Semiconductor device and method for manufacturing the same

By using a plasma injection process to form barrier layers and source-drain regions in semiconductor devices, and using PN junction isolation, the problems of load effect and electrical failure in traditional semiconductor device manufacturing processes are solved, performance is improved and production costs are reduced.

CN114078764BActive Publication Date: 2024-10-22CHANGXIN MEMORY TECH INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010848727.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-21
Publication Date
2024-10-22
Estimated Expiration
2040-08-21

AI Technical Summary

Technical Problem

Traditional semiconductor devices have the risk of load effect, electrical failure and short circuit problems caused by silicon oxide shallow trench isolation during the manufacturing process, resulting in performance degradation.

Method used

A plasma injection process is used to form an independent trench on the semiconductor substrate to form a barrier layer, gate structure and source and drain areas. The barrier layer formed by plasma injection is electrically connected to the channel area, using the built-in electric field of the PN junction. isolation to avoid the defects of shallow trench isolation structures.

Benefits of technology

It effectively avoids various disadvantages of traditional semiconductor devices in the manufacturing process, improves device performance, reduces mask modification costs and process steps, enhances the isolation effect, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114078764B_ABST
    Figure CN114078764B_ABST
Patent Text Reader

Abstract

The present invention provides a semiconductor device and a preparation method thereof, the preparation method comprising the following steps: providing a semiconductor substrate, wherein a plurality of mutually independent grooves are formed in the semiconductor substrate; plasma injection to form a barrier layer between adjacent grooves; forming a gate structure in the grooves; forming a channel region in the semiconductor substrate, wherein the channel region corresponds to the grooves; forming a source-drain region between the grooves and the barrier layer, wherein the source-drain region is electrically connected to the channel region, and the conductivity type of the barrier layer is opposite to that of the source-drain region. The present invention has the advantage that there is no need to form a shallow trench isolation structure, and the barrier layer formed by plasma injection serves as an isolation layer for the source-drain region of adjacent transistors. Since the source-drain region and the barrier layer are injected with opposite ions, a PN junction is formed between the source-drain region and the barrier layer, and the built-in electric field of the PN junction can prevent the diffusion of electrons, thereby achieving an isolation effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor device and a method for preparing the same. Background Art

[0002] As semiconductor technology evolves towards high integration, more and more transistor devices are integrated into chips of the same size. In the traditional integrated circuit layout, the gate of the transistor is placed on the silicon substrate, the length of the channel is defined by photolithography, the source and drain need to be completed at an oblique angle, and the transistor devices are mainly isolated by shallow silicon oxide trenches.

[0003] However, with the miniaturization of chip size and the increase in integration, the gate of the transistor is placed on the silicon substrate, which significantly increases the risk of etching load effect. The channel length defined by photolithography cannot be flexibly fine-tuned according to the actual situation in the process (mask modification is required). The oblique incident doping of the source and drain is easily blocked by the photoresist, resulting in electrical failure. The silicon oxide shallow trench isolation between transistor devices is easily affected by the subsequent cleaning process to produce grooves, causing gate or wire short circuits.

[0004] Therefore, it is necessary to improve the manufacturing process to avoid the various disadvantages of traditional transistor devices in the manufacturing process. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a semiconductor device and a method for preparing the same, which avoids various drawbacks existing in the manufacturing process of traditional transistor devices and improves the performance of the semiconductor device.

[0006] In order to solve the above problems, the present invention provides a method for preparing a semiconductor device, which includes the following steps: providing a semiconductor substrate, in which a plurality of independent grooves are formed; plasma injection to form a barrier layer between adjacent grooves; forming a gate structure in the grooves; forming a channel region in the semiconductor substrate, the channel region corresponding to the grooves; forming a source-drain region between the grooves and the barrier layer, the source-drain region being electrically connected to the channel region, and the conductivity type of the barrier layer being opposite to the conductivity type of the source-drain region.

[0007] Furthermore, in the step of forming a barrier layer between adjacent grooves, the barrier layer is disposed around the outer side surface of the groove, and a distance greater than zero exists between the barrier layer and the outer side surface of the groove.

