A high-temperature compression molding device and molding method for polyetherketoneketone skull repair piece

Through polyetherketoneketone materials and high-temperature compression molding technology, the stress shielding and high cost problems of existing skull repair materials have been solved, and the efficient molding of personalized skull repair patches has been achieved, improving the success rate of surgery and the aesthetics of patient recovery.

CN114347434BActive Publication Date: 2024-10-15ZHEJIANG UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210052987.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-18
Publication Date
2024-10-15
Estimated Expiration
2042-01-18

AI Technical Summary

Technical Problem

Existing skull repair materials such as titanium mesh and PEEK have problems with stress shielding, material waste and high cost, making it difficult to meet personalized shape requirements and economical production.

Method used

The polyetherketoneketone material is combined with a high-temperature compression molding device, and a personalized skull patch is designed through mirror symmetry and surface fitting methods, and is molded using a hot air box and a compression molding machine to reduce material waste and costs.

Benefits of technology

It improves the mechanical properties and personalized adaptability of the skull repair patch, reduces material waste and surgical costs, and enhances the success rate of surgery and the aesthetics of patient recovery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114347434B_ABST
    Figure CN114347434B_ABST
Patent Text Reader

Abstract

A high-temperature compression molding device for a polyetherketoneketone skull patch comprises a compression molding machine and a hot air box, wherein a mold frame corresponding to the compression molding machine is arranged in the hot air box; the mold frame comprises an upper mold plate, a guide column and a lower mold plate connected to each other, wherein the lower mold plate is fixedly connected to the bottom of the hot air box, the upper mold plate is connected to the compression molding machine, and the upper mold plate is overhead arranged under the action of the compression molding machine; the guide column is vertically arranged, and the upper mold plate is slidably connected to the guide column; a concave mold is arranged on the lower mold plate, and a convex mold corresponding to the concave mold is arranged on the upper mold plate; a temperature monitoring module is arranged in the hot air box; compared with the prior art, the defective area of ​​the skull is reconstructed according to the method of contralateral mirror image and surface fitting, and a personalized skull patch is designed. Compared with the implant of a standard titanium mesh that is bent and formed during surgery, the personalized patch is more conducive to the patient's restoration of the original outer shape after surgery and is more beautiful.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of skull repair, and in particular to a high-temperature compression molding device and a molding method for a polyetherketoneketone skull repair piece. Background Art

[0002] Cranioplasty is a common operation in brain surgery. Skull injuries and developmental deformities can cause great harm to patients, seriously affecting their appearance and normal social activities. Due to the huge individual differences, skull implants have strict requirements on biocompatibility and mechanical properties, as well as a high demand for personalized shapes.

[0003] Traditional skull defect repair mainly uses titanium mesh patches. Titanium mesh has the advantages of good biocompatibility, easy processing, excellent mechanical properties and relatively low price. Titanium mesh as a repair material has always been the preferred method in clinical surgery. However, titanium mesh implants also have disadvantages. Its elastic modulus is much higher than that of bones, which can easily cause stress shielding, which may cause bone resorption and loosening, causing the implant to fall off; titanium mesh is a metal material, and large-area titanium patches have serious artifact problems in medical images, which interferes with postoperative diagnosis. In addition to titanium mesh implants, autologous bone, allogeneic bone, polymethyl methacrylate, hydroxyapatite and other materials have also been used as implant materials for skull repair, but these materials also have problems such as limited tissue sources, difficulty in plasticity, low strength, immune rejection after implantation, and high infection rate. Therefore, they have not become mainstream skull repair materials.

[0004] Due to the defects of existing materials, people have turned their attention to a new type of polymer material, polyetheretherketone, which has good biocompatibility; good mechanical properties, elastic modulus similar to human bones, no stress shielding problem; no artifact problems in medical imaging; stable chemical properties and many other advantages. Therefore, PEEK is increasingly used in the medical field. However, the melting point of PEEK is as high as 343°C, so it can only be processed by CNC machining or additive manufacturing. However, due to the large curvature of the skull shape, the strength of the curved surface formed by additive manufacturing is low; the use of CNC machining to form skull repair pieces will cause a lot of material waste, and the price of PEEK materials is very expensive, so the manufacturing cost is extremely high. At present, the use of imported PEEK skull repair pieces for defective skull repair often exceeds 100,000 yuan in material costs. The high cost of use has hindered its development in the medical field.

