Method for manufacturing metal interconnect structure

During the production process of the metal interconnection structure, the interlayer dielectric layer is removed to form holes to ensure that the power supply layer for electroplating does not reflect light, achieving precise alignment of the mask and the precise position of the upper metal block, and solving the problem of inter-layer alignment accuracy. It reduces the problem and improves the integration of the product.

CN114429935BActive Publication Date: 2024-10-25CR RUNAN TECHNOLOGIES (CHONGQING) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011183114.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-10-29
Publication Date
2024-10-25
Estimated Expiration
2040-10-29

AI Technical Summary

Technical Problem

In the existing technology, the inter-layer alignment accuracy is low, resulting in the cross-sectional area of ​​the conductive pillars having to be increased, which limits the integration of the product.

Method used

Before forming the power supply layer for electroplating, the interlayer dielectric layer around the target is removed to form a hole. The power supply layer for electroplating at the hole is non-reflective, so that the mask can be accurately aligned with the target position, thereby filling the upper metal block in the opening.

Benefits of technology

The accuracy of inter-layer alignment is improved, the cross-sectional area of ​​the conductive pillars is reduced, and the integration of the product is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114429935B_ABST
    Figure CN114429935B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing a metal interconnection structure, comprising: providing a lower interconnection layer and an interlayer dielectric layer located on the lower interconnection layer, wherein the interlayer dielectric layer has a conductive column and a target; removing the interlayer dielectric layer around the target to form a hole; forming a power supply layer for electroplating on the interlayer dielectric layer, the conductive column and the target; forming a sacrificial layer on the power supply layer for electroplating and at the hole opening of the hole, and patterning the sacrificial layer to form a plurality of openings; aligning the mask used for patterning with reference to the position of the target; electroplating metal in the opening to form an upper metal block. According to an embodiment of the present invention, when the mask is aligned with the position of the target, the hole causes the power supply layer for electroplating to form a dark ring, which can distinguish the target from the surrounding structure, and can improve the interlayer alignment accuracy, thereby improving the product integration.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for manufacturing a metal interconnection structure. Background Art

[0002] In recent years, with the continuous development of circuit integration technology, electronic products are increasingly moving towards miniaturization, intelligence, high integration, high performance and high reliability. Multi-layer metal interconnection structures can improve product integration.

[0003] When a product requires a multi-layer metal interconnection structure, the inter-layer alignment accuracy will limit the product design specifications. Under the same electrical conductivity performance requirements, the higher the inter-layer alignment accuracy, the smaller the cross-sectional area of ​​the conductive pillar used for inter-layer conduction can be made, while the lower the inter-layer alignment accuracy, the larger the cross-sectional area of ​​the conductive pillar must be, which is not conducive to improving the integration of the product.

[0004] In view of this, it is necessary to provide a new method for manufacturing a metal interconnect structure to improve the inter-layer alignment accuracy, thereby improving product integration. Summary of the invention

[0005] The object of the present invention is to provide a method for manufacturing a metal interconnect structure to improve the inter-layer alignment accuracy, thereby improving product integration.

[0006] To achieve the above object, the present invention provides a method for manufacturing a metal interconnect structure, comprising:

[0007] Providing a lower interconnection layer and an interlayer dielectric layer located on the lower interconnection layer, wherein the interlayer dielectric layer has a conductive column and a target;

[0008] At least removing the interlayer dielectric layer around the target to form a hole;

[0009] forming a power supply layer for electroplating on the interlayer dielectric layer, the conductive pillars and the target; forming a sacrificial layer on the power supply layer for electroplating and at the opening of the hole, and patterning the sacrificial layer to form a plurality of openings; aligning the mask used for patterning with reference to the position of the target;

[0010] Metal is electroplated in the opening to form an upper metal block.

[0011] Optionally, the interlayer dielectric layer is an organic insulating layer, and the interlayer dielectric layer around the target is removed by laser burning.

[0012] Optionally, the material of the organic insulating layer is ABF.

[0013] Optionally, the lower interconnect layer includes a first dielectric layer and a lower metal block and a dummy lower metal block located in the first dielectric layer; when removing the interlayer dielectric layer around the target, the first dielectric layer around the dummy lower metal block carrying the target is also removed.

[0014] Optionally, the dummy lower metal block falls within an orthographic projection of the target on the lower interconnect layer.

