Laminated coil component and mounting structure of laminated coil component
By providing a glass layer on the terminal electrode of the laminated coil component to cover its convex area, and avoiding the formation of solder, the stress concentration problem caused by overlapping the pad electrode and the terminal electrode end is solved, and the crack suppression effect is achieved during installation.
Patent Information
- Application Number
- CN202111214701.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-11-02
- Filing Date
- 2021-10-19
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-10-19
AI Technical Summary
When installing the laminated coil component, the end of the pad electrode and the end of the solder overlap with the end of the terminal electrode, resulting in stress concentration, and cracks are easily generated on the body of the laminated coil component.
A laminated coil component is designed, with a glass layer disposed on the terminal electrode, the glass layer being arranged along the terminal electrode edge containing at least one convex portion and covering a certain area to avoid solder formation, thereby ensuring the end of the pad electrode and the solder The ends of the terminals do not coincide with the terminal electrodes, reducing stress concentration.
Through the design of the glass layer, stress concentration during the installation of the laminated coil components is effectively avoided, cracks are prevented on the body, and installation reliability is improved.
Smart Images

Figure CN114446573B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a laminated coil component and a mounting structure of the laminated coil component. Background Art
[0002] The laminated coil component includes an element body and a pair of terminal electrodes arranged across a mounting surface and an end surface of the element body (for example, refer to Japanese Patent Application Laid-Open No. 2018-200966). Summary of the invention
[0003] The laminated coil component is mounted on a pad electrode such as a circuit substrate by solder. The solder infiltrates and transfers on the terminal electrode and is formed to the end of the terminal electrode. When the laminated coil component is mounted on the pad electrode, if the end of the pad electrode and the end of the solder overlap with the end of the terminal electrode, the stress generated by the deflection of the circuit substrate, etc., can be concentrated on the end of the terminal electrode. As a result, the end of the terminal electrode can be set as the starting point, and cracks can be generated in the element body of the laminated coil component.
[0004] An object of one aspect of the present invention is to provide a laminated coil component and a laminated coil component mounting structure that can suppress the occurrence of cracks in an element body during mounting.
[0005] One aspect of the present invention provides a stacked coil component, comprising: a body formed by stacking a plurality of insulating layers, and having a pair of end faces opposite to each other, a pair of main faces opposite to each other, and a pair of side faces opposite to each other, wherein one main face is a mounting surface; a pair of terminal electrodes, each of which is arranged in a recess formed on the mounting surface on one of the pair of end face sides of the body; a glass layer, which is arranged on the terminal electrodes, and in each of the pair of terminal electrodes, a plurality of first protrusions that become thinner at the front end toward the other terminal electrode side are arranged at the first end portions opposite to each other in the relative directions of the pair of end faces, and the glass layer is arranged at the first end portion of the terminal electrode along the edge of the terminal electrode including at least the first protrusion.
[0006] In a laminated coil component of one aspect of the present invention, a terminal electrode is provided with a plurality of first protrusions at a first end portion that become thinner toward the opposite other terminal electrode side. In this structure, in the laminated coil component, a glass layer is provided at the first end portion of the terminal electrode along the edge of the terminal electrode including at least the first protrusion. Solder is not formed on the glass layer. Therefore, in the laminated coil component, when solder is mounted on a pad electrode such as a circuit substrate, solder is not formed on the glass layer covering the first end portion. Thus, when the laminated coil component is mounted on the pad electrode, the position of the end of the pad electrode and the end of the solder and the position of the end of the terminal electrode will not overlap. That is, in the relative directions of a pair of main surfaces of the element body, the position of the end of the pad electrode and the end of the solder and the position of the end of the terminal electrode are inconsistent. Therefore, in the laminated coil component, stress concentration on the end of the terminal electrode can be avoided. As a result, in the laminated coil component, when it is mounted, cracks can be suppressed from occurring on the element body.
[0007] In one embodiment, the glass layer may cover 60% or more of the area of the convex portion. In this structure, it is possible to more reliably avoid the formation of solder on the first end portion of the terminal electrode.
[0008] In one embodiment, the edge of the end surface side of the glass layer may have a corrugated shape corresponding to the plurality of first protrusions. In this structure, the edge of the first protrusion is covered by the glass layer, and an area for forming solder can be ensured in the terminal electrode.
