A preparation process and structure of an MTM anti-fuse unit based on ONO medium
Through the MTM anti-fuse unit preparation process based on ONO medium, the traditional MTM anti-fuse memory has been solved, with small capacity, large chip area and high programming power consumption, and a high integration and low power consumption anti-fuse unit is realized , supports mass memory and FPGA applications, and is compatible with standard CMOS processes.
Patent Information
- Application Number
- CN202111644021.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-29
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-12-29
AI Technical Summary
Traditional MTM anti-fuse memory has problems such as small capacity, large chip area and high programming power consumption.
Using the MTM type anti-fuse unit preparation process based on ONO medium, including the production of MOS device levels, metal wiring, anti-fuse bottom metal and bottom metal barrier layers on the substrate, and the MTM anti-fuse ONO stacked medium is carried out. The deposit, photolithography and corrosion of the top metal barrier layer are formed to form an island-shaped anti-fuse structure, and the inter-metal dielectric and anti-fuse top metal are deposited to form upper and lower electrodes.
It significantly reduces the programming current of the anti-fuse unit, improves integration, supports high-reliable large-capacity anti-fuse memory at megabit level and tens of millions of gate-level anti-fuse FPGA, reduces leakage and static power consumption, and is compatible with standard CMOS processes.
Smart Images

Figure CN114284217B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of microelectronic process manufacturing, and in particular to a preparation process and structure of an MTM type anti-fuse unit based on an ONO medium. Background Art
[0002] As an OTP (One Time Programming) device, MTM anti-fuse units are usually used in circuit products such as FPGA and PROM. The anti-fuse units in the circuit are programmed according to actual needs to realize the logic function or storage function of the circuit. This type of MTM anti-fuse circuit has the characteristics of excellent radiation resistance, strong confidentiality, and good flexibility, and has broad application prospects in the aerospace and military fields.
[0003] like Figure 1 As shown, the MTM anti-fuse unit structure is located between two layers of metal wiring in the circuit, and is composed of an anti-fuse dielectric layer and dielectric barrier layers on the upper and lower sides and upper and lower metal electrodes of the anti-fuse. Its working principle is: during programming, a preset programming voltage and programming current are applied between the upper and lower electrodes of the anti-fuse, so that the anti-fuse dielectric film is melted through in a relatively short time (milliseconds), forming a conductive channel with good electrical properties and reliability. The establishment of the conductive channel means the completion of data information burning.
[0004] Traditional MTM anti-fuse media are made of amorphous silicon. The size of the resistance after programming is controlled by the programming current. Generally, after the anti-fuse unit is programmed under a programming current of 10mA, the anti-fuse resistance changes from more than 200M ohms before programming to a resistance of about 70 ohms. Since the resistance of the MTM anti-fuse unit of amorphous silicon media is controlled by the programming current, the anti-fuse programming current of the memory unit cannot be less than 5mA, otherwise the long-term reliability of the anti-fuse resistance after programming will be affected. When making large-capacity (>1M bit) anti-fuse memory, the area of the programming current limiting tube becomes the key. Therefore, seeking an anti-fuse medium that can be programmed at a small current (1mA) and has a programming resistance of less than 100 ohms becomes the key to making large-capacity anti-fuse memory. Summary of the invention
[0005] The object of the present invention is to provide a preparation process and structure of an MTM type anti-fuse unit based on ONO medium, so as to solve the problems of small capacity, large chip area and high programming power consumption of traditional MTM anti-fuse memory.