[0015] Optionally, a size range of a boundary of the dummy lower metal block from a boundary of an orthographic projection of the target on the lower interconnect layer is 10 μm to 30 μm.

[0016] Optionally, in the radial direction of the hole, a distance between a boundary of an orthographic projection of the target on the lower interconnect layer and a boundary of an orthographic projection of an interlayer dielectric layer surrounding the target on the lower interconnect layer is in the range of 100 μm to 200 μm.

[0017] Optionally, the power supply layer for electroplating is formed by physical vapor deposition or chemical vapor deposition.

[0018] Optionally, the conductive pillar and the target are made of copper or aluminum.

[0019] Optionally, the material of the sacrificial layer is photoresist.

[0020] Optionally, there are a plurality of targets, and the plurality of targets are located at respective corners of the lower interconnection layer.

[0021] Optionally, the lower interconnect layer is located on the plastic packaging layer and the front side of the die, the front side of the die exposes the pad, and the lower interconnect layer is a rewiring layer.

[0022] Optionally, the lower interconnect layer is located on the front side of a plurality of the dies.

[0023] According to the inventor's analysis, the reason for the low inter-layer alignment accuracy in the related art is that the upper surface of the interlayer dielectric layer, the upper surface of the conductive column and the upper surface of the target are flush. After the electroplating power supply layer and the sacrificial layer are formed on the interlayer dielectric layer, the conductive column and the target in turn, when the sacrificial layer is patterned to form an opening, the entire surface of the electroplating power supply layer reflects light, and the mask used for patterning cannot be aligned with the position of the target, which will cause the opening position to deviate from the preset position, and thus the upper metal block filled in the opening will also deviate from the preset position. If the cross-sectional area of ​​the conductive column is small, the upper metal block cannot be electrically connected to the lower metal block. To avoid the above problems, the cross-sectional area of ​​the conductive column needs to be increased.

[0024] Based on the above analysis, the present invention removes the interlayer dielectric layer around the target to form a hole before forming the power supply layer for electroplating. The thickness of the power supply layer for electroplating is relatively thin and will not fill the hole. This allows the mask used for patterning to use an optical alignment method when the sacrificial layer formed on the power supply layer for electroplating and at the hole opening is patterned. The power supply layer for electroplating at the hole does not reflect light, and the mask can be accurately aligned with the position of the target, so that the opening position can be accurately located at the preset position, and the upper metal block filled in the opening will also be accurately located at the preset position, and the cross-sectional area of ​​the conductive column can be made small.

[0025] Compared with the prior art, the beneficial effect of the present invention is that when the positions of the mask and the target are aligned, the holes form a dark ring on the power supply layer for electroplating, which can distinguish the target from the surrounding structure, improve the inter-layer alignment accuracy, and thus improve the product integration. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 is a flow chart of a method for manufacturing a metal interconnect structure according to a first embodiment of the present invention;

[0027] Figure 2 , Figure 3 , Figures 6 to 10 yes Figure 1 Schematic diagram of the intermediate structure corresponding to the process in;

[0028] Figure 4 and Figure 5 is a schematic diagram of the control structure;

[0029] Fig.11 and Fig.12 is a schematic diagram of an intermediate structure corresponding to a method for manufacturing a metal interconnect structure according to a second embodiment of the present invention;

[0030] Fig.13 and Fig.14 is a schematic diagram of the control structure;

[0031] Figures 15 to 17 It is a schematic diagram of an intermediate structure corresponding to the method for manufacturing a metal interconnection structure according to the third embodiment of the present invention.

[0032] To facilitate understanding of the present invention, all reference numerals appearing in the present invention are listed below:

[0033] Lower interconnect layer 21 First dielectric layer 211

[0034] Lower metal block 212 Dummy lower metal block 213

[0035] Interlayer dielectric layer 22 Conductive pillar 221

[0036] Target 222 Bare die 11

[0037] Front side of die 11a Back side of die 11b

[0038] Solder pad 111 Plastic layer 12

[0039] Back side 12b of plastic sealing layer Front side 12a of plastic sealing layer

[0040] Hole 22a Power supply layer 23 for electroplating

[0041] Sacrificial layer 24 opening 24a

[0042] Upper metal block 25 Support plate 2

[0043] Mask 3 DETAILED DESCRIPTION

[0044] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0045] Figure 1 is a flow chart of a method for manufacturing a metal interconnect structure according to a first embodiment of the present invention; Figure 2 , Figure 3 , Figures 6 to 10 yes Figure 1 Schematic diagram of the intermediate structure corresponding to the process in . Figure 4 and Figure 5 It is a schematic diagram of the control structure.

