A MWT battery back aluminum electrode
By arranging raised portions and broken wire portions on the back aluminum electrode of the MWT battery, the sliding problem caused by the thickness difference between the hole-filling electrode and the back silver electrode is solved, improving the quality rate and service life of the MWT battery, and reducing production costs.
Patent Information
- Application Number
- CN202111469319.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-03
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-12-03
AI Technical Summary
When several MWT batteries are stacked, the hole-filled electrodes can easily scratch the front electrode grid lines, causing grid breakage and affecting the battery's yield rate.
Design a back aluminum electrode for MWT batteries. By setting a protrusion on the back aluminum electrode and the periphery of the hole-filling electrode, and setting a metal mesh layer on the printed screen to form a broken wire part, it can reduce the gap between the hole-filling electrode and the back silver. The thickness difference between the electrodes increases the contact area, reduces the risk of sliding, and improves passability when aluminum slurry penetrates.
It effectively reduces the risk of sliding between silicon wafers, reduces the risk of scratches on the front electrode and broken gates, improves the yield and service life of MWT cells, and reduces production costs.
Smart Images

Figure CN114220875B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of solar cells, and in particular relates to a back aluminum electrode of a MWT cell. Background Art
[0002] Solar cells are semiconductor devices that convert light energy into electrical energy. The lowest possible production cost and the highest possible energy conversion efficiency have always been the goals pursued by the solar cell industry. The negative electrode contact electrode and the positive electrode contact electrode of conventional solar cells are located on the front and back sides of the cell, respectively; the front side of the cell is the light-receiving side, and the coverage of the front metal electrode main grid line and fine grid line will inevitably cause part of the incident sunlight to be reflected by the metal electrode, causing some optical loss. The coverage area of the front metal electrode of an ordinary crystalline silicon solar cell is about 5%, and reducing the front coverage of the metal electrode can directly improve the energy conversion efficiency of the cell.
[0003] At present, crystalline silicon solar energy technology includes heterojunction solar cells (HIT), back electrode contact silicon solar cells (IBC), emitter wrap-through silicon solar cells (EWT), laser groove buried gate cells, inclined evaporated metal contact silicon solar cells (OECO) and metal perforated silicon solar cells (MWT), among which MWT cells are attracting more and more attention due to their high efficiency, small shading area and better appearance. MWT cells are a type of cell in which both the emitter contact electrode and the base contact electrode are located on the back of the cell. In the MWT cell structure, the contact electrode of the emitter located on the light-receiving surface of the cell is guided from the silicon substrate to the back of the cell, and the base contact electrode is located on the back of the cell, so that the current collected by the surface emitter flows out from the back of the cell. Compared with traditional solar cells, the conductive main grid on the front of the cell is replaced by the emitter electrode located on the back, the shading area on the front of the cell is reduced, and the area receiving light is increased, which effectively increases the short-circuit current of the cell, thereby improving the energy conversion efficiency of the cell.
[0004] In the existing technology, there is a thickness difference of more than ten microns between the hole-filling electrode and the back aluminum electrode. As a result, when several MWT batteries are stacked, the hole-filling electrode is easy to scratch the front electrode grid line, or even cause grid breakage, thereby affecting the battery quality rate.
[0005] In view of this, it is necessary to develop a MWT battery back aluminum electrode to solve the above problems. Summary of the invention
[0006] In view of this, an object of the present invention is to provide a MWT battery back aluminum electrode.
[0007] In order to achieve the above object, the technical solution adopted by the present invention is:
[0008] A back aluminum electrode for a MWT battery comprises a crystalline silicon plate and a printed screen, wherein a back aluminum electrode is arranged on the back of the crystalline silicon plate, the back aluminum electrode is electrically connected to a plurality of arrays of back silver electrodes, the crystalline silicon plate array is provided with a plurality of hole-filling electrodes penetrating the crystalline silicon plate, the hole-filling electrodes and the back silver electrodes are arranged at equal intervals, the back aluminum electrode is provided with the printed screen, wherein a protrusion is integrally formed with the back aluminum electrode at a position corresponding to the periphery of the hole-filling electrode, the thickness of the protrusion is equal to the thickness of the hole-filling electrode, and a wire-breaking portion is provided on the printed screen at a position corresponding to the protrusion.
