A roadbed filling method for widening a flooded road section

By using a combination of impermeable concrete retaining walls, construction waste recycled aggregate cushions and foam lightweight soil in the widening of flooded sections, the problems of complex construction and high material consumption are solved, and the stability of the roadbed and the environment are improved. Dual goals of protection.

CN114197261BActive Publication Date: 2024-10-29XIAN HIGHWAY INST
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202210084052.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-19
Publication Date
2024-10-29
Estimated Expiration
2042-01-19

AI Technical Summary

Technical Problem

When existing road widening technology deals with flooded road sections, the construction process is complex and material consumption is large, making it difficult to effectively solve the problems of roadbed stability and environmental protection.

Method used

The roadbed filling method is a combination of impermeable concrete baffle wall, construction waste recycled aggregate cushion and foam lightweight soil. By installing an impermeable concrete baffle wall outside the roadbed slope, the construction waste recycled aggregate cushion is laid. Foam lightweight soil is poured in between to form a new roadbed, which is combined with anti-seepage geotextiles and anti-floating anchors to enhance the stability and waterproof performance of the roadbed.

Benefits of technology

It simplifies the construction process, reduces material consumption and land occupation requirements, improves the stability and water resistance of the roadbed, conforms to the concept of green highway construction, and reduces damage to the environment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114197261B_ABST
    Figure CN114197261B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for filling a roadbed for widening a flooded section of a road. The method comprises: excavating a foundation pit outside the original roadbed slope of the road to be expanded, and installing an impermeable concrete baffle wall outside the foundation pit; laying a cushion layer of recycled aggregates from construction waste at the bottom of the foundation pit; digging steps on the original roadbed slope of the road to be expanded to form a step surface; pouring foamed lightweight soil on the cushion layer of recycled aggregates from construction waste between the impermeable concrete baffle wall and the step surface, and forming a new roadbed after the foamed lightweight soil solidifies. The present invention has a simple structure and a clear governance target, and can effectively solve the problems of large land occupation, differential settlement, and great construction difficulty when filling a roadbed for widening a flooded section of a road; by adopting a cushion layer of recycled aggregates from construction waste, it can effectively solve practical problems such as shortage of building materials and garbage siege, which is in line with the current concept of "green highway" construction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of road widening, and in particular to a roadbed filling method for widening a flooded road section. Background Art

[0002] Expansion of existing roads has become a major measure to improve road capacity, adapt to traffic growth and meet social needs. Due to the vast territory of my country, the process of road reconstruction and expansion will inevitably pass through low-lying areas, or sections near rivers (lakes, reservoirs), or sections with groundwater seepage on the slopes. Conventional treatment methods generally use submerged retaining walls or submerged slope treatment. Submerged retaining walls are constructed by using large-section, masonry retaining walls, concrete expansion foundations, composite piles or permeable replacement fillers to treat the original foundation and then build gravity retaining walls. Submerged slopes are generally protected by masonry fully enclosed slope protection. The above methods have complex construction processes and consume a lot of building materials. Especially for road widening projects, how to deal with the potential harm of flooding to the roadbed and ensure the stability of the roadbed; at the same time, using new materials, devices and methods to improve construction efficiency, reduce environmental damage, and reduce land resources are key issues in widening roads in submerged sections. Summary of the Invention

[0003] In view of the shortcomings of the prior art, the present invention provides a roadbed filling method for widening a flooded road section.

[0004] The present invention discloses a roadbed filling method for widening a flooded road section, the roadbed filling method comprising:

[0005] Excavate a foundation pit outside the original roadbed slope of the road to be expanded, and install an anti-seepage concrete retaining wall outside the foundation pit;

[0006] Laying a cushion layer of recycled aggregate from construction waste at the bottom of the foundation pit;

[0007] The original roadbed slope of the road to be expanded is stepped to form a stepped surface;

[0008] Foam lightweight soil is poured on the construction waste recycled aggregate cushion between the anti-seepage concrete baffle wall and the step surface, and a new roadbed is formed after the foam lightweight soil solidifies. The new roadbed is connected to the original roadbed through the step surface.