[0009] In one embodiment, each of a pair of terminal electrodes may be arranged in a recess formed in each of a pair of end faces, and a plurality of second protrusions tapering toward the main surface side are provided at the second end of the other main surface side of the terminal electrode arranged at the end face, and the glass layer is provided at the second end of the terminal electrode along the edge of the terminal electrode including at least the second protrusion. In this structure, when solder is installed on a pad electrode such as a circuit substrate, solder is not formed on the glass layer covering the second end. Thus, when the stacked coil component is installed on the pad electrode, the position of the end of the solder and the position of the end of the terminal electrode will not overlap. Therefore, in the stacked coil component, stress concentration on the end of the terminal electrode can be avoided. As a result, in the stacked coil component, cracks can be suppressed from occurring in the element body during installation.
[0010] In one embodiment, each of a pair of terminal electrodes may be provided with a plurality of third protrusions tapering toward the end face side at the third end portion on the end face side, and the glass layer may be provided at the third end portion of the terminal electrode along the edge of the terminal electrode including at least the third protrusion. In this structure, when solder is mounted on a pad electrode such as a circuit substrate, solder is not formed on the glass layer covering the first end portion and the third end portion. Thus, when the stacked coil component is mounted on the pad electrode, the positions of the end of the pad electrode and the end of the solder and the end of the terminal electrode will not overlap. Therefore, in the stacked coil component, stress concentration on the end of the terminal electrode can be avoided. As a result, in the stacked coil component, cracks can be avoided in the element body during installation.
[0011] An installation structure according to one aspect of the present invention comprises: the stacked coil component; a circuit substrate having a pad electrode for mounting the stacked coil component; and solder arranged between the terminal electrode and the pad electrode of the coil component, wherein the solder is not formed on the glass layer, and when observed from relative directions of a pair of main surfaces of the element body, the end of the pad electrode, the end of the solder, and the first end of the terminal electrode do not overlap.
[0012] In the mounting structure of one aspect of the present invention, when viewed from the relative directions of a pair of main surfaces of the element body, the end of the pad electrode and the end of the solder do not overlap with the first end of the terminal electrode. Thus, in the mounting structure of the laminated coil component, the position of the end of the pad electrode and the end of the solder and the first end of the terminal electrode deviates. Therefore, in the mounting structure of the laminated coil component, stress concentration on the end of the terminal electrode can be avoided. As a result, in the mounting structure of the laminated coil component, cracks can be suppressed in the element body during installation.
[0013] According to an aspect of the present invention, it is possible to suppress the occurrence of cracks in the element body during mounting. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 This is a perspective view of a laminated coil component according to an embodiment.
[0015] Figure 2 yes Figure 1 An exploded perspective view of a stacked coil component.
[0016] Figure 3 It is a diagram schematically showing the main surface of the element body.
[0017] Figure 4 It is a diagram schematically showing the end surface of the element body.
[0018] Figure 5 It is a diagram showing a mounting structure of a laminated coil component.
[0019] Figure 6This is a diagram schematically showing a main surface of an element body of a laminated coil component according to another embodiment. DETAILED DESCRIPTION
[0020] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings. In the description of the drawings, the same or corresponding elements are denoted by the same reference numerals, and repeated descriptions are omitted.
[0021] Reference Figure 1 and Figure 2 The laminated coil component according to the embodiment will be described. Figure 1 It is a perspective view of a laminated coil component according to an embodiment. Figure 2 yes Figure 1 An exploded perspective view of a laminated coil component. Figure 1 and Figure 2 As shown, the laminated coil component 1 of the embodiment includes: an element body 2; a pair of terminal electrodes 3; a glass layer G (see Figure 3 , 4 );Multiple coil conductors 5c, 5d, 5e, 5f;Connecting conductors 6, 7.
[0022] The element body 2 is in the shape of a rectangular parallelepiped. The rectangular parallelepiped shape includes the shape of a rectangular parallelepiped with chamfered corners and ridges, and the shape of a rectangular parallelepiped with rounded corners and ridges. The element body 2 has end faces 2a, 2b as outer surfaces; main faces 2c, 2d; side faces 2e, 2f. The end faces 2a, 2b are opposite to each other. The main faces 2c, 2d are opposite to each other. The side faces 2e, 2f are opposite to each other. Hereinafter, the relative direction of the side faces 2e, 2f is set as the first direction D1, the relative direction of the end faces 2a, 2b is set as the second direction D2, and the relative direction of the main faces 2c, 2d is set as the third direction D3. The first direction D1, the second direction D2, and the third direction D3 are substantially orthogonal to each other.
[0023] The end faces 2a and 2b extend along the third direction D3 in a manner connecting the main faces 2c and 2d. The end faces 2a and 2b also extend along the first direction D1 in a manner connecting the side faces 2e and 2f. The main faces 2c and 2d also extend along the second direction D2 in a manner connecting the end faces 2a and 2b. The main faces 2c and 2d also extend along the first direction D1 in a manner connecting the side faces 2e and 2f. The side faces 2e and 2f extend along the third direction D3 in a manner connecting the main faces 2c and 2d. The side faces 2e and 2f also extend along the second direction D2 in a manner connecting the end faces 2a and 2b.