[0006] In order to solve the above technical problems, the present invention provides a preparation process of an MTM type anti-fuse unit based on ONO medium, comprising:
[0007] Providing a substrate, and sequentially manufacturing a MOS device layer and an intermediate metal wiring, an anti-fuse bottom metal and a bottom metal barrier layer on the surface thereof;
[0008] Deposition of MTM anti-fuse ONO stack dielectric;
[0009] Depositing a top metal barrier layer;
[0010] Photolithography and etching are performed on the ONO stacked dielectric and the top metal barrier layer to form an island anti-fuse structure, and photolithography and etching are performed on the bottom metal of the anti-fuse to form a lower electrode of the anti-fuse;
[0011] Depositing an intermetallic dielectric IMD, wherein the intermetallic dielectric IMD covers the ONO stacked dielectric and the top metal barrier layer;
[0012] Perform photolithography of anti-fuse vias, deposition of vias and CMP planarization;
[0013] Deposit the anti-fuse top metal, and perform photolithography and etching to form the anti-fuse top electrode.
[0014] Optionally, the deposition of the MTM antifuse ONO stack dielectric includes:
[0015] Depositing the first layer SiO2 of the MTM anti-fuse ONO stack dielectric on the surface of the bottom metal barrier layer;
[0016] Depositing a second SiN layer of the MTM antifuse ONO laminate dielectric on the surface of the first SiO2 layer;
[0017] The third dielectric layer SiO2 of the MTM anti-fuse ONO stack dielectric is deposited on the surface of the second SiN layer.
[0018] Optionally, the thickness of the first SiO layer is 1-3 nm, the thickness of the second SiN layer is 5-9 nm, and the thickness of the third dielectric SiO2 layer is 1-3 nm; all are formed by CVD process.
[0019] Optionally, the substrate is a bulk silicon epitaxial material or an SOI material substrate, and the thickness is the SEMI standard thickness.
[0020] Optionally, the bottom metal barrier layer is made of TiN or TiW, has a thickness of 10 to 200 nm, and is formed by deposition using a CVD process.
[0021] Optionally, the top metal barrier layer is made of TiN or TiW, has a thickness of 50 to 200 nm, and is formed by deposition using a PVD process.
[0022] Optionally, the material component of the intermetallic dielectric IMD is SiO2.
[0023] Optionally, the material of the top metal of the antifuse is AlxSiyCuz or Cu, and the thickness is 500-1200nm.
[0024] The present invention also provides an MTM type anti-fuse unit structure based on ONO medium, which is prepared according to the preparation process of the MTM type anti-fuse unit based on ONO medium.
[0025] The preparation process and structure of the MTM anti-fuse unit based on ONO medium provided by the present invention have the following beneficial effects:
[0026] (1) It makes it possible to advance the MTM antifuse process from 0.15um to 65nm or even more advanced process technology;
[0027] (2) Significantly reduce the programming current of the anti-fuse unit and improve the integration of the anti-fuse unit, which can support the programmable unit of high-reliability and large-capacity anti-fuse PROM memory above the megabit level and anti-fuse FPGA of tens of millions of gates;
[0028] (3) Compared with the conventional MTM anti-fuse unit, the anti-fuse unit of the present invention has a leakage reduction of 1 to 2 orders of magnitude, which can significantly reduce the static power consumption of the circuit;
[0029] (4) It has natural total dose and single particle resistance capabilities, is fully compatible with standard CMOS processes, and has strong operability. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of the MTM type anti-fuse structure;
[0031] Figure 2 It is a schematic diagram of the process flow of preparing an MTM type anti-fuse unit based on ONO medium provided by the present invention;
[0032] Figure 3 It is a schematic diagram of sequentially manufacturing an intermediate metal wiring, an anti-fuse bottom metal and a bottom metal barrier layer on a substrate surface;
[0033] Figure 4 is a schematic diagram of depositing a first layer of SiO2 on the surface of the bottom metal barrier layer;
[0034] Figure 5 It is a schematic diagram of depositing a second layer of SiN on the surface of the first layer of SiO2;
[0035] Figure 6 It is a schematic diagram of depositing a third dielectric layer SiO2 on the surface of the second SiN layer;
[0036] Figure 7 is a schematic diagram of depositing a top metal barrier layer;
[0037] Figure 8 It is a schematic diagram of performing photolithography and etching on the ONO stacked dielectric and the top metal barrier layer and performing photolithography and etching on the bottom metal of the anti-fuse to form the lower electrode of the anti-fuse;
[0038] Fig. 9 It is a schematic diagram of depositing an intermetallic dielectric IMD;
[0039] Fig.10 It is a schematic diagram of performing photolithography of anti-fuse vias, deposition of vias and CMP planarization;
[0040] Fig.11 It is a schematic diagram of depositing the top metal of the antifuse and performing photolithography and etching to form the top electrode of the antifuse. DETAILED DESCRIPTION
[0041] The following is a further detailed description of the preparation process and structure of an MTM type anti-fuse unit based on ONO medium proposed by the present invention in combination with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become clearer according to the following description and claims. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.