[0009] As a further improvement of the present invention, the thickness of the anti-seepage concrete baffle wall is not less than 20 cm, and the lower end of the anti-seepage concrete baffle wall is placed a certain distance below the ground line;

[0010] The lower end of the anti-seepage concrete baffle wall extends horizontally to both sides by no less than 20 cm to form a "T"-shaped structure.

[0011] As a further improvement of the present invention, the anti-seepage concrete in the anti-seepage concrete baffle wall is composed of cement, fly ash, coarse aggregate, fine aggregate and admixture.

[0012] As a further improvement of the present invention, the width of the step surface is not less than 1m;

[0013] The horizontal steps face inwards of the original roadbed with a preset slope, and the slope is not less than 2%.

[0014] As a further improvement of the present invention, the construction waste recycled aggregate cushion layer is placed on the original foundation, and the construction waste recycled aggregate cushion layer is laid by a layered paving method, with a layer thickness of 20cm to 30cm;

[0015] The overall thickness of the construction waste recycled aggregate cushion layer is 50 cm to 60 cm, and the compaction degree of the construction waste recycled aggregate cushion layer is not less than 93%.

[0016] As a further improvement of the present invention, the construction waste recycled aggregate cushion layer is composed of one or more of concrete, mortar, stone and brick, and the maximum particle size of the construction waste recycled aggregate cushion layer is not greater than 150 mm;

[0017] The brick content in the construction waste recycled aggregate cushion layer is no more than 20%; the organic matter content is no more than 5%; the light debris content is no more than 0.3%; and the mud content is no more than 5%.

[0018] As a further improvement of the present invention, the foamed lightweight soil is poured using a layered pouring method;

[0019] The foamed lightweight soil is prepared by mixing one or more of cement, water, foaming agent, mineral powder and fly ash powder.

[0020] As a further improvement of the present invention, the roadbed filling method further comprises:

[0021] Before pouring the foam lightweight soil, a layer of anti-seepage geotextile is laid on the horizontal and vertical surfaces of the step surface of the original roadbed slope and above the construction waste recycled aggregate cushion layer;

[0022] After the foamed lightweight soil solidifies, a layer of anti-seepage geotextile is also laid on the upper side of the foamed lightweight soil;

[0023] The anti-seepage geotextile is a geotechnical anti-seepage material that is composited with a plastic film as an anti-seepage base material and a non-woven fabric.

[0024] As a further improvement of the present invention, the roadbed filling method further comprises:

[0025] After pouring the foam lightweight soil, a plurality of oblique anti-floating anchor rods are driven into the foam lightweight soil at regular intervals along the vertical direction;

[0026] One end of each anti-floating anchor rod is placed in the foam lightweight soil, and the other end obliquely passes through the corresponding step surface and is placed in the original roadbed.

[0027] As a further improvement of the present invention, the anti-floating anchor rod has a diameter not less than The threaded steel anchor rod is inserted into the original roadbed to a depth of 2m-3m;

[0028] The exposed end of the threaded steel anchor rod is not less than 20 cm long, an anchor bar is provided inside the threaded steel anchor rod, and a guide steel bar with a length of not less than 100 mm is provided at the front end of the anchor bar; a sediment section is formed between the guide steel bar and the tail end of the threaded steel anchor rod;

[0029] The cement mortar in the threaded steel anchor rod is grouting in a ratio of 1:1, the water-cement ratio in the cement mortar is 0.4, and the strength of the cement mortar is not less than 30 MPa.

[0030] Compared with the prior art, the present invention has the following beneficial effects:

[0031] The invention has a simple structure and a clear treatment target, and can effectively solve the problems of large land occupation, differential settlement and great construction difficulty when widening the roadbed in flooded sections.

[0032] The present invention adopts the construction waste recycled aggregate cushion layer, which can effectively solve the practical problems such as shortage of construction materials and garbage siege, and is in line with the current concept of "green highway" construction;

[0033] Compared with conventional submerged retaining walls and submerged slopes, this method has a narrow working surface, has low requirements on the bearing capacity of the original foundation, can save a lot of land resources, and reduce a lot of time costs. It has broad practical significance and application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 A schematic diagram of a process for widening a roadbed and filling a flooded road section disclosed in the present invention;

[0035] Figure 2 This is a structural schematic diagram of a roadbed filling method for widening a flooded road section disclosed in the present invention;

[0036] Figure 3 The present invention discloses a schematic diagram of an anti-floating anchor rod structure for a roadbed filling method for widening a flooded road section.

