A method for manufacturing a shielding groove of a PCB and a PCB
Through the combined technology of double-sided controlled depth drilling and through-hole drilling, the problem of processing shielding grooves with high aspect ratio is solved, the efficiency and quality of electroplating are improved, the risk of tool breakage is reduced, and efficient shielding groove production is achieved.
Patent Information
- Application Number
- CN202111528998.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-14
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-12-14
AI Technical Summary
It is difficult to effectively produce shielding grooves with a high thickness-to-diameter ratio using existing technology, resulting in high processing difficulty and low plating efficiency and quality.
The double-sided controlled depth drilling method is used to obtain two non-connected slots, and through holes are drilled in the connection area to make them conductive, thereby forming a shielding groove, and the liquid is fully exchanged during the electroplating process to improve the plating quality.
It reduces the processing difficulty, avoids the phenomenon of drill breakage, improves the plating efficiency and quality of the shielding groove, and ensures good processing quality.
Smart Images

Figure CN114206007B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of PCB (Printed Circuit Board), and in particular to a method for manufacturing a shielding groove of a PCB and the PCB. Background Art
[0002] With the rapid development of electronic communication technology, the number of PCB design layers and board thickness are getting higher and higher, and the aperture is getting smaller and smaller. The requirements for the anti-interference ability of signal lines in PCB boards are also getting higher and higher. At present, PCB designers have proposed: around key signal lines or key signal vias, slots that penetrate the upper and lower board surfaces are made and copper is plated to form a shielding wall to improve the anti-interference ability.
[0003] The shielding wall can not only reduce signal crosstalk, but also play a role in different levels of conduction and grounding in the PCB. However, due to the small spacing between signal lines and the large board thickness, taking the design of 0.2mm shielding slots on both sides of the high-speed signal line and a board thickness of 6mm-8.0mm as an example, the thickness-to-diameter ratio of the shielding slots will reach 30:1-40:1, which seriously exceeds the current production capacity of the PCB drilling and electroplating process. Therefore, the shielding wall is relatively difficult to produce. Summary of the invention
[0004] The purpose of the present invention is to provide a method for manufacturing a shielding groove of a PCB and a PCB, so as to solve the manufacturing problem of a shielding groove with a high aspect ratio in the prior art.
[0005] To achieve this object, the present invention adopts the following technical solutions:
[0006] A method for manufacturing a shielding slot of a PCB, the manufacturing method comprising:
[0007] Providing a laminated board with signal lines or signal vias;
[0008] On the pressing plate, double-sided controlled depth drilling is performed on the periphery of the signal line or the signal via hole to obtain a first slot hole and a second slot hole that are not connected to each other;
[0009] Drilling a through hole in the connection area between the first slot and the second slot so that the first slot and the second slot are connected to form an initial slot;
[0010] The initial groove is electroplated to form a shielding groove with a metallized inner wall.
[0011] Optionally, compared with the adjacent first slot hole or the adjacent second slot hole, the depth of the signal line is not less than the wiring depth of the signal line.
[0012] Optionally, the length direction of the first slot and the second slot is the same as the routing direction of the signal line.
[0013] Optionally, in the step of performing the double-sided controlled depth drilling, a slotting cutter is used for depth controlled drilling; and in the step of drilling a through hole, a drilling cutter is used for drilling a through hole.
[0014] Optionally, the diameter of the through hole is the same as the width of the first slot hole and the second slot hole.
[0015] Optionally, the width of the first slot, the width of the second slot, and the diameter of the through hole are all no greater than 0.3 mm.
[0016] Optionally, there are multiple through holes, which are arranged at intervals along the length direction of the first slot hole and the second slot hole.
[0017] Optionally, the distance between two adjacent through holes is not less than 0.02 mm.
[0018] A PCB comprises a shielding groove, wherein the shielding groove is manufactured according to the manufacturing method as described above.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] The embodiment of the present invention obtains the main structure of the shielding slot by first obtaining two slots by double-sided controlled depth drilling, and then drilling a through hole at the connection portion between the two slots to make the two slots conductive. Since the double-sided controlled depth drilling method is adopted in the entire processing process instead of the traditional method of directly drilling the slot, a micro-groove cutter with a shorter blade length can be used to perform the slot drilling operation, and the shorter the blade length, the stronger the rigidity, so the problem of easy breakage during the slot drilling process can be effectively solved; at the same time, since the two slots are conductive through the through hole, the liquid medicine can be fully exchanged during the electroplating process, so the electroplating efficiency and electroplating quality of the shielding slot can be effectively improved. Therefore, compared with the prior art, the embodiment of the present invention not only greatly reduces the processing difficulty, but also ensures good processing quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0022] Figure 1 A flow chart of a method for manufacturing a shielding groove of a PCB provided in an embodiment of the present invention.
