A design method for functionally graded piezoelectric composite integrator
By placing pressure sensors in various force-generating parts of the human body and optimizing the design of the finite element model, and using simulated annealing algorithms to optimize the mass fraction of piezoelectric ceramics, the problem of a single design of the existing energy collector is solved and more efficient energy conversion efficiency is achieved.
Patent Information
- Application Number
- CN202210070460.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-21
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-01-21
AI Technical Summary
Existing piezoelectric composite flexible energy concentrators have a single design and cannot fully utilize the force states of different body parts during human movement, resulting in low energy conversion efficiency.
By placing pressure sensors in various force-generating parts of the human body, a finite element model is established to optimize the mass fraction of piezoelectric ceramics, and a simulated annealing algorithm is used to optimize the mass fraction of piezoelectric ceramics in each unit to achieve a personalized functional gradient energy concentrator. design.
The energy conversion efficiency is improved, the stress of each force-generating part is fully utilized, the piezoelectric ceramic mass fraction distribution of the energy collector composite material is more reasonable, and the electrical energy conversion performance is improved.
Smart Images

Figure CN114462274B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a design method for a functional gradient piezoelectric composite material integrator, and belongs to the technical field of flexible electric energy collection. Background Art
[0002] The use of various existing electronic devices consumes a large amount of electrical energy, which is often obtained through the conversion of other energies. Large amounts of energy consumption may accelerate the arrival of an energy crisis.
[0003] Energy collectors made of piezoelectric materials can collect energy from the environment and convert it into electrical energy to power portable electronic devices. For example, in the field of wearables, energy collectors made of flexible materials can be placed on the soles of the feet or on the knees, elbows, waist joints and other force-generating parts to generate electricity using the energy of human movement, thereby powering wearable electronic devices.
[0004] Flexible energy collectors usually use piezoelectric composite materials to disperse piezoelectric ceramic particles into a flexible matrix. Piezoelectric ceramics can realize the conversion of mechanical energy into electrical energy, and the matrix material protects the internal ceramics to prevent them from being damaged under stress. Existing piezoelectric composite flexible energy collectors often have a single component and a simple structure. For example, due to the different force states generated by different moving parts of the body when different wearers exercise, the existing single structural design method cannot give full play to the energy conversion effect of the energy collector. Therefore, a personalized functional gradient piezoelectric composite energy collector design method is proposed, which has important theoretical and application significance for improving energy conversion efficiency. Summary of the invention
[0005] In order to solve the above-mentioned existing technical problems, the present invention provides a design method of a functional gradient energy collector which takes into account the state of the force-generating part of the human body during exercise and effectively improves the energy conversion efficiency.
[0006] The technical solution of the present invention:
[0007] A design method for a functionally gradient piezoelectric composite integrator comprises the following steps:
[0008] Step 1: Place pressure sensors at various force-generating parts of the human body to extract the alternating stress [σ1,σ2,…,σ m ] T ;
[0009] Step 2, establishing a finite element model of the piezoelectric composite material, performing finite element simulation on the piezoelectric composite materials with different piezoelectric ceramic contents under different input stress conditions, calculating the output voltage, and obtaining the functional relationship between the output voltage V, the composite material resistance R, the input stress σ, and the piezoelectric ceramic mass fraction ω;
[0010] Step 3: Design the shape of the energy collector according to the collective shape of the tester's force-generating part, discretize the energy collector into n units, and establish the total output voltage V according to the series-parallel relationship of each unit. out Functional relationship with each unit voltage and resistance;
[0011] Step 4, using a simulated annealing algorithm to optimize the design and determine the mass fraction of the piezoelectric ceramics of each dispersed unit;
[0012] Step 5, modeling the optimized structural parameters obtained in step 4 to obtain a personalized functional gradient piezoelectric composite energy collector that takes into account the stress state of the human body's force-generating parts during exercise.
[0013] It is further defined that the force-generating parts in step 1 include shoulder joints, elbow joints, wrist joints, knee joints and / or soles of feet.
[0014] It is further defined that in step 1, the pressure sensors are evenly distributed, and the number of sampling points at each force-generating location is no less than 50, and the force state of each force-generating location is obtained by linear interpolation.