[0024] The main surface 2c is a mounting surface, for example, a surface facing other electronic devices (eg, circuit substrates or laminated electronic components) when the laminated coil component 1 is mounted on other electronic devices (eg, circuit substrates or laminated electronic components) not shown. The end surfaces 2a and 2b are surfaces continuous from the mounting surface (ie, the main surface 2c).
[0025] The length of the element body 2 in the second direction D2 is longer than the length of the element body 2 in the third direction D3 and the length of the element body 2 in the first direction D1. The length of the element body 2 in the third direction D3 and the length of the element body 2 in the first direction D1 are equal to each other. That is, in this embodiment, the end faces 2a and 2b are square, and the main faces 2c, 2d and the side faces 2e and 2f are rectangular. The length of the element body 2 in the second direction D2 may be equal to the length of the element body 2 in the third direction D3 and the length of the element body 2 in the first direction D1, or may be shorter than these lengths. The length of the element body 2 in the third direction D3 and the length of the element body 2 in the first direction D1 may also be different from each other.
[0026] In addition, in this embodiment, “equal” may also include values that include a slight difference or manufacturing error within a predetermined range. For example, if multiple values are within a range of ±5% of the average value of the multiple values, the multiple values are defined as equal.
[0027] A pair of recesses 21 and a pair of recesses 22 are provided on the outer surface of the element body 2. Specifically, one recess 21 is provided on the end face 2a side of the main face 2c and is recessed toward the main face 2d. The other recess 21 is provided on the end face 2b side of the main face 2c and is recessed toward the main face 2d. One recess 22 is provided on the main face 2c side of the end face 2a and is recessed toward the end face 2b. The other recess 22 is provided on the main face 2c side of the end face 2b and is recessed toward the end face 2a.
[0028] A recess 21 and a recess 22 are continuously provided and correspond to a terminal electrode 3. Another recess 21 and another recess 22 are continuously provided and correspond to another terminal electrode 3. The recess 21 and the recess 22 have, for example, the same shape. In the present embodiment, the recess 21 and the recess 22 have different shapes from each other in that the width of the recess 21 (the length in the second direction D2) is shorter than the width of the recess 22 (the length in the third direction D3). A pair of recesses 21 and a pair of recesses 22 are provided separately from the main surface 2d and the side surfaces 2e and 2f. A pair of recesses 21 are provided separately from each other in the second direction D2.
[0029] The element body 2 is formed by stacking a plurality of element body layers (insulator layers) 12a to 12g in a first direction D1. That is, the stacking direction of the element body 2 is the first direction D1. The specific stacking structure will be described later. In the actual element body 2, the plurality of element body layers 12a to 12g are integrated to such an extent that the boundaries between the layers cannot be identified. The element body layers 12a to 12g are composed of, for example, magnetic materials (Ni-Cu-Zn ferrite materials, Ni-Cu-Zn-Mg ferrite materials, or Ni-Cu ferrite materials, etc.). The magnetic materials constituting the element body layers 12a to 12g may also include Fe alloys, etc. The element body layers 12a to 12g may also be composed of non-magnetic materials (glass ceramic materials, dielectric materials, etc.).
[0030] The terminal electrode 3 is provided on the element body 2. Specifically, the terminal electrode 3 is arranged in the recesses 21 and 22. More specifically, one terminal electrode 3 is arranged in one recess 21 and one recess 22, and the other terminal electrode 3 is arranged in the other recess 21 and the other recess 22. The pair of terminal electrodes 3 have, for example, the same shape. In the present embodiment, the conductor portion 31 and the conductor portion 32 have different shapes from each other in that the width of the conductor portion 31 (the length in the second direction D2) is shorter than the width of the conductor portion 32 (the length in the third direction D3). The pair of terminal electrodes 3 are provided on the element body 2 to be separated from each other in the second direction D2. The terminal electrode 3 is formed by stacking a plurality of terminal electrode layers 13b, 13c, 13d, 13e, 13f, and 13g in the first direction D1. That is, the stacking direction of the terminal electrode layers 13b to 13g is the first direction D1. In the actual terminal electrode 3 , the plurality of terminal electrode layers 13 b to 13 g are integrated to such an extent that the boundaries between the layers cannot be recognized.
[0031] From the first direction D1 (refer to Figure 1 ) observed, the terminal electrode 3 is L-shaped. The terminal electrode 3 has a conductor portion 31 and a conductor portion 32 which are provided integrally with each other. The conductor portion 31 extends along the second direction D2. The conductor portion 31 extends along the third direction D3. The conductor portion 31 is arranged in the recess 21. The conductor portion 32 is arranged in the recess 22.
