the fixing part is reliably connected to the bolt part, the position is centered and the verticality meets the requirements when making the fixing part, it can be considered to set a stabilizing device (not shown in the figure) in the bolt receiving groove 2. The function of the stabilizing device is to fasten and lock the support rod of the bolt part placed in the bolt receiving groove to ensure that the position of the bolt part meets the processing and manufacturing requirements of the fixing part and will not easily slide out of the bolt receiving groove 2. In actual operation, the stabilizing device can include but is not limited to any one or more of the following forms: claw-shaped clamps, elastic mechanisms, clamping parts or fillers. The specific implementation method can refer to the positioning, clamping and other similar devices and mechanisms in the mechanical field. Those skilled in the art can understand that the stabilizing device must ensure the stability of the bolt part while ensuring that the placement of the bolt part and the removal of the finished fixing part are convenient and feasible.
[0035] Accordingly, based on the improved fuel tank mold, the present invention provides an embodiment of a method for manufacturing a fixing member, such as Figure 2 , Figure 3 , Figure 4 As shown, Figure 2 Show the production process. Figure 3 It shows the production status before mold closing. Figure 4 The following diagram shows the production status after mold closing. Specifically:
[0036] Step S1 , placing the bolt portion 31 in the bolt receiving groove 2 on the second mold 20 , and making the end 310 of the bolt portion 31 protrude from the second mold 20 .
[0037] Step S2, during the blow molding process of the fuel tank, when the first mold 10 and the second mold 20 are molded together, the softened fuel tank blank 30 between the first flange shaping groove 11 on the first mold 10 and the bolt receiving groove 2 is subjected to extrusion force, and is shaped by the first flange shaping groove 11 to obtain a flange portion 32, and at the same time, the end 310 of the bolt portion 31 is inserted into the flange portion 32 and connected to the flange portion 32. Since the fuel tank blank 30 is in a high-temperature softened state at this manufacturing stage, the connection between the end of the bolt portion and the flange portion in the mold closing stage can be achieved by any one or more of the following methods: embedding, welding or riveting.
[0038] Based on this fixing part manufacturing method, a fixing part for subsequent accessory installation can be manufactured while the fuel tank is being formed. Here, the present invention also provides an embodiment of a fixing part, such as Figure 5As shown, the fixing part includes a separately prefabricated bolt part 31 and a flange part 32 made of the residual material of the fuel tank blank, wherein the bolt part 31 has an end 310 and a support rod 311, wherein the end 310 is fixedly connected to the flange part 32. In combination with the fixing part manufacturing method mentioned above, it can be known that the fixed connection method between the end 310 of the bolt part 31 and the flange part 32 can include any one or more of the following: embedding, riveting or welding. Figure 5 What is shown is an embedding embodiment, that is, an embedding groove 3101 for embedding with the residual material of the tank blank can be opened on the side of the end 310 of the separately prefabricated bolt part 31, and the production method described above can be referred to. When the end 310 is inserted into the residual material of the tank blank 30 in a softened state, a stable embedding relationship can be formed with the residual material of the tank blank 30 by relying on the embedding groove 3101.
[0039] Of course, in addition to this, you can also combine Figure 6 As shown, the end head 310 of the bolt column portion 31 in the fixing member may also be provided with a rivet groove 3102 for riveting with the residual material of the fuel tank blank, and the manufacturing method described above may be referred to. When the end head 310 is inserted into the softened residual material of the fuel tank blank 30, the hot melt blank may be squeezed into the prefabricated rivet groove 3102, so that the end head 310 and the residual material of the fuel tank blank 30 form a stable riveting relationship; Figure 7 As shown, the upper end surface of the end 310 of the bolt part 31 in the fixing piece can also be provided with a protrusion 3103 for welding with the residual material of the fuel tank blank, and the manufacturing method described above can be referred to. When the end 310 is inserted into the softened residual material of the fuel tank blank 30, the high temperature of the blank can melt the protrusion 3103, so that the end 310 and the residual material of the fuel tank blank 30 form a stable welding relationship (it can be understood that the two are welded into one). Finally, it should be pointed out that Figure 5 to Figure 7 The connection structure in the figure is for illustration only. When the end 310 is inserted into the softened tank blank residue 30, the shape and structure of the connection structure in the figure may change due to high temperature (the same plastic material), that is, there is a difference from the figure, which is not elaborated in the present invention.