[0015] Further defined, the specific operation process of step 2 is:
[0016] (1) Modeling a piezoelectric composite material with a piezoelectric ceramic mass fraction of 0%-40% by three-dimensional modeling software or finite element software, importing the model into finite element analysis software, dividing the grid, inputting the stress within the range extracted in step 1 on the upper surface, and calculating, and obtaining the output voltage and resistance of the energy collector by surface integration;
[0017] (2) According to the simulation results of step (1), the output voltage and internal resistance of the piezoelectric composite material with a piezoelectric ceramic mass fraction of 0%-40% under different external pressure load conditions are obtained, and the functional relationship between the output voltage V, the composite material resistance R, the input stress σ and the ceramic mass fraction ω is fitted.
[0018] It is further defined that, during the discretization in step 3, the difference in the forces at different points on the same dispersed unit is within 10%.
[0019] Further defined, the operation process of step 4 is:
[0020] First, each dispersed unit is given a random piezoelectric ceramic mass fraction [ω1,ω2,…,ω n ] T Then, the total output voltage is calculated according to the function formula of step 2 and step 3. After generating new random material parameters, the surface voltage output is also calculated. If the newly generated material parameters are better than the initial values, the new parameters are fully accepted. Otherwise, they are accepted to a certain extent and a new iteration is performed. When no new solution appears after multiple consecutive iterations, the solution is taken as the optimal value and the iteration ends.
[0021] Further, step 4 selects the simulated annealing optimization algorithm to calculate the total output voltage V out Optimization, build optimization model:
[0022] maxV out =f(ω)
[0023]
[0024] Where g i (ω)≥0 is an inequality constraint; h j (ω) = 0 is an equality constraint, and the constraint conditions include geometric constraints, material parameter constraints, and strength constraints; k1 and k2 are the number of inequality constraints and equality constraints, respectively; t(σ) = 0 is the boundary condition for stress;
[0025] The design domain is denoted as S. If a feasible solution ω*∈S is obtained, such that If f(ω*)>f(ω), then ω* is called the optimal solution to the multi-objective optimization problem.
[0026] Further defined, the specific operation process of step 4 is:
[0027] ① First, give each discrete module a random piezoelectric ceramic mass fraction [ω 0 ]=[ω1 0 ,ω2 0 ,…,ω n 0 ] T , and calculate the output voltage V out 0 =f(ω 0 );
[0028] ② The perturbation produces a new solution ω r , calculate the objective function f(ω r ), and calculate Δf=f(ω r )-f(ω 0 );
[0029] ③Δf≥0, then accept the new solution ω 0 =ω r , otherwise the new solution is accepted according to the Metropolis acceptance criteria;
[0030] ④ Repeat steps ② and ③ until the number of iterations is reached, and determine whether the termination condition is met;
[0031] ⑤If the termination condition is met, the operation is terminated and the optimal solution is output. Otherwise, the number of stable reset iterations is slowly reduced, and steps ① to ④ are repeated until the termination condition is met.
[0032] Beneficial effects of the present invention:
[0033] (1) In the design process of the flexible energy collector, the present invention takes into account the state of the user's body force-generating part during exercise and makes a personalized design. Compared with the conventional uniform energy collector design, the functional gradient energy collector design of the present invention can improve the energy conversion efficiency.
[0034] (2) The flexible energy collector designed by the method of the present invention can fully utilize the stress of each force-generating part, so that the mass fraction distribution of the piezoelectric ceramics in the energy collector composite material is more reasonable. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 Design a flow chart for personalized functionally graded piezoelectric composite energy harvesters;
[0036] Figure 2 This is the simulation result diagram of the electric potential distribution when the piezoelectric composite material is subjected to force;
[0037] Figure 3 It is a schematic diagram of the discretization of the energy collector in Example 1;
[0038] Figure 4 Flowchart of simulated annealing optimization algorithm. DETAILED DESCRIPTION
[0039] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0040] The experimental methods used in the following examples are conventional methods unless otherwise specified. The materials, reagents, methods and instruments used are conventional materials, reagents, methods and instruments in the art unless otherwise specified, and can be obtained through commercial channels by those skilled in the art.
[0041] Embodiment 1:
[0042] This embodiment takes the sole of the foot as an example of a force generating part, and designs a method for a personalized functional gradient piezoelectric composite energy collector for the sole of the foot. Figure 1 The specific operation process is as follows:
[0043] Step 1: evenly distribute multiple pressure sensors on the sole of the foot, with no less than 50 sampling points, to extract the alternating stress [σ1,σ2,…,σ m ] T And the force state of the force-generating part of the human body during exercise is obtained through linear interpolation.