[0023] Figure 2 A cross-sectional view of a PCB with a shielding groove provided in an embodiment of the present invention.
[0024] Figure 3 A top view of a PCB with a shielding groove provided in an embodiment of the present invention.
[0025] Illustration: first slot 1, second slot 2, through hole 3, signal line 4, shielding layer 5 DETAILED DESCRIPTION
[0026] In order to make the purpose, features and advantages of the present invention more obvious and easy to understand, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the embodiments described below are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] In order to solve the problem that the existing shielding groove is difficult to process due to its high aspect ratio, an embodiment of the present invention provides a method for manufacturing a shielding groove of a PCB, wherein the main structure of the shielding groove is obtained by first obtaining two slot holes by double-sided controlled depth drilling, and then drilling a through hole at the connecting portion between the two to make the two slot holes conductive.
[0028] Since the whole processing process adopts the double-sided controlled depth drilling method instead of the traditional method of directly drilling the groove, a micro-groove cutter with a shorter blade length can be used to perform the groove drilling operation. The shorter the blade length, the stronger the rigidity. Therefore, the problem of breakage in the process of drilling the groove hole can be effectively solved. At the same time, since the two groove holes are connected by a through hole, the chemical solution can be fully exchanged in the electroplating process, so the electroplating efficiency and electroplating quality of the shielding groove can be effectively improved.
[0029] For details, please refer to Figure 1 to Figure 2 The method for manufacturing a shielding groove of a PCB provided by an embodiment of the present invention comprises:
[0030] Step 101: Provide a laminated board with signal lines 4 or signal vias.
[0031] In this step, the laminated board is formed by laminating multiple core boards at high temperature, the signal line 4 is made on the inner core board by a pattern transfer method before laminating, and the signal via can be made by drilling after laminating.
[0032] It should be noted that the embodiment of the present invention does not limit the order of electroplating operations for the signal vias and the subsequently manufactured shielding grooves. The signal vias may be electroplated first and then the shielding grooves. In actual applications, in order to improve processing efficiency, the signal vias and the shielding grooves may also be electroplated at the same time after the main structure of the shielding grooves is processed.
[0033] Step 102 : On the pressed board, double-sided controlled depth drilling is performed on the periphery of the signal line 4 or the signal via hole to obtain a first slot hole 1 and a second slot hole 2 that are not connected to each other.
[0034] For the convenience of description, the embodiment of the present invention refers to the upper and lower opposite plate surfaces of the pressed plate as the first plate surface and the second plate surface respectively. Since it is made by double-sided controlled depth drilling, the slot of the first slot hole 1 is located on the first plate surface of the pressed plate, and the slot of the second slot hole 2 is located on the second plate surface of the pressed plate. The bottom of the first slot hole 1 and the bottom of the second slot hole 2 are connected as a whole.
[0035] The first slot 1 and the second slot 2 will be combined to form a subsequent shielding slot. Since the purpose of the shielding slot is to reduce signal crosstalk and enhance the anti-interference ability of the signal line 4 and the signal via, the first slot 1 and the second slot 2 constituting the shielding slot are designed on the periphery of the signal line 4 or the signal via to achieve a good anti-interference effect.
[0036] At this time, since the first slot hole 1 and the second slot hole 2 are blind slots, and the depth of the blind slots is significantly smaller than the thickness of the pressed plate, a micro-slot cutter with a shorter blade length can be selected for depth controlled drilling. Compared with the micro-slot cutter with a longer blade length, the micro-slot cutter with a shorter blade length has greater rigidity, thereby effectively reducing the risk of tool breakage during the process of drilling the slot holes.
[0037] Step 103 , drilling a through hole 3 in the connection area between the first slot hole 1 and the second slot hole 2 , so that the first slot hole 1 and the second slot hole 2 are connected to form an initial slot.
[0038] In this step, since only the connecting portion of the first slot hole 1 and the second slot hole 2 needs to be drilled, and the depth of the through hole 3 is relatively small, a micro drill with a shorter blade length can be selected to drill the through hole 3. Since the micro drill with a shorter blade length has greater rigidity, the risk of tool breakage can be further effectively reduced during the process of making the shielding slot.