[0005] Polyetherketoneketone and polyetheretherketone are both polyaryletherketone materials. Studies have shown that compared with PEEK, PEKK has better mechanical properties, biological properties and chemical stability, and it is an ideal material for repairing skull defects. Summary of the invention

[0006] The present invention aims to overcome the defects in the above-mentioned prior art and provide a high-temperature compression molding device and molding method for a polyetherketoneketone skull patch which can ensure the strength of the patch, reduce material loss and reduce the use cost.

[0007] In order to achieve the above-mentioned invention objectives, the present invention adopts the following technical scheme: a high-temperature compression molding device for a polyetherketoneketone skull patch, comprising a compression molding machine and a hot air box, wherein a mold frame corresponding to the compression molding machine is arranged in the hot air box; the mold frame comprises an upper mold plate, a guide column and a lower mold plate connected to each other, the lower mold plate is fixedly connected to the bottom of the hot air box, the upper mold plate is connected to the compression molding machine, and the upper mold plate is overhead under the action of the compression molding machine; the guide column is vertically arranged, and the upper mold plate is slidably connected to the guide column; a concave mold is arranged on the lower mold plate, and a convex mold corresponding to the concave mold is arranged on the upper mold plate; a temperature monitoring module is arranged in the hot air box.

[0008] As a preferred solution of the present invention, the compression molding machine includes a compression head and a bottom plate, the hot air box is placed on the bottom plate, and the compression head is connected to the upper mold plate.

[0009] As a preferred solution of the present invention, four guide columns are provided between the upper template and the lower template, the upper template and the lower template have consistent sizes, the guide columns are connected to the corners of the upper template and the lower template, and the bottom of the guide column has an interference fit with the lower template, and the upper template has a clearance fit with the guide column.

[0010] As a preferred solution of the present invention, a mounting hole corresponding to the concave mold is formed on the lower mold plate, and similarly, a mounting hole corresponding to the convex mold is also formed on the upper mold plate.

[0011] As a preferred solution of the present invention, hot air outlets are formed on both sides of the hot air box, and a flow channel connected to the hot air outlet is provided in the hot air box. The flow channel is arranged around the interior of the hot air box, and air outlets are formed on the flow channel at equal intervals.

[0012] As a preferred solution of the present invention, heat dissipation openings which are arranged opposite to each other are formed on both sides of the hot air box, and the heat dissipation openings are located below the hot air openings.

[0013] As a preferred solution of the present invention, the temperature monitoring module includes a temperature measuring contact, a thermocouple module, a single-chip microcomputer, a computer and a thermal imager. The thermal imager is placed directly in front of the incubator, the temperature measuring contact is installed on the die or the punch, and the temperature measuring contact, the thermocouple module, the single-chip microcomputer and the computer are electrically connected in sequence.

[0014] A molding method of a polyetherketoneketone skull repair piece high-temperature compression molding device comprises the following steps:

[0015] Step A: Based on the contour of the defective skull, the skull is reconstructed and the three-dimensional model of the patch for repairing the defect is extracted based on the mirror symmetry and surface fitting method. The outer surface of the patch is extracted separately and the mesh is smoothed.

[0016] Step B: the outer surface of the patch model is stretched downward in the 3D modeling software to form a concave mold, and then the outer surface of the patch model is reduced inward and stretched upward to form a convex mold, and a mold frame corresponding to the concave mold and the convex mold is designed;

[0017] Step C: inputting the three-dimensional models of the concave mold and the convex mold into the control computer of the 3D printer for printing. After printing, the printed concave mold and the convex mold are separated from the substrate by wire cutting to remove the support, and then grinding and polishing are performed;

[0018] Step D: Before die molding, assemble the die press, hot air box and die frame, install the concave die and the convex die on the die frame, put the die frame into the hot air box, place the hot air box at a suitable position on the bottom plate of the die press, and fix the upper die plate with the die head of the die press in the hot air box, and fix the lower die plate with the bottom plate of the hot air box, thus completing the die preparation;