[0009] Furthermore, a metal mesh layer is provided on the printing screen, and the metal mesh layer includes two groups of vertically interwoven metal wires, a hole-filling electrode shielding layer fixedly connected to the metal wires, and a back silver electrode shielding layer fixedly connected to the metal wires. Several arrays of the hole-filling electrode shielding layers are arranged corresponding to the hole-filling electrodes, and several arrays of the back silver electrode shielding layers are arranged corresponding to the back silver electrodes. The hole-filling electrode shielding layer and the back silver electrode shielding layer are arranged at equal intervals, wherein the position of the metal mesh layer corresponding to the raised portion is set to a group of the metal wires in a single direction to form the broken wire portion.
[0010] Furthermore, the acute angle formed by the extension line of the metal wire and the coordinate axis is defined as the inclination angle θ of the metal mesh layer, and the inclination angle θ of the metal mesh layer is 22.5° or 0°.
[0011] Furthermore, the diameter of the hole-filling electrode shielding layer is larger than the diameter of the hole-filling electrode, and the diameter of the back silver electrode shielding layer is smaller than the diameter of the back silver electrode.
[0012] Furthermore, the hole-filling electrode is filled with metal slurry.
[0013] Furthermore, the metal paste is silver paste.
[0014] Furthermore, the thickness of the protrusion is 20 μm-22 μm.
[0015] Furthermore, the thickness of the back aluminum electrode is 13 μm-15 μm.
[0016] Compared with the prior art, the beneficial effects of the present invention are as follows: the present application reduces or eliminates the thickness difference between the hole-filling electrode and the back aluminum electrode by arranging several protrusions opposite to the periphery of the hole-filling electrode, thereby increasing the contact area between several crystalline silicon plates when they need to be stacked, reducing the probability of sliding between silicon wafers, thereby reducing the risk of scratches and broken gates on the front electrodes of the crystalline silicon plates, improving the yield of the MWT battery, and at the same time increasing the overall service life of the MWT battery.
[0017] In addition, the position of the metal mesh layer corresponding to the raised portion in the present application is set as a group of metal wires in a single direction, thereby forming a broken wire portion. Since the broken wire portion is an area formed by removing a group of metal wires in a single direction on the basis of the original metal mesh layer, the area of the mesh is increased. Therefore, when the aluminum paste is infiltrated into the back aluminum electrode, the paste has a larger passing area in the broken wire portion and better passability, thereby forming a raised portion with a larger thickness.
[0018] Secondly, the material of the protrusion is aluminum paste. Compared with the expensive silver paste, the price of aluminum paste is much lower, and the protrusion is locally set, which is practical and economical. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0020] Figure 1 A schematic diagram of the structure of the back of a crystalline silicon plate in a back aluminum electrode of a MWT cell according to one embodiment of the present invention;
[0021] Figure 2 A back aluminum electrode of a MWT battery according to one embodiment of the present invention Figure 1 AA local enlarged schematic diagram;
[0022] Figure 3 A schematic diagram of the structure of a printed screen in a back aluminum electrode of a MWT battery according to one embodiment of the present invention;
[0023] Figure 4 A back aluminum electrode of a MWT battery according to one embodiment of the present invention Figure 3 A partial enlarged schematic diagram of BB;
[0024] Figure 5 A schematic diagram of the structure of a printed screen in a back aluminum electrode of a MWT battery according to another embodiment of the present invention;
[0025] Figure 6 According to another embodiment of the present invention, a back aluminum electrode of a MWT battery is provided. Figure 5 A partial enlarged schematic diagram of CC.