[0008] Furthermore, the gate structure includes a gate insulating layer and a gate, and the step of forming the gate structure in the trench further includes: forming a gate insulating material in the trench, the gate insulating material covering the sidewalls of the trench and the surface of the semiconductor substrate; filling the trench with a conductive material, the conductive material filling the trench and covering the gate insulating material on the surface of the semiconductor substrate; removing the conductive material and the gate insulating material on the surface of the semiconductor substrate to form a gate insulating layer and a gate located in the trench.

[0009] Furthermore, the step of forming a channel region in the semiconductor substrate further includes performing plasma implantation on the semiconductor substrate to form the channel region.

[0010] Furthermore, the width of the channel region is greater than the width of the trench.

[0011] Furthermore, after the plasma injection, an annealing process is performed to allow the channel region to extend upward along the sidewalls of the trench.

[0012] Furthermore, the plasma implantation depth is changed so that the channel region extends upward along the sidewall of the trench.

[0013] Furthermore, the plasma forming the barrier layer and the plasma forming the channel region are ions of the same conductive type.

[0014] Furthermore, the step of forming a source-drain region between the trench and the barrier layer further includes: performing plasma implantation on the semiconductor substrate to form a shallowly doped drain and a source-drain electrode, wherein the source-drain electrode is electrically connected to the channel region through the shallowly doped drain.

[0015] Furthermore, after the step of forming source and drain regions between the trench and the barrier layer, the following steps are included: forming a passivation layer, wherein the passivation layer covers the surface of the semiconductor substrate and the surface of the gate structure.

[0016] The present invention also provides a semiconductor device, comprising: a semiconductor substrate, in which a plurality of independent grooves are formed; a barrier layer formed between adjacent grooves by a plasma injection process; a gate structure formed in the grooves; a channel region formed in the semiconductor substrate and corresponding to the grooves; a source and drain region arranged between the grooves and the barrier layer and electrically connected to the channel region, the conductivity type of the barrier layer being opposite to the conductivity type of the source and drain region.

[0017] Furthermore, the barrier layer is disposed around the outer side surface of the groove, and there is a gap between the barrier layer and the outer side surface of the groove.

[0018] Furthermore, the gate structure includes a gate insulating layer covering the sidewalls of the trench and a gate filling the trench.

[0019] Furthermore, the width of the channel region is greater than the width of the trench.

[0020] Furthermore, the channel region is arranged at the bottom of the trench and extends upward along the sidewalls of the trench.

[0021] Furthermore, a passivation layer is included, and the passivation layer covers the surface of the semiconductor substrate and the surface of the gate structure.

[0022] The advantage of the present invention is that in the prior art, a shallow trench isolation structure is used as an isolation layer for the source and drain regions of adjacent transistors. The shallow trench isolation structure is affected by subsequent cleaning processes and may produce defects, causing the active regions to contact due to surface tension, resulting in a short circuit in the active regions. However, the present invention does not need to form a shallow trench isolation structure for isolation. The barrier layer formed by plasma injection serves as an isolation layer for the source and drain regions of adjacent transistors. Since the source and drain regions and the barrier layer are injected with counter-type ions, a PN junction is formed between the source and drain regions and the barrier layer. The built-in electric field of the PN junction can prevent the diffusion of electrons, thereby achieving an isolation effect. The preparation method of the present invention avoids the various drawbacks of traditional transistor devices in the process and improves the performance of semiconductor devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the steps of an embodiment of a method for preparing a semiconductor device of the present invention;

[0024] Figure 2 to Figure 10 It is a process flow chart of an embodiment of a method for preparing a semiconductor device of the present invention. DETAILED DESCRIPTION

[0025] The specific implementation manner of the semiconductor device and the preparation method thereof provided by the present invention is described in detail below with reference to the accompanying drawings.

[0026] Figure 1 is a schematic diagram of the steps of an embodiment of the method for preparing a semiconductor device of the present invention, please refer to Figure 1 The method for preparing a semiconductor device of the present invention comprises the following steps: step S10, providing a semiconductor substrate, wherein a plurality of mutually independent grooves are formed in the semiconductor substrate; step S11, plasma injection, forming a barrier layer between adjacent grooves; step S12, forming a gate structure in the groove; step S13, forming a channel region in the semiconductor substrate, wherein the channel region corresponds to the groove; step S14, forming a source-drain region between the groove and the barrier layer, wherein the source-drain region is electrically connected to the channel region.

