Chemical cutting method for coal seam roof

By injecting dilute hydrochloric acid into the coal seam roof for corrosion, a cutting groove is formed to achieve roof collapse, which solves the problems of inconvenient construction, high labor intensity and poor safety of calcium carbonate coal seam roof cutting in the existing technology, and realizes advanced and safe coal seam cutting. top effect.

CN114382484BActive Publication Date: 2024-10-29JIAOZUO QUANAN TECH CO LTD +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210066673.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-20
Publication Date
2024-10-29
Estimated Expiration
2042-01-20

AI Technical Summary

Technical Problem

The existing coal seam roof cutting technology is inconvenient to construct in coal seams containing calcium carbonate as the main component, is labor intensive and has poor safety, making it difficult to achieve effective roof collapse control.

Method used

The chemical roof cutting method is used to open horizontal boreholes in the coal seam roof, inject dilute hydrochloric acid for corrosion, and form cutting grooves to achieve preset collapse of the roof, avoiding explosive blasting and repeated drilling, reducing labor intensity and improving efficiency. Security.

Benefits of technology

It achieves advanced roof cutting in calcium carbonate coal seams, significantly reduces the labor intensity of coal seam roof cutting, improves safety, and does not require explosives and repeated drilling, making the construction more convenient and safer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114382484B_ABST
    Figure CN114382484B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of coal mine top cutting, and specifically relates to a method for chemical top cutting of coal seam roof, comprising the following steps: S1, opening a borehole; S2, sealing; S3, injecting acid; S4, replacing acid solution; S5, repeating step S4 until the top cutting is completed, until a groove capable of causing the top plate to collapse along a preset top cutting line is corroded downward along the horizontal borehole, thereby realizing chemical cutting of the coal seam roof. The beneficial effect of the present invention is that it can realize advanced construction in the coal seam top cutting work, and dilute hydrochloric acid can be injected into the borehole and continuously replaced half a year in advance of the time point of the planned completion of the coal seam top cutting, and the calcium carbonate at the bottom of the borehole is corroded and acidified under the action of gravity, thereby forming a groove capable of causing the top plate to collapse along the preset top cutting line. The present invention can realize coal seam top cutting without explosives or repeated drilling, which is conducive to reducing labor intensity, and is convenient to construct and highly safe.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of coal mine roof cutting, and in particular relates to a coal seam roof chemical roof cutting method. Background Art

[0002] During the mining process, the roof of the mined area is required to collapse in time to reduce the pressure on the roof of the working area and ensure the safety of the working area. After the pillars outside the necessary working area are returned, the roof is required to collapse along a line as required. On this line, one side is the support area and the other side is the roof collapse area. This dividing line is the roof collapse line, also known as the roof cutting line. Technical methods are used to make one side a support area and the other side a roof collapse area, which is called "roof cutting".

[0003] The existing top cutting technology usually involves drilling holes at intervals upward from the coal mining tunnel along a preset top cutting line, with 6 holes set each time and a spacing of 1m between adjacent holes. Explosives are then buried in the holes for blasting and top cutting. For coal seam roofs with calcium carbonate as the main component, this method is inconvenient to construct, has high labor intensity, and has poor safety, and needs to be improved. Summary of the invention

[0004] In view of the above situation, the purpose of the present invention is to develop a method for chemical top cutting of coal seam roof, which can realize advanced top cutting construction in coal seam roof with calcium carbonate as the main component, significantly reduce the labor intensity of coal seam top cutting, and improve the safety of coal seam top cutting.

[0005] In order to achieve the above purpose, the present invention adopts the following technical solutions:

[0006] The method for chemically cutting the coal seam roof comprises the following steps:

[0007] S1. Drilling: using a directional drill to drill a horizontal hole in the coal seam roof above the coal mining tunnel;

[0008] S2, sealing: a sealing plate is arranged at the open end of the horizontal borehole, and an exhaust port, an acid injection port and a liquid discharge port are respectively arranged on the sealing plate, and the exhaust port is aligned with the top of the horizontal borehole; a sealing plug is connected to the inner thread of the liquid discharge port, an acid injection pipe is sealedly penetrated in the acid injection port, and an acid injection valve is arranged at one end of the acid injection pipe away from the horizontal borehole;

