A method for preparing high speed steel for drill bit tool
Through the preparation method of waste recycling and real-time detection, the problems of high-speed steel drill bit tool loss and preparation process lag are solved, efficient reuse of high-speed steel and accurate finished product preparation are achieved, and process time-consuming and raw material waste are reduced.
Patent Information
- Application Number
- CN202111324499.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-09
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-11-09
AI Technical Summary
In the existing technology, high-speed steel drill bits are easily lost during use, and there is a lack of real-time detection in the preparation process, resulting in waste of blades and tool handles and waste of raw materials.
Through steps such as scrap recycling and classification, molten composition detection, mixed molding, multiple drawings and real-time detection, the efficient preparation of high-speed steel is achieved to ensure that the composition and shape of the finished product meet the requirements, and the quality of the finished product is improved through straightening and anti-rust treatment.
It realizes the reuse of high-speed steel, reduces the process difficulty and working hours, reduces the waste of raw materials, and improves the preparation accuracy and the service life of the finished product.
Smart Images

Figure CN114029355B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of high-speed steel, and in particular to a method for preparing high-speed steel for a drill tool. Background Art
[0002] With the continuous development of human technology, the demand for equipment materials in the fields of aerospace transportation and shipping is constantly increasing, and the demand for cutting skills in the corresponding material processing process is also increasing; the emergence of high-speed steel in the existing technology has made up for the shortcomings of cutting technology to a certain extent, but the preparation process of high-speed steel in the existing technology is still insufficient, mainly manifested in: 1) High-speed steel drill tools will inevitably wear out during use, and the tool head cannot be used after it is worn to a certain extent, which easily causes waste of high-speed steel in the blade and handle; 2) The existing preparation process often only performs corresponding shape and composition inspections after the finished product comes out, and some shape and composition defects already exist in the blank and slab processes. The inspection process is single and lagging, which easily leads to waste of labor time and raw materials. Summary of the invention
[0003] In view of the defects and shortcomings in the above-mentioned prior art, the present invention provides a method for preparing high-speed steel for drill tools.
[0004] The technical solution adopted by the present invention is:
[0005] A method for preparing high-speed steel for a drill tool, characterized in that it comprises the following steps:
[0006] S1: Waste recycling and storage in different areas according to the types of waste;
[0007] S2: After the waste materials in each waste area are melted, the waste materials in each classification area are tested for components;
[0008] S3: Determine the composition ratio of the raw materials and newly added raw materials and auxiliary materials in each waste area according to the target composition mass ratio of the high-speed steel to be obtained;
[0009] S4: Mixing and processing the raw materials from each waste area, the newly added raw materials and the auxiliary materials into blanks;
[0010] S5: Detect the shape and composition of the blank;
[0011] S6: The qualified billet is pressed into a flat billet through a rolling mill and then annealed;
[0012] S7: cold rolling the slab through a multi-roll cold rolling mill and then annealing;
[0013] S8: The cold-rolled slab is annealed after multiple drawing and finally formed into a finished product after the last drawing;
[0014] S9: Inspect the appearance and composition of the finished product; straighten the finished product that fails the appearance inspection through a straightening device, and send the finished product that fails the composition inspection to the defective product analysis area;
[0015] S10: Surface treatment of qualified finished products;
[0016] S11: Send the finished product after surface treatment to the cutting machine for fixed length cutting;
[0017] S12: Performing cross-section processing and testing on the cut cross-section;
[0018] S13: The outer surface and cross section of the finished products that have passed the inspection are subjected to rust-proof treatment, and then the finished products are packaged in batches and sent to the finished product warehouse.
[0019] As a further preferred embodiment of the present invention, in step S3, the target composition mass ratio of the high-speed steel to be obtained includes:
[0020] C: 0.8-1.2%;
[0021] W: 10-18%;
[0022] Cr: 1.0-2.2%;
[0023] Mo: 2.0-4.5%;
[0024] V: 2.0-3.5%; the balance is Fe and inevitable impurities.