[0027] Figure 2 to Figure 10It is a process flow chart of an embodiment of a method for preparing a semiconductor device of the present invention.

[0028] Please refer to step S10 and Figure 2 A semiconductor substrate 200 is provided, wherein a plurality of mutually independent trenches 210 are formed in the semiconductor substrate 200. The semiconductor substrate 200 may be a semiconductor substrate such as silicon or germanium. In this embodiment, the semiconductor substrate 200 is described as a silicon substrate.

[0029] In this step, the groove 210 may be formed by photolithography and etching processes. Specifically, in this step, a mask layer and a patterned photoresist layer are formed on the semiconductor substrate 200; the pattern of the photoresist layer is transferred to the mask layer; the semiconductor substrate 200 is etched using the mask layer as a mask to form the groove 210; and the mask layer is removed after the groove 210 is formed.

[0030] Please refer to step S11 and Figure 3 , plasma implantation is performed to form a barrier layer 220 between adjacent trenches 210. In this step, plasma implantation is performed on the semiconductor substrate 200 to form a barrier layer 220 in the semiconductor substrate 200. The barrier layer 220 serves as an isolation layer for the source and drain regions of adjacent transistors formed by the preparation method of the present invention, thereby preventing leakage.

[0031] In this embodiment, when the plasma implantation process is performed, the semiconductor substrate 200 is not shielded, and the barrier layer 220 formed in the semiconductor substrate 200 is arranged around the outer side of the groove 210, and the barrier layer 220 has a distance greater than zero from the outer side of the groove 210. The distance between the barrier layer 220 and the outer side of the groove 210 and the thickness of the barrier layer 220 are determined by the performance of the semiconductor device finally formed. The distance between the barrier layer 220 and the outer side of the groove 210 (i.e., the depth of plasma implantation) and the thickness of the barrier layer 220 can be adjusted by adjusting the energy of plasma implantation, the implantation dose, the type of implanted elements, and the grain boundaries of the semiconductor substrate 200.

[0032] Furthermore, in this embodiment, the plasma implantation process uses vertical implantation, which can make the barrier layer 220 evenly and symmetrically distributed on both sides of the trench 210. If the barrier layer 220 is asymmetrically distributed on both sides of the trench 210, for example, one side is closer to the trench and the other side is farther away from the trench, the barrier layer 220 closer to the trench may overlap with the source and drain regions formed subsequently, resulting in failure.

[0033] In another embodiment of the present invention, when performing a plasma injection process, the semiconductor substrate 200 is partially shielded, and only the area between adjacent grooves 210 is exposed, and the width of the exposed area is smaller than the width between adjacent grooves 210. Then, after plasma injection, a barrier layer is formed only in the exposed area, and the barrier layer has a distance greater than zero from the outer side surface of the groove, and no barrier layer is formed in other areas.

[0034] If an N-type semiconductor device is to be formed, the conductivity type of the plasma injected in this step is P-type. If a P-type semiconductor device is to be formed, the conductivity type of the plasma injected in this step is N-type.

[0035] In the prior art, a shallow trench isolation structure is used as an isolation layer for the source and drain regions of adjacent transistors. Due to the influence of subsequent cleaning processes, the shallow trench isolation structure will produce defects, causing the active regions to contact due to the effect of surface tension, resulting in a short circuit in the active regions. However, the present invention does not need to form a shallow trench isolation structure for isolation. The barrier layer formed by plasma injection is used as an isolation layer for the source and drain regions of adjacent transistors. Since the source and drain regions and the barrier layer are injected with opposite ions, a PN junction is formed between the source and drain regions and the barrier layer. The built-in electric field of the PN junction can prevent the diffusion of electrons, thereby achieving an isolation effect. Among them, the farther the distance between adjacent transistors, the better the isolation effect of the barrier layer 220.

[0036] Please refer to step S12 and Figure 6 , a gate structure 230 is formed in the trench 210 .