[0019] Step E: Place the PEKK plate on the die, place two hot air guns at the hot air inlets on both sides of the hot air box, adjust the power of the hot air gun according to the required molding temperature, and blow hot air into the hot air box through the flow channel to make the ambient temperature of the hot air box reach the required molding temperature;

[0020] Step F: When the temperature in the hot air box reaches the target molding temperature, the PEKK skull patch is molded by controlling the molding program on the molding machine panel. After the molding is completed, the hot air box is cooled, the molded skull patch is taken out, and the edges are trimmed, and a defective skull patch is formed.

[0021] As a preferred solution of the present invention, in the step F, during the die pressing process, a temperature measuring contact is pre-installed on the die or the punch, the temperature measuring contact is guided to the outside of the hot air box, and the voltage signal is converted into an analog quantity recognizable by the PLC through a thermocouple module, and then the analog quantity is converted into temperature data through an analog data conversion program using a single-chip microcomputer, and finally the temperature data is displayed in real time on the computer through the serial port.

[0022] As a preferred solution of the present invention, during the molding process in step F, a thermal imager is placed in front of the incubator to monitor the temperature of the entire incubator, thereby reflecting in real time whether the overall temperature field in the incubator is uniform.

[0023] Compared with the prior art, the present invention has the following beneficial effects:

[0024] 1. For the skull defect area, the defect area is reconstructed according to the contralateral mirror image and surface fitting method, and a personalized skull patch is designed. Compared with the standard titanium mesh implant that is bent and formed during the operation, the personalized patch is more conducive to the patient's restoration of the original appearance after surgery, and is more beautiful;

[0025] 2. In order to solve the stress shielding problem of existing titanium mesh implants, the skull patch is made of polyetherketoneketone material which is more suitable for implantation, which is more conducive to improving the success rate of surgery;

[0026] 3. In view of the current difficulty in molding polyaryletherketone materials, a high-temperature compression molding method is designed. On the basis of ensuring the mechanical properties of the skull patch after molding, it greatly reduces material waste and reduces the surgical costs for patients. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 It is a schematic diagram of the structure of the present invention;

[0028] Figure 2 It is a schematic diagram of the structure of the hot air box;

[0029] Figure 3 It is a structural diagram of the mold frame;

[0030] Figure 4 It is a schematic diagram of the design of the patch;

[0031] Figure markings: molding machine 1, base plate 1-1, pressing head 1-2, hot air box 2, mold frame 3, lower mold plate 3-1, upper mold plate 3-2, guide column 3-3, mounting hole 3-4, defective skull 4, repair piece 5, punch 6, die 7. DETAILED DESCRIPTION

[0032] The embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0033] like Figure 1-4 As shown, a high-temperature compression molding device for a polyetherketoneketone skull patch comprises a compression molding machine 1 and a hot air box 2, wherein a mold frame 3 corresponding to the compression molding machine 1 is arranged in the hot air box 2; the mold frame 3 comprises an upper mold plate 3-2, a guide column 3-3 and a lower mold plate 3-1 connected to each other, the lower mold plate 3-1 is fixedly connected to the bottom of the hot air box 2, the upper mold plate 3-2 is connected to the compression molding machine 1, and the upper mold plate 3-2 is overheadly arranged under the action of the compression molding machine 1; the guide column 3-3 is vertically arranged, and the upper mold plate 3-2 is slidably connected to the guide column 3-3; a concave mold 7 is arranged on the lower mold plate 3-1, and a convex mold 6 corresponding to the concave mold 7 is arranged on the upper mold plate 3-2; a temperature monitoring module is arranged in the hot air box 2.

[0034] The molding machine 1 comprises a pressing head 1-2 and a bottom plate 1-1, a hot air box 2 is placed on the bottom plate 1-1, and the pressing head 1-2 is connected to an upper mold plate 3-2.