[0037] In the picture:

[0038] 1. Original roadbed; 2. New roadbed; 3. Foam lightweight soil; 4. Anti-seepage geotextile; 5. Threaded steel anchor rod; 5-1. Sediment section; 6. Cushion layer of recycled aggregate from construction waste; 7. Anti-seepage concrete retaining wall; 8. Anchor bars; 8-1. Hanging steel bars; 9. Guide steel bars; 10. Centering bracket. DETAILED DESCRIPTION

[0039] To make the objectives, technical solutions, and advantages of the embodiments of the present invention more clear, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts shall fall within the scope of protection of the present invention.

[0040] In the description of the present invention, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings and are intended solely to facilitate and simplify the description of the present invention. They are not intended to indicate or imply that the devices or components referred to must have, be constructed, or operate in a specific orientation, and therefore should not be construed as limitations on the present invention. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0041] In the description of the present invention, it should also be noted that, unless otherwise expressly specified or limited, the terms "mounted," "connected," and "connected" should be understood broadly. For example, they may refer to fixed, detachable, or integral connections; mechanical or electrical connections; direct or indirect connections through an intermediate medium; and internal communication between two components. Those skilled in the art will understand the specific meanings of the above terms in the present invention based on the specific circumstances.

[0042] The present invention is described in further detail below with reference to the accompanying drawings:

[0043] like Figure 1 As shown, the present invention discloses a roadbed filling method for widening a flooded road section, the roadbed filling method comprising:

[0044] A foundation pit is excavated outside the slope of the original roadbed 1 of the road to be expanded, and an anti-seepage concrete retaining wall 7 is installed outside the foundation pit;

[0045] Laying a construction waste recycled aggregate cushion layer 6 at the bottom of the foundation pit;

[0046] Stepping is performed on the slope of the original roadbed 1 of the road to be expanded to form a step surface;

[0047] Foamed lightweight soil 3 is poured on the construction waste recycled aggregate cushion 6 between the anti-seepage concrete baffle wall 7 and the step surface. After the foamed lightweight soil 3 solidifies, a new roadbed 2 is formed. The new roadbed 2 is connected to the original roadbed 1 through the step surface.

[0048] The invention has a simple structure and a clear treatment target, and can effectively solve the problems of large land occupation, differential settlement and great construction difficulty when widening the roadbed in flooded sections.

[0049] The present invention adopts the construction waste recycled aggregate cushion layer 6, which can effectively solve the practical problems such as shortage of construction materials and garbage siege, and is in line with the current concept of "green highway" construction;

[0050] Compared with conventional submerged retaining walls and submerged slopes, this method has a narrow working surface, has low requirements on the bearing capacity of the original foundation, can save a lot of land resources, and reduce a lot of time costs. It has broad practical significance and application prospects.

[0051] Specifically:

[0052] like Figure 2 As shown, the thickness of the anti-seepage concrete baffle wall 7 in the present invention is not less than 20 cm, and the thickness of the anti-seepage concrete baffle wall 7 in the present invention is preferably 20 cm, and the lower end of the anti-seepage concrete baffle wall 7 is placed a certain distance below the ground line; the lower end of the anti-seepage concrete baffle wall 7 extends horizontally to both sides by not less than 20 cm, forming a "T"-shaped structure; the lower end of the anti-seepage concrete baffle wall 7 in the present invention extends horizontally to both sides by 20 cm, and the setting of the "T"-shaped structure can effectively enhance the structural stability of the anti-seepage concrete baffle wall 7. The setting of the anti-seepage concrete baffle wall 7 can ensure a closed spatial environment when pouring the foam lightweight soil 3, and can also improve the impermeability to prevent external water from entering the roadbed.