[0037] The gate structure 230 includes a gate insulating layer 231 and a gate 232. In this embodiment, the method for forming the gate structure further includes the following steps:

[0038] See also Figure 4 , a gate insulating material 400 is formed in the groove 210, and the gate insulating material 400 covers the sidewalls of the groove 210 and the surface of the semiconductor substrate 200. The gate insulating material 400 may be an oxide or a nitride. Among them, the gate insulating material 400 may be formed by in-situ steam generation (ISSG), atomic layer deposition (ALD) or thermal oxidation process. The specific thickness of the gate insulating material is determined by the device voltage. For example, in this embodiment, the thickness of the gate insulating material 400 is 2nm-10nm. In this embodiment, the gate insulating material 400 is formed by an atomic layer deposition process, and the gate insulating material 400 is silicon oxide.

[0039] See also Figure 5, a conductive material 410 is filled in the trench 210, the conductive material 410 fills the trench 210 and covers the gate insulating material 400 on the surface of the semiconductor substrate 200. The conductive material 410 can be a conventional material for forming a gate, such as polysilicon. In this step, the conductive material 400 can be formed by a low pressure chemical vapor deposition process (LPCVD).

[0040] See also Figure 6 , remove the conductive material 410 and the gate insulating material 400 on the surface of the semiconductor substrate 200, and form a gate insulating layer 231 and a gate 232 located in the trench 210. Specifically, in this step, the conductive material 410 and the gate insulating material 400 on the surface of the semiconductor substrate 200 can be removed by etching back, chemical mechanical polishing and cleaning. The gate insulating layer 231 covers the sidewalls of the trench 210, and the gate 232 covers the gate insulating layer 231 and fills the trench 210.

[0041] Please refer to step S13 and Figure 7 A channel region 240 is formed in the semiconductor substrate 200 , and the channel region 240 corresponds to the trench 210 . The barrier layer 220 divides the semiconductor substrate into a plurality of regions, each region having a trench 210 , and a channel region 240 is formed in the semiconductor substrate 200 in the region.

[0042] In this embodiment, the channel region 240 is formed in the semiconductor substrate 200 below the trench 210, and is also formed in the semiconductor substrate 200 on the side of the trench 210, that is, the channel layer 240 extends upward along the sidewall of the trench 210. It can be understood that in order to form the source and drain regions later, the channel region 240 is only formed on part of the side of the trench 210. In another embodiment of the present invention, the channel region 240 may also be formed only in the semiconductor substrate 200 below the trench 210.

[0043] Further, in this embodiment, if Figure 7 As shown, the semiconductor substrate 200 is partially shielded by a photoresist layer to expose the area where the channel needs to be formed; the semiconductor substrate 200 is plasma implanted to form the channel region 240. The depth and thickness of the formed channel region 240 can be adjusted by controlling the energy of the plasma implantation, the implantation dose, the implantation element type and the grain boundary of the semiconductor substrate 200; the opening width of the photoresist layer can be controlled to control the width of the channel region 240.

[0044] Furthermore, in this embodiment, the plasma injection process adopts vertical injection, which can form the channel region 240 directly below the groove 210 and symmetrically distributed, thereby ensuring the channel length; if the plasma injection process adopts oblique incidence, the formed channel region 240 may also be inclined, which may cause the source and drain regions to be unable to be electrically connected to the channel region, affecting the device performance. Further, the width of the channel region 240 is greater than the width of the groove 210 to ensure the channel length. If the width of the channel region 240 is narrow, the source and drain regions need to be injected at a deeper position to form an electrical connection, making the channel length too short, affecting the performance of the semiconductor device.

[0045] For further information, see Figure 8 In this embodiment, after the plasma injection, an annealing process is performed to diffuse the ions in the channel region 240 upward, forming a channel region 240 extending upward along the sidewall of the trench 210. The channel region 240 is arranged corresponding to the bottom and side of the trench 210, so that the source and drain regions 250 (shown in FIG. Fig. 9 The gate structure 230 is connected to the channel region 240, and the overlapping area between the channel region 240 and the gate structure 230 is increased, thereby increasing the length of the channel (the length of the channel H is shown in FIG. 1 ). Fig.10 shown).