[0035] Four guide columns 3-3 are arranged between the upper template 3-2 and the lower template 3-1. The upper template 3-2 and the lower template 3-1 have the same size. The guide columns 3-3 are connected to the corners of the upper template 3-2 and the lower template 3-1, and the bottom of the guide columns 3-3 has an interference fit with the lower template 3-1, and the upper template 3-2 has a clearance fit with the guide columns 3-3.

[0036] The upper template 3-2 and the lower template 3-1 are both horizontally arranged rectangular structures. The bottom of the guide column 3-3 is fixedly connected to the lower template 3-1 by interference fit. The upper template 3-2 and the guide column 3-3 are slidingly connected by clearance fit. The guide column 3-3 plays a guiding role for the upper template 3-2. Through holes corresponding to the guide columns 3-3 are formed on the upper template 3-2 and the lower template 3-1.

[0037] The lower template 3 - 1 is formed with a mounting hole 3 - 4 corresponding to the concave mold 7 , and similarly, the upper template 3 - 2 is also formed with a mounting hole 3 - 4 corresponding to the convex mold 6 .

[0038] Hot air ports 2-1 are formed on both sides of the hot air box 2, and a flow channel 2-2 connected to the hot air port 2-1 is provided inside the hot air box 2. The flow channel 2-2 surrounds the inside of the hot air box 2, and the flow channel 2-2 is formed with air outlets 2-3 arranged at equal intervals, which heat the concave mold 7, the convex mold 6 and the polyetherketoneketone material to make the temperature field more uniform. In order to reduce the heat conduction between the hot air box 2 and the outside world, a composite silicate insulation material is used on the surface of the hot air box 2 for insulation.

[0039] The hot air box 2 is also provided with heat dissipation openings 2-4 which are arranged opposite to each other on both sides. The heat dissipation openings 2-4 are located below the hot air opening 2-1.

[0040] The design of the hot air box 2 needs to ensure the placement of the pressing head 1-2 of the molding machine 1 in terms of size, and needs to take into account the heating efficiency and the uniformity of the thermal field in the hot air box 2.

[0041] The temperature monitoring module includes a temperature measuring contact, a thermocouple module, a single-chip microcomputer, a computer and a thermal imager. The thermal imager is placed in front of the incubator. The temperature measuring contact is installed on the die 7 or the punch 6. The temperature measuring contact, the thermocouple module, the single-chip microcomputer and the computer are electrically connected in sequence.

[0042] A molding method of a polyetherketoneketone skull repair piece high-temperature compression molding device comprises the following steps:

[0043] Step A: Based on the contour of the defective skull 4, the skull is reconstructed and the three-dimensional model of the patch 5 for repairing the defect is extracted based on the mirror symmetry and surface fitting method. The outer surface of the patch 5 is extracted separately and the mesh is smoothed.

[0044] Step B: The outer surface of the patch 5 model is stretched downward in the three-dimensional modeling software to form a concave mold 7, and then the outer surface of the patch 5 model is reduced inward and stretched upward to form a convex mold 6, and a mold frame 3 corresponding to the concave mold 7 and the convex mold 6 is designed.

[0045] Specifically, the outer surface of the repair piece 5 model is stretched downward by 35 mm in the three-dimensional modeling software to form a concave mold 7, and then the outer surface is reduced inward by 2 mm and stretched upward by 35 mm to form a convex mold 6.

[0046] Step C: input the three-dimensional models of the concave mold 7 and the convex mold 6 into the control computer of the 3D printer for printing. After printing, the printed concave mold 7 and the convex mold 6 are separated from the substrate by wire cutting to remove the support, and then ground and polished;

[0047] Specifically, the three-dimensional models of the concave mold 7 and the convex mold 6 are input into the control computer of the SLS metal melting 3D printer, and SLS printing is performed using 316L stainless steel powder.