[0040] In summary, the design concept of the present invention is that, by improving the fuel tank mold, the flange part of the required fixing part is made from the excess part of the fuel tank parison while the fuel tank is blow-molded, and the flange part and the bolt part are connected and fixed synchronously, thereby obtaining a fixing part for subsequent assembly of built-in parts or external parts. Compared with the fixing part obtained by the existing integral processing, it can effectively avoid the change of the verticality of the flange part and the bolt part during transportation, and can significantly reduce the process cost. In actual operation, the present invention only requires the parts supplier to prepare the bolt part separately as needed. Since the shape of the separate bolt part is simple, it is not easy to deform during transportation, and the space utilization rate of the transportation package will also be improved, thereby significantly reducing the transportation cost and packaging difficulty.
[0041] In the embodiments of the present invention, "at least one" refers to one or more, and "more than one" refers to two or more. "And / or" describes the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B may represent the existence of A alone, the existence of A and B at the same time, and the existence of B alone. A and B may be singular or plural. The character " / " generally indicates that the associated objects before and after are in an "or" relationship. "At least one of the following" and similar expressions refer to any combination of these items, including any combination of single or plural items. For example, at least one of a, b and c may represent: a, b, c, a and b, a and c, b and c, or a and b and c, where a, b, c may be single or multiple.
[0042] The above describes in detail the structure, features and effects of the present invention based on the embodiments shown in the drawings, but the above is only a preferred embodiment of the present invention. It should be noted that the technical features involved in the above embodiments and their preferred methods can be reasonably combined and matched into a variety of equivalent schemes by those skilled in the art without departing from or changing the design ideas and technical effects of the present invention; therefore, the present invention is not limited to the scope of implementation shown in the drawings, and all changes made in accordance with the concept of the present invention, or modifications to equivalent embodiments with equivalent changes, which still do not exceed the spirit covered by the specification and drawings, should be within the protection scope of the present invention.
Claims
1. A fuel tank mold for making a fixing part, comprising a first mold and a second mold for blow molding of the fuel tank, characterized in that: A first flange shaping groove is formed at a preset position on the first mold, and a bolt receiving groove is formed at a central position corresponding to the first flange shaping groove on the second mold; The preset position is a mold area on the complete fuel tank mold that is not necessary for the molding process, and the position where the bolt receiving groove is set is a mold area that is not necessary for the molding process; The first mold is at least used to use unnecessary excess blanks to make the flange part of the fixing part when the fuel tank is molded and closed; The process of manufacturing the fixing part by the fuel tank mold includes: placing the bolt part in the bolt receiving groove on the second mold, and making the end of the bolt part protrude from the second mold; During the blow molding process of the fuel tank, when the first mold and the second mold are closed, the softened fuel tank blank residue between the first flange molding groove on the first mold and the bolt accommodating groove is subjected to extrusion force, and a flange portion is formed through the first flange molding groove, and at the same time, the end of the bolt portion is inserted into the flange portion and connected to the flange portion.
2. The fuel tank mold for making a fixing member according to claim 1, characterized in that: A second flange shaping groove is formed on the second mold, and the second flange shaping groove is located outside the bolt accommodating groove.
3. The fuel tank mold for making a fixing member according to claim 2, characterized in that: The second flange forming groove corresponds to an edge position of the first flange forming groove.
4. The fuel tank mold for making a fixing member according to any one of claims 1 to 3, characterized in that: A stabilizing device is provided in the bolt receiving groove, and the stabilizing device is used to fasten the support rod of the bolt portion placed in the bolt receiving groove.
5. The fuel tank mold for making a fixing member according to claim 4, characterized in that: The stabilizing device comprises any one or more of the following: a claw-shaped clamp, an elastic mechanism, a snap-fit component or a filler.
6. The fuel tank mold for making a fixing member according to claim 1, characterized in that: The connection method between the end of the bolt part and the flange part includes any one or more of the following: embedding, welding or riveting.
7. The fuel tank mold for making a fixing member according to claim 1, characterized in that: The side surface of the end head is provided with an embedding groove for engaging with the remaining material of the fuel tank blank; and / or The body of the end head is provided with a riveting groove for riveting with the remaining material of the fuel tank blank; and / or The upper end surface of the end head is provided with a protrusion for welding with the remaining material of the oil tank blank.