[0053] Furthermore, the anti-seepage concrete in the anti-seepage concrete baffle wall 7 of the present invention is composed of cement, fly ash, coarse aggregate, fine aggregate and admixtures. The main raw materials and proportion requirements are as follows:

[0054] 1. Cement: 1) Ordinary Portland cement, strength not less than 32.5Mpa; 2) Use low hydration heat cement, the 7-day hydration heat index of cement shall not be higher than 275kJ / kg, and early strength cement with the letter R shall not be used; 3) The alkali content of cement shall meet the requirement that the total alkali content of cement in each cubic meter of concrete shall not exceed 2.25kg.

[0055] 2. Fly ash: The grade of fly ash shall not be lower than Grade II, and high calcium fly ash shall not be used.

[0056] 3. Coarse aggregate: Coarse aggregate should be continuously graded, and machine-crushed stone with uniform gradation of 5 to 31.5 mm should be used. The mud content should not exceed 1%.

[0057] 4. Fine aggregate: To reduce the late shrinkage of concrete, medium-coarse sand with a fineness modulus of 2.5 to 3.0 should be used. The mud content of sand should not exceed 3%. The mud content should not exceed 1.0%.

[0058] 5. Admixtures: 1) Admixtures should be low-alkali, low-heat-of-hydration waterproofing agents, expansion agents, air-entraining agents, water-reducing agents, or air-entraining water-reducing agents. The admixture dosage should not exceed 5% of the cement mass; 2) They should have early strength properties; 3) Use a high-efficiency water-reducing agent.

[0059] Furthermore, the design requirements for the anti-seepage concrete mix ratio in the present invention are as follows:

[0060] (1) The total amount of cement and mineral admixtures in each cubic meter of concrete should not be less than 320 kg;

[0061] (2) The sand ratio should be 35% to 45%; 3. The air content of anti-permeability concrete mixed with air-entraining agent should be controlled at 3% to 5%. 4. When designing the mix ratio of anti-permeability concrete, an anti-permeability performance test should be added.

[0062] (3) Concrete mixed with air-entraining agent should also be tested for air content.

[0063] During actual construction, the impermeable concrete baffle wall 7 can be cast on-site, based on the required height of the project, after formwork is erected. The formwork is removed after the baffle wall has developed a certain strength. To achieve concrete impermeability, the present invention incorporates air-entraining admixtures to create disconnected bubbles within the concrete, interrupting capillary channels and altering the pore structure, thereby improving the concrete's impermeability. Furthermore, reducing the water-cement ratio, selecting the appropriate type and strength grade of cement, and ensuring construction quality, particularly through vibrating and maintaining adequate curing, all play a significant role in improving concrete impermeability.

[0064] Furthermore, during construction, the impermeable concrete retaining wall 7 not only serves as the outer formwork but also as a finishing touch, enhancing the overall appearance of the foamed lightweight soil 3. During the prefabrication process of the impermeable concrete retaining wall 7, strict dimensional control is required to facilitate installation. Because the foamed lightweight soil 3 is a large structure with varying dimensions at the edges and top, the prefabricated panels are broken down into smaller, custom-sized panels. These panels are then adjusted based on actual conditions during assembly. The panels of the impermeable concrete retaining wall 7 must be securely joined to prevent leakage.

[0065] Furthermore, the width of the step surface in the present invention is not less than 1m; the horizontal step surface is inclined inwardly toward the original roadbed with a preset slope, and the slope is not less than 2%. The width of the step surface in the present invention is preferably 1m; the horizontal step surface is inclined inwardly toward the original roadbed with a preset slope of preferably 2%. The new roadbed 2 in the present invention is connected to the original roadbed 1 through the step surface.

[0066] Furthermore, the construction waste recycled aggregate cushion layer 6 of the present invention is placed on the original foundation 1, and the construction waste recycled aggregate cushion layer 6 is laid by a layered paving method, with a layer thickness of 20cm to 30cm; the overall thickness of the construction waste recycled aggregate cushion layer 6 is 50cm to 60cm, and the compaction degree (heavy duty) of the construction waste recycled aggregate cushion layer 6 should be the same as the compaction degree requirement of the embankment at the same level, and not less than 93%; the construction waste recycled aggregate cushion layer 6 is composed of one or more of concrete, mortar, stone and bricks, and the maximum particle size in the construction waste recycled aggregate cushion layer 6 is not greater than 150mm; the brick content in the construction waste recycled aggregate cushion layer is not greater than 20%; the organic matter content is not greater than 5%, the light debris content is not greater than 0.3%, and the mud content is not greater than 5%. The recycled aggregate technical indicators of the construction waste recycled aggregate cushion layer 6 of the present invention are shown in Table 1.