[0009] S3, acid injection: open the acid injection valve, inject dilute hydrochloric acid into the horizontal borehole through the acid injection pipe, and stop acid injection when acid flows out of the exhaust pipe;

[0010] S4, acid replacement: at regular intervals, drain the waste liquid in the horizontal borehole through the drain port and then re-inject dilute hydrochloric acid through the acid injection pipe; or

[0011] Open the sealing plug regularly and test the acid in the horizontal borehole through the drain port. When the acid concentration drops below 1%, evacuate the waste liquid in the horizontal borehole and re-inject dilute hydrochloric acid through the acid injection pipe;

[0012] S5. Repeat step S4 until the roof cutting is completed: until a groove is corroded downward along the horizontal borehole to cause the roof to collapse along a preset roof cutting line, thereby achieving chemical cutting of the coal seam roof.

[0013] Preferably, in step S1, the distance between the horizontal borehole and the top of the coal mining tunnel is 8 to 12 m, matching the thickness of the coal seam roof.

[0014] Preferably, the diameter of the horizontal hole drilled in step S1 is ≤120 mm, which matches the drill bit diameter of the directional drilling rig and is convenient for construction.

[0015] Preferably, the length of the horizontal borehole is ≤200m, which matches the working depth of the directional drilling rig and is convenient for construction.

[0016] Preferably, in steps S3 and S4, the mass concentration of the dilute hydrochloric acid is 5%, which can reduce the severity of acidolysis and improve the safety of construction.

[0017] Preferably, in step S4, the interval time is ≥ 3 hours, so that the dilute hydrochloric acid can fully hydrolyze the calcium carbonate and improve the utilization rate of the dilute hydrochloric acid.

[0018] The present invention also includes other devices, components or steps that enable the present invention to be used normally, all of which are conventional means in the art. In addition, devices, components or steps not limited in the present invention all adopt the existing technology in the art.

[0019] The beneficial effects of the present invention are as follows: advanced construction can be achieved in coal seam top cutting work, dilute hydrochloric acid can be injected into the borehole and continuously replaced half a year in advance of the planned time point of coal seam top cutting, and the calcium carbonate in the lower part of the borehole is corroded and acidified under the action of gravity, thereby forming a cutting groove that can cause the roof to collapse along a preset top cutting line. The present invention can achieve coal seam top cutting without explosives or repeated drilling, which is beneficial to reducing labor intensity, and is convenient to construct and highly safe. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a process flow chart of the present invention in the embodiment.

[0021] Figure 2 It is a schematic diagram of the arrangement structure of the horizontal drilling of the present invention in an embodiment.

[0022] Figure 3 for Figure 2 Schematic diagram of the enlarged structure of part A in FIG. DETAILED DESCRIPTION

[0023] The technical solution of the present invention will be clearly and completely described below in conjunction with specific embodiments. Obviously, the described embodiments are only some embodiments of the present invention, rather than all embodiments.

[0024] It should be noted that the directions or positional relationships indicated by the terms "upper", "lower", "front", "back", "inside", "outside", etc. are based on the drawings and are only for the convenience of description.

[0025] Example

[0026] like Figures 1 to 3 As shown, the method for chemically cutting the coal seam roof provided by the present invention comprises the following steps:

[0027] S1, drilling: using a directional drill to drill a horizontal borehole 3 in the coal seam roof 2 above the coal mining tunnel 1;

[0028] S2, sealing: a sealing plate 4 is arranged at the open end of the horizontal borehole, and an exhaust port 5, an acid injection port and a liquid discharge port 6 are respectively arranged on the sealing plate, and the exhaust port is aligned with the top of the horizontal borehole; a sealing plug 7 is connected to the inner thread of the liquid discharge port, and an acid injection pipe 8 is sealed and penetrated in the acid injection port, and an acid injection valve 9 is arranged at the end of the acid injection pipe away from the horizontal borehole;

[0029] S3, acid injection: open the acid injection valve, inject dilute hydrochloric acid into the horizontal borehole through the acid injection pipe, and stop acid injection when acid flows out of the exhaust pipe;

[0030] S4, acid replacement: at fixed intervals, the waste liquid in the horizontal borehole is emptied through the drain port and then diluted hydrochloric acid is re-injected through the acid injection pipe;

[0031] S5. Repeat step S4 until the roof cutting is completed: until a groove is corroded downward along the horizontal borehole to cause the roof to collapse along a preset roof cutting line, thereby achieving chemical cutting of the coal seam roof.