[0032] The conductor portion 31 includes an end portion 31a and an end portion (first end portion) 31b that are opposite to each other in the second direction D2. The conductor portion 32 includes an end portion 32a and an end portion (second end portion) 32b that are opposite to each other in the third direction D3. The end portions 31a and 32a are connected to each other and are integrally provided with each other. The end portion 31b of the conductor portion 31 of one terminal electrode 3 and the end portion 31b of the conductor portion 31 of the other terminal electrode 3 are opposite to each other in the second direction D2.
[0033] Figure 3 Schematically shows the main surface of the element body. Figure 3 As shown, a plurality of (here, 5) first convex portions 33 are provided at the end portion 31a of the conductor portion 31. When viewed from the third direction D3, the first convex portion 33 becomes tapered toward the other terminal electrode 3 (end face 2a or end face 2b) opposite thereto. The tapered front end may be a shape in which the first convex portion 33 as a whole tapers toward the front end when viewed from the third direction D3. For example, when viewed from the third direction D3, a concave-convex is formed on the surface of the first convex portion 33, and even if a part thereof protrudes or is recessed, when viewed as the shape of the first convex portion 33 as a whole, when it tapers toward the front end, it can be said that it presents a tapered front end shape. In the present embodiment, when viewed from the third direction D3, the first convex portion 33 presents a triangular shape. The triangular shape mentioned here may be a roughly triangular shape when viewed from the third direction D3.
[0034] Figure 4 Schematically shows the end face of the element body. Figure 4 As shown, a plurality of (here, five) second protrusions 34 are provided at the end 32b of the conductor portion 32. The second protrusions 34 taper toward the main surface 2d when viewed from the second direction D2. In the present embodiment, the second protrusions 34 are triangular in shape when viewed from the second direction D2.
[0035] The terminal electrode 3 may be provided with a plated layer (not shown) containing, for example, Ni, Sn, Au, etc. by electroplating or electroless plating. The plated layer may include, for example, a Ni plated film containing Ni and covering the terminal electrode 3 or an Au plated film containing Au and covering the Ni plated film.
[0036] like Figure 3 and Figure 4 As shown, the glass layer G is composed of, for example, the same component as the glass component contained in the element body 2. The glass layer G is provided on the terminal electrode 3 along the outer edge of the terminal electrode 3. The glass layer G is provided so as to surround the terminal electrode 3.
[0037] like Figure 3As shown, the glass layer G is provided in the conductor part 31 in the region Ga along the outer edge of the side surface 2e and the outer edge of the side surface 2f and in the region Gb covering the first convex part 33 at the end 31b. In the present embodiment, the glass layer G is provided across the main surface 2c of the element body 2 and the conductor part 31. The glass layer G covers most of the first convex part 33 in the region Gb. Specifically, the region Gb is provided so as to cover the entire region on the front end side of the first convex part 33 and expose a part of the base end side of the first convex part 33. The region Gb covers a predetermined area or more of the area of the first convex part 33. The predetermined area is, for example, an area covering 60% or more of the area between the front end of the first convex part 33 and the base end of the first convex part 33, preferably an area covering 80% or more. The edge of the region Gb on the side of the end surface 2a or the end surface 2b is along the concave-convex formed by the first convex part 33. The edge of the region Gb on the side of the end surface 2a or the end surface 2b presents a curved wave shape (sine wave shape). The wave shape of the edge on the end surface 2 a or end surface 2 b side of the region Gb is convex at the first convex portion 33 , and is convex at the valley formed by adjacent first convex portions 33 .
[0038] like Figure 4 As shown, the glass layer G is provided in the conductor part 32 in the region Gc along the outer edge of the side surface 2e and the outer edge of the side surface 2f and the region Gd covering the second convex part 34 of the end 32b. The region Gc is continuous with the region Ga. In the present embodiment, the glass layer G is provided across the end surface 2a or the end surface 2b of the element body 2 and the conductor part 32. The glass layer G covers most of the second convex part 34 in the region Gd. Specifically, the region Gd is provided to cover the entire region on the front end side of the second convex part 34 and to expose a part of the base end side of the second convex part 34. The region Gd covers a predetermined area or more of the area of the second convex part 34. The edge on the main surface 2c side of the region Gd is along the concave and convex formed by the second convex part 34. The edge on the main surface 2c side of the region Gd presents a curved wave shape (sine wave shape). The wave shape of the edge on the main surface 2c side of the region Gd is convex at the second convex part 34, and is convex at the valley formed by the adjacent second convex parts 34.