[0046] In another embodiment of the present invention, the plasma injection depth is changed so that the channel region 240 extends upward along the sidewall of the trench 210. That is, as the depth of the trench 210 decreases, the plasma injection depth gradually decreases to avoid injecting plasma into the gate structure 230 to form a channel region 240 extending upward along the sidewall of the trench 210. For example, for a trench 210 with inclined sidewalls, the trench depth at the bottom is the largest, and correspondingly, the plasma injection depth is the largest, and the trench depth at the sidewall gradually decreases, and correspondingly, the plasma injection depth gradually decreases.

[0047] Furthermore, the plasma used to form the barrier layer 220 and the plasma used to form the channel region 240 are ions of the same conductive type. That is, the barrier layer 220 and the channel region 240 are of the same conductive type. For example, if an N-type semiconductor device is to be formed, the conductive type of the plasma injected in this step is P-type, and if a P-type semiconductor device is to be formed, the conductive type of the plasma injected in this step is N-type.

[0048] Please refer to step S14 and Fig. 9A source-drain region 250 is formed between the trench 210 and the barrier layer 220, and the source-drain region 250 is electrically connected to the channel region 240. The source-drain region 250 is electrically connected to the channel region 240, which means that when a voltage is applied to the gate structure 230, the channel region 240 is turned on, and carriers flow between the source and the drain, thereby forming a current.

[0049] There is a gap between the trench 210 and the barrier layer 220, and the gap is used to form a source-drain region 250. The conductivity type of the source-drain region 250 is opposite to that of the barrier layer 220. For example, if an N-type semiconductor device is to be formed, the conductivity type of the source-drain region 250 is N-type, and the conductivity type of the barrier layer 220 is P-type; if a P-type semiconductor device is to be formed, the conductivity type of the source-drain region 250 is P-type, and the conductivity type of the barrier layer 220 is N-type. The source-drain region 250 forms a PN junction with the barrier layer 220, and the built-in electric field of the PN junction prevents electron diffusion, thereby achieving an isolation effect.

[0050] Furthermore, in this embodiment, a structure such as a photoresist layer is used to partially shield the semiconductor substrate 200, and only the area where the source and drain regions 250 need to be formed is exposed, that is, the interval area between the groove 210 and the barrier layer 220 is exposed, and plasma is implanted into the exposed area of ​​the semiconductor substrate 200 to form the source and drain regions 250. The depth and width of the source and drain regions 250 are determined by the performance of the semiconductor device, and the depth and concentration of the source and drain regions 250 can be adjusted by adjusting the energy of the plasma implantation, the implantation dose, the implantation element type, and the grain boundary of the semiconductor substrate 200.

[0051] In the prior art, the source and drain regions are formed by oblique-incidence doping, and the oblique-incidence doping is easily blocked by the photoresist layer above it, resulting in electrical failure. However, the preparation method of the present invention forms the source and drain regions 250 by a plasma injection process, and there is no oblique-incidence doping, and it will not be blocked by the photoresist layer, thereby not causing electrical failure and improving the performance of the semiconductor device.

[0052] Further, in the present embodiment, the source and drain region 250 includes a shallow doped drain 251 and a source and drain electrode 252. The source and drain electrode 252 is electrically connected to the channel region 240 through the shallow doped drain 251, that is, the shallow doped drain 251 is located below the source and drain electrode 252 and is electrically connected to the channel region 240. In the present embodiment, the shallow doped drain 251 can be formed by a plasma injection process, and then the parameters of the plasma injection are changed to form the source and drain electrode 252. The shallow doped drain 251 and the source and drain electrode 252 can both be formed by a plasma injection process. Compared with the prior art that uses a method of multiple times of oblique incidence doping to form a shallow doped drain and a source and drain electrode, the preparation method of the present invention has good conductivity in forming the shallow doped drain 251 and the source and drain electrode 252.

[0053] For further information, see Fig.10 , after the step of forming the source and drain regions 150 between the trench 210 and the barrier layer 220, the following steps are included: forming a passivation layer 260, the passivation layer 260 covers the surface of the semiconductor substrate 200 and the surface of the gate structure 230. The passivation layer 260 is used to isolate the gate structure 230 from the outside and play a protective role. The passivation layer 260 includes but is not limited to nitride, such as silicon nitride, which can be formed by a low pressure chemical vapor deposition process (LPCVD).