[0032] Specifically, in step S1, the distance between the horizontal borehole and the top of the coal mining tunnel is 10m, which matches the thickness of the coal seam roof. The aperture of the horizontal borehole in step S1 is 120mm, which matches the drill bit diameter of the directional drill, and is convenient for construction. The length of the horizontal borehole is 200m, which matches the working depth of the directional drill, and is convenient for construction. In steps S3 and S4, the mass concentration of the dilute hydrochloric acid is 5%, which can reduce the severity of acidolysis and improve the safety of construction. In step S4, the interval time is 3h, which is convenient for the dilute hydrochloric acid to fully acidolyze calcium carbonate and improve the utilization rate of the dilute hydrochloric acid.

[0033] The present invention can realize advanced construction in coal seam top cutting work. Dilute hydrochloric acid can be injected into the borehole and continuously replaced half a year in advance of the planned time point of coal seam top cutting. Under the action of gravity, the calcium carbonate in the lower part of the borehole is corroded and acidified, thereby forming a cutting groove that can cause the roof to collapse along a preset top cutting line. The present invention can realize coal seam top cutting without explosives or repeated drilling, which is beneficial to reducing labor intensity, and is convenient in construction and highly safe.

[0034] The technical solution of the present invention is not limited to the above-mentioned specific embodiments. Without departing from the scope and spirit of the described embodiments, many modifications and changes are obvious to ordinary technicians in this technical field. Any technical deformation made within the spirit and principles of the present invention falls within the protection scope of the present invention.

Claims

1. A method for chemically cutting the roof of a coal seam, characterized in that: The steps include: S1. Drilling: using a directional drill to drill a horizontal hole in the coal seam roof above the coal mining tunnel; S2, sealing: a sealing plate is arranged at the open end of the horizontal borehole, and an exhaust port, an acid injection port and a liquid discharge port are respectively arranged on the sealing plate, and the exhaust port is aligned with the top of the horizontal borehole; a sealing plug is connected to the inner thread of the liquid discharge port, an acid injection pipe is sealedly penetrated in the acid injection port, and an acid injection valve is arranged at one end of the acid injection pipe away from the horizontal borehole; S3, acid injection: open the acid injection valve, inject dilute hydrochloric acid into the horizontal borehole through the acid injection pipe, and stop acid injection when acid flows out of the exhaust pipe; S4, acid replacement: at regular intervals, drain the waste liquid in the horizontal borehole through the drain port and then re-inject dilute hydrochloric acid through the acid injection pipe; or Open the sealing plug regularly and test the acid in the horizontal borehole through the drain port. When the acid concentration drops below 1%, evacuate the waste liquid in the horizontal borehole and re-inject dilute hydrochloric acid through the acid injection pipe; S5. Repeat step S4 until the roof cutting is completed: until a groove is corroded downward along the horizontal borehole to cause the roof to collapse along a preset roof cutting line, thereby achieving chemical cutting of the coal seam roof.

2. The method for chemically cutting the coal seam roof according to claim 1, characterized in that: In the step S1, the distance between the horizontal borehole and the top of the coal mining tunnel is 8 to 12 m.

3. The method for chemically cutting the coal seam roof according to claim 1, characterized in that: The diameter of the horizontal drilling hole in step S1 is ≤120 mm.

4. The method for chemically cutting the coal seam roof according to claim 1, characterized in that: The length of the horizontal borehole is ≤200m.

5. The method for chemically cutting the coal seam roof according to any one of claims 1 to 4, characterized in that: In the steps S3 and S4, the mass concentration of the dilute hydrochloric acid is 5%.

6. The method for chemically cutting the coal seam roof according to claim 5, characterized in that: In step S4, the interval time is ≥ 3h.

Citation Information

Patent Citations

  • Method of roof cutting pressure relief of narrow coal pillar gob side through static bursting for gob-side entry driving

    CN107701188A

  • Supercritical water processing method for enhancing gas transportation capacity of shale matrix

    CN110107271A