[0039] Step 104: electroplating the initial groove to form a shielding groove with a metallized inner wall.
[0040] In the electroplating process, since the bottoms of the first slot 1 and the second slot 2 are connected through the through hole 3, the electroplating solution can flow effectively and quickly between the two slots, thereby achieving a good electroplating effect.
[0041] It should be noted that in order to ensure that the shielding slot has good anti-interference performance, the depth of the adjacent first slot hole 1 or second slot hole 2 is not less than the wiring depth of the signal line 4 compared with the adjacent first slot hole 1 or second slot hole 2. The length direction of the first slot hole 1 and the second slot hole 2 is the same as the routing direction of the signal line 4.
[0042] The following is an application example: Figure 1 In the cross-sectional view shown, each wiring layer is provided with two groups of differential signal lines in the horizontal direction, and a shielding groove is opened between the left and right groups of signal lines to reduce the signal crosstalk between the left and right groups of differential signal lines; at the same time, multiple groups of differential signal lines are arranged in the vertical direction, and a shielding layer 5 is made between the upper and lower groups of differential signal lines to reduce the signal crosstalk between the upper and lower groups of differential signal lines.
[0043] In fact, the embodiment of the present invention does not limit the specific depths of the first slot 1 and the second slot 2, and can be adjusted according to the wiring position of the signal line 4. Generally speaking, compared with the adjacent first slot 1 or second slot 2, the depth of the adjacent first slot 1 or second slot 2 of the signal line 4 is not less than the wiring depth of the signal line 4. In the case where the upper layer / lower layer adjacent to the signal line 4 is arranged with a shielding layer 5, the depth of the first slot 1 / second slot 2 adjacent to the signal line 4 can be slightly increased to improve the shielding effect.
[0044] To facilitate processing, Figure 3 As shown, the diameter of the through hole 3 is the same as the width of the first slot 1 and the second slot 2, such as a width value not greater than 0.3 mm. To ensure sufficient exchange of the liquid medicine, the number of through holes 3 can be multiple, and they are arranged at intervals along the length direction of the first slot 1 and the second slot 2, and the preferred interval distance is not less than 0.02 mm, so as to avoid tangency or intersection between the holes, and ensure that the drill bit is evenly stressed during the drilling operation and is not easy to break.
[0045] Based on the same inventive concept, an embodiment of the present invention further provides a PCB, including a shielding slot, which is made according to the above-mentioned manufacturing method. Since the shielding slot includes two upper and lower blind slot holes that are connected to each other through the through hole 3 at the bottom of the slot, rather than a traditional through slot structure, the risk of tool breakage can be effectively reduced, which not only greatly reduces the difficulty of processing, but also ensures good processing quality.
[0046] As described above, the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features thereof may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for manufacturing a shielding slot of a PCB, characterized in that: The production method comprises: Providing a laminated board with signal lines or signal vias; On the pressing plate, double-sided controlled depth drilling is performed on the periphery of the signal line or the signal via hole to obtain a first slot hole and a second slot hole that are not connected to each other; Drilling a through hole in the connection area between the first slot hole and the second slot hole so that the first slot hole and the second slot hole are connected to form an initial slot, wherein the number of the through holes is multiple and they are arranged at intervals along the length direction of the first slot hole and the second slot hole, and the distance between two adjacent through holes is not less than 0.02 mm; Electroplating the initial groove to form a shielding groove with metalized inner wall; In the step of performing the double-sided controlled depth drilling, a slot cutter is used for controlled depth drilling; in the step of drilling a through hole, a drill is used for drilling a through hole, the slot cutter is a micro slot cutter, and the drill is a micro drill.
2. The method for manufacturing a shielding groove of a PCB according to claim 1, characterized in that: Compared with the adjacent first slot hole or the adjacent second slot hole, the depth of the signal line is not less than the wiring depth of the signal line.
3. The method for manufacturing a shielding groove of a PCB according to claim 1, characterized in that: The length direction of the first slot and the second slot is the same as the routing direction of the signal line.
4. The method for manufacturing a shielding groove of a PCB according to claim 1, characterized in that: The diameter of the through hole is the same as the width of the first slot hole and the second slot hole.
5. The method for manufacturing a shielding groove of a PCB according to claim 4, characterized in that: The width of the first slot, the width of the second slot, and the diameter of the through hole are all no greater than 0.3 mm.
6. A PCB, comprising a shielding slot, characterized in that: The shielding groove is made according to any one of the manufacturing methods of claims 1 to 5.