[0042] The present invention provides a preparation process of an MTM type anti-fuse unit based on an ONO medium, and the process is as follows: Figure 2 As shown, the following steps are included:
[0043] Step S21, providing a substrate, and sequentially manufacturing a MOS device layer and an intermediate metal wiring, an anti-fuse bottom metal and a bottom metal barrier layer on the surface thereof;
[0044] Step S22, depositing the MTM anti-fuse ONO stack dielectric;
[0045] Step S23, depositing a top metal barrier layer;
[0046] Step S24, photolithography and etching are performed on the ONO laminated dielectric and the top metal barrier layer to form an island antifuse structure; and photolithography and etching are performed on the bottom metal of the antifuse to form a lower electrode of the antifuse;
[0047] Step S25, depositing an intermetallic dielectric IMD, wherein the intermetallic dielectric IMD covers the ONO laminated dielectric and the top metal barrier layer;
[0048] Step S26, performing photolithography of the anti-fuse through hole, deposition of the through hole Via and CMP planarization;
[0049] Step S27, depositing the anti-fuse top metal, and performing photolithography and etching to form the anti-fuse top electrode.
[0050] Specifically, Figure 3 As shown, a substrate 1 is first provided, and an intermediate metal wiring 2, an anti-fuse bottom metal 3 and a bottom metal barrier layer 4 are sequentially formed on the surface thereof; wherein the substrate 1 is a bulk silicon epitaxial material or an SOI material substrate, and the thickness is the SEMI standard thickness; the bottom metal barrier layer 4 is made of TiN or TiW, and the thickness is 10 to 200 nm, and is formed by deposition using a CVD process;
[0051] Next, the MTM antifuse ONO stack dielectric is deposited using a CVD process, including the following steps:
[0052] like Figure 4 As shown, the first layer SiO25 of the MTM anti-fuse ONO laminated dielectric is deposited on the surface of the bottom metal barrier layer 4, and the thickness of the first layer SiO5 is 1-3nm;
[0053] like Figure 5 As shown, a second layer SiN 6 of the MTM anti-fuse ONO laminated dielectric is deposited on the surface of the first layer SiO 25, and the thickness of the second layer SiN 6 is 5 to 9 nm;
[0054] like Figure 6 As shown, the third dielectric layer SiO27 of the MTM anti-fuse ONO stack dielectric is deposited on the surface of the second SiN 6 layer; the thickness of the third dielectric layer SiO27 is 1 to 3 nm.
[0055] Then the top metal barrier layer 8 is deposited, as shown in FIG. Figure 7 As shown, the material of the top metal barrier layer 8 is TiN, TiW, with a thickness of 50 to 200 nm, and is formed by PVD deposition process;
[0056] like Figure 8 As shown, the ONO laminated dielectric (including the first layer SiO25, the second layer SiN6 and the third layer SiO27) and the top metal barrier layer 8 are photolithographically processed and etched to form an island anti-fuse structure 9; the anti-fuse bottom metal 3 is photolithographically processed and etched to form an anti-fuse bottom electrode;
[0057] like Fig. 9 As shown, a metal interlayer dielectric IMD 10 is deposited, and its material component is SiO2; the metal interlayer dielectric IMD 10 covers the ONO stacked dielectric and the top metal barrier layer 8;
[0058] like Fig.10 As shown, the anti-fuse through hole 11 is photolithographically processed, the through hole Via is deposited, and CMP planarization is performed;
[0059] Finally, the anti-fuse top metal 12 is deposited, and then photolithography and etching are performed to form the anti-fuse top electrode, such as Fig.11 As shown; the material of the anti-fuse top metal 12 is AlxSiyCuz or Cu, with a thickness of 500 to 1200nm.