[0025] As a further preferred embodiment of the present invention, in step S5,
[0026] When testing the composition of the blank, the end materials at both ends of the blank and the core material inside the blank are selected for composition testing respectively. If and only if the difference between the composition mass ratio of the end materials and the core materials and the composition mass ratio of the target blank is within the preset range, the blank composition test is considered qualified;
[0027] When performing shape inspection on the blank, first store the model of the preset target blank in advance, and then compare the shape dimensions of the actual blank with the preset blank model. The blank shape inspection is considered qualified if and only if the difference in shape dimensions between the actual blank and the preset blank model is within the preset range.
[0028] As a further preferred embodiment of the present invention, in the steps S7-S8, tube annealing is performed during annealing of the flat slab, the annealing temperature is 850-870°C, the annealing time is 9-10 hours, and the tube is taken out when the annealing temperature is lower than 300°C.
[0029] As a further preferred embodiment of the present invention, in step S9,
[0030] When testing the composition of the finished product, the end materials at both ends of the finished product and the center core material inside the finished product are selected for composition testing. If and only if the difference between the composition mass ratio of the end materials and the core materials and the composition mass ratio of the target finished product is within the preset range, the finished product composition test is considered qualified;
[0031] When performing appearance inspection on a finished product, first store a model of the preset target finished product, then compare the actual finished product with the preset finished product model in terms of appearance dimensions and internal structure. The finished product appearance inspection is considered qualified if and only if the difference in appearance dimensions and internal structure between the actual finished product and the preset finished product model are within the preset range.
[0032] As a further preferred embodiment of the present invention, in step S9, the outer side surfaces of the finished products that fail the appearance inspection are first straightened by a straightening machine, and then the connecting edges and corners are polished.
[0033] As a further preferred embodiment of the present invention, in step S9, the defective product analysis area performs defective component analysis and records the finished products that fail the defective component detection for each component, and after the cycle time, the model of the preset target blank and the model of the preset target finished product are corrected according to the recorded defective component analysis results.
[0034] As a further preferred embodiment of the present invention, in step S10, the surface treatment of the qualified finished product at least includes deburring the surface of the finished product and grinding the concave and convex parts of the surface of the finished product.
[0035] As a further preferred embodiment of the present invention, in step S11, the finished product after surface treatment is fed into a cutting machine for fixed-length cutting, and the length of the finished product is adjusted by the conveying speed of the finished product.
[0036] As a further preferred embodiment of the present invention, in step S12, the cross-section processing at least includes end face straightening, cross-section grinding, cross-section rust prevention and cross-section anti-corrosion treatment; the cross-section inspection at least includes spot, looseness, bubble, pore and crack inspection inside the cross-section.
[0037] Compared with the prior art, the present invention has the following beneficial effects:
[0038] (1) The present invention provides a method for preparing high-speed steel for drill tools. By recycling waste materials and mixing them with newly added raw materials and auxiliary materials to prepare high-speed steel for drill tools, the blade and handle of the worn-out and scrapped tools can be reused. The composition ratio of the blade and handle of the worn-out and scrapped tools is also close to the composition ratio of the high-speed steel to be prepared, thereby reducing the process difficulty and time consumption. While realizing the secondary utilization of waste materials, the process accuracy can be effectively guaranteed through the partitioned storage and corresponding component detection process, as well as the mixed addition of newly added raw materials and auxiliary materials.
[0039] (2) The present invention provides a method for preparing high-speed steel for drill bit tools. In the process, corresponding detection processes are set in the corresponding steps of forming the blank, the finished product, and the cross-section, so that real-time detection can be achieved in the entire process of the entire preparation method, further saving working hours and reducing the waste of raw materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 The figure is a flow chart of the steps of the preparation method of the present invention. DETAILED DESCRIPTION
[0041] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.
[0042] See also Figure 1 The present invention provides a method for preparing high-speed steel for a drill tool, which is characterized by comprising the following steps:
[0043] S1: Waste recycling and classification and storage in different areas according to waste types; to facilitate subsequent component testing according to categories;
[0044] S2: After the waste materials in each waste area are melted, the waste materials in each classification area are tested for composition; the amount of waste materials added in each area and the corresponding composition ratio of new raw materials and auxiliary materials are determined according to the test results.
[0045] S3: Determine the composition ratio of the raw materials in each waste area and the newly added raw materials and auxiliary materials according to the target composition mass ratio of the high-speed steel to be obtained; in this embodiment, the target composition mass ratio of the high-speed steel to be obtained includes at least: C: 0.8-1.2%; W: 10-18%; Cr: 1.0-2.2%; Mo: 2.0-4.5%; V: 2.0-3.5%; the remainder is Fe and unavoidable impurities.