[0026] Reference numerals and component descriptions in the drawings:
[0027] 1-crystalline silicon plate; 11-back aluminum electrode; 111-raised portion; 12-hole-filling electrode; 13-back silver electrode; 2-printed screen; 21-metal mesh layer; 211-broken wire portion; 212-metal wire; 22-hole-filling electrode shielding layer; 23-back silver electrode shielding layer. DETAILED DESCRIPTION
[0028] The technical solution of the present invention will be clearly and completely described below through specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] Example 1
[0030] refer to Figures 1 to 4 A back aluminum electrode for a MWT battery comprises a crystalline silicon plate 1 and a printed screen 2. A back aluminum electrode 11 is arranged on the back of the crystalline silicon plate 1. The back aluminum electrode 11 is electrically connected to a plurality of arrays of back silver electrodes 13. The crystalline silicon plate 1 is provided with a plurality of arrays of hole-filling electrodes 12 penetrating the crystalline silicon plate 1. The hole-filling electrodes 12 and the back silver electrodes 13 are arranged at equal intervals. The back aluminum electrode 11 is provided with a printed screen 2. A protrusion 111 is integrally formed at a position of the back aluminum electrode 11 corresponding to the periphery of the hole-filling electrode 12. The thickness of the protrusion 111 is equal to the thickness of the hole-filling electrode 12. A wire-breaking portion 211 is provided at a position of the printed screen 2 corresponding to the protrusion 111.
[0031] Reference again Figure 1 to Figure 2 The front electrode of the battery is led to the back of the battery through the hole-filling electrode 12, and the current on the back aluminum electrode 11 is collected on the back silver electrode 13. The positive and negative electrodes of the battery are located on the same side, which increases the area of photovoltaic irradiation and improves efficiency. At the same time, a number of protrusions 111 opposite to the periphery of the hole-filling electrode 12 are arranged on the back aluminum electrode 11 to reduce or eliminate the thickness difference between the hole-filling electrode 12, increase the contact area between several crystalline silicon panels 1 when they need to be stacked, reduce the probability of sliding between crystalline silicon panels 1, and thus reduce the risk of scratches and broken gates on the front electrode of the crystalline silicon panel 1, improve the yield of the MWT battery, and at the same time improve the overall service life of the MWT battery.
[0032] It is worth noting that due to production process reasons, the thickness of the protrusion 111 may be slightly less than or slightly greater than the thickness of the hole-filling electrode 12 , but the error is within a controllable allowable range and will not have a substantial impact on the final product effect.
[0033] Reference again Figure 3 to Figure 4A metal mesh layer 21 is arranged on the printing screen 2, and the metal mesh layer 21 includes two groups of vertically interwoven metal wires 212, a hole-filling electrode shielding layer 22 fixedly connected to the metal wires 212, and a back silver electrode shielding layer 23 fixedly connected to the metal wires 212. Several arrays of hole-filling electrode shielding layers 22 are arranged opposite to the hole-filling electrodes 12, and several arrays of back silver electrode shielding layers 23 are arranged opposite to the back silver electrodes 13. The hole-filling electrode shielding layers 22 and the back silver electrode shielding layers 23 are arranged at equal intervals. Specifically, the hole-filling electrode shielding layers 22 and the back silver electrode shielding layers 23 are formed by emulsion covering. The arrangement of the hole-filling electrode shielding layers 22 and the back silver electrode shielding layers 23 can avoid the positions of the hole-filling electrodes 12 and the back silver electrodes 13 when the back aluminum electrode 11 is infiltrated with aluminum paste, thereby avoiding excessive pollution of the two places and ensuring the yield of the product.
[0034] In line with the above, the position of the metal mesh layer 21 corresponding to the raised portion 111 is set as a group of metal wires 212 in a single direction to form a broken wire portion 211. Since the broken wire portion 211 is an area formed by removing a group of metal wires 212 in a single direction on the basis of the original metal mesh layer 21, the area of its mesh holes is increased. When the aluminum paste infiltration process of the back aluminum electrode 11 is carried out, the aluminum paste has a larger passing area in the broken wire portion 211 and better permeability, thereby forming a raised portion 111 with a larger thickness.
[0035] Specifically, the diameter of the hole-filling electrode shielding layer 22 is larger than the diameter of the hole-filling electrode 12 , and the diameter of the back silver electrode shielding layer 23 is smaller than the diameter of the back silver electrode 13 .