[0054] In the prior art, the length of the channel is usually defined by the photolithography process. If the electrical properties of the formed semiconductor device are not good and the channel length needs to be adjusted, the mask needs to be re-made, and the cost of modifying the mask is high, time-consuming and costly. However, the semiconductor device formed by the preparation method of the present invention has a channel length (such as Fig.10 The length of the channel can be directly adjusted by the etching depth of the groove 210 and the plasma injection depth of the source and drain regions 250, and can be fine-tuned at any time, which greatly reduces the production cost and saves time. In addition, the preparation method of the present invention can reduce the number of masks and save process steps.

[0055] The present invention also provides a semiconductor device manufactured by the above manufacturing method. Fig.10 In one embodiment of the semiconductor device of the present invention, the semiconductor device comprises a semiconductor substrate 200, a barrier layer 220, a gate structure 230, a channel region 240 and a source / drain region 250. The gate structure 230, the channel region 240 and the source / drain region 250 form a transistor.

[0056] The semiconductor substrate 200 is formed with a plurality of mutually independent trenches 210. The semiconductor substrate 200 may be a silicon, germanium or other substrate. In this embodiment, the semiconductor substrate 200 is a silicon substrate.

[0057] The barrier layer 220 is formed between adjacent trenches 210 by a plasma implantation process. The barrier layer 220 serves as an isolation layer between adjacent transistors. There is a gap between the trench 210 and the barrier layer 220. In this embodiment, the barrier layer 220 is arranged around the outer side of the trench 210, and the gap between the barrier layer 220 and the outer side of the trench 210 is greater than zero. In another embodiment of the present invention, the barrier layer 220 is only formed between adjacent transistors, but not around the outer side of the trench 210.

[0058] The gate structure 230 is formed in the trench 210 . The gate structure 230 includes a gate insulating layer 231 covering the sidewall of the trench 210 and a gate 232 filling the trench 210 . The gate insulating layer 231 serves as an isolation layer between the gate 232 and the channel region 240 and the source and drain region 250 .

[0059] The channel region 240 is formed in the semiconductor substrate 200 and corresponds to the trench 210. In the present embodiment, the channel region 250 is disposed at the bottom of the trench 210 and extends upward along the sidewall of the trench 210. It is understood that in order to provide sufficient formation space for the source and drain regions 250, the channel region 240 is only formed on a portion of the side surface of the trench 210. In another embodiment of the present invention, the channel region 240 may also be formed only in the semiconductor substrate 200 below the trench 210.

[0060] Furthermore, the width of the channel region 240 is greater than the width of the trench 210 to increase the contact area between the source and drain regions 250 and the channel region 240. If the width of the channel region 240 is narrow, the source and drain regions need to be formed at a deeper position, resulting in a too short channel length, which affects the performance of the semiconductor device.

[0061] The source and drain regions 250 are disposed between the trench 210 and the barrier layer 220 and are electrically connected to the channel region 240. The source and drain regions 250 are formed in the spacing region between the trench 210 and the barrier layer 220. The conductivity type of the barrier layer 220 is opposite to that of the source and drain regions 250. For example, if an N-type semiconductor device is to be formed, the conductivity type of the source and drain regions 250 is N-type, while the conductivity type of the barrier layer 220 is P-type; if a P-type semiconductor device is to be formed, the conductivity type of the source and drain regions 250 is P-type, while the conductivity type of the barrier layer 220 is N-type. The source and drain regions 250 form a PN junction with the barrier layer 220. The built-in electric field of the PN junction prevents electron diffusion and plays an isolation effect.

[0062] Further, in this embodiment, the source and drain region 250 includes a shallowly doped drain 251 and a source and drain electrode 252. The source and drain electrode 252 is electrically connected to the channel region 240 through the shallowly doped drain 251, that is, the shallowly doped drain 251 is located below the source and drain electrode 252 and is electrically connected to the channel region 240.

[0063] Furthermore, the semiconductor device further includes a passivation layer 260, which covers the surface of the semiconductor substrate 200 and the surface of the gate structure 230. The passivation layer 260 is used to isolate the gate structure 230 from the outside and play a protective role. The passivation layer 260 includes but is not limited to nitride, such as silicon nitride.

[0064] The semiconductor device of the present invention has good electrical performance, simple preparation and low process cost.