[0046] First, refer to Figure 1 Step S1 in Figure 2 As shown, a lower interconnection layer 21 and an interlayer dielectric layer 22 located on the lower interconnection layer 21 are provided, and the interlayer dielectric layer 22 has conductive pillars 221 and targets 222 therein.

[0047] In this embodiment, refer to Figure 2 As shown, the lower interconnection layer 21 is located on the plastic encapsulation layer 12 and the front side 11a of the die 11, and the front side 11a of the die 11 exposes the pad 111. In other words, the lower interconnection layer 21 is a redistribution layer (RDL).

[0048] The lower interconnect layer 21 includes a first dielectric layer 211 , and a lower metal block 212 and a dummy lower metal block 213 located in the first dielectric layer 211 .

[0049] The lower metal block 212 is selectively connected to a plurality of pads 111 to implement the circuit layout of the pads 111. The dummy lower metal block 213 is located at the same layer as the lower metal block 212, but has no electrical connection design requirement.

[0050] In this embodiment, the first dielectric layer 211 and the interlayer dielectric layer 22 are made of the same material, ABF (Ajinomoto buildup film). Specifically, the lower metal block 212 and the pseudo lower metal block 213, the conductive column 221 and the target 222 can be formed on the plastic layer 12 and the front surface 11a of the bare chip 11 by electroplating process; then the ABF dry film is applied to the surface of the plastic layer 12 exposed by the conductive column 221, the target 222, the lower metal block 212, the pseudo lower metal block 213, and the lower metal block 212 and the pseudo lower metal block 213; then the ABF dry film is polished until the conductive column 221 and the target 222 are exposed. The ABF dry film is a photosensitive material.

[0051] In other embodiments, the materials of the first dielectric layer 211 and the interlayer dielectric layer 22 may also be organic polymer insulating materials such as polyimide, epoxy resin, PBO (Polybenzoxazole), organic polymer film, organic polymer composite material or other organic materials with similar insulating properties.

[0052] In some embodiments, the material of the first dielectric layer 211 and the interlayer dielectric layer 22 may also be inorganic insulating materials such as silicon dioxide or silicon nitride.

[0053] In some embodiments, the first dielectric layer 211 and the interlayer dielectric layer 22 may be made of different materials.

[0054] In some embodiments, the first dielectric layer 211 and the interlayer dielectric layer 22 are formed in different processes.

[0055] The material of the lower metal block 212 and the dummy lower metal block 213 is a conductive metal such as copper or aluminum.

[0056] The conductive pillar 221 is located on the lower metal block 212 and is used for selectively connecting with the lower metal block 212 .

[0057] Since the dummy lower metal block 213 has no electrical connection design requirements, the target 222 carried by it also has no electrical connection design requirements and only serves as an alignment.

[0058] In this embodiment, refer to Figure 2 As shown, the orthographic projection of the target 222 on the lower interconnect layer 21 falls within the dummy lower metal block 213 .

[0059] The bare die 11 may be formed by dividing a wafer. The wafer includes a front side of the wafer and a back side of the wafer, and the front side of the wafer is provided with a pad 111 and an insulating layer (not shown) for protecting the pad 111. The bare die 11 is formed after the wafer is cut, and accordingly, the bare die 11 includes a front side 11a and a back side 11b, and the front side 11a is provided with a pad 111 and an insulating layer for electrically isolating adjacent pads 111.

[0060] The wafer may be thinned from the back side before dicing to reduce the thickness of the die 11 .

[0061] The material of the plastic encapsulation layer 12 can be epoxy resin, polyimide resin, benzocyclobutene resin, polybenzoxazole resin, polybutylene terephthalate, polycarbonate, polyethylene terephthalate, polyethylene, polypropylene, polyolefin, polyurethane, polyolefin, polyether sulfone, polyamide, polyurethane, ethylene-vinyl acetate copolymer or polyvinyl alcohol, etc. The material of the plastic encapsulation layer 12 can also be various polymers or composite materials of resins and polymers.

[0062] The molding layer 12 may include a front surface 12 a and a back surface 12 b opposite to each other.