[0060] The present invention adopts a method of using a novel ONO dielectric material, significantly reduces the MTM antifuse programming current, and is compatible with standard CMOS processes; innovatively proposes to move the traditional ONO antifuse from between the polycrystalline and active regions to between the back-end metal wiring of the integrated circuit, combining the advantages of the small programming current of the ONO antifuse and the advantage of the MTM antifuse without sacrificing the silicon wafer area, thereby improving the integration of the antifuse; and adopts a CVD process to prepare back-end process ultra-thin SixOy, SixNy and other dielectrics (with a thickness of less than 10 nm) as the dielectric layer of the MTM antifuse.
[0061] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.
Claims
1. A preparation process of an MTM anti-fuse unit based on ONO medium, characterized in that: include: Providing a substrate, and sequentially manufacturing a MOS device layer and an intermediate metal wiring, an anti-fuse bottom metal and a bottom metal barrier layer on the surface thereof; Deposition of MTM anti-fuse ONO stack dielectric; Deposition of a top metal barrier layer; Photolithography and etching are performed on the ONO stacked dielectric and the top metal barrier layer to form an island anti-fuse structure, and photolithography and etching are performed on the bottom metal of the anti-fuse to form a lower electrode of the anti-fuse; Depositing an intermetallic dielectric IMD, wherein the intermetallic dielectric IMD covers the ONO stacked dielectric and the top metal barrier layer; Perform photolithography of anti-fuse vias, deposition of vias and CMP planarization; Deposit the anti-fuse top metal, and perform photolithography and etching to form the anti-fuse top electrode.
2. The preparation process of the MTM anti-fuse unit based on ONO medium according to claim 1, characterized in that: The deposition of MTM antifuse ONO stack dielectric includes: Depositing the first layer SiO2 of the MTM anti-fuse ONO stack dielectric on the surface of the bottom metal barrier layer; Depositing a second SiN layer of the MTM antifuse ONO laminate dielectric on the surface of the first SiO2 layer; The third dielectric layer SiO2 of the MTM anti-fuse ONO stack dielectric is deposited on the surface of the second SiN layer.
3. The preparation process of the MTM type anti-fuse unit based on ONO medium as claimed in claim 2, characterized in that: The thickness of the first SiO2 layer is 1-3 nm, the thickness of the second SiN layer is 5-9 nm, and the thickness of the third dielectric SiO2 layer is 1-3 nm; all are formed by CVD process.
4. The preparation process of the MTM anti-fuse unit based on ONO medium according to claim 1, characterized in that: The substrate is a bulk silicon epitaxial material or an SOI material substrate, and the thickness is in accordance with the SEMI standard thickness.
5. The preparation process of the MTM anti-fuse unit based on ONO medium according to claim 1, characterized in that: The bottom metal barrier layer is made of TiN or TiW, has a thickness of 10-200 nm, and is formed by deposition using a CVD process.
6. The preparation process of the MTM anti-fuse unit based on ONO medium according to claim 1, characterized in that: The material of the top metal barrier layer is TiN, TiW, with a thickness of 50-200nm, and is formed by deposition using a PVD process.
7. The preparation process of the MTM anti-fuse unit based on ONO medium according to claim 1, characterized in that: The material component of the intermetallic dielectric IMD is SiO2.
8. The preparation process of the MTM anti-fuse unit based on ONO medium according to claim 1, characterized in that: The material of the top metal of the anti-fuse is AlxSiyCuz or Cu, and the thickness is 500-1200nm.
9. An MTM anti-fuse unit structure based on ONO medium, characterized in that: The method is prepared according to the preparation process of the MTM type anti-fuse unit based on ONO medium according to any one of claims 1 to 8.