[0067] Table 1 Technical indicators of recycled aggregate

[0068]

[0069]

[0070] Furthermore, during the specific construction of the construction waste recycled aggregate cushion layer 6 in the present invention, construction parameters such as machine combination, compaction machine specifications, loose paving thickness, number of rolling times, rolling speed, and optimal moisture content should be determined based on the on-site paving test section.

[0071] Furthermore, the foamed lightweight soil 3 in the present invention is poured using a layered pouring method. Because its bulk density is generally 20% to 60% of that of ordinary cement concrete, the additional load on the foundation is relatively small. This reduces the requirements for the existing foundation's bearing capacity. Consequently, the traditional concept of "reducing roadbed settlement by strengthening the existing foundation's bearing capacity" has been transformed into "reducing roadbed settlement by reducing the additional load on the roadbed itself."

[0072] Furthermore, the foamed lightweight soil 3 is a lightweight, fluid building material made by mixing one or more of cement, water, a foaming agent, mineral powder, and fly ash powder. The mix ratio of the foamed lightweight soil 3 is selected based on strength, wet bulk density, and fluidity requirements. The foamed lightweight soil 3 of the present invention is produced in two simultaneous steps: the first is the preparation of cement slurry, in which water and cement are stirred and mixed for at least 10 seconds; the second is the preparation of the bubble clusters, in which a foaming agent and water are continuously added to a dilution device in a ratio of 1:39 to produce a diluent, which is then added to the bubble device while maintaining the air pressure at no less than 0.6 MPa. The second step is to stir and mix the cement slurry and bubble clusters for 5 seconds before pumping and pouring.

[0073] During actual construction, the foamed lightweight soil 3's highly fluid nature makes it easy to self-flow and level during construction, eliminating the need for vibration and compaction. This significantly reduces the required working surface area for mechanical construction and reduces the need for land acquisition. The foamed lightweight soil 3 is also self-supporting and, after hardening, exerts minimal lateral forces. This characteristic reduces reliance on the mechanical properties of the retaining structure, reduces the size of the retaining structure, and thus saves on masonry work. Laboratory tests and engineering practice have shown that the hardened foamed lightweight soil 3 possesses the strength, durability, and other mechanical properties of roadbed fillers.

[0074] Furthermore, the roadbed filling method of the present invention further comprises:

[0075] Before pouring the foamed lightweight soil 3, a layer of anti-seepage geotextile 4 is laid on the horizontal and vertical surfaces of the step surface of the original roadbed 1 slope and on the construction waste recycled aggregate cushion 6;

[0076] After the foamed lightweight soil 3 solidifies, a layer of anti-seepage geotextile 4 is also laid on the upper side of the foamed lightweight soil 3;

[0077] The anti-seepage geotextile 4 of the present invention is a geotechnical anti-seepage material composed of a plastic film as an anti-seepage base material and a non-woven fabric. The anti-seepage geotextile 4 of the present invention has a low specific gravity, good extensibility, corrosion resistance, low temperature resistance, and excellent frost resistance, effectively preventing moisture from invading the original roadbed 1. The provision of the anti-seepage geotextile 4 on both the horizontal and vertical surfaces of the stepped surface of the present invention effectively enhances the interlocking ability between the original roadbed 1 and the new roadbed 2.

[0078] like Figure 1-2 As shown, the roadbed filling method in the present invention also includes:

[0079] After pouring the foamed lightweight soil 3, a plurality of oblique anti-floating anchor rods are driven into the foamed lightweight soil 3 at regular intervals along the vertical direction;

[0080] One end of each anti-floating anchor rod is placed in the foam lightweight soil 3, and the other end obliquely passes through the corresponding step surface and is placed in the original roadbed.