[0063] In this embodiment, the back side 12b of the plastic encapsulation layer 12 is flush with the front side 11a of the die 11, and a support plate 2 may be provided on the front side 12a of the plastic encapsulation layer 12 to support the plastic encapsulation structure of the die 11 in subsequent processes.

[0064] The support plate 2 is a hard plate, which may include a plastic plate, a glass plate, a ceramic plate or a metal plate.

[0065] An adhesive layer may be provided between the front side 12a of the plastic sealing layer 12 and the support plate 2 to achieve fixation between the two.

[0066] The adhesive layer may be made of an easily peelable material so as to peel off the support plate 2, for example, a thermal separation material that can lose its stickiness by heating or a UV separation material that can lose its stickiness by ultraviolet irradiation may be used.

[0067] In some embodiments, the lower interconnect layer 21 may be located on a semiconductor substrate. A semiconductor substrate, such as a silicon substrate, has several devices formed therein, such as transistors, etc. In other words, the lower interconnect layer 21 is a metal interconnect structure in the die 11 and is not used for a packaging structure.

[0068] Next, refer to Figure 1 Step S2 in Figure 3 As shown, at least the interlayer dielectric layer 22 around the target 222 is removed to form a hole 22a.

[0069] When the material of the interlayer dielectric layer 22 is an organic high molecular polymer insulating material, the removal is performed by a laser burning method.

[0070] When the material of the interlayer dielectric layer 22 is an inorganic insulating material, the removal is performed by dry etching or wet etching.

[0071] In this embodiment, since the first dielectric layer 211 and the interlayer dielectric layer 22 are made of the same material, when the interlayer dielectric layer 22 is removed, the first dielectric layer 211 around the dummy lower metal block 213 is also removed, thereby increasing the depth of the hole 22a.

[0072] In some embodiments, when the first dielectric layer 211 and the interlayer dielectric layer 22 are made of different materials, only the interlayer dielectric layer 22 around the target 222 may be removed.

[0073] In the radial direction of the hole 22a, the distance D1 between the boundary of the orthographic projection of the target 222 on the lower interconnection layer 21 and the boundary of the orthographic projection of the interlayer dielectric layer 22 surrounding the target 222 on the lower interconnection layer 21 may be in the range of 100 μm to 200 μm. This is because:

[0074] Reference Figure 4 As shown, if the range of dimension D1 is too large, the removal amount of interlayer dielectric layer 22 and first dielectric layer 211 is too much, and due to insufficient laser energy or etching time, the interlayer dielectric layer 22 / first dielectric layer 211 will remain around the target 222 and / or the dummy lower metal block 213.

[0075] Reference Figure 5 As shown, if the size D1 is too small, the mask used to form the hole 22 a may have an alignment error, which may cause the target 222 and / or the dummy lower metal block 213 to adhere to the surrounding interlayer dielectric layer 22 / first dielectric layer 211 .

[0076] Afterwards, refer to Figure 1 Step S3 in Figure 6 As shown, a power supply layer 23 for electroplating is formed on the interlayer dielectric layer 22, the conductive pillar 221 and the target 222; Figure 7 and Figure 8 As shown, a sacrificial layer 24 is formed on the electroplating power supply layer 23 and at the opening of the hole 22 a , and the sacrificial layer 24 is patterned to form a plurality of openings 24 a ; the mask 3 used for patterning is aligned with reference to the position of the target 222 .

[0077] Step S3 may include the following steps S31 to S34.

[0078] Step S31: forming a power supply layer 23 for electroplating.

[0079] In step S31, refer to Figure 6 As shown, the material of the electroplating power supply layer 23 can be copper or aluminum, and can be formed by physical vapor deposition or chemical vapor deposition. The thickness of the electroplating power supply layer 23 is relatively thin, so when deposited, it will be formed on the bottom wall and / or side wall of the hole 22a, but will not fill the hole 22a.

[0080] Step S32: forming a sacrificial layer 24.

[0081] In this embodiment, refer to Figure 7 As shown, the material of the sacrificial layer 24 can be a photoresist layer. In an optional solution, the photoresist layer formed can be a photosensitive film. The photosensitive film can be torn off from the tape and applied to the electroplating power supply layer 23 and the hole 22a. In other optional solutions, the photoresist layer can also be formed by first applying a liquid photoresist and then heating and curing.

[0082] In some embodiments, the material of the sacrificial layer 24 may be an inorganic insulating material such as silicon nitride or silicon dioxide. At this time, a photoresist layer needs to be formed on the sacrificial layer 24. In an optional solution, the formed photoresist layer may be a photosensitive film.