[0039] Figure 1 The plurality of coil conductors 5c to 5f shown are connected to each other to form a coil 10 in the element body 2. The coil axis 10a of the coil 10 is arranged along the first direction D1. When viewed from the first direction D1, the coil conductors 5c to 5f are arranged so that at least a portion overlaps with each other. The coil conductors 5c to 5f are arranged separately from the end faces 2a, 2b, the main faces 2c, 2d, and the side faces 2e, 2f.
[0040] The coil conductors 5c to 5f are formed by stacking a plurality of coil conductor layers 15c, 15d, 15e, and 15f in the first direction D1. That is, the plurality of coil conductor layers 15c to 15f are arranged so that they all overlap each other when viewed from the first direction D1. The coil conductors 5c to 5f may also be formed by a single coil conductor layer 15c to 15f. Figure 2 In the figure, only one coil conductor layer 15c to 15f is shown. In the actual coil conductors 5c to 5f, the plurality of coil conductor layers 15c to 15f are integrated to such an extent that the boundaries between the layers cannot be recognized.
[0041] The connection conductor 6 extends along the second direction D2 and is connected to the coil conductor 5c and the other conductor portion 32. The connection conductor 7 extends along the second direction D2 and is connected to the coil conductor 5f and the one conductor portion 32. The connection conductors 6 and 7 are formed by stacking a plurality of connection conductor layers 16 and 17 in the first direction D1. Figure 2 Only one connection conductor layer 16, 17 is shown in FIG. In actual connection conductors 6, 7, a plurality of connection conductor layers 16, 17 are integrated to such an extent that the boundaries between the layers cannot be recognized.
[0042] The terminal electrode layers 13b to 13g, the coil conductor layers 15c to 15f, and the connection conductor layers 16 and 17 are made of a conductive material (for example, Ag or Pd). These layers may be made of the same material or different materials.
[0043] The laminated coil component 1 includes a plurality of layers La, Lb, Lc, Ld, Le, Lf, and Lg. The laminated coil component 1 is formed by, for example, laminating two layers La, one layer Lb, three layers Lc, three layers Ld, three layers Le, three layers Lf, one layer Lg, and two layers La in order from the side surface 2f. In addition, Figure 2 In FIG. 1 , one of each of the three layers Lc, the three layers Ld, the three layers Le, and the three layers Lf is shown, and the other two are omitted.
[0044] The layer La is composed of the element layer 12a.
[0045] The layer Lb is formed by combining the element body layer 12b and the pair of terminal electrode layers 13b. The element body layer 12b is provided with a defective portion Rb having a shape corresponding to the shape of the pair of terminal electrode layers 13b, into which the pair of terminal electrode layers 13b are embedded. The element body layer 12b and the pair of terminal electrode layers 13b are in a complementary relationship as a whole.
[0046] The layer Lc is formed by combining the element layer 12c, a pair of terminal electrode layers 13c, and a coil conductor layer 15c. The element layer 12c is provided with a defective portion Rc having a shape corresponding to the shape of the pair of terminal electrode layers 13 and the coil conductor layer 15c, into which the pair of terminal electrode layers 13c, the coil conductor layer 15c, and the connection conductor layer 16 are embedded. The element layer 12c and the pair of terminal electrode layers 13c, the coil conductor layer 15c, and the connection conductor layer 16 are in a complementary relationship as a whole.
[0047] The layer Ld is formed by combining the element layer 12d, the pair of terminal electrode layers 13d, and the coil conductor layer 15d. The element layer 12d is provided with a defective portion Rd having a shape corresponding to the shape of the pair of terminal electrode layers 13d and the coil conductor layer 15d, and the pair of terminal electrode layers 13d and the coil conductor layer 15d are embedded. The element layer 12d and the pair of terminal electrode layers 13d and the coil conductor layer 15d are in a complementary relationship as a whole.
[0048] The layer Le is formed by combining the element layer 12e, the pair of terminal electrode layers 13e, and the coil conductor layer 15e. The element layer 12e is provided with a defective portion Re having a shape corresponding to the shape of the pair of terminal electrode layers 13e and the coil conductor layer 15e, and the pair of terminal electrode layers 13e and the coil conductor layer 15e are embedded. The element layer 12e and the pair of terminal electrode layers 13e and the coil conductor layer 15e are in a complementary relationship as a whole.