[0044] Step 2, first, draw a composite material model with different piezoelectric ceramic mass fractions through the modeling module of the 3D modeling software, the mass fraction range is between 0-40%, and divide the grid through the finite element software. The upper and lower surfaces of the model are set to equipotential respectively, and the upper surface is input with the stress within the range measured in step 1 and then calculated. The output voltage and resistance of the collector are obtained by surface integration. The simulation results of the potential distribution of the piezoelectric composite material when it is stressed are shown in Figure 2 As shown;
[0045] Then, according to the simulation results, the output voltage and internal resistance of composites with different mass fractions under different external pressure loads are obtained, and the functional relationship between the output voltage V, composite material resistance R, input stress σ and ceramic mass fraction ω is fitted:
[0046] V=f1(σ,ω)
[0047] R=f2(σ,ω)
[0048] Where: V is the output voltage, R is the resistance of the composite material, σ is the input stress, and ω is the ceramic mass fraction.
[0049] Step 3: Discretize the energy collector at the sole of the foot during exercise. The discretization diagram is shown in Figure 3 As shown, its shape is the basic outline of the sole. The force difference at different points on the same unit is within 10%. The vertical layering is not less than 3 layers. The number of dispersed units is n. According to the series-parallel relationship of each unit, the total output voltage V is established. out Functional relationship with each unit voltage and resistance:
[0050] V out =f3(V1,V2,...V n ,R1,R2,...R n )
[0051] Where: V out is the final output voltage of the energy collector, V i is the output voltage of the i-th unit, R i is the resistance of the i-th unit, 1≤i≤n.
[0052] Step 4: Use simulated annealing optimization algorithm to optimize the output voltage and optimize the main design parameters ω=[ω1,ω2,…,ω n ] T Make optimizations.
[0053] The optimization model is established as:
[0054] maxV out =f(ω)
[0055]
[0056] The design domain is denoted as S. If a feasible solution ω*∈S can be obtained, such that If f(ω*)>f(ω), then ω* is called the optimal solution to the multi-objective optimization problem, g i (ω)≥0 is an inequality constraint, h j (ω) = 0 is an equality constraint. The constraint conditions include geometric constraints, material parameter constraints, and strength constraints. k1 and k2 are the number of inequality constraints and equality constraints, respectively. t(σ) = 0 is the boundary condition for stress.
[0057] Optimize the process such as Figure 4 As shown, the specific process is as follows:
[0058] (1) Give each discrete module a random piezoelectric ceramic mass fraction: ω 0 =[ω1 0 ,ω2 0 ,…,ω n 0 ] T , and calculate the output voltage V out 0 =f(ω 0 );
[0059] (2) Perturbation produces new solution ω r , calculate the objective function f(ω r ), and calculate the change ΔV of the output voltage before and after the disturbance out =f(ω r )-f(ω 0 );
[0060] (3) When ΔV out ≥0, then accept the new solution ω 0 =ω r , otherwise the new solution is accepted according to the Metropolis acceptance criterion, and the acceptance probability is:
[0061] P = exp(ΔV out / T)
[0062] Where P is the acceptance probability and T is the control parameter of the annealing process;
[0063] Randomly generate a random number α between 0 and 1. If P ≥ α, accept the new solution ω 0 =ω r , otherwise the new solution is not accepted;
[0064] (4) Repeat steps (2) and (3) until the number of iterations N is reached, and determine whether the termination condition is met;
[0065] (5) If the termination condition is met, the operation is terminated and the optimal solution is output; otherwise, the annealing temperature is lowered, the number of iterations is reset, and steps (1) to (4) are repeated until the termination condition is met.
[0066] The above description is only a preferred embodiment of the present invention. In view of the fact that technicians in the field of the present invention can make appropriate changes and modifications to the above implementation, the present invention is not limited to the specific implementation described above. Some modifications and changes to the present invention should also fall within the scope of protection of the claims of the present invention.