[0081] Furthermore, the vertical anchors in the multiple anti-floating anchors of the present invention can be spaced at regular intervals based on the roadbed height, such as at each step. Horizontally, anchors can be placed every 5 meters. The installation of multiple anti-floating anchors effectively prevents the buoyancy of water from affecting the stability of the foamed lightweight soil roadbed, thereby enhancing the roadbed's stability through the anchoring effect of the anchors.

[0082] Furthermore, the anti-floating anchor rod in the present invention has a diameter not less than The threaded steel anchor rod 5 of the present invention preferably has a diameter of The threaded steel anchor rod 5 is inserted into the original roadbed 1 to a depth that can be adjusted according to the filler of the original roadbed 1. The threaded steel anchor rod 5 of the present invention is preferably inserted into the original roadbed 1 to a depth of 2m-3m.

[0083] Furthermore, in order to enhance the anchoring effect of the anchor rod, the exposed end of the threaded steel anchor rod 5 is not less than 20 cm in length. The exposed end of the threaded steel anchor rod 5 in the present invention is preferably 20 cm. In order to ensure that the anchor rod remains centered in the air, the anchor rod in the present invention is provided with a centering bracket 10 at a certain length. The centering bracket 10 in the present invention is preferably a round steel with a diameter of 8 mm.

[0084] Furthermore, an anchor bar 8 is provided in the threaded steel anchor rod 5 of the present invention, and a guide steel bar 9 with a length of 100 mm is provided at the front end of the anchor bar 8. The guide steel bar 9 of the present invention is composed of two sections not less than The above threaded steel bars are welded; the rear end of the anchor bar 8 is welded with a hanging steel bar 8-1; in the present invention, a steel mesh can be provided in the foam lightweight soil 3 to facilitate the hanging steel bar 8-1 at the rear end of the anchor bar to span the grid of the steel mesh; between the guide steel bar 9 and the tail of the threaded steel anchor rod 5 is a sediment section 5-1, and the length of the sediment section 5-1 can be adjusted according to actual working conditions.

[0085] During actual construction, the threaded steel anchor rod 5 of the present invention is filled with cement mortar, wherein 1:1 grouting is adopted, the water-cement ratio in the cement mortar is 0.4, and the mortar strength is not less than 30 MPa.

[0086] Furthermore, in the present invention, a construction joint should be set according to the mixing requirements and volume before pouring the foam lightweight soil 3. The present invention is set corresponding to the construction joint of the anti-seepage concrete baffle wall 7 and the foundation of the anti-seepage concrete baffle wall 7, and is filled with asphalt wood boards or plywood. The width of the construction joint in the present invention is preferably 1 cm.

[0087] Furthermore, in the present invention, due to the high fluidity of the foamed lightweight soil 3, it is not easy to adjust the longitudinal and transverse slopes of the roadbed during the pouring process. After reaching a certain strength, the pouring elevation is adjusted in sections according to the longitudinal and transverse slopes of the roadbed, and then local adjustments are made on the road surface subbase.

[0088] Furthermore, in the present invention, after the foam lightweight soil 3 is poured, an anti-seepage geotextile is promptly laid after the foam lightweight soil 3 has finally set, and spraying measures are adopted to strengthen the post-maintenance, which can effectively prevent the shrinkage and cracking of the foam lightweight soil 3 before solidification.

[0089] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Those skilled in the art will readily appreciate that various modifications and variations of the present invention are possible. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present invention shall be included within the scope of protection of the present invention.