[0065] The above is only a preferred embodiment of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for preparing a semiconductor device, characterized in that: The steps include: Providing a semiconductor substrate, wherein a plurality of trenches independent of each other are formed in the semiconductor substrate; Plasma implantation to form a barrier layer between adjacent grooves, wherein the barrier layer is formed around the outer side of the groove, and there is a gap between the barrier layer and the outer side of the groove, and the barrier layers between adjacent grooves are connected to each other; forming a gate structure in the trench; forming a channel region in the semiconductor substrate, the channel region corresponding to the trench; A source / drain region is formed between the trench and the barrier layer, the source / drain region is electrically connected to the channel region, and the distance between the surface of the semiconductor substrate and the top of the source / drain region is greater than the distance between the surface of the semiconductor substrate and the top of the barrier layer; The conductivity type of the barrier layer is opposite to that of the source and drain regions, and the conductivity type of the barrier layer is the same as that of the channel region; a PN junction is formed between the source and drain regions and the barrier layer, and a built-in electric field of the PN junction prevents electron diffusion.

2. The method for preparing a semiconductor device according to claim 1, wherein: The gate structure includes a gate insulating layer and a gate, and the step of forming the gate structure in the trench further includes: forming a gate insulating material in the trench, wherein the gate insulating material covers the trench sidewalls and the surface of the semiconductor substrate; Filling the trench with a conductive material, wherein the conductive material fills the trench and covers the gate insulating material on the surface of the semiconductor substrate; The conductive material and the gate insulating material on the surface of the semiconductor substrate are removed to form a gate insulating layer and a gate located in the trench.

3. The method for preparing a semiconductor device according to claim 1, characterized in that: The step of forming a channel region in the semiconductor substrate further includes performing plasma implantation on the semiconductor substrate to form the channel region.

4. The method for preparing a semiconductor device according to claim 3, characterized in that: The width of the channel region is greater than the width of the trench.

5. The method for preparing a semiconductor device according to claim 4, characterized in that: After the plasma implantation, an annealing process is performed to allow the channel region to extend upward along the sidewall of the trench.

6. The method for preparing a semiconductor device according to claim 4, characterized in that: The plasma implantation depth is changed so that the channel region extends upward along the sidewall of the trench.

7. The method for preparing a semiconductor device according to claim 1, characterized in that: The step of forming a source and drain region between the trench and the barrier layer further includes: performing plasma implantation on the semiconductor substrate to form a shallowly doped drain and a source and drain electrode, wherein the source and drain electrode is electrically connected to the channel region through the shallowly doped drain.

8. The method for preparing a semiconductor device according to claim 1, wherein: After the step of forming source and drain regions between the trench and the barrier layer, the method includes the following steps: forming a passivation layer, wherein the passivation layer covers the surface of the semiconductor substrate and the surface of the gate structure.

9. A semiconductor device, characterized in that: include: A semiconductor substrate having a plurality of mutually independent trenches formed therein; A barrier layer is formed between adjacent grooves by a plasma implantation process, the barrier layer is arranged around the outer side of the groove, and there is a gap between the barrier layer and the outer side of the groove, and the barrier layers between adjacent grooves are connected to each other; a gate structure formed in the trench; a channel region formed in the semiconductor substrate and corresponding to the trench; A source-drain region, disposed between the trench and the barrier layer and electrically connected to the channel region, wherein the distance between the surface of the semiconductor substrate and the top of the source-drain region is greater than the distance between the surface of the semiconductor substrate and the top of the barrier layer; The conductivity type of the barrier layer is opposite to that of the source and drain regions, and the conductivity type of the barrier layer is the same as that of the channel region; a PN junction is formed between the source and drain regions and the barrier layer, and a built-in electric field of the PN junction prevents electron diffusion.

10. The semiconductor device according to claim 9, characterized in that The gate structure includes a gate insulating layer covering the sidewall of the trench and a gate filling the trench.

11. The semiconductor device according to claim 9, characterized in that The width of the channel region is greater than the width of the trench.

12. The semiconductor device according to claim 9, characterized in that The channel region is disposed at the bottom of the trench and extends upward along the sidewall of the trench.

13. The semiconductor device according to claim 9, wherein: It also includes a passivation layer, which covers the surface of the semiconductor substrate and the surface of the gate structure.