[0046] S4: Mixing and processing the raw materials from each waste area, the newly added raw materials and the auxiliary materials into blanks;
[0047] S5: Detect the shape and composition of the blank; wherein, when detecting the composition of the blank, select the end materials at both ends of the blank and the core material in the center of the blank for component detection respectively, and the blank composition detection is considered qualified when and only when the difference between the mass ratio of the end materials and the core materials and the mass ratio of the target blank composition is within a preset range; at the same time, select the end materials and the core materials for component detection to ensure the accuracy and uniformity of the composition of the blank as much as possible; when detecting the shape of the blank, first pre-store the model of the preset target blank, and then compare the outer dimensions of the actual blank with the preset blank model, and the blank shape detection is considered qualified when and only when the difference between the outer dimensions of the actual blank and the preset blank model is within the preset range; preferably, in this embodiment, the difference between the outer dimensions of the actual blank and the preset blank model is generally controlled to be around 0.5-1mm.
[0048] S6: The qualified billet is pressed into a flat billet through a rolling mill and then annealed;
[0049] S7: cold rolling the slab through a multi-roll cold rolling mill and then annealing;
[0050] S8: The cold-rolled slab is annealed after multiple drawing and finally formed into a finished product after the last drawing. In this embodiment, in the steps S7-S8, the slab is annealed in a tube to reduce the possibility of oxidation on the surface of the slab. The annealing temperature is 850-870°C and the annealing time is 9-10 hours. When the annealing temperature is lower than 300°C, the tube is taken out.
[0051] S9: inspect the appearance and composition of the finished product; straighten the finished product that fails the appearance inspection through a straightening device, and send the finished product that fails the composition inspection to the defective product analysis area; in the step S9, when the finished product is inspected for composition, the end materials at both ends of the finished product and the core material in the center of the finished product are selected for composition inspection respectively, and the finished product composition inspection is considered qualified only when and only when the difference between the mass ratio of the end materials and the core materials and the mass ratio of the target finished product composition is within a preset range; at the same time, the end materials and the core materials are selected for composition inspection to ensure the accuracy and uniformity of the composition of the blank as much as possible; when the finished product is inspected for appearance, a model of a preset target finished product is first stored in advance, and then the actual finished product is compared with the preset finished product model for appearance size and internal structure. The finished product appearance inspection is considered qualified only when and only when the difference between the actual finished product and the preset finished product model and the internal structure condition are within a preset range; in this embodiment, the internal structure condition at least includes internal density, the presence or absence of obvious bubbles and cracks, etc. In this embodiment, the outer side surfaces of the finished products that fail the appearance inspection are first straightened by a straightener, and then the connecting edges are polished to avoid possible damage to the finished products themselves or the conveying device due to the sharp edges. In the defective product analysis area in this embodiment, the defective components of each finished product that fails the component inspection are analyzed and recorded, and the model of the preset target blank and the model of the preset target finished product are corrected according to the recorded defective component analysis results after the cycle time.
[0052] S10: Surface treatment of the qualified finished products; in this embodiment, surface treatment of the qualified finished products at least includes deburring the surface of the finished products and grinding the concave and convex parts of the surface of the finished products.
[0053] S11: The surface treated finished product is fed into a cutting machine for cutting to a fixed length; the length of the surface treated finished product is fed into a cutting machine for cutting to a fixed length and is adjusted by the conveying speed of the finished product; preferably, before cutting to a fixed length, a three-axis adjustment device can be used, for example, to achieve three-axis position adjustment of the finished product relative to the cutter head of the cutting machine.
[0054] S12: Performing cross-section processing and inspection on the cut section; in the present embodiment, the cross-section processing at least includes end face straightening, cross-section grinding, cross-section rust prevention and cross-section anti-corrosion treatment; the cross-section inspection at least includes spot, looseness, bubble, pore and crack inspection on the inside of the cross-section.
[0055] S13: The outer surface and cross section of the finished products that have passed the inspection are subjected to rust-proof treatment, and then the finished products are packaged in batches and sent to the finished product warehouse.