[0049] The layer Lf is formed by combining the element layer 12f and a pair of terminal electrode layers 13f, the coil conductor layer 15f, and the connecting conductor layer 17. The element layer 12f is provided with a defective portion Rf having a shape corresponding to the shape of the pair of terminal electrode layers 13, the coil conductor layer 15f, and the connecting conductor layer 17, and the pair of terminal electrode layers 13f, the coil conductor layer 15f, and the connecting conductor layer 17 are embedded. The element layer 12f and the pair of terminal electrode layers 13, the coil conductor layer 15f, and the connecting conductor layer 17 are in a complementary relationship as a whole.
[0050] The layer Lg is formed by combining the element body layer 12g and the pair of terminal electrode layers 13g. The element body layer 12g is provided with a defective portion Rg having a shape corresponding to the shape of the pair of terminal electrode layers 13g, into which the pair of terminal electrode layers 13g are embedded. The element body layer 12g and the pair of terminal electrode layers 13g are in a complementary relationship as a whole.
[0051] The defective parts Rb, Rc, Rd, Re, Rf, and Rg are integrated to form the above-mentioned pair of recesses 21 and the pair of recesses 22. The width of the defective parts Rb to Rg (hereinafter, the width of the defective parts) is basically set to be wider than the width of the terminal electrode layers 13b to 13g, the coil conductor layers 15c to 15f, and the connecting conductor layers 16 and 17 (hereinafter, the width of the conductor part). In order to improve the adhesion between the element layers 12b, 12c, 12d, 12e, 12f, and 12g and the terminal electrode layers 13b to 13g, the coil conductor layers 15c to 15f, and the connecting conductor layers 16 and 17, the width of the defective parts may be intentionally set to be narrower than the width of the conductor part. The value obtained by subtracting the width of the conductor part from the width of the defective part is preferably, for example, not less than -3 μm and not more than 10 μm, and more preferably not less than 0 μm and not more than 10 μm.
[0052] An example of a method for manufacturing the laminated coil component 1 according to the embodiment will be described.
[0053] First, a body forming layer is formed by applying a body paste containing the constituent materials of the above-mentioned body layers 12a to 12g and a photosensitive material on a substrate (for example, a PET film). The photosensitive material contained in the body paste may be either a negative type or a positive type, and a known material may be used. Next, the body forming layer is exposed and developed by a photolithography method using a Cr mask, for example, to form a body pattern on the substrate in a shape corresponding to the shape of the conductor forming layer described later. The body pattern is a layer that becomes the body layers 12b to 12g after heat treatment. That is, a body pattern is formed in which defective portions that become defective portions Rb to Rg are provided. In addition, the "photolithography method" of this embodiment is not limited to the type of mask, etc. as long as it is a method of processing a layer of a processing object containing a photosensitive material into a desired pattern by exposing and developing it.
[0054] On the other hand, a conductor forming layer is formed by applying a conductor paste containing the constituent materials of the above-mentioned terminal electrode layers 13b~13g, coil conductor layers 15c~15f and connecting conductor layers 16 and 17, and a photosensitive material on a substrate (for example, a PET film). The photosensitive material contained in the conductor paste can also be either negative or positive, and known materials can be used. Next, the conductor forming layer is exposed and developed by a photolithography method using a Cr mask, for example, to form a conductor pattern on the substrate. The conductor pattern is a layer that becomes the terminal electrode layers 13b~13g, the coil conductor layers 15c~15g and the connecting conductor layers 16 and 17 after heat treatment.
[0055] Next, the element forming layer is transferred from the substrate to the support. In this embodiment, the element forming layer transfer step is repeated twice, so that two layers of element forming layers are stacked on the support. These element forming layers become the layer La after the heat treatment.
[0056] Next, by repeatedly transferring the conductor pattern and the element pattern onto the support, the conductor pattern and the element pattern are stacked in the first direction D1. Specifically, first, the conductor pattern is transferred from the substrate to the element forming layer. Next, the element pattern is transferred from the substrate to the element forming layer. The conductor pattern is combined with the defective portion of the element pattern, and the element pattern and the conductor pattern become the same layer on the element forming layer. In addition, the transfer process of the conductor pattern and the element pattern is repeatedly implemented, and the conductor pattern and the element pattern are stacked in a state of being combined with each other. Thus, the layers Lb to Lg are stacked after the heat treatment.
[0057] Next, the element forming layer is transferred from the substrate to the layer stacked in the transfer process of the conductor pattern and the element pattern. In this embodiment, the transfer process of the element forming layer is repeated twice, so that two layers of element forming layers are stacked on the layer. These element forming layers are the layers that become the layer La after the heat treatment.
[0058] Through the above, the laminated body constituting the laminated coil component 1 after heat treatment is formed on the support. Next, the obtained laminated body is cut into a predetermined size. Then, the cut laminated body is subjected to a binder removal treatment and then subjected to heat treatment. The heat treatment temperature is, for example, about 850 to 900° C. As required, the terminal electrode 3 may be electroplated or electroless plated after heat treatment to provide a plating layer.