Claims
1. A design method for a functionally gradient piezoelectric composite integrator, characterized in that: The method comprises the following steps: Step 1: Place pressure sensors at various force-generating parts of the human body to extract the alternating stress [σ1,σ2,…,σ m ] T ; Step 2, establishing a finite element model of the piezoelectric composite material, performing finite element simulation on the piezoelectric composite materials with different piezoelectric ceramic contents under different input stress conditions, calculating the output voltage, and obtaining the functional relationship between the output voltage V, the composite material resistance R, the input stress σ, and the piezoelectric ceramic mass fraction ω; Step 3: Design the shape of the energy collector according to the collective shape of the force-generating part of the tester, discretize the energy collector into n units, and establish the total output voltage V according to the series-parallel relationship of each unit. out Functional relationship with each unit voltage and resistance; Step 4, using a simulated annealing algorithm to optimize the design and determine the mass fraction of the piezoelectric ceramics of each dispersed unit; Step 5, modeling the optimized structural parameters obtained in step 4 to obtain a personalized functional gradient piezoelectric composite energy collector that takes into account the stress state of the human body's force-generating parts during exercise.
2. The design method of a functionally gradient piezoelectric composite integrator according to claim 1, characterized in that: The force-generating parts in step 1 include the shoulder joint, elbow joint, wrist joint, knee joint and / or sole of the foot.
3. The design method of a functionally gradient piezoelectric composite integrator according to claim 1, characterized in that: In the step 1, the pressure sensors are evenly distributed, and the number of sampling points at each force-generating part is no less than 50, and the force state of each force-generating part is obtained by linear interpolation.
4. The design method of a functionally gradient piezoelectric composite integrator according to claim 1, characterized in that: The specific operation process of step 2 is as follows: (1) Modeling a piezoelectric composite material with a piezoelectric ceramic mass fraction of 0%-40% by three-dimensional modeling software or finite element software, importing the model into finite element analysis software, dividing the grid, inputting the stress within the range extracted in step 1 on the upper surface, and calculating, and obtaining the output voltage and resistance of the energy collector by surface integration; (2) According to the simulation results of step (1), the output voltage and internal resistance of the piezoelectric composite material with a piezoelectric ceramic mass fraction of 0%-40% under different external pressure load conditions are obtained, and the functional relationship between the output voltage V, the composite material resistance R, the input stress σ and the ceramic mass fraction ω is fitted.
5. The design method of a functionally gradient piezoelectric composite integrator according to claim 1, characterized in that: When the step 3 is discretized, the difference in force between different points on the same dispersed unit is within 10%.
6. The design method of a functionally gradient piezoelectric composite integrator according to claim 1, characterized in that: The operation process of step 4 is as follows: First, a random piezoelectric ceramic mass fraction [ω1,ω2,…,ω n ] T Then, the total output voltage is calculated according to the function formula of step 2 and step 3. After generating new random material parameters, the surface voltage output is also calculated. If the newly generated material parameters are better than the initial values, the new parameters are fully accepted. Otherwise, they are accepted to a certain extent and a new iteration is performed. When no new solution appears after multiple consecutive iterations, the solution is taken as the optimal value and the iteration ends.
7. The design method of a functionally gradient piezoelectric composite integrator according to claim 1, characterized in that: Step 4 selects a simulated annealing optimization algorithm to calculate the total output voltage V out Optimization, build optimization model: maxV out =f(ω) Where g i (ω)≥0 is an inequality constraint; h j (ω) = 0 is an equality constraint, and the constraint conditions include geometric constraints, material parameter constraints, and strength constraints; k1 and k2 are the number of inequality constraints and equality constraints, respectively; t(σ) = 0 is the boundary condition for stress; The design domain is denoted as S. If a feasible solution ω*∈S is obtained, such that If f(ω*)>f(ω), then ω* is called the optimal solution to the multi-objective optimization problem; The specific operation process of step 4 is as follows: ① First, give each discrete module a random piezoelectric ceramic mass fraction [ω 0 ]=[ω1 0 ,ω2 0 ,…,ω n 0 ] T , and calculate the output voltage V out 0 =f(ω 0 ); ② The perturbation produces a new solution ω r , calculate the objective function f(ω r ), and calculate Δf=f(ω r )-f(ω 0 ); ③Δf≥0, then accept the new solution ω 0 =ω r , otherwise the new solution is accepted according to the Metropolis acceptance criteria; ④ Repeat steps ② and ③ until the number of iterations is reached, and determine whether the termination condition is met; ⑤If the termination condition is met, the operation is terminated and the optimal solution is output. Otherwise, the number of stable reset iterations is slowly reduced, and steps ① to ④ are repeated until the termination condition is met.