[0056] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.
Claims
1. A method for preparing high-speed steel for drill bit tools, Features: The following steps are involved: S1: Waste recycling and storage in different areas according to the types of waste; S2: After the waste materials in each waste area are melted, the waste materials in each classification area are tested for components; S3: Determine the composition ratio of the raw materials and newly added raw materials and auxiliary materials in each waste area according to the target composition mass ratio of the high-speed steel to be obtained; S4: Mixing and processing the raw materials from each waste area, the newly added raw materials and the auxiliary materials into blanks; S5: Detect the shape and composition of the blank; S6: The qualified billet is pressed into a flat billet through a rolling mill and then annealed; S7: cold rolling the slab through a multi-roll cold rolling mill and then annealing; S8: The cold-rolled slab is annealed after multiple drawing and finally formed into a finished product after the last drawing; S9: Inspect the appearance and composition of the finished product; straighten the finished product that fails the appearance inspection through a straightening device, and send the finished product that fails the composition inspection to the defective product analysis area; S10: Surface treatment of qualified finished products; S11: Send the finished product after surface treatment to the cutting machine for fixed length cutting; S12: Performing cross-section processing and testing on the cut cross-section; S13: The outer surface and cross section of the finished product after the inspection are subjected to rust prevention treatment, and then the finished products are packaged in batches and sent to the finished product warehouse; In step S3, the target composition mass ratio of the high-speed steel to be obtained includes: C:0.8-1.2%; W:10-18%; Cr:1.0-2.2%; Mo: 2.0-4.5%; V: 2.0-3.5%; the balance is Fe and unavoidable impurities; In the step S5, When testing the composition of the blank, the end materials at both ends of the blank and the core material inside the blank are selected for composition testing respectively. If and only if the difference between the composition mass ratio of the end materials and the core materials and the composition mass ratio of the target blank is within the preset range, the blank composition test is considered qualified; When inspecting the shape of the blank, first store the model of the preset target blank in advance, then compare the actual blank with the preset blank model in terms of shape dimensions. If and only if the difference between the shape dimensions of the actual blank and the preset blank model is within the preset range, the blank shape inspection is considered qualified. In the step S9, When testing the composition of the finished product, the end materials at both ends of the finished product and the center core material inside the finished product are selected for composition testing. If and only if the difference between the composition mass ratio of the end materials and the core materials and the composition mass ratio of the target finished product is within the preset range, the finished product composition test is considered qualified; When performing appearance inspection on finished products, the model of the preset target finished product is first stored in advance, and then the actual finished product is compared with the preset finished product model in terms of appearance size and internal structure. If and only if the difference in appearance size and internal structure between the actual finished product and the preset finished product model are within the preset range, the finished product appearance inspection is considered qualified; The internal structural condition at least includes internal density, presence or absence of obvious bubbles and cracks; In step S9, the defective product analysis area analyzes and records the defective components of each finished product that fails the component detection, and corrects the model of the preset target blank and the model of the preset target finished product according to the recorded defective component analysis results after the cycle time.
2. A method for preparing high speed steel for drill bit tool according to claim 1, Features: In the steps S7-S8, the slab is annealed by tube loading, the annealing temperature is 850-870°C, the annealing time is 9-10 hours, and the tube is taken out when the annealing temperature is lower than 300°C.
3. A method for preparing high speed steel for drill bit tool according to claim 1, Features: In the step S9, the outer side surfaces of the finished products that fail the appearance inspection are first straightened by a straightening machine, and then the connecting edges and corners are polished.
4. The method for preparing high speed steel for drill bit tool according to claim 1, Features: In the step S10, the surface treatment of the qualified finished product at least includes deburring the surface of the finished product and grinding the concave and convex parts of the surface of the finished product.
5. The method for preparing high speed steel for drill bit tool according to claim 1, Features: In the step S11, the finished product after surface treatment is fed into a cutting machine for fixed-length cutting, and the length of the finished product is adjusted by the conveying speed of the finished product.
6. The method for preparing high speed steel for drill bit tool according to claim 1, Features: In the step S12, the cross-section processing at least includes cross-section grinding and cross-section rust prevention treatment; the cross-section detection at least includes spot, looseness, bubble, pore and crack detection inside the cross-section.