[0059] Next, a glass layer G is formed on the terminal electrode 3. The glass layer G forms a mask covering the portion other than the portion where the glass layer G is formed, and a paste containing a glass component is applied (printed). Then, the paste is dried to form the glass layer G. In addition, the glass layer G can also be formed by precipitation of a glass component contained in the element body 2. In the above manner, the laminated coil component 1 is manufactured.
[0060] Figure 5 FIG. 2 is a diagram showing the mounting structure of a laminated coil component. Figure 5 As shown, in the mounting structure 100, the laminated coil component 1 is mounted on the pad electrodes 120 and 130 provided on the circuit substrate 110 by means of solder F. One terminal electrode 3 of the laminated coil component 1 is fixed to the pad electrode 120 by means of solder F. The other terminal electrode 3 of the laminated coil component 1 is fixed to the pad electrode 130 by means of solder F. The solder F is formed by spanning the conductor portion 31 and the conductor portion 32 of the terminal electrode 3. The solder F is disposed between the conductor portion 31 of the terminal electrode 3 and the pad electrodes 120 and 130.
[0061] In this embodiment, solder F is not formed on the glass layer G of the laminated coil component 1. Therefore, in the mounting structure 100 of the laminated coil component 1, as shown in FIG. Figure 5As shown in the portion surrounded by the dotted line in FIG. 1 , when viewed from the first direction D1, the ends of the pad electrodes 120 and 130 and the end of the solder F do not overlap with the end 31b of the terminal electrode 3. That is, in the first direction D1, the positions of the ends of the pad electrodes 120 and 130 and the end of the solder F do not coincide with the position of the end 31b of the terminal electrode 3. Figure 5 As shown by the portion surrounded by the dotted line in FIG. 1 , the end of the solder F does not overlap with the end 32b of the terminal electrode 3 when viewed from the second direction D2. That is, in the second direction D2, the position of the end of the solder F does not coincide with the position of the end 32b of the terminal electrode 3.
[0062] As described above, in the laminated coil component 1 of the present embodiment, the terminal electrode 3 is provided with a plurality of first protrusions 33 that taper toward the opposite terminal electrode 3 side at the end 31b of the conductor portion 31. In this structure, in the laminated coil component 1, a glass layer G is provided along the edge of the terminal electrode 3 including the first protrusions 33 at the end 31b of the conductor portion 31 of the terminal electrode 3. The solder F is not formed on the glass layer G. Therefore, in the laminated coil component 1, when the solder is mounted on the pad electrodes 120 and 130 of the circuit substrate 110, the solder F is not formed on the glass layer G covering the end 31b. Therefore, when the laminated coil component 1 is mounted on the pad electrodes 120 and 130, the positions of the ends of the pad electrodes 120 and 130 and the ends of the solder F do not overlap with the positions of the ends of the terminal electrodes 3. That is, in the first direction D1, the positions of the ends of the pad electrodes 120 and 130 and the ends of the solder F do not coincide with the positions of the ends of the terminal electrodes 3. Therefore, in the laminated coil component 1, stress concentration on the ends of the terminal electrodes 3 can be avoided. As a result, in the laminated coil component, when mounted, cracks can be suppressed from being generated in the element body 2.
[0063] In the laminated coil component 1 of the present embodiment, the glass layer G covers 60% or more of the area of the first protrusion 33. In this structure, it is possible to more reliably avoid the formation of solder F on the end portion 31b of the terminal electrode 3.
[0064] In the laminated coil component 1 of this embodiment, the edge of the glass layer G on the end surface 2a or 2b side has a corrugated shape corresponding to the first protrusion 33. In this structure, the glass layer G covers the edge of the first protrusion 33 and ensures a region for forming solder F in the terminal electrode 3.
[0065] In the laminated coil component 1 of the present embodiment, each of a pair of terminal electrodes 3 is arranged in a recess 22 formed in each of a pair of end faces 2a. A plurality of second protrusions 34 tapering toward the main surface 2d are provided at the end 32b on the main surface 2d side of the conductor portion 32 of the terminal electrode 3 arranged at the end face 2a or the end face 2b. The glass layer G is provided at the end 32b of the conductor portion 32 of the terminal electrode 3 along the edge of the terminal electrode 3 including the second protrusion 34. In this structure, when solder is mounted on the pad electrodes 120 and 130 of the circuit substrate 110, solder is not formed on the glass layer G covering the end 32b. Thus, when the laminated coil component 1 is mounted on the pad electrodes 120 and 130, the position of the end of the solder F and the position of the end of the terminal electrode 3 do not overlap. Therefore, in the laminated coil component 1, stress concentration on the end of the terminal electrode 3 can be avoided. As a result, in the laminated coil component 1 , it is possible to suppress the occurrence of cracks in the element body 2 during mounting.