[0048] Step D: Before die molding, assemble the die press 1, the hot air box 2 and the die frame 3, install the concave die 7 and the convex die 6 on the die frame 3, put the die frame 3 into the hot air box 2, place the hot air box 2 at a suitable position of the bottom plate 1-1 of the die press 1, and fix the upper die plate 3-2 with the pressing head 1-2 of the die press 1 in the hot air box 2, and fix the lower die plate 3-1 with the bottom plate 1-1 of the hot air box 2, thus completing the die preparation;

[0049] Step E: Place the PEKK plate on the concave mold 7, place two hot air guns at the hot air inlets on both sides of the hot air box 2, adjust the power of the hot air guns according to the required molding temperature, and blow hot air into the hot air box 2 through the flow channel 2-2, so that the ambient temperature of the hot air box 2 reaches the required molding temperature;

[0050] Step F: When the temperature in the hot air box 2 reaches the target molding temperature, the molding program on the panel of the molding machine 1 is controlled to perform molding of the PEKK skull patch 5. After the molding is completed and the hot air box 2 is cooled, the molded skull patch 5 is taken out and the edges are trimmed. The molding of a patch 5 for a defective skull 4 is completed.

[0051] During the die pressing process, a temperature measuring contact is pre-installed on the die 7 or the punch 6, and the temperature measuring contact is guided to the outside of the hot air box 2. The voltage signal is converted into an analog quantity that can be recognized by the PLC through the thermocouple module, and then the analog quantity is converted into temperature data through the analog data conversion program by the single-chip microcomputer, and finally the temperature data is displayed in real time on the computer through the serial port.

[0052] During the molding process, a thermal imager is placed in front of the incubator to monitor the temperature of the entire incubator, reflecting in real time whether the overall temperature field in the incubator is uniform.

[0053] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention; therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

[0054] Although the following terms are used more frequently in this article: die press 1, base plate 1-1, ram 1-2, hot air box 2, mold frame 3, lower mold plate 3-1, upper mold plate 3-2, guide column 3-3, mounting hole 3-4, defective skull 4, patch 5, male mold 6, female mold 7, etc., the possibility of using other terms is not excluded. These terms are used only to more conveniently describe and explain the essence of the present invention; interpreting them as any additional limitation is contrary to the spirit of the present invention.

Claims

1. A molding method of a polyetherketoneketone skull repair piece high temperature compression molding device, characterized in that: The invention comprises a molding machine (1) and a hot air box (2), wherein a mold frame (3) corresponding to the molding machine (1) is arranged in the hot air box (2); the mold frame (3) comprises an upper mold plate (3-2), a guide column (3-3) and a lower mold plate (3-1) connected to each other, wherein the lower mold plate (3-1) is fixedly connected to the bottom of the hot air box (2), the upper mold plate (3-2) is connected to the molding machine (1), and the upper mold plate (3-2) is arranged in an overhead manner under the action of the molding machine (1); the guide column (3-3) is arranged vertically, and the upper mold plate (3-2) is slidably connected to the guide column (3-3); the lower mold plate (3-1) is provided with a concave mold (7), and the upper mold plate (3-2) is provided with a convex mold (6) corresponding to the concave mold (7); the hot air box (2) is provided with a temperature monitoring module, and the method further comprises the following steps: Step A: Based on the contour of the defective skull (4), the skull is reconstructed and a three-dimensional model of a patch (5) for repairing the defective part is extracted based on the mirror symmetry and surface fitting method, and the outer surface of the patch (5) is extracted separately and meshed and smoothed; Step B: the outer surface of the patch (5) model is stretched downward in a three-dimensional modeling software to form a concave mold (7), and then the outer surface of the patch (5) model is reduced inward and stretched upward to form a convex mold (6), and a mold frame (3) corresponding to the concave mold (7) and the convex mold (6) is designed; Step C: inputting the three-dimensional models of the concave mold (7) and the convex mold (6) into the control computer of the 3D printer for printing. After printing, the printed concave mold (7) and the convex mold (6) are separated from the substrate by removing the support through wire cutting, and then grinding and polishing are performed; Step D: Before die-casting, the die-casting machine (1), the hot air box (2) and the die frame (3) are assembled, the concave die (7) and the convex die (6) are mounted on the die frame (3), and the die frame (3) is placed in the hot air box (2), the hot air box (2) is placed at a suitable position on the bottom plate (1-1) of the die-casting machine (1), and the upper die plate (3-2) is fixed to the pressing head (1-2) of the die-casting machine (1) in the hot air box (2), and the lower die plate (3-1) is fixed to the bottom plate (1-1) of the hot air box (2), thereby completing the die-casting preparation; Step E: placing the PEKK plate on the concave mold (7), placing two hot air guns at the hot air inlet ports on both sides of the hot air box (2), adjusting the power of the hot air guns according to the required molding temperature, and blowing hot air into the hot air box (2) through the flow channel (2-2) so that the ambient temperature of the hot air box (2) reaches the required molding temperature; Step F: When the temperature in the hot air box (2) reaches the target molding temperature, the molding program on the panel of the molding machine (1) is controlled to perform molding of the PEKK skull patch (5). After the molding is completed and the hot air box (2) is cooled, the molded skull patch (5) is taken out and the edges are trimmed. Thus, a patch (5) for a defective skull (4) is formed.