[0083] Step S33: Continue to refer to Figure 7 As shown, the mask 3 for patterning the sacrificial layer 24 is aligned with reference to the position of the target 222 .

[0084] Since there is a height difference between the inside and outside of the hole 22a, the hole 22a is not filled with the electroplating power supply layer 23. Therefore, when the mask 3 is optically aligned, the electroplating power supply layer 23 in the hole 22a does not reflect light, and a dark ring can be formed to distinguish the target 222 from the surrounding structure. In this way, the mask 3 can be accurately aligned with the position of the target 222. The deeper the hole 22a, the darker the color of the dark ring.

[0085] Reference Figure 4 As shown, if the range of dimension D1 is too large, the interlayer dielectric layer 22 / first dielectric layer 211 will remain around the target 222 and / or the dummy lower metal block 213 . When the mask 3 is optically aligned, the remaining interlayer dielectric layer 22 / first dielectric layer 211 will reflect light, affecting the position identification of the target 222 .

[0086] Reference Figure 5 As shown, if the range of dimension D1 is too small, the target 222 and / or the pseudo lower metal block 213 will adhere to the surrounding interlayer dielectric layer 22 / first dielectric layer 211, the power supply layer 23 for electroplating will not be disconnected, and there will be no dark ring at the undisconnected position, which will affect the position identification of the target 222.

[0087] Step S34: Refer to Figure 8 As shown, the photoresist layer is exposed and developed to form a patterned photoresist layer.

[0088] When the material of the sacrificial layer 24 is an inorganic insulating material such as silicon nitride or silicon dioxide, the sacrificial layer 24 is etched using the patterned photoresist layer as a mask to form an opening 24 a.

[0089] Since the mask 3 used for patterning the sacrificial layer 24 can be precisely aligned with the position of the target 222 , the position of the opening 24 a can be precisely located at the preset position.

[0090] Next, refer to Figure 1 Step S4 in Fig. 9 As shown, metal is electroplated in the opening 24a to form an upper metal block 25.

[0091] Electroplating can include electrolytic plating or electrodeless plating. Electrolytic plating is to use the workpiece to be plated as the cathode and electrolyze the electrolyte to form a layer of metal on the workpiece to be plated. Electroless plating is a method of reducing and precipitating metal ions in the solution to form a metal layer on the workpiece to be plated.

[0092] The material of the electroplated metal can be copper or aluminum.

[0093] After electroplating, the upper metal block 25 can be polished to achieve a smooth upper surface, such as chemical mechanical polishing.

[0094] Reference Fig.10 As shown, after the electroplating is completed, the sacrificial layer 24 can be removed.

[0095] When the material of the sacrificial layer 24 is a photoresist layer, the sacrificial layer 24 is removed by an ashing method.

[0096] When the material of the sacrificial layer 24 is an inorganic insulating material such as silicon nitride or silicon dioxide, the sacrificial layer 24 is removed by wet etching with an etching solution, for example, silicon nitride is removed by hot phosphoric acid, and silicon dioxide is removed by hydrofluoric acid.

[0097] Continue to refer to Fig.10 As shown, after the sacrificial layer 24 is removed, the exposed electroplating power supply layer 23 may be removed by dry etching or wet etching.

[0098] Afterwards, the support plate 2 can be removed. The support plate 2 can be removed by conventional removal methods such as laser stripping and UV irradiation.

[0099] Fig.11 and Fig.12 It is a schematic diagram of an intermediate structure corresponding to the method for manufacturing a metal interconnection structure according to the second embodiment of the present invention. Fig.13 and Fig.14 is a schematic diagram of the control structure. Fig.11 and Fig.12 As shown, the method for manufacturing the metal interconnection structure in this embodiment is similar to Figure 1 The manufacturing method of the metal interconnection structure of the first embodiment is substantially the same, except that in step S1, in the provided lower interconnection layer 21 and the target 222, the dummy lower metal block 213 falls within the orthographic projection of the target 222 on the lower interconnection layer 21. Fig.13As shown, when the first dielectric layer 211 and the interlayer dielectric layer 22 need to be removed simultaneously to form a deeper hole 22 a , the dummy lower metal block 213 will not be exposed after removing the interlayer dielectric layer 22 , and the first dielectric layer 211 will not be unable to be removed.