Claims

1. A method for widening a roadbed in a flooded section, characterized in that: The roadbed filling method comprises: A foundation pit is excavated outside the original roadbed slope of the road to be expanded, and an impermeable concrete baffle wall is installed outside the foundation pit; the impermeable concrete in the impermeable concrete baffle wall is composed of cement, fly ash, coarse aggregate, fine aggregate and admixture; the cement is low hydration heat cement, and the admixture is a low-alkali, low hydration heat waterproofing agent, expansion agent, air entraining agent, water reducing agent or air entraining water reducing agent; the lower end of the impermeable concrete baffle wall is placed a certain distance below the ground line; the lower end of the impermeable concrete baffle wall extends horizontally to both sides by not less than 20 cm, forming a "T"-shaped structure; Laying a cushion layer of recycled aggregate from construction waste at the bottom of the foundation pit; The original roadbed slope of the road to be expanded is stepped to form a step surface; pouring foamed lightweight soil on the construction waste recycled aggregate cushion between the anti-seepage concrete baffle wall and the step surface, and forming a new roadbed after the foamed lightweight soil solidifies, and the new roadbed is connected to the original roadbed through the step surface; Also includes: Before pouring the foamed lightweight soil, a layer of anti-seepage geotextile is laid on the horizontal and vertical surfaces of the step surface of the original roadbed slope and above the cushion layer of recycled aggregate from construction waste; After pouring the foamed lightweight soil, a plurality of oblique anti-floating anchor rods are driven into the foamed lightweight soil at certain intervals along the vertical direction; After the foamed lightweight soil solidifies, a layer of anti-seepage geotextile is also laid on the upper side of the foamed lightweight soil.

2. The method for widening the roadbed of a flooded road section according to claim 1, characterized in that: The thickness of the impermeable concrete baffle wall is not less than 20 cm.

3. The method for widening a roadbed in a flooded section according to claim 1, characterized in that: The width of the step surface is not less than 1m; The horizontal step faces the original roadbed and has a preset slope inwardly inclined, and the slope is not less than 2%.

4. The method for widening a flooded road section according to claim 1, characterized in that: The construction waste recycled aggregate cushion layer is placed on the original foundation, and the construction waste recycled aggregate cushion layer is laid by a layered paving method, with a layer thickness of 20 cm to 30 cm; The overall thickness of the construction waste recycled aggregate cushion layer is 50 cm to 60 cm, and the compaction degree of the construction waste recycled aggregate cushion layer is not less than 93%.

5. The method for widening the roadbed of a flooded road section according to claim 4, characterized in that: The construction waste recycled aggregate cushion layer is composed of one or more of concrete, mortar, stone and brick, and the maximum particle size of the construction waste recycled aggregate cushion layer is not greater than 150mm; The brick content in the construction waste recycled aggregate cushion layer is not more than 20%; The organic matter content is not more than 5%, the light debris content is not more than 0.3%, and the mud content is not more than 5%.

6. The method for widening the roadbed of a flooded road section according to claim 1, characterized in that: The foamed lightweight soil is poured by a layered pouring method; The foamed lightweight soil is prepared by mixing one or more of cement, water, foaming agent, mineral powder and fly ash powder.

7. The method for widening a roadbed in a flooded section according to any one of claims 1 to 6, characterized in that: The anti-seepage geotextile is a geotechnical anti-seepage material which is composited with a non-woven fabric and takes a plastic film as an anti-seepage base material.

8. The method for widening a roadbed in a flooded section according to any one of claims 1 to 6, characterized in that: One end of each anti-floating anchor rod is placed in the foam lightweight soil, and the other end obliquely passes through the corresponding step surface and is placed in the original roadbed.

9. The method for widening a roadbed in a flooded section according to claim 8, characterized in that: The anti-floating anchor rod is a threaded steel anchor rod with a diameter of not less than φ20, and the threaded steel anchor rod is inserted into the original roadbed to a depth of 2m-3m; The exposed end of the threaded steel anchor rod has a length of not less than 20 cm, an anchor bar is arranged inside the threaded steel anchor rod, and a guide steel bar with a length of not less than 100 mm is arranged at the front end of the anchor bar; a sediment section is formed between the guide steel bar and the tail of the threaded steel anchor rod; The cement mortar in the threaded steel anchor rod is grouted in a ratio of 1:1, the water-cement ratio in the cement mortar is 0.4, and the strength of the cement mortar is not less than 30Mpa.

Citation Information

Patent Citations

  • Roadbed structure applied to road widening and construction method

    CN105019326A

  • Reinforced roadbed taking concrete construction waste mixed soil as roadbed filler and construction method thereof

    CN112726310A

  • Pile type anchor rod foam light soil widening structure for expressway in active service

    CN214362621U