[0066] As mentioned above, although embodiment of this invention was described, this invention is not necessarily limited to the said embodiment, Various changes can be made within the range which does not deviate from the summary.
[0067] In the above embodiment, the terminal electrode 3 has a conductor portion 31 and a conductor portion 32 as an example. However, the terminal electrode 3 only needs to have at least the conductor portion 31. Figure 6 As shown, the laminated coil component 1A includes a terminal electrode 3A. The terminal electrode 3A is provided with a plurality of first convex portions 33A tapered toward the other terminal electrode 3A side at the end 31Ab opposite in the second direction D2, and a plurality of third convex portions 35 tapered toward the end face 2a or the end face 2b side at the end (third end) 31Aa. The glass layer G is provided along the edge of the terminal electrode 3A including the first convex portions 33A and the third convex portions 35. The glass layer G is provided in the conductor portion 31A in the region Ga along the outer edge of the side face 2e and the outer edge of the side face 2f, the region Gb covering the first convex portion 33A of the end 31Ab, and the region Ge covering the third convex portion 35 of the end 31Aa.
[0068] In this structure, when solder is mounted on the pad electrodes 120 and 130 of the circuit substrate 110, solder is not formed on the glass layer G covering the first convex portion 33A and the third convex portion 35. Thus, when the laminated coil component 1A is mounted on the pad electrodes 120 and 130, the ends of the pad electrodes 120 and 130 and the ends of the solder F do not overlap with the ends of the terminal electrodes 3A. Therefore, in the laminated coil component 1A, stress concentration on the ends of the terminal electrodes 3A can be avoided. As a result, in the laminated coil component 1A, cracks can be suppressed from being generated in the element body 2 when mounted.
[0069] In the above embodiment, the first convex portion 33, 33A, the second convex portion 34 and the third convex portion 35 are described as an example in which the first convex portion 33, 33A, the second convex portion 34 and the third convex portion 35 are triangular in shape. However, the convex portion may be in a tapered shape, for example, a trapezoidal shape.
Claims
1. A laminated coil component comprising: A body formed by laminating a plurality of insulating layers and having a pair of end faces facing each other, a pair of main faces facing each other, and a pair of side faces facing each other, wherein the main faces are mounting faces; a pair of terminal electrodes arranged in a recess formed on the mounting surface, on each of the pair of end surfaces of the element body; and a glass layer disposed on the terminal electrode, In each of the pair of terminal electrodes, a plurality of first protrusions are provided at first ends facing each other in the opposing direction of the pair of end faces, the first protrusions being tapered toward the other terminal electrode facing each other. The glass layer is provided at the first end portion of the terminal electrode along the edge of the terminal electrode including at least the first protrusion. The glass layer has a shape corresponding to the plurality of first protrusions of the terminal electrode.
2. The laminated coil component according to claim 1, wherein The glass layer covers more than 60% of the area of the first convex portion.
3. The laminated coil component according to claim 1, wherein An edge of the glass layer on the end surface side has a corrugated shape corresponding to the plurality of first protrusions.
4. The laminated coil component according to claim 2, wherein An edge of the glass layer on the end surface side has a corrugated shape corresponding to the plurality of first protrusions.
5. The laminated coil component according to any one of claims 1 to 4, wherein Each of the pair of terminal electrodes is arranged in a recess formed in the mounting surface, and is arranged in a recess formed in each of the pair of end surfaces. A plurality of second protrusions tapering toward the main surface are provided at the second end portion on the other main surface side of the terminal electrode arranged on the end surface. The glass layer is provided at the second end portion of the terminal electrode along an edge of the terminal electrode including at least the second protrusion.
6. The laminated coil component according to any one of claims 1 to 4, wherein Each of the pair of terminal electrodes has a plurality of third protrusions at a third end portion on the end surface side, the third protrusions being tapered toward the end surface side. The glass layer is provided at the third end portion of the terminal electrode along an edge of the terminal electrode including at least the third protrusion.
7. A mounting structure for a laminated coil component, comprising: The laminated coil component according to any one of claims 1 to 6; a circuit board having a pad electrode on which the laminated coil component is mounted; and Solder is arranged between the terminal electrode and the pad electrode of the coil component, The solder is not formed on the glass layer, When viewed from the opposing direction of the pair of main surfaces of the element body, the end of the pad electrode and the end of the solder do not overlap with the first end portion of the terminal electrode.