[0036] Specifically, the acute angle formed by the extension line of the metal wire 212 and the coordinate axis is defined as the inclination angle θ of the metal mesh layer 21. In this embodiment, the inclination angle θ is set to 22.5°. In addition, other settings of the inclination angle θ are not limited.
[0037] Furthermore, the hole-filling electrode 12 is filled with metal paste, specifically, the metal paste is silver paste. It is worth noting that because silver paste is expensive, the protrusion 111 is provided to reduce the large number of scratches generated when the silicon wafers are stacked. The protrusion 111 is made of aluminum paste, which can greatly reduce the production cost.
[0038] Furthermore, the thickness of the back aluminum electrode 11 is 13μm-15μm, and the thickness of the back aluminum electrode 11 can be adjusted according to actual production specifications and is not limited to the above-mentioned thickness size. Further, the thickness of the protrusion 111 is 20μm-22μm, and the thickness of the protrusion 111 is actually selected according to the thickness of the hole-filling electrode 12 and is not limited to the above-mentioned thickness size.
[0039] Example 2
[0040] refer to Figure 5 to Figure 6 Optionally, the inclination angle of the metal mesh layer 21 is 0°, and the metal mesh layer 21 with this inclination angle can be selected for setting in the actual production process.
[0041] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A MWT battery back aluminum electrode, characterized in that: It comprises a crystalline silicon plate and a printing screen, wherein a back aluminum electrode is arranged on the back of the crystalline silicon plate, wherein the back aluminum electrode is electrically connected to a plurality of arrays of back silver electrodes, wherein the crystalline silicon plate array is provided with a plurality of hole-filling electrodes penetrating the crystalline silicon plate, wherein the hole-filling electrodes and the back silver electrodes are arranged at equal intervals, wherein the back aluminum electrode is printed by the printing screen, wherein a protrusion is integrally formed at a position of the back aluminum electrode corresponding to the periphery of the hole-filling electrode, wherein the thickness of the protrusion is equal to the thickness of a portion of the hole-filling electrode protruding from the surface of the crystalline silicon plate, wherein a metal mesh layer is arranged on the printing screen, wherein the metal mesh layer comprises two groups of vertically interwoven metal wires, wherein the position of the metal mesh layer corresponding to the protrusion is provided as a group of the metal wires in a single direction to form a broken wire portion.
2. A MWT battery back aluminum electrode as claimed in claim 1, characterized in that: The printing screen is provided with a metal mesh layer, the metal mesh layer includes two groups of vertically interwoven metal wires, a hole-filling electrode shielding layer fixedly connected to the metal wires, and a back silver electrode shielding layer fixedly connected to the metal wires. Several arrays of the hole-filling electrode shielding layers are arranged corresponding to the hole-filling electrodes, several arrays of the back silver electrode shielding layers are arranged corresponding to the back silver electrodes, and the hole-filling electrode shielding layer and the back silver electrode shielding layer are arranged at equal intervals, wherein the position of the metal mesh layer corresponding to the protruding portion is arranged as a group of the metal wires in a single direction to form the broken wire portion.
3. A MWT battery back aluminum electrode as claimed in claim 2, characterized in that: The acute angle formed by the extension line of the metal wire and the coordinate axis is defined as the inclination angle θ of the metal mesh layer, and the inclination angle θ of the metal mesh layer is 22.5° or 0°.
4. A MWT battery back aluminum electrode as claimed in claim 2, characterized in that: The diameter of the hole-filling electrode shielding layer is larger than the diameter of the hole-filling electrode, and the diameter of the back silver electrode shielding layer is smaller than the diameter of the back silver electrode.
5. The MWT battery back aluminum electrode according to claim 1, characterized in that: The hole-filling electrode is filled with metal slurry.
6. A MWT battery back aluminum electrode as claimed in claim 5, characterized in that: The metal paste is silver paste.
7. The MWT battery back aluminum electrode according to claim 1, characterized in that: The thickness of the protrusion is 20 μm-22 μm.
8. The MWT battery back aluminum electrode according to claim 1, characterized in that: The thickness of the back aluminum electrode is 13 μm-15 μm.