[0100] Reference Fig.12 As shown, the dimension D2 of the boundary of the dummy lower metal block 213 from the boundary of the orthographic projection of the target 222 on the lower interconnect layer 21 is preferably in the range of 10 μm to 30 μm. This is because:

[0101] If the size D2 is too small, the target 222 and the dummy lower metal block 213 may be misaligned. Fig.13 Problems in

[0102] If the range of dimension D2 is too large, refer to Fig.14 As shown, the first dielectric layer 211 around the dummy lower metal block 213 is blocked by the target 222 , and the first dielectric layer 211 will remain around the dummy lower metal block 213 . When the mask 3 is optically aligned, the remaining first dielectric layer 211 will reflect light, affecting the position identification of the target 222 .

[0103] Figures 15 to 17 is a schematic diagram of an intermediate structure corresponding to a method for manufacturing a metal interconnect structure according to a third embodiment of the present invention, wherein Fig.16 It is along Fig.15 The cross-sectional view of the AA line in. Figures 15 to 17 As shown, the manufacturing method of the metal interconnection structure in this embodiment is substantially the same as the manufacturing method of the metal interconnection structure in Embodiments 1 and 2, with the only difference being that in step S1 , the provided lower interconnection layer 21 is located on the front side 11 a of the plastic encapsulation layer 12 and the plurality of bare chips 11 .

[0104] It is understandable that manufacturing the rewiring layers of a plurality of bare chips 11 in the same process can improve manufacturing efficiency compared to manufacturing the rewiring layers for each bare chip 11 separately.

[0105] Reference Fig.17 As shown, after the structure of the back side 12b of the plastic packaging layer is manufactured, it can be cut along the cutting path to form a plurality of chip packaging structures.

[0106] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for manufacturing a metal interconnect structure, characterized in that: include: Providing a lower interconnection layer and an interlayer dielectric layer located on the lower interconnection layer, wherein the interlayer dielectric layer has a conductive column and a target; At least the interlayer dielectric layer around the target is removed to form a hole; wherein the lower interconnect layer includes a first dielectric layer and a lower metal block and a dummy lower metal block located in the first dielectric layer; when removing the interlayer dielectric layer around the target, the first dielectric layer around the dummy lower metal block carrying the target is also removed; the dummy lower metal block falls within the orthographic projection of the target on the lower interconnect layer; A power supply layer for electroplating is formed on the interlayer dielectric layer, the conductive pillar and the target; a sacrificial layer is formed on the power supply layer for electroplating and at the opening of the hole, and the sacrificial layer is patterned to form a plurality of openings; the mask used for patterning is aligned with reference to the position of the target; wherein the power supply layer for electroplating is formed on the bottom wall and / or side wall of the hole, and the hole is not filled; Metal is electroplated in the opening to form an upper metal block.

2. The method for manufacturing a metal interconnect structure according to claim 1, characterized in that: The interlayer dielectric layer is an organic insulating layer, and the interlayer dielectric layer around the target is removed by laser burning.

3. The method for manufacturing a metal interconnection structure according to claim 2, characterized in that: The material of the organic insulating layer is ABF.

4. The method for manufacturing a metal interconnect structure according to claim 1, characterized in that: The distance between the boundary of the dummy lower metal block and the boundary of the orthographic projection of the target on the lower interconnect layer is in the range of 10 μm to 30 μm.

5. The method for manufacturing a metal interconnect structure according to claim 1, characterized in that: In the radial direction of the hole, the distance between the boundary of the orthographic projection of the target on the lower interconnection layer and the boundary of the orthographic projection of the interlayer dielectric layer surrounding the target on the lower interconnection layer is in the range of 100 μm to 200 μm.

6. The method for manufacturing a metal interconnect structure according to claim 1, characterized in that: The material of the conductive pillar and the target is copper or aluminum; and / or the material of the sacrificial layer is photoresist.

7. The method for manufacturing a metal interconnect structure according to claim 1, characterized in that: There are a plurality of targets, and the plurality of targets are located at respective corners of the lower interconnection layer.

8. The method for manufacturing a metal interconnection structure according to claim 1, characterized in that: The lower interconnection layer is located on the plastic packaging layer and the front side of the die, the front side of the die exposes the pad, and the lower interconnection layer is a rewiring layer.

9. The method for manufacturing a metal interconnection structure according to claim 8, characterized in that: The underlying interconnect layer is located on the front sides of a plurality of the dies.