2. The molding method of a polyetherketoneketone skull repair piece high temperature compression molding device according to claim 1 is characterized in that: In the step F, during the die pressing process, a temperature measuring contact is pre-installed on the die (7) or the punch (6), and the temperature measuring contact is guided to the outside of the hot air box (2). The voltage signal is converted into an analog quantity that can be recognized by the PLC through the thermocouple module, and then the analog quantity is converted into temperature data through the analog data conversion program by the single chip microcomputer, and finally the temperature data is displayed in real time on the computer through the serial port.

3. The molding method of a polyetherketoneketone skull repair piece high temperature compression molding device according to claim 2 is characterized in that: In the step F, during the molding process, a thermal imager is placed in front of the heat preservation box to monitor the temperature of the entire heat preservation box, and reflects in real time whether the overall temperature field in the heat preservation box is uniform.

4. The molding method of a polyetherketoneketone skull repair piece high temperature compression molding device according to claim 1, characterized in that: The die pressing machine (1) comprises a pressing head (1-2) and a bottom plate (1-1), a hot air box (2) is placed on the bottom plate (1-1), and the pressing head (1-2) is connected to an upper mold plate (3-2).

5. The molding method of a polyetherketoneketone skull repair piece high temperature compression molding device according to claim 1, characterized in that: Four guide columns (3-3) are arranged between the upper template (3-2) and the lower template (3-1); the upper template (3-2) and the lower template (3-1) have the same size; the guide columns (3-3) are connected to the corners of the upper template (3-2) and the lower template (3-1); the bottom of the guide columns (3-3) is interference fit with the lower template (3-1); and the upper template (3-2) and the guide columns (3-3) are clearance fit.

6. The molding method of the polyetherketoneketone skull repair piece high temperature compression molding device according to claim 5 is characterized in that: The lower template (3-1) is formed with a mounting hole (3-4) corresponding to the concave mold (7), and similarly, the upper template (3-2) is also formed with a mounting hole (3-4) corresponding to the convex mold (6).

7. The molding method of a polyetherketoneketone skull repair piece high temperature compression molding device according to claim 1, characterized in that: The hot air box (2) has hot air outlets (2-1) arranged opposite to each other formed on both sides thereof, a flow channel (2-2) connected to the hot air outlet (2-1) is arranged inside the hot air box (2), the flow channel (2-2) is arranged around the inside of the hot air box (2), and air outlets (2-3) arranged at equal distances are formed on the flow channel (2-2).

8. The molding method of the polyetherketoneketone skull repair piece high temperature compression molding device according to claim 7 is characterized in that: The hot air box (2) is also provided with heat dissipation openings (2-4) arranged opposite to each other on both sides, and the heat dissipation openings (2-4) are located below the hot air opening (2-1).

9. The molding method of a polyetherketoneketone skull repair piece high temperature compression molding device according to claim 1, characterized in that: The temperature monitoring module comprises a temperature measuring contact, a thermocouple module, a single chip microcomputer, a computer and a thermal imager. The thermal imager is placed in front of the heat preservation box. The temperature measuring contact is installed on the concave mold (7) or the convex mold (6). The temperature measuring contact, the thermocouple module, the single chip microcomputer and the computer are electrically connected in sequence.